A rapid die-casting process and die-casting equipment

The adhesion between the casting and the mold cavity is reduced by the hydraulic telescopic rod and the air blowing assembly, which solves the problems of difficulty in demoulding and mold damage in the existing technology, and achieves easier demoulding and higher yield.

CN118162600BActive Publication Date: 2024-10-15WUYI YUSHUN IND & TRADE CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410519903.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-28
Publication Date
2024-10-15
Estimated Expiration
2044-04-28

AI Technical Summary

Technical Problem

When demolding existing die-casting equipment, due to the strong adhesion between the casting and the mold cavity, the push rod requires a large thrust, which increases the difficulty of demoulding and may damage the mold cavity or the casting.

Method used

The hydraulic telescopic rod is used in conjunction with the blowing component. The mold and the fixed mold are moved through the hydraulic telescopic rod to form a die-casting cavity. The air compressor is used to generate compressed gas to reduce the adhesion between the casting and the cavity. The ejection component is used. Push the casting out of the mold.

Benefits of technology

The thrust required for demoulding is reduced, damage to the mold and castings caused by excessive adhesion is avoided, the yield is improved and the service life of the mold is extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118162600B_ABST
    Figure CN118162600B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of die casting, and specifically relates to a rapid die casting process and die casting equipment. The die casting equipment comprises a machine platform, and a chassis is fixed on the top of the machine platform. The present invention makes a push block contact with a push plate by moving a movable mold, so that the push plate is used to push the push blocks at the upper and lower ends of the built-in plate to drive the built-in plate to move, so that the push column at the front of the built-in plate moves into the cavity in the movable mold to push out the molded casting for demolding operation, and an air compressor is used to generate compressed gas and inject it into the cavity through the air hole, and the gas is used to act between the cavity and the casting to reduce the adhesion between the casting and the cavity. After the adhesion is reduced, the thrust required by the push plate is reduced, so that demolding is easier, and the adhesion between the casting and the inner wall of the cavity is reduced by blowing air to avoid damage to the mold cavity and the casting body when the casting is directly pushed due to excessive adhesion. Not only the yield rate is improved, but also the service life of the mold is extended.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of die casting, in particular to a rapid die casting process and die casting equipment. Background Art

[0002] Die casting equipment is the equipment used for die casting process. Die casting equipment provides high pressure to inject molten metal liquid into the die casting mold cavity. After the casting is cooled and solidified in the mold cavity, the casting is pushed out of the mold cavity using a push rod to complete the die casting of the casting.

[0003] The prior art also proposes some solutions. For example, a patent application with publication number CN218785178U discloses a die-casting equipment, including a die-casting equipment bottom box, and a die-casting equipment outer box is installed above the die-casting equipment bottom box. The application inserts the positioning card block into the second positioning groove and the first positioning groove to make the upper pressure plate and the lower pressure plate fit more closely.

[0004] When the die-casting equipment is demolding, a push rod is used to push the casting. If the adhesion between the casting and the cavity is large, a large thrust is required, which will increase the difficulty of demolding and cause a large load on the push rod and related equipment. Directly pushing the casting may cause deformation of the casting or damage the mold cavity.

[0005] To this end, the present invention provides a rapid die-casting process and die-casting equipment. Summary of the invention

[0006] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.

[0007] The technical solution adopted by the present invention to solve the technical problem is: a rapid die-casting process described in the present invention, the die-casting process steps are as follows:

[0008] S1: Check and clean the mold, install the mold in the die-casting equipment, use the die-casting equipment to melt the required alloy and maintain the appropriate temperature;

[0009] S2: Using die-casting equipment to close the mold to form a die-casting cavity, injecting the molten alloy into the pressure chamber of the die-casting equipment, and pressing the alloy into the die-casting cavity under high pressure to fill and form;

[0010] S3: Maintain a certain pressure in the mold to ensure the density of the casting, and allow the casting to cool and solidify in the mold;

[0011] S4: Use the die-casting equipment to open the mold, cooperate with the demoulding mechanism to push the casting out of the mold, take out the casting, and complete the die-casting.

