A method, device and equipment for matching heating power for growing gallium oxide single crystal

By establishing a numerical model of heat transfer flow, the heating power configuration and cooling rate during the gallium oxide single crystal growth process were optimized, solving the problem of difficulty in determining the power configuration of multiple heaters, improving the crystallization rate and reducing energy consumption.

CN118147750BActive Publication Date: 2024-11-01BEIJING HONGYUN TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410428771.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-10
Publication Date
2024-11-01
Estimated Expiration
2044-04-10

AI Technical Summary

Technical Problem

In the process of gallium oxide single crystal growth, the impact of multiple heater power configurations and power reduction rates on crystallization quality and efficiency is difficult to determine, leading to problems such as poor crystallization quality or excessive energy consumption.

Method used

By establishing a numerical model of heat transfer flow in a single crystal furnace, different heater power ratios and cooling rate schemes are simulated. The cooling rate is adjusted to match the optimal heating power configuration, avoid bubble formation, and shorten the solidification time.

Benefits of technology

This method achieves improved crystallization speed and reduced energy consumption without affecting the quality of single crystal growth, thus optimizing the gallium oxide single crystal growth process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118147750B_ABST
    Figure CN118147750B_ABST
Patent Text Reader

Abstract

The present application provides a heating power matching method, device and equipment for gallium oxide single crystal growth, and relates to the field of single crystal growth technology. The method comprises: geometrically modeling and meshing a single crystal furnace, setting boundary conditions and control equations, and obtaining a heat transfer flow numerical model; simulating the crystal growth process of gallium oxide from complete melting to complete crystallization according to a set cooling rate scheme under a target power ratio through the heat transfer flow numerical model; adjusting and obtaining a new cooling rate scheme according to whether liquid bubbles appear during the crystal growth process of gallium oxide and the length of solidification time; resimulating the crystal growth process of gallium oxide from complete melting to complete crystallization according to the new cooling rate scheme under the target power ratio; determining the cooling rate scheme that can meet the requirement that no liquid bubbles are generated during the crystal growth process of gallium oxide and the shortest solidification time as the best cooling rate scheme matching the target power ratio.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of single crystal growth, and in particular to a heating power matching method, device and equipment for gallium oxide single crystal growth. Background Art

[0002] Gallium oxide is a new type of ultra-wide bandgap semiconductor material. Gallium oxide single crystals also have unique ultraviolet transmittance characteristics and the advantages of low energy loss, high thermal stability and chemical stability. It is an optimal semiconductor material for manufacturing high-temperature, high-frequency, high-power microelectronic devices, solar-blind ultraviolet photodetectors, and ultraviolet transparent conductive electrodes.

[0003] In the process of growing gallium oxide single crystals, multiple heaters are often used for heating and temperature control. However, in the actual growth process, the power configuration and power reduction rate between multiple heaters will affect the crystallization quality and crystallization efficiency of gallium oxide. For example, when the power reduction rate is too fast, it is easy to cause poor quality of gallium oxide crystallization, while when the power reduction rate is too slow, it is easy to cause gallium oxide crystallization time to be too long and energy consumption to be too high. Therefore, it is necessary to develop a heating power matching method, device and equipment for gallium oxide single crystal growth to determine the most suitable heating power related parameters in the gallium oxide single crystal growth process. Summary of the invention

[0004] In view of the above problems, the embodiments of the present application provide a heating power matching method, device and equipment for gallium oxide single crystal growth, so as to overcome the above problems or at least partially solve the above problems.

[0005] A first aspect of an embodiment of the present application provides a heating power matching method for growing a gallium oxide single crystal, comprising:

[0006] Performing geometric modeling on a single crystal furnace to obtain a geometric model; the single crystal furnace is a furnace for growing gallium oxide single crystals using a Bridgman method or a furnace for growing gallium oxide single crystals using a vertical gradient solidification method;

[0007] Based on the geometric model, meshing is performed on each area in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model;

[0008] The heat transfer flow numerical model is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power;

[0009] According to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time, a new cooling rate scheme is adjusted;

[0010] Resimulating the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the new cooling rate scheme;

[0011] The cooling rate scheme that can satisfy the requirement that no liquid bubbles are generated during the crystal growth of gallium oxide and that the solidification time is the shortest is determined as the optimal cooling rate scheme that matches the target power ratio.

[0012] A second aspect of the embodiment of the present application further provides a heating power matching device for growing a gallium oxide single crystal, the device comprising:

[0013] A numerical modeling module is used to perform geometric modeling on a single crystal furnace to obtain a geometric model, wherein the single crystal furnace is a furnace for growing gallium oxide single crystals by a Bridgman method or a furnace for growing gallium oxide single crystals by a vertical gradient solidification method; based on the geometric model, meshing is performed on each area in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model;

[0014] The thermal field simulation module is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and the set cooling rate scheme through the heat transfer flow numerical model; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power;

[0015] A scheme adjustment module is used to adjust a new cooling rate scheme according to whether liquid bubbles appear in the gallium oxide during the crystal growth process and the length of the solidification time;

[0016] A simulation module, used to re-simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the new cooling rate scheme;

[0017] The optimal cooling rate scheme determination module is used to determine the cooling rate scheme that can meet the requirement that no bubbles are generated during the crystal growth of gallium oxide and the solidification time is the shortest as the optimal cooling rate scheme matching the target power ratio.

[0018] A third aspect of an embodiment of the present application further provides an electronic device, comprising a memory, a processor, and a computer program stored on the memory, wherein the processor executes the computer program to implement the steps in the heating power matching method for growing gallium oxide single crystals described in the first aspect of an embodiment of the present application.

[0019] The fourth aspect of the embodiments of the present application further provides a computer-readable storage medium having a computer program / instruction stored thereon. When the computer program / instruction is executed by a processor, the steps in the heating power matching method for growing gallium oxide single crystals described in the first aspect of the embodiments of the present application are implemented.

[0020] The fifth aspect of the embodiments of the present application further provides a computer program product, which, when executed on an electronic device, enables a processor to implement the steps in the heating power matching method for growing a gallium oxide single crystal as described in the first aspect of the embodiments of the present application.

