A method for manufacturing enhanced resin lens

Through the combination of the liquid detection unit and the RBF neural network, precise quantitative pouring and quality inspection of resin lenses are achieved, which solves the problem of insufficient or excessive pouring in the existing technology and improves the quality and production efficiency of the lenses.

CN118290637BActive Publication Date: 2024-10-11DANYANG ALDI OPTICAL GLASSES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410726995.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-06
Publication Date
2024-10-11
Estimated Expiration
2044-06-06

AI Technical Summary

Technical Problem

In the manufacturing process of resin lenses, it is difficult to achieve precise quantitative pouring and quality inspection with existing technology, resulting in insufficient or excessive pouring, affecting lens quality and efficiency.

Method used

The liquid detection unit is used to monitor the liquid height and gap value in the glass mold through the image acquisition module, calculate the unpoured volume value, and perform quantitative control through the filling unit. At the same time, the RBF neural network is used in the finished product inspection to detect lens defects and optical performance. detection.

Benefits of technology

It achieves precise quantitative pouring, improves the yield rate and detection efficiency, and ensures the optical performance and quality of the lens.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118290637B_ABST
    Figure CN118290637B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing an enhanced resin lens, comprising the following processes: a first step, preparing monomer materials and auxiliary materials, wherein the monomer materials include styrene, tetramethylolpropane tetraacrylate, and ethoxylated bisphenol A diacrylate, and the auxiliary materials include colorants, antioxidants, and initiators, and the monomer materials and auxiliary materials are mixed to prepare a casting liquid; a second step, the casting liquid obtained in the first step is poured into a glass mold through a filling unit, and during the quantitative pouring process of the filling unit, a liquid detection unit monitors the casting liquid in the glass mold. The present invention can achieve precise quantitative filling, high detection accuracy, and improve the yield rate. By setting the detection time, the detection amount can be reduced and the detection efficiency can be improved. During the production process of the resin lens, the refractive index, dispersion, and light transmittance can be detected to ensure the quality of the lens, and the data of each non-conforming type of the lens can be plotted and sent to the user.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lens manufacturing, and in particular to a method for manufacturing a reinforced resin lens. Background Art

[0002] The main categories of optical resin lenses currently include acrylic series, polystyrene (PS), polycarbonate (PC), styrene-acrylonitrile copolymer (SAN), poly-4-methylpentene-1 (TPX) and allyl diglycol dicarbonate (trade name CR-39). The key to manufacturing resin lenses is to choose the right resin material. Different resin materials have very different performance, optical properties, wear resistance, light resistance and other aspects. It is necessary to have an in-depth understanding of the characteristics of various resins and optimize the performance of the resin by adjusting the formula and adding specific additives. In addition, the optical parameters of the lens such as refractive index, scattering, dispersion, and light transmittance should be optimized, and defects such as pitting, bubbles, lint and scratches on the lens should be considered (such as Figure 5 ), thereby ensuring that clear and accurate vision can be provided. Moreover, in the actual production process of resin lenses, the liquid level of the resin in the glass mold is basically observed by naked eyes, and then the control valve is closed to prevent the resin from overflowing. This method often causes insufficient or excessive pouring. Insufficient pouring will lead to reduced pouring quality and greatly increased defective rate, and excessive pouring will cause waste. In view of the above problems, the present invention proposes a method for manufacturing enhanced resin lenses. Summary of the invention

[0003] The invention aims to provide a method for manufacturing an enhanced resin lens, which has the advantages of quantitative accurate casting and quality detection.