[0012] Preferably, the die-casting equipment includes a machine platform, a chassis is fixed on the top of the machine platform, a moving plate is arranged at the front end of the chassis, a hydraulic telescopic rod is installed inside the chassis, the front end of the hydraulic telescopic rod extends from the inside of the chassis and is fixedly connected to the moving plate, a fixed plate is arranged at the front end of the moving plate, the fixed plate is fixed to the machine platform, a moving mold and a fixed mold are arranged between the moving plate and the fixed plate, the moving mold is installed at the front of the moving plate, the fixed mold is installed at the back of the fixed plate, a shot assembly is arranged at the front end of the fixed plate, the shot assembly is used to fill the molten metal into the mold cavity and provide the pressure required for die-casting, a push assembly is arranged at the rear end inside the moving mold, the push assembly is used to push the casting in the mold cavity, the upper and lower ends of the push assembly are provided with push assemblies, the push assembly is used to push the push assembly to move, the upper and lower ends of the moving mold are provided with blowing assemblies, the blowing assembly is used to inflate the mold cavity, and the upper and lower ends of the front of the moving mold are provided with sealing assemblies, the sealing assemblies are used to seal the blowing assembly.

[0013] Preferably, the pushing assembly includes an inner cavity opened at the rear end of the movable mold, an inner plate is provided inside the inner cavity, a pushing column is fixed to the front of the inner plate, the front end of the pushing column extends into the cavity in the movable mold, guide grooves are provided on both sides of the inner plate, guide columns penetrate the guide grooves, the guide columns are fixed in the inner cavity, a return spring is wound around the outside of the guide column, the return spring is placed at the front end of the inner plate, one end of the return spring is fixedly connected to the inner plate, and the other end of the return spring is fixedly connected to the inner wall of the inner cavity.

[0014] Preferably, the inner diameter of the guide groove matches the outer diameter of the guide column, and the built-in plate slides outside the guide column through the guide groove.

[0015] Preferably, the push assembly includes a through cavity opened at the upper and lower ends of the movable mold, the through cavity is connected to the interior of the inner cavity, push blocks are fixed to the upper and lower ends of the built-in plate, the push blocks extend from the through cavity, a push groove is fixed to the back of the push block, through grooves are opened at the upper and lower ends of the movable plate, the positions of the through grooves and the push grooves correspond exactly, and push plates are fixed to the upper and lower ends of the front of the chassis, the positions of the push plates and the through grooves and the push grooves correspond exactly.

[0016] Preferably, the push plate can pass through the through slot and be inserted into the push groove, and the push block can move horizontally in the through cavity.

[0017] Preferably, the blowing assembly includes connecting grooves opened at the upper and lower ends of the movable mold, an air hole is opened at one end of the connecting groove, the air hole is connected with the cavity inside the movable mold, air guide boxes are installed at the upper and lower ends of the movable mold, the interior of the air guide box is connected to the connecting groove, an injection box is fixed to the side wall of the movable mold, the upper and lower ends of the injection box are connected with connecting pipes, the other end of the connecting pipe is connected to the air guide box, one side of the injection box is connected with an air duct, one end of the air duct is connected to an air compressor, and the air compressor is installed on the side wall of the machine.

[0018] Preferably, the number of the air holes and the connecting grooves is the same, and the air holes and the connecting grooves are evenly spaced at the upper and lower ends inside the movable mold.

[0019] Preferably, the blocking component includes slots opened at the upper and lower ends of the movable mold, the slot is located at the bottom end of the air hole and is connected to the air hole, a blocking pin is arranged inside the slot, the top end of the blocking pin extends into the air hole, a movable block is fixed to the outside of the blocking pin, the top of the movable block abuts against the inner wall of the slot, a fixed block is arranged at the bottom end of the movable block, the bottom end of the blocking pin passes through the fixed block, the fixed block is fixed in the slot, a telescopic spring is fixed to the top of the fixed block, the top of the telescopic spring is fixedly connected to the movable block, the telescopic spring is wound around the outside of the blocking pin, and plug blocks are fixed to the upper and lower ends of the back of the fixed mold, a top block is fixed to the end of the plug block, and the top block is located at the bottom of the blocking pin.

[0020] Preferably, the end of the top block is an inclined end surface, and the inclined end surface of the top block can scoop up the bottom of the blocking pin.