[0021] The embodiment of the present application provides a heating power matching method, device and equipment for gallium oxide single crystal growth, the method comprising: geometrically modeling a single crystal furnace to obtain a geometric model; the single crystal furnace is a gallium oxide single crystal growth furnace using a Bridgman method or a gallium oxide single crystal growth furnace using a vertical gradient solidification method; based on the geometric model, meshing is performed on each region in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model; using the heat transfer flow numerical model, simulating the crystallization process of gallium oxide from complete melting to complete crystallization according to a set cooling rate scheme under a target power ratio growth process; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace to the total heating power; according to whether there are bubbles in the gallium oxide during the crystal growth process and the length of the solidification time, a new cooling rate scheme is adjusted; the crystallization growth process of gallium oxide from complete melting to completion of crystallization under the target power ratio and according to the new cooling rate scheme is re-simulated; the cooling rate scheme that can meet the requirements of no bubble generation during the crystal growth process of gallium oxide and the shortest solidification time is determined as the optimal cooling rate scheme matching the target power ratio.

[0022] The method proposed in the present application establishes a numerical model of heat transfer flow in a single crystal furnace to simulate the crystal growth process of gallium oxide from complete melting to completion of crystallization according to a set cooling rate scheme under a target power ratio (power ratio of multiple heaters when the total heating power is constant). Thus, the cooling rate scheme is continuously adjusted according to the simulation results (whether liquid bubbles appear during the crystal growth of gallium oxide, and the length of the solidification time) until the optimal cooling rate scheme is found, so as to achieve the matching of the heater power ratio (target power ratio) and the solidification rate (cooling rate scheme), and obtain the most suitable heating power (i.e., cooling rate) during the growth of gallium oxide single crystals, thereby achieving the improvement of gallium oxide crystallization speed and reduction of energy consumption without affecting the quality of single crystal growth. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the description of the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0024] Figure 1 It is a flow chart of the steps of a heating power matching method for growing a gallium oxide single crystal provided in an embodiment of the present application;

[0025] Figure 2 is a structural schematic diagram of a heating power matching device provided in an embodiment of the present application;

[0026] Figure 3 It is a schematic diagram of an electronic device provided in an embodiment of the present application. DETAILED DESCRIPTION

[0027] The exemplary embodiments of the present application will be described in more detail below in conjunction with the accompanying drawings in the embodiments of the present application. Although the exemplary embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present application and to enable the scope of the present application to be fully communicated to those skilled in the art.

[0028] Gallium oxide is a new type of ultra-wide bandgap semiconductor material. It has five isomers, including α, β, and γ. Under specific temperature conditions, the five isomers can be converted into each other, among which β-Ga2O3 is the most stable. The bandgap width of gallium oxide single crystal is about 4.7-4.9eV, and the breakdown field strength is about 8MV / cm, which is much higher than semiconductor materials such as gallium nitride (GaN) and silicon carbide (SiC). Gallium oxide single crystal also has unique ultraviolet transmittance characteristics and the advantages of low energy loss, high thermal stability and chemical stability. It is the preferred semiconductor material for manufacturing high-temperature, high-frequency, high-power microelectronic devices, solar-blind ultraviolet photodetectors, and ultraviolet transparent conductive electrodes. Gallium oxide has also attracted widespread attention from scholars at home and abroad, and is considered to be a new generation of semiconductor materials that will support the rapid development of information, energy, transportation, manufacturing, national defense and other fields in the future.

[0029] At present, multiple heaters are often used for heating and temperature control in the process of growing gallium oxide single crystals. However, in the actual growth process, the power configuration of multiple heaters and their power reduction rate are important issues. If the optimal scheme of the power configuration of multiple heaters and their power reduction rate is determined by experimental method, it is not only time-consuming and labor-intensive, but also the changes of the thermal field and the solid-liquid interface during the growth of single crystals cannot be observed intuitively, and it is difficult to determine the influence of the current heater power configuration and its power reduction rate on the crystal quality of gallium oxide.

[0030] In view of the above problems, the embodiments of the present application propose a heating power matching method, device and equipment for gallium oxide single crystal growth to solve the above problems such as the inability to determine the power reduction rate of the heater. The heating power matching method for gallium oxide single crystal growth provided by the embodiments of the present application is described in detail below with reference to the accompanying drawings through some embodiments and their application scenarios.

[0031] In a first aspect, the present application provides a method for matching heating power for growing a gallium oxide single crystal, referring to Figure 1 , Figure 1 A flow chart of the steps of a heating power matching method for growing a gallium oxide single crystal provided in an embodiment of the present application, such as Figure 1 As shown, the method includes:

[0032] Step S101, geometric modeling is performed on a single crystal furnace to obtain a geometric model, wherein the single crystal furnace is a furnace for growing gallium oxide single crystals using a Bridgman method or a furnace for growing gallium oxide single crystals using a vertical gradient solidification method.

[0033] In the embodiment of the present application, a gallium oxide single crystal growth furnace using the Bridgman method or a gallium oxide single crystal growth furnace using the vertical gradient solidification method is used to prepare gallium oxide single crystals. Specifically, the single crystal furnace is composed of 9 main parts, namely: an insulation layer, a support component, a base, argon, a crucible, a gallium oxide melt, and a heating component. Among them, the heating component is composed of an upper and lower heater installed on the side of the single crystal furnace cavity, and both heaters are heated by resistance. The single crystal furnace is suitable for growing gallium oxide single crystals with a diameter of 100×100mm, and is also suitable for growing gallium oxide single crystals of other sizes using other methods.

[0034] The structural dimension parameters of the selected single crystal furnace (i.e., the single crystal furnace is a furnace for growing gallium oxide single crystals by the Bridgman method or a furnace for growing gallium oxide single crystals by the vertical gradient solidification method) are obtained, and the structure of the single crystal furnace is subjected to axisymmetric geometric modeling by using modeling software (such as Gambit software) to obtain a geometric model.

[0035] Step S102, based on the geometric model, mesh each area in the single crystal furnace (using meshing software) (wherein the mesh adopts quadrilateral mesh), and set boundary conditions and control equations to obtain a heat transfer flow numerical model.

[0036] In a possible implementation manner, the step S102, based on the geometric model, meshing each area in the single crystal furnace, and setting boundary conditions and control equations to obtain a heat transfer flow numerical model, includes:

[0037] Step S1021, based on the geometric model, meshing each area inside the single crystal furnace.

[0038] Step S1022, defining the boundary conditions and working pressure between the components inside the geometric model. The boundary conditions are as follows:

[0039] The outer wall temperature of the furnace in the geometric model is set to 300K, and the pressure inside the furnace is set to atmospheric pressure 101325Pa;

[0040] The boundary conditions of the gas-liquid interface (free surface) in the geometric model are set as follows:

[0041] Among them, λ l represents the thermal conductivity of the melt, λ g represents the thermal conductivity of argon, T g represents the temperature of argon gas, T l represents the melt temperature, represents the normal direction of the free interface, q rad,l Represents the latent heat of the melt.