[0004] To achieve the above object, the present invention proposes the following technical solution: a method for manufacturing an enhanced resin lens, characterized in that it includes the following steps:

[0005] The first step is to prepare monomer materials and auxiliary materials, wherein the monomer materials include styrene, tetramethylolpropane tetraacrylate, and ethoxylated bisphenol A diacrylate, and the auxiliary materials include colorants, antioxidants, and initiators, and the monomer materials and auxiliary materials are mixed to prepare a casting liquid;

[0006] In the second step, the pouring liquid obtained in the first step is poured into the glass mold through the filling unit. During the quantitative pouring process of the filling unit, the liquid detection unit monitors the pouring liquid in the glass mold. After the pouring is qualified, it is placed in the high-temperature molding unit for one-time curing and molding;

[0007] The liquid detection unit obtains the image data of the glass mold through the image acquisition module, and the image of the glass mold includes vertical image data and horizontal image data. The time point when the image acquisition module starts to obtain the image data of the glass mold is determined to be T2 by analyzing the historical data, and the gap value of the glass mold, the height value of the top liquid level and the arc value of the outer edge that is not poured are obtained. The unpoured volume value P in the glass mold is calculated, and the quantitative pouring remaining amount of the filling unit is quantitatively controlled so that the quantitative pouring remaining amount is equal to the unpoured volume value.

[0008] The third step is to take out the molded lens after the mold is opened, trim and clean it through the cleaning unit lens, and then perform secondary curing on the lens to obtain the finished substrate lens after the mold is opened.

[0009] The fourth step is to coat the surface. The substrate lens is placed on a coating machine, a transparent coating is applied to the substrate lens, and the lens surface is additionally processed. After that, the lens defect detection and optical performance detection are performed by the lens quality detection unit.

[0010] The detection unit sets the thresholds of the lens refractive index, dispersion, and transmittance as n1, V d 1. T t If the refractive index, dispersion and transmittance parameter values ​​of the tested lens do not meet the requirements, it will be marked as a defective product and marked as a non-conforming type. Then, the data of each non-conforming type of the lens will be plotted in a chart and sent to the user.

[0011] Furthermore, in the present invention, the initiator is azobis(tert-butyl 2-cyanoacrylate), the colorant is an organic pigment, and the antioxidant is mercaptopropanol.

[0012] Furthermore, in the present invention, in the first step, styrene, tetramethylolpropane tetraacrylate, ethoxylated bisphenol A diacrylate, azobis(tert-butyl 2-cyanoacrylate), organic pigment, and mercaptopropane alcohol are mixed in a beaker to ensure that the proportions of the various components are accurate. Under the action of an initiator, vacuum is drawn at 40° C. for 60 minutes, and an oscillator is used to continuously shake and mix the mixture to obtain a casting solution.

[0013] Furthermore, in the present invention, in the second step, the single filling volume data within a specific time of the filling unit is obtained; the filling volume data includes the time and volume of each filling, the filling time and volume data are sorted from small to high, and the filling time and volume average values ​​T1 and V1 are determined, and the detection time T2 is obtained through the filling time T1, T2= T1÷2.

[0014] Furthermore, in the present invention, at time point T2, the image acquisition module starts to acquire image data of the glass mold, and the image of the glass mold acquired includes vertical image data and horizontal image data. The vertical image data is used to calculate the small gap value between the upper mold and the lower mold of the glass mold, and the horizontal image data is used to obtain the height of the top liquid level during pouring, and then calculate the volume value P to be poured, and adjust the remaining filling amount V2 of the filling unit, V2=P.

[0015] Furthermore, in the present invention, vertical image data is acquired starting from time T2, bilateral filtering is used to reduce image noise, and histogram equalization is used to enhance the denoised image. The bright area with high grayscale value is the edge thickness of the glass mold, and the distance between the two bright areas is the gap between the two molds. Edge detection is performed on the image after noise reduction and contrast enhancement, and then the edge of the glass mold gap is extracted, and the broken edge part of the discontinuous edge is repaired by using an image repair algorithm. The image repair algorithm can fill the broken part based on local pixel information or global image features, and then the Sobel edge detection algorithm is used to make the broken edge clearer and continuous, and then the small gap value between the upper mold and the lower mold of the glass mold is calculated.

