Glass substrate coating etching method and system
By configuring a temperature sensor and using a particle filter algorithm in the vacuum magnetron sputtering method, the temperature vector is adjusted to control the substrate temperature, which solves the problem of inaccurate temperature measurement in vacuum scenarios and improves the control reliability of glass substrate coating.
Patent Information
- Application Number
- CN202411066780.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-08-06
AI Technical Summary
In the vacuum magnetron sputtering method, the surface temperature of the substrate to be coated cannot be directly measured, resulting in a difference between the measured temperature and the actual temperature. The substrate temperature cannot be accurately controlled, which reduces the control reliability of glass substrate coating.
By configuring the first temperature sensor at a preset distance from the substrate to be coated and the second temperature sensor at the ionization point of process gas atoms, combined with the particle filter algorithm, the bias environment data and coating environment data are obtained, and the temperature noise vector, plasma The body heat conduction vector and the heating temperature vector are used to adjust the initial temperature of the temperature particles and generate control electrical signals to regulate the substrate surface temperature.
It achieves more accurate measurement and control of the surface temperature of the substrate to be coated, improves the control reliability of glass substrate coating, and solves the problem of inaccurate coating control caused by the difference between temperature measurement and actual temperature.
Smart Images

Figure CN118579996B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of control of a coating process, and in particular to a glass substrate coating etching method and system. Background Art
[0002] Vacuum magnetron sputtering is a widely used method for coating glass substrates. During the coating process, the substrate to be coated (glass substrate) is placed above the vacuum sputtering chamber facing the coating material, and process gas atoms (argon atoms) are injected into the vacuum chamber and ionized into argon ions using an external voltage. A magnetic field is then set on the surface of the coating material to capture the argon ions, so that the argon ions hit and ionize the coating material, and the coating material is sputtered into the vacuum until it is sputtered onto the substrate to be coated for deposition, deposited into a thin film to complete the coating, and after the coating is completed, the etching process is used to further etch the substrate. In the specific coating process, the temperature of the substrate to be coated needs to be measured in real time to achieve high-precision coating control.
[0003] It is understandable that in the related art, the substrate to be coated is in a vacuum scene, and it is impossible to directly contact the substrate to be coated to achieve accurate temperature acquisition. Instead, a temperature sensor is configured around the substrate to be coated to obtain the monitoring temperature. In this way, due to the vacuum scene and a certain distance, the surface temperature of the substrate to be coated is directly measured, resulting in a difference between the measured temperature and the surface temperature, and the temperature of the substrate to be coated cannot be accurately controlled, which makes the reliability of the glass substrate coating control poor. Summary of the invention
[0004] In order to solve the technical problem that the surface temperature of the substrate to be coated is directly measured in the related art, resulting in a difference between the measured temperature and the surface temperature, and the temperature of the substrate to be coated cannot be accurately controlled, resulting in poor reliability of glass substrate coating control, the present invention provides a glass substrate coating etching method and system, and the technical solutions adopted are as follows:
[0005] The present invention provides a glass substrate coating etching method, wherein the coating etching includes an ionization bias process, a coating process and an etching process, wherein a first temperature sensor is arranged at a preset distance from a substrate to be coated, and a second temperature sensor is arranged at an ionization position of process gas atoms, and the method includes:
[0006] Periodically acquiring bias environment data during the ionization bias process and coating environment data during the coating process, wherein the bias environment data includes bias voltage, ionization power, and plasma temperature acquired by the second temperature sensor; the coating environment data includes the monitoring temperature acquired by the first temperature sensor and the heating temperature for heating the substrate to be coated;
[0007] Determine temperature particles based on a particle filter algorithm, wherein the substrate initial temperature of the temperature particle is the temperature value corresponding to when the heating temperature is consistent with the monitoring temperature; determine a heating temperature vector according to the substrate initial temperature and the heating temperature at the current moment; determine the plasma added intensity of the process gas atoms after ionization bias according to the substrate initial temperature, the plasma temperature and the ionization power; determine a plasma heat conduction vector in combination with the bias voltage, the substrate initial temperature and the plasma added intensity; determine a temperature noise vector according to the plasma added intensity combined with the monitoring temperature;
[0008] Combining the temperature noise vector, the plasma heat conduction vector and the heating temperature vector, adjusting the initial temperature of the substrate of particles with different temperatures to obtain an adjusted temperature, and combining the adjusted temperatures of all temperature particles to determine the real-time temperature of the substrate;
[0009] A control electrical signal is generated based on the real-time temperature of the substrate, and the surface temperature of the substrate is regulated based on the control electrical signal to complete the coating; and the coated glass substrate is etched using an etching process.
[0010] Furthermore, the method for obtaining the heating temperature vector includes:
[0011] The difference between the initial temperature of the substrate and the heating temperature at the current moment is used as the heating temperature vector.
[0012] Furthermore, the method for obtaining the additional intensity of the plasma after the process gas atoms are ionized and biased comprises:
[0013] The product of the ionization power and the collection period is taken as the periodic power consumption;
[0014] Based on the average translational kinetic energy formula and the ideal gas state equation, combined with the periodic power consumption, the number of microscopic particles is determined as the added intensity of plasma.
[0015] Furthermore, based on the average translational kinetic energy formula and the ideal gas state equation, combined with the periodic power consumption, the number of microscopic particles is determined as the plasma's added intensity, and the corresponding calculation formula is:
[0016] ; In the formula, Indicates the added intensity of plasma, represents the preset pressure value for the ionization bias process, Represents the preset scene volume during ionization bias, represents the Boltzmann constant, Indicates the cycle power consumption, represents the molar gas constant.
