A method for manufacturing an iron-based soft magnetic powder core

By forming an insulating coating film on the surface of FeSiAl matrix powder and performing high-temperature annealing, a fully encapsulated iron-based soft magnetic powder core was prepared, solving the problems of magnetic leakage and device interference in inductors. This resulted in a miniaturized and low-loss soft magnetic powder core suitable for multiple fields.

CN118073041BActive Publication Date: 2024-11-15SHANDONG HENGRUI MAGNET TECH CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410301877.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-03-17
Publication Date
2024-11-15
Estimated Expiration
2044-03-17

AI Technical Summary

Technical Problem

Existing inductors suffer from magnetic leakage and mutual interference between components, making it difficult to meet the demands for miniaturization, high frequency, and high integration of electronic devices.

Method used

A method for manufacturing iron-based soft magnetic powder cores is adopted. By forming a uniform insulating coating film on the surface of FeSiAl matrix powder and combining it with high-temperature annealing treatment, a fully encapsulated soft magnetic powder core is prepared to avoid magnetic leakage and device interference.

Benefits of technology

It achieves a soft magnetic powder core with no magnetic leakage and no device interference, and features miniaturization, low loss and high shielding performance, making it suitable for applications in multiple fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118073041B_ABST
    Figure CN118073041B_ABST
Patent Text Reader

Abstract

The present application discloses a method for manufacturing an iron-based soft magnetic powder core, which belongs to the field of soft magnetic powder cores for inductors. The method comprises the following steps: Step 1: Select an appropriate amount of FeSiAl matrix powder; Step 2: Mix the FeSiAl matrix powder with a coating solution, and put it into a coating solution mixing device for mixing, so as to form a uniform insulating coating film on the surface of the FeSiAl matrix powder; Step 3: Add a lubricant to the product of step 2 and mix it thoroughly; Step 4: Press the product of step 3 by a molding machine; Step 5: Put the pressed product in step 4 into an annealing device for high-temperature annealing heat treatment. The present application has the advantages of a fully enclosed structure, no magnetic leakage, and no mutual interference between devices. At the same time, the present application also has the advantages of small size, low loss, excellent shielding performance, high reliability, and suitable for high-density surface mounting such as mobile phones.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of soft magnetic powder cores for inductors, and in particular to a method for manufacturing an iron-based soft magnetic powder core. Background Art

[0002] As high-speed, high-capacity 5G communication technology and third-generation semiconductor technologies such as GaN gradually become practical, electronic devices are accelerating towards miniaturization, high frequency, high integration, multi-function, and wearability. This also puts forward new requirements for electronic information materials. As soft magnetic materials and devices that are indispensable in the processes of electromagnetic transformation, transmission, and information emission, transmission, reception, processing, and recording, they face huge challenges of high frequency and low power consumption, and have become a key factor restricting the development of the next generation of electronic devices. Electronic terminal products are constantly developing in the direction of "miniaturization, integration, multi-function, and high power". Traditional plug-in inductors can no longer meet the needs of downstream electronic equipment, and new types of power inductors need to be developed.

[0003] The chip inductors currently produced by inductors have the characteristics of a wide inductance range, high inductance accuracy, low loss, large allowable current, strong and simple manufacturing process inheritance, and excellent anti-saturation characteristics, but they are relatively expensive and have problems with magnetic leakage and mutual interference between devices. Summary of the invention

[0004] The present invention solves the problems of magnetic leakage and mutual interference between devices in the prior art. To this end, the present invention proposes a method for manufacturing an iron-based soft magnetic powder core, which has the characteristics of a full-enclosed structure, no magnetic leakage, and no mutual interference between devices.

[0005] To achieve the above object, the present application provides a method for manufacturing an iron-based soft magnetic powder core, comprising the following steps:

[0006] Step 1: Select an appropriate amount of FeSiAl matrix powder;

[0007] Step 2: putting the FeSiAl matrix powder and the coating solution into a coating solution mixing device for mixing, so as to form a uniform insulating coating film on the surface of the FeSiAl matrix powder;

[0008] Step 3: Add lubricant to the product of step 2 and mix thoroughly;

[0009] Step 4, pressing the product of step 3 into shape by a molding machine;

[0010] Step 5: placing the product pressed in step 4 into an annealing device for high temperature annealing heat treatment;

[0011] Step 6: The finished product after annealing in step 5 is subjected to performance testing using an electron microscope.

