A pressure sensor and a method for manufacturing the same
By forming heavily doped regions and cavity on the substrate surface, combining epitaxial structure and insulating materials, the sticking and high cost problems in capacitive pressure sensor manufacturing are solved, and the effect of simplifying the process and reducing costs is achieved.
Patent Information
- Application Number
- CN202411159728.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-22
AI Technical Summary
In the existing capacitive pressure sensor manufacturing methods, the sacrificial layer process leads to film sticking problems, the bonding process is complex and costly, making it difficult to achieve efficient and low-cost variable capacitance structure manufacturing.
A heavily doped region is formed on one side surface of the substrate, and a plurality of holes are etched in the thickness direction to form a cavity between the columnar convex and the heavily doped region, the cavity is closed with an epitaxial structure, and on the epitaxial structure The etching ring groove is filled with insulating material to form the movable and fixed plates of the pressure sensor to avoid sticking.
The process is simplified and cost is reduced, and the stickiness between the movable plate and the fixed plate is avoided, which improves the manufacturing efficiency and reliability of the pressure sensor.
Smart Images

Figure CN118684187B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of pressure sensors, and in particular to a pressure sensor and a manufacturing method thereof. Background Art
[0002] A capacitive pressure sensor is a sensor that detects pressure by using the change in capacitance between two plates. Specifically, a capacitive pressure sensor has a variable capacitance structure. When external pressure acts on the sensor, the variable capacitance structure deforms, causing the capacitance gap to change, thereby changing the capacitance value. Compared with piezoresistive pressure sensors, capacitive pressure sensors have lower temperature drift and are more suitable for applications with higher temperature stability.
[0003] The common manufacturing methods of capacitive pressure sensors are: ① using the sacrificial layer process to manufacture variable capacitors; ② using the bonding process to manufacture variable capacitors. However, when using the sacrificial layer process to form variable capacitors, the film adhesion problem during the release of the sacrificial layer may cause device failure. When using the bonding process to manufacture variable capacitors, the process is complex and the production cost is high. Summary of the invention
[0004] The embodiments of the present invention provide a pressure sensor and a method for manufacturing the same, aiming to improve the problems that may occur during the manufacturing process of the pressure sensor.
[0005] In order to solve the above technical problems, the embodiments of the present invention disclose the following technical solutions:
[0006] In one aspect, a method for manufacturing a pressure sensor is provided, comprising:
[0007] Providing a substrate, and diffusing or implanting ions on a surface of one side of the substrate to form a heavily doped region in the substrate;
[0008] Etching a plurality of holes in the heavily doped region along the thickness direction of the substrate, with columnar protrusions between adjacent holes, and the etching depth of the plurality of holes being less than the depth of the heavily doped region;
[0009] Etching a connection between the columnar protrusion and the heavily doped region to form a cavity between the columnar protrusion and the heavily doped region;
[0010] Fabricating an epitaxial structure on a surface of one side of the substrate where the heavily doped region is located, wherein the epitaxial structure is used to seal the cavity;
[0011] Etching on the epitaxial structure to form a first annular groove penetrating the epitaxial structure and filling the first annular groove with an insulating material;
[0012] Manufacturing an insulating structure, wherein the insulating structure covers a surface of the epitaxial structure that is away from the substrate;
[0013] Manufacturing an electrical connection structure, the electrical connection structure comprising a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove;
[0014] The epitaxial structure located in the first annular groove forms a movable electrode plate of the pressure sensor, and the substrate located in the heavily doped region and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
[0015] In addition to or as an alternative to one or more features disclosed above, the doping type of the substrate in the heavily doped region, the doping type of the substrate outside the heavily doped region, and the doping type of the epitaxial structure are the same.
[0016] In addition to or as an alternative to one or more features disclosed above, etching the connection between the columnar protrusion and the heavily doped region to form a cavity between the columnar protrusion and the heavily doped region includes:
[0017] At least two cavities are formed between the columnar protrusion and the heavily doped region, and the at least two cavities are physically isolated from each other.
[0018] In addition to or as an alternative to one or more of the features disclosed above, etching on the epitaxial structure to form a first annular groove penetrating the epitaxial structure, and filling the first annular groove with an insulating material includes:
[0019] A first annular groove penetrating the epitaxial structure is etched on the epitaxial structure above each cavity, and an insulating material is filled in each first annular groove.