[0021] The beneficial effects of the present invention are as follows:

[0022] 1. A rapid die-casting process and die-casting equipment described in the present invention, through the movement of the movable mold, the push block is brought into contact with the push plate, so that the push plate pushes the push blocks at the upper and lower ends of the built-in plate to drive the built-in plate to move, so that the push column at the front of the built-in plate moves into the cavity in the movable mold to push out the molded casting for demolding operation, and an air compressor is used to generate compressed gas and inject it into the cavity through the air hole, and the gas is used to act between the cavity and the casting to reduce the adhesion between the casting and the cavity. After the adhesion is reduced, the thrust required by the push plate is reduced, making demolding easier, and the adhesion between the casting and the inner wall of the cavity is reduced by blowing air to avoid damage to the mold cavity and the casting body when the casting is directly pushed due to excessive adhesion. This not only improves the yield rate, but also helps to extend the service life of the mold.

[0023] 2. A rapid die-casting process and die-casting equipment described in the present invention, when the hydraulic telescopic rod pushes the movable plate to drive the movable mold to move toward the position of the fixed mold to close the mold, the plug blocks at the upper and lower ends of the back of the fixed mold and the top blocks at the ends thereof gradually move into the slots, the inclined end faces of the top blocks shovel up the bottom of the blocking pin to move the blocking pin upward, the top of the blocking pin moves into the air hole to block the air hole, and at the same time, the upward moving blocking pin drives the movable block to move upward to pull the telescopic spring to extend, and when the hydraulic telescopic rod is used to pull the movable plate to drive the movable mold away from the fixed mold to open the mold, the upper and lower ends of the back of the fixed mold The plug block at the end and the top block at its end are gradually moved out of the slot, and the blocking pin loses the thrust of the top block. Under the elastic force of the telescopic spring, the telescopic spring pulls the moving block to drive the blocking pin to move out from the inside of the pore to open the pore. When the mold is closed to inject the alloy, the end of the blocking pin moves into the pore to block and close the pore. When the mold is opened, the end of the blocking pin moves out of the pore to open the pore. By blocking the pore, the molten alloy is prevented from flowing into the pore when the mold is closed for die casting, causing blockage of the pore or affecting the molding effect of the casting. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The present invention will be further described below in conjunction with the accompanying drawings.

[0025] Figure 1 It is the overall structural diagram of the present invention;

[0026] Figure 2 It is a front view structural diagram of the present invention;

[0027] Figure 3 It is a partial structural diagram of the present invention;

[0028] Figure 4 It is a local structure split diagram in the present invention;

[0029] Figure 5 It is a local structure cutaway view of the present invention. Figure 1 ;

[0030] Figure 6 The present invention Figure 5 Enlarged view of point A in the middle;

[0031] Figure 7 It is a local structure cutaway view of the present invention. Figure 2 ;

[0032] Figure 8 It is a partial front cross-sectional view in the present invention;

[0033] Fig. 9 It is a structural diagram of the pusher assembly and the air blowing assembly in the present invention;

[0034] Fig.10 It is a structural diagram of the air blowing assembly in the present invention;

[0035] In the figure: 1, machine table; 2, chassis; 3, hydraulic telescopic rod; 4, moving plate; 5, fixed plate; 6, injection assembly; 7, moving mold; 8, fixed mold; 9, ejector assembly; 91, ejector plate; 92, through groove; 93, through cavity; 94, ejector block; 95, ejector groove; 10, ejector assembly; 101, inner cavity; 102, built-in plate; 103, ejector column; 104, guide groove; 105, guide Column; 106, return spring; 11, blowing assembly; 111, air hole; 112, connecting groove; 113, air guide box; 114, air injection box; 115, connecting pipe; 116, air compressor; 117, air duct; 12, plugging assembly; 121, slot; 122, plug block; 123, top block; 124, plugging pin; 125, fixed block; 126, telescopic spring; 127, moving block. DETAILED DESCRIPTION

[0036] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0037] like Figures 1 to 10 As shown, a rapid die-casting process according to an embodiment of the present invention, the die-casting process steps are as follows:

[0038] S1: Check and clean the mold, install the mold in the die-casting equipment, use the die-casting equipment to melt the required alloy and maintain the appropriate temperature;

[0039] S2: Using die-casting equipment to close the mold to form a die-casting cavity, injecting the molten alloy into the pressure chamber of the die-casting equipment, and pressing the alloy into the die-casting cavity under high pressure to fill and form;

[0040] S3: Maintain a certain pressure in the mold to ensure the density of the casting, and allow the casting to cool and solidify in the mold;

[0041] S4: Use the die-casting equipment to open the mold, cooperate with the demoulding mechanism to push the casting out of the mold, take out the casting, and complete the die-casting.

