A pre-blow molding method based on injection blow molding machine
By acquiring molding data and preset mold data, combining material thickness distribution and auxiliary blowing guidance control, the problem of uneven wall thickness in injection blowing hollow molding is solved, and the quality and efficiency of the pre-blown molding body are improved.
Patent Information
- Application Number
- CN202410932230.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-12
AI Technical Summary
During the injection-blowing hollow molding process, the wall thickness and unevenness caused by large deformation of the shape of the blow molding stage are difficult to ensure the quality of the pre-blowing molding body.
By obtaining the molding data of the target molding part and the pre-blowing mold data, the target wall thickness of the pre-blowing body is determined based on the wall thickness and blow-pull deformation variables, and the material thickness distribution control method and auxiliary blow-pushing guidance control method are used to adjust the raw materials and blow pressure to achieve uniform control of wall thickness.
The blow molding quality and efficiency of the pre-blown molded body are improved, and the uneven wall thickness and blow-breaking problems of molded parts are avoided, ensuring the quality of the final product.
Smart Images

Figure CN118456834B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of injection blow molding, and in particular to a pre-blow molding method based on an injection blow hollow molding machine. Background Art
[0002] Injection blow molding machine is an advanced equipment for producing hollow plastic products. Its technical background covers many fields such as plastic processing, molding process and automatic control. The core of this technology lies in the combination of injection molding and blow molding. The molten plastic is injected into the injection mold by the injection machine to form a tube blank, which is formed on the core rod with micropores on the wall; Then it is moved to the blow mold while hot; Then the mold is closed and compressed air is introduced from the pipe of the core rod to blow the raw material and stick it to the cavity wall of the blow mold; Finally, after pressure maintenance and cooling, the compressed air is released and the mold is opened to take out the hollow structure plastic part. This molding method is widely used in the production of various plastic products such as bottles, containers, toys, etc., and how to ensure that the quality of blow molded products meets the expected standards is a hot topic that people are currently committed to studying. In the blow molding process, the raw material needs to be expanded and molded under the action of air pressure. Due to the large size gap between the blow molded body and the raw material, the blow molded body is prone to breakage, deformation or uneven thickness during molding. In order to avoid the above problems, pre-blow molding is usually introduced before formal blow molding for transition to ensure the quality of the final product.
[0003] Chinese Patent Authorization Announcement No.: CN103079796B discloses a method for manufacturing a container from a rough blank by using feedback based on the detection of a minimum pressure value, comprising: measuring the internal pressure of the rough blank in the pre-blowing stage; detecting the moment corresponding to the local minimum pressure in the rough blank; storing the moment when the pressure minimum is generated and the corresponding pressure in the rough blank; comparing the moment and pressure of the detected local minimum pressure value with the predetermined moment and pressure of the theoretical minimum pressure value, respectively; if the measured minimum value and the theoretical minimum value do not coincide, controlling to change at least one of the following parameters: pre-blowing pressure, pre-blowing flow rate, stretching speed, heating temperature.
[0004] It can be seen that the method provided by the invention for manufacturing containers from rough blanks by using feedback based on the detected minimum pressure value has the following problems: it is only based on comparing the moment and pressure of the detected local minimum pressure value with the predetermined moment and pressure of the theoretical minimum pressure value, so as to judge whether it is necessary to change the pre-blowing parameters in the pre-blowing stage. The factors affecting the rough blank (pre-finished raw material or intermediate container) are not considered comprehensively, and it is difficult to ensure the quality of the rough blank, that is, it is difficult to ensure the quality of the pre-blown body. Summary of the invention
[0005] To this end, the present invention provides a pre-blow molding method based on an injection blow molding machine to overcome the problem of uneven wall thickness caused by large wall thickness and shape deformation in the blow molding stage in the prior art.