[0020] In addition to or as an alternative to one or more of the features disclosed above, the manufacturing of the electrical connection structure, the electrical connection structure comprising a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove, comprising:
[0021] A second electrical connector is disposed in each of the first annular grooves.
[0022] In addition to or as an alternative to one or more of the features disclosed above, the thicknesses of the insulating structures located above different cavities are the same or different.
[0023] In addition to or as an alternative to one or more of the features disclosed above, the doping concentration of the substrate in the heavily doped region is between 10 18 -10 20 cm -3 The doping concentration of the epitaxial structure is 10 18 -10 20 cm -3 .
[0024] In addition to or as an alternative to one or more of the features disclosed above, etching a first annular groove penetrating the epitaxial structure and filling the first annular groove, the first annular groove being located above the cavity, the manufacturing method further comprises:
[0025] An oxide layer structure is manufactured, wherein the oxide layer structure at least covers the inner wall of the cavity, the surface of the epitaxial structure exposed in the cavity, and the surface of the columnar protrusion exposed in the cavity.
[0026] In addition to or as an alternative to one or more of the features disclosed above, the method of manufacturing the oxide layer structure includes:
[0027] Etching a first groove on the epitaxial structure, wherein the first groove is connected to the cavity;
[0028] thermally oxidizing the interior of the cavity through the first trench to form the oxide layer structure;
[0029] The first trench is filled to reclose the cavity.
[0030] In addition to or as an alternative to one or more of the features disclosed above, the epitaxial structure is manufactured by a high temperature epitaxial process.
[0031] In addition to or as an alternative to one or more of the features disclosed above, the manufacturing of the electrical connection structure, the electrical connection structure comprising a first electrical connection member and a second electrical connection member, the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure, the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove, comprising:
[0032] Making a first through hole and a second through hole penetrating the insulating structure, wherein in the thickness direction of the substrate, the first through hole is located outside the first annular groove, and the second through hole is located inside the first annular groove;
[0033] Filling the first through hole with a conductive material to form the first electrical connector;
[0034] The second through hole is filled with a conductive material to form the second electrical connection member.
[0035] In another aspect, a pressure sensor is provided, comprising:
[0036] A substrate, wherein one side surface of the substrate is a heavily doped region, wherein a surface of the heavily doped region facing away from the substrate has a plurality of holes, wherein columnar convex portions are provided between adjacent holes, and adjacent columnar convex portions are connected to form a mesh structure;
[0037] an epitaxial structure, the epitaxial structure being located on the mesh structure and forming a closed cavity on the substrate together with the mesh structure, the epitaxial structure comprising a first annular groove penetrating the epitaxial structure, the first annular groove being filled with an insulating material;
[0038] An insulating structure, the insulating structure covering a surface of the epitaxial structure away from the substrate;
[0039] An electrical connection structure, the electrical connection structure comprising a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove;
[0040] The epitaxial structure located in the first annular groove forms a movable electrode plate of the pressure sensor, and the substrate located in the heavily doped region and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
[0041] In addition to or as an alternative to one or more features disclosed above, the doping type of the substrate in the heavily doped region, the doping type of the substrate outside the heavily doped region, and the doping type of the epitaxial structure are the same.
[0042] In addition to or as an alternative to one or more of the features disclosed above, the number of the enclosed cavities is at least two, and the at least two enclosed cavities are physically isolated from each other.
[0043] In addition to or as an alternative to one or more of the features disclosed above, the epitaxial structure above each of the cavities includes a first annular groove penetrating through the epitaxial structure, and each of the first annular grooves is filled with insulating material.
[0044] In addition to or as an alternative to one or more of the features disclosed above, a second electrical connector is disposed in each of the first annular grooves.
[0045] In addition to or as an alternative to one or more of the features disclosed above, the thicknesses of the insulating structures located above different cavities are the same or different.
[0046] In addition to or as an alternative to one or more of the features disclosed above, an oxide layer structure is further included, which covers at least the inner wall of the cavity, the surface of the epitaxial structure exposed in the cavity, and the surface of the columnar protrusion exposed in the cavity.
