A method for preparing alum compound

By reacting waste aluminum cans with sodium hydroxide to generate aluminum sulfate, and using modified flocculants and potassium sulfate for crystallization, the problem of raw material reduction and high cost in alum production is solved, and the effective utilization of resources and productivity improvement are achieved. , simplifying the process steps and reducing energy consumption and waste water generation.

CN118458808BActive Publication Date: 2024-10-18HENGYANG JIANHENG IND DEV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410931575.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-10-18
Estimated Expiration
2044-07-12

AI Technical Summary

Technical Problem

Existing alum production methods have problems such as reduced raw materials, high production costs, large amounts of waste water, high labor intensity, long cycles, and high energy consumption, and natural alunite resources are gradually decreasing.

Method used

Using waste aluminum cans as raw materials, aluminum sulfate is generated by cutting, grinding, and reacting with sodium hydroxide solution. It is combined with modified flocculant and potassium sulfate for crystallization to prepare alum compounds. UV light-induced polymerization is used to improve flocculation efficiency, reduce energy consumption and production costs.

Benefits of technology

Effective utilization of resources is achieved, production costs are reduced, productivity is increased, waste water and energy consumption are reduced, process steps are simplified, and the settling effect of aluminum sulfate and alum production are improved.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for preparing an alum compound, wherein the raw materials are calculated by weight as follows: 100-150 parts of discarded aluminum cans, 80-100 parts of sodium hydroxide solution, 85-105 parts of concentrated sulfuric acid solution, 10-15 parts of modified flocculants, and 70-90 parts of potassium sulfate. The discarded aluminum cans are used as raw materials, which saves costs and realizes the effective utilization of resources; concentrated sulfuric acid is used to produce aluminum sulfate, and the reaction is exothermic, no heat source is required, and energy consumption is reduced; wherein the modified flocculant is a polyacrylamide flocculant, which has the advantages of many functional groups, large molecular weight, strong adsorption and bridging ability, etc., and has good flocculation efficiency, strong flocculation, less scum, no corrosion to processing equipment, can greatly improve flocculation efficiency, improve yield, and through ultraviolet light induced polymerization, the preparation operation is simple and the reaction speed is fast.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of alum preparation methods, and in particular relates to an alum compound and a preparation method thereof. Background Art

[0002] Potassium aluminum sulfate dodecahydrate is an inorganic substance, also known as alum, with a chemical formula of KAl(SO4)2·12H2O. It is a complex salt of potassium sulfate and aluminum sulfate containing water of crystallization. It is soluble in water but insoluble in ethanol. Chinese medicine believes that alum is sour and astringent, cold, and has antibacterial and astringent effects. It can also be used to prepare aluminum salts, baking powder, paint, tanning materials, clarifiers, mordants, papermaking, waterproofing agents, etc. It was often used in water purification in life. The aluminum hydroxide colloid formed after alum is dissolved in water has a strong adsorption capacity, which can adsorb suspended impurities in water and form precipitation to make the water clear.

[0003] At present, the common alum production methods include bauxite method, aluminum hydroxide method, and natural alunite processing method; among them, the bauxite method uses sulfuric acid to decompose bauxite ore to produce aluminum sulfate solution, and then adds potassium sulfate to react, and obtains potassium aluminum sulfate products through filtration, crystallization, centrifugal dehydration, and drying. However, the former bauxite raw materials are reduced, the quality of the raw materials is low, and a large amount of acidic waste residue and wastewater will be generated during the production process, which consumes a lot of manpower and material resources, resulting in high production costs and high labor intensity of the product. The aluminum hydroxide method, which dissolves aluminum hydroxide in sulfuric acid, then adds a measured potassium sulfate solution to heat the reaction, and obtains the finished product of potassium aluminum sulfate through filtration, concentration, crystallization, centrifugal separation, drying, and this method has the problems of high cost and large amount of wastewater. Finally, the natural alunite processing method: crushing the alunite, roasting, dehydration, weathering, steam leaching, sedimentation, crystallization, and crushing to obtain the finished product of potassium aluminum sulfate; the production cycle is long, the yield is low, the energy consumption is high, and with the continuous exploitation of natural alunite deposits, the resources are becoming less and less, the mining cost is also increasing, and the production cost is also very high.