[0006] To achieve the above object, on the one hand, the present invention provides a pre-blow molding method based on an injection blow molding machine, comprising:
[0007] Step S1, obtaining molding data and pre-blow mold data of a target molded part;
[0008] Step S2, determining the target wall thickness of the corresponding position of the pre-blow molded body according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation amount during the molding process;
[0009] Step S3, determining a wall thickness control method of the pre-blow molding process based on the maximum difference in target wall thicknesses at adjacent positions of the pre-blow molding body, including a material thickness distribution control method and an auxiliary blowing guide control method;
[0010] in,
[0011] Under the first relative difference condition, the material thickness distribution control method is used to determine the wall thickness adjustment area according to the area of the position with the maximum blowing and stretching deformation in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions;
[0012] Under the second relative difference condition, the auxiliary blowing guide control mode is used to determine the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow molded body and the internal blowing pressure of the core rod;
[0013] The maximum difference corresponding to the second relative difference condition is greater than the maximum difference corresponding to the first relative difference condition.
[0014] Furthermore, in step S3, the auxiliary blowing guide control method includes:
[0015] The pre-blow molded body is formed in a pre-blow mold, and the pre-blow mold is provided with a corresponding air outlet to perform the external blowing pressure;
[0016] During the pre-blow molding process, the raw material on the core rod is blown simultaneously from both sides of the raw material wall thickness with the internal blowing pressure and the corresponding external blowing pressure to complete the pre-blow molding process.
[0017] Furthermore, in the step S3, the material thickness distribution control method includes:
[0018] Adjusting the distribution of the raw material on the mandrel according to the wall thickness adjustment area and the wall thickness adjustment amount;
[0019] During the pre-blow molding process, the raw material on the core rod is blown from the core rod side according to the corresponding internal blowing pressure to complete the pre-blow molding process.
[0020] Furthermore, in the step S2, it includes:
[0021] Step S21, constructing a characteristic parameter model according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation amount during the molding process;
[0022] Step S22: reversely simulating the blow molding process of the target molded body according to the characteristic parameter model to obtain the target wall thickness of the corresponding position of the pre-blow molded body.
[0023] Furthermore, in the step S3, determining the wall thickness control method of the pre-blow molding process includes:
[0024] If the maximum difference is greater than the first preset threshold, it is determined that the second relative difference condition is met, and the auxiliary blowing guidance control method is used;
[0025] If the maximum difference is not greater than the first preset threshold, it is determined that the first relative difference condition is met and the material thickness distribution control method is used.
[0026] Further, in the step S3, determining the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow mold and the internal blowing pressure of the core rod includes:
[0027] Constructing a pressure-wall thickness model according to the target wall thickness of each adjacent position of the pre-blow molded body and the blowing pressure inside the core rod;
[0028] The external blowing pressure at the corresponding position of the pre-blow mold is determined according to the pressure-wall thickness model.
[0029] Further, in the step S3, the wall thickness adjustment region is determined according to the area of the position with the maximum blow-stretch deformation in the pre-blow molding process and the wall thickness difference between the corresponding adjacent positions, including:
[0030] Determine the raw material region on the mandrel corresponding to the region having an area greater than a preset area or a wall thickness difference between adjacent positions greater than a preset wall thickness difference as a wall thickness adjustment region;
[0031] The wall thickness adjustment amount is calculated according to the area of the position with the maximum blow-stretch deformation amount in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions.
[0032] Further, under the third relative difference condition, blow molding is performed according to the blowing pressure inside the core rod;
[0033] Among them, the maximum difference corresponding to the third relative difference condition is smaller than the maximum difference corresponding to the first relative difference condition.
[0034] Further, the maximum difference is calculated based on the maximum radial deformation of the pre-blow molded body within a preset length in the axial direction of the core rod;
[0035] The preset length is determined according to the ratio of the dimension of the pre-blow mold along the axial direction of the core rod to the number of axial deformations.
[0036] Furthermore, when the auxiliary blowing guide control method is used, the corresponding external blowing position is determined according to the maximum position of the blowing and stretching deformation amount in the pre-blow molding process.
