Crude alcohol purification and recovery process based on coal-based fuel ethanol
By modifying fly ash, composite diatomaceous earth and reinforced particles, the parameters of the distillation tower are optimized, and the problem of insufficient removal capacity of by-product impurities in the prior art is solved, and the purity of the finished ethanol is significantly improved.
Patent Information
- Application Number
- CN202411053897.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-08-02
AI Technical Summary
In the prior art, when the coal-based fuel crude ethanol is purified by using a distillation tower, the ability to remove by-product impurities is limited, which makes it difficult to improve the purity of the finished ethanol.
Adsorbents are prepared by materials such as modified fly ash, composite diatomaceous earth and reinforced particles. Complex zinc acetate with 5,5'-methylene bis(1H-benzotriazole) to form reinforced particles and with Compound diatomaceous earth and modified fly ash are mixed, filled in the distillation tower, optimized the filling method of adsorbent and the distillation tower parameters, and improved adsorption efficiency.
Effectively reduce the methanol, n-propanol, moisture and acid content in crude ethanol, improve the purity of the finished ethanol, and prepare high-purity ethanol.
Smart Images

Figure CN118561660B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of crude fuel ethanol refining, and in particular to a crude alcohol purification and recovery process based on coal-based fuel ethanol. Background Art
[0002] The consumption of fossil energy and the carbon emissions caused by it are forcing people to look for new renewable energy sources. Fuel ethanol, as a renewable green biofuel, has attracted widespread attention and has become one of the most widely used renewable clean energy sources in the world. It can supplement and replace fossil energy, reduce greenhouse gas and pollutant emissions, and fuel ethanol is also a high-quality automotive alternative liquid fuel and oil quality improver. Data show that in 2020, the world's fuel ethanol production reached 98.644 billion liters, and the blended ethanol gasoline exceeded 60% of the total global automotive gasoline consumption in the same period.
[0003] With the continuous growth of global energy demand and increasingly severe environmental problems, finding clean and renewable energy alternatives has become a consensus of the international community. Coal-based fuel ethanol, as an important biofuel and chemical raw material, has the advantages of wide sources, strong renewability, environmental protection and low carbon, and is gradually becoming an ideal substitute for traditional petroleum-based fuels.
[0004] However, the coal-based fuel ethanol production process in the prior art produces a large amount of by-products, such as water, methanol, acetic acid and other organic impurities, which have low direct utilization value and cause certain pollution to the environment. At present, purifying coal-based fuel crude ethanol by distillation tower is a common purification and recovery method in the coal-based fuel ethanol production process. In the process of using distillation tower to distill crude ethanol, molecular sieves are usually selected as filler adsorbents in the distillation tower. However, molecular sieves have poor selectivity for by-products in fuel crude ethanol. Limited by the porosity of the molecular sieve itself, the molecular sieve has limited adsorption capacity for by-products in fuel crude ethanol, resulting in the purity of the finished ethanol prepared by purification and recovery of crude ethanol needs to be further improved.
[0005] In view of the technical defects in this aspect, a solution is now proposed. Summary of the invention
[0006] The purpose of the present invention is to provide a crude alcohol purification and recovery process based on coal-based fuel ethanol, which is used to solve the technical problems in the prior art that in the process of refining crude fuel ethanol using a distillation tower, the removal of by-product impurities in the finished ethanol is limited, and the purity of the finished ethanol prepared by purifying and recovering crude fuel ethanol needs to be further improved.
[0007] The purpose of the present invention can be achieved by the following technical scheme: A crude alcohol purification and recovery process based on coal-based fuel ethanol comprises the following steps:
[0008] S1, placing adsorbent on the top of each tray of the ethanol distillation tower to form an adsorption bed;
[0009] S2, transporting crude ethanol from a feed pipe to the interior of an ethanol distillation tower, wherein the reflux ratio inside the ethanol distillation tower is 5.90-5.95 and the pressure is 0.15-0.20 MPa;
[0010] S3, the finished ethanol after purification and adsorption in the ethanol distillation tower is extracted from the discharge pipe at the top of the outer side of the ethanol distillation tower, wherein the extraction amount is 55000-58000 kg / h, and the distillate feed ratio is 0.5100-0.5200;
[0011] S4, the recombinant composition after purification and adsorption in the ethanol distillation tower is collected at the inner bottom of the ethanol distillation tower and discharged from the bottom discharge pipe;
[0012] The adsorbent is prepared by mixing mixed powder, purified water, template, reinforcing particles and seed crystals in a ratio of 10g:100mL:3g:3g:0.5g to prepare composite particles, and then granulating the composite particles. The mixed powder is composed of modified fly ash, composite diatomaceous earth and sodium hydroxide in a weight ratio of 3:2:4.
[0013] Furthermore, in step S1, the number of plates of the ethanol distillation tower is 100, the height of the adsorption bed is 7-10m, the porosity is 0.4-0.5, and the bulk density is 580-720kg / m 3 ;
[0014] In step S2, the feed pipe is located above the 56th tray from bottom to top;
[0015] In step S3, the position of the discharge pipe is above the 92nd tower plate from bottom to top.
[0016] Furthermore, the adsorbent is obtained by processing the following steps:
[0017] A1. Add modified fly ash, composite diatomaceous earth and sodium hydroxide into a ball mill and mix them for 20-30 minutes to obtain a mixed powder;
[0018] A2, adding the mixed powder and purified water into a reactor and stirring, adding the template, reinforcing particles and seed crystals into the reactor, stirring for 30-50 minutes, adjusting the system pH to 11 at room temperature, standing and aging for 6-8 hours, raising the temperature of the reactor to reflux the system, heat preservation treatment for 20-22 hours, and post-processing to obtain composite particles;
[0019] A3, the composite particles and purified water are mixed and added into a disc granulator for granulation to obtain an adsorbent body with a particle size of 5-8 mm;
[0020] A4. Transfer the adsorbent body to a muffle furnace, increase the temperature of the muffle furnace to 400-500°C, and calcine for 4-6 hours to obtain the adsorbent.
[0021] Furthermore, in step A2, the post-treatment includes: after the reaction is completed, the temperature of the reactor is lowered to room temperature, the filter is filtered, the filter cake is washed with purified water until it is neutral and then dried, the filter cake is transferred to a drying oven at a temperature of 70-80°C, and dried to constant weight to obtain composite particles; in step A3, the weight ratio of the composite particles to purified water is 10:1.2-1.5.