[0042] τ l =τ g =0; where τ l Indicates the shear stress of the melt / Pa, τ g It represents the shear stress of argon gas / Pa.

[0043] The boundary conditions of the contact surface between the inner wall of the crucible and the melt (crystal) in the geometric model are set as follows:

[0044] Among them, λ l(s) represents the thermal conductivity of the melt / crystal, λ c represents the thermal conductivity of the crucible wall, T l(s) represents the temperature of the melt / crystal,

[0045] The boundary conditions of other solid-gas interfaces in the geometric model are set as follows:

[0046]

[0047] Set all radiation surfaces in the geometric model to diffuse gray surfaces, that is:

[0048] Where I represents the radiation intensity, represents the position vector, Ω represents the spatial solid angle, represents the direction vector, ε represents the surface emissivity of the radiating surface, Represents the radiation intensity at the contact boundary between solid and gas.

[0049] Step S1023, setting the control equations of each region in the geometric model, and discretizing them to obtain discrete equations.

[0050] Set the control equations that each region in the geometric model satisfies. The control equations are as follows:

[0051] Set the heat transfer flow governing equations satisfied by the melt-crystal region in the geometry model, including:

[0052] Continuity equation: Wherein, the subscript l represents gallium oxide melt; Indicates fluid flow velocity / m·s -1 .

[0053] Momentum equation: Where ρ represents the density of gallium oxide melt / kg·m -3 ;p l Indicates the working pressure of gallium oxide melt / Pa; represents the shear stress of gallium oxide melt / Pa; T m represents the melting point temperature of gallium oxide / K; g represents the acceleration due to gravity / m·s -2 ; T l represents the fluid temperature, t represents the time, β l represents the thermal expansion coefficient of gallium oxide melt, Represents a unit vector in the z direction.

[0054] Energy equation: Among them, C Pl Expresses the constant-pressure specific heat capacity of gallium oxide melt / J·kg -1 ·K -1 ; l Indicates the thermal conductivity of gallium oxide melt / W·m -1 ·K -1 , ΔH represents the latent heat of solidification of gallium oxide.

[0055] Set the heat transfer flow governing equations that the gas region in the geometry model satisfies, including:

[0056] The mass conservation equation: in, Indicates gas flow velocity / m·s -1 , ρ g Indicates gas density / kg·m -3 ;

[0057] Momentum conservation equation: Among them, p g Indicates the working pressure of gas / Pa.

[0058] Energy conservation equation: Among them, C Pg Indicates the constant pressure specific heat capacity of the gas region / J·kg -1 ·K -1 ,λ g represents the thermal conductivity of the gas, T g Indicates the gas temperature.

[0059] Ideal gas state equation: p g =R g ρg T g ; Among them, R g represents the ideal gas constant.

[0060] Set up the energy conservation equations for the heater region in the geometry model:

[0061] Where, the subscript h represents the heater, and ρ h Indicates the density of the heater area / kg·m -3 , C Ph Indicates the specific heat capacity of the heater area at constant pressure / J·kg -1 ·K -1 , T h represents the temperature of the heater zone, Q h represents the heat source of the heater area, λ h Indicates the thermal conductivity of the heater area / W·m -1 ·K -1 .

[0062] Set up the energy conservation equations for other solid regions in the geometry:

[0063] Wherein, the subscript i represents other solid regions, and ρ i Indicates the density of other solid areas / kg·m -3 , C Pi Indicates the constant pressure specific heat capacity of other solid regions / J·kg -1 ·K -1 , T i represents the temperature of other solid regions, λ i Indicates the thermal conductivity of other solid areas / W·m -1 ·K -1 .

[0064] In a possible implementation manner, setting the control equations of each region in the geometric model includes:

[0065] The phase change equation of the region where the gallium oxide solid-liquid interface is located in the geometric model is set as follows:

[0066]

[0067] Wherein, H=h+ΔH; H is the total enthalpy of the gallium oxide melt or crystal, h is the sensible enthalpy of the gallium oxide melt or crystal, ΔG is the latent heat of the phase change process, ρ is the density of the gallium oxide melt, λ is the thermal conductivity, u is the velocity of the melt, and ΔH is calculated by the following formula:

[0068]

[0069] Among them, L h is the latent heat of phase change, T0 is the melting point of gallium oxide, and T is the temperature of the melt or crystal region at the current moment;

[0070] The method further comprises:

[0071] According to the calculation result of the phase change equation, it is determined whether liquid bubbles appear at the solid-liquid interface at the current moment.

[0072] The control equations of each region set above are discretized to obtain discrete equations.

[0073] Step S1024, the physical parameters of each component are brought into the discrete equation to obtain the heat transfer flow numerical model. Specifically, the density, thermal conductivity, specific heat capacity of the solid materials involved in the single crystal furnace and the surface emissivity of the solid materials in contact with the gas need to be brought into the discrete equation to obtain the heat transfer flow numerical model; and the thermal conductivity, specific heat capacity and dynamic viscosity of the protective atmosphere - argon gas need to be brought into the equation.

[0074] Step S1025, assigning an initial value to each node in the model grid, wherein the initial value includes: the velocity, temperature and pressure of the grid node when all gallium oxide is melted.

[0075] The numerical model is initialized, that is, an initial value is assigned to each node in the divided model grid, and the initial value is the value of each node when all the gallium oxide raw materials are melted (including speed, temperature, pressure, etc.).

[0076] Step S103, simulating the crystal growth process of gallium oxide from complete melting to completion of crystallization under the target power ratio and the set cooling rate scheme through the heat transfer flow numerical model; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power.

[0077] Select a target power ratio for the heater of the single crystal furnace (the upper and lower heaters located on the side of the single crystal furnace cavity). The power ratio is the proportion of the heating power of each of the upper and lower heaters on the side of the single crystal furnace in the total heating power (the total power is distributed by different percentages). Exemplarily, according to the position of the heater, the power ratio of the upper and lower heaters can be set to 6:4, 8:2 or 10:0. According to the selected target power ratio, the thermal field distribution inside the single crystal growth furnace is numerically simulated and calculated to obtain the thermal field distribution in the crucible area, that is, the thermal field distribution at each moment in the crystal growth process from complete melting to completion of crystallization of gallium oxide according to the set cooling rate scheme.