[0042] like Figures 1 to 10As shown, the die-casting equipment includes a machine table 1, a chassis 2 is fixed on the top of the machine table 1, a movable plate 4 is arranged at the front end of the chassis 2, a hydraulic telescopic rod 3 is installed inside the chassis 2, the front end of the hydraulic telescopic rod 3 extends from the inside of the chassis 2 and is fixedly connected to the movable plate 4, a fixed plate 5 is arranged at the front end of the movable plate 4, the fixed plate 5 is fixed on the machine table 1, a movable mold 7 and a fixed mold 8 are arranged between the movable plate 4 and the fixed plate 5, the movable mold 7 is installed at the front of the movable plate 4, the fixed mold 8 is installed at the back of the fixed plate 5, and a shot assembly 6 is arranged at the front end of the fixed plate 5, and the shot assembly 6 is used to To fill the mold cavity with molten metal and provide the pressure required for die casting, a push assembly 10 is provided at the rear end of the movable mold 7, and the push assembly 10 is used to push the casting in the mold cavity. Push assemblies 9 are provided at the upper and lower ends of the push assembly 10, and the push assembly 9 is used to push the push assembly 10 to move. Blow assemblies 11 are provided at the upper and lower ends of the movable mold 7, and the blow assembly 11 is used to inflate the mold cavity. Sealing assemblies 12 are provided at the upper and lower ends of the front of the movable mold 7, and the sealing assembly 12 is used to seal the blowing assembly 11.

[0043] When the die-casting equipment is demolding, excessive adhesion will cause a large load on the push rod and related equipment. In addition, direct pushing of the casting will cause deformation of the casting or damage the mold cavity. Therefore, when the die-casting equipment is working, the required alloy is first melted by the injection assembly 6 to maintain a suitable temperature, and then the hydraulic telescopic rod 3 is used to push the movable plate 4 to drive the movable mold 7 to move toward the position of the fixed mold 8 to close the mold to form a die-casting cavity. After that, the injection assembly 6 is used to inject the molten alloy into the pressure chamber of the die-casting equipment, and the alloy is pressed into the die-casting cavity under high pressure to fill and shape it, so that a certain pressure is maintained in the mold to ensure that the casting is dense and the casting is cooled in the mold. But it solidifies. Finally, the hydraulic telescopic rod 3 is used to pull the movable plate 4 to drive the movable mold 7 away from the fixed mold 8 to open the mold, the sealing component 12 is used to open the hole groove, and the blowing component 11 is used to blow air to the casting in the cavity to reduce the adhesion between the casting and the inner wall of the cavity. The pushing component 9 is then used to push the pushing component 10 to push the casting formed in the movable mold 7 out of the mold. The casting is taken out to complete the die-casting operation. The adhesion between the casting and the inner wall of the cavity is reduced by blowing air, which avoids damage to the mold cavity and the casting body when the casting is directly pushed due to excessive adhesion. This not only improves the yield rate, but also helps to extend the service life of the mold.

[0044] like Figure 4 , Figure 5 , Figures 7 to 9As shown, the pusher assembly 10 includes an inner cavity 101 opened at the rear end of the movable mold 7, an inner cavity 101 is provided with an inner plate 102, a pusher column 103 is fixed to the front of the inner plate 102, and the front end of the pusher column 103 extends into the cavity in the movable mold 7, guide grooves 104 are provided on both sides of the inner plate 102, and a guide column 105 runs through the inner portion of the guide groove 104, and the guide column 105 is fixed in the inner cavity 101, and a return spring 106 is wound around the outer portion of the guide column 105, and the return spring 106 is placed at the front end of the inner plate 102, one end of the return spring 106 is fixedly connected to the inner plate 102, and the other end of the return spring 106 is fixedly connected to the inner wall of the inner cavity 101, the inner diameter of the guide groove 104 matches the outer diameter of the guide column 105, the inner plate 102 slides on the outer portion of the guide column 105 through the guide groove 104, and the inner plate 1 02 is moved by the pushing assembly 9; when the movable mold 7 and the fixed mold 8 are moved away from each other to open the mold, the pushing assembly 9 is used to push the built-in plate 102 to move, and the built-in plate 102 drives the pushing column 103 to gradually move into the cavity in the movable mold 7, and the pushing column 103 gradually pushes out the casting in the cavity of the movable mold 7. When the built-in plate 102 moves, it will slide on the outside of the guide column 105 through the guide groove 104 and squeeze the return spring 106 to contract. The guide groove 104 and the guide column 105 can guide the movement of the built-in plate 102 and make it move in the horizontal direction. When the movable mold 7 and the fixed mold 8 are close to each other to close the mold, the pushing assembly 9 gradually loses its effect on the built-in plate 102, and the elastic force of the return spring 106 is used to push the built-in plate 102 back to the initial position, and the pushing column 103 is also gradually moved out of the cavity in the movable mold 7.

