A production equipment for tinned strip
By spraying flux in the soft melting treatment system of the tin-plating belt production equipment and performing quality evaluation and correction, the problem of uneven flux distribution is solved, and the corrosion resistance and brightness of the tin-plating belt is improved.
Patent Information
- Application Number
- CN202411213583.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-30
AI Technical Summary
During the production process of tin plating belt, it is difficult to distribute the flux uniformly on the tin layer, and spraying the flux before the tin layer melts is easily lost due to the transmission movement of the electroplating belt, resulting in uneven flux distribution on the tin layer.
Using production equipment including pretreatment systems, electroplating tin systems, soft melting treatment systems and post-treatment systems, spray fluxes when the tin layer is soft-melting through a soft melting furnace, and the coating quality is evaluated using a visual scanner, and the matte roller set is used to evaluate the The defects are cut, and the telescopic frame is re-coated to ensure uniform distribution of flux.
The uniform distribution of flux on the tin layer is achieved, the corrosion resistance and brightness of the tin strip are improved, and the quality and appearance of the tin layer are ensured.
Smart Images

Figure CN118704059B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of steel strip metallurgy, in particular to a production device for tinned strips. Background Art
[0002] The production of tin-plated strips requires multiple continuous process steps, aiming to evenly coat tin on the cold-rolled steel strip to form a tin-plated sheet with excellent corrosion resistance and good appearance. After the initial tin plating, the tin-plated strip generally needs to go through a soft melting process. During the soft melting process, the tin layer melts and reacts with the strip steel substrate to form a layer of tin-iron alloy (FeSn2), thereby improving the corrosion resistance of the tin-plated sheet. In the prior art, such as the invention patent with patent number CN201010594947.1, a resistance soft melting method is used to heat the strip steel (using the resistance thermal effect generated when the current passes through the strip steel to heat it), thereby realizing the soft melting work, which is widely used. During the soft melting of the tin layer, a flux is usually added to improve the quality of the coating. At present, in the flux spraying, the flux is sprayed when the tin layer reaches a molten state, and the flux is difficult to be evenly distributed on the tin layer. When the flux is sprayed before the tin layer is melted, the flux is easily lost due to the transmission movement of the electroplating strip, which still makes it difficult to evenly distribute the flux on the tin layer.
[0003] Therefore, it is necessary to provide a tin-plated strip production equipment to solve the problems raised in the above background technology. Summary of the invention
[0004] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a tin-plated strip production equipment, comprising: a pre-treatment system, an electro-tinning system, a soft melting treatment system and a post-treatment system, wherein the pre-treatment system performs surface treatment on the steel strip by means of cleaning, chemical degreasing, oil removal and rust removal, and pickling and activation, so as to remove grease and oxides on the surface of the steel strip;
[0005] The electroplating tin system transfers the steel strip to the electroplating tank through the hanger, and deposits tin ions on the surface of the steel strip to form a tin layer during the electroplating process;
[0006] The post-treatment system uses electrolytic passivation and oiling to treat the surface of the tin-plated strip to prevent rust, so as to enhance the corrosion resistance and brightness of the tin-plated strip;
[0007] A soft melting treatment system is arranged between the electrotinning system and the post-treatment system, wherein the soft melting treatment system uses a flux to reduce the surface tension of the molten tin during the soft melting of the tin layer on the surface of the tin-plated strip, thereby enhancing the flow and spreading of the tin layer under the heating state;
[0008] The soft melting treatment system comprises: two conveying rollers, the two conveying rollers are used to roll in or send out the tinned strip, two chokes are distributed between the conveying rollers, one side of one of the chokes is distributed with multiple groups of transfer rollers, a soft melting furnace is arranged on one side of the transfer roller, an extrusion device is arranged outside the soft melting furnace, and a variable frequency power supply is also arranged outside the soft melting furnace, and the variable frequency power supply uses a three-phase transformer to provide heating voltage to the tinned strip;
[0009] The soft melting furnace is provided with three independent hot chambers, and a flux coating component is provided in the front independent hot chamber, and the flux coating component sprays flux on the front and back sides of the tin-plated strip so that the flux is evenly attached to the tin layer.
[0010] Further, as a preference, the flux coating assembly comprises: two tension roller groups distributed on the left and right, a first coating mechanism is arranged between the tension roller groups, a flip roller group is arranged outside the tension roller group located on the right, the flip roller group flips the tinned strip over and over, and a second coating mechanism is arranged outside the flip roller group;
[0011] The first coating mechanism and the second coating mechanism have the same composition structure.