[0078] Compared with other crystalline materials, gallium oxide has a high melting point, a low thermal conductivity, and a large latent heat of solidification. Therefore, during the dynamic directional solidification growth of gallium oxide, the latent heat of solidification released by the central melt cannot be transferred to the surrounding area well, and the latent heat of solidification continues to accumulate, which will eventually cause the solid-liquid interface of gallium oxide to bulge downward, and the bulge increases with the increase of dynamic solidification height, and liquid bubbles appear in the late stage of dynamic solidification. At the same time, it will take a long time to completely transfer the latent heat of solidification, which does not meet the actual needs of engineering.

[0079] Therefore, the general single crystal preparation method for preparing silicon and other crystals is not suitable for preparing gallium oxide crystals. In the process of preparing gallium oxide single crystals by the Bridgman method or the vertical gradient solidification method, it is necessary to more accurately control the heating power of multiple heaters of the single crystal furnace, that is, to find the best cooling rate scheme that matches the power ratio of the upper and lower heaters, so as to avoid the power reduction rate being too fast, resulting in poor gallium oxide crystallization quality (the solidification latent heat continues to accumulate and liquid bubbles are generated), and the power reduction rate being too slow, resulting in gallium oxide crystallization time being too long and energy consumption being too large. Among them, the cooling rate scheme represents the change of the reduction rate of the heating power of the heater over time, that is, the power reduction rate of the heater at each moment in the process from complete melting to complete crystallization of gallium oxide.

[0080] In a possible implementation manner, the step S103, simulating the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme through the heat transfer flow numerical model, includes:

[0081] By using the heat transfer flow numerical model and according to the target power ratio, the total power of the heater is set so that the temperature in the crucible of the single crystal furnace is greater than the melting point of gallium oxide, and a steady-state thermal field when gallium oxide is completely melted is simulated.

[0082] In the embodiment of the present application, firstly, according to the heat transfer flow numerical model, by setting the total power of the heater under the target power ratio, a steady-state thermal field is established when gallium oxide is completely melted, so that in the steady-state thermal field, the temperature in the crucible is higher than the melting point of gallium oxide (2080K). Exemplarily, when the power ratio of the upper and lower heaters on the side of the single crystal furnace is 6:4, the total power (input power) of the two heaters is set to 12560.5W.

[0083] Specifically, based on the obtained heat transfer flow numerical model, the corresponding energy equation, standard ke turbulence model, S2S radiation model, and solidification and melting model (Solidification & Melting model) are selected, and the melting point, specific heat capacity, thermal conductivity, thermal expansion coefficient, density, dynamic viscosity, solidification latent heat, surface emissivity and other parameters of gallium oxide are brought into the corresponding model; the density, thermal conductivity, specific heat capacity of the solid materials involved in the single crystal furnace and the surface emissivity of the solid materials in contact with the gas are also needed to be brought into the corresponding model; finally, the thermal conductivity, specific heat capacity and dynamic viscosity of the protective atmosphere - argon gas are also brought into the corresponding model. Then, calculations are performed based on the above models to simulate the steady-state thermal field when gallium oxide is completely melted.

[0084] Based on the steady-state thermal field, the thermal field distribution during the crystal growth process of gallium oxide from complete melting to completion of crystallization is simulated according to the cooling rate at each moment in the cooling rate scheme; the cooling rate represents the reduction in the total power of the heater per unit time.

[0085] In this embodiment, after the gallium oxide is completely melted, in order to cool and crystallize the gallium oxide, it is necessary to gradually reduce the total power of the heater so that the temperature in the crucible is lower than the melting point of gallium oxide (2080K). Based on the established steady-state thermal field, the same cooling time is set, and the cooling rate scheme for this simulation of the thermal field distribution (the reduction in the total power of the heater at each moment in the same cooling time) is set to calculate the thermal field distribution during the crystallization of gallium oxide. Exemplarily, when the power ratio of the upper and lower heaters on the side of the single crystal furnace is 8:2, the total power (input power) of the two heaters is set to 12678.5W. The cooling time is fixed to 10h, and the cooling rate scheme for this simulation is set to: the cooling rate at each moment is 43.2W·h -1 , that is, the total power drops by 43.2W per hour. Therefore, the simulation results show that the cooling rate is 43.2W·h -1 The thermal field distribution at each moment during the cooling and crystallization process of gallium oxide is calculated to realize the dynamic thermal field simulation of the process.

[0086] In a possible implementation manner, the step S103, simulating the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme through the heat transfer flow numerical model, includes:

[0087] Step S1031, according to the cooling rate scheme in the pre-written user-defined file (udf file), the parameter change of the heat source in the discrete equation of the heater area is controlled to obtain the discrete equation to be solved this time, and the initial value is substituted into the discrete equation to be solved this time to solve it. The solved value represents the thermal field information and flow field information in the heat transfer flow numerical model at the current moment.

[0088] Heat source parameter Q in the discrete equation for the heater region h , represents a parameter related to the heating power of the heater (for example, the total power of the upper and lower heaters, and the heating power of each heater allocated according to the target power ratio). When the initial value in step S1025 is substituted into the discrete equation for the first time, gallium oxide is in a completely molten state, and the temperature in the crucible in the corresponding discrete equation is higher than the melting point of gallium oxide (2080K). At this time, the value obtained by solving the discrete equation characterizes the information of the thermal field and flow field in the heat transfer flow numerical model, that is, the thermal field information and flow field information when gallium oxide is completely melted are obtained, that is, through steps S102-step S103 (the initial value in step S1025 is substituted into the discrete equation for the first time for solving), the steady-state thermal field when gallium oxide is completely melted is simulated.

[0089] In this embodiment, in order to realize the dynamic simulation of the process of gallium oxide melt being able to crystallize into gallium oxide crystals in a directional manner by gradually reducing the heating power of the heater, it is first necessary to select a linear power reduction scheme (i.e., a cooling rate scheme): the input power (total power of the upper and lower heaters) when the gallium oxide is completely melted and completely crystallized under a fixed power is used as the initial value, and the cooling time is selected as 10h (the cooling time is the time required for the total power when it is completely melted to be reduced to the total power when it is completely crystallized), (full melting power-full solidification power) ÷ cooling time = cooling rate, and the cooling rate represents the value of the total power when it is completely melted minus the total power when it is completely crystallized and then divided by the cooling time, that is, the power is reduced from the power when it is completely melted at the above-mentioned cooling rate as time increases. Then, according to the set cooling rate scheme, a corresponding udf file (user-defined file) is written, and the function of changing the input power of the heater (i.e., controlling the change of Qh in the heater area control equation) is controlled (for example, by computational heat transfer software) according to the udf file.