[0017] Furthermore, the method for obtaining the plasma heat conduction vector comprises:
[0018] The first distance is obtained by obtaining the Euclidean distance between two electrodes generating the bias voltage during the ionization bias process; the second distance is obtained by obtaining the Euclidean distance between the incident port of the process gas atoms and the position of the coating material during the coating process; the third distance is obtained by obtaining the Euclidean distance between the coating material and the substrate to be coated;
[0019] The sum of the second distance and the third distance is used as the motion trajectory length of the plasma formed after the process gas atoms are ionized; the ratio of the bias voltage to the first distance is used as the bias electric field strength;
[0020] Determining the material ion bombardment energy of the coating material in combination with the motion trajectory length and the bias electric field strength, wherein the motion trajectory length and the bias electric field strength are both positively correlated with the material ion bombardment energy;
[0021] Determine the material ion bombardment temperature according to the average translational kinetic energy formula, combined with the material ion bombardment energy and the plasma added intensity;
[0022] Taking the difference between the plasma temperature and the initial temperature of the substrate as the plasma change temperature difference;
[0023] The plasma temperature difference and the material ion bombardment temperature are forwardly fused to determine the plasma heat conduction vector.
[0024] Furthermore, the method for obtaining the temperature noise vector includes:
[0025] Taking a preset number of moments before the current moment as the impact moment, and calculating the mean and standard deviation of the monitored temperatures at all the impact moments;
[0026] Performing maximum and minimum normalization processing on the newly added plasma intensity to obtain an ionization energy noise factor;
[0027] Determining an ionization energy influence mean according to the mean of the monitored temperatures and the ionization energy noise factor, wherein both the mean of the monitored temperatures and the ionization energy noise factor are positively correlated with the ionization energy influence mean;
[0028] Substituting the ionization energy influence mean and the standard deviation of the monitored temperature into a Gaussian function to obtain an error probability distribution function;
[0029] A temperature noise vector for each temperature particle is randomly generated based on the error probability distribution function.
[0030] Further, the combining temperature noise vector, the plasma heat conduction vector and the heating temperature vector to adjust the initial temperature of the substrate of particles with different temperatures to obtain the adjusted temperature includes:
[0031] Determine the sum of the temperature noise vector, the plasma heat conduction vector and the heating temperature vector of each temperature particle as an adjustment vector;
[0032] The sum of the substrate initial temperature and the adjustment vector is used as the adjustment temperature of the corresponding temperature particle.
[0033] Further, the step of determining the real-time temperature of the substrate by combining the adjusted temperatures of all temperature particles comprises:
[0034] The average of the adjusted temperatures of all temperature particles is used as the real-time temperature of the substrate to be coated.
[0035] Furthermore, the step of generating a control electrical signal based on the real-time temperature of the substrate, and regulating the surface temperature of the substrate based on the control electrical signal to complete the coating process includes:
[0036] Based on the PID control method, the real-time temperature of the substrate is used as data input and a control electrical signal is output, wherein the control electrical signal is used to perform vacuum magnetron sputtering coating on the glass substrate.
[0037] On the other hand, a glass substrate coating and etching system is also provided, the system comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, the processor implementing the steps of a glass substrate coating and etching method as described in any one of the foregoing items when executing the computer program.
[0038] The present invention has the following beneficial effects:
[0039] The embodiment of the present invention acquires bias environment data and coating environment data and combines a particle filter algorithm to achieve data analysis in three dimensions: temperature noise vector, plasma heat conduction vector, and heating temperature vector. The heating temperature vector characterizes the influence of the heating device on the temperature of the substrate to be coated; the plasma heat conduction vector characterizes the influence of the temperature rise of the substrate to be coated caused by the plasma; and the temperature noise vector represents the surface charge imbalance of the substrate to be coated caused by the plasma, resulting in the absorption of free electrons on the surface of the substrate to be coated, and the electrons hit the substrate to be coated and offset the heat energy generated by the positive charge; then, each temperature particle is adjusted based on the vector data of the three dimensions to determine the adjustment temperature of the temperature particle, that is, the temperature information affecting the temperature of the substrate to be coated is integrated, and the surface temperature of the substrate to be coated is corrected. Compared with directly using the monitored temperature as the surface temperature of the substrate to be coated, a more accurate real-time temperature of the substrate at the current moment can be obtained, which solves the problem that in the process of controlling the coating of the substrate to be coated by the vacuum magnetron sputtering method, the surface temperature of the substrate to be coated cannot be directly measured, resulting in a difference between the measured temperature and the surface temperature, and the surface temperature of the substrate to be coated cannot be accurately obtained, thereby improving the reliability of the coating control of the glass substrate. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present invention or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0041] Figure 1 A flow chart of a glass substrate coating and etching method provided by one embodiment of the present invention;
[0042] Figure 2 A structural diagram of a sputtering chamber provided in accordance with an embodiment of the present invention;
[0043] Figure 3 A schematic flow chart of a method for obtaining additional plasma intensity provided by an embodiment of the present invention;
[0044] Figure 4 A distance analysis structure diagram provided by an embodiment of the present invention;
[0045] Figure 5 A flowchart of a method for obtaining a temperature noise vector provided by an embodiment of the present invention;
[0046] Figure 6 A schematic diagram of temperature particle distribution visualization provided by an embodiment of the present invention;
[0047] Figure 7 A schematic diagram of real-time temperature visualization of a substrate provided by an embodiment of the present invention;
[0048] Figure 8 A structural diagram of a glass substrate coating and etching system provided by one embodiment of the present invention;
[0049] The serial numbers in the figure represent: 1. sputtering chamber shell, 2. injected argon atomic flow, 3. argon atomic flow injection equipment, 4. bias electrode plate, 5. second temperature sensor, 6. substrate to be coated, 7. permanent magnet, 8. coating material, 9. magnetic field area. DETAILED DESCRIPTION
[0050] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the following is a detailed description of a glass substrate coating etching method proposed by the present invention, its specific implementation, structure, features and effects, in conjunction with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.
