Polymer nanospray needle manufacturing method based on leaf veins and polymer nanospray needle
Through the manufacturing method of polymer nano-jet needles based on leaf veins, using technologies such as casting stretching method and low-temperature milling, the preparation process of nano-jet needles is simplified, solving the problems of complex process and high cost in the existing technology, and achieving high efficiency, Low-cost nanojet manufacturing.
Patent Information
- Application Number
- CN202410958312.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2044-07-17
AI Technical Summary
In the existing technology, the preparation process of nano-jet needles is complicated, relies on expensive experimental equipment and ultra-clean environment, and the manufacturing cost is high. The brittleness of silicon nano-molds leads to increased process steps and higher costs.
The polymer nano-jet needle manufacturing method based on leaf veins is used to replicate the leaf vein pattern to obtain a micron structure. Nano-channels are manufactured using repeated casting and stretching methods, and the needle channels are sealed through low-temperature milling and oxygen plasma treatment to simplify the process steps. , reduce costs.
The manufacturing of nanochannels smaller than 100nm is realized, avoiding the dependence on ultra-clean environment and expensive equipment. The process is simple and low-cost, which significantly reduces the manufacturing cost of nano-jet preparation.
Smart Images

Figure CN118493714B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of micro-electromechanical technology, and in particular to a method for manufacturing a polymer nano-spray needle based on leaf veins and the polymer nano-spray needle. Background Art
[0002] Electrohydraulic jet printing technology in the field of additive manufacturing can obtain higher resolution printed graphics by using nanospray needles. Therefore, how to prepare nanospray needles to improve the printing resolution to the nanometer level is a technical problem that needs to be studied and solved at present. The key structure of the nanospray needle is the nanochannel of the spray needle. The manufacture of spray needle nanochannels by nanomanufacturing technology is currently a conventional process manufacturing method. For example, the focused ion beam uses high energy to bombard the sample to remove the surface material, and the nanochannel can be directly engraved without masking and additional etching process; the laser direct writing technology uses laser irradiation to remove the surface material of the workpiece and directly obtain the nanochannel. The above methods can all obtain high-precision, high-quality nanographics, and the processing size is flexible and controllable. However, this method relies on expensive processing equipment, has serial and time-consuming processing characteristics, and has high manufacturing costs.
[0003] Therefore, the prior art discloses a new preparation process, patent application number: CN202010893592.X; patent name: a method for manufacturing a micro-nano cross-scale polymer spray needle: the prior art uses side etching stripping method and reactive ion deep etching technology to prepare a silicon nano mold; the pattern of the silicon nano mold is transferred to PDMS by PDMS casting technology to prepare a PDMS nano mold with a nano channel pattern. The pattern of the PDMS nano mold is transferred to the photoresist by hot embossing to form a nano channel; a reverse ultraviolet exposure method is used to manufacture a micron channel and simultaneously ultraviolet cure the nanostructure. The micro-nano channel is encapsulated by oxygen plasma-assisted thermal bonding with a photoresist cover plate to obtain a micro-nano cross-scale polymer spray needle. After thermal bonding, a wet etching method is used to remove the glass substrate under the polymer spray needle, so that the front part of the polymer spray needle tip is suspended in the air, forming a polymer spray needle with a suspended tip and a micro-nano composite pattern. In the prior art, the pattern of the PDMS nano mold is transferred to the photoresist by hot embossing to form a nano channel, and then the photoresist cover plate is assisted by oxygen plasma thermal bonding to encapsulate the micro-nano channel to form a polymer spray needle. By means of hot embossing, it is necessary to prepare a silicon nano concave mold with a nanometer scale pattern in advance, but the silicon nano concave mold preparation process is extremely complicated, and ultraviolet exposure, wet etching, metal deposition, peeling, dry etching, and aqua regia are required to remove gold. In these process steps, all of them rely on expensive experimental equipment and require a clean room environment of 100 levels of cleanliness, and the silicon nano concave mold is expensive. Further, the silicon nano concave mold material is brittle, and it is very easy to crack with the silicon nano concave mold for hot embossing, thereby becoming consumables, greatly improving the manufacturing cost. Therefore, it is also necessary to further adopt the PDMS casting method to replicate the silicon nano concave mold pattern, obtain the PDMS nano convex mold as a hot pressing mold, indirectly improve the silicon nano concave mold life, but also increase the experimental steps of the process. Finally, hot-embossing photoresist is used to obtain the needle nano-channel, and ultraviolet lithography is used to obtain the needle micron pattern. Both require an ultra-clean experimental environment, and the operation steps are complicated and costly.