[0022] Furthermore, the preparation method of the enhanced particles is: zinc acetate, 5,5'-methylenebis(1H-benzotriazole) and a mixed solution are added to a reactor, ultrasonically dispersed for 20-30 minutes, the reactor temperature is increased to 120-130°C, stirred for 20-24 hours, and post-treated to obtain enhanced particles.
[0023] The synthetic reaction principle of enhanced particles is:
[0024] Under high temperature, the center Zn on zinc acetate 2+ The nitrogen atom of the triazole ring on 5,5'-methylenebis(1H-benzotriazole) and the carboxylate ion react to form a complex. In the complex, the metal Zn 2+ As the central atom, it has a six-coordinated geometric configuration. The Zn 2+ The nitrogen from three other triazoles is coordinated to form a hexacoordinated configuration with three triazoles and one acetate ion coordinated therewith, thereby preparing enhanced particles.
[0025] Furthermore, the mixed solution is composed of glacial acetic acid and N,N-dimethylformamide in a volume ratio of 1:20, and the amount ratio of zinc acetate, 5,5'-methylenebis(1H-benzotriazole) and the mixed solution is 3g:1g:50mL. The post-treatment includes: after the reaction is completed, the temperature of the reactor is lowered to room temperature, filtered, the filter cake is washed with N,N-dimethylformamide, washed 3 times with anhydrous ethanol and then dried, and the filter cake is transferred to a drying oven at a temperature of 70-80°C, and dried to constant weight to obtain reinforced particles.
[0026] Furthermore, the composite diatomite is obtained by processing the following steps:
[0027] C1. Add diatomite and activation solution into a reactor, raise the temperature of the reactor to 60-80°C, and perform ultrasonic dispersion for 6-8h to obtain a diatomite mixed solution;
[0028] C2, squeeze and compress the polyurethane foam block and add it to the diatomaceous earth mixture to make it completely immersed, release it naturally, so that the diatomaceous earth mixture enters the polyurethane foam block, take it out of the diatomaceous earth mixture, repeat the above operation 3-5 times, transfer the polyurethane foam block to a freeze dryer at a temperature of -20°C, freeze-dry to constant weight, and obtain a loaded foam block;
[0029] C3, placing the loaded foam block into a tubular furnace, raising the temperature of the tubular furnace to 850-930°C, and heat preservation for 2-3 hours, and post-processing to obtain modified diatomaceous earth;
[0030] C4, adding modified diatomite and strengthening liquid into the reactor and stirring, raising the temperature of the reactor to the reflux of the system, keeping the temperature to react for 60-65h, and post-treating to obtain the composite diatomite precursor;
[0031] C5. Put the composite diatomite precursor into a tubular furnace, raise the temperature of the tubular furnace to 600-700°C, keep the temperature for 3-5 hours, cool it naturally to room temperature, discharge it, and obtain the composite diatomite.
[0032] The synthetic reaction principle of composite diatomite is:
[0033] Hexadecyltrimethylammonium chloride is used as an active agent to promote the uniform dispersion of sodium silicate, sodium chloride and diatomaceous earth in an aqueous solution. Sodium silicate is used as an alkali source to react with part of the amorphous silicon dioxide in the diatomaceous earth to form nano-silicon on the surface of the diatomaceous earth, thereby increasing the porosity and surface area of the diatomaceous earth. Sodium chloride is used as an electrolyte to promote the ion exchange reaction of the solution at an appropriate temperature. By using polyurethane foam as a template and diatomaceous earth powder as a load, the polyurethane template is burned out during the high-temperature sintering process to form a diatom shell. The invention discloses a method for preparing a modified diatomite by using tetrapropylammonium hydroxide as a catalyst and ethyl orthosilicate as a silicon source, wherein the silicon source undergoes hydrolysis and polycondensation reaction under alkaline conditions, and a composite diatomite precursor of modified diatomite coated with silicon dioxide is generated on the modified diatomite; under the action of high-temperature sintering, the organic matter in the composite diatomite precursor is further pyrolyzed and carbonized, and the silicon dioxide precursor undergoes polycondensation reaction to form a stable silicon dioxide network structure, and the composite diatomite is prepared.
[0034] Furthermore, in step C1, the ratio of the amount of diatomaceous earth to the activation solution is 1 g: 2 mL, and the activation solution is composed of sodium silicate, sodium chloride, hexadecyltrimethylammonium chloride and purified water in a ratio of 5 g: 3 g: 2 g: 180 mL; in step C2, the ratio of the amount of the polyurethane foam block to the diatomaceous earth mixed solution is 1 cm 3:7mL; in step C3, the post-treatment includes: after the reaction is completed, the tubular furnace is naturally cooled to room temperature, the foam block is taken out from the tubular furnace, crushed, and passed through a 60-mesh sieve to obtain modified diatomite; in step C4, the modified diatomite and the enhancement liquid are used in a ratio of 1g:10mL, and the enhancement liquid is composed of tetrapropylammonium hydroxide, ethyl orthosilicate and purified water in a ratio of 1g:4g:5mL, and the post-treatment includes: after the reaction is completed, the temperature of the reactor is lowered to room temperature, purified water is added to the reactor, stirred for 20-30min, filtered, the filter cake is washed 3 times with purified water and then dried, and the filter cake is transferred to a drying oven at a temperature of 70-80°C, and dried to constant weight to obtain a composite diatomite precursor.
[0035] Furthermore, the preparation method of the modified fly ash is: adding fly ash and nitric acid solution into a reactor, ultrasonically dispersing for 50-60 minutes at room temperature, and post-treating to obtain the modified fly ash.
[0036] The synthetic reaction principle of modified fly ash is:
[0037] Using nitric acid as acid liquid, the fly ash and the acid liquid are ultrasonically mixed to promote the dissolution of iron and impurity metals in the fly ash, thereby forming porous modified fly ash with a high silicon dioxide content.