[0047] One of the above technical solutions has the following advantages or beneficial effects: an epitaxial structure is made on one side surface of the substrate, and the epitaxial structure is used to form a movable electrode plate of the pressure sensor, and the substrate opposite to the movable electrode plate forms the fixed electrode plate of the pressure sensor. Specifically, the present application forms a heavily doped region on one side surface of the substrate, and etches a plurality of holes in the heavily doped region, with columnar protrusions between adjacent holes, and forms a cavity between the columnar protrusions and the heavily doped region. In this way, on the plane of the substrate where the heavily doped region is located, a plurality of columnar protrusions are interconnected in a mesh, which can be used to support the epitaxial structure. At the same time, because the aperture of the hole etched in the heavily doped region is small, the material used to form the epitaxial structure is not easy to enter the cavity from the hole. When the pressure detection is actually performed, the epitaxial structure located above the cavity is deformed, the spacing between the movable electrode plate and the fixed electrode plate changes, and the columnar protrusion can prevent the movable electrode plate from sticking to the fixed electrode plate. Compared with the formation of variable capacitors using a sacrificial layer process and the manufacture of variable capacitors using a bonding process, the present application has a simple process and low cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] The technical solutions and other beneficial effects of the present invention will be made apparent by describing in detail the specific embodiments of the present invention in conjunction with the accompanying drawings.
[0049] Figure 1 4 is a flow chart of a method for manufacturing a pressure sensor according to an embodiment of the present invention.
[0050] Figure 2-12 Schematic diagram of the process of manufacturing a pressure sensor according to an embodiment of the present invention.
[0051] Figure 13-15 It is a schematic diagram of the process of manufacturing a pressure sensor with at least two cavities provided in an embodiment of the present invention.
[0052] Fig.16 1 is a schematic top view of a pressure sensor having at least two cavities provided in accordance with an embodiment of the present invention.
[0053] Fig.17 1 is a schematic top view of a pressure sensor for manufacturing a cavity provided in accordance with an embodiment of the present invention.
[0054] Fig.18It is a schematic top view of a process corresponding to step S300 in the method for manufacturing a pressure sensor provided according to an embodiment of the present invention.
[0055] Figure 19-21 is an equivalent circuit diagram of a pressure sensor provided according to an embodiment of the present invention.
[0056] Description of reference numerals:
[0057] 10, substrate; 101, heavily doped region; 102, hole; 103, columnar protrusion; 104, cavity;
[0058] 20. Oxide layer structure;
[0059] 30. epitaxial structure; 301. first trench; 302. first ring groove;
[0060] 40. Insulation structure;
[0061] 50. Electrical connection structure; 501. First electrical connection member; 502. Second electrical connection member; 503. First through hole; 504. Second through hole. DETAILED DESCRIPTION
[0062] In order to make the purpose, technical solution and beneficial effects of the present invention more clear, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described in this specification are only for explaining the present invention, not for limiting the present invention.
[0063] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "multiple" refers to two or more, unless otherwise clearly and specifically defined.
[0064] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0065] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0066] The present invention discloses a method for manufacturing a pressure sensor. Figure 1 , the manufacturing method of a pressure sensor comprises:
[0067] S100. Providing a substrate;
[0068] S200. Diffusing or implanting ions on one side of the substrate surface to form a heavily doped region in the substrate;
[0069] S300. Etching a plurality of holes in the heavily doped region along the thickness direction of the substrate, with columnar protrusions between adjacent holes, and the etching depth of the plurality of holes being less than the depth of the heavily doped region;
[0070] S400. Etching the connection between the columnar protrusion and the heavily doped region to form a cavity between the columnar protrusion and the heavily doped region;
[0071] S500. Fabricating an epitaxial structure on one side of the substrate where the heavily doped region is located, the epitaxial structure being used to enclose the cavity;
[0072] S600. Etching on the epitaxial structure to form a first annular groove penetrating the epitaxial structure and filling the first annular groove with an insulating material;
[0073] S700. Fabricating an insulating structure, the insulating structure covering a surface of the epitaxial structure away from the substrate;
[0074] S800. Make an electrical connection structure, which includes a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove.
