Device packaging structure and manufacturing method thereof, radio frequency chip module, and electronic equipment
By using sealant in chip-scale packaging to form a cavity structure with close characteristics to the chip die, the problem of solder ball cracking is solved, device performance and isolation are improved, and device miniaturization is achieved.
Patent Information
- Application Number
- CN202410641923.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-23
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-05-23
AI Technical Summary
In chip-scale packaging, the solder ball of the filter is easy to crack, which affects the performance of the device. This is mainly due to the large difference in thermal expansion coefficient between the filter wafer and the organic film, which leads to increased stress in extreme environments and affects the stability of the solder ball. sex.
A cavity structure is formed between the sealant and the bare chip. The material properties of the sealant are close to or the same as those of the bare chip, which reduces the difference in material properties and avoids the generation of stress. Micron-level precision sealing is achieved through the dispensing process and reduces the cost of welding. Possibility of stressing the ball.
It effectively avoids solder ball cracking, improves the performance and isolation of the device packaging structure, and achieves device miniaturization and performance improvement.
Smart Images

Figure CN118231359B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of terminal equipment, and in particular to a device packaging structure and a manufacturing method thereof, a radio frequency chip module, and an electronic device. Background Art
[0002] Electronic devices include RF chip modules to achieve wireless communication. RF chip modules include devices such as filters, low-noise amplifiers, power amplifiers, and RF switches. For filters, the filters include a cavity structure to provide vibration space for sound waves. At present, when the filter is packaged using the chip scale package (CSP) packaging process, the filter wafer is soldered to the substrate through solder balls, and a layer of organic film is covered on the surface of the filter wafer to form a cavity structure; then it is packaged with epoxy molding compound (EMC) material.
[0003] However, in CSP packaging, the filter wafer is in direct contact with the organic film, and the thermal expansion coefficient of the organic film is usually between 80 and 170 × 10 -6 / ℃, while the thermal expansion constant of the filter wafer is usually between 4~10×10 -6 / ℃ range. Due to the large difference in thermal expansion coefficients between the filter wafer and the organic film, solder balls are prone to cracking in extreme environments (such as hot and cold cycle tests), affecting device performance. Summary of the invention
[0004] The present application provides a device packaging structure and a manufacturing method thereof, a radio frequency chip module, and an electronic device to solve the problem that the existing packaging method easily causes solder balls to crack and affects device performance.
[0005] In a first aspect, the present application provides a device packaging structure, including: a substrate, a chip bare crystal and a sealant. The substrate includes a first surface, the chip bare crystal includes a plurality of solder balls, the chip bare crystal is soldered to the first surface through the plurality of solder balls, and there is a gap between the chip bare crystal and the substrate; a sealant ring is arranged around the gap to seal the gap, and forms a cavity with the substrate and the chip bare crystal; the material properties of the sealant and the material properties of the chip bare crystal satisfy a first relationship.
[0006] The device packaging structure provided in the embodiment of the present application uses a sealant to form the cavity required by the device packaging structure, and the sealant has a good contact coupling effect with the chip bare crystal. The material properties of the sealant are the same or close to the material properties of the chip bare crystal, and there will be no difference in material properties after the two are coupled, or the difference in material properties is small, thereby avoiding the performance of the device packaging structure being affected by the large difference in material properties.
[0007] In some implementations, the material property includes a thermal expansion coefficient; the first relationship includes an absolute value of a difference between a thermal expansion coefficient of the sealant and a thermal expansion coefficient of the chip die being less than or equal to a first threshold; the first threshold being 20×10 -6 / ℃. In this way, the difference in thermal expansion coefficients between the sealant and the chip bare die is small or non-existent, so that no stress or small stress is generated between the two after coupling. In this way, the solder balls are not subjected to stress or are subjected to small stress, so that the solder balls will not crack, thereby improving the performance of the device packaging structure.
[0008] In some implementations, the material property includes a dielectric constant; the first relationship includes a first ratio between the dielectric constant of the sealant and the dielectric constant of the chip die; the first ratio ranges from 0.75 to 1.5. In this way, the dielectric constants of the chip die and the sealant are both low and close to or the same, and the relative dielectric constants of the two after coupling are still low, so that the parasitic capacitance of the device packaging structure is reduced, so as to improve the isolation between different frequency bands, so that the filtering frequency bands do not interfere with each other, so as to improve the filtering accuracy.
[0009] In some implementations, a sealant ring is provided on the side surface of the chip die and extends to the first surface of the substrate to seal the gap; an angle is formed between the side surface and the first surface. In this way, the sealant is formed around the chip die in a semi-covering manner, and while forming a cavity, the contact area between the sealant and the chip die can be ensured, so as to ensure that the coupling effect between the sealant and the chip die meets the requirements.
[0010] In some implementations, the sealant covers the second surface and the side surface of the chip die and extends to the first surface of the substrate to seal the gap; the second surface is the surface of the chip die that is opposite to the first surface, and the side surface is connected to the second surface. In this way, the sealant is formed around the chip die in a full-coverage manner, and while forming a cavity, the contact area between the sealant and the chip die can be increased to further improve the coupling effect between the sealant and the chip die.
[0011] In some implementations, the material property includes a thermal expansion coefficient and a dielectric constant; the sealant includes a first sealant and a second sealant; the first relationship includes that a difference between a thermal expansion coefficient of the first sealant and a thermal expansion coefficient of the chip die is less than or equal to a first threshold, and the first threshold is 20×10 -6 / ℃, and the dielectric constant of the second sealant has a first ratio to the dielectric constant of the chip bare crystal, and the value range of the first ratio is 0.75~1.5; the chip bare crystal includes a side surface and a second surface connected to each other, and the second surface is the surface of the chip bare crystal facing away from the first surface; one of the first sealant and the second sealant is arranged on the side surface and extends to the first surface of the substrate to seal the gap; the other of the first sealant and the second sealant covers the second surface; the first sealant and the second sealant are connected. In this way, the device packaging structure can avoid cracking of solder balls, and can also realize miniaturization of devices, and can even improve isolation to ensure the performance of the device packaging structure.
[0012] In some implementations, one of the first sealant and the second sealant used to cover the second surface extends from the second surface along the outer surface of the other of the first sealant and the second sealant to the first surface of the substrate. In this way, the chip bare die and the first sealant are wrapped with the second sealant, which can improve reliability.
[0013] In some implementations, it also includes: an inner shielding layer; the inner shielding layer covers the first outer surface of the sealant and extends to the first surface of the substrate. In this way, the device packaging structure itself has an independent separation function, avoiding mutual interference when it is packaged with other device packaging structures into the RF chip module, thereby reducing the volume of the RF chip module.
[0014] In some implementations, the device further includes: a plastic encapsulation layer; the plastic encapsulation layer covers the second outer surface of the inner shielding layer and the first surface of the substrate. In this way, the plastic encapsulation layer can ensure the functional stability of the device packaging structure.
[0015] In some implementations, the method further includes: a protective adhesive covering the second outer surface of the inner shielding layer, so that the inner shielding layer can be protected by the protective adhesive to avoid damage to the inner shielding layer when the plastic sealing layer is formed by compression molding.
[0016] In some implementations, the device further includes: a plastic encapsulation layer; the plastic encapsulation layer covers the fourth outer surface of the protective glue and the first surface of the substrate. In this way, the plastic encapsulation layer can ensure the functional stability of the device packaging structure.
[0017] In some implementations, it further includes: an outer shielding layer; the outer shielding layer covers the third outer surface of the plastic packaging layer and the first surface of the substrate. In this way, the outer shielding layer can be used to isolate the RF chip module from other modules in the electronic device to avoid mutual interference between the modules.
[0018] In a second aspect, the present application also provides a method for manufacturing a device packaging structure, the method comprising: providing a chip bare crystal and a substrate, the substrate comprising a first surface; coating a plurality of solder balls on one surface of the chip bare crystal to obtain a semi-packaged structure; placing the semi-packaged structure upside down on the first surface of the substrate, the chip bare crystal being welded to the substrate via the solder balls, and a gap being provided between the chip bare crystal and the substrate; using a dispensing process to dispense sealant around the gap to seal the gap, and the sealant, the chip bare crystal and the substrate form a cavity.
[0019] The manufacturing method of the device packaging structure provided in the embodiment of the present application utilizes the micron-level precision characteristics of the dispensing process to make the width of the sealant less than 100μm, and the sealant can seal the gap in a small area, which can achieve the miniaturization of the device. The sealant is used to form the cavity required for the device packaging structure. Based on the low fluidity and low thermal expansion coefficient of the sealant, contamination of the resonator and cracking of the solder balls can be avoided. Based on the low dielectric constant of the sealant, the parasitic capacitance of the device packaging structure is reduced to improve the isolation between different frequency bands, so that the filtering frequency bands do not interfere with each other, thereby improving the filtering accuracy. In this way, the performance of the device packaging structure can be improved.
