Methods for improving overlay accuracy and semiconductor manufacturing equipment

By modifying the back side of the wafer to change it from hydrophilic to hydrophobic, the problem of high friction between the wafer and the stage was solved, and the overlay accuracy was improved.

CN117908337BActive Publication Date: 2026-11-10SHANGHAI HUALI MICROELECTRONICS CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410224373.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-02-28
Publication Date
2026-11-10
Estimated Expiration
2044-02-28

AI Technical Summary

Technical Problem

The friction between the wafer and the stage is relatively large, which affects the overlay accuracy.

Method used

The back side of the wafer is modified to change it from hydrophilic to hydrophobic, thereby reducing surface free energy and friction.

Benefits of technology

By reducing the surface free energy on the back side of the wafer, the surface tension and intermolecular forces at the interface are reduced, thus improving the overlay accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117908337B_ABST
    Figure CN117908337B_ABST
Patent Text Reader

Abstract

This invention provides a method for improving overlay accuracy and a semiconductor manufacturing apparatus. The method for improving overlay accuracy includes: after photoresist spraying, modifying the back side of the wafer to change it from hydrophilic to hydrophobic. This configuration, by modifying the back side of the photoresist-coated wafer from hydrophilic to hydrophobic, reduces the surface free energy of the back side of the wafer, resulting in reduced surface tension, increased contact angle, reduced intermolecular forces at the interface, and decreased polarity. This reduces the friction between the back side of the wafer and the stage, thereby improving the overlay accuracy of the exposure machine.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing, and in particular to a method for improving overlay accuracy and semiconductor manufacturing equipment. Background Technology

[0002] In semiconductor manufacturing, as the number of wafers produced by lithography machines increases, the wafer stage inside the exposure machine experiences wear. Due to the warping of the wafer edges, the stage edges are more prone to slippage during adhesion, accelerating stage wear. Even with reduced roughness, the wear-prone stage can still increase friction when in contact with the wafer due to van der Waals forces, ultimately affecting overlay accuracy. Furthermore, the friction between the wafer and stage is also influenced by the surface free energy of the contact surface (i.e., the back face). The back face is typically made of silicon or silicon-containing materials, which readily absorb moisture from the air, making the surface hydrophilic, increasing surface tension, decreasing the contact angle, and strengthening the intermolecular forces at the interface. This high polarity further increases friction, impacting overlay accuracy.

[0003] Therefore, how to reduce the friction between the wafer and the stage to improve the overlay accuracy has become a technical problem that urgently needs to be solved by those skilled in the art. Summary of the Invention

[0004] The purpose of this invention is to provide a method and semiconductor manufacturing equipment for improving overlay accuracy, so as to solve the problem that the large friction between the wafer and the stage affects the overlay accuracy.

[0005] To achieve the above objectives, the present invention provides a method for improving overlay accuracy, comprising: after completing photoresist spraying, modifying the back side of the wafer to change the back side of the wafer from hydrophilic to hydrophobic.

[0006] Optionally, the modification treatment of the back side of the wafer includes:

[0007] A modifier is sprayed onto the back side of the wafer;

[0008] The back side of the wafer is dried.

[0009] Optionally, the modifier includes silazane-based reagents.

[0010] Optionally, the modifier may include a gaseous modifier and / or a liquid modifier.

[0011] Optionally, the modifier can be sprayed onto a partial or complete area of ​​the back side of the wafer using a spin-spraying method.

[0012] Optionally, the back side of the wafer can be dried by spin drying.

[0013] To achieve the above objectives, the present invention also provides a semiconductor manufacturing apparatus for implementing the method for improving overlay accuracy as described above, comprising: a transfer unit, a processing unit, and a task unit;

[0014] The task unit includes a coating subunit and an exposure subunit. The transfer unit is connected in sequence to the coating subunit, the processing unit and the exposure subunit. The transfer unit is used to load the wafer and enables the wafer to flow between the coating subunit, the processing unit and the exposure subunit.

[0015] The processing unit is used to modify the back side of the wafer to change it from hydrophilic to hydrophobic.