[0075] In the pressure sensor manufactured in this way, the epitaxial structure 30 located in the first annular groove 302 forms a movable electrode plate of the pressure sensor, and the substrate 10 located in the heavily doped region 101 and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
[0076] Reference Figure 2 In step S200, ions are diffused or implanted on one side of the substrate 10 to form a heavily doped region 101 in the substrate 10. In some embodiments, the penetration depth of the ions in the heavily doped region 101 in the thickness direction of the substrate 10 is 10 μm-15 μm, and the projection shape of the heavily doped region 101 can be circular, polygonal, or irregular. In some embodiments, the doping concentration of the heavily doped region 101 is 10 μm-15 μm. 18 -10 20 cm -3 . In some embodiments, the doping type of the substrate 10 located in the heavily doped region 101 is the same as the doping type of the substrate 10 located outside the heavily doped region 101. Specifically, when the doping type of the substrate 10 located outside the heavily doped region 101 is N-type, the doping type of the substrate 10 located in the heavily doped region 101 is also N-type; when the doping type of the substrate 10 located outside the heavily doped region 101 is P-type, the doping type of the substrate 10 located in the heavily doped region 101 is also P-type. It should be noted that the substrate 10 is generally made of silicon material with a resistivity of 1-10Ω·cm.
[0077] Reference Figure 3 In step S300, a plurality of holes 102 are etched in the heavily doped region 101 along the thickness direction of the substrate 10, and columnar protrusions 103 are provided between adjacent holes 102, and adjacent columnar protrusions 103 are connected. Fig.18, on the plane of the substrate 10 where the heavily doped region 101 is located, adjacent columnar protrusions 103 are connected to form a mesh structure, which can be used to support the epitaxial structure 30. At the same time, because the aperture of the hole 102 etched in the heavily doped region 101 is small, the material used to form the epitaxial structure 30 is not easy to enter the cavity 104 from the hole 102. It should be noted that the multiple holes 102 etched in the heavily doped region 101 can be circular holes 102, polygonal holes 102, or irregular holes 102. In some embodiments, the etching depth of all holes 102 is less than the depth of the heavily doped region. In some embodiments, the etching depth of the hole 102 is generally between 7-8μm. It is worth mentioning that when a plurality of holes 102 are etched in the heavily doped region 101, the non-etched area can be covered with photoresist to prevent the area where the columnar protrusion 103 is located from being etched.
[0078] Reference Figure 4 , step S400 etches the connection between the columnar protrusion 103 and the heavily doped region 101 to form a cavity 104 between the columnar protrusion 103 and the heavily doped region 101. Specifically, the cavity 104 can serve as a deformation space for the movable plate. When making the cavity 104, the connection between the columnar protrusion 103 and the heavily doped region 101 can be etched by an isotropic etching method or an anisotropic etching method. Isotropic etching refers to the process of etching the surface of a material using the same etching chemical (such as a solution or gas). In isotropic etching, the chemical will evenly reduce or dissolve the outer layer of the material so that its entire surface is evenly and flatly treated. Anisotropic etching refers to the process of etching the material using a chemical different from the etched material. In anisotropic etching, the chemical will selectively act on a specific material without significantly affecting other materials. This can be used to achieve precise manufacturing processes and form complex structures or devices. It is worth mentioning that in the process of forming the cavity 104 , the size of the columnar protrusion 103 in the thickness direction of the substrate 10 will also be shortened. In some embodiments, the size of the shortened columnar protrusion 103 is usually between 1 and 3 μm.
[0079] Reference Figure 5, step S500 forms an epitaxial structure 30 on one side surface of the substrate 10 where the heavily doped region 101 is located to close the cavity 104. The epitaxial structure 30 at least covers the remaining surface of the heavily doped region 101 and the end surface of all columnar protrusions 103 away from the cavity 104. In some embodiments, the epitaxial structure 30 also covers the surfaces of other substrates 10 except the heavily doped region 101. In some embodiments, the epitaxial structure 30 is formed by a high-temperature epitaxial process. The high-temperature epitaxial process refers to placing the substrate 10 in a high-temperature reaction chamber and depositing the material in the gas phase on the surface of the substrate 10 by heating to form the epitaxial structure 30. Specifically, the temperature and atmosphere are controlled in the high-temperature reaction chamber, usually using methods such as chemical vapor deposition (CVD) or molecular beam epitaxy (MBE), so that the surface of the substrate 10 reacts with the material in the gas phase, thereby growing the epitaxial structure 30 on the substrate 10. In practical applications, the thickness of the epitaxial structure 30 is set according to the sensitivity requirements of the pressure sensor. In some embodiments, the doping concentration of the epitaxial structure 30 is between 10 18 -10 20 cm -3 . In some embodiments, the doping type of the substrate 10 located in the heavily doped region 101 is the same as the doping type of the epitaxial structure 30. Specifically, when the doping type of the substrate 10 located in the heavily doped region 101 is N-type, the doping type of the epitaxial structure 30 is also N-type; when the doping type of the substrate 10 located in the heavily doped region 101 is P-type, the doping type of the epitaxial structure 30 is also P-type. It should be noted that when the epitaxial structure 30 is manufactured using a high-temperature epitaxial process, the temperature is usually around 1150°C. This temperature will cause the migration of silicon atoms, which will further shorten the size of the columnar protrusion 103, usually by several hundred nanometers, so that the end of the columnar protrusion 103 facing the bottom of the cavity 104 can be smoothed.