[0038] Furthermore, the usage ratio of the fly ash and the nitric acid solution is 1g:7mL, the nitric acid solution is composed of 2-3mol / L nitric acid and 20wt% hydrogen peroxide in a volume ratio of 10:1, and the post-treatment includes: after the reaction is completed, filtering, washing the filter cake with purified water until it is neutral and then drying, transferring the filter cake to a drying oven at a temperature of 70-80°C, and drying to constant weight to obtain modified fly ash.
[0039] Furthermore, the preparation method of the seed crystal is: adding purified water to the reactor and stirring, raising the temperature of the reactor to reflux the system, adding sodium aluminate, sodium silicate, reinforcing particles and sodium hydroxide to the reactor, keeping warm for 30-50 minutes, lowering the temperature of the reactor to room temperature, aging for 6-8 hours, and post-treating to obtain the seed crystal.
[0040] The synthesis reaction principle of the seed crystal is:
[0041] Under alkaline conditions, sodium aluminate and sodium silicate dissociate into aluminum ions and silicate ions, respectively. The reinforcing particles act as nucleation centers and participate in the growth of crystals. Aluminum ions and silicate ions undergo polymerization in the solution to form aluminosilicate precursors. As the reaction proceeds and the temperature decreases, the precursors gradually precipitate and grow on the reinforcing particles to obtain seed particles with a specific structure.
[0042] Furthermore, the ratio of purified water, sodium aluminate, sodium silicate, reinforcing particles and sodium hydroxide is 100mL:3g:15g:1g:0.5g, and the post-treatment includes: after the reaction is completed, filtering, washing the filter cake with purified water until it is neutral and then drying, transferring the filter cake to a drying oven at a temperature of 70-80°C, drying to constant weight, and obtaining seed crystals.
[0043] The present invention has the following beneficial effects:
[0044] 1. The crude alcohol purification and recovery process based on coal-based fuel ethanol of the present invention comprises the following steps: in the purification process of the crude ethanol of coal-based fuel, zinc acetate is complexed with 5,5'-methylenebis(1H-benzotriazole) to prepare reinforced particles in which zinc ions are coordinated and complexed with three triazoles and one acetate ion, and the particles are compounded with composite diatomaceous earth and modified fly ash to prepare an adsorbent, and then the adsorbent is filled into a distillation tower, and the gas phase composition of methanol, ethanol, n-propanol and acetic acid in the whole tower is analyzed, and the filling mode of the adsorbent in the distillation tower and the feed and discharge positions of the distillation tower are optimized, and then the feed position sensitivity and reflux ratio sensitivity of the ethanol distillation tower are analyzed, and the distillation parameters such as the reflux ratio, distillation pressure, and feed and discharge flow rates of the distillation tower are explored, so that not only the methanol, n-propanol and water content in the crude ethanol can be effectively reduced, but also the acid content and aldehyde content in the crude ethanol can be reduced, so as to prepare high-purity finished ethanol.
[0045] 2. The crude alcohol purification and recovery process based on coal-based fuel ethanol of the present invention comprises the following steps: activating diatomite with an activation liquid, loading it on a polyurethane foam block, preparing a three-dimensional network skeleton co-built with diatomite by a polyurethane template method, and then enhancing and modifying it with an enhancement liquid to form a silicon dioxide coating on the modified diatomite to prepare a composite diatomite precursor, and then sintering it at a high temperature to form a stable silicon dioxide network structure on the modified diatomite to prepare a composite diatomite; the diatomite is treated with an alkali of sodium silicate and treated at a high temperature with polyurethane foam as a template, so that the composite diatomite forms a three-dimensional network skeleton composed of diatom shells, which not only effectively increases the porosity and surface area of the diatomite, but also provides more adsorption channels. The composite diatomite has a plurality of channels and active sites. During the distillation process, this structure is conducive to the effective separation of ethanol molecules and impurity molecules, so that the composite diatomite can effectively adsorb and capture trace impurities in the distillation process, improve the adsorption efficiency and the quality of the finished ethanol, and the composite diatomite treated with the enhancement liquid has a further increase in its porosity and surface area, thereby further improving the adsorption performance of the composite diatomite on the impurity molecules in the crude ethanol and improving the purity of the finished ethanol; the composite diatomite is treated with high-temperature sintering, and the organic matter in it is fully pyrolyzed and carbonized, and the silicon dioxide network structure is more stable. This chemical stability enables the composite diatomite to maintain its adsorption performance during the distillation process and will not fail due to high temperature or solvent. Therefore, the composite diatomite can work stably in the distillation environment for a long time, providing reliable guarantee for the preparation of finished ethanol.
[0046] 3. The crude alcohol purification and recovery process based on coal-based fuel ethanol of the present invention comprises the following steps: modifying fly ash, reducing the content of impurity metals such as iron in fly ash, increasing the silicon content and porosity of modified fly ash, and then compounding the fly ash with reinforcing particles and composite diatomaceous earth to prepare an adsorbent; when preparing the composite particles, adding crystal seeds thereto can induce crystal precipitation, and promote the newly generated crystals to grow along the structure of the crystal seeds, thereby maintaining a morphology similar to that of the crystal seeds, making the crystals induced by the crystal seeds more orderly and uniform, and the crystals of the prepared composite particles more complete and regular, which is helpful to improve the purity and quality of the microparticle product and reduce the generation of impurities and defects; the triazole ring in the reinforcing particles is an electron-rich system, and the lone pair electrons on the nitrogen atom can react with Zn 2+The ions form stable coordination bonds. At the same time, the triazole ring itself and its substituents (such as methyl) may provide additional π electron clouds, which can serve as active sites for adsorbing impurities. In addition, due to the presence of various functional groups and active sites on the surface of the enhanced particles, impurities can be adsorbed through different mechanisms. For example, electrostatic attraction can capture ions with opposite charges; π-π interactions can adsorb aromatic compounds; hydrogen bonds can capture molecules containing hydroxyl groups, carboxyl groups, etc. This diverse adsorption mechanism enables the enhanced particles to selectively adsorb a variety of impurities in ethanol, thereby improving the overall performance of the adsorbent; the adsorbent uses enhanced particles to improve the structural strength and selective adsorption capacity of the adsorbent, and modified fly ash to increase the specific surface area, porosity and active sites of the adsorbent. Based on the high porosity, large specific surface area and three-dimensional network structure of the composite diatomaceous earth, when the enhanced particles, modified fly ash and composite diatomaceous earth act on the adsorbent together, the three will synergistically combine to provide excellent adsorption performance for the entire adsorption system. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0048] Figure 1 It is a schematic diagram of the overall structure of the ethanol distillation tower in the present invention;
[0049] Figure 2 This is a gas phase composition diagram of methanol, ethanol, n-propanol and acetic acid in the whole tower in the present invention;
[0050] Figure 3 Sensitivity analysis of the feed position of the ethanol distillation tower in the present invention Figure 1 ;
[0051] Figure 4 Sensitivity analysis of the feed position of the ethanol distillation tower in the present invention Figure 2 ;
[0052] Figure 5 Sensitivity analysis of feed reflux ratio of ethanol distillation tower in the present invention Figure 1 ;
[0053] Figure 6 Sensitivity analysis of feed reflux ratio of ethanol distillation tower in the present invention Figure 2 .