[0020] In a third aspect, the present application provides a radio frequency chip module, including a main substrate, and a plurality of device packaging structures provided in the first aspect; the plurality of device packaging structures are spaced apart and located on the surface of the main substrate.
[0021] In a fourth aspect, the present application provides an electronic device, comprising the radio frequency chip module provided in the third aspect.
[0022] It can be understood that the RF chip modules and electronic devices provided in the above-mentioned aspects are all applied to the device packaging structure provided above. Therefore, the beneficial effects that can be achieved can refer to the beneficial effects in the device packaging structure provided above, and will not be repeated here. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to more clearly illustrate the technical solution of the present application, the drawings required for use in the embodiments are briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0024] Figure 1 is a schematic diagram of the structure of an electronic device provided in an embodiment of the present application;
[0025] Figure 2 It is a structural diagram of a radio frequency front-end module;
[0026] Figure 3 It is a schematic diagram of the structure of a packaged device;
[0027] Figure 4 yes Figure 3 The first structural diagram of the AA section;
[0028] Figure 5 yes Figure 3 The second structural diagram of the AA section;
[0029] Figure 6 This is a first structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0030] Figure 7 is a process flow chart of a method for manufacturing a device packaging structure provided in an embodiment of the present application;
[0031] Figure 8 is a second structural schematic diagram of the device packaging structure provided in an embodiment of the present application;
[0032] Fig. 9 is a third structural schematic diagram of the device packaging structure provided in an embodiment of the present application;
[0033] Fig.10 is a fourth structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0034] Fig.11 is a fifth structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0035] Fig.12 is a sixth structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0036] Fig.13 is a seventh structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0037] Fig.14 This is an eighth structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0038] Fig.15 is a ninth structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0039] Fig.16 is the tenth structural schematic diagram of the device packaging structure provided in the embodiment of the present application;
[0040] Fig.17 is an eleventh structural schematic diagram of a device packaging structure provided in an embodiment of the present application;
[0041] Fig.18 This is a first structural diagram of a radio frequency chip module provided in an embodiment of the present application;
[0042] Fig.19This is a second structural diagram of the RF chip module provided in an embodiment of the present application.
[0043] Illustration Description:
[0044] 10-display screen, 20-middle frame, 30-RF front-end module, 31-filter, 311-device wafer, 312-resonance unit, 313-solder ball, 314-plastic package, 315-organic film, 316-cavity structure, 317-side wall structure, 318-top structure, 319-copper column, 32-low noise amplifier, 33-power amplifier, 34-RF switch, 35-isolator, 40-PCB substrate, 100-substrate, 101-first surface, 102-routing, 200-chip bare crystal, 201 -solder ball, 202-side surface, 203-second surface, 204-resonator, 300-sealant, 301-first sealant, 302-second sealant, 303-first outer surface, 400-cavity, 500-inner shielding layer, 501-second outer surface, 502-first connection end, 600-plastic sealing layer, 601-third outer surface, 700-protective glue, 701-fourth outer surface, 800-outer shielding layer, 801-second connection end, 50-RF chip module, 51-main substrate, 52-device packaging structure. DETAILED DESCRIPTION
[0045] The technical solutions in the embodiments of the present application will be described clearly below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments of the present application, other embodiments obtained by ordinary technicians in this field without making creative work all belong to the protection scope of the present application.
[0046] In the description of this application, the terms "first", "second", etc. are used for descriptive purposes only and are not to be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the feature. In the description of this application, unless otherwise specified, "plurality" means two or more.
[0047] In addition, in the present application, directional terms such as "upper" and "lower" are defined relative to the orientation of the components in the drawings. It should be understood that these directional terms are relative concepts. They are used for relative description and clarification, and they can change accordingly according to the changes in the orientation of the components in the drawings.
[0048] The professional terms mentioned in the embodiments of the present application are explained below to facilitate understanding by those skilled in the art.
[0049] Chip Scale Package (CSP): CSP packaging is a memory chip packaging technology that realizes the electrical interconnection between the chip and the substrate by flip-chip bonding of bumps to the substrate, with the chip facing down and the chip soldering area directly interconnected with the substrate soldering area. CSP packaging can make the ratio of chip area to package area not exceed 1:1.2.
[0050] Wafer Level Package (WLP): WLP packaging technology can package the chip while it is still on the wafer. It has the advantages of small size, excellent electrical performance, good heat dissipation and low cost.
[0051] Epoxy Molding Compound (EMC): Also known as epoxy resin molding compound, it is a thermosetting chemical material used for semiconductor packaging. EMC is a key material to ensure the stable function of the chip. EMC is made of epoxy resin as the base resin, high-performance phenolic resin as the curing agent, silicon micropowder and other fillers, and a variety of additives. Its main function is to protect semiconductor chips from the influence of the external environment (water vapor, temperature, pollution, etc.), and to achieve composite functions such as thermal conductivity, insulation, moisture resistance, pressure resistance, and support.
[0052] The electronic device described in the embodiments of the present application includes but is not limited to a mobile phone, a notebook computer, a tablet computer, a laptop computer, a personal digital assistant or a wearable device, etc. The following description is made by taking the electronic device as a mobile phone.
[0053] Figure 1 It is a schematic diagram of the structure of an electronic device provided in an embodiment of the present application.
[0054] like Figure 1 As shown, the electronic device may include a display screen 10, a middle frame 20 and a rear shell, wherein the display screen 10 and the rear shell are located on opposite sides of the middle frame 20, and the display screen 10, the middle frame 20 and the rear shell are buckled together in sequence to form a whole machine cavity. Among them, the whole machine cavity includes components such as a communication module, a circuit board, a battery, a speaker assembly and a camera assembly, which are not listed here one by one.
[0055] The communication module is mainly composed of antenna, RF front-end module, RF transceiver module, baseband signal processing, etc. The RF front-end module is between the antenna and the RF transceiver module, and is the core of wireless communication.
[0056] To facilitate the explanation of the positions of various components in an electronic device, the embodiment of the present application exemplarily establishes a three-dimensional coordinate system based on the electronic device, wherein the x-axis direction is the width direction of the electronic device, the y-axis direction is the length direction of the electronic device, and the z-axis direction is the thickness direction of the electronic device.
[0057] Figure 2 It is a structural diagram of a radio frequency front-end module.
[0058] like Figure 2 As shown, the RF front-end module 30 mainly includes: a filter (Filter) 31, a low noise amplifier (Low Noise Amplifier, LNA) 32, a power amplifier (Power Amplifier, PA) 33 and a RF switch (RF Switch) 34.
[0059] As a key component of the RF front-end module 30, the filter 31 can filter out-of-band interference and noise to retain the signal within a specific frequency band and meet the communication requirements of electronic equipment. The filter 31 includes a surface acoustic wave filter (SAW filter), a solid-mounted film bulk acoustic wave filter (SMR Bulk Acoustic Wave Filter) and a film cavity resonator filter (FBAR).
[0060] The low noise amplifier 32 is a circuit for amplifying weak signals. Its main function is to receive the signal from the antenna, process it through the amplifier, and then send it to the next stage circuit for processing.
[0061] The power amplifier 33 is used to increase the amplitude, power output or driving capability of the radio frequency signal. Generally speaking, the power amplifier 33 is located near the system antenna to provide a high-power signal to the transmitting antenna.
[0062] The radio frequency switch 34 is a common device in radio frequency circuits, and is used to implement switching between different signal paths, including switching between reception and transmission, different frequency bands, and different antennas.
[0063] The above-mentioned devices are integrated into the RF front-end module 30 after device packaging, and the packaging method includes CSP packaging or WLP packaging.
[0064] Figure 3 It is a schematic diagram of the structure of a packaged device; Figure 4 yes Figure 3 The first structural diagram of the AA section. Figure 4 The structure of a device using CSP packaging is shown.
[0065] like Figure 3 and Figure 4 As shown, taking the packaged device as a filter 31 as an example, the filter 31 generally includes a cavity structure 316, and the cavity structure 316 is used to provide a vibration space for the sound wave when the filter 31 converts the electromagnetic wave into the sound wave.
[0066] When the cavity structure 316 is manufactured by adopting the CSP packaging process, the filter 31 includes a device wafer 311 , a resonance unit 312 , solder balls 313 , a plastic package 314 and an organic film 315 .
[0067] Based on the CSP packaging technology, a plurality of resonant units 312 are arranged on a surface of a device wafer 311, and a plurality of solder balls 313 are made around the edges of the surface of the device wafer 311. Then, the device wafer 311 is soldered to a printed circuit board (PCB) substrate 40 in a flip-chip form through the solder balls 313.