[0004] In summary, the shortcomings of the prior art are:
[0005] (1) The process is too complicated. The entire needle preparation process is mainly divided into silicon nano-concave mold preparation, PDMS nano-convex mold preparation, and polymer needle preparation.
[0006] (2) The preparation process of silicon nano-concave mold is extremely complicated, and requires: UV exposure, wet etching, metal deposition, stripping, dry etching, and aqua regia gold removal. These process steps rely on expensive experimental equipment and require a Class 100 clean room environment.
[0007] (3) After obtaining the silicon nano-concave mold, since silicon is brittle, it is very easy to crack during hot pressing. Therefore, it is necessary to cast the silicon nano-concave mold with PDMS to obtain a PDMS nano-convex mold, which can replace the silicon nano-concave mold for hot pressing, indirectly extending the life of the mold.
[0008] (4) The preparation of polymer spray needles relies on hot embossing of the previously prepared PDMS mold, and also relies on UV exposure. Hot embossing obtains nanochannels, and UV exposure obtains microchannels. Among them, UV exposure still relies on expensive experimental equipment, photolithography, and photolithography requires a Class 100 clean laboratory environment. Summary of the invention
[0009] The present invention overcomes the shortcomings of the prior art and provides a method for manufacturing a polymer nano-spray needle based on leaf veins and a polymer nano-spray needle. The micron structure is obtained by casting and replicating the leaf vein pattern, and the polymer spray needle nano-channel is obtained by repeated casting and stretching. The polymer spray needle micro-channel is manufactured by a low-temperature milling method. Finally, the polymer spray needle micro-nano channel is sealed by an oxygen plasma treatment method to obtain a complete polymer nano-spray needle.
[0010] To achieve the above object, the technical solution adopted by the present invention is: a method for manufacturing polymer nano-spray needles based on leaf veins, comprising the following steps:
[0011] Step S1, preparing unbonded polymer nanospray needles and polymer nanospray needle cover plates, and proceeding to step 2;
[0012] The method for preparing the unbonded polymer nanospray needle comprises the following steps:
[0013] Step S1.a1, duplicating the plant venation array micron pattern by casting method to manufacture a PDMS array micron concave mold;
[0014] The steps of obtaining the plant vein array micrometer pattern include:
[0015] Step S1.a1.1, obtaining a plant body having a plant venation structure, and purifying and drying the plant body;
[0016] Step S1.a1.2, laying the purified and dried plant body on a PMMA substrate, pouring a PDMS curing agent mixed solution onto the plant body and curing it to obtain a PDMS array micron concave mold;
[0017] Step S1.a2, manufacturing a polymer needle nanochannel carrier by a repeated casting and stretching method on the PDMS array micron concave mold obtained in step S1.a1;
[0018] Step S1.a3, performing cryogenic milling on the polymer needle nanochannel carrier obtained in step S1.a2 to manufacture a polymer needle microchannel to obtain an unbonded polymer nanoneedle;
[0019] The preparation method of the polymer nanospray needle cover plate comprises the following steps:
[0020] Step S1.b1, pouring the PDMS curing agent mixed solution on the PMMA substrate and placing it in a vacuum environment to evacuate;
[0021] Step S1.b2, placing the PMMA substrate with the PDMS curing agent mixed solution treated in step S1.b1 in an oven for curing, separating the cured PDMS solid body from the PMMA substrate, and using the separated PDMS solid body as a polymer nanospray needle cover plate;
[0022] Step 2, respectively subjecting the unbonded polymer nanospray needle and the polymer spray needle cover plate to oxygen plasma treatment, and proceeding to step 3;
[0023] Step 3, bonding the unbonded polymer nanospray needle treated in step 2 to the polymer nanospray needle cover plate, sealing the spray needle micro-nano channel on the unbonded polymer nanospray needle, and obtaining a complete polymer nanospray needle.
[0024] In a preferred embodiment of the present invention, in step S1.a1.1, the purification and drying of the plant body comprises the following steps:
[0025] The plant body is ultrasonically cleaned with deionized water for 10 to 30 minutes, wherein the ultrasonic power is 60 to 100 W and the temperature is 20 to 26° C. The cleaned plant body is blown dry with a nitrogen air gun, and then the plant body is wiped with an alcohol cotton ball, and then the plant body is repeatedly rinsed in deionized water for 3 times, and then the plant body is blown dry with a nitrogen air gun and placed in a ventilated and dry place to remove moisture from the plant body; and the cleaned plant body is hydrophobic treated.