[0016] Optionally, the processing unit includes a driving subunit and a spraying subunit;

[0017] The spraying subunit is used to spray a modifier onto the back side of the wafer;

[0018] The transfer unit can transfer the wafer to the driving subunit, and the driving subunit can rotate around an axis to drive the wafer to rotate when the spraying subunit is spraying.

[0019] Optionally, the processing unit further includes a reaction chamber, in which both the driving subunit and the spraying subunit are disposed. The spraying subunit is used to spray gaseous modifier and / or liquid modifier onto the back side of the wafer.

[0020] Optionally, after the spraying subunit completes the spraying on the back side of the wafer, the driving subunit drives the wafer to rotate, thereby achieving the drying process of the wafer.

[0021] In summary, the method for improving overlay accuracy provided in this application has the following advantages compared to the prior art:

[0022] The method for improving overlay accuracy provided in this application modifies the back side of the wafer after photoresist spraying, changing it from hydrophilic to hydrophobic. This reduces the surface free energy of the back side of the wafer, thereby reducing surface tension, increasing the contact angle, decreasing the intermolecular forces at the interface, and lowering the polarity. As a result, the friction between the back side of the wafer and the stage is reduced, thus improving the overlay accuracy of the exposure machine. Attached Figure Description

[0023] Figure 1 This is a top view of a platform in the prior art;

[0024] Figure 2 A side view of a wafer being loaded onto a stage in the prior art;

[0025] Figure 3 for Figure 2 A schematic diagram of the stage in section A when it is not worn;

[0026] Figure 4 for Figure 2 A schematic diagram showing the wear and tear on the platform in section A.

[0027] Figure 5 This is a map of a wafer in the prior art when the stage is not worn.

[0028] Figure 6 This is a map of a wafer worn on a stage in existing technology.

[0029] Figure 7 A flowchart of a method for improving overlay accuracy provided in an embodiment of the present invention;

[0030] Figure 8 Molecular structure diagrams of the back side of a wafer before and after modification, provided for embodiments of the present invention;

[0031] Figure 9 This is a schematic diagram of the structure of the processing unit provided in an embodiment of the present invention;

[0032] The explanations of the reference numerals in the accompanying drawings are as follows:

[0033] 1-Wafer; 2-Stage;

[0034] 3-Processing unit; 31-Drive sub-unit; 32-Spraying sub-unit; 33-Reaction chamber. Detailed Implementation

[0035] To make the objectives, advantages, and features of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to facilitate and clarify the explanation of the embodiments of this invention. Furthermore, the structures shown in the drawings are often part of the actual structures. In particular, different figures may emphasize different aspects and may sometimes use different scales.

[0036] As used herein, the singular forms “a,” “an,” and “the” include plural objects; the term “or” is generally used to mean “and / or”; the term “a number” is generally used to mean “at least one”; and the term “at least two” is generally used to mean “two or more”. Furthermore, the terms “first,” “second,” and “third” are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as “first,” “second,” or “third” may explicitly or implicitly include one or at least two of that feature. “One end” and “the other end,” as well as “proximal end” and “distal end,” generally refer to two corresponding parts, including not only endpoints. The terms “installed,” “connected,” and “joined” should be interpreted broadly; for example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two elements or the interaction between two elements. Furthermore, as used in this specification, the phrase "one element is disposed on another element" generally only indicates that there is a connection, coupling, cooperation, or transmission relationship between the two elements, and the connection, coupling, cooperation, or transmission between the two elements can be direct or indirect through an intermediate element. It should not be construed as indicating or implying a spatial positional relationship between the two elements, i.e., one element can be located arbitrarily inside, outside, above, below, or to the side of another element, unless otherwise explicitly stated. The terms "above," "below," "top," and "bottom" generally refer to relative positional relationships arranged according to the direction of gravity; the terms "vertical" or "vertical direction" generally refer to the direction of gravity, which is generally perpendicular to the ground; "horizontal" or "horizontal plane direction" generally refers to a direction parallel to the ground. Those skilled in the art can understand the specific meaning of the above terms in this specification according to the specific circumstances.