[0051] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0052] A specific scheme of a glass substrate coating and etching method provided by the present invention is described in detail below with reference to the accompanying drawings.
[0053] See also Figure 1 , which shows a flow chart of a glass substrate coating and etching method provided by an embodiment of the present invention, the method comprising:
[0054] S101: Periodically acquiring bias environment data in an ionization bias process and coating environment data in a coating process, wherein the bias environment data includes bias voltage, ionization power and plasma temperature acquired by a second temperature sensor; and the coating environment data includes a monitoring temperature acquired by a first temperature sensor and a heating temperature for heating a substrate to be coated.
[0055] Combination Figure 2 The coating scenario corresponding to the embodiment of the present invention is specifically analyzed. Figure 2 A structural diagram of a sputtering chamber provided for one embodiment of the present invention.
[0056] In the embodiment of the present invention, argon atoms are used as process gas atoms, that is, Figure 2It can be seen that argon atoms are injected into the sputtering chamber from the argon atom flow injection device 3, and then ionized by the bias electrode plate 4 to obtain argon ion plasma, which is accelerated by the bias electrode plate 4 and the permanent magnet 7, and then a magnetic field area 9 is set on the surface of the coating material 8 to capture the argon ions, so that the argon ions hit and ionize the coating material 8, and the coating material 8 is sputtered into the vacuum until it is sputtered onto the substrate 6 (glass substrate) to be coated for deposition, and deposited into a thin film to complete the coating.
[0057] In a specific implementation of the embodiment of the present invention, when a glass substrate is coated by a magnetron sputtering coating method, quartz glass is used as the substrate to be coated, argon gas with a purity of 99.99% is used as the process gas, an aluminum target material is selected as the coating material, and the vacuum pressure is set to Pascal, argon flow rate is set to 80 sccm or 80 standard cubic centimeters per minute.
[0058] Of course, in other embodiments of the present invention, the process gas atoms may also be oxygen atoms, nitrogen atoms, hydrogen atoms, etc., which are analyzed according to actual scenarios and are not limited to this.
[0059] It should be noted that during the coating process, the surface temperature of the glass substrate needs to be kept stable to ensure the coating efficiency. Therefore, it is necessary to measure the surface temperature of the substrate to be coated in real time through a non-contact temperature measurement device and implement temperature control based on the real-time temperature.
[0060] Among them, since the sputtering chamber is a closed environment, although the interior can be observed through the observation window, this embodiment uses a first temperature sensor configured at a preset distance from the substrate to be coated to measure the temperature of the surface of the substrate to be coated to obtain a monitoring temperature.
[0061] During the temperature measurement process, since the first temperature sensor cannot directly contact the surface of the substrate to be coated, there is a difference between the monitored temperature measured by the first temperature sensor and the actual surface temperature of the substrate to be coated. It is necessary to accurately analyze the surface of the substrate to be coated based on the monitored temperature, so as to achieve effective substrate surface temperature control.
[0062] The preset distance is the distance between the first temperature sensor and the substrate to be coated. The preset distance in the embodiment of the present invention may be specifically, for example, a distance of 5 cm, and there is no limitation to this.
[0063] Among them, considering that the temperature control range of the designed sputtering chamber is within 770 Kelvin, a K-type thermocouple with a measuring range of -125 to +1650 Kelvin is used as the first temperature sensor and the second temperature sensor to collect the temperature inside the sputtering chamber cavity.
[0064] It is understandable that, in order to facilitate the analysis of the overall solution, the embodiment of the present invention divides the total coating and etching process of the entire sputtering chamber into an ionization bias process, a coating process, and an etching process, and the ionization bias process corresponds to bias environment data, and the coating process corresponds to coating environment data. In the embodiment of the present invention, the data collection period can be specifically, for example, 0.1 seconds, that is, the bias environment data and the coating environment data are obtained every 0.1 seconds, and there is no limitation on this.
[0065] Among them, the bias environment data includes the bias voltage, the ionization power and the plasma temperature obtained by the second temperature sensor; the coating environment data includes the monitoring temperature obtained by the first temperature sensor and the heating temperature for heating the substrate to be coated.
[0066] Among them, considering that the plasma in the sputtering chamber will increase the temperature of the substrate to be coated, the bias voltage applied to the sputtering chamber at the current moment is recorded, which can be directly obtained through the control terminal of the sputtering chamber. The specific acquisition method is a technology well known in the art and is not limited to this.
[0067] In order to obtain the energy condition of argon atoms ionized in the sputtering chamber, the electric power of the bias electrode plate 4 for ionizing the argon atomic flow between the argon atomic flow injection device 3 and the magnetic field region 9 of the coating material 8 is obtained, which is recorded as the ionization power.