[0054] In the figure: 100, ethanol distillation tower; 200, feed pipe; 300, discharge pipe; 400, discharge pipe. DETAILED DESCRIPTION
[0055] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0056] Example 1
[0057] This embodiment provides a method for preparing an adsorbent for a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0058] S1. Preparation of enhanced particles
[0059] Mix glacial acetic acid and N,N-dimethylformamide in a volume ratio of 1:20 to obtain a mixed solution;
[0060] Weigh: 30 g of zinc acetate, 10 g of 5,5'-methylenebis(1H-benzotriazole) and 500 mL of the mixed solution, add them into a reactor, ultrasonically disperse for 20 min, raise the temperature of the reactor to 120°C, and keep stirring for 20 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with N,N-dimethylformamide, wash it three times with anhydrous ethanol and then dry it, transfer the filter cake to a drying oven at 70°C, and dry it to constant weight to obtain reinforced particles.
[0061] S2. Preparation of modified diatomite
[0062] Sodium silicate, sodium chloride, hexadecyltrimethylammonium chloride and purified water were mixed uniformly in a dosage ratio of 5g:3g:2g:180mL to obtain an activation solution;
[0063] Weigh: 100 g of diatomaceous earth and 200 mL of activation solution, add them into a reactor, raise the temperature of the reactor to 60°C, and perform ultrasonic dispersion for 6 hours to obtain a diatomaceous earth mixed solution;
[0064] The polyurethane foam block was squeezed and compressed and added to the diatomaceous earth mixture to make it completely immersed and released naturally so that the diatomaceous earth mixture entered the polyurethane foam block and was taken out from the diatomaceous earth mixture. The above operation was repeated 3 times and the polyurethane foam block was transferred to a freeze dryer at a temperature of -20°C and freeze-dried to constant weight to obtain a loaded foam block. The usage ratio of the polyurethane foam block to the diatomaceous earth mixture was 1 cm 3 :7mL;
[0065] The loaded foam block was placed in a tubular furnace, the temperature of the tubular furnace was raised to 850°C, and the temperature was kept for 2 hours. After the reaction was completed, the tubular furnace was naturally cooled to room temperature. The foam block was taken out of the tubular furnace, crushed, and passed through a 60-mesh sieve to obtain modified diatomaceous earth.
[0066] S3. Preparation of composite diatomite
[0067] Tetrapropylammonium hydroxide, ethyl orthosilicate and purified water were mixed uniformly in a dosage ratio of 1 g:4 g:5 mL to obtain an enhanced solution;
[0068] Weigh: 100 g of modified diatomite and 1000 mL of enhancement solution are added to the reactor and stirred. The temperature of the reactor is raised to the reflux of the system and the reaction is kept warm for 60 hours. After the reaction is completed, the temperature of the reactor is lowered to room temperature, 500 mL of purified water is added to the reactor, stirred for 20 minutes, and filtered. The filter cake is washed with purified water 3 times and then dried. The filter cake is transferred to a drying oven at a temperature of 70° C. and dried to constant weight to obtain a composite diatomite precursor;
[0069] The composite diatomite precursor was placed in a tubular furnace, the temperature of the tubular furnace was raised to 600° C., and the furnace was kept warm for 3 hours, and then naturally cooled to room temperature and discharged to obtain the composite diatomite.
[0070] S4. Preparation of modified fly ash
[0071] 2 mol / L nitric acid and 20 wt % hydrogen peroxide were mixed in a volume ratio of 10:1 to obtain a nitric acid solution;
[0072] Weigh: 100 g of fly ash and 700 mL of nitric acid solution, add them into a reactor, and ultrasonically disperse them at room temperature for 50 minutes. After the reaction is completed, filter and wash the filter cake with purified water until it is neutral and then dry it. Transfer the filter cake to a drying oven at 70°C and dry it to constant weight to obtain modified fly ash.
[0073] S5. Preparation of seed crystals
[0074] Weigh: 500 mL of purified water was added to the reactor and stirred. The temperature of the reactor was raised to reflux, 15 g of sodium aluminate, 75 g of sodium silicate, 5 g of reinforced particles and 2.5 g of sodium hydroxide were added to the reactor. The reaction mixture was kept warm for 30 min. The temperature of the reactor was lowered to room temperature and aged for 6 h. After the reaction was completed, the filter cake was washed with purified water until it was neutral and then dried. The filter cake was transferred to a drying oven at 70°C and dried to constant weight to obtain seed crystals.
[0075] S6. Preparation of composite particles
[0076] Add modified fly ash, composite diatomaceous earth and sodium hydroxide in a weight ratio of 3:2:4 into a ball mill, and mix by ball milling for 20 minutes to obtain a mixed powder;
[0077] Weigh: 10 kg of mixed powder and 100 L of purified water, add into the reactor and stir, add 3 kg of hexadecyltrimethylammonium bromide, 3 kg of enhanced particles and 500 g of seed crystals into the reactor, stir for 30 min, adjust the system pH to 11 at room temperature, let stand and age for 6 h, increase the temperature of the reactor to reflux the system, and keep warm for 20 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with purified water until it is neutral and then dry, transfer the filter cake to a drying oven at 70°C, dry to constant weight, and obtain composite particles.