[0068] An organic film 315 is covered on the outer surface of the device wafer 311. The organic film 315 extends to the surface of the PCB substrate 40, so as to form a cavity structure 316 between the device wafer 311 and the PCB substrate 40 by utilizing the height of the solder ball 313. A plurality of resonant units 312 are located in the cavity structure 316, and are used to maintain the vibration of the sound waves in the cavity when the filter 31 converts the electromagnetic waves into sound waves. Finally, EMC materials are used for injection molding to form a plastic package 314 on the outer surface of the organic film 315 and the surface of the PCB substrate 40 to obtain the filter 31. When the lamination process is used to form the cavity structure 316 required for the filter 31, the width W of the organic film 315 is 315 Above 150μm-200μm.
[0069] However, under CSP packaging, the device wafer 311 is in direct contact with the organic film 315. The organic film 315 is made of organic materials, and the thermal expansion coefficient (hereinafter referred to as CTE coefficient) of the organic film 315 is usually 80~170×10 -6 / ℃ range; the device wafer 311 is made of piezoelectric material, and the CTE coefficient of the device wafer 311 is usually between 4 and 10×10 -6 / ℃ range. When the module size is large, it is easy to produce large stress between the two due to the large difference in CTE coefficients in extreme environments (such as hot and cold cycle tests). Due to the existence of the cavity structure 316, large stress acts on the solder ball 313, causing the solder ball 313 to crack, affecting the performance of the filter 31.
[0070] Figure 5 yes Figure 3 The second structural diagram of the AA section. Figure 5 The structure of a device packaged with WLP is shown.
[0071] like Figure 5As shown, when the WLP packaging process is used to manufacture the cavity structure 316 , the filter 31 includes a device wafer 311 , a resonant unit 312 , a solder ball 313 , a plastic package 314 , a side wall structure (wall) 317 , a roof structure (roof) 318 and a copper pillar (CuP) 319 .
[0072] Based on the WLP packaging technology, multiple resonant units 312 are arranged on a surface of the device wafer 311, and multiple sidewall structures 317 and capping structures 318 are prefabricated on the surface. Multiple sidewall structures 317 are arranged at intervals on the surface of the device wafer 311, and the capping structure 318 is connected to one end of the multiple sidewall structures 317 away from the device wafer 311, so that multiple independent cavity structures 316 are surrounded by the device wafer 311, two adjacent sidewall structures 317 and the capping structure 318, and each cavity structure 316 includes at least one resonant unit 312. Among them, the sidewall structure 317 and the capping structure 318 can be made of organic materials, such as resin.
[0073] A copper pillar 319 is arranged in the side wall structure 317, one end of the copper pillar 319 is connected to the device wafer 311, and the other end is passed through the capping structure 318. A solder ball 313 is pre-set at the other end of the copper pillar 319. EMC material is used for injection molding to cover the outer surface of the device wafer 311, the outer surface of the side wall structure 317 and the outer surface of the capping structure 318 to form a plastic package 314, and the solder ball 313 is exposed from the surface of the plastic package 314. Finally, the above-mentioned combination is welded to the PCB substrate 40 using the solder ball 313 to obtain the filter 31. Among them, the device wafer 311 is electrically connected to the PCB substrate 40 through the copper pillar 319.
[0074] When the WLP packaging process is used to make the cavity structure 316 in the filter 31, although this process does not use the organic film 315, it can solve the problem of cracking of the solder ball 313 after temperature cycling. However, the WLP packaging process is complicated and costly, and the packaged filter 31 includes a side wall structure 317 and a capping structure 318, which results in a larger size of the filter 31, which is not conducive to miniaturization.
[0075] In addition, since the filter 31 usually uses multiple passbands to implement filtering in different frequency bands, there needs to be a gap between each passband to avoid mutual influence. Therefore, the filter 31 needs to have a certain degree of isolation to avoid the passbands from being close to each other and affecting each other, resulting in inaccurate filtering frequency bands, and further resulting in inaccurate filtering results.
[0076] The relative dielectric constant (or dielectric constant for short) Er of the device wafer 311 is relatively low, about 2.8~3.6 F / m, and the relative dielectric constant Er of the organic film 315 and the EMC material is high, about 10F / m. Under the CSP package, the device wafer 311 is in direct contact with the organic film 315, and under the WLP package, the device wafer 311 is in direct contact with the EMC material. After the device wafer 311 and the organic film 315 (EMC material) are coupled, the relative dielectric constant of the filter 31 will increase, such as Er>4. The increase in the relative dielectric constant of the filter 31 will make the parasitic capacitance of the filter 31 larger, which will lead to the deterioration of the isolation.
[0077] It can be seen that when the filter 31 is packaged in the above packaging method, not only will the solder balls 313 crack, but the volume of the filter 31 may also be increased, and the isolation may even be deteriorated, affecting the performance of the filter 31.
[0078] See again Figure 2 After the cavity structure 316 of the filter 31 is made by using CSP packaging, or the cavity structure 316 of the filter 31 is made by using WLP packaging, when each filter 31 and other devices are integrated into the RF front-end module 30, an additional isolation member 35 is required as a shielding layer for isolation. The isolation member 35 wraps each device to prevent mutual interference between the devices in the RF front-end module 30. In this way, the volume of the RF front-end module 30 will increase, and the internal space occupied by the electronic device will increase, which will affect the development of thinness and lightness of the electronic device.
[0079] In order to solve the above problems, an embodiment of the present application provides a device packaging structure, which can prevent the solder ball 313 from cracking, realize the miniaturization of the device, and even improve the isolation.
[0080] The device packaging structure provided in the embodiment of the present application can be a filter, a low-noise amplifier, a power amplifier or a radio frequency switch, etc. The device packaging structure provided in the embodiment of the present application is exemplified below by taking the device packaging structure as a filter as an example.
[0081] Figure 6 This is the first structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0082] like Figure 6 As shown, in some embodiments, the device packaging structure includes a substrate 100 , a chip die 200 and a sealant 300 .
[0083] The substrate 100 may be a PCB. The substrate 100 includes a first surface 101 .
[0084] The chip bare crystal 200 can be made of piezoelectric material, such as lead zirconate titanate (Piezoelectric, PZT) piezoelectric ceramic material; the chip bare crystal 200 can also use a multi-layer bonding material, which includes silicon, silicon dioxide and piezoelectric material stacked in sequence. In the embodiment of the present application, the specific material of the chip bare crystal 200 is not specifically limited.
[0085] A surface of the chip bare die 200 includes a plurality of solder bumps 201, and the plurality of solder bumps 201 can be arranged around the edges of the surface at intervals. It should be noted that the structure of the solder bumps 201 and the chip bare die 200 can refer to Figure 3 The structure of the solder balls 313 and the device wafer 311 is shown.
[0086] The chip die 200 is soldered to the first surface 101 via a plurality of solder balls 201 . Due to the height of the solder balls 201 , a gap L1 is provided between the chip die 200 and the substrate 100 .
[0087] The sealant 300 is arranged around the gap L1 to seal the gap L1. The edges of the sealant 300 extend to the first surface 101 of the substrate 100 and the side surface of the chip die 200, respectively, so that the sealant 300, the substrate 100 and the chip die 200 form a cavity 400. At the same time, the sealant 300 can also be used to fix the chip die 200 to prevent the chip die 200 from displacement and change, which affects the performance of the device packaging structure.
[0088] The cavity 400 is used to provide a working space when the device packaging structure is working. Exemplarily, when the device packaging structure is a filter, the cavity 400 is used to provide a vibration space for the sound wave when the filter converts the electromagnetic wave into the sound wave.
[0089] In this scenario, one surface of the chip die 200 includes a plurality of resonators 204, and the plurality of resonators 204 are located between a plurality of solder balls 201. The resonators 204 are used to keep the vibration of the sound waves in the cavity 400 when the filter converts the electromagnetic waves into sound waves. The plurality of resonators 204 share the same cavity 400, which can reduce the volume of the filter.
[0090] The sealant 300 contacts the chip die 200 to generate a coupling effect, and the sealant 300 and the chip die 200 are coupled to form a composite material. The material properties of the sealant 300 and the material properties of the chip die 200 satisfy a first relationship, such as the material properties of the sealant 300 are the same as or close to the material properties of the chip die 200, to avoid a large difference in material properties after the sealant 300 and the chip die 200 are coupled, thereby affecting the performance of the device packaging structure.
[0091] The device packaging structure provided in the embodiment of the present application uses a sealant 300 to form the cavity 400 required for the device packaging structure, and the sealant 300 has a good contact coupling effect with the chip bare crystal 200. The material properties of the sealant 300 are the same as or close to the material properties of the chip bare crystal 200, and there will be no difference in material properties after the two are coupled, or the difference in material properties is small, thereby avoiding the performance of the device packaging structure being affected by the large difference in material properties.