[0068] Among them, in the existing scenario, in order to ensure that the substrate to be coated itself has a certain initial substrate temperature, a heating device will be arranged near the substrate to be coated. The temperature of the heating device will make the temperature of the substrate to be coated converge with the temperature of the heating device through heat conduction. Therefore, the temperature of the heating device at the current moment is monitored in real time and recorded as the heating temperature.
[0069] The present invention aims to combine the temperature influence of process gas atoms in the sputtering chamber and the temperature influence of the heating device, etc., to achieve accurate analysis of the temperature of the substrate to be coated itself, and then achieve overall coating control. The specific analysis process is shown in the subsequent embodiments.
[0070] S102: Determine the temperature particle based on the particle filter algorithm, wherein the substrate initial temperature of the temperature particle is the temperature value corresponding to the heating temperature being consistent with the monitoring temperature; determine the heating temperature vector according to the substrate initial temperature and the heating temperature at the current moment; determine the plasma added intensity of the process gas atoms after ionization bias according to the substrate initial temperature, plasma temperature and ionization power; determine the plasma heat conduction vector by combining the bias voltage, substrate initial temperature and plasma added intensity; determine the temperature noise vector according to the plasma added intensity combined with the monitoring temperature.
[0071] In the embodiment of the present invention, a specific temperature change analysis can be performed from three dimensions, namely, the heating temperature vector, the plasma heat conduction vector and the temperature noise vector. Among them, the heating temperature vector represents the influence of the heating device on the temperature of the substrate to be coated, the plasma heat conduction vector represents the influence of the temperature rise of the substrate to be coated caused by the plasma, and the temperature noise vector represents the charge imbalance on the surface of the substrate to be coated caused by the plasma, resulting in the absorption of free electrons on the surface of the substrate to be coated, and the electrons hit the substrate to be coated and offset the positive charge to generate heat energy.
[0072] It should be noted that the substrate to be coated will be heated to a certain temperature before coating begins. Since coating has not started yet, the temperature rise of the substrate to be coated due to plasma striking is not considered at this time. At this time, the substrate to be coated is in a vacuum environment with very little heat loss. At this time, the substrate to be coated will be at the same temperature as the heating device, and the heating temperature at this time is recorded as the initial temperature of the substrate.
[0073] Analyze the heating temperature vector: Since the heating temperature vector represents the influence of the heating device on the temperature of the substrate to be coated, and since the temperature of the substrate to be coated is the same as that of the heating device, the temperature value is the initial temperature of the substrate. Therefore, the difference between the current heating temperature and the initial temperature of the substrate is used as the influence value of the heating device on the temperature of the substrate to be coated, that is, the heating temperature vector.
[0074] It should be noted that the heating temperature vector has positive and negative characteristics, and its positive and negative characteristics indicate whether the heating device has an effect of increasing or decreasing the temperature of the substrate to be coated at this time, and the larger the absolute value of the heating temperature vector, the more severe the impact on the substrate to be coated.
[0075] Analysis of plasma heat conduction vector: Since the temperature of the plasma is affected by the applied bias voltage, the plasma heat conduction vector can be analyzed in combination with the increased plasma intensity of the ionization bias. Therefore, the increased plasma intensity is first specifically analyzed.
[0076] Further, in some embodiments of the present invention, in combination Figure 3 , which is a flow chart of a method for obtaining additional plasma intensity provided by an embodiment of the present invention.
[0077] S301: The product of the ionization power and the collection period is taken as the periodic power consumption.
[0078] Among them, the collection period can be specifically 0.1 second, for example. Since the process gas atoms will be heated during the ionization process, and the larger the bias voltage, the stronger the heating effect, that is, the higher the power, the stronger the heating effect. Therefore, the heating effect analysis is performed based on the ionization power and the collection period.
[0079] In the embodiment of the present invention, the product of the ionization power and the collection period is calculated and can be used as the power consumption in the period, that is, the periodic power consumption.
[0080] S302: Based on the average translational kinetic energy formula and the ideal gas state equation, combined with the periodic power consumption, the number of microscopic particles is determined as the increased intensity of the plasma.
[0081] In the embodiment of the present invention, the formula for average translational kinetic energy is: , where E is energy, k is the Boltzmann constant, and T is temperature; the ideal gas state equation is , where P is the preset pressure value of the ionization bias process, V is the volume of the preset scene in the ionization bias process, n is the number of microscopic particles, R is the molar gas constant, and T is the temperature.
[0082] In the embodiment of the present invention, the change in the number of microscopic particles is used as the additional plasma intensity, and the temperature T represents the increased temperature of the plasma after the bias voltage is applied.
[0083] Further, in some embodiments of the present invention, the calculation formula corresponding to the number of microscopic particles and the increased plasma intensity is:
[0084] ; In the formula, Indicates the added intensity of plasma, represents the preset pressure value for the ionization bias process, Represents the preset scene volume during ionization bias, represents the Boltzmann constant, Indicates the cycle power consumption, represents the molar gas constant.
[0085] Among them, the preset pressure value and the preset scene volume are data obtained in the scene, which will not be described in detail, and the Boltzmann constant and the molar gas constant are constant values well known to those skilled in the art, which will not be described in detail.
[0086] By combining the mean translational kinetic energy formula and the ideal gas state equation, changes at the microscopic particle level can be achieved, and the increased number of microscopic particles can be used as the increased plasma intensity.
[0087] It should be noted that part of the ionization power of the process gas atoms is to heat the process gas atoms during the ionization process, and part is to ionize the process gas atoms. Therefore, the plasma added intensity can only characterize the relative size of the number of plasmas. The greater the plasma added intensity, the more plasma of process gas atoms is generated at the current moment, and the corresponding material plasma sputtered from the coating material is also more, which will lead to an increase in the substrate surface temperature.