[0012] Preferably, the coating solution is a nitric acid ethanol passivation solution prepared from anhydrous ethanol and concentrated nitric acid.

[0013] Preferably, after forming the insulating coating film in step 2, a binder needs to be added and coated on the surface of the nitrated FeSiAl matrix powder, and the binder is sodium silicate.

[0014] Preferably, the coating solution mixing device in step 2 comprises:

[0015] A mixing bin, wherein a rotating motor is installed on the side of the mixing bin, a heater is installed at the front end of the mixing bin, and a bin door that is controlled to move by an electric telescopic rod is installed at the bottom discharge port of the mixing bin;

[0016] A mixing assembly mounted on the output shaft of a rotating motor, the mixing assembly includes a rotating rod mounted on the output shaft of the rotating motor, a stirring blade is fixed on the outside of the rotating rod, a shovel is slidably connected to the piston in the internal sealing movable groove of the stirring blade, a hollow airbag connected to the sealing movable groove is fixed on the side of the stirring blade, a hollow block is fixed in the middle of the rotating rod, and two annular pressure plates for squeezing the hollow airbag are installed inside the hollow block through multiple linkage components. When the rotating motor controls the mixing assembly to rotate clockwise, the mixing assembly only has a mixing effect. When the mixing is completed and the material is discharged, the rotating motor controls the mixing assembly to rotate counterclockwise, and the shovel in the stirring blade will extend to scrape off the material attached to the inner wall of the mixing bin and discharge it through the discharge port.

[0017] Preferably, the linkage assembly includes a three-way hydraulic chamber, wherein the two ports of the three-way hydraulic chamber are both piston-slidingly connected with a push rod, the other end port of the three-way hydraulic chamber is connected and fixed with a liquid storage capsule, a hollow track rod is fixed on the outer side of the three-way hydraulic chamber close to the liquid storage capsule, and a cylindrical metal rod is movably connected inside the hollow track rod. When the mixing assembly rotates counterclockwise, the cylindrical metal rod squeezes the liquid storage capsule, and the annular pressure plate is pushed out through the two push rods of the three-way hydraulic chamber, so as to trigger the hollow airbag on the stirring blade.

[0018] Preferably, a cavity is provided inside the shovel plate, a plurality of through holes communicating with the cavity are provided on the front inclined surface of the shovel plate, a baffle is rotatably connected to the side of the cavity of the shovel plate, and a hemisphere is fixed to the side of the baffle. When the shovel plate rotates counterclockwise, the scraped material will enter the cavity through the through hole and then flow to the discharge port of the mixing bin, which is convenient for collecting the material.

[0019] Preferably, a two-way hydraulic bin is embedded at the bottom of the mixing bin, a pressure rod is slidably connected to one end of the two-way hydraulic bin, a hydraulic rod is slidably connected to the other end of the two-way hydraulic bin, and a transverse pressure rod is rotatably connected to the top of the hydraulic rod via a torsion spring shaft. When the transverse pressure rod is pushed upward, the hemispherical shape of the side of the lower shovel plate will be squeezed during rotation, causing the baffle to flip, thereby improving the discharge accuracy of the material in the shovel plate cavity.

[0020] Preferably, the upper end of the interior of the mixing bin is equipped with a filtering device, the filtering device includes a feed pipe, the interior of the feed pipe is slidably connected with an arched filter screen, the two sides of the arched filter screen are respectively connected to the inner wall of the feed pipe through an accordion cover, an arc block is fixed on the side of the arched filter screen, a spring is fixed between the arc block and the feed pipe, the left side of the feed pipe is rotatably connected to a first bevel gear rod through a bracket block, a squeezing ball is fixed on the first bevel gear rod, the side of the feed pipe is rotatably connected to a second bevel gear rod, and the second bevel gear rod is connected to the output shaft of the rotating motor through a transmission belt. Before the coating solution and the FeSiAl matrix powder are put into the mixing bin, they will be filtered by the arched filter screen to prevent the agglomerated FeSiAl matrix powder from entering.

[0021] Preferably, the second bevel gear rod is vertically meshed with the first bevel gear rod, and the arc block is located on the movement path of the extrusion ball.

