Shielded gate field effect transistor and preparation method thereof, and electronic device
By etching in the shielded gate field effect transistor to form a second trench and forming a liner layer on its side walls, the problem of excessive depth and aspect ratio of the shielded gate trench filling is solved, and the high-density plasma deposition process is reduced. It is required to avoid sidewall oxidation and improve the stability and electrical properties of the device.
Patent Information
- Application Number
- CN202410926299.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-07-11
AI Technical Summary
In metal oxide semiconductor field effect transistors, the smaller key size of the shielded gate trench leads to an increase in the filling depth-to-face ratio of the deposition process of the dielectric material layer between the gates. Ordinary high-density plasma deposition processes cannot meet the process requirements, and During the thermal oxidation process, the side walls of the shielded gate trench are oxidized, expanding their size and affecting the threshold voltage.
By etching the shielding dielectric layer above the first shielding gate and forming a liner layer on its side walls, a second shielding gate and an inter-gate dielectric layer are formed, and then a portion of the dielectric layer and the liner are removed. The third trench is formed to reduce the depth-to-width ratio of the trench, reduce the requirements of the high-density plasma deposition process, and prevent sidewall oxidation.
It effectively reduces the requirements of high-density plasma deposition process, reduces filling holes, improves device electricality and yield, ensures the consistency of the shape and size of the gate structure, avoids the influence of threshold voltage, and improves device stability and reliability.
Smart Images

Figure CN118471799B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a shielded gate field effect transistor and a preparation method thereof, and an electronic device. Background Art
[0002] Shielded Gate Trench (SGT) is widely used in advanced logic circuit processes. Its quality will directly affect the performance of the device. For example, shielded gate trench is used in metal oxide semiconductor field effect transistor (MOSFET).
[0003] In the related art, when the shielding gate trench is applied to the metal oxide semiconductor field effect transistor, a trench extending from the surface of the substrate to the inside of the substrate is usually formed first, a shielding dielectric material layer is formed on the bottom, sidewalls and surface of the trench, a shielding gate of a certain depth is filled in the trench, and a portion of the shielding dielectric material layer in the trench is removed by back etching to form a shielding dielectric layer. Since the critical dimensions of the shielding gate trench applied to the low voltage platform are relatively small, the filling depth-to-width ratio of the deposition process of the inter-gate dielectric material layer will increase, and the excessive filling depth-to-width ratio has high requirements for the high density plasma (HDP) deposition process. The ordinary HDP deposition process cannot meet the process requirements, that is, the relevant preparation process has the problem of HDP deposition process limitation.
[0004] In the related art, there is also a method of directly using a one-step molding process to form an inter-gate dielectric layer (for example, thermally oxidizing a portion of the shielding gate). However, since the side walls on both sides of the shielding gate trench are exposed, the side walls on both sides of the shielding gate trench will also be oxidized during the thermal oxidation. If the oxide layer is subsequently removed, the critical dimension (CD) on both sides of the shielding gate trench will be enlarged, thereby enlarging the size of the gate structure subsequently formed on the shielding gate, thereby affecting the threshold voltage (Vth). Summary of the invention
[0005] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0006] In view of the existing problems, the present invention provides a method for preparing a shielded gate field effect transistor, the method comprising: providing a substrate, forming a first trench extending from the surface of the substrate to the interior of the substrate, forming a shielding dielectric layer at the bottom and at least a portion of the sidewalls of the first trench, and forming a first shielding gate located on the shielding dielectric layer in the first trench, wherein the top surface of the first shielding gate is lower than the top surface of the shielding dielectric layer; etching the shielding dielectric layer above the first shielding gate to remove a portion of the thickness of the shielding dielectric layer to form a second trench above the first shielding gate; groove; forming a liner layer on the sidewall of the second groove, and an opening is also formed in the liner layer, wherein the opening exposes at least a portion of the top surface of the first shielding gate; forming a second shielding gate in the second groove, wherein the top surface of the second shielding gate is lower than the surface of the substrate, and the second shielding gate is connected to the first shielding gate; forming an inter-gate dielectric layer in the second groove to cover the second shielding gate; etching and removing part of the shielding dielectric layer, part of the liner layer, and part of the inter-gate dielectric layer to form a third groove located on the inter-gate dielectric layer; forming a gate structure in the third groove.
[0007] In one embodiment of the present application, forming a liner layer on the sidewall of the second trench includes: forming a liner material layer on the bottom and sidewall of the second trench; etching at least a portion of the liner material layer located at the bottom of the second trench to form the liner layer including the opening.
[0008] In one embodiment of the present application, forming an inter-gate dielectric layer in the second trench to cover the second shield gate includes: oxidizing a portion of the second shield gate to oxidize the portion of the second shield gate into the inter-gate dielectric layer.
[0009] In one embodiment of the present application, after the step of etching away part of the shielding dielectric layer, part of the liner layer, and part of the inter-gate dielectric layer to form a third trench located on the inter-gate dielectric layer, the top surfaces of the shielding dielectric layer, the liner layer, and the inter-gate dielectric layer are flush.
[0010] In one embodiment of the present application, a gate structure is formed in the third trench, including: forming a gate dielectric layer on the sidewall of the third trench; forming a gate electrode layer to fill the third trench and cover the gate dielectric layer to form the gate structure, wherein the gate structure includes the gate dielectric layer and the gate electrode layer.