[0016] Furthermore, in the present invention, the horizontal image data acquired at time T2 is smoothed using a Gaussian kernel to reduce the influence of noise. The Gaussian filter blurs the image by weighted averaging the pixel values ​​around each pixel, so that the high-frequency noise in the image is blurred, thereby reducing the influence of noise while retaining the main structure and features of the image. The image after noise removal is divided into regions and the local segmentation threshold corresponding to each region is obtained;

[0017] The calculation method of the local segmentation threshold is as follows:

[0018] ;

[0019] ;

[0020] (x, y) is the coordinate of the target pixel, g(x, y) is the gray value, r×r is the area centered on the coordinate point, m(x, y) is the gray mean in the area, and s(x, y) is the gray variance in the area;

[0021] Obtain the local segmentation threshold T(x, y) based on s(x, y) and m(x, y):

[0022] ;

[0023] T(x, y) is the local segmentation threshold, m(x, y) is the grayscale mean in the domain, s(x, y) is the grayscale variance in the domain, k is the correction parameter, and R is the dynamic range of the standard variance;

[0024] A binary image is obtained through the local segmentation threshold. The binary image can show the height of the top liquid level and the uncast arc surface of the outer edge of the glass mold. The height value of the top liquid level and the uncast arc surface value of the outer edge of the glass mold are obtained. The uncast volume value P in the glass mold is calculated through the gap value, height value and uncast arc surface value of the glass mold, and the quantitative pouring remaining amount of the filling unit is quantitatively controlled so that the quantitative pouring remaining amount is equal to the uncast volume value.

[0025] Furthermore, in the present invention, in the fourth step, a transparent silica coating is applied to the substrate lens on a coating machine.

[0026] Furthermore, in the present invention, in the fourth step, the detection unit processes the image as follows:

[0027] Reduce image noise and segment the image, use feature extraction to obtain the features of the segmented defect area, and finally use RBF neural network to identify the defect type;

[0028] The RBF neural network includes an input layer, a hidden layer, and an output layer. The transfer function of the hidden layer is a Gaussian kernel function, and the transfer function of the output layer is a linear function.

[0029]

[0030] ci is the center of the ith basis function, σi is the variable of the ith perception, m is the number of perception units, ‖x-ci‖ is the norm of x-ci, which represents the Euclidean distance between x and ci;

[0031] The refractive index is calculated as follows:

[0032] ;

[0033] ;

[0034] ;

[0035] R is the molar refractive index; n is the refractive index; ρ is the density; M is the relative molecular weight; V is the molar volume; N A is Avogadro's constant; γ is the polarizability of the medium.

[0036] The calculation method of dispersion is as follows:

[0037] ;

[0038] ;

[0039] is the molecular dispersion, which is proportional to the difference in polarizability between the λ1 and λ2 wavelength media;

[0040] Where nD, nF, nC are the refractive indices corresponding to the D line (587.56nm), F line (486.13nm), and C line (656.28nm) in the corresponding Flaunhofer line of the solar spectrum;

[0041] Translucent T t The detection formula is as follows:

[0042] ;

[0043] Where T2 is the luminous flux passing through the lens, and T1 is the luminous flux incident on the lens surface.

[0044] Beneficial effects: The technical solution of this application has the following technical effects:

[0045] The present invention can achieve precise quantitative filling, high detection accuracy, and improve the yield rate. By setting the detection time, the detection amount can be reduced and the detection efficiency can be improved. The refractive index, dispersion and light transmittance can be detected during the production process of resin lenses to ensure the quality of the lenses. The data of each non-conforming type of the lenses can be plotted in a chart and sent to the user.

[0046] It should be appreciated that all combinations of the foregoing concepts, as well as additional concepts described in greater detail below, may be considered to be part of the inventive subject matter of the present disclosure, provided such concepts are not mutually inconsistent.

[0047] The foregoing and other aspects, embodiments and features of the present invention can be more fully understood from the following description in conjunction with the accompanying drawings. Other additional aspects of the present invention, such as the features and / or beneficial effects of the exemplary embodiments, will be apparent from the following description or learned from the practice of the specific embodiments according to the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] The drawings are not intended to be drawn to scale. In the drawings, each identical or nearly identical component shown in various figures may be represented by the same reference numeral. For clarity, not every component is labeled in every figure. Embodiments of various aspects of the present invention will now be described by way of example and with reference to the accompanying drawings, in which:

[0049] Figure 1 It is a schematic diagram of the process of the present invention.