[0022] The benefits of this application are:

[0023] (1) The present application has the advantages of a fully enclosed structure, no magnetic leakage, and no mutual interference between devices. At the same time, the present application also has the advantages of small size, low loss, excellent shielding performance, high reliability, and is suitable for high-density surface mounting such as mobile phones. It has broad application prospects in 5G communications, computers, consumer electronics, digital products, automotive electronics, artificial intelligence, industrial control, aerospace and other fields.

[0024] (2) The present application mixes the coating solution with the FeSiAl matrix powder by setting up a coating solution mixing device. After the mixing is completed, the mixing component is controlled by a rotary motor to rotate in the opposite direction, which can not only accelerate the discharge of materials, but also hang down the materials attached to the inner wall of the mixing bin, thereby improving the recovery efficiency of the materials.

[0025] (3) In the present application, a filtering device is provided so that the coating solution and the FeSiAl matrix powder are filtered by an arched filter before being added to the mixing bin to prevent the agglomerated FeSiAl matrix powder from entering. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The drawings constituting a part of this application are used to provide a further understanding of this application, so that other features, purposes and advantages of this application become more obvious. The schematic embodiment drawings and their descriptions of this application are used to explain this application and do not constitute an improper limitation on this application. In the drawings:

[0027] Figure 1 It is a schematic structural diagram of the coating solution mixing device of the present invention.

[0028] Figure 2 It is a schematic diagram of the structure of the coating solution mixing device of the present invention when viewed from above.

[0029] Figure 3 It is a schematic cross-sectional structural diagram of the coating solution mixing device of the present invention.

[0030] Figure 4 It is a schematic diagram of the structure of the mixing assembly of the present invention.

[0031] Figure 5 It is a schematic diagram of the cross-sectional structure of the stirring blade of the present invention.

[0032] Figure 6 It is a partial structural schematic diagram of the mixing assembly of the present invention.

[0033] Figure 7 It is a structural schematic diagram of the linkage assembly of the present invention.

[0034] Figure 8 It is a partial structural schematic diagram of the coating solution mixing device of the present invention.

[0035] Fig. 9 It is a structural schematic diagram of the shovel plate of the present invention.

[0036] Fig.10 It is a schematic diagram of the connection structure at the discharge port of the mixing bin of the present invention.

[0037] Fig.11 It is a schematic structural diagram of the filtering device of the present invention.

[0038] Fig.12 It is a schematic cross-sectional view of the filter device of the present invention.

[0039] In the above figure,

[0040] 100, mixing bin; 200, rotating motor; 300, heater; 400, electric telescopic rod; 500, bin door; 600, mixing assembly; 610, rotary rod; 620, stirring blade; 630, sealing movable groove; 640, shovel plate; 641, through hole; 642, cavity; 643, baffle; 644, hemisphere; 645, two-way hydraulic bin; 646, pressure rod; 647, hydraulic rod; 648, transverse pressure rod; 650, Hollow airbag; 660, hollow block; 670, annular pressure plate; 680, three-way hydraulic chamber; 690, push rod; 6100, liquid storage capsule body; 6110, hollow track rod; 6120, cylindrical metal rod; 700, feed pipe; 710, arched filter; 720, bracket block; 730, first bevel gear rod; 740, squeeze ball; 750, second bevel gear rod; 760, transmission belt; 770, arc block; 780, accordion cover. DETAILED DESCRIPTION

[0041] In order to enable those skilled in the art to better understand the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only embodiments of a part of the present application, not all embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work should fall within the scope of protection of the present application.

[0042] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application are described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, the process, method, system, product or equipment comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or equipment.

[0043] In the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "middle", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.

[0044] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.