[0011] In one embodiment of the present application, the material of the liner layer includes at least one of the following: silicon nitride, silicon carbide, silicon carbonitride; and / or the material of the first shielding gate and the second shielding gate includes polysilicon.
[0012] According to the second aspect of the present application, a shielded gate field effect transistor is also provided, the shielded gate field effect transistor comprising: a substrate, a first trench, a shielding dielectric layer, a first shielding gate, a second trench, a liner layer, a second shielding gate, an inter-gate dielectric layer, a third trench and a gate structure; wherein the first trench extends from the surface of the substrate to the interior of the substrate; the shielding dielectric layer is formed on the bottom and part of the side wall of the first trench; the first shielding gate is formed in the first trench and is located on the shielding dielectric layer, and the top surface of the first shielding gate is lower than the top surface of the shielding dielectric layer; the second trench is arranged on the first shielding gate and is located on the first shielding gate The shielding dielectric layer surrounds the part on the square side of the second trench; the liner layer is arranged on the side wall of the second trench, wherein an opening is also formed in the liner layer, and the opening exposes at least a part of the top surface of the first shielding gate; the second shielding gate is arranged in the second trench, wherein the top surface of the second shielding gate is lower than the surface of the substrate, and the second shielding gate is connected to the first shielding gate; the inter-gate dielectric layer is arranged in the second trench and covers the top surface of the second shielding gate; the third trench extends from the surface of the substrate to the inside of the substrate, and is located on the shielding dielectric layer, the liner layer and the inter-gate dielectric layer; the gate structure is arranged in the third trench.
[0013] In one embodiment of the present application, top surfaces of the shielding dielectric layer, the liner layer, and the inter-gate dielectric layer are flush.
[0014] In one embodiment of the present application, the gate structure includes a gate dielectric layer and a gate electrode layer, the gate dielectric layer is disposed on the sidewall of the third trench, and the gate electrode layer fills the third trench and covers the gate dielectric layer.
[0015] According to a third aspect of the present application, an electronic device is further provided, comprising any one of the shielded gate field effect transistors described above.
[0016] The shielded gate field effect transistor and its preparation method and electronic device of the embodiment of the present invention, by etching the shielding dielectric layer above the first shielding gate, removing a portion of the thickness of the shielding dielectric layer to form a second trench above the first shielding gate, and forming a liner layer on the sidewall of the second trench and forming a second shielding gate in the second trench; then forming an inter-gate dielectric layer in the second trench to cover the second shielding gate. In the scheme of the present application, by forming a liner layer on the sidewall of the second trench, it can prevent the sidewall of the second trench from being oxidized when the inter-gate dielectric layer is formed, thereby avoiding the expansion of the critical dimension (CD) on both sides of the second trench, making the shape and size of the gate structure more consistent with the design, thereby avoiding the impact on the threshold voltage (Vth) and improving the stability and reliability of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The following drawings of the present invention are used as part of the present invention for understanding the present invention. The drawings show embodiments of the present invention and their descriptions to explain the principles of the present invention. In the drawings:
[0018] Figure 1 A schematic cross-sectional view of a shielding gate trench obtained by implementing an existing shielding gate trench preparation method is shown;
[0019] Figure 2 A flow chart showing a method for preparing a shielded gate field effect transistor according to a specific embodiment of the present invention;
[0020] Figures 3A-3G The cross-sectional schematic diagram of a shielded gate field effect transistor obtained by sequentially implementing a method for preparing a shielded gate field effect transistor according to a specific embodiment of the present invention is shown. DETAILED DESCRIPTION
[0021] Next, the present invention will be more fully described in conjunction with the accompanying drawings, in which embodiments of the present invention are shown. However, the present invention can be implemented in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present invention to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.
[0022] It should be understood that when an element or layer is referred to as being "on, adjacent to, connected to or coupled to other elements or layers, it may be directly on, adjacent to, connected to or coupled to other elements or layers, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on, directly adjacent to, directly connected to or directly coupled to other elements or layers, there may be no intervening elements or layers. It should be understood that, although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below may be represented as a second element, component, region, layer or part.
[0023] Spatially relative terms such as "under," "below," "below," "under," "above," "above," etc., may be used herein for ease of description to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatially relative terms are intended to include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, then the elements or features described as "under other elements" or "under" or "under" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device may be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.
[0024] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present invention. When used herein, the singular forms "a", "an", and "said / the" are also intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0025] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic diagrams of ideal embodiments (and intermediate structures) of the invention. Thus, variations from the shapes shown due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, embodiments of the invention should not be limited to the specific shapes of the zones shown herein, but include shape deviations due to, for example, manufacturing. For example, an implanted region shown as a rectangle typically has rounded or curved features and / or an implant concentration gradient at its edges, rather than a binary change from an implanted region to a non-implanted region. Similarly, a buried region formed by implantation may result in some implantation in the region between the buried region and the surface through which the implantation is performed. Therefore, the regions shown in the figures are schematic in nature, and their shapes are not intended to show the actual shape of the region of the device and are not intended to limit the scope of the invention.
[0026] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by one of ordinary skill in the art in the field of the present invention. It will also be understood that terms such as those defined in commonly used dictionaries should be understood to have a meaning consistent with their meaning in the context of the relevant art and / or this specification, and should not be interpreted in an ideal or overly formal sense unless expressly defined as such herein.