[0078] S7. Preparation of adsorbent
[0079] The composite particles and purified water were mixed in a weight ratio of 10:1.2 and added into a disc granulator for granulation to obtain an adsorbent body with a particle size of 5-8 mm;
[0080] The adsorbent body was transferred to a muffle furnace, the temperature of the muffle furnace was increased to 400°C, and the body was kept warm and calcined for 4 hours to obtain the adsorbent.
[0081] Example 2
[0082] This embodiment provides a method for preparing an adsorbent for a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0083] S1. Preparation of enhanced particles
[0084] Mix glacial acetic acid and N,N-dimethylformamide in a volume ratio of 1:20 to obtain a mixed solution;
[0085] Weigh: 30 g of zinc acetate, 10 g of 5,5'-methylenebis(1H-benzotriazole) and 500 mL of the mixed solution, add them into a reactor, ultrasonically disperse for 25 min, raise the temperature of the reactor to 125°C, and keep stirring for 22 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with N,N-dimethylformamide, wash it three times with anhydrous ethanol and then dry it, transfer the filter cake to a drying oven at a temperature of 75°C, and dry it to constant weight to obtain reinforced particles.
[0086] S2. Preparation of modified diatomite
[0087] Sodium silicate, sodium chloride, hexadecyltrimethylammonium chloride and purified water were mixed uniformly in a dosage ratio of 5g:3g:2g:180mL to obtain an activation solution;
[0088] Weigh: 100 g of diatomaceous earth and 200 mL of activation solution, add them into a reactor, raise the temperature of the reactor to 70°C, and perform ultrasonic dispersion for 7 hours to obtain a diatomaceous earth mixed solution;
[0089] The polyurethane foam block was squeezed and compressed and added to the diatomaceous earth mixture to completely immerse it. The diatomaceous earth mixture was released naturally to allow the diatomaceous earth mixture to enter the polyurethane foam block, and the block was taken out of the diatomaceous earth mixture. The above operation was repeated 4 times, and the polyurethane foam block was transferred to a freeze dryer at a temperature of -20°C and freeze-dried to constant weight to obtain a loaded foam block, wherein the amount ratio of the polyurethane foam block to the diatomaceous earth mixture was 1 cm 3 :7mL;
[0090] The loaded foam block was placed in a tubular furnace, the temperature of the tubular furnace was raised to 890°C, and the temperature was kept for 2.5 hours. After the reaction was completed, the tubular furnace was naturally cooled to room temperature. The foam block was taken out of the tubular furnace, crushed, and passed through a 60-mesh sieve to obtain modified diatomaceous earth.
[0091] S3. Preparation of composite diatomite
[0092] Tetrapropylammonium hydroxide, ethyl orthosilicate and purified water were mixed uniformly in a dosage ratio of 1 g:4 g:5 mL to obtain an enhanced solution;
[0093] Weigh: 100 g of modified diatomite and 1000 mL of enhancement solution are added to the reactor and stirred. The temperature of the reactor is raised to the reflux of the system and the reaction is kept warm for 63 hours. After the reaction is completed, the temperature of the reactor is lowered to room temperature, 500 mL of purified water is added to the reactor, stirred for 25 minutes, and filtered. The filter cake is washed with purified water 3 times and then dried. The filter cake is transferred to a drying oven at a temperature of 75° C. and dried to constant weight to obtain a composite diatomite precursor;
[0094] The composite diatomite precursor was placed in a tubular furnace, the temperature of the tubular furnace was raised to 650° C., and the furnace was kept warm for 4 hours, and then naturally cooled to room temperature and discharged to obtain the composite diatomite.
[0095] S4. Preparation of modified fly ash
[0096] 2.5 mol / L nitric acid and 20 wt % hydrogen peroxide were mixed in a volume ratio of 10:1 to obtain a nitric acid solution;
[0097] Weigh: 100 g of fly ash and 700 mL of nitric acid solution, add them into the reactor, and ultrasonically disperse them at room temperature for 55 minutes. After the reaction is completed, filter and wash the filter cake with purified water until it is neutral and then dry it. Transfer the filter cake to a drying oven at a temperature of 75°C and dry it to constant weight to obtain modified fly ash.
[0098] S5. Preparation of seed crystals
[0099] Weigh: 500 mL of purified water was added to the reactor and stirred. The temperature of the reactor was raised to reflux, 15 g of sodium aluminate, 75 g of sodium silicate, 5 g of reinforced particles and 2.5 g of sodium hydroxide were added to the reactor. The reaction mixture was kept warm for 40 min. The temperature of the reactor was lowered to room temperature and aged for 7 h. After the reaction was completed, the filter cake was washed with purified water until it was neutral and then dried. The filter cake was transferred to a drying oven at 75°C and dried to constant weight to obtain seed crystals.
[0100] S6. Preparation of composite particles
[0101] Add modified fly ash, composite diatomaceous earth and sodium hydroxide in a weight ratio of 3:2:4 into a ball mill, and mix by ball milling for 25 minutes to obtain a mixed powder;
[0102] Weigh: 10 kg of mixed powder and 100 L of purified water, add into the reactor and stir, add 3 kg of hexadecyltrimethylammonium bromide, 3 kg of enhanced particles and 500 g of seed crystals into the reactor, stir for 40 min, adjust the system pH to 11 at room temperature, let stand and age for 7 h, increase the temperature of the reactor to reflux the system, and keep warm for 21 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with purified water until it is neutral and then dry, transfer the filter cake to a drying oven at 75°C, and dry to constant weight to obtain composite particles.
[0103] S7. Preparation of adsorbent
[0104] The composite particles and purified water were mixed in a weight ratio of 10:1.3 and added into a disc granulator for granulation to obtain an adsorbent body with a particle size of 5-8 mm;
[0105] The adsorbent body was transferred to a muffle furnace, the temperature of the muffle furnace was increased to 450°C, and the body was kept at this temperature for 5 hours to obtain the adsorbent.
[0106] Example 3
[0107] This embodiment provides a method for preparing an adsorbent for a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0108] S1. Preparation of enhanced particles
[0109] Mix glacial acetic acid and N,N-dimethylformamide in a volume ratio of 1:20 to obtain a mixed solution;
[0110] Weigh: 30 g of zinc acetate, 10 g of 5,5'-methylenebis(1H-benzotriazole) and 500 mL of the mixed solution, add them into a reactor, ultrasonically disperse for 30 min, raise the temperature of the reactor to 130°C, and keep stirring for 24 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with N,N-dimethylformamide, wash it three times with anhydrous ethanol and then dry it, transfer the filter cake to a drying oven at 80°C, and dry it to constant weight to obtain reinforced particles.