[0045] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0046] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments. Example

[0047] This embodiment provides a method for manufacturing an iron-based soft magnetic powder core, comprising the following steps:

[0048] Step 1: Select an appropriate amount of FeSiAl matrix powder;

[0049] Step 2: Place the FeSiAl matrix powder and the coating solution into a coating solution mixing device for mixing, and form a uniform insulating coating film on the surface of the FeSiAl matrix powder. The coating solution is a nitric acid ethanol passivation solution composed of anhydrous ethanol and concentrated nitric acid. After the insulating coating film is formed on the surface of the FeSiAl matrix powder, since the FeSiAl matrix powder used in this application is a spherical iron silicon aluminum magnetic powder, it is difficult to form and is fragile during the pressing process, and it is easy to crack during the demolding process. Therefore, sodium silicate is used as a binder and coated on the surface of the iron silicon aluminum magnetic powder after nitration, which can improve the molding performance of the magnetic powder. In addition, sodium silicate is an insulating medium and can also increase the insulation between magnetic powder particles;

[0050] Step 3: Add lubricant to the product of step 2 and mix thoroughly. (During the pressing process, there is a large friction between the magnetic powder and the press mold, and the friction will increase with the increase of the pressing pressure, which will cause great damage to the mold. Therefore, in order to reduce the friction between the magnetic powder and the press mold and extend the service life of the mold, it is necessary to add an appropriate amount of lubricant to the magnetic powder before pressing);

[0051] Step 4: weigh 1 g of FeSiAl magnetic powder completely mixed with lubricant, pour it into a mold, pre-press it with a pressure of 60 kN for 30 seconds to remove the air between the particles, and then maintain the pressure at a pressure of 100 kN for 1 minute to press it into a ring-shaped soft magnetic composite material with an inner diameter of 5.5 mm, an outer diameter of 9.7 mm, and a thickness of 3.3 mm;

[0052] Step 5: Place the product pressed in step 4 into a vacuum tube furnace, introduce nitrogen as a protective atmosphere, heat up at a rate of 2°C / min, keep at 400°C for 1 hour, then continue to heat up to 770°C at a rate of 5°C / min, keep at 770°C for 3 hours, and cool to room temperature with the furnace after the heat preservation ends;

[0053] Step 6: The finished product after annealing in step 5 is subjected to performance testing using an electron microscope.

[0054] The FeSiAl matrix powder used in this application is aerosolized FeSiAl magnetic powder made in the laboratory.

[0055] The iron-based soft magnetic powder core manufactured by the above steps first forms a uniform insulating coating film on the surface of the FeSiAl matrix powder, which effectively increases the resistance of the magnetic powder surface to block the eddy current between the magnetic powder particles and reduce the eddy current loss. However, the insulating medium generated on the surface of the magnetic powder particles is often a non-magnetic phase. If the coating film is too thick, the magnetic properties of the magnetic powder core will decrease. Therefore, the insulating coating layer on the surface of the magnetic powder is required to be thin and uniform. In addition, after the metal magnetic powder is insulated and coated, it needs to be pressed and annealed at high temperature. Therefore, it is required that the coating layer has a strong bonding force with the magnetic powder matrix, will not break and fall off during the pressing process, and the coating layer has good thermal stability and will not decompose in the final annealing process.

[0056] See also Figure 1-Figure 12 The coating solution mixing device in step 2 includes a mixing chamber 100, a rotating motor 200 is installed on the side of the mixing chamber 100, a heater 300 is installed at the front end of the mixing chamber 100, and a chamber door 500 controlled to move by an electric telescopic rod 400 is installed at the bottom discharge port of the mixing chamber 100;