[0027] In order to fully understand the present invention, detailed steps and structures will be presented in the following description to illustrate the technical solution proposed by the present invention. The preferred embodiments of the present invention are described in detail below, but in addition to these detailed descriptions, the present invention may also have other implementations.
[0028] In the related art, the polysilicon formed inside the shielding gate trench is used as the shielding gate, which can also be called source polysilicon (Source Poly). It is a wine glass structure, which can use EPI (epitaxial layer) with smaller resistance under the same Bv (breakdown voltage), thereby reducing Rdson (on-resistance). When the shielding gate trench is applied to metal oxide semiconductor field effect transistors, the following preparation processes are usually used: Figure 1 As shown, a trench 101 is formed in a substrate 100, a shielding dielectric material layer is formed on the sidewalls, bottom and surface of the trench 101, and a shielding gate 103 is partially filled in the trench 101, and the shielding gate is in a shape similar to a "wine glass". Part of the shielding dielectric material layer is removed by back etching to form a shielding dielectric layer 102. At this time, the distance between the sidewalls above the shielding gate 103 in the trench 101 is W0, and the distance between the top surface of the shielding gate 103 in the trench 101 and the surface of the substrate 100 is L0. Subsequently, an inter-gate dielectric material layer is deposited to fill the trench 101, for example, by a high density plasma (HDP) deposition process to form an inter-gate dielectric material layer to fill the trench 101.
[0029] The inventors of this application have found that the critical dimensions of the shielding gate grooves used in low-voltage platforms are relatively small, which will lead to an increase in the filling depth-to-width ratio of the deposition process of the inter-gate dielectric material layer. Excessively large filling depth-to-width ratios place high demands on the high-density plasma (HDP) deposition process. If the ordinary HDP deposition process is used to fill the inter-gate dielectric material layer, the filling window will be insufficient when the inter-gate dielectric material layer is filled, so that voids are likely to appear during the filling process of the inter-gate dielectric material layer, thereby affecting the electrical properties of the product and reducing the product yield. In other words, the ordinary HDP deposition process for filling the inter-gate dielectric material layer cannot meet the process requirements. Figure 1 As shown, when L0:W0 is greater than 2.5:1 (L0 / W0 is greater than 2.5), the ordinary HDP deposition process cannot meet the preparation process requirements due to limited filling capacity, that is, the relevant preparation process shown above has the problem of HDP deposition process limitation.
[0030] In the related art, there is also a method of directly using a one-step molding process to form an inter-gate dielectric layer (for example, thermally oxidizing a portion of the shielding gate). However, since the side walls on both sides of the shielding gate trench are exposed, the side walls on both sides of the shielding gate trench will also be oxidized during the thermal oxidation. If the oxide layer is subsequently removed, the critical dimension (CD) on both sides of the shielding gate trench will be enlarged, thereby enlarging the size of the gate structure subsequently formed on the shielding gate, thereby affecting the threshold voltage (Vth).
[0031] Therefore, in view of the existence of the above-mentioned technical problems, the present invention proposes a method for preparing a shielded gate field effect transistor, such as Figure 2 As shown, it mainly includes the following steps:
[0032] Step S1, providing a substrate, forming a first trench extending from a surface of the substrate to an interior of the substrate, forming a shielding dielectric layer at the bottom and at least a portion of a sidewall of the first trench, and forming a first shielding grid located on the shielding dielectric layer in the first trench, wherein a top surface of the first shielding grid is lower than a top surface of the shielding dielectric layer;
[0033] Step S2, etching the shielding dielectric layer above the first shielding gate to remove a portion of the thickness of the shielding dielectric layer to form a second trench above the first shielding gate;
[0034] Step S3, forming a liner layer on the sidewalls of the second trench, wherein an opening is formed in the liner layer, wherein the opening exposes at least a portion of the top surface of the first shielding grid;
[0035] Step S4, forming a second shielding gate in the second trench, wherein a top surface of the second shielding gate is lower than a surface of the substrate, and the second shielding gate is connected to the first shielding gate;
[0036] Step S5, forming an inter-gate dielectric layer in the second trench to cover the second shielding gate;
[0037] Step S6, etching and removing a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer to form a third trench located on the inter-gate dielectric layer;
[0038] Step S7, forming a gate structure in the third trench.
[0039] In the above scheme, the shielding dielectric layer above the first shielding gate is etched to remove a portion of the thickness of the shielding dielectric layer, so as to form a second trench above the first shielding gate, and a liner layer is formed on the sidewall of the second trench, and a second shielding gate is formed in the second trench; then, an inter-gate dielectric layer is formed in the second trench to cover the second shielding gate. The aspect ratio of the second trench can be reduced, so that the filling depth of the second trench is reduced, and the filling aspect ratio of the second trench is effectively reduced, thereby reducing the requirements for the high-density plasma deposition process and solving the problem of HDP deposition process limitations. It can also increase the filling window, reduce the occurrence of filling voids, improve the filling effect, and improve the electrical properties and yield of the device. In the scheme of the present application, by forming a liner layer on the sidewall of the second trench, it can play a role in preventing the sidewall of the second trench from being oxidized when the inter-gate dielectric layer is formed, thereby avoiding the expansion of the critical dimension (CD) on both sides of the second trench, making the shape and size of the gate structure more consistent with the design, thereby avoiding the impact on the threshold voltage (Vth) and improving the stability and reliability of the device.