[0037] Compared with the prior art, the beneficial effect of the present invention lies in that the present invention determines the target wall thickness of the corresponding position of the pre-blown body according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation of the molding process, and determines the wall thickness control method of the pre-blowing process based on the maximum difference in the target wall thickness of adjacent positions of the pre-blown body, including a material thickness distribution control method and an auxiliary blowing guide control method, which can more accurately control the target wall thickness of the pre-blown body, thereby improving the blow molding quality of the pre-blown body.
[0038] Furthermore, the auxiliary blowing guide control method adjusts the wall thickness of the raw material by combining the external blowing pressure performed by each air outlet of the pre-blow molding mold with the internal blowing pressure of the core rod to complete the pre-blow molding process. Under the joint action of the internal and external blowing pressures, the target wall thickness can be achieved quickly and evenly, avoiding the situation where the pre-blow molding body is unevenly blown by relying solely on the core rod blowing, and can improve the blow molding efficiency and quality of the pre-blow molding body.
[0039] Furthermore, the material thickness distribution control method can timely adjust the wall thickness of the raw material on the core rod where the force is uneven by adjusting the wall thickness of the raw material before pre-blow molding, thereby assisting the formation of the pre-blow molded body and making the material thickness distribution more uniform during the pre-blow molding process, thereby avoiding the blow-out of the molded part due to the large wall thickness difference of the pre-blow molded body or the poor wall thickness quality due to the large wall thickness deviation, thereby improving the blow molding quality of the pre-blow molded body.
[0040] Furthermore, a characteristic parameter model is constructed according to the wall thickness and blowing deformation at each position of the molded part in the molding data to determine the target wall thickness at the corresponding position of the pre-blown body, which can improve the accuracy of determining the target wall thickness of the pre-blown body and thus improve the quality of the pre-blown body.
[0041] Further, the wall thickness control method of the pre-blowing process is determined according to the maximum difference of the target wall thickness of the adjacent positions of the pre-blowing body. If the maximum difference is not greater than the first preset threshold value and greater than the second preset threshold value, it indicates that the surface morphology difference of the adjacent positions of the pre-blowing body can be controlled by the material thickness distribution control method. By adjusting the wall thickness of each movable body at the corresponding position of the pre-blowing mold, the uniformity of the blow-molded wall thickness of the pre-blowing body can be improved. If the maximum difference is greater than the first preset threshold value, it indicates that the surface morphology difference of the adjacent positions of the pre-blowing body is large, and the blow molding difficulty of the pre-blowing body is relatively high. Only adjusting the wall thickness of each movable body at the corresponding position of the pre-blowing mold may cause uneven blow molding of the pre-blowing body. Through the auxiliary blowing guide control method, during the pre-blowing process, the raw material on the core rod is blown from both sides of the raw material wall thickness by the internal blowing pressure of the core rod and the corresponding external blowing pressure to complete the pre-blowing process, which can improve the blow molding efficiency of the pre-blowing body.
[0042] Furthermore, a pressure-wall thickness model is constructed based on the target wall thickness at each adjacent position of the pre-blow molded body and the blowing pressure inside the core rod to determine the blowing pressure at the corresponding external position. This can accurately determine the blowing pressure of the blow mold at each position and improve the blow molding quality of the pre-blow molded body.
[0043] Furthermore, the wall thickness adjustment area of the raw material on the core rod is determined based on the area of the position with the maximum blowing deformation in the molding process and the difference in wall thickness at the corresponding adjacent positions. If there is a wall thickness adjustment area, it indicates that the area of the position with the maximum blowing deformation at the corresponding position is large or the difference in wall thickness at the corresponding adjacent positions is large, both of which will lead to large wall thickness deviation during the pre-blow molding process, thereby making the blow-molded wall thickness uneven and requiring wall thickness adjustment.