[0012] Further, as a preference, the first coating mechanism comprises: an upper rack rod, which is horizontally erected in the soft melting furnace and located directly above the tinning strip, the upper rack rod is arranged in parallel with the tinning strip, and two telescopic racks are arranged below the upper rack rod, the two telescopic racks are telescopically adjusted in the vertical direction, and a plurality of spray heads are arranged below the telescopic racks along the width direction of the tinning strip, and each of the spray heads is connected to a delivery pipe for continuously delivering flux;
[0013] The variable frequency power supply provides heating power to the tinned strip sections in the area below each telescopic frame.
[0014] Further, as a preferred embodiment, the variable frequency power supply heats the tinned strip in the area below the telescopic frame to , flux in The temperature produces heat melting and covers the tin layer.
[0015] Further, as a preference, a front cooling device is provided between the telescopic racks, and the front cooling device contacts the surface of the tinned strip through a plurality of cooling rollers, and the front cooling device cools the tinned strip to , so that the flux Adhere to the tin layer at low temperature.
[0016] Further, preferably, a visual scanner is provided on one side of the front cooling device between the telescopic racks, and the visual scanner acquires the flux image on the tin-plated strip, thereby outputting the coating characteristic image of each section of the flux on the tin-plated strip, and the main control module outside the visual scanner evaluates the flux coating quality based on the grayscale of the acquired coating characteristic image, and identifies abnormal defects in the coating layer;
[0017] A grinding roller group is provided on one side of the visual scanner, and a plurality of the grinding roller groups are horizontally arranged on the tinned strip;
[0018] A rear cooling device is arranged between the telescopic frame and the tensioning roller group at the rear.
[0019] Furthermore, preferably, the grinding roller group adopts a gradient grinding feed rate to reduce the flux on the surface of the tin layer in the tin-plated strip in view of abnormal defects in the coating layer; and a plurality of distributed scanners are arranged at intervals between the grinding roller groups.
[0020] Further, as a preference, the grinding roller group comprises: a plurality of mounting seats arranged along the width direction of the tin-plated strip, a bottom roller is rotatably arranged at the lower part of each mounting seat, a roller frame is vertically slidably connected to the mounting seat, a grinding roller is rotatably connected in the roller frame, a linear loading part is fixed on the mounting seat, and one end of the linear loading part is fixed to the roller frame;
[0021] The grinding roller rotates in the opposite direction to the transmission direction of the tinned strip during operation;
[0022] A plurality of air passages are axially distributed on the grinding roller, and the plurality of air passages are circumferentially staggered and arranged on the side wall of the grinding roller. A negative pressure pipe is coaxially arranged in the grinding roller, and the negative pressure pipe is connected with each of the air passages.
[0023] Further, preferably, the grinding rollers in adjacent grinding roller groups are staggered in distribution.
[0024] Compared with the prior art, the present invention has the following beneficial effects:
[0025] The present invention adopts a pre-treatment system, an electrotinning system, a soft melting treatment system and a post-treatment system to jointly construct a tinning process for a steel strip, and the soft melting treatment system can use the resistive thermal effect to soft-melt the tin layer of the tin-plated strip, thereby improving the quality of the tin layer; wherein, the soft melting furnace mainly arranged can coat the plating layer with a flux coating component in a front independent hot chamber, and the molten solvent can solidify on the surface of the tin layer after cooling, and then a visual scanner is used to scan defects, so that the grinding roller group can reduce the spraying defects, thereby performing secondary coating correction through the spray head on the rear telescopic frame to ensure the uniformity of the flux coating. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 is a process flow chart of the present invention;
[0027] Figure 2 It is a structural schematic diagram of the soft melt processing system in the present invention;
[0028] Figure 3 It is a structural schematic diagram of the flux coating assembly in the present invention;
[0029] Figure 4 It is a schematic diagram of the structure of the grinding roller group in the present invention;
[0030] Figure 5 It is a schematic diagram of the structure of the grinding roller in the present invention;