[0090] Step S1032, using the solved value as the initial value of the next round of solution, and performing iterative solution until the temperature value of each grid node on the free interface of gallium oxide (the melt surface in contact with the protective atmosphere) is less than the melting point of gallium oxide, thereby obtaining the thermal field distribution during the crystal growth process.

[0091] The solved value is used as the initial value of the second iteration, and then iterations are performed continuously (the solved value is re-entered into the discrete equation) until the temperature value of each grid node on the melt free interface is less than the melting point, and the thermal field distribution at each moment in the crystal growth process of gallium oxide from complete melting to complete crystallization is obtained.

[0092] Therefore, the embodiment of the present application obtains the information of the thermal field and flow field at each moment (the temperature, velocity and pressure corresponding to each grid node) by solving the energy equation, the standard Ke turbulence equation, the radiation equation and the phase change equation (enthalpy equation), and realizes the dynamic numerical simulation of the growth process of gallium oxide single crystal by continuously updating the thermal field and flow field information.

[0093] Step S104, adjusting a new cooling rate scheme according to whether bubbles appear during the crystal growth of gallium oxide and the length of the solidification time.

[0094] In this embodiment, by observing the changes in the solid-liquid interface in the thermal field distribution (i.e., the dynamic crystal growth process of gallium oxide) obtained in step S102, whether liquid bubbles appear, and the time required for complete crystallization (i.e., complete solidification), the selected cooling rate scheme (i.e., Q in the heater zone energy equation controlled by the udf file) under the target power ratio is determined. h The cooling rate scheme is then changed to repeat the above steps until a solidification process (cooling rate scheme) is found in which no bubbles appear during the crystallization of gallium oxide and the crystallization time is shorter.

[0095] In a possible implementation, the new cooling rate scheme is adjusted according to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time, including:

[0096] When no bubbles appear during the crystal growth of gallium oxide, the cooling rate at each moment in the current cooling rate scheme is increased by 50% to obtain the new cooling rate scheme; when no bubbles appear during the crystal growth of gallium oxide, the cooling rate can be appropriately increased (for example, the cooling rate is increased from 40W / h to 60W / h), thereby shortening the time required for gallium oxide cooling and crystallization (i.e., solidification time).

[0097] When bubbles appear during the crystal growth of gallium oxide, a first time period is determined, where the first time period represents the time period from when the gallium oxide is completely melted to when bubbles appear at the solid-liquid interface.

[0098] The cooling rate at each moment after the first time period in the current cooling rate scheme is reduced by 50% to obtain the new cooling rate scheme. Exemplarily, in the original cooling rate scheme, the cooling rate at each moment is 80W / h, and starting from the complete melting of gallium oxide, bubbles appear at the solid-liquid interface at the 2h10min. Then, in the new cooling rate scheme, the cooling rate is 80W / h in the time period from 0 to 2h10min, and the cooling rate is 40W / h in the time period after 2h10min.

[0099] In a possible implementation, the new cooling rate scheme is adjusted according to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time, including:

[0100] When no liquid bubble appears during the crystal growth of gallium oxide, the cooling rate at each moment in the current cooling rate scheme is increased by 50% to obtain the new cooling rate scheme;

[0101] When liquid bubbles appear during the crystal growth of gallium oxide, a second time period is determined, wherein the second time period represents the time period from when the gallium oxide is completely melted to when a negative temperature gradient appears in the gallium oxide;

[0102] The cooling rate at each moment after the second time period in the current cooling rate scheme is reduced by 50% to obtain the new cooling rate scheme. Specifically, when the cooling rate is too fast, the gallium oxide crystal is prone to a negative temperature gradient (the temperature inside the crystal is higher than the temperature inside the melt, and heat is transferred from the crystal to the melt), which leads to the appearance of vacuole. Therefore, when a negative temperature gradient appears in gallium oxide, the cooling rate scheme is adjusted to appropriately reduce the cooling rate, thereby avoiding the appearance of vacuole when gallium oxide crystallizes.

[0103] Step S105, resimulating the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio according to the new cooling rate scheme. Specifically, resimulating according to steps S101 to S104 to obtain the thermal field distribution of gallium oxide from complete melting to complete crystallization under the new cooling rate scheme.

[0104] Step S106, determining a cooling rate scheme that can meet the requirement of no liquid bubbles being generated during the crystal growth of gallium oxide and having the shortest solidification time as the best cooling rate scheme matching the target power ratio.

[0105] The method proposed in this application establishes a numerical model of heat transfer flow in a single crystal furnace to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio (power ratio of multiple heaters under a certain total heating power) according to the set cooling rate scheme. Therefore, the cooling rate scheme is continuously adjusted according to the simulation results (whether liquid bubbles appear during the crystal growth of gallium oxide and the length of solidification time) until the optimal cooling rate scheme is found to achieve the matching of heater power ratio (target power ratio) and solidification rate (cooling rate scheme).

[0106] In a possible implementation, the method further includes:

[0107] When the target power ratio is 8:2, the optimal cooling rate scheme is determined as follows: starting from the complete melting of gallium oxide, the cooling rate at each moment is 86.4 W / h, and the cooling rate at each moment after the third time period is 43.2 W / h;

[0108] The single crystal furnace is used to prepare gallium oxide single crystals. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12678.5 W to 12246.5 W.

[0109] Specifically, when the target power ratio is 8:2, step S101-step S106 is executed, and the total power of the heater is initially set to 12678.5W to obtain the steady-state thermal field when the gallium oxide is completely melted, and then the cooling rate is adjusted according to the simulated thermal field distribution (whether there are bubbles during the crystallization growth of gallium oxide, and the length of the solidification time), and then the thermal field distribution during the gallium oxide crystallization process under the target power ratio (8:2) is recalculated. The cooling time is set to 10h. When the target power ratio is 8:2, no negative temperature gradient (i.e., no bubbles are generated) occurs during the solidification of the gallium oxide melt. In order to study how to grow gallium oxide single crystals faster without negative temperature gradients, the cooling time at the 8:2 power ratio is reduced, that is, the cooling rate at the 8:2 power ratio is increased. Through multiple simulations, it was determined that when the power ratio was 8:2, when the cooling rate of 86.4W / h was used, the gallium oxide melt had a negative temperature gradient in the late solidification stage, and when the cooling rate of 86.4W / h was first used and then 43.2W / h, the gallium oxide melt did not have a negative temperature gradient in the late solidification stage, and the solidification time was short. Therefore, the optimal cooling rate scheme is determined as follows: starting from the complete melting of gallium oxide, the cooling rate at each moment is 86.4W / h, and the cooling rate at each moment after the third time is 43.2W / h. The third time represents the time required to reduce the total power when gallium oxide is fully melted minus two-thirds of the total power when gallium oxide is fully crystallized. Exemplarily, from a total power of 90W / h when gallium oxide is fully melted, it is reduced to a total power of 30W / h when gallium oxide is fully crystallized at a fixed cooling rate, and the total time is 9h. The third duration represents the time required to reduce the total power from 90W / h when gallium oxide is fully melted, minus two-thirds of the total power from 30W / h when gallium oxide is fully crystallized, that is, the time required to reduce it to 50W / h, which is 6h.