[0040] Example 1
[0041] Below, reference Figures 2 to 3G The preparation method of the shielded gate field effect transistor of the present invention is described in detail, wherein: Figure 2 A flowchart of a method for preparing a shielded gate field effect transistor according to a specific embodiment of the present invention is shown. Figures 3A-3G The cross-sectional schematic diagram of a shielded gate field effect transistor obtained by sequentially implementing a method for preparing a shielded gate field effect transistor according to a specific embodiment of the present invention is shown.
[0042] Exemplarily, the method for preparing the shielded gate field effect transistor of the present invention comprises the following steps:
[0043] First, perform step S1, provide a substrate, form a first groove extending from the surface of the substrate to the inside of the substrate, form a shielding dielectric layer at the bottom and at least part of the sidewall of the first groove, and form a first shielding gate located on the shielding dielectric layer in the first groove, and the top surface of the first shielding gate is lower than the top surface of the shielding dielectric layer.
[0044] In some embodiments, the substrate 300 may include a semiconductor base and an epitaxial layer formed on the semiconductor base. Optionally, the semiconductor base and the epitaxial layer may have the same conductivity type. In other embodiments, the substrate 300 may include only a semiconductor base without forming an epitaxial layer.
[0045] Specifically, Figure 3AAs shown, the substrate 300 includes a semiconductor base, and the semiconductor base may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the semiconductor base may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form a semiconductor base are described herein, any material that can be used as a semiconductor base falls within the scope of protection of the present invention. In addition, the substrate 300 may be divided into active areas, and / or a doped well (not shown) may be formed in the substrate 300, etc.
[0046] In one example, if Figure 3A As shown, a first trench 301 extending from the surface of the substrate 300 to the inside of the substrate 300 is formed, a shielding dielectric layer 302 is formed at the bottom and at least part of the sidewalls of the first trench 301, and a first shielding gate 303 is formed in the first trench 301, and the top surface of the first shielding gate 303 is lower than the top surface of the shielding dielectric layer 302. At this time, the distance from the top surface of the first shielding gate 303 to the surface of the substrate 300 is a first depth L1, and the distance between the sidewalls of the portion of the trench (also referred to as a sub-trench in this article) in the first trench 301 located above the first shielding gate 303 is a first width W1, and the first depth L1 is substantially equal to Figure 1 The distance L0 shown in FIG. 1 and the first width W1 are greater than Figure 1 The distance W0 shown in the figure, that is, the width of the sub-groove of the first groove 301 increases, and the aspect ratio of the sub-groove of the first groove 301 decreases, so that the filling aspect ratio of the deposition process used to fill other materials in the sub-groove of the first groove 301 in the subsequent preparation of the second shielding gate is reduced, thereby reducing the requirements for the high-density plasma deposition process and solving the problem of HDP deposition process limitations. It can also increase the filling window, thereby reducing the appearance of voids during filling, improving the filling effect, and improving the device electrical properties and yield.
[0047] In one example, the shielding dielectric layer 302 may include a silicon oxide layer, or a stack of a silicon oxide layer and a silicon nitride layer, or a stack of two silicon oxide layers with a silicon nitride layer sandwiched between them. That is, the shielding dielectric layer 302 may be formed of one or more silicon oxide layers. Of course, in other embodiments, other materials may also be used as the shielding dielectric layer 302.
[0048] Exemplarily, the material of the first shielding grid 303 may include polysilicon or other suitable materials. Exemplarily, the method for forming polysilicon may be a low pressure chemical vapor deposition (LPCVD) process. The process conditions for forming polysilicon include: the reaction gas is silane (SiH4), and the flow rate of silane may range from 100 to 200 cubic centimeters per minute (sccm), such as 150 sccm; the temperature range in the reaction chamber may be 700 to 750 degrees Celsius; the pressure in the reaction chamber may be 250 to 350 millimeters of mercury (mTorr), such as 300 mTorr; the reaction gas may also include a buffer gas, which may be helium (He) or nitrogen, and the flow rate of helium and nitrogen may range from 5 to 20 liters per minute (slm), such as 8 slm, 10 slm or 15 slm.
[0049] Next, step S2 is performed to etch the shielding dielectric layer above the first shielding gate to remove a portion of the shielding dielectric layer to form a second trench above the first shielding gate. Figure 3B In this step, only the shielding dielectric layer 302 above the first shielding gate 303 is etched, thereby removing a portion of the shielding dielectric layer 302 along the deposition thickness direction of the shielding dielectric layer 302 to form a second trench 304 .
[0050] By way of example, a wet etching process may be used to etch away the shielding dielectric layer 302 above the first shielding gate 303, and a portion of the thickness of the shielding dielectric layer 302 may be removed to form a second trench 304 above the first shielding gate 303. In this embodiment, the wet etching process only etches the shielding dielectric layer 302 and hardly etches the first shielding gate 303 and the substrate 300. By way of example, a selective etching process may be used to only etch away the shielding dielectric layer 302 above the first shielding gate 303, without etching away the first shielding gate 303.