[0044] Furthermore, under the third relative difference condition, it is shown that the blow-molded wall thickness of the pre-blown body changes little, and no corresponding wall thickness control method is required to assist blow molding. The blow molding of the pre-blown body can be completed by blowing only through the air outlets of the core rod, which can improve the blow molding efficiency of the pre-blown body. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 It is a schematic diagram of the steps of the pre-blow molding method based on the injection blow molding machine of the present invention;
[0046] Figure 2 It is a step-by-step schematic diagram of step S2 of the present invention;
[0047] Figure 3 It is a logic decision diagram of the wall thickness control method of the present invention. DETAILED DESCRIPTION
[0048] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0049] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.
[0050] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.
[0051] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0052] See also Figure 1 and Figure 3 As shown, Figure 1 Schematic diagram of the steps of the pre-blow molding method based on the injection blow molding machine of the present invention, Figure 3 The embodiment of the present invention provides a pre-blow molding method based on an injection blow molding machine, comprising:
[0053] Step S1, obtaining molding data and pre-blow mold data of a target molded part;
[0054] Specifically, the molding data of the target molded part includes: the three-dimensional size data of the target molded part, the wall thickness at each position, and the surface flatness. The pre-blow mold data includes: the mechanical structure of the pre-blow mold, the mold size, and the three-dimensional size data of the cavity. Among them, the blowing and stretching deformation at each position of the molding process can be calculated based on the three-dimensional size data of the target molded part and the three-dimensional size data of the cavity of the pre-blow mold.
[0055] Step S2, determining the target wall thickness of the corresponding position of the pre-blow molded body according to the wall thickness of each position of the target molded part in the molding data and the amount of blow-stretch deformation during the molding process.
[0056] See also Figure 2 , which is a step-by-step schematic diagram of step S2 of the present invention, wherein step S2 includes:
[0057] Step S21, constructing a characteristic parameter model according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation amount during the molding process;
[0058] Step S22: reversely simulating the blow molding process of the target molded body according to the characteristic parameter model to obtain the target wall thickness of the corresponding position of the pre-blow molded body.
[0059] In a specific embodiment, the wall thickness at each position of the target molded part and the amount of blowing and stretching deformation during the molding process are compared with the initial state of the raw material, the wall thickness is used as the output, the amount of blowing and stretching deformation is used as the input, and a characteristic parameter model is constructed based on the physical change of plastic deformation. The blow molding process of the target molded body is reversely simulated based on the characteristic parameter model, so that the target wall thickness at the corresponding position can be obtained based on the amount of blowing and stretching deformation at each position of the pre-blow molded body.
[0060] The present invention constructs a characteristic parameter model according to the wall thickness of each position of the target molded part and the blowing and stretching deformation in the molding data to determine the target wall thickness of the corresponding position of the pre-blown body, which can improve the accuracy of determining the target wall thickness of the pre-blown body, thereby improving the quality of the pre-blown body.
[0061] Specifically, under the third relative difference condition, blow molding is performed according to the blowing pressure inside the core rod;
[0062] Among them, the maximum difference corresponding to the third relative difference condition is smaller than the maximum difference corresponding to the first relative difference condition.
[0063] Specifically, the third relative difference condition is that the maximum difference of the target wall thicknesses at adjacent positions of the pre-blow molded body is less than a second preset threshold.
[0064] Specifically, the maximum difference is calculated based on the maximum radial deformation of the pre-blow molded body within a preset length in the axial direction of the core rod;
[0065] Among them, the preset length is determined according to the ratio of the size of the pre-blow mold along the axial direction of the core rod to the number of axial deformations. For example, if the size of the pre-blow mold along the axial direction of the core rod is 25 cm and the number of axial deformations is 4 times, the preset length is set to 25 / 4=6.25 cm.