[0111] S2. Preparation of modified diatomite
[0112] Sodium silicate, sodium chloride, hexadecyltrimethylammonium chloride and purified water were mixed uniformly in a dosage ratio of 5g:3g:2g:180mL to obtain an activation solution;
[0113] Weigh: 100 g of diatomaceous earth and 200 mL of activation solution, add them into a reactor, raise the temperature of the reactor to 80°C, and perform ultrasonic dispersion for 8 hours to obtain a diatomaceous earth mixed solution;
[0114] The polyurethane foam block was squeezed and compressed and added to the diatomaceous earth mixture to make it completely immersed and released naturally so that the diatomaceous earth mixture entered the polyurethane foam block and was taken out from the diatomaceous earth mixture. The above operation was repeated 5 times and the polyurethane foam block was transferred to a freeze dryer at a temperature of -20°C and freeze-dried to constant weight to obtain a loaded foam block. The usage ratio of the polyurethane foam block to the diatomaceous earth mixture was 1 cm 3 :7mL;
[0115] The loaded foam block was placed in a tubular furnace, the temperature of the tubular furnace was raised to 930°C, and the temperature was kept for 3 hours. After the reaction was completed, the tubular furnace was naturally cooled to room temperature. The foam block was taken out of the tubular furnace, crushed, and passed through a 60-mesh sieve to obtain modified diatomaceous earth.
[0116] S3. Preparation of composite diatomite
[0117] Tetrapropylammonium hydroxide, ethyl orthosilicate and purified water were mixed uniformly in a dosage ratio of 1 g:4 g:5 mL to obtain an enhanced solution;
[0118] Weigh: 100 g of modified diatomite and 1000 mL of enhancement solution are added to the reactor and stirred. The temperature of the reactor is raised to the reflux of the system and the reaction is kept warm for 65 hours. After the reaction is completed, the temperature of the reactor is lowered to room temperature, 500 mL of purified water is added to the reactor, stirred for 30 minutes, and filtered. The filter cake is washed with purified water 3 times and then dried. The filter cake is transferred to a drying oven at a temperature of 80° C. and dried to constant weight to obtain a composite diatomite precursor;
[0119] The composite diatomite precursor was placed in a tubular furnace, the temperature of the tubular furnace was raised to 700° C., and the furnace was kept warm for 5 hours, and then naturally cooled to room temperature and discharged to obtain the composite diatomite.
[0120] S4. Preparation of modified fly ash
[0121] 3 mol / L nitric acid and 20 wt % hydrogen peroxide were mixed in a volume ratio of 10:1 to obtain a nitric acid solution;
[0122] Weigh: 100 g of fly ash and 700 mL of nitric acid solution, add them into a reactor, and ultrasonically disperse them at room temperature for 60 minutes. After the reaction is completed, filter and wash the filter cake with purified water until it is neutral and then dry it. Transfer the filter cake to a drying oven at 80°C and dry it to constant weight to obtain modified fly ash.
[0123] S5. Preparation of seed crystals
[0124] Weigh: 500 mL of purified water was added to the reactor and stirred. The temperature of the reactor was raised to reflux, 15 g of sodium aluminate, 75 g of sodium silicate, 5 g of reinforced particles and 2.5 g of sodium hydroxide were added to the reactor. The reaction mixture was kept warm for 50 min. The temperature of the reactor was lowered to room temperature and aged for 8 h. After the reaction was completed, the filter cake was washed with purified water until it was neutral and then dried. The filter cake was transferred to a drying oven at 80°C and dried to constant weight to obtain seed crystals.
[0125] S6. Preparation of composite particles
[0126] Add modified fly ash, composite diatomaceous earth and sodium hydroxide in a weight ratio of 3:2:4 into a ball mill, and mix by ball milling for 30 minutes to obtain a mixed powder;
[0127] Weigh: 10 kg of mixed powder and 100 L of purified water, add into the reactor and stir, add 3 kg of hexadecyltrimethylammonium bromide, 3 kg of enhanced particles and 500 g of seed crystals into the reactor, stir for 50 min, adjust the system pH to 11 at room temperature, let stand and age for 8 h, increase the temperature of the reactor to reflux the system, and keep warm for 22 h. After the reaction is completed, lower the temperature of the reactor to room temperature, filter, wash the filter cake with purified water until it is neutral and then dry, transfer the filter cake to a drying oven at 80°C, and dry to constant weight to obtain composite particles.
[0128] S7. Preparation of adsorbent
[0129] The composite particles and purified water were mixed in a weight ratio of 10:1.5 and added into a disc granulator for granulation to obtain an adsorbent body with a particle size of 5-8 mm;
[0130] The adsorbent body was transferred to a muffle furnace, the temperature of the muffle furnace was increased to 500°C, and the body was kept warm and calcined for 6 hours to obtain the adsorbent.
[0131] Example 4
[0132] See also Figure 1-6 This embodiment provides a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0133] Step 1: Select a distillation tower with 100 plates as the ethanol distillation tower 100, and fill the adsorbent prepared in Example 1 on the top of each plate of the ethanol distillation tower 100 to form an adsorption bed. The height of the adsorption bed is 7 m, the porosity is 0.4, and the bulk density is 580 kg / m 3 .
[0134] Step 2: A feed pipe 200 is set outside the ethanol distillation tower 100, one end of the feed pipe 200 extends into the interior of the ethanol distillation tower 100 and is located above the 56th tower plate from bottom to top, and the crude ethanol is transported from the feed pipe 200 to the interior of the ethanol distillation tower 100, and the reflux ratio inside the ethanol distillation tower 100 is set to 5.90 and the pressure is set to 0.15 MPa.
[0135] Step 3: A discharge pipe 300 is set at the outer top of the ethanol distillation tower 100, one end of the discharge pipe 300 extends to the interior of the ethanol distillation tower 100 and is located above the 92nd tower plate from bottom to top. The finished ethanol after purification and adsorption by the ethanol distillation tower 100 is produced from the discharge pipe 300 at the outer top of the ethanol distillation tower 100, wherein the production volume is 55000 kg / h and the distillate feed ratio is 0.5100.