[0037] The purpose of this invention is to provide a method and semiconductor manufacturing equipment for improving overlay accuracy, so as to solve the problem that the large friction between the wafer and the stage affects the overlay accuracy.

[0038] The following explanation is based on the accompanying drawings.

[0039] Please refer to Figures 1 to 6 As those skilled in the art will understand, the friction between wafer 1 and stage 2 affects the overlay accuracy of the product. The main factors affecting friction are the surface free energy and surface roughness of the contact surface (usually the back of the wafer), and the following relationship exists among the three: F f =τ eff *A r , of which F f For friction, τ eff For surface free energy, Ar For surface roughness; it should be noted that although the frictional force in the above formula is directly proportional to both surface free energy and surface roughness, it does not mean that reducing either one will necessarily reduce the frictional force, because frictional force is also affected by other factors, such as van der Waals forces. Generally speaking, the greater the frictional force, the worse the overlay accuracy of wafer 1. To reduce the frictional force between wafer 1 and stage 2, it can be achieved by changing the surface roughness or reducing the surface free energy. Changing the surface roughness can be achieved by adjusting the surface roughness of stage 2. Figures 1 to 6 In the illustrated example, in actual production, both the stage 2 and the wafer 1 are disk-shaped components (such as...). Figure 1 As shown), wafer 1 is vacuum-adsorbed onto stage 2 (as shown). Figure 2 As shown), the operator will periodically use diamond-like materials to polish the joints on the platform 2, removing them from their worn state due to long-term use (such as...). Figure 4 As shown) it becomes rough again (as shown) Figure 3 As shown), long-term observation shows that the overlay accuracy of wafer 1 when stage 2 is in a rough state (as shown) Figure 5 (As shown) is superior to the overlay accuracy of stage 2 when it is in a worn state (e.g.) Figure 6 (As shown). Although polishing the stage 2 increases surface roughness, the corresponding friction tends to decrease due to the influence of van der Waals forces. However, regularly maintaining the surface roughness of the stage 2 would result in a waste of manpower and resources. Therefore, this application adopts the method of reducing the surface free energy of the crystal back to reduce friction. By modifying the hydrophilicity of the crystal back surface to hydrophobicity, the surface free energy of the crystal back is reduced, thereby reducing the friction between the wafer 1 and the stage 2.

[0040] Please refer to Figure 7 The present invention provides a method for improving overlay accuracy, comprising:

[0041] Step S1: After the photoresist coating is completed, the back side of wafer 1 is modified to change the back side of wafer 1 from hydrophilic to hydrophobic.

[0042] It should be noted that in existing semiconductor manufacturing processes, the photoresist spin coating process is usually followed directly by the exposure process. This application, however, modifies the back side of wafer 1 between the photoresist spin coating and exposure processes, thereby reducing the surface free energy of the back side of wafer 1 and further improving the overlay accuracy of the exposure process. The back side of wafer 1 is generally made of silicon or silicon-containing materials, which easily absorbs moisture from the air, making the surface hydrophilic. Common modification processes include plasma modification and chemical modification. Plasma modification uses gas plasma to modify the surface of wafer 1; for example, oxygen plasma can make the surface of wafer 1 hydrophilic, while hydrogen plasma can make the surface of wafer 1 hydrophobic. Chemical modification uses chemical reagents to treat the surface of wafer 1. Commonly used surfactants can be adsorbed onto the surface of wafer 1 to form hydrophobic or hydrophilic groups. The hydrophobicity of the surface of wafer 1 can be increased by using surfactants containing non-polar hydrophobic tail groups, and the hydrophilicity can be increased by using surfactants containing polar hydrophilic head groups. Those skilled in the art can select appropriate modification treatment schemes according to actual conditions, and this embodiment is not limited to this.

[0043] With this configuration, this embodiment modifies the back side of the wafer 1 after photoresist spraying, changing it from hydrophilic to hydrophobic. This reduces the surface free energy of the back side of the wafer 1, resulting in reduced surface tension, increased contact angle, reduced intermolecular forces at the interface, and reduced polarity. Consequently, it reduces the friction between the back side of the wafer 1 and the stage 2, thereby improving the overlay accuracy of the exposure machine.