[0026] In a preferred embodiment of the present invention, in step S1.a1.2, the curing operation of pouring the PDMS curing agent mixed solution onto the plant body comprises the following steps:
[0027] The PDMS substrate with the plant body cast with the PDMS curing agent mixed solution is placed in a vacuum environment below 10Pa and evacuated for 1-2 hours, then placed on a horizontal flat table for curing for 24 hours. After curing, the PDMS casting layer and the plant body are separated to obtain a PDMS array micron concave mold with a width of 4-8 mm.
[0028] In a preferred embodiment of the present invention, the repeated casting and stretching method comprises the following steps:
[0029] Step S1.a2.1, fix the PDMS array micron concave mold, stretch the length to 40-50% of the original PDMS array micron concave mold, then fix the stretched PDMS array micron concave mold on the PMMA substrate, and pour the PDMS curing agent mixed solution into the stretched PDMS array micron concave mold and cure it to obtain a PDMS array micron convex mold;
[0030] Step S1.a2.1 is repeated until a polymer needle nanochannel support with PDMS array nanochannels with a size less than 100 nm is obtained.
[0031] In a preferred embodiment of the present invention, in step S1.a2.1, a PDMS array micron concave mold with a width of 4 to 8 mm is fixed and stretched, and the stretching length is 40 to 50% of the original PDMS array micron concave mold to obtain a PDMS array micron concave mold with a width of 2.8 to 5.6 mm; the PDMS array micron concave mold with a width of 2.8 to 5.6 mm is fixed on a PMMA substrate, and a PDMS curing agent mixed solution with a ratio of 20:1 to 30:1 is poured into the PDMS array micron concave mold with a width of 2.8 to 5.6 mm and placed in a vacuum environment below 10 Pa for 1 to 2 hours, and then placed in a 60 to 85°C oven for curing for 1.5 to 4 hours, and then a PDMS array micron convex mold with a width of 2.8 to 5.6 mm is obtained;
[0032] The PDMS array micron convex mold with a width of 2.8~5.6mm is fixed and stretched to 40~50% of the length of the PDMS array micron convex mold of 2.8~5.6mm to obtain a PDMS array micron convex mold with a width of 2.1~4.1mm; the casting and stretching cycle is repeated 9 times until a PDMS array nanochannel with a size less than 100nm is obtained.
[0033] In a preferred embodiment of the present invention, in step S1.a3, the polymer needle nanochannel carrier is subjected to cryogenic milling processing, and the cryogenic milling processing comprises the following steps: at one end of the 100nm nanochannel of the polymer needle nanochannel carrier, needle micro-channels with widths of 50mm and 100mm are milled sequentially from the inside to the outside, and a needle liquid reservoir with a diameter of 3mm is processed at the tail end of the 100mm needle micro-channel under liquid nitrogen low temperature conditions; finally, an unbonded polymer nano-needle is obtained.
[0034] Specifically, from the inside to the outside, it borders on a 100nm channel, followed by 50um and then 100um.
[0035] In a preferred embodiment of the present invention, in step S1.a1, the PDMS curing temperature is 20-26° C., and the curing time is 24 h;
[0036] and / or, the ratio of PDMS to curing agent in the PDMS curing agent mixed solution in step S1.a1 and step S1.a2 is 20:1 to 30:1;
[0037] and / or, in step S1.a3, liquid nitrogen is directly added to the cutting zone during cryogenic milling;
[0038] and / or, the ratio of PDMS to curing agent in the PDMS curing agent mixed solution in step S1.b1 is 5:1 to 10:1;
[0039] And / or, the vacuum environment in step S1.b1 is a vacuum environment below 10Pa, and the vacuuming time is 1 to 2 hours;
[0040] And / or, the temperature of the oven in step S1.b2 is 60-85°C, and the drying time is 1.5-4h;
[0041] And / or, in step S2, the processing parameters of the oxygen plasma treatment are: the processing power of the oxygen plasma is 15-25 W, and the processing time is 10-25 s.
[0042] In a preferred embodiment of the present invention, the hydrophobic treatment of the plant body comprises the following steps: dripping 1-2 ml of trimethylsiloxane into a sealed drying tower, and after volatilization for 5-10 minutes, vertically placing the plant body into a sealed drying tower with a trimethylsiloxane atmosphere for atmosphere treatment for 10-20 minutes;
[0043] And / or, in step S1.a1.2, the PDMS curing agent mixed solution is poured onto the plant body and placed on a horizontal stationary table to cure at room temperature for 24 hours.
