Memory and method for manufacturing the same

By removing the patterned mask layer and filling the second dielectric layer in the preparation of the three-dimensional phase change memory, the cost increase and grinding problems of the sacrificial layer are solved, and process simplification and cost reduction are achieved.

CN118714854BActive Publication Date: 2024-12-06SHENZHEN HONGQIXIN TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411200954.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-12-06
Estimated Expiration
2044-08-29

AI Technical Summary

Technical Problem

In the preparation of existing three-dimensional phase change memories, it is necessary to add sacrificial layers to protect the memory blocks, resulting in increased costs and problems of chemical mechanical grinding.

Method used

The storage stack array and the first dielectric layer are formed on the substrate, the patterned mask layer is removed, the first conductive layer of the top electrode is formed, and the second dielectric layer is filled in the peripheral area, avoiding the addition of additional sacrificial layers, thereby Simplify the process and reduce costs, solving the grinding problems caused by the sacrificial layer.

Benefits of technology

The process flow is simplified, the cost is reduced, and the problems caused by the sacrificial layer in subsequent chemical mechanical grinding are avoided, improving the reliability of the process and product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118714854B_ABST
    Figure CN118714854B_ABST
Patent Text Reader

Abstract

The present application provides a memory and a method for preparing the same. First, a memory stack array and a first dielectric layer are formed on a substrate. The memory stack array includes memory stacks arranged at intervals and a patterned mask layer located on the side of the memory stack away from the substrate. The first dielectric layer is filled between adjacent memory stacks and in the peripheral area of ​​the memory stack array. Then, the patterned mask layer is removed, and then a first conductive layer covering the top electrode of the memory stack is formed. Finally, the first conductive layer and the first dielectric layer in the peripheral area are removed, and a second dielectric layer is filled in the peripheral area. Therefore, the first conductive layer can protect the first dielectric layer between adjacent memory stacks from being removed, and there is no need to add a sacrificial layer for protection. Therefore, the process can be simplified and the cost can be reduced, and the grinding problem caused by the sacrificial layer for the subsequent CMP process can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application generally relates to the field of electronic devices, and more specifically, to a memory and a method for preparing the same. Background Art

[0002] Semiconductor memory is the foundation of information technology. As a candidate for the next generation of non-volatile semiconductor memory, Phase Change Random Access Memory (PCRAM) has received widespread attention due to its advantages such as high-speed reading, high erasable and write times, non-volatility, small component size, low power consumption, and resistance to strong vibration and radiation.

[0003] The preparation of the existing three-dimensional phase change memory is to first define the storage blocks and the peripheral areas between the storage blocks through an etching process, and then prepare the word lines and word line contacts.

[0004] However, in the etching process for defining the storage block, a sacrificial layer (such as silicon nitride) needs to be added to protect the dielectric layer between the storage stacks in the storage block from being etched. This not only increases the cost, but the sacrificial layer also causes polishing problems for subsequent chemical mechanical polishing (CMP). Summary of the invention

[0005] The purpose of the present application is to provide a memory and a method for preparing the same, aiming to reduce costs and solve the grinding problem caused by the sacrificial layer.

[0006] In a first aspect, the present application provides a method for preparing a memory, comprising:

[0007] A storage stack array and a first dielectric layer are formed on a substrate; the storage stack array comprises storage stacks arranged at intervals and a patterned mask layer located on a side of the storage stack away from the substrate, and the first dielectric layer is filled between adjacent storage stacks and in a peripheral area of ​​the storage stack array;

[0008] removing the patterned mask layer;

[0009] forming a first conductive layer covering a top electrode of the memory stack;

[0010] The first conductive layer and the first dielectric layer in the peripheral area are removed, and a second dielectric layer is filled in the peripheral area.

[0011] In some embodiments, the step of removing the patterned mask layer includes:

[0012] The patterned mask layer and the first dielectric layer are subjected to chemical mechanical polishing to remove the patterned mask layer and a portion of the first dielectric layer.

[0013] In some embodiments, the steps of removing the first conductive layer and the first dielectric layer in the peripheral area to form the peripheral area, and filling the second dielectric layer in the peripheral area include:

[0014] removing the first conductive layer and the first dielectric layer in the peripheral area to form a trench in the peripheral area;

[0015] forming an initial second dielectric layer in the trench and on a side of the first conductive layer away from the storage stack;

[0016] The initial second dielectric layer is subjected to chemical mechanical polishing to form the second dielectric layer, wherein the chemical mechanical polishing stops at a surface of the first conductive layer away from the storage stack.

[0017] In some embodiments, it also includes:

[0018] forming a through hole penetrating the second dielectric layer in the peripheral region;

[0019] A second conductive layer covering the first conductive layer and a conductive contact filling the through hole are formed.

[0020] In some embodiments, it also includes:

[0021] The second conductive layer is etched to form a plurality of second conductive lines parallel to each other, and the first conductive layer is etched to form a plurality of first conductive lines parallel to each other, wherein the first conductive lines correspond to the second conductive lines one by one and are self-aligned with the corresponding second conductive lines.

[0022] In some embodiments, it also includes:

[0023] Using the second conductive line as a mask, etching the storage stack to form a storage unit;

[0024] Wherein, a plurality of the memory cells are arranged in a row along a first direction, and one of the first conductive lines connects the memory cells in one row.