[0110] After obtaining the optimal cooling rate scheme, the single crystal furnace was used to prepare gallium oxide single crystals. After the gallium oxide was completely melted, the heater was controlled to cool and crystallize according to the optimal cooling rate scheme, so that the total power of the heater was reduced from 12678.5W to 12246.5W.

[0111] In a possible implementation, the method further includes:

[0112] When the target power ratio is 10:0, the optimal cooling rate scheme is determined as follows: starting from the complete melting of gallium oxide, the cooling rate at each moment is 129.6 W / h;

[0113] The single crystal furnace is used to prepare gallium oxide single crystals. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12867.8W to 12218.4W.

[0114] Specifically, when the target power ratio is 10:0 (i.e., the upper heater is retained and the lower heater is suspended), steps S101 to S106 are performed, and the total power of the heater is initially set to 12867.8W to obtain the steady-state thermal field when the gallium oxide is completely melted, and then the cooling rate is adjusted according to the simulated thermal field distribution (whether there are bubbles during the crystallization growth of gallium oxide, and the length of the solidification time), and then the thermal field distribution during the gallium oxide crystallization process under the target power ratio (10:0) is recalculated. The cooling time is set to 10h. When the target power ratio is 10:0, no negative temperature gradient (i.e., no bubble is generated) occurs during the solidification of the gallium oxide melt. In order to study how to grow gallium oxide single crystals faster without negative temperature gradients, the cooling time at the 10:0 power ratio is reduced, that is, the cooling rate at the 10:0 power ratio is increased. Through multiple simulations, it was determined that when the power ratio was 10:0, a negative temperature gradient appeared in the gallium oxide melt at the late stage of solidification when a cooling rate of 259.2W / h was used, while no negative temperature gradient appeared in the gallium oxide melt at the late stage of solidification when a cooling rate of 129.6W / h was used, and the solidification time was shorter. Therefore, the optimal cooling rate scheme was determined to be: starting from the complete melting of gallium oxide, the cooling rate at each moment was 129.6W / h.

[0115] After obtaining the optimal cooling rate scheme, the single crystal furnace was used to prepare gallium oxide single crystals. After the gallium oxide was completely melted, the heater was controlled to cool and crystallize according to the optimal cooling rate scheme, so that the total power of the heater was reduced from 12867.8W to 12218.4W.

[0116] In addition, when the target power ratio is 6:4, step S101-step S106 is performed, and the total power of the heater is initially set to 12560.5W to obtain the steady-state thermal field when the gallium oxide is completely melted, and then the cooling rate is adjusted according to the simulated thermal field distribution (whether there are bubbles in the gallium oxide during the crystallization growth process, and the length of the solidification time), and then the thermal field distribution of the gallium oxide crystallization process under the target power ratio (6:4) is recalculated. The cooling time is set to 10h. When the target power ratio is 6:4, a negative temperature gradient appears in the late solidification process of the gallium oxide melt. In order to study under what circumstances the negative temperature gradient will not appear, the cooling time at the 6:4 power ratio is increased, that is, the cooling rate at the 6:4 power ratio is reduced. Through multiple simulations, it is determined that when the power ratio is 6:4, the gallium oxide melt will have a negative temperature gradient in the late solidification period under multiple cooling rate schemes. Therefore, when the 6:4 power ratio is determined, it is not suitable for growing gallium oxide single crystals.

[0117] The second aspect of the embodiment of the present application further provides a heating power matching device for growing a gallium oxide single crystal, referring to Figure 2 , Figure 2 A schematic diagram of the structure of a heating power matching device is shown. Figure 2 As shown, the device comprises:

[0118] A numerical modeling module is used to perform geometric modeling on a single crystal furnace to obtain a geometric model, wherein the single crystal furnace is a furnace for growing gallium oxide single crystals by a Bridgman method or a furnace for growing gallium oxide single crystals by a vertical gradient solidification method; based on the geometric model, meshing is performed on each area in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model;

[0119] The thermal field simulation module is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and the set cooling rate scheme through the heat transfer flow numerical model; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power;

[0120] A scheme adjustment module is used to adjust a new cooling rate scheme according to whether liquid bubbles appear in the gallium oxide during the crystal growth process and the length of the solidification time;

[0121] A simulation module, used to re-simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the new cooling rate scheme;

[0122] The optimal cooling rate scheme determination module is used to determine the cooling rate scheme that can meet the requirement that no bubbles are generated during the crystal growth of gallium oxide and the solidification time is the shortest as the optimal cooling rate scheme matching the target power ratio.

[0123] In a possible implementation, the scheme adjustment module includes:

[0124] A first adjustment submodule is used for increasing the cooling rate at each moment in the current cooling rate scheme by 50% to obtain the new cooling rate scheme when no liquid bubble appears during the crystal growth of gallium oxide;

[0125] A first time determination submodule, used for determining a first time when bubbles appear during the crystal growth of gallium oxide, wherein the first time indicates the time from when the gallium oxide is completely melted to when bubbles appear at the solid-liquid interface;

[0126] The second adjustment submodule is used to reduce the cooling rate at each moment after the first time period in the current cooling rate scheme by 50% to obtain the new cooling rate scheme.

[0127] In a possible implementation manner, the scheme adjustment module further includes:

[0128] A third adjustment submodule is used for increasing the cooling rate at each moment in the current cooling rate scheme by 50% to obtain the new cooling rate scheme when no liquid bubble appears during the crystal growth process of gallium oxide;

[0129] A second time determination submodule, used for determining a second time when bubbles appear in the gallium oxide during the crystal growth process, wherein the second time indicates the time from when the gallium oxide is completely melted to when a negative temperature gradient appears in the gallium oxide;

[0130] The fourth adjustment submodule is used to reduce the cooling rate at each moment after the second time period in the current cooling rate scheme by 50% to obtain the new cooling rate scheme.