[0044] And / or, in step S1.a2, before repeatedly casting and stretching the PDMS array micron-concave mold obtained in step S1.a1, the PDMS array micron-concave mold is subjected to trimethylsiloxane hydrophobic treatment, and the treatment time is 15 to 20 minutes.
[0045] In a preferred embodiment of the present invention, the plant body includes ginkgo leaves, creepers, or foxtail grass;
[0046] And / or, plant matter can be replaced with silk or spider silk.
[0047] In a preferred embodiment of the present invention, the hydrophobic treatment of the plant body comprises the following steps:
[0048] 1-2 ml of trimethylsiloxane was dripped into a sealed drying tower and evaporated for 5-10 minutes. Then, the plant was placed vertically in a sealed drying tower with trimethylsiloxane atmosphere for 10-20 minutes.
[0049] And / or, in step S1.a1.2, the PDMS curing agent mixed solution is poured onto the plant body and placed on a horizontal stationary table to cure at room temperature for 24 hours.
[0050] And / or, in step S1.a2, before repeatedly casting and stretching the PDMS array micron-concave mold obtained in step S1.a1, the PDMS array micron-concave mold is subjected to trimethylsiloxane hydrophobic treatment, and the treatment time is 15 to 20 minutes.
[0051] In a preferred embodiment of the present invention, in step S1.b2, the PMMA substrate with the PDMS curing agent mixed solution is placed in an oven for curing time of 1.5 h at 85°C, 2 h at 80°C, 2.5 h at 75°C, 3 h at 70°C, 3.5 h at 65°C, and 4 h at 60°C; the PDMS oxygen plasma treatment parameters are a treatment power of 15-25 W and a treatment time of 10-25 s.
[0052] In a preferred embodiment of the present invention, a polymer nano-spray needle based on leaf veins is prepared by a polymer nano-spray needle manufacturing method based on leaf veins.
[0053] The present invention solves the defects existing in the technical background, and the beneficial technical effects of the present invention are:
[0054] The present invention discloses a method for manufacturing a polymer nano-spray needle based on leaf veins and a polymer nano-spray needle. The micron structure is obtained by casting and replicating the leaf vein pattern, and the polymer nano-spray needle nano-channel is obtained by repeated casting and stretching. The polymer nano-spray needle micro-channel is manufactured by a low-temperature milling method. Finally, the micro-nano channel of the unbonded polymer nano-spray needle is sealed by an oxygen plasma treatment method to obtain a complete polymer nano-spray needle.
[0055] The present invention adopts a stretching casting method to manufacture a polymer spray needle nanochannel less than 100nm, and adopts a low-temperature milling method to manufacture a polymer spray needle micron channel. The method of the present invention is used to manufacture nano spray needles, which does not rely on ultra-clean experimental environment and expensive experimental equipment, and has the beneficial effects of simple process, low cost, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0056] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0057] Figure 1This is a flow chart for manufacturing polymer needle nanochannels based on leaf veins in a preferred embodiment of the present invention.
[0058] Figure 2 It is a flow chart of manufacturing polymer needle micro-channel in a preferred embodiment of the present invention.
[0059] Figure 3 It is a flow chart of polymer needle bonding in a preferred embodiment of the present invention.
[0060] Figure 4 It is a schematic diagram of the polymer nanospray needle structure in a preferred embodiment of the present invention.
[0061] Figure 5 It is a microscope image of ginkgo leaves in a preferred embodiment of the present invention.
[0062] Figure 6 This is a SEM image of a polymer needle nanochannel based on leaf veins in a preferred embodiment of the present invention.
[0063] Figure 7 This is a SEM image of the polymer nanospray needle microchannel and liquid reservoir based on leaf veins in a preferred embodiment of the present invention.
[0064] In the figure: 1. Ginkgo leaf; 2. PDMS curing agent mixed solution; 3. PDMS array micron convex mold; 4. PDMS array nanochannel; 5. 50mm milling cutter; 6. 100mm milling cutter; 7. 3mm milling cutter; 8. Punch; 9. Polymer nanospray needle cover plate; 10. Oxygen plasma ashing instrument. DETAILED DESCRIPTION
[0065] The present invention will now be further described in detail with reference to the accompanying drawings and embodiments. These drawings are simplified schematic diagrams that only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.