[0092] In some embodiments, the material property may include a thermal expansion coefficient, and the sealant 300 has a low thermal expansion coefficient. For example, the sealant 300 may be a modified polysiloxane mixture having a low thermal expansion coefficient of about 10×10 -6 / ℃ or so. The main material in the modified polysiloxane mixture is modified polysiloxane, and the modified polysiloxane mixture is made of modified polysiloxane, polysiloxane containing vinyl groups, polysiloxane containing silicon hydrogen groups, boron-containing polysiloxane, modified platinum metal catalyst, diethyl maleate, dibutyl maleate, dioctyl maleate, silicon powder, silicon dioxide and diatomaceous earth. Exemplarily, the sealant 300 can be made of electron beam curing (EB) glue or ultraviolet curing (UV) glue.
[0093] The first relationship may include that the absolute value of the difference between the thermal expansion coefficient of the sealant 300 and the thermal expansion coefficient of the chip die 200 is less than or equal to a first threshold value, and the first threshold value is 20×10 -6 / ℃. The absolute value of the difference between the thermal expansion coefficient of the sealant 300 and the thermal expansion coefficient of the chip bare die 200 is in the range of [0, 20]×10 -6 / ℃, that is, the thermal expansion coefficient of the sealant 300 and the thermal expansion coefficient of the chip die 200 can be the same or close. For example, the CTE coefficient of the chip die 200 is generally between 4 and 10×10 -6 / ℃ range, the CTE coefficient of sealant 300 is about 10×10 -6 / ℃ approximately.
[0094] In extreme environments (such as hot and cold cycle tests), the difference in CTE coefficients between the sealant 300 and the chip bare die 200 is small or non-existent, so that no stress or small stress is generated between the two after coupling. In this way, the solder ball 201 is not subjected to stress or is subjected to small stress, so that the solder ball 201 will not crack, thereby improving the performance of the device packaging structure.
[0095] In some embodiments, the sealant 300 may also have poor fluidity, so that the sealant 300 only adheres to the periphery of the chip die 200 to seal the gap L1 , but does not enter the cavity 400 to avoid contamination of the resonator 204 .
[0096] In some embodiments, the sealant 300 may be formed around the gap L1 in a semi-covering manner. The sealant 300 may be disposed around the side surface 202 of the chip die 200 (see Figure 7 The structure shown in (c) in FIG. 1 is shown in FIG. 1 , and extends to the first surface 101 of the substrate 100 to seal the gap L1. The side surface 202 and the first surface 101 have an angle, and the angle can be a right angle.
[0097] The sealant 300 can be formed around the chip bare die 200 by a dispensing process, and the dispensing accuracy can be controlled within the micron range. That is, the width W of the sealant 300 is 300 Within 100μm. Figure 4 The coating process of the filter 31 shown in FIG. 1 is as follows: the width W of the organic film 315 is 315 Above 150μm-200μm, the width W of the sealant 300 300 By reducing the size of the device packaging structure, the device packaging structure can be miniaturized.
[0098] In the device packaging structure provided by the embodiment of the present application, the sealant 300 is continuously covered on the side surface 202 of the chip bare crystal 200 and the first surface of the substrate 100 in a semi-covering manner. While forming the cavity 400, the contact area between the sealant 300 and the chip bare crystal 200 can be guaranteed to ensure that the coupling effect between the sealant 300 and the chip bare crystal 200 meets the requirements, and then the difference in the CTE coefficient between the sealant 300 and the chip bare crystal 200 can be accurately determined. Since the CTE coefficients of the sealant 300 and the chip bare crystal 200 are the same or close, the difference in the CTE coefficients of the sealant 300 and the chip bare crystal 200 is small or no difference, and then no stress is generated between the two or the stress generated is small. In this way, the solder ball 201 will not be subjected to stress or the stress is small, so that the solder ball 201 will not crack, and then the performance of the device packaging structure can be improved.
[0099] In some embodiments, the process flow of the device packaging structure may include a lift-off process and a flip-chip process (FC). The lift-off process is to obtain a patterned photoresist structure or a metal mask (shadow mask) on a substrate using a photolithography process, coat the mask with a target coating using a coating process, and then use a degumming solution (also known as a stripping solution) to dissolve the photoresist or mechanically remove the metal hard mask to obtain a target graphic structure consistent with the pattern. The flip-chip process is a chip-to-substrate connection technology, which refers to directly depositing solder balls 201 on the I / O pads of the chip, and then flipping the chip for heating so that the molten solder combines with the substrate, with the electrical side of the chip facing down.
[0100] Figure 7 It is a process flow chart of the method for manufacturing the device packaging structure provided in the embodiment of the present application.
[0101] like Figure 7 As shown, in some embodiments, the present application provides a method for manufacturing a device packaging structure, the method comprising the following steps S101-S104:
[0102] like Figure 7 As shown in (a), step S101, providing a chip bare crystal 200.
[0103] When the device packaging structure is a filter, the filter includes a resonator 204. A plurality of resonators 204 are fabricated on the chip die 200 by using a stripping process to form a resonant cavity structure. The plurality of resonators 204 are spaced apart and located on one surface of the chip die 200, and the resonator 204 is in the form of a thin film.
[0104] Exemplarily, a patterned photoresist structure (mask) is obtained on the chip bare crystal 200 (substrate) by a photolithography process, a thin film material (target coating) is coated on the mask by a coating process, and then the mask is removed by a stripping solution to form a plurality of patterned spaced resonators 204 on the surface of the chip bare crystal 200.
[0105] like Figure 7 As shown in (b), in step S102, a plurality of solder balls 201 are coated on a surface of the chip bare die 200 to obtain a semi-encapsulated structure.
[0106] The solder paste is prefabricated on the surface of the resonator structure, and is reflow-oxidized to form solder balls 201 to obtain a semi-encapsulated structure.
[0107] The solder balls 201 are located around the edges of one surface of the chip die 200 . The solder balls 201 are directly connected to the I / O pads of the chip die 200 and have metal conductive properties. A plurality of resonators 204 are located in the area surrounded by the solder balls 201 .
[0108] like Figure 7 As shown in (c), step S103 , providing a substrate 100 , the substrate 100 includes a first surface 101 , placing the semi-encapsulation structure upside down on the first surface 101 of the substrate 100 , and soldering the chip die 200 to the substrate 100 via solder balls 201 .
[0109] The flip-chip process is adopted to flip the semi-package structure upside down on the first surface 101 of the substrate 100, and the solder balls 201 are heated to combine the molten solder with the substrate 100, so as to use the solder balls 201 to solder the chip die 200 and the substrate 100. Due to the influence of the height of the solder balls 201, a gap L1 is formed between the chip die 200 and the substrate 100.
[0110] like Figure 7 As shown in (d), step S104 , a sealant 300 is dispensed around the gap using a dispensing process to seal the gap. The sealant 300 , the chip die 200 and the substrate 100 form a cavity 400 .
[0111] Using dispensing technology, combined with Figure 7 In (c), the sealant 300 is dispensed onto the side surface 202 of the chip die 200, and continuously dispensed onto the first surface 101 of the substrate 100. In this way, the sealant 300 is disposed around the side surface 202 of the chip die 200 in a semi-covering manner to seal the gap L1, so that the sealant 300, the substrate 100 and the chip die 200 form a cavity 400.
[0112] The manufacturing method of the device packaging structure provided in the embodiment of the present application utilizes the micron-level precision characteristics of the dispensing process to make the width of the sealant 300 less than 100 μm, and the sealant 300 can seal the gap L1 in a small area, thereby realizing the miniaturization of the device. The sealant 300 is used to form the cavity 400 required for the device packaging structure. Based on the low fluidity and low thermal expansion coefficient characteristics of the sealant 300, contamination of the resonator 204 and cracking of the solder ball 201 can be avoided, thereby improving the performance of the device packaging structure.
[0113] Figure 8 This is a second structural schematic diagram of the device packaging structure provided in an embodiment of the present application.
[0114] like Figure 8 As shown, in some embodiments, the sealant 300 may be formed around the gap L1 in a fully covering manner.
[0115] Combination Figure 7In the structure shown in (c), the sealant 300 with a low thermal expansion coefficient covers the second surface 203 and the side surface 202 of the chip die 200, wherein the second surface 203 is the surface of the chip die 200 facing away from the first surface 101 of the substrate 100, and the side surface 202 is connected to the second surface 203. The edges of the sealant 300 extend to the first surface 101 of the substrate 100 to seal the gap L1.
[0116] When manufacturing such a device packaging structure, step S104 may include: using a dispensing process to continuously dispense the sealant 300 onto the second surface 203 and the side surface 202 of the chip die 200 , and extending it to the first surface 101 of the substrate 100 to seal the gap L1 .