[0045] like Figure 4 , Figure 5 , Figures 7 to 9As shown, the push assembly 9 includes a through cavity 93 opened at the upper and lower ends of the movable mold 7, the through cavity 93 is connected to the inside of the inner cavity 101, and the upper and lower ends of the built-in plate 102 are fixed with push blocks 94, the push blocks 94 extend from the through cavity 93, and the back of the push block 94 is fixed with a push groove 95. The upper and lower ends of the movable plate 4 are provided with through grooves 92, and the positions of the through grooves 92 and the push grooves 95 are exactly corresponding. The upper and lower ends of the front of the chassis 2 are fixed with push plates 91, and the positions of the push plates 91 and the through grooves 92 and the push grooves 95 are exactly corresponding. The push plates 91 can pass through the through grooves 92 and be inserted into the push grooves 95, and the push blocks 94 can move horizontally in the through cavity 93; When the hydraulic telescopic rod 3 is used to pull the movable plate 4 to drive the movable mold 7 away from the fixed mold 8 to open the mold, the movable plate 4 drives the movable mold 7 to move toward the position of the chassis 2, and the push plate 91 gradually moves into the through groove 92, and is inserted into the push groove 95 opened on the back of the push block 94 through the through groove 92. The push plate 91 gradually pushes the push block 94 to move forward in the through cavity 93. When the hydraulic telescopic rod 3 is used to push the movable plate 4 to drive the movable mold 7 close to the fixed mold 8 to close the mold, the movable plate 4 and the movable mold 7 gradually move away from the chassis 2, and the push plate 91 gradually moves out of the push groove 95 on the back of the push block 94 and disengages from the through groove 92, and the push block 94 gradually loses the pressure of the push plate 91.

[0046] like Figures 5 to 10 As shown, the blowing assembly 11 includes a connecting groove 112 opened at the upper and lower ends of the movable mold 7, an air hole 111 is opened at one end of the connecting groove 112, and the air hole 111 is connected to the cavity inside the movable mold 7. The upper and lower ends of the movable mold 7 are installed with air guide boxes 113, and the interior of the air guide box 113 is connected to the connecting groove 112. The side wall of the movable mold 7 is fixed with an air injection box 114, and the upper and lower ends of the air injection box 114 are connected to a connecting pipe 115, and the other end of the connecting pipe 115 is connected to the air guide box 113. One side of the air injection box 114 is connected to an air duct 117, and one end of the air duct 117 is connected to an air compressor 116. The air compressor 116 is installed on the side wall of the machine 1, and the air hole 111 is connected to the connecting The number of grooves 112 is the same, and the air holes 111 and the connecting grooves 112 are evenly spaced at the upper and lower ends inside the movable mold 7; when the mold is gradually opened, the air compressor 116 is started, and the air compressor 116 is used to continuously inject high-speed gas into the gas injection box 114 through the air duct 117. The high-speed gas is introduced into the connecting pipe 115 through the gas injection box 114, and the high-speed gas is injected into the air guide box 113 by the connecting pipe 115, and then injected into the connecting groove 112 by the air guide box 113, and finally the high-speed gas is injected into the air hole 111 by the connecting groove 112, and then the high-speed gas is blown into the mold cavity by the air hole 111, and the gas acts between the cavity and the casting to reduce the adhesion of the casting, so that the casting can be demolded more easily.