[0066] It should be noted that if there are directional indications (such as up, down, bottom, top, etc.) involved in the embodiments of the present invention, the directional indication is only used to explain the relative position relationship, movement, etc. between the components in a certain specific posture. If the specific posture changes, the directional indication will also change accordingly. The terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. Unless otherwise clearly specified and defined, the terms "set", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected, or indirectly connected through an intermediate medium, or it can be the internal connection of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. Embodiment 1
[0067] like Figure 1-Figure 7 As shown, in order to achieve the above purpose, the technical solution adopted by the present invention is: a method for manufacturing polymer nano-spray needles based on leaf veins, comprising the following steps:
[0068] Step S1, preparing unbonded polymer nanospray needles and polymer nanospray needle cover plate 9, and proceeding to step 2;
[0069] The method for preparing the unbonded polymer nanospray needle comprises the following steps:
[0070] Step S1.a1, duplicating the plant venation array micron pattern by casting method to manufacture a PDMS array micron concave mold.
[0071] Specifically, the steps for obtaining the plant vein array micrometer pattern include:
[0072] Step S1.a1.1, obtain a plant body with a plant venation structure, and purify and dry the plant body. The purification and drying treatment of the plant body includes the following steps: ultrasonically clean the plant body with deionized water for 10 to 30 minutes, wherein the ultrasonic power is 60 to 100 W and the temperature is 20 to 26°C; blow dry the cleaned plant body with a nitrogen air gun, and then wipe the plant body with an alcohol cotton ball, and then put the plant body into deionized water again and rinse it repeatedly for 3 times, and then use a nitrogen air gun to blow dry the plant body and place it in a ventilated and dry place to remove the moisture of the plant body; and then perform a hydrophobic treatment on the cleaned plant body. The hydrophobic treatment process of the plant body includes: dripping 1 to 2 ml of trimethylsiloxane into a sealed drying tower, and after volatilization for 5 to 10 minutes, the plant body is vertically placed in a sealed drying tower with a trimethylsiloxane atmosphere for atmosphere treatment for 10 to 20 minutes (such as Figure 5 shown).
[0073] Step S1.a1.2, laying the purified and dried plant body on a PMMA (polymethyl methacrylate) substrate, pouring the PDMS curing agent mixed solution 2 onto the plant body and curing it (such as Figure 5 As shown), obtain a PDMS array micron concave mold (as shown Figure 1 1a in step 1). Further, the curing operation of pouring the PDMS curing agent mixed solution onto the plant body comprises the following steps: placing the PMMA substrate with the plant body poured with the PDMS curing agent mixed solution 2 in a vacuum environment below 10Pa for 1-2 hours, and then placing it on a horizontal stationary table for curing for 24 hours, and separating the PDMS pouring layer from the plant body after curing to obtain a PDMS array micron concave mold with a width of 4-8 mm.
[0074] Step S1.a2, manufacturing a polymer needle nanochannel carrier by repeatedly casting and stretching the PDMS array micron-concave mold obtained in step S1.a1; before repeatedly casting and stretching the PDMS array micron-concave mold, the PDMS array micron-concave mold is first subjected to trimethylsiloxane hydrophobic treatment for 15 to 20 minutes.
[0075] The repeated casting and stretching method comprises the following steps:
[0076] Step S1.a2.1, fix the PDMS array micron concave mold, and stretch the length to 40-50% of the original PDMS array micron concave mold (such as Figure 1 As shown in step 1b in the figure), the stretching length here is the length after stretching minus the length before stretching, and then the PDMS array micron concave mold after this stretching is fixed on the PMMA substrate; the PDMS curing agent mixed solution is poured into the PDMS array micron concave mold after this stretching and cured to obtain the PDMS array micron convex mold 3 (as shown in the figure Figure 1 Then fix the PDMS array micron convex mold 3, and stretch the PDMS array micron convex mold 3 to a length of 40-50% (as shown in step 1c of FIG. Figure 1 The stretching length here is the length after stretching minus the length before stretching; the PDMS curing agent mixed solution is poured into the PDMS array micron convex mold 3 after this stretching and cured to obtain a PDMS array micron concave mold, and the step S1.a2.1 is repeated until a polymer needle nanochannel carrier with a PDMS array nanochannel 4 with a size less than 100 nm is obtained (such as Figure 2 as shown in step 2a in the previous step).
[0077] Step S1.a3, the polymer needle nanochannel carrier (such as Figure 2 The polymer needle micron channel is manufactured by cryogenic milling (as shown in step 2a in FIG. Figure 2 As shown in steps 2b, 2c, and 2d in the figure), an unbonded polymer nanospray needle is obtained.