[0004] Nowadays, more and more food and beverages are packaged in aluminum cans. However, the current recycling methods for discarded aluminum cans are relatively simple. Using them in the production and preparation of alum is a new way to utilize discarded aluminum cans. Summary of the invention

[0005] The purpose of the present invention is to overcome the defects of the prior art and provide a method for preparing an alum compound.

[0006] The purpose of the present invention can be achieved by the following technical solutions:

[0007] A method for preparing an alum compound comprises the following steps:

[0008] A1. Cut the discarded aluminum cans into pieces and polish their surfaces with sandpaper;

[0009] A2, mixing the polished aluminum sheet obtained in step A1 with a sodium hydroxide solution, heating in a water bath until no hydrogen is generated, and filtering under reduced pressure while hot to collect the filtrate;

[0010] A3, adding the filtrate obtained in step A2 and the concentrated sulfuric acid solution into a reactor, sealing the reactor, stirring, and when the pressure in the reactor reaches 0.4 MPa, stopping stirring and standing to obtain a crude aluminum sulfate solution;

[0011] A4, the aluminum sulfate crude is precipitated, the aluminum sulfate crude liquid obtained in step A3 is added to a sedimentation barrel, and compressed air is introduced into the bottom, and after blowing to boiling, a modified flocculant is added to produce alum flowers, and the pH value is adjusted to 2-4, and the mixture is allowed to stand, and the supernatant is sent to a filter press. After filter pressing, the filtrate obtained is the aluminum sulfate mother liquor;

[0012] A5. Add the aluminum sulfate mother liquor obtained in step A4 into a concentration tank, heat it, add potassium sulfate, start stirring, complete the reaction, cool it, crystallize it, wash it with water, and dry it in the sun to obtain an alum compound.

[0013] Furthermore, the raw materials are calculated in parts by weight as follows: 100-150 parts of discarded aluminum cans, 80-100 parts of sodium hydroxide solution, 85-105 parts of concentrated sulfuric acid solution, 10-15 parts of modified flocculant, and 70-90 parts of potassium sulfate.

[0014] Furthermore, the mesh number of the sandpaper in step A1 is 800-1000.

[0015] Furthermore, in step A3, the stirring speed is 15-20 r / min, the time is 20-30 min, and the standing time is 5-6 h.

[0016] Furthermore, in step A4, the flow rate of compressed air is 2-3 MPa; and the standing time is 5-6 h.

[0017] Furthermore, in step A5, the heating temperature is 60-70° C.; the stirring time is 2-3 hours; the cooling time is 2-3 days; and the drying time is 1-2 days.

[0018] Furthermore, the modified flocculant is prepared by the following steps:

[0019] S1. In a three-necked flask equipped with a stirring reflux device, add toluene and 2-imidazoline, heat to 60°C, and stir continuously until the solid is dissolved, add propylene oxide, heat to 80°C, reflux for 1h, and the reaction is complete. Cool to room temperature, filter, take the filter residue, and vacuum dry to obtain an intermediate; the ratio of toluene, 2-imidazoline, and propylene oxide is 50mL:6.9g:5.8g;

[0020] 2-Imidazolidine undergoes a ring-opening substitution reaction with propylene oxide to obtain an intermediate;