[0057] A mixing assembly 600 is mounted on the output shaft of a rotating motor 200. The mixing assembly 600 includes a rotating rod 610 mounted on the output shaft of the rotating motor 200. A stirring blade 620 is fixed on the outer side of the rotating rod 610. A total of six stirring blades 620 are provided, and each of the three stirring blades 620 is symmetrically fixed on the outer side of the rotating rod 610 in a circular array. A sealing movable groove 630 is provided inside each stirring blade 620, and a shovel plate 640 is connected to the inside of each sealing movable groove 630 by a piston sliding. A hollow air bag 650 connected to the sealing movable groove 630 is fixed on the side of each stirring blade 620. When the hollow air bag 650 is squeezed, the gas inside it will enter the sealing movable groove 630. Under the pressure of the gas When it becomes larger, the shovel plate 640 is pushed out, and a hollow block 660 is fixed in the middle of the rotating rod 610. The interior of the hollow block 660 is equipped with two annular pressure plates 670 for squeezing the hollow airbag 650 through multiple linkage components. The linkage component includes a three-way hydraulic warehouse 680, and the two ports of the three-way hydraulic warehouse 680 are both piston-slidingly connected with a push rod 690. The other end port of the three-way hydraulic warehouse 680 is connected and fixed with a liquid storage bag body 6100. A hollow track rod 6110 is fixed on the outer side of the three-way hydraulic warehouse 680 close to the liquid storage bag body 6100. The interior of the hollow track rod 6110 is movably connected with a cylindrical metal rod 6120. When the rotating motor 200 controls the mixing assembly 600 to rotate clockwise When the mixing assembly 600 is in motion, the mixing component 600 only has a mixing effect. When the mixing is completed and the material is discharged, the mixing component 600 is controlled to rotate counterclockwise by the rotating motor 200. When the mixing component 600 rotates counterclockwise, the cylindrical metal rod 6120 will squeeze the liquid storage capsule 6100, and the two ejector rods 690 of the three-way hydraulic chamber 680 will push out the annular pressure plate 670, so that it triggers the hollow airbag 650 on the stirring blade 620. At this time, the shovel plate 640 in the stirring blade 620 will extend to scrape off the material attached to the inner wall of the mixing chamber 100 and discharge it with the discharge port. The shovel plate 640 is provided with a cavity 642 inside, and a plurality of through holes 641 connected to the cavity 642 are provided on the front end inclined surface of the shovel plate 640. When the mixing component 600 rotates counterclockwise, the cylindrical metal rod 6120 will squeeze the liquid storage capsule 6100, and the two ejector rods 690 of the three-way hydraulic chamber 680 will push out the annular pressure plate 670, so that it triggers the hollow airbag 650 on the stirring blade 620. At this time, the shovel plate 640 in the stirring blade 620 will extend to scrape off the material attached to the inner wall of the mixing chamber 100 and discharge it with the discharge port. When rotating, the shovel plate 640 is in contact with the mixing bin 100 and scrapes the materials on the inner wall of the mixing bin 100. As the shovel plate 640 scrapes, the materials attached to the inner wall of the mixing bin 100 will enter the cavity 642 through the through hole 641. Since the lateral opening of the cavity 642 is close to the discharge port of the mixing bin 100, the materials collected in the cavity 642 will flow toward the discharge port of the mixing bin 100, which is convenient for collecting the materials attached to the inner wall of the mixing bin 100. The side of the cavity 642 of the shovel plate 640 is rotatably connected with a baffle plate 643, and a hemisphere 644 is fixed to the side of the baffle plate 643. A two-way hydraulic bin 645 is embedded in the bottom of the mixing bin 100, and a pressure rod 646 is slidably connected to one end of the inner side of the two-way hydraulic bin 645.The other end of the two-way hydraulic chamber 645 is slidably connected to a hydraulic rod 647, and the top of the hydraulic rod 647 is rotatably connected to a transverse pressure rod 648 through a torsion spring shaft. When the mixing chamber 100 is discharging materials, the electric telescopic rod 400 is first used to control the sliding of the chamber door 500 to open the discharging port of the mixing chamber 100. At the same time, as the chamber door 500 moves, the pressure rod 646 is squeezed to move. At this time, since the pressure rod 646 is squeezed into the two-way hydraulic chamber 645, the hydraulic rod 647 drives the transverse pressure rod 648 to rise, so that the transverse pressure rod 648 is located on the motion trajectory of the hemisphere 644, which is used to trigger the rotation of the baffle 643.