[0078] The cryogenic milling process comprises the following steps: milling a 50 mm wide nozzle micron channel (such as Figure 2 2b in step 2) and a 100 mm needle micron channel (as shown in Figure 2 As shown in step 2c in the figure), a 3 mm diameter needle reservoir is machined at the tail end of the 100 mm needle micro-channel under liquid nitrogen cryogenic conditions (as shown in step 2c in the figure). Figure 2 Finally, an unbonded polymer nanospray needle is obtained (as shown in step 2d in FIG. Figure 2 As shown in step 2e in ). Further, the specific low-temperature milling processing steps include: placing the polymer needle nanochannel carrier on the low-temperature milling processing platform, using a 50mm milling cutter 5 with a diameter of 50mm at one end of the 100nm nanochannel of the polymer needle nanochannel carrier to mill a needle microchannel with a width of 50mm on the basis of the 100nm nanochannel of the polymer needle nanochannel carrier. Then use a 100mm milling cutter 6 with a diameter of 100mm to mill a needle microchannel with a width of 100mm on the basis of the 50mm channel. Finally, a 3mm milling cutter 7 with a diameter of 3mm is used to process a needle reservoir with a diameter of 3mm under liquid nitrogen low temperature conditions. Finally, a non-bonded polymer nano-spray needle across the micro-nano scale is obtained. Among them, liquid nitrogen is directly added to the cutting area during the low-temperature milling process. Since PDMS is a soft elastic material, the milling cutter cannot accurately process soft elastic materials at room temperature. Liquid nitrogen is used to reduce the temperature during the milling process of PDMS, making PDMS brittle and hardened, making it easier to process.
[0079] The preparation method of the polymer nanospray needle cover plate 9 comprises the following steps:
[0080] Step S1.b1, pouring the PDMS curing agent mixed solution on the PMMA substrate and placing it in a vacuum environment for evacuation; wherein the ratio of PDMS and curing agent in the PDMS curing agent mixed solution is 5:1~10:1; the vacuum environment is a vacuum environment below 10Pa, and the vacuuming time is 1~2h.
[0081] Step S1.b2, place the PMMA substrate with the PDMS curing agent mixed solution treated in step S1.b1 in an oven for curing, the oven temperature is 60~85℃, and the heat drying time is 1.5~4h. The PDMS oxygen plasma treatment parameters are: the treatment power is 15~25W, and the treatment time is 10~25s. Separate the cured PDMS solid body from the PMMA substrate, and use the separated PDMS solid body as the polymer nanospray needle cover plate 9. Figure 3 As shown in step 3a, the polymer nano-spray needle cover plate is fixed, and a hole is made on the polymer nano-spray needle cover plate 9 by a punch 8 (such as Figure 3 As shown in 3b in FIG, the opening position corresponds to the needle reservoir on the unbonded polymer nanoneedle.
[0082] Step 2: Place the unbonded polymer nanospray needle and the polymer spray needle cover plate into an oxygen plasma ashing apparatus 10 for oxygen plasma treatment (eg Figure 3 As shown in 3c in FIG), the processing power of the oxygen plasma treatment is 15-25W, and the processing time is 10-25s; then proceed to step 3;
[0083] Step 3, bonding the unbonded polymer nanospray needles treated in step 2 to the polymer nanospray needle cover plate 9, sealing the spray needle micro-nano channels on the unbonded polymer nanospray needles, and obtaining a complete polymer nanospray needle (such as Figure 3 3D in Figure 4 as shown). Embodiment 2
[0084] On the basis of Example 1, in step S1.a2.1, the PDMS array micron concave mold with a width of 4-8 mm is fixed and stretched, and the stretching length is 40-50% of the original PDMS array micron concave mold, to obtain a PDMS array micron concave mold with a width of 2.8-5.6 mm, where the stretching length is the length after stretching minus the length before stretching. The PDMS array micron concave mold with a width of 2.8-5.6 mm is fixed on a PMMA substrate, and a PDMS curing agent mixed solution with a ratio of 20:1-30:1 is poured into the PDMS array micron concave mold with a width of 2.8-5.6 mm and placed in a vacuum environment below 10 Pa for 1-2 hours, and then placed in a 60-85°C oven for curing for 1.5-4 hours, and then a PDMS array micron convex mold 3 with a width of 2.8-5.6 mm is obtained. The PDMS array micron convex mold 3 with a width of 2.8-5.6 mm is fixed and stretched to a length of 40-50% of the length of the PDMS array micron convex mold 3 with a width of 2.1-4.1 mm, where the stretching length is the length after stretching minus the length before stretching. The casting and stretching cycle is repeated 9 times until a PDMS array nanochannel 4 with a size less than 100 nm is obtained. Embodiment 3
[0085] On the basis of Example 1 or Example 2, the plant body includes Ginkgo biloba leaves 1 (such as Figure 5 as shown). Embodiment 4
[0086] On the basis of the first or second embodiment, the plant body may also be plants with striped veins such as Parthenocissus tricuspidata and Foxtail grass.