[0021] S2. In a three-necked flask equipped with a stirring device, acrylamide, intermediate and toluene are added and stirred and mixed evenly, then azobisisobutyronitrile (initiator, AIBN) is added and nitrogen is introduced. At room temperature, an ultraviolet lamp (wavelength 365nm) is used to irradiate for 1.5 hours. After the irradiation is completed, it is placed in a dark place for aging for 2 hours, and precipitated and purified with a mixed solution of acetone / ethanol in a volume ratio of 2:1, and vacuum dried to obtain a modified flocculant; the ratio of acrylamide, intermediate, toluene and azobisisobutyronitrile is 10g:3g:100mL:0.2g;

[0022] Under the action of ultraviolet radiation, a polymerization reaction is initiated to obtain a modified flocculant;

[0023] The prepared modified flocculant is a polyacrylamide flocculant, which has the advantages of multiple functional groups, large molecular weight, strong adsorption and bridging ability, etc., and has good flocculation efficiency, strong flocculation, less scum, no corrosion to treatment equipment, and the introduction of imidazoline structure through graft polymerization can further enhance the flocculation effect of the modified flocculant, improve the sedimentation effect of aluminum sulfate crude liquid, improve the yield, and save the tedious steps of repeatedly washing the bottom scum.

[0024] Beneficial effects of the present invention:

[0025] 1. Use discarded aluminum cans as raw materials to save costs and achieve effective utilization of resources; use sandpaper to grind off the aluminum oxide on the surface of the aluminum cans, making the surface of the aluminum cans rougher and promoting the reaction with sulfuric acid;

[0026] 2. Use concentrated sulfuric acid to produce aluminum sulfate. The reaction is exothermic, no heat source is required, and energy consumption is reduced;

[0027] 3. The prepared modified flocculant can greatly improve the flocculation efficiency and increase the yield, and through ultraviolet light-induced polymerization, the preparation operation is simple and the reaction speed is fast. DETAILED DESCRIPTION

[0028] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] Example 1

[0030] Preparation of modified flocculant:

[0031] S1. In a three-necked flask equipped with a stirring reflux device, add 50 mL of toluene and 6.9 g of 2-imidazoline, heat to 60 ° C, and stir continuously until the solid is dissolved, add 5.8 g of propylene oxide, heat to 80 ° C, reflux for 1 h, and the reaction is completed. Cool to room temperature, filter, take the filter residue, and vacuum dry to obtain an intermediate;

[0032] S2. In a three-necked flask equipped with a stirring device, add 10g acrylamide, 3g intermediate and 100mL toluene, stir and mix evenly, then add 0.2g azobisisobutyronitrile and pass nitrogen. At room temperature, use an ultraviolet lamp (wavelength 365nm) to irradiate for 1.5h. After irradiation, let it stand in the dark for 2h, precipitate and purify with a mixed solution of acetone / ethanol in a volume ratio of 2:1, and vacuum dry to obtain a modified flocculant.

[0033] Example 2

[0034] Preparation of modified flocculant:

[0035] S1. In a three-necked flask equipped with a stirring reflux device, add 100 mL of toluene and 13.8 g of 2-imidazoline, heat to 60 ° C, and stir continuously until the solid is dissolved, add 11.6 g of propylene oxide, heat to 80 ° C, reflux for 1 h, and the reaction is completed. Cool to room temperature, filter, take the filter residue, and vacuum dry to obtain an intermediate;

[0036] S2. In a three-necked flask equipped with a stirring device, add 20g acrylamide, 6g intermediate and 200mL toluene, stir and mix evenly, then add 0.4g azobisisobutyronitrile and pass nitrogen. At room temperature, use an ultraviolet lamp (wavelength 365nm) to irradiate for 1.5h. After the irradiation, let it stand in the dark for 2h, precipitate and purify with a mixed solution of acetone / ethanol in a volume ratio of 2:1, and vacuum dry to obtain a modified flocculant.