[0080] Reference Fig. 9 , usually after the epitaxial structure 30 is formed, the oxide layer structure 20 is formed, and the oxide layer structure 20 at least covers the inner wall of the cavity 104, the surface of the epitaxial structure 30 exposed in the cavity 104, and the surface of the columnar protrusion 103 exposed in the cavity 104. In some embodiments, the oxide layer structure 20 is formed by the following steps: Figure 6 , a first trench 301 is formed by etching on the epitaxial structure 30, and the first trench 301 is connected to the cavity 104; referring to ,7, the interior of the cavity 104 is thermally oxidized through the first trench 301 to form an oxide layer structure 20; referring to Figure 8, fill the first trench 301 to reclose the cavity 104. Specifically, the first trench 301 is used to act as an injection channel for the gas of thermal oxidation when making the oxide layer structure 20. The gas used for thermal oxidation is usually oxygen or an oxygen mixture. At high temperature, the oxygen molecules can react with the inner wall surface of the cavity 104 to form the oxide layer structure 20. The oxide layer structure 20 can play an insulating role to prevent the epitaxial structure 30 from contacting and disconnecting the bottom of the cavity 104. Further, in some embodiments, the first trench 301 is filled by low pressure chemical vapor deposition (LPCVD). Specifically, the filling material can be tetraethoxysilane (TEOS) or other insulating materials.
[0081] Furthermore, when the oxide layer structure 20 is manufactured, the silicon material in contact with oxygen or oxygen mixture will be oxidized, and the material of the substrate 10 and the material of the epitaxial structure 30 are usually silicon. Therefore, when the oxide layer structure 20 is manufactured, the surface of the epitaxial structure 30 facing away from the cavity 104 will also generate the oxide layer structure 20 (refer to Figure 7 In some embodiments, after the oxide layer structure 20 inside the cavity 104 is formed, the oxide layer structure 20 on the surface of the epitaxial structure 30 facing away from the cavity 104 is removed by etching back or chemical mechanical polishing (CMP).
[0082] Continue to refer to Fig. 9 and Fig.17 , step S600 etches on the epitaxial structure 30 to form a first annular groove 302 that penetrates the epitaxial structure 30 and fills the first annular groove 302 with insulating material. Specifically, the first annular groove 302 is located above the cavity 104, and separates the epitaxial structure 30 into the epitaxial structure 30 located inside the first annular groove 302 and the epitaxial structure 30 located outside the first annular groove 302. The epitaxial structure 30 in the first annular groove 302 is used to act as a movable electrode plate of the pressure sensor, and the substrate 10 located in the heavily doped region 101 and opposite to the movable electrode plate is used to act as a fixed electrode plate of the pressure sensor. It should be noted that, in combination with the columnar protrusion 103 manufactured in the above steps, when pressure acts on the movable electrode plate, the movable electrode plate is deformed, and the gap between the movable electrode plate and the fixed electrode plate becomes smaller. The columnar protrusion 103 can act as a stop structure to effectively prevent the movable electrode plate from being attracted to the fixed electrode plate.
[0083] Reference Fig.10 , step S700 manufactures an insulating structure 40, and the insulating structure 40 covers the surface of the epitaxial structure 30 away from the substrate 10. It should be noted that, in some embodiments, filling the first annular groove 302 and manufacturing the insulating structure 40 can usually be performed simultaneously. Specifically, in some embodiments, the first annular groove 302 is filled and the insulating structure 40 is manufactured by low pressure chemical vapor deposition (LPCVD), and the filling material can be tetraethoxysilane (TEOS) or other insulating materials.