[0050] Figure 2It is a schematic diagram of the processing process of the present invention.

[0051] Figure 3 It is a schematic diagram of the gap between the upper mold and the lower mold of the glass mold of the present invention.

[0052] Figure 4 It is a binary image of the present invention.

[0053] Figure 5 Schematic diagram of lens defects in the prior art of the present invention.

[0054] Figure 6 Schematic diagram of the RBF neural network of the present invention. DETAILED DESCRIPTION

[0055] In order to better understand the technical content of the present invention, specific embodiments are cited and described as follows in conjunction with the accompanying drawings. Various aspects of the present invention are described in this disclosure with reference to the accompanying drawings, in which many illustrative embodiments are shown. The embodiments of the present disclosure are not necessarily defined to include all aspects of the present invention. It should be understood that the various concepts and embodiments introduced above, as well as those described in more detail below, can be implemented in any of many ways, because the concepts and embodiments disclosed in the present invention are not limited to any implementation. In addition, some aspects disclosed in the present invention can be used alone, or in any appropriate combination with other aspects disclosed in the present invention.

[0056] A method for manufacturing an enhanced resin lens comprises the following steps:

[0057] The first step is to prepare the required resin monomer raw materials, colorants, antioxidants and initiators. The resin monomer raw materials are styrene, tetramethylolpropane tetraacrylate, and ethoxylated bisphenol A diacrylate. The initiator is azobis(tert-butyl 2-cyanoacrylate), and the colorant is an organic pigment. The materials are weighed according to the formula requirements, and the above materials are mixed in a beaker to ensure that the proportions of various components are accurate. Under the action of the initiator, vacuum is drawn at 40° C. for 60 minutes, and an oscillator is used to continuously shake and mix evenly to obtain a casting liquid.

[0058] Step 2: Pour the pouring liquid in the beaker of the first step into the glass mold through the filling unit. During the quantitative pouring process of the filling unit, the liquid detection unit monitors the pouring liquid in the glass mold. After the pouring is qualified, it is placed in the high-temperature molding unit for one-time curing and molding.

[0059] The filling unit includes a lens filling machine. The lens mold that needs to be prepared for pouring is placed under the lens filling machine. The lens mold has the required shape of the lens. The lens mold uses a glass mold, and the liquid material to be poured in the first step is loaded into the liquid supply system of the machine. The liquid supply system includes a liquid storage tank, a delivery pipeline and a control valve to ensure that the liquid material is accurately delivered to the mold. After the glass mold is accurately positioned, ensure that the sealing is good to prevent liquid overflow, start the lens filling machine, and control the valve of the liquid supply system to slowly and evenly inject the liquid material into the mold. The injection process must control the injection speed, pressure and time to ensure the quality and consistency of the lens. The liquid material fills the glass mold and reaches the required shape. Curing is achieved by heating to convert the liquid material into a solid material. After curing is completed, the mold is removed from the machine and the cured lens is removed from the mold.

[0060] The third step is to take out the molded lens after the mold is opened, trim and clean it through the cleaning unit lens, and then perform secondary curing on the lens to obtain the finished substrate lens after the mold is opened.

[0061] The fourth step is to coat the surface. Place the substrate lens on a coating machine and apply a transparent coating on the substrate lens. The substrate lens on the coating machine is coated with a transparent coating of silica. The transparent coating of silica can improve the hardness and wear resistance of the lens, while improving the optical performance. The lens surface is then additionally processed and then the lens defect detection and optical performance detection are carried out through the lens quality inspection unit.