[0037] Example 3

[0038] A1. Cut 100g of discarded aluminum cans into pieces and polish their surfaces with 800-grit sandpaper;

[0039] A2. Mix the polished aluminum sheet obtained in step A1 with 80 g of sodium hydroxide solution (mass fraction 16%), heat in a water bath until no hydrogen is generated, and filter under reduced pressure while hot to collect the filtrate;

[0040] A3, add the filtrate obtained in step A2 and 85g of concentrated sulfuric acid solution (mass fraction is 98%) into the reactor, seal the reactor, stir for 20min (stirring speed is 15r / min), when the pressure in the reactor is 0.4MPa, stop stirring, let stand for 5h, and obtain crude aluminum sulfate liquid;

[0041] A4, the aluminum sulfate crude is precipitated, the aluminum sulfate crude liquid obtained in step A3 is added to a sedimentation barrel, and compressed air (flow rate is 2MPa) is introduced into the bottom, and after blowing to boiling, 10g of the modified flocculant prepared in Example 1 is added, and after alum flowers are generated, the pH value is adjusted to 2, and the mixture is allowed to stand for 5h, and the supernatant is sent to a filter press, and after filtration, the filtrate obtained is the aluminum sulfate mother liquor;

[0042] A5. Add the aluminum sulfate mother liquor obtained in step A4 into a concentration tank, heat to 60° C., add potassium sulfate, start stirring, stir for 2 hours, and complete the reaction. Cool for 2 days, crystallize, wash with water, and dry in the sun for 1 day to obtain an alum compound.

[0043] Example 4

[0044] A1. Cut 125g of discarded aluminum cans into pieces and polish their surfaces with 900-grit sandpaper;

[0045] A2. Mix the polished aluminum sheet obtained in step A1 with 90 g of sodium hydroxide solution (mass fraction 16%), heat in a water bath until no hydrogen is generated, and filter under reduced pressure while hot to collect the filtrate;

[0046] A3, the filtrate obtained in step A2 and 95g of concentrated sulfuric acid solution (mass fraction of 98%) were added to the reactor, the reactor was sealed, and stirred for 25min (stirring speed was 18r / min). When the pressure in the reactor reached 0.4MPa, stirring was stopped, and the reactor was allowed to stand for 5.5h to obtain a crude aluminum sulfate solution;

[0047] A4, the aluminum sulfate crude is precipitated, the aluminum sulfate crude liquid obtained in step A3 is added to a sedimentation barrel, and compressed air (flow rate is 3 MPa) is introduced into the bottom, and after blowing to boiling, 12.5 g of the modified flocculant prepared in Example 2 is added, and after alum flowers are generated, the pH value is adjusted to 3, and the mixture is allowed to stand for 5.5 hours. The supernatant is sent to a filter press, and after filtration, the filtrate obtained is the aluminum sulfate mother liquor;

[0048] A5. Add the aluminum sulfate mother liquor obtained in step A4 into a concentration tank, heat to 65° C., add potassium sulfate, start stirring, stir for 2.5 hours, and complete the reaction. Cool for 3 days, crystallize, wash with water, and dry in the sun for 2 days to obtain an alum compound.

[0049] Example 5

[0050] A1. Cut 150g of discarded aluminum cans into pieces and polish their surfaces with 1000-mesh sandpaper;

[0051] A2. Mix the polished aluminum sheet obtained in step A1 with 100 g of sodium hydroxide solution (mass fraction 16%), heat in a water bath until no hydrogen is generated, and filter under reduced pressure while hot to collect the filtrate;

[0052] A3, the filtrate obtained in step A2 and 105g of concentrated sulfuric acid solution (mass fraction of 98%) were added to the reactor, the reactor was sealed, and stirred for 30min (stirring speed was 20r / min). When the pressure in the reactor reached 0.4MPa, stirring was stopped and the reactor was allowed to stand for 6h to obtain a crude aluminum sulfate solution;

[0053] A4, the aluminum sulfate crude is precipitated, the aluminum sulfate crude liquid obtained in step A3 is added to a sedimentation barrel, and compressed air (flow rate is 3MPa) is introduced into the bottom, and after blowing to boiling, 15g of the modified flocculant prepared in Example 2 is added, and after alum flowers are generated, the pH value is adjusted to 4, and the mixture is allowed to stand for 6h, and the supernatant is sent to a filter press, and after filtration, the filtrate obtained is the aluminum sulfate mother liquor;

[0054] A5. Add the aluminum sulfate mother liquor obtained in step A4 into a concentration tank, heat to 70°C, add potassium sulfate, start stirring, stir for 3 hours, and complete the reaction. Cool for 3 days, crystallize, wash with water, and dry in the sun for 2 days to obtain an alum compound.