[0087] But it is not limited to this. In other embodiments, the plant body can also be replaced by silk or spider silk. Embodiment 5
[0088] The polymer nanospray needle is prepared by the method for manufacturing the polymer nanospray needle based on leaf veins of Example 1, Example 2 or Example 3, such as Figure 4 shown.
[0089] Working principle:
[0090] The present invention adopts a stretching casting method to manufacture a polymer spray needle nanochannel less than 100nm, and adopts a low-temperature milling method to manufacture a polymer spray needle micron channel. The method of the present invention is used to manufacture nano spray needles, which does not rely on ultra-clean experimental environment and expensive experimental equipment, and has the beneficial effects of simple process, low cost, etc.
[0091] The above specific implementation methods are specific support for the scheme ideas proposed in the present invention, and cannot be used to limit the protection scope of the present invention. Any equivalent changes or equivalent modifications made on the basis of this technical scheme in accordance with the technical ideas proposed in the present invention still fall within the scope of protection of the technical scheme of the present invention.
Claims
1. A method for manufacturing polymer nano-spray needles based on leaf veins, characterized in that: The following steps are involved: Step S1, preparing unbonded polymer nanospray needles and polymer nanospray needle cover plates, and proceeding to step 2; The method for preparing the unbonded polymer nanospray needle comprises the following steps: Step S1.a1, duplicating the plant venation array micron pattern by casting method to manufacture a PDMS array micron concave mold; The steps of obtaining the plant vein array micrometer pattern include: Step S1.a1.1, obtaining a plant body having a plant venation structure, and purifying and drying the plant body; Step S1.a1.2, laying the purified and dried plant body on a PMMA substrate, pouring a PDMS curing agent mixed solution onto the plant body and curing it to obtain a PDMS array micron concave mold; Step S1.a2, manufacturing a polymer needle nanochannel carrier by a repeated casting and stretching method on the PDMS array micron concave mold obtained in step S1.a1; Step S1.a3, performing cryogenic milling on the polymer needle nanochannel carrier obtained in step S1.a2 to manufacture a polymer needle microchannel to obtain an unbonded polymer nanoneedle; The preparation method of the polymer nanospray needle cover plate comprises the following steps: Step S1.b1, pouring the PDMS curing agent mixed solution on the PMMA substrate and placing it in a vacuum environment to evacuate; Step S1.b2, placing the PMMA substrate with the PDMS curing agent mixed solution treated in step S1.b1 in an oven for curing, separating the cured PDMS solid body from the PMMA substrate, and using the separated PDMS solid body as a polymer nanospray needle cover plate; Step 2, respectively subjecting the unbonded polymer nanospray needle and the polymer spray needle cover plate to oxygen plasma treatment, and proceeding to step 3; Step 3, bonding the unbonded polymer nanospray needle treated in step 2 to the polymer nanospray needle cover plate, sealing the spray needle micro-nano channel on the unbonded polymer nanospray needle, and obtaining a complete polymer nanospray needle; In step S1.a1.1, the purification and drying process of the plant body comprises the following steps: The plant body is ultrasonically cleaned with deionized water for 10 to 30 minutes, wherein the ultrasonic power is 60 to 100 W and the temperature is 20 to 26° C. The cleaned plant body is blown dry with a nitrogen air gun, and then the plant body is wiped with an alcohol cotton ball, and then the plant body is repeatedly rinsed in deionized water for 3 times, and then the plant body is blown dry with a nitrogen air gun and placed in a ventilated and dry place to remove moisture from the plant body; and then the cleaned plant body is subjected to hydrophobic treatment; In step S1.a1.2, the curing operation of pouring the PDMS curing agent mixed solution onto the plant body includes the following steps: The PMMA substrate with the plant body casted with the PDMS curing agent mixed solution is placed in a vacuum environment below 10Pa for 1-2 hours, and then placed on a horizontal stationary table for curing for 24 hours. After curing, the PDMS casting layer and the plant body are separated to