[0031] In the figure: 1. frequency conversion power supply; 11. conveying roller; 12. choke; 13. transfer roller; 14. extrusion device; 2. soft melting furnace; 21. independent hot chamber; 3. flux coating assembly; 31. tensioning roller group; 32. flip roller group; 4. second coating mechanism; 41. upper rack rod; 42. telescopic frame; 43. spray head; 44. front cooling device; 45. visual scanner; 5. frosting roller group; 51. mounting seat; 52. bottom roller; 53. roller frame; 54. linear loading part; 6. frosting roller; 61. airway; 62. negative pressure pipe. DETAILED DESCRIPTION
[0032] See also Figure 1~Figure 5 In an embodiment of the present invention, a tin-plated strip production equipment includes: a pre-treatment system, an electro-tinning system, a soft melting treatment system and a post-treatment system. The pre-treatment system uses cleaning, chemical degreasing, oil removal and rust removal, pickling and activation to treat the surface of the steel strip, so as to remove grease and oxides on the surface of the steel strip; the specific process is as follows:
[0033] S1. First, remove the oil, dirt, dust and grease on the surface of the steel strip by washing with water or alkaline cleaning agent to reduce the subsequent processing obstruction and improve the cleanliness;
[0034] S2. Then use chemical degreasing agent to thoroughly remove stubborn oil and grease, improve cleanliness and prevent coating adhesion;
[0035] S3. Secondly, use an acidic solution, such as hydrochloric acid, sulfuric acid, phosphoric acid, to remove rust and oxide layer on the surface of the steel strip to expose fresh metal, which is conducive to plating adhesion;
[0036] S4. Finally, a layer of microscopic roughened surface is formed through chemical or electrolysis to increase the contact area, improve the bonding strength between the coating and the steel strip, and achieve an anti-corrosion effect.
[0037] The electroplating tin system transfers the steel strip to the electroplating tank through the hanger, and deposits tin ions on the surface of the steel strip to form a tin layer during the electroplating process;
[0038] The post-treatment system uses electrolytic passivation and oiling to treat the surface of the tin-plated strip to prevent rust, so as to enhance the corrosion resistance and brightness of the tin-plated strip;
[0039] A soft melting treatment system is arranged between the electrotinning system and the post-treatment system, wherein the soft melting treatment system uses a flux to reduce the surface tension of the molten tin during the soft melting of the tin layer on the surface of the tin-plated strip, thereby enhancing the flow and spreading of the tin layer under the heating state;
[0040] The soft melting treatment system comprises: two conveying rollers 11, the two conveying rollers 11 are used to roll in or send out the tinned strip, two chokes 12 are distributed between the conveying rollers 11, and the chokes 12 are energized to generate alternating current, forming a high-frequency magnetic field, and the magnetic field induces eddy currents in the steel strip, so as to achieve the resistance thermal effect to heat the steel strip, and a plurality of groups of transfer rollers 13 are distributed on one side of one of the chokes 12, and a soft melting furnace 2 is arranged on one side of the transfer roller 13, and an extrusion device 14 is arranged outside the soft melting furnace 2, and a variable frequency power supply 1 is also arranged outside the soft melting furnace 2, and the variable frequency power supply 1 uses a three-phase transformer to provide heating voltage to the tinned strip;
[0041] The soft melting furnace 2 is provided with three independent hot chambers 21, and a flux coating component 3 is provided in the front independent hot chamber 21. The flux coating component 3 sprays flux on the front and back sides of the tin-plated strip so that the flux is evenly attached to the tin layer.
[0042] In this embodiment, the flux coating assembly 3 includes: two tension roller groups 31 distributed on the left and right, a first coating mechanism is arranged between the tension roller groups 31, a flip roller group 32 is arranged outside the tension roller group 31 located on the right side, the flip roller group 32 flips the tinned strip front and back, and a second coating mechanism 4 is arranged outside the flip roller group 32;
[0043] The first coating mechanism and the second coating mechanism 4 have the same composition structure, that is, the first coating mechanism and the second coating mechanism 4 spray flux on the front and back sides of the tin-plated strip respectively.
[0044] As a preferred embodiment, the first coating mechanism includes: an upper rack rod 41, which is horizontally erected in the soft melting furnace 2 and located directly above the tinned strip, the upper rack rod 41 is arranged parallel to the tinned strip, and two telescopic racks 42 are arranged below the upper rack rod 41, the two telescopic racks 42 are telescopically adjusted in the vertical direction, and a plurality of spray heads 43 are arranged below the telescopic racks 42 along the width direction of the tinned strip, and each of the spray heads 43 is connected to a conveying pipe for continuously conveying flux;
[0045] The variable frequency power supply provides heating power to the tinned strip sections in the area below each of the telescopic frames 42, so that the tinned strip sections can be heated.