[0088] Thus, a method for obtaining a plasma heat conduction vector in combination with the newly added plasma intensity includes: obtaining the Euclidean distance between two electrodes generating a bias voltage during an ionization bias process as a first distance; obtaining the Euclidean distance between an incident port of process gas atoms and a position of a coating material during a coating process as a second distance; obtaining the Euclidean distance between the coating material and a substrate to be coated as a third distance; taking the sum of the second distance and the third distance as the motion trajectory length of a plasma formed after the process gas atoms are ionized; taking the ratio of the bias voltage to the first distance as the bias electric field intensity; determining the material ion bombardment energy of the coating material in combination with the motion trajectory length and the bias electric field intensity, wherein both the motion trajectory length and the bias electric field intensity are positively correlated with the material ion bombardment energy; determining the material ion bombardment temperature in combination with the material ion bombardment energy and the newly added plasma intensity according to the average translational kinetic energy formula; taking the difference between the plasma temperature and the initial temperature of the substrate as the plasma change temperature difference; and forwardly fusing the plasma change temperature difference and the material ion bombardment temperature to determine the plasma heat conduction vector.
[0089] It can be understood that since most of the ions of the process gas atoms generated are captured by the magnetic field to sputter the plasma of the coating material, the plasma of the sputtered process gas atoms can be regarded as the plasma consumed in real time to sputter the coating material. Therefore, the greater the additional intensity of the plasma, the more plasma of the coating material is sputtered onto the substrate to be coated at the current moment, and the stronger the heat conduction of the plasma in the sputtering chamber to the substrate to be coated.
[0090] Among them, the actual combination of the first distance, the second distance and the third distance Figure 4 Conduct a specific analysis. Figure 4 A distance analysis structure diagram provided for an embodiment of the present invention. That is, the sum of the second distance and the third distance is taken as the approximate motion trajectory of the plasma formed by the process gas atoms after ionization, and the length thereof is taken as the motion trajectory length. The ratio of the bias voltage to the first distance is taken as the bias electric field strength, and thus, the material ion bombardment energy of the coating material is determined by combining the motion trajectory length and the bias electric field strength.
[0091] Among them, the material ion bombardment energy is specifically characterized by the energy generated by the continuous acceleration of the plasma in the bias electric field. Therefore, the motion trajectory length and the bias electric field strength are positively correlated with the material ion bombardment energy.
[0092] Among them, a positive correlation relationship indicates that the dependent variable will increase as the independent variable increases, and the dependent variable will decrease as the independent variable decreases. The specific relationship can be a multiplication relationship, an addition relationship, or the power of an exponential function, which is determined by actual applications; a negative correlation relationship indicates that the dependent variable will decrease as the independent variable increases, and the dependent variable will increase as the independent variable decreases. It can be a subtraction relationship, a division relationship, etc., which is determined by actual applications. In some embodiments of the present invention, the product of the motion trajectory length and the bias electric field strength can be calculated to obtain the material ion bombardment energy.
[0093] In one embodiment of the present invention, the normalization processing can be specifically, for example, maximum and minimum value normalization processing, and the normalization in subsequent steps can all adopt maximum and minimum value normalization processing. In other embodiments of the present invention, other normalization methods can be selected according to the specific range of numerical values, which will not be described in detail.
[0094] It can be understood that according to the average translational kinetic energy formula, the material ion bombardment temperature is equal to the material bombardment energy multiplied by the plasma added intensity divided by the Boltzmann constant divided by two-thirds. The average translational kinetic energy formula is a well-known empirical formula in the field of thermodynamics. Therefore, the material ion bombardment temperature can be determined directly by combining the material ion bombardment energy and the plasma added intensity.
[0095] Since the difference between the temperature of the plasma and the initial temperature of the substrate will also cause the energy change of the plasma itself, the difference between the temperature of the plasma and the initial temperature of the substrate is taken as the temperature difference of the plasma change.
[0096] In the embodiment of the present invention, the plasma heat conduction vector can be determined by combining the plasma temperature difference and the material ion bombardment temperature, and the relationship is a forward fusion relationship, that is, the sum of the plasma temperature difference and the material ion bombardment temperature can be calculated as the plasma heat conduction vector.
[0097] Analysis of the temperature noise vector: The temperature noise vector indicates that the plasma causes an imbalance in the charge on the surface of the substrate to be coated, which causes the surface of the substrate to be coated to absorb free electrons. The electrons hit the substrate to be coated and offset the positive charge to generate heat energy. Figure 5 , Figure 5 A flowchart of a method for obtaining a temperature noise vector provided by an embodiment of the present invention;
[0098] S501: taking a preset number of moments before the current moment as the impact moment, and calculating the mean and standard deviation of the monitored temperatures at all the impact moments.
[0099] The preset number is the number of impact moments before the preset current moment. Optionally, the preset number may be specifically 50, for example, that is, the number of impact moments is set to 50. Of course, it can also be adjusted according to actual needs.
[0100] It should be noted that the plasma causes an imbalance in the charge on the surface of the substrate to be coated, resulting in the absorption of free electrons on the surface of the substrate to be coated. The electrons hit the substrate to be coated and offset the positive charge to generate heat energy. Part of the charge on the surface of the substrate to be coated is offset by attracting electrons, and part is transferred away through the fixing clamp of the substrate to be coated. The ability of the charge on the surface of the substrate to be coated to attract electrons is related to the electron distribution in the sputtering chamber. However, the electron distribution in the plasma is affected by many factors, such as whether the shutters are opened, the trajectory of the plasma flow in space, etc. Therefore, this part of the temperature is difficult to calculate and is analyzed and processed as noise affecting the temperature measurement.