[0066] Specifically, during the injection blow molding process, the injection molding material is formed on a core rod with an air outlet on the peripheral wall and moved into a pre-blow molding mold. Then, blowing air is introduced from the pipe of the core rod for pre-blow molding, so that the raw material is blown and attached to the cavity wall of the pre-blow molding mold to form a pre-blow molding, completing the pre-blow molding process.
[0067] In a specific embodiment, if the maximum difference in target wall thickness at adjacent positions of the pre-blown body is less than a second preset threshold value, it indicates that the blow-molded wall thickness of the pre-blown body changes little, and no corresponding wall thickness control method is required to assist blow molding. The blow molding of the pre-blown body can be completed by blowing air through the air outlets of the core rod alone, thereby improving the blow molding efficiency of the pre-blown body.
[0068] Step S3, determining a wall thickness control method of the pre-blow molding process based on the maximum difference in target wall thicknesses at adjacent positions of the pre-blow molding body, including a material thickness distribution control method and an auxiliary blowing guide control method;
[0069] in,
[0070] Under the first relative difference condition, the material thickness distribution control method is used to determine the wall thickness adjustment area according to the area of the position with the maximum blowing and stretching deformation in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions;
[0071] Under the second relative difference condition, the auxiliary blowing guide control mode is used to determine the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow molded body and the internal blowing pressure of the core rod;
[0072] Specifically, in step S3, determining the wall thickness control method of the pre-blow molding process includes:
[0073] If the maximum difference is greater than the first preset threshold, it is determined that the second relative difference condition is met, and the auxiliary blowing guidance control method is used;
[0074] If the maximum difference is not greater than the first preset threshold and greater than the second preset threshold, it is determined that the first relative difference condition is met and the material thickness distribution control method is used.
[0075] It can be understood that the second preset threshold is smaller than the first preset threshold. In implementation, the actual implementer can set the first preset threshold and the second preset threshold based on the expert system according to the actual situation of the target wall thickness at adjacent positions of the pre-blown body, or calculate in the following way: calculate the average wall thickness L at each position of the pre-blown body, then the value range of the first preset threshold can be set to 1.2 times to 1.5 times of L, and the value range of the second preset threshold can be set to 0.9 times to 1.1 times of L.
[0076] In the present invention, the wall thickness control method of the pre-blowing process is determined according to the maximum difference of the target wall thickness of the adjacent positions of the pre-blowing body. If the maximum difference is not greater than the first preset threshold value and greater than the second preset threshold value, it indicates that the surface morphology difference of the adjacent positions of the pre-blowing body can be controlled by the material thickness distribution control method. By adjusting the wall thickness of each movable body at the corresponding position of the pre-blowing mold, the uniformity of the blow-molded wall thickness of the pre-blowing body can be improved. If the maximum difference is greater than the first preset threshold value, it indicates that the surface morphology difference of the adjacent positions of the pre-blowing body is large, and the blow molding difficulty of the pre-blowing body is relatively high. Only adjusting the wall thickness of each movable body at the corresponding position of the pre-blowing mold may cause uneven blow molding of the pre-blowing body. Through the auxiliary blowing guide control method, during the pre-blowing process, the raw material on the core rod is blown from both sides of the raw material wall thickness by the internal blowing pressure of the core rod and the corresponding external blowing pressure to complete the pre-blowing process, which can improve the blow molding efficiency of the pre-blowing body.
[0077] Specifically, in step S3, the material thickness distribution control method includes:
[0078] Adjusting the distribution of the raw material on the mandrel according to the wall thickness adjustment area and the wall thickness adjustment amount;
[0079] During the pre-blow molding process, the raw material on the core rod is blown from the core rod side according to the corresponding internal blowing pressure to complete the pre-blow molding process.
[0080] Specifically, the material thickness distribution control method can timely adjust the wall thickness of the raw material on the core rod at the position where the force is unevenly applied on the core rod by adjusting the wall thickness of the raw material before pre-blow molding, thereby assisting the formation of the pre-blow molded body and making the material thickness distribution more uniform during the pre-blow molding process. This avoids the blow-out of the molded parts due to large wall thickness differences of the pre-blow molded body or poor wall thickness quality due to large wall thickness deviations, thereby improving the blow molding quality of the pre-blow molded body.