[0046] In this embodiment, the variable frequency power supply heats the tinned strip in the area below the telescopic frame 42 to , flux in The temperature produces heat melting and covers the tin layer. The variable frequency power supply provides adjustable high-frequency AC power. By precisely controlling the current and voltage frequency, it is accurately heated to the set temperature to ensure that the area under the tin-plated strip reaches the melting point of the flux without overheating.
[0047] In this embodiment, a front cooling device 44 is provided between the telescopic racks 42. The front cooling device 44 contacts the surface of the tinned strip through a plurality of cooling rollers. The front cooling device 44 cools the tinned strip to a temperature of , so that the flux The flux adheres to the tin layer at a low temperature, so that the flux will not be affected by the transmission vibration and uneven flow distribution will occur during the transmission of the tin-plated strip.
[0048] In this embodiment, a visual scanner 45 is provided on one side of the front cooling device 44 between the telescopic racks 42. The visual scanner 45 acquires the flux image on the tin-plated strip, thereby outputting the coating characteristic image of each section of the flux on the tin-plated strip. The main control module outside the visual scanner 45 evaluates the flux coating quality based on the grayscale of the acquired coating characteristic image, and identifies abnormal defects in the coating layer (such as bubbles, cracks, particles, missing, dripping points, etc.);
[0049] A grinding roller group 5 is provided on one side of the visual scanner 45, and a plurality of the grinding roller groups 5 are horizontally arranged on the tinned strip;
[0050] A rear cooling device is provided between the telescopic frame 42 and the tensioning roller group 31 at the rear, that is, each spray head 43 on the telescopic frame 42 at the rear is mainly used for repairing the defective positions of flux spraying on the tin-plated strip, so as to achieve uniform distribution of flux.
[0051] As a preferred embodiment, the grinding roller group 5 adopts a gradient grinding feed rate to reduce the flux on the surface of the tin layer in the tin-plated strip in response to abnormal defects in the coating layer; a plurality of distributed scanners are arranged at intervals between the grinding roller groups 5, and the distributed scanners can acquire and analyze images of the flux reduction area to avoid wear on the surface of the tin-plated strip.
[0052] In this embodiment, the grinding roller group 5 includes: a plurality of mounting seats 51 arranged along the width direction of the tinned strip, a bottom roller 52 is rotatably arranged at the lower part of each mounting seat 51, a roller frame 53 is vertically slidably connected to the mounting seat 51, a grinding roller 6 is rotatably connected to the roller frame 53, a linear loading part 54 is fixed to the mounting seat 51, and one end of the linear loading part 54 is fixed to the roller frame 53;
[0053] The grinding roller 6 rotates in the opposite direction to the conveying direction of the tinned strip during operation, so that the flux is reduced through the rough surface of the grinding roller.
[0054] A plurality of air passages 61 are axially distributed on the grinding roller 6, and the plurality of air passages 61 are circumferentially staggered on the side wall of the grinding roller 6. A negative pressure pipe 62 is coaxially arranged in the grinding roller 6, and the negative pressure pipe 62 is connected with each of the air passages 61, so that particulate matter generated during the grinding of the defects of the flux spraying on the tin-plated strip can be collected to avoid secondary adhesion.
[0055] In this embodiment, the grinding rollers 6 in the adjacent grinding roller groups 5 are staggered and distributed so as to cover the entire width of the tin-plated strip.