[0055] In the description of the specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0056] The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.

Claims

1. A method for preparing an alum compound, characterized in that: The following steps are involved: A1. Cut the discarded aluminum cans into pieces and polish their surfaces with sandpaper; A2, mixing the polished aluminum sheet obtained in step A1 with a sodium hydroxide solution, heating in a water bath until no hydrogen is generated, and filtering under reduced pressure while hot to collect the filtrate; A3, adding the filtrate obtained in step A2 and the concentrated sulfuric acid solution into a reactor, sealing the reactor, stirring, and when the pressure in the reactor reaches 0.4 MPa, stopping stirring and standing to obtain a crude aluminum sulfate solution; A4, the aluminum sulfate crude is precipitated, the aluminum sulfate crude liquid obtained in step A3 is added to a sedimentation barrel, and compressed air is introduced into the bottom, and after blowing to boiling, a modified flocculant is added to produce alum flowers, and the pH value is adjusted to 2-4, and the mixture is allowed to stand, and the supernatant is sent to a filter press. After filter pressing, the filtrate obtained is the aluminum sulfate mother liquor; A5. Add the aluminum sulfate mother liquor obtained in step A4 into a concentration tank, heat it, add potassium sulfate, start stirring, complete the reaction, cool it, crystallize it, wash it with water, and dry it in the sun to obtain an alum compound; The modified flocculant is prepared by the following steps: S1. Add toluene and 2-imidazoline to a three-necked flask, heat to 60°C, and stir continuously until the solid is dissolved, add propylene oxide, reflux at 80°C for 1h, and after the reaction is complete, cool to room temperature, filter, take the filter residue, and vacuum dry to obtain an intermediate; S2. In a three-necked flask, add acrylamide, intermediate and toluene, stir and mix evenly, then add azobisisobutyronitrile and pass nitrogen. At room temperature, irradiate with a UV lamp for 1.5 hours. After irradiation, let it stand in a dark place for 2 hours, precipitate and purify with a mixed solution of acetone / ethanol in a volume ratio of 2:1, and vacuum dry to obtain a modified flocculant.

2. The method for preparing an alum compound according to claim 1, wherein In step S1, the ratio of toluene, 2-imidazoline and propylene oxide is 50 mL: 6.9 g: 5.8 g.

3. The method for preparing an alum compound according to claim 1, wherein In step S2, the ratio of acrylamide, intermediate, toluene and azobisisobutyronitrile is 10 g:3 g:100 mL:0.2 g.

4. The method for preparing an alum compound according to claim 1, wherein The raw materials are calculated in parts by weight as follows: 100-150 parts of discarded aluminum cans, 80-100 parts of sodium hydroxide solution, 85-105 parts of concentrated sulfuric acid solution, 10-15 parts of modified flocculant, and 70-90 parts of potassium sulfate.

5. The method for preparing an alum compound according to claim 1, wherein The grit of the sandpaper in step A1 is 800-1000.

6. The method for preparing an alum compound according to claim 1, characterized in that: In step A3, the stirring speed is 15-20 r / min, the time is 20-30 min, and the standing time is 5-6 h.

7. The method for preparing an alum compound according to claim 1, wherein In step A5, the heating temperature is 60-70° C.; the stirring time is 2-3 hours; the cooling time is 2-3 days; and the sun drying time is 1-2 days.