[0047] like Figures 5 to 10As shown, the plugging assembly 12 includes slots 121 opened at the upper and lower ends of the movable mold 7, the slot 121 is located at the bottom end of the air hole 111 and is connected to the air hole 111, a plugging pin 124 is arranged inside the slot 121, the top of the plugging pin 124 extends into the air hole 111, a moving block 127 is fixed to the outside of the plugging pin 124, the top of the moving block 127 is in contact with the inner wall of the slot 121, a fixed block 125 is arranged at the bottom end of the moving block 127, the bottom end of the plugging pin 124 passes through the fixed block 125, the fixed block 125 is fixed in the slot 121, a telescopic spring 126 is fixed on the top of the fixed block 125, and the telescopic spring 126 is fixed to the top of the fixed block 125. 6 is fixedly connected with the moving block 127, the telescopic spring 126 is wound around the outside of the blocking pin 124, the upper and lower ends of the back of the fixed mold 8 are fixed with plug blocks 122, the ends of the plug blocks 122 are fixed with top blocks 123, the top blocks 123 are located at the bottom of the blocking pin 124, the end of the top block 123 is an inclined end surface, and the inclined end surface of the top block 123 can shovel up the bottom of the blocking pin 124; when the hydraulic telescopic rod 3 is used to push the moving plate 4 to drive the moving mold 7 to move toward the position of the fixed mold 8 to close the mold, the plug blocks 122 at the upper and lower ends of the back of the fixed mold 8 and the top blocks 123 at their ends are gradually moved into the slots 121, and the top blocks 123 The inclined end surface of the plugging pin 124 scoops up the bottom of the plugging pin 124 to move the plugging pin 124 upward. When the bottom of the plugging pin 124 contacts the top of the top block 123, the top of the moving block 127 contacts the top of the slot 121 tightly, and the top of the plugging pin 124 moves into the air hole 111 to block the air hole 111. At the same time, the upwardly moved plugging pin 124 drives the moving block 127 to move upward to pull the telescopic spring 126 to extend. When the hydraulic telescopic rod 3 is used to pull the moving plate 4 to drive the moving mold 7 away from the fixed mold 8 to open the mold, the plug blocks 122 at the upper and lower ends of the back of the fixed mold 8 and the top blocks 123 at their ends are gradually moved out of the slot 121, and the plugging pin 124 Without the thrust of the top block 123, under the elastic force of the telescopic spring 126, the telescopic spring 126 drives the blocking pin 124 to move out from the inside of the pore 111 by pulling the movable block 127 to open the pore 111. When the mold is closed to inject the alloy, the end of the blocking pin 124 moves into the pore 111 to block the pore 111 and close it. When the mold is opened, the end of the blocking pin 124 moves out of the pore 111 to open the pore 111. By blocking the pore 111, the molten alloy is prevented from flowing into the pore 111 when the mold is closed for die casting, causing the pore 111 to be blocked or affecting the molding effect of the casting.

[0048] Working principle: First, use the injection assembly 6 to melt the required alloy and maintain a suitable temperature. Then use the hydraulic telescopic rod 3 to push the movable plate 4 to drive the movable mold 7 to move toward the position of the fixed mold 8 to close the mold and form a die-casting cavity. When the movable mold 7 moves toward the position of the fixed mold 8 to close the mold, the plug blocks 122 at the upper and lower ends of the back of the fixed mold 8 and the top block 123 at its end gradually move into the slot 121, and the inclined end surface of the top block 123 shovels the bottom of the blocking pin 124 to move the blocking pin 124 upward. When the bottom of the blocking pin 124 conflicts with the top of the top block 123, the top of the moving block 127 tightly conflicts with the top of the slot 121, and the top of the blocking pin 124 moves into the air hole 111 to block the air hole 111. At the same time, the upward moving blocking pin 124 drives the moving block 127 to move upward to pull the telescopic spring 126 to extend;