[0081] Specifically, in the step S3, the wall thickness adjustment area of the injection molding material on the core rod is determined according to the area of the position with the maximum blow-stretch deformation in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions, including:
[0082] Determine the raw material region on the mandrel corresponding to the region having an area greater than a preset area or a wall thickness difference between adjacent positions greater than a preset wall thickness difference as a wall thickness adjustment region;
[0083] Calculate the wall thickness adjustment amount h according to the area of the position with the maximum blow-stretch deformation in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions;
[0084] Among them, the wall thickness adjustment h is determined by the following formula:
[0085] ;
[0086] in, To adjust the wall thickness of the injection molding material on the front core rod, is the area of the maximum blowing deformation in the pre-blow molding process, is the surface area of the pre-blow mold cavity; The maximum value of the wall thickness difference between adjacent positions corresponding to the position with the maximum blowing and stretching deformation in the pre-blow molding process; It is the average value of the target wall thickness corresponding to each position of the pre-blow molded body.
[0087] It can be understood that the wall thickness adjustment amount corresponds to the maximum position of the blowing and stretching deformation in the pre-blow molding process of the raw material area on the core rod or the maximum position of the wall thickness difference between adjacent positions, and the edge of the wall thickness adjustment area is evenly transitioned to smoothly connect with the wall thickness of the raw material area on the core rod that has not been adjusted.
[0088] In implementation, the preset area is determined according to the surface area of the pre-blow mold cavity. Preferably, the preset area is set to 0.2-0.4 times the surface area of the pre-blow mold cavity; the preset wall thickness difference is set to 0.5-0.8 times the average wall thickness of the injection molding material on the core rod.
[0089] Specifically, in actual application, the maximum position of the blowing and stretching deformation in the pre-blow molding process is the position of the maximum blowing and stretching deformation corresponding to the process of pre-blowing the injection molding raw material on the core rod to form a pre-blow molded body, and the blowing and stretching deformation control position is the position of the blowing and stretching deformation control value corresponding to the process of pre-blowing the injection molding raw material on the core rod to form a pre-blow molded body, and the area of the maximum blowing and stretching deformation position in the pre-blow molding process is the area of the raw material on the core rod extending from the maximum blowing and stretching deformation position to the blowing and stretching deformation control positions on both sides, wherein the blowing and stretching deformation control value is set to 0.8 times the maximum blowing and stretching deformation in the pre-blow molding process.
[0090] The present invention determines the wall thickness adjustment area of the raw material on the core rod according to the area of the position with the maximum blowing deformation in the molding process and the wall thickness difference of the corresponding adjacent positions. If the wall thickness adjustment area exists, it indicates that the area of the position with the maximum blowing deformation at the corresponding position is large or the wall thickness difference of the corresponding adjacent positions is large, both of which will lead to large wall thickness deviation in the pre-blow molding process, thereby making the blow-molded wall thickness uneven and requiring wall thickness adjustment.
[0091] Specifically, in step S3, the auxiliary blowing guide control method includes:
[0092] The pre-blow molded body is formed in a pre-blow mold, and the pre-blow mold is provided with a corresponding air outlet to perform the external blowing pressure;
[0093] During the pre-blow molding process, the raw material on the core rod is blown simultaneously from both sides of the raw material wall thickness with the internal blowing pressure and the corresponding external blowing pressure to complete the pre-blow molding process.
[0094] Specifically, the auxiliary blowing guide control method adjusts the wall thickness of the raw material by matching the external blowing pressure performed by each air outlet of the pre-blow molding mold with the internal blowing pressure of the core rod to complete the pre-blow molding process. Under the joint action of the internal and external blowing pressures, the target wall thickness can be achieved quickly and evenly, avoiding the situation where the pre-blow molding body is unevenly blown by relying solely on the core rod blowing, and can improve the blow molding efficiency and quality of the pre-blow molding body.