[0056] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A tinned strip production equipment, include: Pre-treatment system, electro-tinning system, soft melting treatment system and post-treatment system, characterized in that the pre-treatment system uses cleaning, chemical degreasing, oil removal and rust removal, pickling and activation to treat the surface of the steel strip, so as to remove grease and oxides on the surface of the steel strip; The electroplating tin system transfers the steel strip to the electroplating tank through the hanger, and deposits tin ions on the surface of the steel strip to form a tin layer during the electroplating process; The post-treatment system uses electrolytic passivation and oiling to treat the surface of the tin-plated strip to prevent rust, so as to enhance the corrosion resistance and brightness of the tin-plated strip; A soft melting treatment system is arranged between the electrotinning system and the post-treatment system, wherein the soft melting treatment system uses a flux to reduce the surface tension of the molten tin during the soft melting of the tin layer on the surface of the tin-plated strip, thereby enhancing the flow and spreading of the tin layer under the heating state; The soft melting treatment system comprises: two conveying rollers (11) distributed, the two conveying rollers (11) being used to roll in or send out the tinned strip, two chokes (12) distributed between the conveying rollers (11), one side of one of the chokes (12) being distributed with a plurality of transfer rollers (13), a soft melting furnace (2) being provided on one side of the transfer roller (13), an extrusion device (14) being provided outside the soft melting furnace (2), and a variable frequency power supply (1) being provided outside the soft melting furnace (2), the variable frequency power supply (1) using a three-phase transformer to provide a heating voltage to the tinned strip; The reflow furnace (2) is provided with three independent hot chambers (21), and a flux coating component (3) is provided in the front independent hot chamber (21), and the flux coating component (3) sprays flux on the front and back sides of the tin-plated strip so that the flux is evenly attached to the tin layer; The flux coating assembly (3) comprises: two tension roller groups (31) distributed on the left and right, a first coating mechanism being arranged between the tension roller groups (31), a flip roller group (32) being arranged outside the tension roller group (31) on the right, the flip roller group (32) flipping the tinned strip over, and a second coating mechanism (4) being arranged outside the flip roller group (32); The first coating mechanism and the second coating mechanism (4) have the same composition structure; The first coating mechanism comprises: an upper rack rod (41) which is horizontally mounted in the soft melting furnace (2) and is located directly above the tinned strip, the upper rack rod (41) is arranged parallel to the tinned strip, and two telescopic racks (42) are arranged below the upper rack rod (41), the two telescopic racks (42) are telescopically adjustable in the vertical direction, and a plurality of spray heads (43) are arranged below the telescopic racks (42) along the width direction of the tinned strip, and each of the spray heads (43) is connected to a delivery pipe for continuously delivering flux; The variable frequency power supply (1) provides heating power to the tinned strip sections in the area below each telescopic frame (42); A front cooling device (44) is arranged between the telescopic frames (42), and the front cooling device (44) contacts the surface of the tinned strip through a plurality of cooling rollers. The front cooling device (44) cools the tinned strip to a temperature of t 2 , so that the flux at t 2 Adhere to the tin layer at low temperature; A rear cooling device is provided between the telescopic frame (42) and the tensioning roller group (31) located at the rear; A visual scanner (45) is provided between the telescopic racks (42) and located on one side of the front cooling device (44). The visual scanner (45) acquires an image of the flux on the tin-plated strip, thereby outputting a coating characteristic image of the flux at each section on the tin-plated strip. A main control module outside the visual scanner (45) evaluates the coating quality of the flux based on the grayscale of the acquired coating characteristic image, and identifies abnormal defects in the coating layer. A grinding roller group (5) is provided on one side of the visual scanner (45), and a plurality of the grinding roller groups (5) are horizontally arranged on the tinned strip.
2. The tin-plated strip production equipment according to claim 1, Features: The variable frequency power supply (1) heats the tinned strip in the area below the telescopic frame (42) to t 1 , flux at t 1 The temperature produces heat melting and covers the tin layer.
3. The tin-plated strip production equipment according to claim 1, Features: The grinding roller group (5) uses a gradient grinding feed rate to reduce the flux on the surface of the tin layer in the tin-plated strip in response to abnormal defects in the coating layer; a plurality of distributed scanners are arranged at intervals between the grinding roller groups (5).
4. The tin-plated strip production equipment according to claim 1, Features: The grinding roller group (5) comprises: a plurality of mounting seats (51) arranged along the width direction of the tin-plated strip, a bottom roller (52) being rotatably arranged at the bottom of each mounting seat (51), a roller frame (53) being vertically slidably connected to the mounting seat (51), a grinding roller (6) being rotatably connected to the roller frame (53), a linear loading portion (54) being fixed to the mounting seat (51), one end of the linear loading portion (54) being fixed to the roller frame (53); The grinding roller (6) rotates in the opposite direction to the transmission direction of the tinned strip during operation; A plurality of air passages (61) are axially distributed on the grinding roller (6), and the plurality of air passages (61) are circumferentially staggered and arranged on the side wall of the grinding roller (6). A negative pressure pipe (62) is coaxially arranged in the grinding roller (6), and the negative pressure pipe (62) is connected to each of the air passages (61).
5. A tin-plated strip production device according to claim 4, Features: The grinding rollers (6) in adjacent grinding roller groups (5) are staggered in distribution.