[0101] In the embodiment of the present invention, a temperature noise vector is finally constructed. The vector consists of two parts. The first part is to determine a Gaussian function by monitoring the temperature fluctuation, and the second part is the heat energy generated by the surface charge offset of the substrate to be coated.
[0102] Therefore, by analyzing the mean and standard deviation of the monitored temperature at all influencing moments and combining the newly added plasma intensity, the construction of the Gaussian function is achieved. For details, please refer to the subsequent embodiments.
[0103] S502: performing maximum and minimum normalization processing on the newly added plasma intensity to obtain an ionization energy noise factor.
[0104] Among them, the maximum and minimum value normalization is a technology well known to those skilled in the art. Of course, various other linear normalization methods can also be used in the embodiment of the present invention to facilitate the specific analysis of the added plasma intensity.
[0105] S503: Determine the ionization energy influence mean value according to the mean value of the monitored temperature and the ionization energy noise factor, wherein the mean value of the monitored temperature and the ionization energy noise factor are both positively correlated with the ionization energy influence mean value.
[0106] Among them, the product of the mean of the monitored temperature and the ionization energy noise factor can be calculated as the mean of the ionization energy influence, which characterizes the influence of the new plasma intensity and temperature change on the ionization energy at all influencing moments. At the same time, the mean of the ionization energy influence can also be used as the mean feature of the subsequent Gaussian function.
[0107] S504: Substitute the ionization energy influence mean and the standard deviation of the monitoring temperature into a Gaussian function to obtain an error probability distribution function.
[0108] The Gaussian function can be specifically a one-dimensional Gaussian function, that is, the error probability distribution analysis of the Gaussian distribution is performed by combining the ionization energy to affect the mean and standard deviation. The one-dimensional Gaussian function obtains the error probability distribution function. The horizontal axis of the function is the temperature noise vector, and the vertical axis is the probability. A value on the function is recorded as , indicating that the temperature noise vector is The probability is The one-dimensional Gaussian function is a commonly used mathematical model in the field of engineering data processing, and its specific implementation will not be described in detail.
[0109] S505: Randomly generate a temperature noise vector for each temperature particle based on the error probability distribution function.
[0110] After the error probability distribution function is calculated, the Gaussian distribution analysis of the temperature noise vector is realized, and the temperature noise vector of each temperature particle is randomly determined according to the Gaussian distribution probability under the corresponding value.
[0111] That is, the temperature noise vector of each temperature particle is randomly obtained from the error probability distribution function, and the random probability conforms to the numerical distribution of the error probability distribution function.
[0112] The embodiment of the present invention determines the temperature noise vector based on Gaussian distribution, which can effectively combine the charge distribution characteristics of temperature particles to construct a more objective and effective temperature noise vector situation, thereby realizing the electron distribution analysis in the overall plasma and ensuring the reliability of the temperature noise vector.
[0113] S103: Combining the temperature noise vector, the plasma heat conduction vector and the heating temperature vector, adjusting the initial temperature of the substrate of particles with different temperatures to obtain the adjusted temperature, and combining the adjusted temperatures of all temperature particles to determine the real-time temperature of the substrate.
[0114] In the embodiment of the present invention, the temperature noise vector, the plasma heat conduction vector and the heating temperature vector are all influence values corresponding to the temperature particles. The adjustment of the temperature particles can be specifically analyzed in combination with these three characteristics.
[0115] Furthermore, in some embodiments of the present invention, the sum of the temperature noise vector, plasma heat conduction vector and heating temperature vector of each temperature particle can be calculated as the corresponding temperature particle adjustment vector, and the sum of the substrate initial temperature and the adjustment vector can be used as the adjustment temperature of the corresponding temperature particle.
[0116] That is to say, in the embodiment of the present invention, the sum of the temperature noise vector, the plasma heat conduction vector and the heating temperature vector of each temperature particle can be directly calculated to obtain the adjustment vector of each temperature particle. It can be understood that this vector can be used for the temperature particles of the moving particle filter algorithm. Since the temperature particle is a one-dimensional particle, it only has a temperature characteristic. Therefore, the sum of the initial temperature of the substrate and the adjustment vector can be directly calculated as the adjustment temperature of the corresponding temperature particle.
[0117] Optionally, in some embodiments of the present invention, the average of the adjusted temperatures of all temperature particles may be used as the real-time temperature of the substrate to be coated.
[0118] It should be noted that since the temperature noise vector is a vector based on Gaussian distribution, that is, the adjustment temperature of each temperature particle also conforms to Gaussian distribution. Figure 6~Figure 7 As shown, Figure 6 A schematic diagram of temperature particle distribution visualization provided by an embodiment of the present invention. Figure 7 A schematic diagram of the real-time temperature visualization of a substrate provided by an embodiment of the present invention, wherein 465°C is the initial temperature of the substrate, and the other points in the figure are the adjusted temperatures of the temperature particles, and by averaging all the adjusted temperatures, the adjusted real-time temperature of the substrate is 470°C.
[0119] Of course, in other embodiments of the present invention, each temperature particle may also be assigned a weight, and the weight assignment may be specifically analyzed based on actual characteristics, which will not be described in detail in the embodiments of the present invention.