[0044] For further details, please refer to... Figure 8 The back side of wafer 1 is modified, including:

[0045] Step S1-1: Spray modifier onto the back side of wafer 1;

[0046] Step S1-2: Dry the back side of wafer 1.

[0047] It should be noted that the modification process in this embodiment is achieved through chemical modification, specifically by forming a hydrophobic group on the back side of wafer 1, thus changing the back side of wafer 1 from hydrophilic to hydrophobic. The modifier is a silazane-based reagent, specifically hexamethyldisilazane. Gaseous and / or liquid modifiers can be used; specifically, in this embodiment, it can be hexamethyldisilazane gas, hexamethyldisilazane solvent, or a mixture of both. The modifier is sprayed onto the back side of wafer 1 using a spin-coating method, i.e., a drive unit (which can be a rotary motor, see reference for details). Figure 9 The drive subunit 31 in the middle drives the wafer 1 to rotate while the spraying part (which can be the nozzle of the pipeline, see reference for details) is sprayed. Figure 9The spraying subunit 32) sprays a modifier onto the back side of wafer 1. The modifier can be sprayed only onto a local area of ​​the back side of wafer 1 (which may be an area with a high moisture content) or onto the entire back side of wafer 1. After the spraying unit completes the spraying of the modifier, the wafer 1 can be driven to rotate by the drive unit to spin off the excess modifier, thus completing the drying process. In some embodiments, drying can also be performed by baking, but considering the influence of temperature changes on the photoresist, spin drying is preferable.

[0048] In another embodiment, please refer to Figure 9 The present invention also provides a semiconductor manufacturing apparatus for implementing the method for improving overlay accuracy as described above, comprising: a transfer unit (not shown in the figure), a processing unit 3, and a task unit (not shown in the figure); the task unit includes a photoresist coating subunit (not shown in the figure) and an exposure subunit (not shown in the figure), the transfer unit being sequentially connected to the photoresist coating subunit, the processing unit 3, and the exposure subunit, the transfer unit being used to load wafer 1 and enabling wafer 1 to flow between the photoresist coating subunit, the processing unit 3, and the exposure subunit; the processing unit 3 being used to modify the back side of wafer 1, so that the back side of wafer 1 is modified from hydrophilic to hydrophobic. Those skilled in the art will understand that semiconductor manufacturing processes have multiple steps, each processed by different equipment. For example, the photoresist coating subunit is used to perform photoresist spin coating on wafer 1, which can be completed by a photoresist coating unit in the semiconductor manufacturing apparatus or by a separate photoresist coating machine; the exposure subunit can be a separate exposure machine; the transfer unit can be a component capable of carrying wafer 1, such as a robotic arm or a conveyor belt. Those skilled in the art can configure the transfer unit, coating sub-unit, and exposure sub-unit reasonably according to the actual situation, and this embodiment is not limited in this respect.

[0049] Furthermore, the processing unit 3 includes a driving subunit 31 and a spraying subunit 32; the spraying subunit 32 is used to spray a modifier onto the back side of the wafer 1; the transfer unit can transfer the wafer 1 to the driving subunit 31, and the driving subunit 31 can rotate around an axis to drive the wafer 1 to rotate while the spraying subunit 32 is spraying. It should be noted that... Figure 9 For example, the driving subunit 31 can be a rotary motor, which can drive the wafer 1 to rotate during the spraying process of the spraying subunit 32, so as to achieve all-round modification treatment of the back side of the wafer 1; the spraying subunit 32 can be a delivery pipeline and a nozzle, which transports the modifier (in this embodiment, it is a silazane reagent, specifically hexamethyldisilazane) through the delivery pipeline and sprays the modifier through the nozzle.

[0050] As an optional embodiment, the processing unit 3 further includes a reaction chamber 33, with both the driving subunit 31 and the spraying subunit 32 disposed within the reaction chamber 33. The spraying subunit 32 is used to spray gaseous modifiers and / or liquid modifiers onto the back side of the wafer 1. Figure 9 In the illustrated example, the reaction chamber 33 is a semi-closed cavity with an opening at one end. The reaction chamber 33 is suitable for spraying a liquid modifier in the spraying sub-unit 32. If the spraying sub-unit 32 needs to spray a gaseous modifier or a mixture of gaseous and liquid modifiers, then the reaction chamber 33 needs to be a closed cavity so that the gaseous modifier can function without overflowing from the opening of the reaction chamber 33.