[0117] By using the dispensing process, the thickness H of the sealant 300 located on the second surface 203 is 300 Less than 65μm, which is conducive to further miniaturization of the device packaging structure.
[0118] In the device packaging structure provided by the embodiment of the present application, the sealant 300 continuously covers the second surface 203 and the side surface 202 of the chip bare crystal 200, as well as the first surface 101 of the substrate 100 in a full coverage manner, so that the contact area between the sealant 300 and the chip bare crystal 200 is increased while forming the cavity 400, thereby further improving the coupling effect between the sealant 300 and the chip bare crystal 200, so as to more accurately determine the difference in CTE coefficients between the sealant 300 and the chip bare crystal 200. Since the CTE coefficients of the sealant 300 and the chip bare crystal 200 are the same or close, the difference in CTE coefficients between the sealant 300 and the chip bare crystal 200 is small or no difference, thereby ensuring that no stress or small stress is generated between the two after coupling. In this way, the solder ball 201 will not be subjected to stress or the stress is small, so that the solder ball 201 will not crack, thereby improving the performance of the device packaging structure.
[0119] It should be noted that Figure 8 The remaining structural characteristics of the device package structure shown can refer to Figure 6 The corresponding structural characteristics of the device packaging structure shown are not repeated here.
[0120] In some embodiments, the accuracy of the determined CTE coefficient difference between the sealant 300 and the chip die 200 is positively correlated with the contact area between the sealant 300 and the chip die 200. The larger the contact area between the sealant 300 and the chip die 200, for example, the sealant 300 is formed around the chip die 200 in a full-covering manner, the better the coupling effect between the sealant 300 and the chip die 200, and the more accurate the determined CTE coefficient difference. The smaller the contact area between the sealant 300 and the chip die 200, for example, the sealant 300 is formed around the chip die 200 in a semi-covering manner, the coupling effect between the sealant 300 and the chip die 200 is relatively poor under the premise of meeting the coupling requirements, and the accuracy of the determined CTE coefficient difference is relatively low under the premise of meeting the accuracy requirements. That is, in the embodiment where the sealant 300 is formed around the chip die 200 in a semi-covering manner, the coupling effect between the sealant 300 and the chip die 200 meets the requirements, and the accuracy of the determined CTE coefficient difference meets the accuracy requirements, which can ensure that the solder ball 201 will not crack. In the embodiment where the sealant 300 is formed around the chip die 200 in a full-covering manner, it can further ensure that the solder ball 201 will not crack.
[0121] Fig. 9 This is the third structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0122] like Fig. 9 As shown, in some embodiments, the material property may include a dielectric constant. The sealant 300 may be an organic sealant with a low-K (low dielectric constant) property, so that the sealant 300 has a low dielectric constant. Exemplarily, the sealant 300 may be a styrene mixture, whose dielectric constant is about 2.5 F / m, the main material in the styrene mixture is styrene, and the styrene mixture is made of styrene, butadiene, isoprene, stearic acid monoglyceride, polyamide resin and phenolic resin.
[0123] The first relationship may include a first ratio between the dielectric constant of the sealant 300 and the dielectric constant of the chip die 200; the first ratio ranges from 0.75 to 1.5, including the end value but excluding zero. In other words, the dielectric constant of the sealant 300 and the dielectric constant of the chip die 200 may be the same or close.
[0124] In this way, since the dielectric constants of the chip bare crystal 200 and the sealant 300 are both low and close to or the same, the relative dielectric constant of the composite material obtained after the sealant 300 is coupled with the chip bare crystal 200 is still low, such as Er<4, so that the parasitic capacitance of the device packaging structure is reduced to improve the isolation between different frequency bands, so that the filtering frequency bands do not interfere with each other, thereby improving the filtering accuracy.
[0125] In some embodiments, the sealant 300 of low-K property can be formed around the gap L1 in a semi-covering manner. The sealant 300 can be disposed around the side surface 202 of the chip die 200 (see Figure 7 The structure shown in (c) in FIG. 1 is shown in FIG. 1 , and extends to the first surface 101 of the substrate 100 to seal the gap L1.
[0126] When manufacturing such a device packaging structure, step S104 may include: using a dispensing process to continuously dispense the sealant 300 onto the side surface 202 of the chip die 200 and the first surface 101 of the substrate 100 .
[0127] The sealant 300 can be formed around the chip die 200 by a dispensing process, and the width W of the sealant 300 is 300 Within 100 μm, the size of the device packaging structure can be reduced. In addition, the sealant 300 has poor fluidity, so that the sealant 300 only adheres to the periphery of the chip die 200 to seal the gap L1, and does not enter the cavity 400 to pollute the resonator 204.
[0128] In this way, the embodiment of the present application utilizes a dispensing process and forms a sealant 300 around the gap L1 in a semi-covering manner, so as to utilize the sealant 300 to form a cavity 400 , thereby realizing miniaturization of the device packaging structure.
[0129] In some embodiments, the low-K sealant 300 may also have poor fluidity, so that the sealant 300 only adheres to the periphery of the chip die 200 to seal the gap L1 without entering the cavity 400 to avoid contamination of the resonator 204 .
[0130] In the device packaging structure provided by the embodiment of the present application, the sealant 300 with low-K properties can be formed in a semi-covering manner around the gap L1. While forming the cavity 400, the contact area between the sealant 300 and the chip bare crystal 200 can be guaranteed to ensure that the coupling effect between the sealant 300 and the chip bare crystal 200 meets the requirements, and then the difference in dielectric constant between the sealant 300 and the chip bare crystal 200 can be accurately determined. Since the dielectric constants of the sealant 300 and the chip bare crystal 200 are the same or close, the difference in dielectric constant between the sealant 300 and the chip bare crystal 200 is small or no difference, and then the dielectric constant of the composite material after the two are coupled is still low. In this way, the parasitic capacitance of the device packaging structure can be greatly reduced, the isolation between different frequency bands can be improved, and the filtering frequency bands can be made to not interfere with each other, so as to improve the filtering accuracy.
[0131] It should be noted that Fig. 9 The remaining structural characteristics of the device package structure shown can refer to Figure 6The structural characteristics of the device packaging structure shown are not described in detail here.
[0132] Fig.10 This is the fourth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0133] like Fig.10 As shown, in some embodiments, a sealant 300 with a low-K property may be formed around the gap L1 in a full coverage manner.
[0134] Combination Figure 7 In the structure shown in (c), the sealant 300 covers the second surface 203 and the side surface 202 of the chip die 200 , and the edges of the sealant 300 extend to the first surface 101 of the substrate 100 to seal the gap L1 .
[0135] When manufacturing such a device packaging structure, step S104 may include: using a dispensing process to continuously dispense the sealant 300 onto the second surface 203 and the side surface 202 of the chip die 200 , and extending it to the first surface 101 of the substrate 100 to seal the gap L1 .
[0136] By using the dispensing process, the thickness H of the sealant 300 located on the second surface 203 is 300 Less than 65 μm, the width W of the sealant 300 at the side surface 202 300 Within 100μm, this is conducive to further miniaturization of the device packaging structure.
[0137] In the device packaging structure provided by the embodiment of the present application, the sealant 300 of low-K property continuously covers the second surface 203 and the side surface 202 of the chip bare crystal 200, as well as the first surface 101 of the substrate 100 in a full coverage manner, so that the contact area between the sealant 300 and the chip bare crystal 200 is increased. While forming the cavity 400, the contact area between the sealant 300 and the chip bare crystal 200 can be increased to further improve the coupling effect between the sealant 300 and the chip bare crystal 200, so as to more accurately determine the difference in dielectric constant between the sealant 300 and the chip bare crystal 200. Since the dielectric constants of the sealant 300 and the chip bare crystal 200 are the same or close, the difference in dielectric constants between the sealant 300 and the chip bare crystal 200 is small or no difference occurs, so that the dielectric constant of the composite material after the two are coupled is still low. In this way, the parasitic capacitance of the device packaging structure can be greatly reduced, and the isolation between different frequency bands of the device sealing structure can be further improved to improve the filtering accuracy.
[0138] In some embodiments, the isolation of the filter is positively correlated with the contact area between the sealant 300 and the chip die 200. The larger the contact area between the sealant 300 and the chip die 200, for example, the sealant 300 is formed around the chip die 200 in a full-coverage manner, the higher the isolation of the filter is, and it is suitable for filters with high isolation requirements. The smaller the contact area between the sealant 300 and the chip die 200, for example, the sealant 300 is formed around the chip die 200 in a semi-coverage manner, the isolation of the filter is relatively low while meeting the isolation requirements, and it is suitable for filters with relatively low isolation requirements.
[0139] It should be noted that Fig.10 The remaining structural characteristics of the device package structure shown can refer to Figure 8 The structural characteristics of the device packaging structure shown are not described in detail here.