[0136] Step 4: The recombined components after purification and adsorption in the ethanol distillation tower 100 are collected at the inner bottom of the ethanol distillation tower 100 and discharged from the bottom discharge pipe 400.
[0137] Example 5
[0138] See also Figure 1-6 This embodiment provides a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0139] Step 1: Select a distillation tower with 100 plates as the ethanol distillation tower 100, and fill the adsorbent prepared in Example 2 on the top of each plate of the ethanol distillation tower 100 to form an adsorption bed. The height of the adsorption bed is 8.5 m, the porosity is 0.45, and the bulk density is 650 kg / m 3 .
[0140] Step 2: A feed pipe 200 is set outside the ethanol distillation tower 100, one end of the feed pipe 200 extends into the interior of the ethanol distillation tower 100 and is located above the 56th tower plate from bottom to top, and the crude ethanol is transported from the feed pipe 200 to the interior of the ethanol distillation tower 100, and the reflux ratio inside the ethanol distillation tower 100 is set to 5.93 and the pressure is set to 0.17 MPa.
[0141] Step three, a discharge pipe 300 is set at the outer top of the ethanol distillation tower 100, one end of the discharge pipe 300 extends to the interior of the ethanol distillation tower 100 and is located above the 92nd tower plate from bottom to top, and the finished ethanol after purification and adsorption by the ethanol distillation tower 100 is produced from the discharge pipe 300 at the outer top of the ethanol distillation tower 100, wherein the production volume is 56500 kg / h, and the distillate feed ratio is 0.5150.
[0142] Step 4: The recombined components after purification and adsorption in the ethanol distillation tower 100 are collected at the inner bottom of the ethanol distillation tower 100 and discharged from the bottom discharge pipe 400.
[0143] Example 6
[0144] See also Figure 1-6 This embodiment provides a crude alcohol purification and recovery process based on coal-based fuel ethanol, comprising the following steps:
[0145] Step 1: Select a distillation tower with 100 plates as the ethanol distillation tower 100, and fill the adsorbent prepared in Example 3 on the top of each plate of the ethanol distillation tower 100 to form an adsorption bed. The height of the adsorption bed is 10 m, the porosity is 0.5, and the bulk density is 720 kg / m 3 .
[0146] Step 2: A feed pipe 200 is set outside the ethanol distillation tower 100, one end of the feed pipe 200 extends into the interior of the ethanol distillation tower 100 and is located above the 56th tower plate from bottom to top, and the crude ethanol is transported from the feed pipe 200 to the interior of the ethanol distillation tower 100, and the reflux ratio inside the ethanol distillation tower 100 is set to 5.95 and the pressure is set to 0.20 MPa.
[0147] Step 3: A discharge pipe 300 is set at the outer top of the ethanol distillation tower 100, one end of the discharge pipe 300 extends to the interior of the ethanol distillation tower 100 and is located above the 92nd tower plate from bottom to top. The finished ethanol after purification and adsorption by the ethanol distillation tower 100 is produced from the discharge pipe 300 at the outer top of the ethanol distillation tower 100, wherein the production volume is 58000 kg / h, and the distillate feed ratio is 0.5200.
[0148] Step 4: The recombined components after purification and adsorption in the ethanol distillation tower 100 are collected at the inner bottom of the ethanol distillation tower 100 and discharged from the bottom discharge pipe 400.
[0149] Comparative Example 1
[0150] The difference between this comparative example and Example 6 is that, during the preparation of the adsorbent prepared in Example 3 used in step 1, step S1 is omitted, and no reinforcing particles are used in steps S5 and S6.
[0151] Comparative Example 2
[0152] The difference between this comparative example and Example 6 is that, during the preparation of the adsorbent prepared in Example 3 used in step 1, step S2 is omitted, and the modified diatomaceous earth in step S3 is replaced by the diatomaceous earth in step S2.
[0153] Comparative Example 3
[0154] The difference between this comparative example and Example 6 is that, during the preparation of the adsorbent prepared in Example 3 used in step 1, step S3 is omitted, and the composite diatomaceous earth in step S6 is replaced by the modified diatomaceous earth in step S2.
[0155] Comparative Example 4
[0156] The difference between this comparative example and Example 6 is that, during the preparation of the adsorbent prepared in Example 3 used in step 1, step S4 is omitted, and the fly ash in step S4 replaces the modified fly ash in step S6.
[0157] Example 5
[0158] The difference between this comparative example and Example 6 is that, during the preparation of the adsorbent prepared in Example 3 used in step 1, step S5 is omitted, and no seed crystal is added in step S6.
[0159] Performance Test:
[0160] With reference to the standard GB / T 6820-2016 "Industrial Ethanol", the content, moisture, acid content, aldehyde content, methanol content and n-propanol content of the finished ethanol prepared in Examples 4-6 and Comparative Examples 1-5 were tested. The specific test results are shown in Table 1.
[0161] Table 1-Performance test results of samples
[0162]
[0163] Data Analysis:
[0164] A comparative analysis of the data in Table 1 above shows that the ethanol content of the finished ethanol prepared by the present invention reaches 99.86%, the moisture content is reduced to 0.10%, the acid content in the finished ethanol is reduced to 7.2 mg / L, the aldehyde content is reduced to 6.5 mg / L, the methanol content is reduced to 12.8 mg / L, and the n-propanol content is reduced to 111.9 mg / L. The values of various performance test values are all better than those of the comparative example. The present invention prepares the adsorbent by compounding the reinforced particles with composite diatomaceous earth and modified fly ash, optimizes the filling method of the adsorbent in the distillation tower, the feed and discharge positions of the distillation tower, the reflux ratio of the distillation tower, the distillation pressure, the feed and discharge flow rates and other distillation parameters, which can not only effectively reduce the methanol, n-propanol and moisture contents in the crude ethanol, but also reduce the acid content and aldehyde content in the crude ethanol, so as to prepare high-purity finished ethanol.
[0165] The above contents are merely examples and explanations of the structure of the present invention. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the structure of the invention or exceed the scope defined by the claims, they should all fall within the protection scope of the present invention.