[0084] Reference Fig.12 , step S800 manufactures an electrical connection structure 50, and the electrical connection structure 50 includes a first electrical connection member 501 and a second electrical connection member 502. Specifically, the first electrical connection member 501 and the second electrical connection member 502 both penetrate the insulating structure 40 and are connected to the epitaxial structure 30, the first electrical connection member 501 is located outside the first annular groove 302, and the second electrical connection member 502 is located inside the first annular groove 302. The epitaxial structure 30 located outside the first annular groove 302 is connected to the substrate 10, the first electrical connection member 501 can lead out the electrical signal of the fixed electrode plate, and the second electrical connection member 502 can lead out the electrical signal of the movable electrode plate. In some embodiments, the electrical connection structure 50 is manufactured by the following steps, referring to Fig.11 First, a first through hole 503 and a second through hole 504 are made to penetrate the insulating structure 40. In the thickness direction of the substrate 10, the first through hole 503 is located outside the first annular groove 302, and the second through hole 504 is located inside the first annular groove 302; Fig.12 , a conductive material is filled in the first through hole 503 to form a first electrical connector 501, and a conductive material is filled in the second through hole 504 to form a second electrical connector 502. It should be noted that the conductive material can be a conductive metal. It should be noted that, in combination with the structure made in the above steps, when pressure acts on the movable electrode plate, the movable electrode plate is deformed, the gap between the movable electrode plate and the fixed electrode plate becomes smaller, and the capacitance signal can be output through the first electrical connector 501 and the second electrical connector 502.
[0085] Reference Fig.13 , Fig.14 and Fig.16 In some embodiments, the step S400 of etching the connection between the columnar protrusion 103 and the heavily doped region 101 to form a cavity 104 between the columnar protrusion 103 and the heavily doped region 101 includes: forming at least two cavities 104 between the columnar protrusion 103 and the heavily doped region 101, and the at least two cavities 104 are physically isolated from each other. At the same time, when making the first annular groove 302 in step S600, a first annular groove 302 penetrating the epitaxial structure 30 is etched on the epitaxial structure 30 above each cavity 104, and an insulating material is filled in each first annular groove 302. Similarly, when making the electrical connection structure 50 in step S800, a second electrical connector 502 is provided in each first annular groove 302. The bottom of each cavity 104 and the epitaxial structure 30 in the first annular groove 302 corresponding to the cavity 104 constitute a capacitive pressure sensor. The sizes of different cavities 104 can be the same or different. Cavities 104 of different sizes have different sensitivities.
[0086] Reference Fig.15In some embodiments, the thickness of the insulating structure 40 located above different cavities 104 is the same or different. The thickness of the insulating structure 40 is related to the sensitivity of the pressure sensor, and pressure sensors with different sensitivities and capacitance values can be obtained by changing the thickness of the insulating structure 40.
[0087] It is worth mentioning that when only one cavity 104 is opened, the equivalent circuit of the pressure sensor is as follows: Fig.19 As shown, one electrode of the capacitor is equivalent to the movable plate, and the other electrode is equivalent to the fixed plate. The signal lines on both sides of the electrode are used to connect to the electrical connector of each electrode. When two cavities 104 are opened, the equivalent circuit of the pressure sensor is referred to as Fig. 20 As shown, the fixed electrodes of the two capacitors share a signal line, and the two capacitors form a half-bridge capacitor. When four cavities 104 are opened, the equivalent circuit of the pressure sensor is as follows: Fig.21 As shown, the fixed electrode of capacitor C1 and the fixed electrode of capacitor C2 share a signal line, the movable electrode of capacitor C1 and the movable electrode of capacitor C4 share a signal line, the fixed electrode of capacitor C4 and the fixed electrode of capacitor C3 share a signal line, and the movable electrode of capacitor C2 and the movable electrode of capacitor C3 share a signal line. The four capacitors can form a Wheatstone bridge capacitor.