[0095] Specifically, in the step S3, determining the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow mold and the internal blowing pressure of the core rod includes:
[0096] Constructing a pressure-wall thickness model according to the target wall thickness of each adjacent position of the pre-blow molded body and the blowing pressure inside the core rod;
[0097] The external blowing pressure at the corresponding position of the pre-blow mold is determined according to the pressure-wall thickness model.
[0098] In a specific embodiment, a finite element analysis simulation can be performed on the blow molding process, and a neural network model between the target wall thickness and the optimization objective function can be established using the simulation results. The model is used to solve the objective function in the optimization iteration process in real time, and a multi-population parallel genetic algorithm is combined to obtain the target wall thickness. A mathematical model for wall thickness optimization is established, and the model is solved to obtain an optimized target wall thickness distribution curve. The optimized pressure-wall thickness model is determined based on the relationship between pressure and wall thickness obtained from the experiment.
[0099] The present invention constructs a pressure-wall thickness model according to the target wall thickness at each adjacent position of the pre-blown body and the blowing pressure inside the core rod, thereby determining the blowing pressure at the corresponding external position, and can accurately determine the blowing pressure of the blow mold at each position, thereby improving the blow molding quality of the pre-blown body.
[0100] The maximum difference corresponding to the second relative difference condition is greater than the maximum difference corresponding to the first relative difference condition.
[0101] It should be noted that the maximum difference corresponding to the second relative difference condition is greater than the maximum difference corresponding to the first relative difference condition, that is, when the maximum difference in target wall thickness at adjacent positions of the pre-blow molded body is small (under the first relative difference condition), the blow molding difficulty of the pre-blow molded body is relatively small, and the blow molding can be assisted by the material thickness distribution control method; but when the maximum difference in target wall thickness at adjacent positions of the pre-blow molded body is large (under the second relative difference condition), the blow molding difficulty of the pre-blow molded body is relatively large, and it is difficult to ensure the blow molding quality of the pre-blow molded body by assisting blow molding by means of material thickness distribution control. Therefore, it is necessary to assist blow molding by means of auxiliary blowing guide control, which can not only ensure the blow molding quality of the pre-blow molded body, but also improve the blow molding efficiency of the pre-blow molded body.
[0102] Specifically, when the auxiliary blowing guide control method is used, the corresponding external blowing position is determined according to the maximum position of the blowing and stretching deformation amount in the pre-blow molding process.
[0103] Specifically, the blow molding difficulty corresponding to the position of the maximum blow-stretch deformation is relatively high. Only relying on the blowing pressure inside the core rod may cause uneven blow molding of the pre-blown body, and it is necessary to rely on auxiliary blowing guide control method to assist blow molding. Only increasing the external blowing pressure at the position of the maximum blow-stretch deformation can not only improve the blow molding quality, but also reduce the complexity of controlling the external blowing pressure.
[0104] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.