[0120] In the embodiment of the present invention, the real-time temperature of the substrate is the temperature value obtained by analyzing multiple different temperature influencing characteristics during the entire coating process, thereby adjusting the initial temperature of the substrate. It should be noted that since the analysis is performed at different moments, the initial temperature of the substrate at the next moment is the real-time temperature of the substrate at the current moment, thereby realizing continuous iterative updating of the real-time temperature of the substrate and obtaining the accurate temperature value of the substrate to be coated at each moment.
[0121] S104: Generate a control electrical signal based on the real-time temperature of the substrate, and adjust the surface temperature of the substrate based on the control electrical signal to complete the coating; and etch the coated glass substrate using an etching process.
[0122] The embodiment of the present invention aims to obtain a more accurate and reliable real-time temperature of the substrate. After determining a more accurate real-time temperature of the substrate, the control effect of the glass substrate during the coating process can be achieved according to the real-time temperature of the substrate.
[0123] Furthermore, in some embodiments of the present invention, the real-time temperature of the substrate can be used as data input based on a PID control method to output a control electrical signal, wherein the control electrical signal is used to perform vacuum magnetron sputtering coating on a glass substrate.
[0124] That is to say, the real-time temperature of the substrate is used as the input of the PID control, and then the corresponding control signal is output. It can be understood that the PID control method is a commonly used technology in the field of industrial control, and no further limitation or elaboration is made on this.
[0125] The present invention may also use a variety of other control situations, such as linear control based on the real-time temperature of the substrate, etc., which is not limited.
[0126] Furthermore, the surface temperature of the substrate during the coating process is controlled by an electrical signal to complete the coating. After the coating is completed, the coated substrate can be etched using a wet etching technique in this embodiment. The specific process of the wet etching technique includes:
[0127] Exposure: A specific light is irradiated through a mask to form a light pattern, which is then irradiated onto the substrate to be coated. The chemical properties of a specific area are changed by covering the coating material so that it will not be dissolved by the developer.
[0128] Development: Use a developer to dissolve the resist in the exposed area, revealing the underlying material of the substrate to be coated, in preparation for the next etching step;
[0129] Etching: The substrate to be coated is immersed in the etching solution. The chemical substances in the etching solution react with the material on the surface of the substrate, causing the area not protected by the resist to be etched away to form the desired pattern or structure.
[0130] Stripping: Use specific solvents or chemical methods to remove residual resist, thus completing the entire wet etching process.
[0131] Finally, the coating and etching of the glass substrate were completed.
[0132] The embodiment of the present invention acquires bias environment data and coating environment data and combines a particle filter algorithm to achieve data analysis in three dimensions: temperature noise vector, plasma heat conduction vector, and heating temperature vector. The heating temperature vector represents the influence of the heating device on the temperature of the substrate to be coated; the plasma heat conduction vector represents the influence of the temperature rise of the substrate to be coated caused by the plasma; and the temperature noise vector represents the surface charge imbalance of the substrate to be coated caused by the plasma, resulting in the absorption of free electrons on the surface of the substrate to be coated, and the electrons hit the substrate to be coated and offset the heat energy generated by the positive charge; then, each temperature particle is adjusted based on the vector data of the three dimensions to determine the adjustment temperature of the temperature particle, that is, the temperature information affecting the temperature of the substrate to be coated is integrated, and the surface temperature of the substrate to be coated is corrected. Compared with directly using the monitored temperature as the surface temperature of the substrate to be coated, a more accurate real-time temperature of the substrate at the current moment can be obtained, which solves the problem that in the process of controlling the coating of the substrate to be coated by the vacuum magnetron sputtering method, the surface temperature of the substrate to be coated cannot be directly measured, resulting in a difference between the measured temperature and the surface temperature, and the temperature of the substrate to be coated cannot be accurately controlled, thereby improving the reliability of the coating control of the glass substrate.
[0133] The present invention also provides a glass substrate coating and etching system, see Figure 8 , Figure 8 This is a structural diagram of a glass substrate coating and etching system provided in one embodiment of the present invention. The system 600 includes a memory 601, a processor 602, and a computer program 603 stored in the memory 601 and executable on the processor 602. When the processor 602 executes the computer program 603, the steps of the aforementioned glass substrate coating and etching method are implemented.
[0134] This embodiment also provides a computer-readable storage medium, in which a computer program code is stored. When the computer program code is run on a computer, the computer executes the above-mentioned related method steps to implement a glass substrate coating and etching method provided in the above embodiment.
[0135] This embodiment further provides a computer program product. When the computer program product is run on a computer, the computer is enabled to execute the above-mentioned related steps to implement a glass substrate coating and etching method provided in the above embodiment.
[0136] Among them, the system, computer-readable storage medium or computer program product provided in this embodiment is used to execute the corresponding glass substrate coating and etching method provided above. Therefore, the beneficial effects that can be achieved can refer to the beneficial effects in the corresponding method provided above, and will not be repeated here.
[0137] It should be noted that the sequence of the above embodiments of the present invention is only for description and does not represent the advantages and disadvantages of the embodiments. The processes depicted in the accompanying drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.
[0138] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.