[0049] Afterwards, the molten alloy is injected into the pressure chamber of the die-casting equipment by using the injection assembly 6, and the alloy is pressed into the die-casting cavity under high pressure to fill and form, so that a certain pressure is maintained in the mold to ensure the density of the casting, and the casting is allowed to cool and solidify in the mold. Finally, the hydraulic telescopic rod 3 is used to pull the movable plate 4 to drive the movable mold 7 away from the fixed mold 8 to open the mold. When the movable mold 7 is away from the fixed mold 8 to open the mold, the insert blocks 122 at the upper and lower ends of the back of the fixed mold 8 and the top blocks 123 at its ends are gradually moved out of the slots 121, and the blocking pin 124 loses the thrust of the top block 123. Under the elastic force of the telescopic spring 126, the telescopic spring 126 drives the blocking pin 124 to move by pulling the movable block 127 The pin 124 is moved out from the inside of the air hole 111 to open the air hole 111. When the air hole 111 is opened, the air compressor 116 is started, and the air compressor 116 is used to continuously inject high-speed gas into the air injection box 114 through the air duct 117. The high-speed gas is introduced into the connecting pipe 115 through the air injection box 114, and the high-speed gas is injected into the air guide box 113 by the connecting pipe 115, and then injected into the connecting groove 112 by the air guide box 113, and finally the high-speed gas is injected into the air hole 111 by the connecting groove 112, and then the high-speed gas is blown into the mold cavity by the air hole 111, and the gas acts between the mold cavity and the casting to reduce the adhesion of the casting, so that the casting can be demolded more easily;

[0050] When the hydraulic telescopic rod 3 is used to pull the movable plate 4 to drive the movable mold 7 away from the fixed mold 8 to open the mold, the movable plate 4 drives the movable mold 7 to move toward the position of the chassis 2, and the push plate 91 gradually moves into the through groove 92, and is inserted into the push groove 95 opened on the back of the push block 94 through the through groove 92, and the push plate 91 gradually pushes the push block 94 to move forward in the through cavity 93, and drives the built-in plate 102 to move by pushing the push block 94 to move, and the movable built-in plate 102 slides on the outside of the guide column 105 through the guide groove 104 and squeezes the return spring 106 to contract, and the movable built-in plate 102 drives the push column 103 to gradually move into the cavity in the movable mold 7, and the push column 103 gradually pushes out the casting in the cavity of the movable mold 7, thereby completing the casting push-out operation;

[0051] When the hydraulic telescopic rod 3 is used to push the movable plate 4 to drive the movable mold 7 to move toward the fixed mold 8 so that the mold is closed to form a die-casting cavity, the push assembly 9 gradually loses its effect on the inner plate 102, and the elastic force of the return spring 106 is used to push the inner plate 102 back to the initial position, and the push column 103 is also gradually moved out of the cavity in the movable mold 7;

[0052] By moving the movable mold 7, the push block 94 is brought into contact with the push plate 91, so that the push plate 91 pushes the push blocks 94 at the upper and lower ends of the built-in plate 102 to drive the built-in plate 102 to move, so that the push column 103 at the front of the built-in plate 102 moves into the cavity in the movable mold 7 to push the molded casting out for demolding operation, and the air compressor 116 is used to generate compressed gas and inject it into the cavity through the air hole 111, and the gas is used to act between the cavity and the casting to reduce the adhesion between the casting and the cavity. After reducing the adhesion, the thrust required by the push plate 91 is reduced, making demolding easier. Moreover, the adhesion between the casting and the inner wall of the cavity is reduced by blowing air to avoid damage to the mold cavity and the casting body when the casting is directly pushed due to excessive adhesion. This not only improves the yield rate, but also helps to extend the service life of the mold.