[0062] In the second step, the detection process of the liquid detection unit is as follows:

[0063] Get the single filling volume data within a specific time of the filling unit; the filling volume data includes the time and volume of each filling, the filling time and volume data are sorted from small to large, and the filling time and volume average values ​​T1 and V1 are determined. The detection time T2 is obtained through the filling time T1, T2= T1÷2, thereby reducing the image data volume, which helps to improve the detection efficiency;

[0064] At time point T2, the image acquisition module starts to acquire image data of the glass mold. The image of the glass mold includes vertical image data and horizontal image data. The vertical image data is used to calculate the small gap value between the upper mold and the lower mold of the glass mold. The horizontal image data is used to obtain the height of the top liquid level during pouring, and then calculate the volume value P to be poured, and adjust the remaining filling volume V2 of the filling unit, V2=P.

[0065] Among them, vertical image data is acquired starting from time T2, bilateral filtering is used to reduce image noise, and histogram equalization is used to enhance the denoised image. The bright area with high grayscale value is the edge thickness of the glass mold, and the distance between the two bright areas is the gap between the two molds. Edge detection is performed on the image after noise reduction and contrast enhancement to extract the edge of the glass mold gap, and the image restoration algorithm is used to repair the broken edge part of the discontinuous edge. The image restoration algorithm can fill the broken part based on local pixel information or global image features, and then the Sobel edge detection algorithm is used to make the broken edge clearer and continuous, and then the small gap value between the upper mold and the lower mold of the glass mold is calculated, such as Figure 3 shown.

[0066] Among them, the Gaussian kernel is used to smooth the horizontal image data obtained at time T2 to reduce the influence of noise. The Gaussian filter blurs the image by weighted averaging the pixel values ​​around each pixel, so that the high-frequency noise in the image will be blurred, thereby reducing the influence of noise and retaining the main structure and features of the image. The image with noise removed is divided into regions and the local segmentation threshold corresponding to each region is obtained;

[0067] The calculation method of the local segmentation threshold is as follows:

[0068] ;

[0069] ;

[0070] (x, y) is the coordinate of the target pixel, g(x, y) is the gray value, r×r is the area centered on the coordinate point, m(x, y) is the gray mean in the area, and s(x, y) is the gray variance in the area;

[0071] Obtain the local segmentation threshold T(x, y) based on s(x, y) and m(x, y):

[0072] ;

[0073] T(x, y) is the local segmentation threshold, m(x, y) is the grayscale mean in the domain, s(x, y) is the grayscale variance in the domain, k is the correction parameter, and R is the dynamic range of the standard variance;

[0074] The binary image is obtained by local segmentation threshold, and the height of the top liquid level and the uncast arc surface of the outer edge of the glass mold can be displayed in the binary image, such as Figure 4As shown, the height value of the top liquid level and the uncast arc value of the outer edge of the glass mold are obtained, and the uncast volume value P in the glass mold is calculated through the glass mold gap value, height value and uncast arc value of the outer edge, and the quantitative pouring remaining amount of the filling unit is quantitatively controlled so that the quantitative pouring remaining amount is equal to the uncast volume value.

[0075] In the fourth step, the detection unit includes an industrial camera and an LED light source, and the detection unit processes the image as follows:

[0076] Reduce image noise and segment the image, specifically S-curve transformation, region of interest extraction, Gaussian filtering, binarization and contour extraction, extract the defect area of ​​the lens, use feature extraction to obtain the features of the segmented defect area, and finally use RBF neural network to identify the defect type, such as Figure 6 shown.

[0077] The RBF neural network of the present invention comprises an input layer, a hidden layer and an output layer, the transfer function of the hidden layer is a Gaussian kernel function, and the transfer function of the output layer is a linear function;

[0078]

[0079] ci is the center of the ith basis function, σi is the variable of the ith perception, m is the number of perception units, ‖x-ci‖ is the norm of x-ci, which represents the Euclidean distance between x and ci.

[0080] In the fourth step, the detection unit includes an Abbe refractometer, and the thresholds of the refractive index, dispersion, and transmittance of the lens are set to n1, V d 1. T t If the refractive index and dispersion of the detected lens do not meet the requirements, it will be marked as defective and the non-conforming type will be marked. Then the data of each non-conforming type of the lens will be plotted in a chart and sent to the user.