[0131] In a possible implementation, the thermal field simulation module includes:

[0132] A steady-state thermal field simulation submodule is used to set the total power of the heater according to the target power ratio through the heat transfer flow numerical model, so that the temperature in the crucible of the single crystal furnace is greater than the melting point of gallium oxide, and simulate the steady-state thermal field when gallium oxide is completely melted;

[0133] The dynamic thermal field simulation submodule is used to simulate the thermal field distribution of the gallium oxide during the crystal growth process from complete melting to completion of crystallization based on the steady-state thermal field and the cooling rate at each moment in the cooling rate scheme; the cooling rate represents the reduction in the total power of the heater per unit time.

[0134] In a possible implementation, the numerical modeling module includes:

[0135] A meshing submodule, used for meshing each area inside the single crystal furnace based on the geometric model;

[0136] A boundary condition definition submodule, used to define boundary conditions and working pressures between various components within the geometric model;

[0137] A discrete submodule, used for setting the control equations of each region in the geometric model and performing discretization to obtain discrete equations;

[0138] A parameter input submodule is used to input the physical parameters of each component into the discrete equation to obtain the heat transfer flow numerical model;

[0139] An initialization submodule is used to assign an initial value to each node in the model grid, wherein the initial value includes: the speed, temperature and pressure of the grid node when all gallium oxide is melted;

[0140] The thermal field simulation module comprises:

[0141] A solving submodule, for controlling the change of heat source parameters in the discrete equation of the heater region according to the cooling rate scheme in the pre-written user-defined file, obtaining the discrete equation to be solved this time, substituting the initial value into the discrete equation to be solved this time, and solving the value obtained by the solution to represent the thermal field information and flow field information in the heat transfer flow numerical model at the current moment;

[0142] The iterative submodule is used to substitute the solved value as the initial value for the next round of solution, and perform iterative solution until the temperature value of each grid node on the free interface of gallium oxide obtained by solution is less than the melting point of gallium oxide, thereby obtaining the thermal field distribution.

[0143] In a possible implementation, the discrete submodule includes:

[0144] The phase change equation setting unit is used to set the phase change equation of the region where the gallium oxide solid-liquid interface is located in the geometric model, and the phase change equation is as follows:

[0145] Wherein, H=h+ΔH; H is the total enthalpy of the gallium oxide melt or crystal, h is the sensible enthalpy of the gallium oxide melt or crystal, ΔH is the latent heat of the phase change process, ρ is the density of the gallium oxide melt, λ is the thermal conductivity, u is the velocity of the gallium oxide melt, and ΔH is calculated by the following formula:

[0146]

[0147] Among them, L h is the latent heat of phase change, T0 is the melting point of gallium oxide, and T is the temperature of the melt or crystal region at the current moment.

[0148] In a possible implementation, the device further includes:

[0149] The first scheme determination module is used to determine, when the target power ratio is 8:2, that the optimal cooling rate scheme is: starting from the complete melting of gallium oxide, the cooling rate at each moment is 86.4 W / h, and the cooling rate at each moment after the third time length is 43.2 W / h; the third time length is the time required to reduce the total power when gallium oxide is fully melted minus two-thirds of the total power when gallium oxide is fully crystallized;

[0150] The first single crystal preparation module is used to prepare gallium oxide single crystals using the single crystal furnace. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12678.5W to 12246.5W.

[0151] In a possible implementation, the device further includes:

[0152] The second scheme determination module is used to determine that the optimal cooling rate scheme is: starting from the complete melting of gallium oxide, the cooling rate at each moment is 129.6 W / h when the target power ratio is 10:0;

[0153] The second single crystal preparation module is used to prepare gallium oxide single crystals using the single crystal furnace. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12867.8W to 12218.4W.

[0154] The present application also provides an electronic device, referring to Figure 3 , Figure 3 Schematic diagram of an electronic device proposed in an embodiment of the present application. Figure 3 As shown, the electronic device 100 includes: a memory 110 and a processor 120. The memory 110 and the processor 120 are connected via a bus communication. A computer program is stored in the memory 110. The computer program can be run on the processor 120 to implement the steps in the heating power matching method for growing gallium oxide single crystals disclosed in the embodiment of the present application.

[0155] The embodiment of the present application also provides a computer-readable storage medium having a computer program / instruction stored thereon. When the computer program / instruction is executed by a processor, the steps in the heating power matching method for growing a gallium oxide single crystal as disclosed in the embodiment of the present application are implemented.

[0156] The embodiment of the present application further provides a computer program product. When the computer program product is run on an electronic device, the processor is enabled to implement the steps of the heating power matching method for growing a gallium oxide single crystal as disclosed in the embodiment of the present application.

[0157] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0158] The embodiments of the present application are described with reference to the flowcharts and / or block diagrams of the methods, apparatuses, electronic devices, and computer program products according to the embodiments of the present application. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of the processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing terminal device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing terminal device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.

[0159] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing terminal device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce a manufactured product including an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.

[0160] These computer program instructions can also be loaded onto a computer or other programmable data processing terminal device so that a series of operating steps are executed on the computer or other programmable terminal device to produce a computer-implemented process, thereby providing instructions for executing on the computer or other programmable terminal device to implement the process. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.

[0161] Although the preferred embodiments of the present application have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the embodiments of the present application.

[0162] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "including one..." do not exclude the existence of other identical elements in the process, method, article or terminal device including the elements.

[0163] The above is a detailed introduction to the heating power matching method, device and equipment for the growth of gallium oxide single crystals provided by the present application. Specific examples are used in this article to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method of the present application and its core idea; at the same time, for general technicians in this field, according to the ideas of the present application, there will be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as a limitation on the present application.