[0053] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A die-casting device, characterized in that: The die-casting equipment comprises a machine platform (1), a machine box (2) is fixed on the top of the machine platform (1), a movable plate (4) is arranged at the front end of the machine box (2), a hydraulic telescopic rod (3) is installed inside the machine box (2), the front end of the hydraulic telescopic rod (3) extends from the inside of the machine box (2) and is fixedly connected to the movable plate (4), a fixed plate (5) is arranged at the front end of the movable plate (4), the fixed plate (5) is fixed on the machine platform (1), a movable mold (7) and a fixed mold (8) are arranged between the movable plate (4) and the fixed plate (5), the movable mold (7) is installed at the front of the movable plate (4), the fixed mold (8) is installed at the back of the fixed plate (5), and a shot assembly (6) is arranged at the front end of the fixed plate (5) , the injection assembly (6) is used to fill the metal liquid into the mold cavity and provide the pressure required for die casting, the rear end of the movable mold (7) is provided with a push assembly (10), the push assembly (10) is used to push the casting in the mold cavity, the upper and lower ends of the push assembly (10) are provided with push assemblies (9), the push assemblies (9) are used to push the push assembly (10) to move, the upper and lower ends of the movable mold (7) are provided with blowing assemblies (11), the blowing assembly (11) is used to blow air into the mold cavity, and the upper and lower ends of the front of the movable mold (7) are provided with blocking assemblies (12), the blocking assembly (12) is used to block the blowing assembly (11); The air blowing assembly (11) comprises a connecting groove (112) provided at the upper and lower ends of the movable mold (7); an air hole (111) is provided at one end of the connecting groove (112); the air hole (111) is connected to the mold cavity inside the movable mold (7); air guide boxes (113) are installed at the upper and lower ends of the movable mold (7); the interior of the air guide box (113) is connected to the connecting groove (112); an air injection box (114) is fixed to the side wall of the movable mold (7); the upper and lower ends of the air injection box (114) are connected to connecting pipes (115); the other end of the connecting pipe (115) is connected to the air guide box (113); one side of the air injection box (114) is connected to an air duct (117); one end of the air duct (117) is connected to an air compressor (116); the air compressor (116) is installed on the side wall of the machine (1); The number of the air holes (111) and the connecting grooves (112) is the same, and the air holes (111) and the connecting grooves (112) are evenly spaced at the upper and lower ends of the movable mold (7); The plugging component (12) comprises slots (121) provided at the upper and lower ends of the movable mold (7), the slot (121) being located at the bottom end of the air hole (111) and being connected to the air hole (111), a plugging pin (124) being arranged inside the slot (121), the top end of the plugging pin (124) extending into the air hole (111), a moving block (127) being fixed outside the plugging pin (124), the top of the moving block (127) being in contact with the inner wall of the slot (121), a fixed block (125) being arranged at the bottom end of the moving block (127), and the sealing The bottom end of the blocking pin (124) passes through the fixed block (125), the fixed block (125) is fixed in the slot (121), a telescopic spring (126) is fixed on the top of the fixed block (125), the top of the telescopic spring (126) is fixedly connected to the moving block (127), the telescopic spring (126) is wound around the outside of the blocking pin (124), the upper and lower ends of the back of the fixed mold (8) are fixed with plug blocks (122), the end of the plug block (122) is fixed with a top block (123), and the top block (123) is located at the bottom of the blocking pin (124); The end of the top block (123) is an inclined end surface, and the inclined end surface of the top block (123) can scoop up the bottom of the blocking pin (124).

2. A die-casting device according to claim 1, characterized in that: The pusher assembly (10) comprises an inner cavity (101) opened at the rear end of the movable mold (7), an inner plate (102) is arranged inside the inner cavity (101), a pusher column (103) is fixed at the front of the inner plate (102), the front end of the pusher column (103) extends into the cavity in the movable mold (7), guide grooves (104) are formed on both sides of the inner plate (102), a guide column (105) passes through the guide groove (104), the guide column (105) is fixed in the inner cavity (101), a return spring (106) is wound around the outside of the guide column (105), the return spring (106) is placed at the front end of the inner plate (102), one end of the return spring (106) is fixedly connected to the inner plate (102), and the other end of the return spring (106) is fixedly connected to the inner wall of the inner cavity (101).

3. A die-casting device according to claim 2, characterized in that: The inner diameter of the guide groove (104) matches the outer diameter of the guide column (105), and the built-in plate (102) slides outside the guide column (105) through the guide groove (104).

4. A die-casting device according to claim 3, characterized in that: The push assembly (9) comprises a through cavity (93) provided at the upper and lower ends of the movable mold (7), the through cavity (93) being connected to the interior of the inner cavity (101), push blocks (94) being fixed at the upper and lower ends of the built-in plate (102), the push block (94) extending out from the through cavity (93), a push groove (95) being fixed at the back of the push block (94), through grooves (92) being provided at the upper and lower ends of the interior of the movable plate (4), the positions of the through grooves (92) and the push grooves (95) being exactly corresponding, and push plates (91) being fixed at the upper and lower ends of the front of the chassis (2), the positions of the push plates (91) and the through grooves (92) and the push grooves (95) being exactly corresponding.

5. A die-casting device according to claim 4, characterized in that: The push plate (91) can pass through the through groove (92) and be inserted into the push groove (95), and the push block (94) can move horizontally in the through cavity (93).

Citation Information

Patent Citations

  • Die casting equipment

    CN218785178U

  • Air ejection rapid demolding device for injection mold production

    CN113021797A

  • Rapid forming die-casting machine

    CN115194122A

  • Aluminum alloy product die-casting forming device and technology

    CN116571709A