[0088] The embodiment of the present invention discloses a pressure sensor, referring to Fig.12 , including: a substrate 10, an epitaxial structure 30, an insulating structure 40 and an electrical connection structure 50. One side surface of the substrate 10 is a heavily doped region 101. In the heavily doped region 101, a surface of the heavily doped region away from the substrate has a plurality of holes, and columnar protrusions 103 are provided between adjacent holes 102. Adjacent columnar protrusions 103 are connected to form a mesh structure, and a cavity 104 is provided between the columnar protrusions 103 and the substrate 10. The epitaxial structure 30 is located on the mesh structure, and together with the mesh structure, a closed cavity 104 is formed on the substrate 10. The epitaxial structure 30 includes a first annular groove 302 that penetrates the epitaxial structure 30, and the first annular groove 302 is filled with an insulating material. The insulating structure 40 covers a side surface of the epitaxial structure 30 away from the substrate 10. The electrical connection structure 50 includes a first electrical connector 501 and a second electrical connector 502. The first electrical connector 501 and the second electrical connector 502 both penetrate the insulating structure 40 and are connected to the epitaxial structure 30. The first electrical connector 501 is located outside the first annular groove 302, and the second electrical connector 502 is located inside the first annular groove 302. The epitaxial structure 30 located inside the first annular groove 302 forms a movable electrode plate of the pressure sensor, and the substrate 10 located in the heavily doped region 101 and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
[0089] In some embodiments, the doping type of the substrate 10 in the heavily doped region 101 , the doping type of the substrate 10 outside the heavily doped region 101 , and the doping type of the epitaxial structure 30 are the same.
[0090] In some embodiments, reference Fig.14 There are at least two closed cavities 104 , and at least two closed cavities 104 are physically isolated from each other.
[0091] In some embodiments, the epitaxial structure 30 above each cavity 104 includes a first annular groove 302 penetrating the epitaxial structure 30 , and each first annular groove 302 is filled with insulating material.
[0092] In some embodiments, a second electrical connector 502 is disposed in each first annular groove 302 .
[0093] In some embodiments, the thicknesses of the insulating structures 40 located above different cavities 104 are the same or different.
[0094] In some embodiments, the pressure sensor further includes an oxide layer structure 20 , which covers at least an inner wall of the cavity 104 , a surface of the epitaxial structure 30 exposed in the cavity 104 , and a surface of the columnar protrusion 103 exposed in the cavity 104 .
[0095] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0096] The above embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.
Claims
1. A method for manufacturing a pressure sensor, characterized in that: include: Providing a substrate, and diffusing or implanting ions on a surface of one side of the substrate to form a heavily doped region in the substrate; Etching a plurality of holes in the heavily doped region along the thickness direction of the substrate, with columnar protrusions between adjacent holes, and the etching depth of the plurality of holes being less than the depth of the heavily doped region; Etching a connection between the columnar protrusion and the heavily doped region to form a cavity between the columnar protrusion and the heavily doped region; Fabricating an epitaxial structure on a surface of one side of the substrate where the heavily doped region is located, wherein the epitaxial structure is used to seal the cavity; Etching on the epitaxial structure to form a first annular groove penetrating the epitaxial structure and filling the first annular groove with an insulating material; Manufacturing an insulating structure, wherein the insulating structure covers a surface of the epitaxial structure that is away from the substrate; Manufacturing an electrical connection structure, the electrical connection structure comprising a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove; The epitaxial structure located in the first annular groove forms a movable electrode plate of the pressure sensor, and the substrate located in the heavily doped region and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
2. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The doping type of the substrate in the heavily doped region, the doping type of the substrate outside the heavily doped region, and the doping type of the epitaxial structure are the same.
3. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The etching of the connection between the columnar protrusion and the heavily doped region to form a cavity between the columnar protrusion and the heavily doped region comprises: At least two cavities are formed between the columnar protrusion and the heavily doped region, and the at least two cavities are physically isolated from each other.
4. The method for manufacturing a pressure sensor according to claim 3, characterized in that: The etching on the epitaxial structure to form a first annular groove penetrating the epitaxial structure, and filling the first annular groove with an insulating material comprises: A first annular groove penetrating the epitaxial structure is etched on the epitaxial structure above each cavity, and an insulating material is filled in each first annular groove.
5. The method for manufacturing a pressure sensor according to claim 4, characterized in that: The method for manufacturing an electrical connection structure, wherein the electrical connection structure includes a first electrical connection member and a second electrical connection member; the first electrical connection member and the second electrical connection member both penetrate the insulating structure and are connected to the epitaxial structure; the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove, comprises: A second electrical connector is disposed in each of the first annular grooves.
6. The method for manufacturing a pressure sensor according to claim 3, characterized in that: The thickness of the insulating structures located above different cavities may be the same or different.
7. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The doping concentration of the substrate in the heavily doped region is between 10 18 -10 20 cm -3 The doping concentration of the epitaxial structure is 10 18 -10 20 cm -3 .
8. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The step of etching the epitaxial structure to form a first annular groove penetrating the epitaxial structure and filling the first annular groove, wherein the first annular groove is located above the cavity, and the manufacturing method further comprises: An oxide layer structure is manufactured, wherein the oxide layer structure at least covers the inner wall of the cavity, the surface of the epitaxial structure exposed in the cavity, and the surface of the columnar protrusion exposed in the cavity.
9. The method for manufacturing a pressure sensor according to claim 8, characterized in that: The manufacturing of the oxide layer structure comprises: Etching a first groove on the epitaxial structure, wherein the first groove is connected to the cavity; thermally oxidizing the interior of the cavity through the first trench to form the oxide layer structure; The first trench is filled to reclose the cavity.
10. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The epitaxial structure is manufactured by a high-temperature epitaxial process.
11. The method for manufacturing a pressure sensor according to claim 1, characterized in that: The method of manufacturing an electrical connection structure, wherein the electrical connection structure includes a first electrical connection member and a second electrical connection member, wherein both the first electrical connection member and the second electrical connection member penetrate the insulating structure and are connected to the epitaxial structure, wherein the first electrical connection member is located outside the first annular groove, and the second electrical connection member is located inside the first annular groove, comprises: Making a first through hole and a second through hole penetrating the insulating structure, wherein in the thickness direction of the substrate, the first through hole is located outside the first annular groove, and the second through hole is located inside the first annular groove; Filling the first through hole with a conductive material to form the first electrical connector; The second through hole is filled with a conductive material to form the second electrical connection member.
12. A pressure sensor, characterized in that: include: A substrate (10), wherein one side surface of the substrate (10) is a heavily doped region (101), wherein a surface of the heavily doped region (101) facing away from the substrate (10) has a plurality of holes (102) opened therein, and columnar protrusions (103) are provided between adjacent holes (102), and adjacent columnar protrusions (103) are connected to form a network structure; an epitaxial structure (30), the epitaxial structure (30) being located on the mesh structure and forming a closed cavity (104) on the substrate (10) together with the mesh structure, the epitaxial structure (30) comprising a first annular groove (302) penetrating the epitaxial structure (30), the first annular groove (302) being filled with an insulating material; An insulating structure (40), the insulating structure (40) covering a surface of the epitaxial structure (30) that is away from the substrate (10); An electrical connection structure (50), the electrical connection structure (50) comprising a first electrical connection member (501) and a second electrical connection member (502); the first electrical connection member (501) and the second electrical connection member (502) both penetrate the insulating structure (40) and are connected to the epitaxial structure (30); the first electrical connection member (501) is located outside the first annular groove (302), and the second electrical connection member (502) is located inside the first annular groove (302); The epitaxial structure (30) located in the first annular groove (302) forms a movable electrode plate of the pressure sensor, and the substrate (10) located in the heavily doped region (101) and opposite to the movable electrode plate forms a fixed electrode plate of the pressure sensor.
13. The pressure sensor according to claim 12, characterized in that: The doping type of the substrate (10) located in the heavily doped region (101), the doping type of the substrate (10) located outside the heavily doped region (101), and the doping type of the epitaxial structure (30) are the same.
14. The pressure sensor according to claim 12, characterized in that: There are at least two sealed cavities (104), and the at least two sealed cavities (104) are physically isolated from each other.
15. The pressure sensor according to claim 14, characterized in that: The epitaxial structure (30) above each cavity (104) comprises a first annular groove (302) penetrating the epitaxial structure (30), and each first annular groove (302) is filled with insulating material.
16. The pressure sensor according to claim 15, characterized in that: A second electrical connector (502) is disposed in each of the first annular grooves (302).
17. The pressure sensor according to claim 15, characterized in that: The thicknesses of the insulating structures (40) located above different cavities (104) are the same or different.
18. The pressure sensor according to claim 12, characterized in that: It also includes an oxide layer structure (20), wherein the oxide layer structure (20) at least covers the inner wall of the cavity (104), the surface of the epitaxial structure (30) exposed in the cavity (104), and the surface of the columnar protrusion (103) exposed in the cavity (104).