Claims
1. A pre-blow molding method based on an injection blow molding machine, characterized in that: include: Step S1, obtaining molding data and pre-blow mold data of a target molded part; Step S2, determining the target wall thickness of the corresponding position of the pre-blow molded body according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation amount during the molding process; Step S3, determining a wall thickness control method of the pre-blow molding process based on the maximum difference in target wall thicknesses at adjacent positions of the pre-blow molding body, including a material thickness distribution control method and an auxiliary blowing guide control method; in, Under the first relative difference condition, the material thickness distribution control method is used to determine the wall thickness adjustment area according to the area of the position with the maximum blowing and stretching deformation in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions; Under the second relative difference condition, the auxiliary blowing guide control mode is used to determine the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow molded body and the internal blowing pressure of the core rod; Wherein, the maximum difference corresponding to the second relative difference condition is greater than the maximum difference corresponding to the first relative difference condition; In step S3, the auxiliary blowing guide control method includes: The pre-blow molded body is formed in a pre-blow mold, and the pre-blow mold is provided with a corresponding air outlet to perform the external blowing pressure; During the pre-blow molding process, the raw material on the core rod is blown simultaneously from both sides of the raw material wall thickness with the internal blow pressure and the corresponding external blow pressure to complete the pre-blow molding process; In the step S3, the material thickness distribution control method includes: Adjusting the distribution of the raw material on the mandrel according to the wall thickness adjustment area and the wall thickness adjustment amount; During the pre-blow molding process, the raw material on the core rod is blown from the core rod side according to the corresponding internal blowing pressure to complete the pre-blow molding process; In the step S3, determining the wall thickness control method of the pre-blow molding process includes: If the maximum difference is greater than the first preset threshold, it is determined that the second relative difference condition is met, and the auxiliary blowing guidance control method is used; If the maximum difference is not greater than the first preset threshold and greater than the second preset threshold, it is determined that the first relative difference condition is met and the material thickness distribution control method is used; In the step S3, determining the external blowing pressure at the corresponding position of the pre-blow mold according to the target wall thickness at the adjacent position of the pre-blow mold and the internal blowing pressure of the core rod includes: Constructing a pressure-wall thickness model according to the target wall thickness of each adjacent position of the pre-blow molded body and the blowing pressure inside the core rod; Determining the external blowing pressure at the corresponding position of the pre-blow mold according to the pressure-wall thickness model; In step S3, the wall thickness adjustment region is determined according to the area of the position with the maximum blow-stretch deformation in the pre-blow molding process and the wall thickness difference between the corresponding adjacent positions, including: Determine the raw material region on the mandrel corresponding to the region having an area greater than a preset area or a wall thickness difference between adjacent positions greater than a preset wall thickness difference as a wall thickness adjustment region; The wall thickness adjustment amount is calculated according to the area of the position with the maximum blow-stretch deformation amount in the pre-blow molding process and the wall thickness difference of the corresponding adjacent positions.
2. The pre-blow molding method based on the injection blow molding machine according to claim 1, characterized in that: In the step S2, it includes: Step S21, constructing a characteristic parameter model according to the wall thickness of each position of the target molded part in the molding data and the blowing and stretching deformation amount during the molding process; Step S22: reversely simulating the blow molding process of the target molded body according to the characteristic parameter model to obtain the target wall thickness of the corresponding position of the pre-blow molded body.
3. The pre-blow molding method based on the injection blow molding machine according to claim 2, characterized in that: Under the third relative difference condition, blow molding is performed according to the blowing pressure inside the core rod; Among them, the maximum difference corresponding to the third relative difference condition is smaller than the maximum difference corresponding to the first relative difference condition.
4. The pre-blow molding method based on the injection blow molding machine according to claim 3, characterized in that: The maximum difference is calculated based on the maximum radial deformation of the pre-blow molded body within a preset length in the axial direction of the core rod; The preset length is determined according to the ratio of the dimension of the pre-blow mold along the axial direction of the core rod to the number of axial deformations.
5. The pre-blow molding method based on the injection blow molding machine according to claim 4, characterized in that: When the auxiliary blowing guide control method is used, the corresponding external blowing position is determined according to the maximum position of the blowing and stretching deformation amount in the pre-blow molding process.
Citation Information
Patent Citations
Method for manufacturing a container from a blank by feedback based on the minimum detected pressure
CN103079796B
Injection blowing hollow forming control system based on multi-data monitoring
CN115256882A
Injection blow molding intelligent manufacturing system based on remote monitoring
CN115284580A
Control system for injection blow molding machine
CN117021546A
Plastic hollow body producing method, involves detecting variations of wall thickness distribution of hollow bodies, and correcting variations by intervening molding process or by changing outflow speed of plastic melt from die gap
DE102008052611B3