[0166] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0167] 4. The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. Crude alcohol purification and recovery process based on coal-based fuel ethanol, It is characterized in that The following steps are involved: S1, placing an adsorbent on the top of each tray of the ethanol distillation tower (100) to form an adsorption bed; S2, transporting the crude ethanol from the feed pipe (200) to the interior of the ethanol distillation tower (100), wherein the reflux ratio inside the ethanol distillation tower (100) is 5.90-5.95 and the pressure is 0.15-0.20 MPa; S3, the finished ethanol after purification and adsorption in the ethanol distillation tower (100) is taken out from the discharge pipe (300) at the top of the outer side of the ethanol distillation tower (100), wherein the output is 55000-58000 kg / h and the distillate feed ratio is 0.5100-0.5200; S4, the recombinant product after purification and adsorption in the ethanol distillation tower (100) is collected at the inner bottom of the ethanol distillation tower (100) and discharged from the bottom discharge pipe (400); The adsorbent is prepared by mixing mixed powder, purified water, hexadecyltrimethylammonium bromide, reinforcing particles and seed crystals in a ratio of 10g:100mL:3g:3g:0.5g to prepare composite particles, and then granulating the composite particles. The mixed powder is composed of modified fly ash, composite diatomaceous earth and sodium hydroxide in a weight ratio of 3:2:
4. The adsorbent is obtained by processing the following steps: A1. Add modified fly ash, composite diatomaceous earth and sodium hydroxide into a ball mill and mix them for 20-30 minutes to obtain a mixed powder; A2, adding the mixed powder and purified water into a reactor and stirring, adding hexadecyltrimethylammonium bromide, enhanced particles and seed crystals into the reactor, stirring for 30-50 minutes, adjusting the system pH to 11 at room temperature, standing and aging for 6-8 hours, raising the temperature of the reactor to reflux the system, heat preservation treatment for 20-22 hours, and post-treating to obtain composite particles; A3, mixing the composite particles and purified water and adding them into a disc granulator for granulation to obtain an adsorbent body with a particle size of 5-8 mm, wherein the weight ratio of the composite particles to the purified water is 10:1.2-1.5; A4. The adsorbent body is transferred to a muffle furnace, the temperature of the muffle furnace is increased to 400-500°C, and the body is kept warm and calcined for 4-6 hours to obtain the adsorbent; The preparation method of the reinforced particles is as follows: zinc acetate, 5,5'-methylenebis(1H-benzotriazole) and a mixed solution are added to a reactor, ultrasonically dispersed for 20-30 minutes, the temperature of the reactor is increased to 120-130° C., the mixture is kept warm and stirred for 20-24 hours, and post-processed to obtain the reinforced particles, wherein the mixed solution is composed of glacial acetic acid and N,N-dimethylformamide in a volume ratio of 1:20, and the amount ratio of zinc acetate, 5,5'-methylenebis(1H-benzotriazole) and the mixed solution is 3g:1g:50mL; The composite diatomite is obtained by processing the following steps: C1. Add diatomaceous earth and activation solution into a reactor, raise the temperature of the reactor to 60-80°C, and perform ultrasonic dispersion for 6-8h to obtain a diatomaceous earth mixed solution, wherein the amount ratio of the diatomaceous earth to the activation solution is 1g:2mL, and the activation solution is composed of sodium silicate, sodium chloride, hexadecyltrimethylammonium chloride and purified water in an amount ratio of 5g:3g:2g:180mL; C2, squeeze and compress the polyurethane foam block and add it to the diatomaceous earth mixture to make it completely immersed, release it naturally, so that the diatomaceous earth mixture enters the polyurethane foam block, take it out of the diatomaceous earth mixture, repeat the above operation 3-5 times, transfer the polyurethane foam block to a freeze dryer at a temperature of -20°C, freeze-dry to constant weight, and obtain a loaded foam block, wherein the amount ratio of the polyurethane foam block to the diatomaceous earth mixture is 1cm 3 :7mL; C3, placing the loaded foam block into a tubular furnace, raising the temperature of the tubular furnace to 850-930°C, and heat preservation for 2-3 hours, and post-processing to obtain modified diatomaceous earth; C4, adding modified diatomite and enhancing liquid into a reactor and stirring, raising the temperature of the reactor to reflux the system, keeping the temperature for reaction for 60-65h, and post-treating to obtain a composite diatomite precursor, wherein the modified diatomite and enhancing liquid are used in a ratio of 1g:10mL, and the enhancing liquid is composed of tetrapropylammonium hydroxide, ethyl orthosilicate and purified water in a ratio of 1g:4g:5mL; C5, placing the composite diatomite precursor into a tubular furnace, raising the temperature of the tubular furnace to 600-700°C, keeping the temperature for 3-5 hours, cooling naturally to room temperature, discharging the material, and obtaining the composite diatomite; The preparation method of the modified fly ash is as follows: adding fly ash and nitric acid solution into a reactor, ultrasonically dispersing for 50-60 minutes at room temperature, and post-treating to obtain the modified fly ash, wherein the fly ash and nitric acid solution are used in an amount ratio of 1 g:7 mL, and the nitric acid solution is composed of 2-3 mol / L nitric acid and 20 wt% hydrogen peroxide in a volume ratio of 10:1; The preparation method of the seed crystal is as follows: adding purified water to a reactor and stirring, raising the temperature of the reactor to system reflux, adding sodium aluminate, sodium silicate, reinforcing particles and sodium hydroxide to the reactor, heat preservation treatment for 30-50 minutes, lowering the temperature of the reactor to room temperature, aging for 6-8 hours, and post-treating to obtain the seed crystal, wherein the amount ratio of purified water, sodium aluminate, sodium silicate, reinforcing particles and sodium hydroxide is 100mL:3g:15g:1g:0.5g.
2. The crude alcohol purification and recovery process based on coal-based fuel ethanol according to claim 1, It is characterized in that In step S1, the number of plates of the ethanol distillation tower (100) is 100, the height of the adsorption bed is 7-10 m, the porosity is 0.4-0.5, and the bulk density is 580-720 kg / m 3 ; In step S2, the feed pipe (200) is located above the 56th tray from bottom to top; In step S3, the position of the discharge pipe (300) is above the 92nd tower plate from bottom to top.