[0051] In one example, if Figure 3B As shown, the shielding dielectric layer 302 above the first shielding gate 303 is etched, and a portion of the thickness of the shielding dielectric layer 302 is removed to form a second groove 304 above the first shielding gate 303. The distance from the top surface of the first shielding gate 303 to the surface of the substrate is the second depth L2, and the second depth L2 is substantially equal to the first depth L1. At this time, the distance W2 between the side walls of the second groove 304 located above the first shielding gate 303 is greater than the first width W1, that is, the width of the second groove 304 is increased and the depth remains unchanged. Therefore, the aspect ratio of the second groove 304 is reduced. As a result, the filling aspect ratio of the deposition process in the subsequent process of filling other materials in the second groove 304 is reduced, thereby reducing the requirements for the high-density plasma deposition process and solving the problem of HDP deposition process limitations. It can also increase the filling window, thereby reducing the appearance of voids during filling, improving the filling effect, and improving the electrical properties and yield of the device.
[0052] Then, step S3 is performed to form a liner layer on the sidewall of the second trench, wherein an opening is formed in the liner layer, wherein the opening exposes at least a portion of the top surface of the first shielding gate. Figure 3C A liner layer 306 is formed on the sidewall of the second trench 304, the liner layer 306 is only located above the first shielding gate 303, and an opening is formed in the liner layer 306 at the bottom of the second trench 304, so that the top surface of the first shielding gate 303 is at least partially exposed from the opening.
[0053] Exemplarily, the method of forming a liner layer on the sidewall of the second trench may include: Figure 3B and Figure 3C As shown, a liner material layer 305 is formed on the bottom and sidewalls of the second trench 304; at least a portion of the liner material layer 305 located at the bottom of the second trench 304 is etched to form a liner layer 306 including an opening. For example, the liner material layer 305 is first formed on the bottom and sidewalls of the second trench 304 by deposition, and then at least a portion of the liner material layer located at the bottom of the second trench is etched to form the liner layer 306 including the opening.
[0054] For example, reference Figure 3C After forming a liner material layer on the bottom and sidewalls of the second trench, the liner material layer 305 located inside the second trench 304 can be filled with photoresist 307 (PR), and the photoresist 307 can be patterned using a photolithography template 308 (Mask), and only the photoresist 307 at the bottom of the second trench 304 can be removed to expose the liner material layer at the bottom of the second trench 304, and then the liner material layer at the bottom of the second trench 304 can be etched using a wet etching process such as but not limited to, to form an opening that exposes at least a portion of the top surface of the first shielding gate. Then, the photoresist 307 can be removed.
[0055] Exemplarily, the material of the liner layer 306 may include at least one of the following: silicon nitride, silicon carbide, and silicon carbonitride. Specifically, the material of the liner layer 306 may be only any one of silicon nitride, silicon carbide, and silicon carbonitride; or, the material of the liner layer 306 may be only any two of silicon nitride, silicon carbide, and silicon carbonitride; or, the material of the liner layer 306 may be a material composed of a combination of silicon nitride, silicon carbide, and silicon carbonitride.
[0056] Then, step S4 is performed to form a second shielding gate in the second trench, wherein the top surface of the second shielding gate is lower than the surface of the substrate, and the second shielding gate is connected to the first shielding gate. Figure 3D, a second shielding gate 309 may be formed in the second trench 304 , and the second shielding gate 309 does not fill up the second trench 304 , so that a top surface of the second shielding gate 309 is lower than a surface of the substrate 300 .
[0057] Exemplarily, the material of the second shielding grid 309 may include polysilicon or other suitable materials. Exemplarily, the method for forming polysilicon may be a low pressure chemical vapor deposition (LPCVD) process. The process conditions for forming polysilicon include: the reaction gas is silane (SiH4), and the flow rate of silane may range from 100 to 200 cubic centimeters per minute (sccm), such as 150 sccm; the temperature range in the reaction chamber may be 700 to 750 degrees Celsius; the pressure in the reaction chamber may be 250 to 350 millimeters of mercury (mTorr), such as 300 mTorr; the reaction gas may also include a buffer gas, which may be helium (He) or nitrogen, and the flow rate range of helium and nitrogen may be 5 to 20 liters per minute (slm), such as 8 slm, 10 slm or 15 slm.
[0058] Optionally, in the process of forming the second shield gate in the second trench, the second shield gate can fill the second trench 304 and cover the surface of the substrate 300, or, in some embodiments, the second shield gate can also partially fill the second trench 304, for example, cover the side wall of the second trench 304 and cover the first shield gate 303 and the shielding dielectric layer 302.
[0059] Next, step S5 is performed to form an inter-gate dielectric layer in the second trench to cover the second shield gate. Figure 3E The inter-gate dielectric layer 310 may be further formed in the second trench 304 , and the inter-gate dielectric layer 310 covers the second shield gate 309 . For example, the top surface of the inter-gate dielectric layer 310 may be lower than the surface of the substrate 300 .
[0060] Exemplarily, the method of forming an inter-gate dielectric layer in the second trench to cover the second shielding gate may include: performing an oxidation process on a portion of the second shielding gate to oxidize the portion of the second shielding gate into the inter-gate dielectric layer. Exemplarily, referring to Figure 3E , a relatively thick second shielding gate 309 material may be deposited, and then a portion of the second shielding gate 309 material may be oxidized to oxidize a portion of the second shielding gate into an inter-gate dielectric layer 310. In the above embodiment, the inter-gate dielectric layer 310 is formed by oxidizing a portion of the second shielding gate 309, and during the oxidation process, the liner layer 306 covers the sidewalls of the second trench 304, thereby preventing the sidewalls of the second trench 304 from being oxidized, so that the critical dimension of the second trench 304 will not expand, thereby making the morphology of the subsequently formed gate structure more compatible with the design, thereby preventing the threshold voltage (Vth) from being affected.