[0058] When the coating solution mixing device is used, the coating solution and the FeSiAl matrix powder are first put into the mixing bin 100, and then the rotating motor 200 is turned on to control the mixing assembly 600 to rotate clockwise. At this time, the mixing assembly 600 only has a mixing effect. After mixing for a period of time, when the bin door 500 needs to be opened for discharge, first, the bin door 500 is controlled to slide by the electric telescopic rod 400 to open the discharge port of the mixing bin 100. At the same time, as the bin door 500 is opened, the mixing bin 100 is opened. 0, will squeeze the pressure rod 646 to move. At this time, since the pressure rod 646 is squeezed into the two-way hydraulic chamber 645, the hydraulic rod 647 will drive the lateral pressure rod 648 to rise, so that the lateral pressure rod 648 is located on the movement trajectory of the hemisphere 644. At this time, the discharge of the material has begun. Then, the mixing component 600 is controlled to rotate counterclockwise by the rotating motor 200. When the mixing component 600 rotates counterclockwise, under the action of inertia, the cylindrical metal rod 6120 will squeeze the liquid storage capsule 6100, and the material will be discharged. The two push rods 690 of the three-way hydraulic chamber 680 push out the annular pressure plate 670, so that it triggers the hollow airbag 650 on the mixing blade 620. At this time, the shovel plate 640 in the mixing blade 620 will extend to scrape off the material attached to the inner wall of the mixing chamber 100 and discharge it through the discharge port. At the same time, when the shovel plate 640 is attached to the mixing chamber 100, the material on the inner wall of the mixing chamber 100 is scraped. As the shovel plate 640 scrapes, the material attached to the inner wall of the mixing chamber 100 enters through the through hole 641. In the cavity 642, since the lateral opening of the cavity 642 is close to the discharge port of the mixing bin 100, the material collected in the cavity 642 will flow toward the discharge port of the mixing bin 100, which is convenient for collecting the material attached to the inner wall of the mixing bin 100. At the same time, since the lateral pressure rod 648 is located on the movement trajectory of the hemisphere 644, whenever the stirring blade 620 moves to this point, the lateral pressure rod 648 will squeeze the hemisphere 644, causing the baffle 643 to swing, thereby increasing the discharge of the material in the cavity 642 of the shovel plate 640.

[0059] It is worth noting that in order to prevent debris or agglomerated FeSiAl matrix powder from entering the mixing bin 100, a filtering device is installed at the upper end of the mixing bin 100, and the filtering device includes a feed pipe 700, and an arched filter screen 710 is slidably connected to the inside of the feed pipe 700. The two sides of the arched filter screen 710 are respectively connected to the inner wall of the feed pipe 700 through an accordion cover 780, and an arc block 770 is fixed to the side of the arched filter screen 710. The arc block 770 is connected to the feed pipe 700. 0, a spring piece is fixed between the left side of the feed pipe 700, the first bevel gear rod 730 is rotatably connected to the left side of the feed pipe 700 through the bracket block 720, a squeezing ball 740 is fixed on the first bevel gear rod 730, the side of the feed pipe 700 is rotatably connected to the second bevel gear rod 750, the second bevel gear rod 750 is connected to the output shaft of the rotating motor 200 through a transmission belt 760, the second bevel gear rod 750 is vertically meshed with the first bevel gear rod 730, and the arc block 770 is located on the movement path of the squeezing ball 740.

[0060] When the above-mentioned filtering device is actually used, before the coating solution and the FeSiAl matrix powder are put into the mixing bin 100, they will first be filtered by the arched filter screen 710 to filter and separate the impurities or agglomerated FeSiAl matrix powder. At the same time, since the output shaft of the rotating motor 200 is connected to the second bevel gear rod 750 through the transmission belt 760, the second bevel gear rod 750 is driven to rotate by the output shaft of the rotating motor 200 under the action of the transmission belt 760, and then the first bevel gear rod 730 vertically meshed with the second bevel gear rod 750 follows the rotation. At this time, the first bevel gear rod 730 is rotated. The squeezing ball 740 on the outside of the wheel rod 730 will intermittently squeeze the arc block 770. Since the arc block 770 is connected to the arch filter 710 and there is a spring between the arc block 770 and the feed pipe 700, the arc block 770 will continuously move left and right in a circular motion under the intermittent squeezing state of the squeezing ball 740, thereby driving the arch filter 710 to move left and right in a circular motion. Through the left and right circular motion of the arch filter 710, the debris or agglomerated FeSiAl matrix powder filtered out from the middle of the arch filter 710 will be shaken to the edge area to ensure the filtering effect of the arch filter 710.