[0051] In another alternative embodiment, after the spraying subunit 32 completes the spraying on the back side of wafer 1, the driving subunit 31 drives wafer 1 to rotate, thereby achieving the drying process of wafer 1. It should be noted that the driving subunit 31 also serves to remove excess modifier; that is, the driving subunit 31 remains rotating during the spraying process of the spraying subunit 32, achieving rotary spraying. After the spraying subunit 32 completes its spraying, the driving subunit 31 continues to rotate to remove excess modifier, thus not affecting subsequent processes.

[0052] In summary, in the method and semiconductor manufacturing equipment for improving overlay accuracy provided in the embodiments of the present invention, the method for improving overlay accuracy includes: after completing the photoresist spraying, modifying the back side of the wafer to change it from hydrophilic to hydrophobic.

[0053] This configuration modifies the back side of the wafer after photoresist coating, changing it from hydrophilic to hydrophobic. This reduces the surface free energy of the back side of the wafer, resulting in decreased surface tension, increased contact angle, reduced intermolecular forces at the interface, and decreased polarity. Consequently, it reduces the friction between the back side of the wafer and the stage, improving the overlay accuracy of the exposure machine.

[0054] The above description is merely a description of preferred embodiments of the present invention and is not intended to limit the scope of the present invention in any way. Any changes or modifications made by those skilled in the art based on the above disclosure shall fall within the protection scope of the claims.

Claims

1. A method for improving overlay accuracy, characterized in that, include: After the photoresist coating is completed, the back side of the wafer is modified to change it from hydrophilic to hydrophobic. The modification treatment of the back side of the wafer includes: A modifier is sprayed onto the back side of the wafer; The back side of the wafer is dried. The modifier is applied to a partial or complete area of ​​the back side of the wafer using a rotary spraying method.

2. The method for improving overlay accuracy as described in claim 1, characterized in that, The modifiers include silazane-based reagents.

3. The method for improving overlay accuracy as described in claim 1, characterized in that, The modifier includes gaseous modifiers and / or liquid modifiers.

4. The method for improving overlay accuracy as described in claim 1, characterized in that, The back side of the wafer is dried by spin drying.

5. A semiconductor manufacturing apparatus for implementing the method for improving overlay accuracy as described in any one of claims 1 to 4, characterized in that, include: Transfer unit, processing unit, and task unit; The task unit includes a coating subunit and an exposure subunit. The transfer unit is connected in sequence to the coating subunit, the processing unit and the exposure subunit. The transfer unit is used to load the wafer and enables the wafer to flow between the coating subunit, the processing unit and the exposure subunit. The processing unit is used to modify the back side of the wafer to change it from hydrophilic to hydrophobic.

6. The semiconductor manufacturing equipment as described in claim 5, characterized in that, The processing unit includes a driving subunit and a spraying subunit; The spraying subunit is used to spray a modifier onto the back side of the wafer; The transfer unit can transfer the wafer to the driving subunit, and the driving subunit can rotate around an axis to drive the wafer to rotate when the spraying subunit is spraying.

7. The semiconductor manufacturing equipment as described in claim 6, characterized in that, The processing unit further includes a reaction chamber, and the driving subunit and the spraying subunit are both disposed in the reaction chamber. The spraying subunit is used to spray gaseous modifier and / or liquid modifier onto the back side of the wafer.

8. The semiconductor manufacturing equipment as described in claim 6, characterized in that, After the spraying subunit completes the spraying on the back side of the wafer, the driving subunit drives the wafer to rotate, thereby achieving the drying process of the wafer.

Citation Information

Patent Citations

  • Method of forming resist pattern and semiconductor device manufactured with the same

    US20080241489A1

  • Substrate, a substrate holder, a substrate coating apparatus, a method for coating the substrate and a method for removing the coating

    US20210223696A1