[0061] Next, step S6 is performed to etch and remove a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer to form a third trench on the inter-gate dielectric layer.
[0062] For example, reference Figure 3F , a portion of the shielding dielectric layer 302 , a portion of the liner layer 306 , and a portion of the inter-gate dielectric layer 310 may be etched from top to bottom to form a third trench 311 above the remaining inter-gate dielectric layer 310 .
[0063] For example, reference Figure 3F After etching away a portion of the shielding dielectric layer 302, a portion of the liner layer 306, and a portion of the inter-gate dielectric layer 310 to form a third trench 311 on the inter-gate dielectric layer 310, the top surfaces of the shielding dielectric layer 302, the liner layer 306, and the inter-gate dielectric layer 310 are flush. It is worth mentioning that the top surface flush means relatively flush. Due to errors in the processing technology, the flush may mean that the height difference between the top of the shielding dielectric layer 302, the top of the liner layer 306, and the top of the inter-gate dielectric layer 310 is less than a predetermined height, or part of them are flush, and part of them have a certain height difference.
[0064] In one example, if Figure 3F As shown, a portion of the shielding dielectric layer 302, a portion of the liner layer 306, and a portion of the inter-gate dielectric layer 310 are etched and removed to form a third trench 311 located on the inter-gate dielectric layer 310. The distance from the top surface of the shielding dielectric layer 302 to the surface of the substrate is the third depth L3. Due to the presence of the first shielding gate 303, the second shielding gate 309, and the remaining inter-gate dielectric layer 310, the third depth L3 is less than the second depth L2, so that the filling depth of the subsequent deposition process is further reduced, and at this time, the distance W3 between the side walls of the third trench 311 located above the inter-gate dielectric layer 310 is greater than the second width W2, that is, the width of the third trench 311 is increased and the depth is reduced, so the aspect ratio of the third trench is reduced. As a result, the filling aspect ratio of the subsequent gate electrode layer deposition process is reduced, thereby reducing the requirements for the high-density plasma deposition process and solving the problem of HDP deposition process limitations. It can also increase the filling window, thereby reducing the appearance of voids during filling, improving the filling effect, and improving the electrical properties and yield of the device.
[0065] Finally, step S7 is performed to form a gate structure in the third trench. Figure 3G , the gate structure 314 may be formed in the third trench 311 in any manner.
[0066] Exemplarily, the method for forming a gate structure in the third trench may include: forming a gate dielectric layer on the sidewall of the third trench; forming a gate electrode layer to fill the third trench and cover the gate dielectric layer to form a gate structure, wherein the gate structure includes a gate dielectric layer and a gate electrode layer. Exemplarily, refer to Figure 3G The gate structure 314 may include a gate dielectric layer 312 formed on the sidewall of the third trench 311 , and a gate electrode layer 313 filled in the third trench 311 .
[0067] Exemplarily, the gate dielectric layer 312 may be silicon oxide (SiO2) or silicon oxynitride (SiON). The gate dielectric layer of silicon oxide may be formed by an oxidation process known to those skilled in the art, such as furnace tube oxidation, rapid thermal annealing oxidation (RTO), in-situ steam oxidation (ISSG), etc. The silicon oxide may be subjected to a nitridation process to form silicon oxynitride, wherein the nitridation process may be high temperature furnace tube nitridation, rapid thermal annealing nitridation or plasma nitridation. Of course, other nitridation processes may also be used, which will not be described in detail here.
[0068] Exemplarily, the material of the gate electrode layer 313 may include polysilicon or other suitable materials, and the method for forming polysilicon may be a low pressure chemical vapor deposition (LPCVD) process. The process conditions for forming polysilicon include: the reaction gas is silane (SiH4), and the flow rate of silane may range from 100 to 200 cubic centimeters per minute (sccm), such as 150 sccm; the temperature range in the reaction chamber may be 700 to 750 degrees Celsius; the pressure in the reaction chamber may be 250 to 350 millimeters of mercury (mTorr), such as 300 mTorr; the reaction gas may also include a buffer gas, and the buffer gas may be helium (He) or nitrogen, and the flow rate of helium and nitrogen may range from 5 to 20 liters per minute (slm), such as 8 slm, 10 slm or 15 slm.
[0069] In some embodiments, the material of the gate electrode layer 313 may also include a metal material, such as tungsten (W) or other suitable metal materials.
[0070] So far, the description of the key steps of the method for preparing the shielded gate field effect transistor of the present invention has been completed. The preparation of a complete shielded gate field effect transistor may also include other steps, which will not be described one by one here. It is worth mentioning that the order of the above steps can be adjusted without conflict.
[0071] In summary, the preparation method of the embodiment of the present invention, by etching the shielding dielectric layer above the first shielding gate, removes a portion of the thickness of the shielding dielectric layer, so as to form a second trench above the first shielding gate, and forms a liner layer on the sidewall of the second trench, and forms a second shielding gate in the second trench; then forms an inter-gate dielectric layer in the second trench to cover the second shielding gate. It is possible to reduce the aspect ratio of the second trench, so that the filling depth of the second trench is reduced, and the filling aspect ratio of the second trench is effectively reduced, thereby reducing the requirements for the high-density plasma deposition process, and solving the problem of HDP deposition process limitations.