[0140] Fig.11 This is the fifth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0141] like Fig.11 As shown, in some embodiments, the material properties may include a thermal expansion coefficient and a dielectric constant. The sealant 300 may include a first sealant 301 and a second sealant 302. The first relationship includes that the absolute value of the difference between the thermal expansion coefficient of the first sealant 301 and the thermal expansion coefficient of the chip die 200 is less than or equal to a first threshold value, and the first threshold value is 20×10 -6 / °C; and, the dielectric constant of the second sealant 302 and the dielectric constant of the chip die 200 have a first ratio, and the value range of the first ratio is between 0.75 and 1.5.
[0142] It should be noted that the properties of the first sealant 301 can be referred to Figure 6 The characteristics of the sealant 300 used in the device packaging structure shown in FIG. 1 and the characteristics of the second sealant 302 can be referred to as Fig. 9 The characteristics of the sealant 300 used in the device packaging structure are not described in detail here.
[0143] One of the first sealant 301 and the second sealant 302 is disposed on the side surface 202 of the chip die 200 and extends to the first surface 101 of the substrate 100 to seal the gap L1. The other of the first sealant 301 and the second sealant 302 covers the second surface 203 of the chip die 200, and the first sealant 301 and the second sealant 302 are connected.
[0144] When making such a device packaging structure, step S104 may include: using a dispensing process to continuously dispense one of the first sealant 301 and the second sealant 302 to the side surface 202 of the chip bare crystal 200 and the first surface 101 of the substrate 100 to seal the gap L1; dispensing the other of the first sealant 301 and the second sealant 302 to the second surface 203 of the chip bare crystal 200, so that the first sealant 301 and the second sealant 302 are combined.
[0145] Exemplarily, a dispensing process is used to continuously dispense the first sealant 301 to the side surface 202 of the chip die 200 and extend to the first surface 101 of the substrate 100 to seal the gap L1; the second sealant 302 is dispensed to the second surface 203 of the chip die 200. The first sealant 301 and the second sealant 302 are combined to continuously cover the second surface 203 and the side surface 202 of the chip die 200, as well as the first surface 101 of the substrate 100 in a full coverage manner.
[0146] By using the dispensing process, the width W of the first sealant 301 is 301 Less than 100 μm, the thickness H of the second sealant 302 302 Less than 65μm, which is conducive to further miniaturization of the device packaging structure.
[0147] Since the fluidity of the first sealant 301 and the second sealant 302 is poor, the second sealant 302 usually does not overflow during dispensing. In other embodiments, in order to prevent the second sealant 302 from overflowing in special scenarios, the amount of the second sealant 302 can be controlled, or a mold can be used to prevent the second sealant 302 from overflowing.
[0148] In the device packaging structure provided by the embodiment of the present application, both the first sealant 301 and the second sealant 302 can contact the chip bare crystal 200, thereby ensuring the coupling effect between the first sealant 301 and the chip bare crystal 200, and the coupling effect between the second sealant 302 and the chip bare crystal 200. By utilizing the low thermal expansion coefficient characteristic of the first sealant 301, the solder ball 201 can be prevented from cracking; by utilizing the low dielectric constant characteristic of the second sealant 302, the isolation can be improved. In this way, the device packaging structure can prevent the solder ball 201 from cracking, and can also realize the miniaturization of the device, and can even improve the isolation, ensuring the performance of the device packaging structure.
[0149] It should be noted that Fig.11 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0150] Fig.12This is the sixth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0151] like Fig.12 As shown, in some embodiments, Fig.11 Based on the device packaging structure shown, one of the first sealant 301 and the second sealant 302 used to cover the second surface 203 extends from the second surface 203 along the outer surface of the other of the first sealant 301 and the second sealant 302 to the first surface 101 of the substrate 100.
[0152] When making such a device packaging structure, step S104 may include: using a dispensing process to continuously dispense one of the first sealant 301 and the second sealant 302 to the side surface 202 of the chip bare crystal 200 and the first surface 101 of the substrate 100 to seal the gap L1; dispensing the other of the first sealant 301 and the second sealant 302 to the second surface 203 of the chip bare crystal 200, and extending from the second surface 203 along the outer surface of the other of the first sealant 301 and the second sealant 302 to the first surface 101 of the substrate 100, so that the first sealant 301 and the second sealant 302 are combined.
[0153] Exemplarily, a dispensing process is used to continuously dispense the first sealant 301 onto the side surface 202 of the chip die 200 and extend it to the first surface 101 of the substrate 100 to seal the gap L1; the second sealant 302 is continuously extended from the second surface 203 of the chip die 200 along the outer surface of the first sealant 301 to the first surface 101 of the substrate 100.
[0154] In this way, the second sealant 302 can be used to wrap the chip bare die 200 and the first sealant 301 to improve reliability.
[0155] It should be noted that Fig.12 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0156] In some embodiments, the sealant 300 may be made of a material having both a low thermal expansion coefficient and a low dielectric constant, so that the material properties of the sealant 300 and the material properties of the chip bare die 200 satisfy a first relationship. In this way, the device packaging structure can not only prevent the solder ball 201 from cracking, but also improve the isolation and filtering accuracy to ensure the performance of the device packaging structure. The structural characteristics and beneficial effects of the sealant 300 can all refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0157] Fig.13This is the seventh structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0158] like Fig.13 As shown, in some embodiments, the device packaging structure may further include: an inner shielding layer 500 .
[0159] The inner shielding layer 500 can be made of shielding materials, such as stainless steel, gold, copper or gold-copper alloy, etc. The inner shielding layer 500 is used to isolate the various components in the RF chip module to solve the problem of mutual interference between the various components in the RF chip module.
[0160] The inner shielding layer 500 cannot contact the chip bare die 200 to avoid affecting the performance of the device packaging structure. Therefore, the sealant 300 needs to be combined with the chip bare die 200 in a full coverage manner. The structure of the sealant 300 combined with the chip bare die 200 in a full coverage manner can be referred to Figure 8 , Fig.10 , Fig.11 and Fig.12 The device packaging structure provided by any one of the embodiments is as follows: Figure 8 An inner shielding layer 500 is provided on the device packaging structure for exemplary description.
[0161] Combination Figure 8 In the structure shown, the sealant 300 may include a first outer surface 303. The inner shielding layer 500 may cover the first outer surface 303 of the sealant 300, and the edges of the inner shielding layer 500 extend to the first surface 101 of the substrate 100, so that the inner shielding layer 500 completely covers the sealant 300.
[0162] When manufacturing such a device packaging structure, the manufacturing method of the device packaging structure may further include: using a physical vapor deposition (PVD) sputtering process to continuously sputter the shielding material on the first outer surface 303 of the sealant 300 and the first surface 101 of the substrate 100 to form an inner shielding layer 500 .
[0163] The substrate 100 includes a plurality of traces 102 , one end of the trace 102 is exposed from the first surface 101 , and the other end is exposed from a surface of the substrate 100 opposite to the first surface 101 , so as to facilitate integration of the device packaging structure into the RF chip module.
[0164] The inner shielding layer 500 includes a first connection end 502 extending along the first surface 101 of the substrate 100 and in contact with the trace 102. In this way, the inner shielding layer 500 is electrically connected to the substrate 100, and the inner shielding layer 500 can achieve an anti-interference effect.
[0165] The device packaging structure provided in the embodiment of the present application has an inner shielding layer 500 sputtered on the first outer surface 303 of the sealant 300, so that the device packaging structure itself has an independent separation function, avoiding mutual interference when it is packaged together with other device packaging structures into the RF chip module. Figure 2 The solution of additionally setting up an isolation member 35 as a shielding layer is shown. In the embodiment of the present application, during the stage of manufacturing the device packaging structure, an inner shielding layer 500 is set. When it is integrated into the RF chip module, independent cavity shielding can be achieved. The process is simple and there is no need to set up an additional shielding layer to reduce the volume of the RF chip module.
[0166] It should be noted that Fig.13 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0167] Fig.14 This is the eighth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0168] like Fig.14 As shown, in some embodiments, the device packaging structure may further include: a plastic packaging layer 600. Exemplarily, the plastic packaging layer 600 may be made of EMC material.
[0169] Combination Fig.13 The inner shielding layer 500 includes a second outer surface 501, and the plastic sealing layer 600 covers the second outer surface 501 of the inner shielding layer 500 and the first surface 101 of the substrate 100. The inner shielding layer 500 is wrapped with the plastic sealing layer 600 to prevent the inner shielding layer 500 from leaking out, thereby affecting the performance of the inner shielding layer 500 and further affecting the performance of the device packaging structure. The plastic sealing layer 600, the inner shielding layer 500 and the sealant 300 can jointly fix the chip bare crystal 200 to further improve reliability.