obtain a PDMS array micron concave mold with a width of 4-8 mm; The repeated casting and stretching method comprises the following steps: Step S1.a2.1, fix the PDMS array micron concave mold, stretch the length to 40-50% of the original PDMS array micron concave mold, then fix the stretched PDMS array micron concave mold on the PMMA substrate, and pour the PDMS curing agent mixed solution into the stretched PDMS array micron concave mold and cure it to obtain a PDMS array micron convex mold; Step S1.a2.1 is repeated until a polymer needle nanochannel support with a PDMS array nanochannel having a size less than 100 nm is obtained; In step S1.a2.1, a PDMS array micron concave mold with a width of 4-8 mm is fixed and stretched to a length of 40-50% of the original PDMS array micron concave mold, to obtain a PDMS array micron concave mold with a width of 2.8-5.6 mm; a PDMS array micron concave mold with a width of 2.8-5.6 mm is fixed on a PMMA substrate, a PDMS curing agent mixed solution with a ratio of 20:1-30:1 is poured into the PDMS array micron concave mold with a width of 2.8-5.6 mm and placed in a vacuum environment below 10 Pa for 1-2 hours, and then placed in a 60-85°C oven for curing for 1.5-4 hours, and then a PDMS array micron convex mold with a width of 2.8-5.6 mm is obtained; The PDMS array micron convex mold with a width of 2.8-5.6 mm is fixed and stretched to 40-50% of the length of the PDMS array micron convex mold with a width of 2.8-5.6 mm to obtain a PDMS array micron convex mold with a width of 2.1-4.1 mm; the casting and stretching cycle is repeated 9 times until a PDMS array nanochannel with a size less than 100 nm is obtained; In step S1.a3, the polymer needle nanochannel support is subjected to cryogenic milling. The low-temperature milling process comprises the following steps: milling a 50 mm and a 100 mm wide nozzle micro-channel from the inside out at one end of a 100 nm nano-channel of a polymer nozzle nano-channel carrier, and processing a nozzle liquid reservoir with a diameter of 3 mm at the tail end of the 100 mm nozzle micro-channel under liquid nitrogen low temperature conditions; and finally obtaining an unbonded polymer nano-needle.
2. The method for manufacturing polymer nano-spray needles based on leaf veins according to claim 1, characterized in that: In step S1.a1, the PDMS curing temperature is 20-26°C and the curing time is 24h; and / or, the ratio of PDMS to curing agent in the PDMS curing agent mixed solution in step S1.a1 and step S1.a2 is 20:1 to 30:1; and / or, in step S1.a3, liquid nitrogen is directly added to the cutting zone during cryogenic milling; and / or, the ratio of PDMS to curing agent in the PDMS curing agent mixed solution in step S1.b1 is 5:1 to 10:1; And / or, the vacuum environment in step S1.b1 is a vacuum environment below 10Pa, and the vacuuming time is 1 to 2 hours; And / or, the temperature of the oven in step S1.b2 is 60-85°C, and the drying time is 1.5-4h; And / or, in step S2, the processing parameters of the oxygen plasma treatment are: the processing power of the oxygen plasma is 15-25 W, and the processing time is 10-25 s.
3. The method for manufacturing polymer nano-spray needles based on leaf veins according to claim 2, characterized in that: The hydrophobic treatment of the plant body comprises the following steps: dripping 1-2 ml of trimethylsiloxane into a sealed drying tower, and after volatilization for 5-10 minutes, vertically placing the plant body into a sealed drying tower with a trimethylsiloxane atmosphere for atmosphere treatment for 10-20 minutes; And / or, in step S1.a1.2, the PDMS curing agent mixed solution is poured onto the plant body and placed on a horizontal stationary table to cure at room temperature for 24 hours; And / or, in step S1.a2, before repeatedly casting and stretching the PDMS array micron-concave mold obtained in step S1.a1, the PDMS array micron-concave mold is subjected to trimethylsiloxane hydrophobic treatment, and the treatment time is 15 to 20 minutes.
4. The method for manufacturing polymer nano-spray needles based on leaf veins according to claim 3, characterized in that: The plant body includes ginkgo leaves, creepers, or foxtail grass; And / or, the plant material can be replaced with silk or spider silk.
5. A polymer nanospray needle based on leaf veins, characterized in that: The polymer nano-spray needle is prepared by the method for manufacturing the polymer nano-spray needle based on leaf veins as described in any one of claims 1 to 4.