[0061] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A method for manufacturing an iron-based soft magnetic powder core, characterized in that: The following steps are involved: Step 1: Select an appropriate amount of FeSiAl matrix powder; Step 2: putting the FeSiAl matrix powder and the coating solution into a coating solution mixing device for mixing, so as to form a uniform insulating coating film on the surface of the FeSiAl matrix powder; Step 3: Add lubricant to the product of step 2 and mix thoroughly; Step 4, pressing the product of step 3 into shape by a molding machine; Step 5: placing the product pressed in step 4 into an annealing device for high temperature annealing heat treatment; Step 6: Performing a performance test on the finished product after annealing in step 5 through an electron microscope; The coating solution in step 2 is a nitric acid ethanol passivation solution prepared from anhydrous ethanol and concentrated nitric acid; After forming the insulating coating film in step 2, a binder needs to be added and coated on the surface of the nitrated FeSiAl matrix powder, and the binder is sodium silicate; The coating solution mixing device in step 2 comprises: A mixing bin (100), wherein a rotating motor (200) is mounted on a side of the mixing bin (100), a heater (300) is mounted on a front end of the mixing bin (100), and a bin door (500) is mounted at a bottom discharge port of the mixing bin (100) and is controlled to move by an electric telescopic rod (400); A mixing assembly (600) mounted on an output shaft of a rotating motor (200), the mixing assembly (600) comprising a rotating rod (610) mounted on the output shaft of the rotating motor (200), a stirring blade (620) being fixed on the outer side of the rotating rod (610), a shovel plate (640) being slidably connected to a piston in a sealed movable groove (630) inside the stirring blade (620), a hollow airbag (650) being fixed on the side of the stirring blade (620) and being connected to the sealed movable groove (630), a hollow block (660) being fixed in the middle of the rotating rod (610), and two annular pressing plates (670) for pressing the hollow airbag (650) being mounted inside the hollow block (660) via a plurality of linkage components; The linkage assembly comprises a three-way hydraulic chamber (680), wherein two ports of the three-way hydraulic chamber (680) are both piston-slidingly connected to a push rod (690), and the other end port of the three-way hydraulic chamber (680) is connected to and fixed with a liquid storage capsule (6100), and a hollow track rod (6110) is fixed on the outer side of the three-way hydraulic chamber (680) close to the liquid storage capsule (6100), and a cylindrical metal rod (6120) is movably connected inside the hollow track rod (6110); The upper end of the interior of the mixing bin (100) is equipped with a filtering device, the filtering device comprising a feed pipe (700), the interior of the feed pipe (700) is slidably connected to an arched filter screen (710), both sides of the arched filter screen (710) are respectively connected to the inner wall of the feed pipe (700) via an accordion cover (780), an arc block (770) is fixed to the side of the arched filter screen (710), a spring piece is fixed between the arc block (770) and the feed pipe (700), the left side of the feed pipe (700) is rotatably connected to a first bevel gear rod (730) via a bracket block (720), a squeezing ball (740) is fixed to the first bevel gear rod (730), the side of the feed pipe (700) is rotatably connected to a second bevel gear rod (750), and the second bevel gear rod (750) is transmission-connected to an output shaft of a rotating motor (200) via a transmission belt (760).

2. The method for manufacturing an iron-based soft magnetic powder core according to claim 1, characterized in that: A cavity (642) is provided inside the shovel plate (640), a plurality of through holes (641) in communication with the cavity (642) are provided on the front end inclined surface of the shovel plate (640), a baffle (643) is rotatably connected to the side of the cavity (642) of the shovel plate (640), and a hemispherical body (644) is fixed to the side of the baffle (643).

3. The method for manufacturing an iron-based soft magnetic powder core according to claim 1, characterized in that: A two-way hydraulic chamber (645) is embedded in the bottom of the mixing chamber (100); one end of the two-way hydraulic chamber (645) is slidably connected to a pressure rod (646); the other end of the two-way hydraulic chamber (645) is slidably connected to a hydraulic rod (647); the top end of the hydraulic rod (647) is rotatably connected to a transverse pressure rod (648) via a torsion spring shaft.

4. The method for manufacturing an iron-based soft magnetic powder core according to claim 1, characterized in that: The second bevel gear rod (750) is vertically meshed with the first bevel gear rod (730), and the arc block (770) is located on the movement path of the squeezing ball (740).

Citation Information

Patent Citations

  • Iron-based nanocrystalline magnetic powder core with magnetic conductivity mu of 90 and preparing method thereof

    CN107578877A

  • Intelligent metal soft magnetic powder core production system

    CN108357946A

  • Method and equipment for mixing and stirring refractory castable

    CN116175768A

  • Alumina ceramic slurry mixing equipment and use method thereof

    CN116198019A

  • Preparation method of phosphoric acid / graphene / silicon nitride coated Fe-Si-Al magnetic powder core

    CN116364405A