[0170] When manufacturing such a device packaging structure, the manufacturing method of the device packaging structure may further include: using a compression molding process to compression mold the EMC material on the second outer surface 501 of the inner shielding layer 500 and the first surface 101 of the substrate 100 to form a plastic packaging layer 600 .
[0171] The compression molding process can use molding, which refers to a method of sealing by melting and then solidifying plastic epoxy materials. Molding methods include transfer molding (T-Molding) and compression molding (C-Molding). The process parameters of these two molding methods are different. The T-Molding process has a high pressure on the wafer during molding and low cost; the C-Molding process has a low pressure on the wafer during molding and high cost.
[0172] In order to avoid the inner shielding layer 500 being damaged by the molding process when the plastic encapsulation layer 600 is formed by compression molding, the embodiment of the present application may adopt a C-Molding process with a small process pressure, which will not damage the inner shielding layer 500.
[0173] The device packaging structure provided in the embodiment of the present application can ensure the functional stability of the device packaging structure by using the plastic packaging layer 600, and can make the device packaging structure not be affected by the external environment (water vapor, temperature, pollution, etc.), and realize the composite functions of thermal conductivity, insulation, moisture resistance, pressure resistance, support, etc.
[0174] It should be noted that Fig.14 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0175] Fig.15 This is the ninth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0176] like Fig.15 As shown, in some embodiments, the device packaging structure may further include: an outer shielding layer 800 .
[0177] The outer shielding layer 800 is made of the same material as the inner shielding layer 500, and can be made of stainless steel, gold, copper, or gold-copper alloy, etc. The outer shielding layer 800 is used to isolate the RF chip module from other modules in the electronic device to prevent mutual interference between the modules.
[0178] The outer shielding layer 800 covers the third outer surface 601 of the plastic packaging layer 600 and the first surface 101 of the substrate 100 . The outer shielding layer 800 is the outermost structure of the device packaging structure, or can be used as the outermost structure of the RF chip module.
[0179] When manufacturing such a device packaging structure, the manufacturing method of the device packaging structure may further include: using a physical vapor deposition (PVD) sputtering process to continuously sputter the shielding material on the third outer surface 601 of the plastic packaging layer 600 and the first surface 101 of the substrate 100 to form an outer shielding layer 800 .
[0180] The outer shielding layer 800 includes a second connection end 801 extending along the first surface 101 of the substrate 100 and in contact with the trace 102. In this way, the outer shielding layer 800 is electrically connected to the substrate 100, and the outer shielding layer 800 can achieve an anti-interference effect.
[0181] The device packaging structure provided in the embodiment of the present application includes an inner shielding layer 500 and an outer shielding layer 800. The inner shielding layer 500 is used to make the device packaging structure itself have an independent separation function, so as to avoid mutual interference when it is packaged with other device packaging structures into a radio frequency chip module. The outer shielding layer 800 is used to isolate the radio frequency chip module from other modules in the electronic device, so as to avoid mutual interference between the modules.
[0182] It should be noted that Fig.15 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0183] Fig.16 This is the tenth structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0184] like Fig.16 As shown, in some embodiments, the device packaging structure may further include: a protective glue 700. The protective glue 700 is used to protect the inner shielding layer 500 to avoid damage to the inner shielding layer 500 when the plastic sealing layer 600 is molded.
[0185] The protective glue 700 completely covers the second outer surface 501 of the inner shielding layer 500 to prevent the inner shielding layer 500 from being exposed. The protective glue 700 is made of the same material as the sealant 300. If the sealant 300 is made of a material with a low thermal expansion coefficient, the protective glue 700 is also made of a material with a low thermal expansion coefficient; if the sealant 300 is made of a sealant with a low-K property, the protective glue 700 is also made of a sealant with a low-K property.
[0186] When manufacturing such a device packaging structure, the manufacturing method of the device packaging structure may further include: using a dispensing process to continuously dispense the protective glue 700 onto the second outer surface 501 of the inner shielding layer 500 .
[0187] In the device packaging structure provided by the embodiment of the present application, the inner shielding layer 500 is located between the protective glue 700 and the sealant 300, so that the inner shielding layer 500 will neither contact the chip bare crystal 200 nor be exposed to the outside. The protective glue 700 is used to protect the inner shielding layer 500 to avoid damage to the inner shielding layer 500 when the plastic sealing layer 600 is subsequently formed by the molding process. In addition, it is also convenient to select the lower-cost T-Molding process in the subsequent process to reduce the process cost.
[0188] It should be noted that Fig.16 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0189] Fig.17 This is the eleventh structural schematic diagram of the device packaging structure provided in the embodiment of the present application.
[0190] like Fig.17 As shown, in some embodiments, based on Fig.16 The device packaging structure shown may further include: a plastic packaging layer 600. Fig.16 The plastic encapsulation layer 600 covers the fourth outer surface 701 of the protective glue 700 and the first surface 101 of the substrate 100 .
[0191] When manufacturing such a device packaging structure, the manufacturing method of the device packaging structure may further include: using a molding process to compression mold the EMC material onto the fourth outer surface 701 of the protective glue 700 and the first surface 101 of the substrate 100 to form a plastic packaging layer 600 .
[0192] Since the inner shielding layer 500 can be protected by the protective glue 700, the T-Molding process can be selected to press-mold the plastic sealing layer 600. In this way, the inner shielding layer 500 will not be damaged and the process cost can be reduced.
[0193] The device packaging structure provided in the embodiment of the present application can ensure the functional stability of the device packaging structure by using the plastic packaging layer 600, and can make the device packaging structure not be affected by the external environment (water vapor, temperature, pollution, etc.), and realize the composite functions of thermal conductivity, insulation, moisture resistance, pressure resistance, support, etc.
[0194] In some embodiments, Fig.17 The device packaging structure shown may further include: an outer shielding layer 800; the outer shielding layer 800 covers the third outer surface 601 of the plastic packaging layer 600 and the first surface 101 of the substrate 100. Fig.15 As shown, the outer shielding layer 800 is used to isolate the RF chip module from other modules in the electronic device to avoid mutual interference between the modules.
[0195] It should be noted that Fig.17 The remaining structural characteristics and beneficial effects of the device packaging structure shown can refer to the corresponding contents of the device packaging structure provided in any of the aforementioned embodiments, and will not be repeated here.
[0196] Each device packaging structure provided in the embodiment of the present application does not need to use CSP packaging to pre-cover the organic film when making the cavity 400 required for the device packaging structure, nor does it need to use the WLP process to make the wall structure and the roof structure, but uses an organic sealant 300 to make it. The sealant 300 can choose materials with different characteristics, such as EB glue with a very low CTE coefficient or an organic glue with low-K properties, which is low in cost. According to different scenarios, a covering method of half-covering or full-covering the chip bare crystal 200 can also be adopted to solve the problem of solder ball cracking caused by the large difference in CTE coefficient and the problem of isolation deterioration caused by the large relative dielectric constant, respectively, and the implementation is simple. The sealant 300 can achieve a small area coverage of the chip bare crystal 200, which is conducive to the miniaturization requirements during the later compression molding process. The device packaging structure is provided with an inner shielding layer 500 to directly realize independent cavity shielding. Therefore, the device packaging structure provided in the embodiment of the present application can not only reduce the cost of device packaging, but also use different packaging materials and packaging shapes according to different scenarios, greatly improving device performance and reliability.
[0197] In some embodiments, the device packaging structure and corresponding manufacturing method provided in each embodiment of the present application are not only applicable to packaging filters, but also applicable to packaging low-noise amplifiers, power amplifiers, RF switches and other devices. The structural characteristics, manufacturing methods and beneficial effects achieved when packaging low-noise amplifiers, power amplifiers, RF switches and other devices can all refer to the corresponding contents provided in any of the aforementioned embodiments, and will not be repeated here.
[0198] It should be noted that for devices that do not need to form a cavity 400, the chip bare crystal 200 can be directly soldered to the substrate 100 without the need to go through a lift-off process to make a resonant cavity structure, and without the need to pre-set the solder ball 201 structure. In this way, when making such a device, it is not necessary to execute the content of making the resonator structure in step S101 and the content of step S102, but directly use solder paste for soldering, and the gap between the chip bare crystal 200 and the substrate 100 can be reduced by reducing the amount of solder paste. The sealant 300 can be covered around the chip bare crystal 200 in a semi-covering or fully covering manner. The remaining structural characteristics, manufacturing methods and beneficial effects achieved can all refer to the corresponding contents provided in any of the aforementioned embodiments, and will not be repeated here.
[0199] Fig.18 This is the first structural diagram of the RF chip module provided in the embodiment of the present application.
[0200] like Fig.18 As shown, in some embodiments, the radio frequency chip module 50 is an important component of the communication module of the electronic device and is the core of realizing wireless communication of the electronic device.