Claims
1. A method for etching a glass substrate coating, characterized in that: The coating etching includes an ionization bias process, a coating process and an etching process. A first temperature sensor is arranged at a preset distance of the substrate to be coated, and a second temperature sensor is arranged at the ionization position of the process gas atoms. The method includes: Periodically acquiring bias environment data during the ionization bias process and coating environment data during the coating process, wherein the bias environment data includes bias voltage, ionization power, and plasma temperature acquired by the second temperature sensor; the coating environment data includes the monitoring temperature acquired by the first temperature sensor and the heating temperature for heating the substrate to be coated; Determine temperature particles based on a particle filter algorithm, wherein the substrate initial temperature of the temperature particle is the temperature value corresponding to when the heating temperature is consistent with the monitoring temperature; determine a heating temperature vector according to the substrate initial temperature and the heating temperature at the current moment; determine the plasma added intensity of the process gas atoms after ionization bias according to the substrate initial temperature, the plasma temperature and the ionization power; determine a plasma heat conduction vector in combination with the bias voltage, the substrate initial temperature and the plasma added intensity; determine a temperature noise vector according to the plasma added intensity combined with the monitoring temperature; Combining the temperature noise vector, the plasma heat conduction vector and the heating temperature vector, adjusting the initial temperature of the substrate of particles with different temperatures to obtain an adjusted temperature, and combining the adjusted temperatures of all temperature particles to determine the real-time temperature of the substrate; Generate a control electrical signal based on the real-time temperature of the substrate, and adjust the surface temperature of the substrate based on the control electrical signal to complete the coating; and etch the coated glass substrate using an etching process; The method for obtaining the heating temperature vector comprises: The difference between the initial temperature of the substrate and the heating temperature at the current moment is used as the heating temperature vector; The method for obtaining the newly added intensity of the plasma after the process gas atoms are ionized and biased comprises: The product of the ionization power and the collection period is taken as the periodic power consumption; Based on the average translational kinetic energy formula and the ideal gas state equation, combined with the periodic power consumption, the number of microscopic particles is determined as the added intensity of plasma; The method for obtaining the plasma heat conduction vector comprises: The first distance is obtained by obtaining the Euclidean distance between two electrodes generating the bias voltage during the ionization bias process; the second distance is obtained by obtaining the Euclidean distance between the incident port of the process gas atoms and the position of the coating material during the coating process; the third distance is obtained by obtaining the Euclidean distance between the coating material and the substrate to be coated; The sum of the second distance and the third distance is used as the motion trajectory length of the plasma formed after the process gas atoms are ionized; the ratio of the bias voltage to the first distance is used as the bias electric field strength; Determining the material ion bombardment energy of the coating material in combination with the motion trajectory length and the bias electric field strength, wherein the motion trajectory length and the bias electric field strength are both positively correlated with the material ion bombardment energy; Determine the material ion bombardment temperature according to the average translational kinetic energy formula, combined with the material ion bombardment energy and the plasma added intensity; Taking the difference between the plasma temperature and the initial temperature of the substrate as the plasma change temperature difference; Performing forward fusion on the plasma temperature difference and the material ion bombardment temperature to determine the plasma heat conduction vector; The method for obtaining the temperature noise vector comprises: Taking a preset number of moments before the current moment as the impact moment, and calculating the mean and standard deviation of the monitored temperatures at all the impact moments; Performing maximum and minimum normalization processing on the newly added plasma intensity to obtain an ionization energy noise factor; Determining an ionization energy influence mean according to the mean of the monitored temperatures and the ionization energy noise factor, wherein both the mean of the monitored temperatures and the ionization energy noise factor are positively correlated with the ionization energy influence mean; Substituting the ionization energy influence mean and the standard deviation of the monitored temperature into a Gaussian function to obtain an error probability distribution function; A temperature noise vector for each temperature particle is randomly generated based on the error probability distribution function.
2. A glass substrate coating etching method as claimed in claim 1, characterized in that: Based on the average translational kinetic energy formula and the ideal gas state equation, combined with the periodic power consumption, the number of microscopic particles is determined as the plasma's added intensity, and the corresponding calculation formula is: ; In the formula, Indicates the added intensity of plasma, Indicates the preset pressure value for the ionization bias process, Represents the preset scene volume during ionization bias, represents the Boltzmann constant, Indicates the cycle power consumption, represents the molar gas constant.
3. A glass substrate coating etching method as claimed in claim 1, characterized in that: The combining temperature noise vector, the plasma heat conduction vector and the heating temperature vector to adjust the initial temperature of the substrate of particles with different temperatures to obtain the adjusted temperature comprises: Determine the sum of the temperature noise vector, the plasma heat conduction vector and the heating temperature vector of each temperature particle as an adjustment vector; The sum of the substrate initial temperature and the adjustment vector is used as the adjustment temperature of the corresponding temperature particle.
4. A glass substrate coating etching method as claimed in claim 1, characterized in that: The method of determining the real-time temperature of the substrate by combining the adjusted temperatures of all temperature particles comprises: The average of the adjusted temperatures of all temperature particles is used as the real-time temperature of the substrate to be coated.
5. A glass substrate coating etching method as claimed in claim 1, characterized in that: The method of generating a control electrical signal based on the real-time temperature of the substrate, and regulating the surface temperature of the substrate based on the control electrical signal to complete the coating includes: Based on the PID control method, the real-time temperature of the substrate is used as data input and a control electrical signal is output, wherein the control electrical signal is used to perform vacuum magnetron sputtering coating on the glass substrate.
6. A glass substrate coating and etching system, the system comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the computer program, the steps of the method according to any one of claims 1 to 5 are implemented.
Citation Information
Patent Citations
Method for predicting components by analytical process to prepare Fe-Ga alloy film
CN103590013A
Fabrication method of inductor with electronic plating method
KR100119274B1