[0081] The refractive index is calculated as follows:

[0082] ;

[0083] ;

[0084] ;

[0085] R is the molar refractive index; n is the refractive index; ρ is the density; M is the relative molecular weight; V is the molar volume; N A is Avogadro's constant; γ is the polarizability of the medium.

[0086] The calculation method of dispersion is as follows:

[0087] ;

[0088] ;

[0089] is the molecular dispersion, which is proportional to the difference in polarizability between the λ1 and λ2 wavelength media;

[0090] Where nD, nF, and nC are the refractive indices corresponding to the D line (587.56nm), F line (486.13nm), and C line (656.28nm) in the corresponding Flaunhofer line of the solar spectrum.

[0091] Translucent T t The detection formula is as follows:

[0092] ;

[0093] Where T2 is the luminous flux passing through the lens, and T1 is the luminous flux incident on the lens surface.

[0094] Although the present invention has been disclosed as above with preferred embodiments, it is not intended to limit the present invention. A person with ordinary knowledge in the technical field to which the present invention belongs may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be determined by the definition of the claims.

Claims

1. A method for manufacturing an enhanced resin lens, characterized in that: The process includes the following: The first step is to prepare monomer materials and auxiliary materials, wherein the monomer materials include styrene, tetramethylolpropane tetraacrylate, and ethoxylated bisphenol A diacrylate, and the auxiliary materials include colorants, antioxidants, and initiators, and the monomer materials and auxiliary materials are mixed to prepare a casting liquid; In the second step, the pouring liquid obtained in the first step is poured into the glass mold through the filling unit. During the quantitative pouring process of the filling unit, the liquid detection unit monitors the pouring liquid in the glass mold. After the pouring is qualified, it is placed in the high-temperature molding unit for one-time curing and molding; The liquid detection unit obtains the image data of the glass mold through the image acquisition module, and the image of the glass mold includes vertical image data and horizontal image data. The time point when the image acquisition module starts to obtain the image data of the glass mold is determined to be T2 by analyzing the historical data, and the gap value of the glass mold, the height value of the top liquid level and the arc value of the outer edge that is not poured are obtained. The unpoured volume value P in the glass mold is calculated, and the quantitative pouring remaining amount of the filling unit is quantitatively controlled so that the quantitative pouring remaining amount is equal to the unpoured volume value. The third step is to take out the molded lens after the mold is opened, perform edge trimming and cleaning through the cleaning unit lens, and then perform secondary curing on the lens, and obtain the finished substrate lens after the mold is opened; The fourth step is to coat the surface. The substrate lens is placed on a coating machine, a transparent coating is applied to the substrate lens, and the lens surface is additionally processed. After that, the lens defect detection and optical performance detection are performed by the lens quality detection unit. The detection unit sets the thresholds of the lens refractive index, dispersion, and transmittance as n1, V d 1. T t If the refractive index, dispersion and transmittance parameter values ​​of the tested lens do not meet the requirements, it will be marked as defective and the non-conforming type will be marked. Then, the data of each non-conforming type of the lens will be plotted and sent to the user; The initiator is azobis(tert-butyl 2-cyanoacrylate), the colorant is an organic pigment, and the antioxidant is mercaptopropane alcohol; In the first step, styrene, tetramethylolpropane tetraacrylate, ethoxylated bisphenol A diacrylate, azobis(tert-butyl 2-cyanoacrylate), organic pigment, and mercaptopropane alcohol are mixed in a beaker to ensure that the proportions of the various components are accurate. Under the action of an initiator, vacuum is drawn at 40° C. for 60 minutes, and an oscillator is used to continuously shake and mix the mixture to obtain a casting solution. In the second step, the single filling volume data within a specific time of the filling unit is obtained; the filling volume data includes the time and volume of each filling, and the filling time and volume data are sorted from small to high, and the filling time and volume average values ​​T1 and V1 are determined. The detection time T2 is obtained through the filling time T1, T2= T1÷2; At time