[0072] Specifically, a first trench extending from the surface of the substrate to the inside of the substrate is first formed, a shielding dielectric layer is formed at the bottom and at least part of the sidewalls of the first trench, and a first shielding gate located on the shielding dielectric layer is formed in the first trench; then the shielding dielectric layer above the first shielding gate is etched to remove a portion of the thickness of the shielding dielectric layer to form a second trench above the first shielding gate, and a liner layer is formed on the sidewalls of the second trench, and a second shielding gate is formed in the second trench; then an inter-gate dielectric layer is formed in the second trench to cover the second shielding gate, and a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer are etched to remove a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer to form a third trench located on the inter-gate dielectric layer, and a gate structure is formed in the third trench. The above-mentioned preparation process includes three etching steps and steps of forming the first trench, the second trench, and the third trench respectively, which can reduce the aspect ratio of the first trench, the second trench, and the third trench, so that the filling depth of the trench is reduced, and the filling aspect ratio of the trench is effectively reduced, thereby reducing the requirements for the high-density plasma deposition process and solving the problem of HDP deposition process limitations. It can also increase the filling window, reduce the appearance of filling voids, improve the filling effect, and enhance the device electrical properties and yield. The preparation method shown in the above application can be applied to support HDP deposition processes with any filling depth-to-width ratio, ensuring that the selection of the filling process in the process of forming the inter-gate dielectric layer is not limited by the depth-to-width ratio of the trench, thus solving the problem of HDP deposition process limitations.
[0073] In some of the above embodiments, a shielding dielectric layer above the first shielding gate is etched to remove a portion of the thickness of the shielding dielectric layer, so as to form a second trench above the first shielding gate, and a liner layer is formed on the sidewalls of the second trench, and a second shielding gate is formed in the second trench; then, an inter-gate dielectric layer is formed in the second trench to cover the second shielding gate. In the scheme of the present application, by forming a liner layer on the sidewalls of the second trench, the sidewalls of the second trench can be prevented from being oxidized when the inter-gate dielectric layer is formed, thereby avoiding the expansion of the critical dimension (CD) on both sides of the second trench, so that the shape and size of the gate structure are more consistent with the design, thereby avoiding the impact on the threshold voltage (Vth) and improving the stability and reliability of the device.
[0074] Example 2
[0075] The present invention also provides a shielded gate field effect transistor, which is prepared by the method in the above-mentioned embodiment 1. Specifically, the shielded gate field effect transistor includes: a substrate, a first trench, a shielding dielectric layer, a first shielding gate, a second trench, a liner layer, a second shielding gate, an inter-gate dielectric layer, a third trench and a gate structure; wherein the first trench extends from the surface of the substrate to the inside of the substrate; the shielding dielectric layer is formed on the bottom and part of the sidewall of the first trench; the first shielding gate is formed in the first trench and is located on the shielding dielectric layer, and the top surface of the first shielding gate is lower than the top surface of the shielding dielectric layer; the second trench is arranged on the first shielding gate and is located above the first shielding gate. The first shielding gate is surrounded by a shielding dielectric layer; a liner layer is arranged on the side wall of the second groove, wherein an opening is also formed in the liner layer, and the opening exposes at least a portion of the top surface of the first shielding gate; the second shielding gate is arranged in the second groove, wherein the top surface of the second shielding gate is lower than the surface of the substrate, and the second shielding gate is connected to the first shielding gate; the inter-gate dielectric layer is arranged in the second groove and covers the top surface of the second shielding gate; the third groove extends from the surface of the substrate to the inside of the substrate, and is located on the shielding dielectric layer, the liner layer and the inter-gate dielectric layer; the gate structure is arranged in the third groove. Since the device of the present application is prepared by the aforementioned method, it has the same advantages as the aforementioned method.
[0076] Specifically, Figure 3A As shown, the substrate 300 includes a semiconductor base, and the semiconductor base may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the semiconductor base may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form a semiconductor base are described herein, any material that can be used as a semiconductor base falls within the scope of protection of the present invention. In addition, the substrate 300 may be divided into active areas, and / or a doped well (not shown) may be formed in the substrate 300, etc.
[0077] For example, reference Figure 3F , the top surfaces of the shielding dielectric layer 302, the liner layer 306 and the inter-gate dielectric layer 310 are flush. It is worth mentioning that the top surface flush means relatively flush. Due to the error of the processing technology, the flush may mean that the height difference between the top of the shielding dielectric layer 302, the top of the liner layer 306 and the top of the inter-gate dielectric layer 310 is less than the predetermined height, or part of them are flush and part of them have a certain height difference.
[0078] For example, reference Figure 3GThe gate structure 314 may include a gate dielectric layer 312 and a gate electrode layer 313 , the gate dielectric layer 312 is disposed on the sidewall of the third trench 311 , and the gate electrode layer 313 fills the third trench 311 and covers the gate dielectric layer 312 .
[0079] The structure of the shielded gate field effect transistor of the present invention has been introduced so far. A complete device may also include other component structures, which will not be described in detail here.