[0201] The radio frequency chip module 50 may include a main substrate 51 and a device packaging structure 52 provided in any of the aforementioned embodiments, wherein a plurality of device packaging structures 52 are spaced apart on the surface of the main substrate 51 .
[0202] The multiple device packaging structures 52 may include devices such as filters, low noise amplifiers, power amplifiers, and radio frequency switches. The devices such as filters, low noise amplifiers, power amplifiers, and radio frequency switches are integrated on the main substrate 51 to obtain the radio frequency chip module 50. The main substrate 51 may be formed integrally by the substrates 100 in each device packaging structure 52.
[0203] Since the device packaging structure 52 includes an inner shielding layer 500 that can prevent interference, when it is integrated into the RF chip module 50, there is no need to set up an additional shielding layer, and independent cavity shielding can be achieved between devices.
[0204] In this way, the distance between two adjacent devices can be reduced, thereby reducing the size of the RF chip module 50.
[0205] Fig.19 This is a second structural diagram of the RF chip module provided in an embodiment of the present application. Fig.19 Show Fig.18 , and only shows the structures of two device packaging structures 52.
[0206] like Fig.19 As shown, in some embodiments, the plastic encapsulation layer 600 and the outer shielding layer 800 can be formed when manufacturing the RF chip module 50 .
[0207] Since each device packaging structure 52 can achieve independent cavity shielding, when performing the molding process, each device packaging structure 52 in the RF chip module 50 can be uniformly packaged to form a total plastic packaging layer 600 covering all the device packaging structures 52.
[0208] Similarly, the shielding material can be uniformly sputtered onto the outer surface of the total plastic layer 600 of the RF chip module 50 by using the PVD process to form a total outer shielding layer 800, so as to cover the entire RF chip module 50 with the outer shielding layer 800. The outer shielding layer 800 and the inner shielding layer 500 are respectively in contact with the traces 102 in the main substrate 51 to achieve electrical connection between the outer shielding layer 800 and the inner shielding layer 500 and the main substrate 51.
[0209] In this way, when the RF chip module 50 is applied to an electronic device, the inner shielding layer 500 can be used to isolate the various components in the RF chip module 50 to avoid mutual interference between the components; the outer shielding layer 800 can be used to isolate the RF chip module 50 from other modules in the electronic device to avoid mutual interference between the modules.
[0210] In the RF chip module 50 provided in the embodiment of the present application, each device packaging structure 52 does not need to independently package the plastic packaging layer 600 and the outer shielding layer 800, but is packaged uniformly during the stage of manufacturing the RF chip module 50, which can further simplify the manufacturing process, reduce costs, and reduce the volume of the RF chip module 50.
[0211] An electronic device provided in an embodiment of the present application includes the radio frequency chip module 50 provided in the aforementioned embodiment, and wireless communication is achieved by using the radio frequency chip module 50.
[0212] It should be noted that those skilled in the art will readily come up with other embodiments of the present application after considering the specification and practicing the application disclosed herein. The present application is intended to cover any variations, uses or adaptations of the present application, which follow the general principles of the present application and include common knowledge or customary technical means in the art that are not disclosed in the present application. The specification and examples are intended to be exemplary only, and the true scope of the present application is indicated by the following claims.
[0213] It should be understood that the present application is not limited to the precise structures that have been described above and shown in the drawings, and that various modifications and changes may be made without departing from the scope thereof. The scope of the present application is limited only by the appended claims.
Claims
1. A device packaging structure, characterized in that: include: A substrate (100) comprising a first surface (101); A chip bare crystal (200) is soldered to the first surface (101) via a plurality of solder balls (201), and a gap is provided between the chip bare crystal (200) and the substrate (100); A sealant (300) is arranged around the gap to seal the gap, and forms a cavity (400) with the substrate (100) and the chip bare crystal (200); The material properties of the sealant (300) and the material properties of the chip bare die (200) satisfy a first relationship; The material properties include coefficient of thermal expansion and dielectric constant; The sealant (300) comprises a first sealant (301) and a second sealant (302); the first relationship comprises that an absolute value of a difference between a thermal expansion coefficient of the first sealant (301) and a thermal expansion coefficient of the chip bare die (200) is less than or equal to a first threshold, and the first threshold is 20×10 -6 / °C, and the dielectric constant of the second sealant and the dielectric constant of the chip bare die (200) have a first ratio, and the value range of the first ratio is 0.75-1.5; The first sealant (301) and the second sealant (302) are connected and cover the chip bare die (200), and seal the gap.
2. The device packaging structure according to claim 1, characterized in that: The material properties include coefficient of thermal expansion; The first relationship includes that an absolute value of a difference between a thermal expansion coefficient of the sealant (300) and a thermal expansion coefficient of the chip die (200) is less than or equal to a first threshold; The first threshold is 20×10 -6 / ℃.
3. The device packaging structure according to claim 1, characterized in that: The material properties include a dielectric constant; The first relationship includes that the dielectric constant of the sealant (300) and the dielectric constant of the chip die (200) have a first ratio; The value range of the first ratio is 0.75~1.
5.
4. The device packaging structure according to claim 2 or 3, characterized in that: The sealant (300) is disposed around the side surface (202) of the chip bare crystal (200) and extends to the first surface (101) of the substrate (100) to seal the gap.
5. The device packaging structure according to claim 2 or 3, characterized in that: The sealant (300) covers the second surface (203) and the side surface (202) of the chip bare crystal (200), and extends to the first surface (101) of the substrate (100) to seal the gap; The second surface (203) is a surface of the chip bare crystal (200) that is opposite to the first surface (101), and the side surface (202) is connected to the second surface (203).
6. The device packaging structure according to claim 1, characterized in that: The chip bare crystal (200) comprises a side surface (202) and a second surface (203) connected to each other, wherein the second surface (203) is a surface of the chip bare crystal (200) that is opposite to the first surface (101); A ring of the first sealant (301) and the second sealant (302) is provided on the side surface (202) and extends to the first surface (101) of the substrate (100) to seal the gap; The other of the first sealant (301) and the second sealant (302) covers the second surface (203).
7. The device packaging structure according to claim 6, characterized in that: One of the first sealant (301) and the second sealant (302) for covering the second surface (203) extends from the second surface (203) along the outer surface of the other of the first sealant (301) and the second sealant (302) to the first surface (101) of the substrate (100).
8. The device packaging structure according to claim 1, characterized in that: Also included: an inner shielding layer (500); The inner shielding layer (500) covers the first outer surface (303) of the sealant (300) and extends to the first surface (101) of the substrate (100).
9. The device packaging structure according to claim 8, characterized in that: Also includes: a plastic sealing layer (600); The plastic encapsulation layer (600) covers the second outer surface (501) of the inner shielding layer (500) and the first surface (101) of the substrate (100).
10. The device packaging structure according to claim 8, characterized in that: Also includes: protective glue (700); The protective glue (700) covers the second outer surface (501) of the inner shielding layer (500).
11. The device packaging structure according to claim 10, characterized in that: Also includes: a plastic sealing layer (600); The plastic encapsulation layer (600) covers the fourth outer surface (701) of the protective glue (700) and the first surface (101) of the substrate (100).
12. The device packaging structure according to claim 9 or 11, characterized in that: Also includes: an outer shielding layer (800); The outer shielding layer (800) covers the third outer surface (601) of the plastic encapsulation layer (600) and the first surface (101) of the substrate (100).
13. A method for manufacturing a device packaging structure, characterized in that: For manufacturing the device packaging structure according to any one of claims 1 to 12, the method comprises: Providing a chip die and a substrate, wherein the substrate comprises a first surface; Coating a plurality of solder balls on one surface of the chip bare die to obtain a semi-encapsulated structure; The semi-encapsulation structure is inverted on the first surface of the substrate, the chip bare die is soldered to the substrate via the solder balls, and a gap is formed between the chip bare die and the substrate; The first sealant and the second sealant are continuously dispensed around the gap by a dispensing process to cover the chip bare crystal and seal the gap. The first sealant, the second sealant, the chip bare crystal and the substrate form a cavity.
14. A radio frequency chip module, characterized in that: It comprises a main substrate, and a plurality of device packaging structures according to any one of claims 1 to 12; A plurality of the device packaging structures are spaced apart and located on the surface of the main substrate.
15. An electronic device, characterized in that: Comprising the radio frequency chip module as claimed in claim 14.
Citation Information
Patent Citations
Integrated packaging structure
CN112563249A
Package including substrate, integrated device, and encapsulation layer having undercut
CN115485830A
Semiconductor package having electromagnetic interference shielding layer and method of fabricating the same
KR1020180021336A
Package stress management
US20060001158A1
Thermally enhanced semiconductor package and process for making the same
US20180166358A1