point T2, the image acquisition module starts to acquire image data of the glass mold. The image of the glass mold includes vertical image data and horizontal image data. The vertical image data is used to calculate the small gap value between the upper mold and the lower mold of the glass mold. The horizontal image data is used to obtain the height of the top liquid level during pouring, and then calculate the volume value P to be poured, and adjust the remaining filling volume V2 of the filling unit, V2=P; At T2, vertical image data is acquired, bilateral filtering is used to reduce image noise, and histogram equalization is used to enhance the denoised image. The bright area with high grayscale value is the edge thickness of the glass mold, and the distance between two bright areas is the gap between the two molds. Edge detection is performed on the image after noise reduction and contrast enhancement to extract the edge of the glass mold gap, and the image restoration algorithm is used to repair the broken edge part of the discontinuous edge. The image restoration algorithm can fill the broken part based on local pixel information or global image features, and then the Sobel edge detection algorithm is used to make the broken edge clearer and continuous, and then the small gap value between the upper mold and the lower mold of the glass mold is calculated. The horizontal image data acquired at time T2 is smoothed using the Gaussian kernel to reduce noise. The Gaussian filter blurs the image by weighted averaging the pixel values ​​around each pixel, so that the high-frequency noise in the image is blurred, the noise is reduced, and the core structure and features of the image are retained. The image with the noise removed is divided into regions and the local segmentation threshold corresponding to each region is obtained. The calculation method of the local segmentation threshold is as follows: ; ; (x, y) is the coordinate of the target pixel, g(x, y) is the gray value, r×r is the area centered on the coordinate point, m(x, y) is the gray mean in the area, and s(x, y) is the gray variance in the area; Obtain the local segmentation threshold T(x, y) based on s(x, y) and m(x, y): ; T(x, y) is the local segmentation threshold, m(x, y) is the grayscale mean in the domain, s(x, y) is the grayscale variance in the domain, k is the correction parameter, and R is the dynamic range of the standard variance; A binary image is obtained through a local segmentation threshold, and the height of the top liquid level and the uncast arc surface of the outer edge of the glass mold can be displayed in the binary image. The height value of the top liquid level and the uncast arc surface value of the outer edge of the glass mold are obtained, and the uncast volume value P in the glass mold is calculated through the gap value, height value and uncast arc surface value of the glass mold, and the quantitative pouring remaining amount of the filling unit is quantitatively controlled so that the quantitative pouring remaining amount is equal to the uncast volume value; In the fourth step, the detection unit processes the image as follows: Reduce image noise and segment the image, use feature extraction to obtain the features of the segmented defect area, and finally use RBF neural network to identify the defect type; The RBF neural network includes an input layer, a hidden layer, and an output layer. The transfer function of the hidden layer is a Gaussian kernel function, and the transfer function of the output layer is a linear function. ci is the center of the ith basis function, σi is the variable of the ith perception, m is the number of perception units, ‖x-ci‖ is the norm of x-ci, which represents the Euclidean distance between x and ci; The refractive index is calculated as follows: ; ; ; R is the molar refractive index; n is the refractive index; ρ is the density; M is the relative molecular weight; V is the molar volume; N A is Avogadro's constant; γ is the polarizability of the medium; The calculation method of dispersion is as follows: ; ; is the molecular dispersion, which is proportional to the difference in polarizability between the λ1 and λ2 wavelength media; Where nD, nF, nC are the refractive indices corresponding to the D line (587.56nm), F line (486.13nm), and C line (656.28nm) in the corresponding Flaunhofer line of the solar spectrum; Translucent T t The detection formula is as follows: ; Where T2 is the luminous flux passing through the lens, and T1 is the luminous flux incident on the lens surface.

2. The method for manufacturing a reinforced resin lens according to claim 1, characterized in that: In the fourth step, a transparent coating of silicon dioxide is applied to the substrate lens on a coating machine.