Claims

1. A heating power matching method for gallium oxide single crystal growth, characterized in that: The method comprises: Performing geometric modeling on a single crystal furnace to obtain a geometric model, wherein the single crystal furnace is a furnace for growing gallium oxide single crystals using a Bridgman method or a furnace for growing gallium oxide single crystals using a vertical gradient solidification method; Based on the geometric model, meshing is performed on each area in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model; The heat transfer flow numerical model is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power; According to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time, a new cooling rate scheme is adjusted; Resimulating the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the new cooling rate scheme; Determine a cooling rate scheme that can satisfy the requirement that no liquid bubbles are generated during the crystal growth of gallium oxide and that the solidification time is the shortest as the optimal cooling rate scheme that matches the target power ratio; Wherein, based on the geometric model, each area in the single crystal furnace is meshed, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model, including: Based on the geometric model, meshing each area inside the single crystal furnace; defining boundary conditions and working pressures between various components within the geometric model; Setting the control equations of each region in the geometric model and discretizing them to obtain discrete equations; Substituting the physical property parameters of each component into the discrete equation to obtain the heat transfer flow numerical model; Assigning an initial value to each node in the model grid, the initial value comprising: the velocity, temperature and pressure of the grid node when all gallium oxide is melted; The heat transfer flow numerical model is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme, including: According to the cooling rate scheme in the pre-written user-defined file, the parameter change of the heat source in the discrete equation of the heater area is controlled to obtain the discrete equation to be solved this time, and the initial value is substituted into the discrete equation to be solved this time, and the solved value represents the thermal field information and flow field information in the heat transfer flow numerical model at the current moment; The solved value is used as the initial value of the next round of solution, and the solution is iterated until the temperature value of each grid node on the free interface of gallium oxide obtained by the solution is less than the melting point of gallium oxide, thereby obtaining the thermal field distribution during the crystal growth process; The control equations for each region in the geometric model are set, including: The phase change equation of the region where the gallium oxide solid-liquid interface is located in the geometric model is set as follows: Wherein, H=h+ΔH; H is the total enthalpy of the gallium oxide melt or crystal, h is the sensible enthalpy of the gallium oxide melt or crystal, ΔH is the latent heat of the phase change process, ρ is the density of the gallium oxide melt, λ is the thermal conductivity of the gallium oxide melt, u is the velocity of the gallium oxide melt, and ΔH is calculated by the following formula: Among them, L h is the latent heat of phase change, T0 is the melting point of gallium oxide, and T is the temperature of the melt or crystal region at the current moment.

2. The heating power matching method for gallium oxide single crystal growth according to claim 1, characterized in that: The method of adjusting the cooling rate according to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time includes: When no liquid bubble appears during the crystal growth of gallium oxide, the cooling rate at each moment in the current cooling rate scheme is increased by 50% to obtain the new cooling rate scheme; When bubbles appear during the crystal growth of gallium oxide, a first time duration is determined, wherein the first time duration represents the time duration from when the gallium oxide is completely melted to when bubbles appear at the solid-liquid interface; In the current cooling rate scheme, the cooling rate at each moment after the first time period is reduced by 50% to obtain the new cooling rate scheme.

3. The heating power matching method for gallium oxide single crystal growth according to claim 1, characterized in that: The method of adjusting the cooling rate according to whether vacuole appears in the gallium oxide during the crystal growth process and the length of the solidification time includes: When no liquid bubble appears during the crystal growth of gallium oxide, the cooling rate at each moment in the current cooling rate scheme is increased by 50% to obtain the new cooling rate scheme; When liquid bubbles appear during the crystal growth of gallium oxide, a second time period is determined, wherein the second time period represents the time period from when the gallium oxide is completely melted to when a negative temperature gradient appears in the gallium oxide; In the current cooling rate scheme, the cooling rate at each moment after the second time period is reduced by 50% to obtain the new cooling rate scheme.

4. The heating power matching method for gallium oxide single crystal growth according to claim 1, characterized in that: The heat transfer flow numerical model is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the set cooling rate scheme, including: By using the heat transfer flow numerical model, according to the target power ratio, the total power of the heater is set so that the temperature in the crucible of the single crystal furnace is greater than the melting point of gallium oxide, and a steady-state thermal field when gallium oxide is completely melted is simulated; Based on the steady-state thermal field, the thermal field distribution during the crystal growth process of gallium oxide from complete melting to completion of crystallization is simulated according to the cooling rate at each moment in the cooling rate scheme; the cooling rate represents the reduction in the total power of the heater per unit time.

5. The heating power matching method for gallium oxide single crystal growth according to claim 1, characterized in that: The method further comprises: When the target power ratio is 8:2, the optimal cooling rate scheme is determined as follows: starting from the complete melting of gallium oxide, the cooling rate at each moment is 86.4 W / h, and the cooling rate at each moment after the third time period is 43.2 W / h; the third time period is the time required to reduce the total power when gallium oxide is fully melted minus two-thirds of the total power when gallium oxide is fully crystallized; The single crystal furnace is used to prepare gallium oxide single crystals. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12678.5 W to 12246.5 W.

6. The heating power matching method for gallium oxide single crystal growth according to claim 1, characterized in that: The method further comprises: When the target power ratio is 10:0, the optimal cooling rate scheme is determined as follows: starting from the complete melting of gallium oxide, the cooling rate at each moment is 129.6 W / h; The single crystal furnace is used to prepare gallium oxide single crystals. After the gallium oxide is completely melted, the heater is controlled to perform cooling and crystallization according to the optimal cooling rate scheme, so that the total power of the heater is reduced from 12867.8W to 12218.4W.

7. A heating power matching device for gallium oxide single crystal growth, characterized in that: A heating power matching method for growing a gallium oxide single crystal according to any one of claims 1 to 6, the device comprising: A numerical modeling module is used to perform geometric modeling on a single crystal furnace to obtain a geometric model, wherein the single crystal furnace is a furnace for growing gallium oxide single crystals by a Bridgman method or a furnace for growing gallium oxide single crystals by a vertical gradient solidification method; based on the geometric model, meshing is performed on each area in the single crystal furnace, and boundary conditions and control equations are set to obtain a heat transfer flow numerical model; The thermal field simulation module is used to simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and the set cooling rate scheme through the heat transfer flow numerical model; the target power ratio is the proportion of the heating power of the upper and lower heaters on the side of the single crystal furnace in the total heating power; A scheme adjustment module is used to adjust a new cooling rate scheme according to whether liquid bubbles appear in the gallium oxide during the crystal growth process and the length of the solidification time; A simulation module, used to re-simulate the crystal growth process of gallium oxide from complete melting to complete crystallization under the target power ratio and according to the new cooling rate scheme; The optimal cooling rate scheme determination module is used to determine the cooling rate scheme that can meet the requirement that no bubbles are generated during the crystal growth of gallium oxide and the solidification time is the shortest as the optimal cooling rate scheme matching the target power ratio.

8. An electronic device, characterized in that: The method comprises a memory, a processor and a computer program stored in the memory, wherein the processor executes the computer program to implement the heating power matching method for growing a gallium oxide single crystal according to any one of claims 1 to 6.