[0080] Example (III)
[0081] The present invention also provides an electronic device, comprising any of the above-mentioned shielded gate field effect transistors. Exemplarily, the electronic device may be a chip such as, but not limited to, a processor, a storage device, etc., which includes a shielded gate field effect transistor. Exemplarily, the electronic device may also be a terminal device such as a smartphone, a tablet computer, a desktop computer, a smart wearable device, etc., in which part of the chip uses the above-mentioned shielded gate field effect transistor.
[0082] Although multiple embodiments are described herein, it should be understood that a variety of other modifications and embodiments may be conceived by those skilled in the art, all of which will fall within the spirit and scope of the concepts disclosed in the present invention. More particularly, various modifications and changes may be made to the arrangements and / or components of the combined arrangements of the subject matter within the scope of the present disclosure, the drawings, and the appended claims. In addition to modifications and changes to the components and / or arrangements, the use of alternatives is also an obvious option for those skilled in the art.
Claims
1. A method for preparing a shielded gate field effect transistor, It is characterized in that The method comprises: Providing a substrate, forming a first trench extending from a surface of the substrate to an interior of the substrate, forming a shielding dielectric layer at the bottom and at least a portion of a sidewall of the first trench, and forming a first shielding grid located on the shielding dielectric layer in the first trench, wherein a top surface of the first shielding grid is lower than a top surface of the shielding dielectric layer; Etching the shielding dielectric layer above the first shielding gate to remove a portion of the thickness of the shielding dielectric layer to form a second trench above the first shielding gate; forming a liner layer on the sidewall of the second trench, wherein an opening is further formed in the liner layer, wherein the opening exposes the entire top surface of the first shielding grid; forming a second shielding gate in the second trench, wherein a top surface of the second shielding gate is lower than a surface of the substrate, and the second shielding gate is connected to the first shielding gate; forming an inter-gate dielectric layer in the second trench to cover the second shielding gate; Etching and removing a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer to form a third trench located on the inter-gate dielectric layer; A gate structure is formed in the third trench.
2. The preparation method according to claim 1, It is characterized in that The step of forming a liner layer on the sidewall of the second trench comprises: forming a liner material layer on the bottom and sidewalls of the second trench; At least a portion of the liner material layer located at the bottom of the second trench is etched to form the liner layer including the opening.
3. The preparation method according to claim 1, It is characterized in that Forming an inter-gate dielectric layer in the second trench to cover the second shielding gate includes: Performing oxidation treatment on a portion of the second shielding gate to oxidize a portion of the second shielding gate into the inter-gate dielectric layer.
4. The preparation method according to claim 1, It is characterized in that After the step of etching and removing a portion of the shielding dielectric layer, a portion of the liner layer, and a portion of the inter-gate dielectric layer to form a third trench on the inter-gate dielectric layer, the top surfaces of the shielding dielectric layer, the liner layer, and the inter-gate dielectric layer are flush.
5. The preparation method according to claim 1, It is characterized in that forming a gate structure in the third trench, comprising: forming a gate dielectric layer on the sidewalls of the third trench; A gate electrode layer is formed to fill the third trench and cover the gate dielectric layer to form the gate structure, wherein the gate structure includes the gate dielectric layer and the gate electrode layer.
6. The preparation method according to claim 1, It is characterized in that The material of the liner layer includes at least one of the following: silicon nitride, silicon carbide, silicon carbonitride; and / or The materials of the first shielding gate and the second shielding gate include polysilicon.
7. A shielded gate field effect transistor prepared by the preparation method according to any one of claims 1 to 6, It is characterized in that The shielded gate field effect transistor comprises: substrate; A first trench extending from the surface of the substrate to the interior of the substrate; a shielding dielectric layer formed on the bottom and a portion of the sidewall of the first trench; A first shielding grid is formed in the first trench and is located on the shielding dielectric layer, wherein a top surface of the first shielding grid is lower than a top surface of the shielding dielectric layer; a second trench, which is disposed on the first shielding gate and is surrounded by a portion of the shielding dielectric layer located above the first shielding gate; A liner layer is disposed on the sidewall of the second trench, wherein an opening is formed in the liner layer, and the opening exposes at least a portion of the top surface of the first shielding grid; A second shielding gate is disposed in the second trench, wherein a top surface of the second shielding gate is lower than a surface of the substrate, and the second shielding gate is connected to the first shielding gate, wherein a width of the second shielding gate is greater than a width of the first shielding gate; an inter-gate dielectric layer, disposed in the second trench and covering a top surface of the second shielding gate; a third trench extending from the surface of the substrate to the interior of the substrate and located on the shielding dielectric layer, the liner layer and the inter-gate dielectric layer; The gate structure is disposed in the third trench.
8. The shielded gate field effect transistor according to claim 7, It is characterized in that The top surfaces of the shielding dielectric layer, the liner layer and the inter-gate dielectric layer are flush.
9. The shielded gate field effect transistor according to claim 7, It is characterized in that The gate structure includes a gate dielectric layer and a gate electrode layer. The gate dielectric layer is arranged on the sidewall of the third trench, and the gate electrode layer fills the third trench and covers the gate dielectric layer.
10. An electronic device, It is characterized in that Comprising a shielded gate field effect transistor as claimed in any one of claims 7 to 9.
Citation Information
Patent Citations
Shield gate field effect transistor and forming method thereof
CN111681963A
Insulated gate semiconductor device structure
CN203325907U