[0025] In some embodiments, the first dielectric layer is a spin-on dielectric layer, and the second dielectric layer is a silicon oxide layer.

[0026] In a second aspect, the present application provides a memory, including:

[0027] A storage unit is located on the substrate;

[0028] A first dielectric layer and a second dielectric layer are located on the substrate, wherein the first dielectric layer is located between adjacent storage units, and the second dielectric layer is located on the first dielectric layer and in the peripheral area of ​​the storage unit;

[0029] A plurality of first conductive lines are located on the first dielectric layer and a side of the memory cells away from the substrate, each of the first conductive lines covering a top electrode of a row or a column of the memory cells;

[0030] A plurality of second conductive lines correspond to the first conductive lines one by one, cover the corresponding first conductive lines and extend to the peripheral area.

[0031] In some embodiments, a surface of the first conductive line away from the substrate is flush with a surface of the second dielectric layer away from the substrate.

[0032] In some embodiments, it also includes:

[0033] A conductive contact is located in the peripheral area and penetrates the second dielectric layer, and the conductive contact is connected to the second conductive line.

[0034] The present application provides a memory and a method for manufacturing the same. First, a memory stack array and a first dielectric layer are formed on a substrate. The memory stack array includes memory stacks arranged at intervals and a patterned mask layer located on a side of the memory stack away from the substrate. The first dielectric layer is filled between adjacent memory stacks and in the peripheral area of ​​the memory stack array. Then, the patterned mask layer is removed, and then a first conductive layer covering the top electrode of the memory stack is formed. Finally, the first conductive layer and the first dielectric layer in the peripheral area are removed, and a second dielectric layer is filled in the peripheral area. The present application first removes the patterned mask layer to expose the top electrode of the memory stack, and then forms a first conductive layer connecting the top electrode, and finally removes the first conductive layer and the first dielectric layer in the peripheral area and fills the second dielectric layer in the peripheral area. Therefore, the first conductive layer can protect the first dielectric layer between adjacent memory stacks from being removed, and there is no need to add a sacrificial layer to protect it. Therefore, the process can be simplified to reduce costs, and the grinding problem caused by the sacrificial layer for the subsequent CMP process can be solved. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] The technical solution and other beneficial effects of the present application will be made apparent by describing in detail the specific implementation methods of the present application in conjunction with the accompanying drawings.

[0036] Figure 1 is a schematic flow chart of a method for preparing a memory provided in some embodiments of the present application;

[0037] Figures 2A-2F is a schematic diagram of the structure of the memory provided in some embodiments of the present application during the preparation process;

[0038] Figure 3 is a schematic flow chart of a method for preparing a memory provided in some embodiments of the present application;

[0039] Figures 4A-4C is a schematic diagram of the structure of the memory provided in some embodiments of the present application during the preparation process;

[0040] Figure 5 It is a schematic diagram of the structure of the storage system provided in some embodiments of the present application. DETAILED DESCRIPTION

[0041] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0042] It should be understood that although the terms first, second, etc. may be used herein to describe various components, these components should not be limited to these terms. These terms are used to distinguish one component from another component. For example, a first component may be referred to as a second component, and similarly, a second component may be referred to as a first component without departing from the scope of the present application.

[0043] It should be understood that when a component is said to be "on" or "connected" another component, it can be directly on or connected to another component, or there may be an intervening component. Other words used to describe the relationship between components should be interpreted in a similar manner.

[0044] As used herein, the term "layer" refers to a portion of a material including an area having a thickness. A layer may extend over the entire underlying or superstructure, or may have an extent that is less than the extent of the underlying or superstructure. In addition, a layer may be an area of ​​a uniform or non-uniform continuous structure having a thickness that is less than the thickness of a continuous structure. For example, a layer may be located between the top and bottom surfaces of a continuous structure or between any set of horizontal planes at the top and bottom surfaces. A layer may extend horizontally, vertically and / or along a tapered surface. A substrate may be a layer, which may include one or more layers, and / or may have one or more layers on, above and / or below it. A layer may include multiple layers. For example, an interconnect layer may include one or more conductive layers and a contact layer and one or more dielectric layers.

[0045] It should be noted that the illustrations provided in the embodiments of the present application are only used to illustrate the basic concept of the present application in a schematic manner. Although the illustrations only show components related to the present application and are not drawn according to the number, shape and size of components in actual implementation, the type, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.

[0046] This article uses Cartesian coordinates to represent directions, with the base as the reference, "Y" represents the first direction, which is parallel to the base; "X" represents the second direction parallel to the base; and "Z" represents the direction perpendicular to the base.

[0047] See also Figure 1 , Figure 1 is a flow chart of a method for preparing a memory provided in some embodiments of the present application. Figures 2A-2F , Figures 2A-2F It is a schematic diagram of the structure of the memory provided in some embodiments of the present application during the preparation process.

[0048] The method for preparing the memory includes the following steps S1-S4.

[0049] Step S1: forming a storage stack array 10 and a first dielectric layer 40b on a substrate; the storage stack array 10 includes spaced storage stacks 11 and a patterned mask layer 30 located on a side of the storage stack 11 away from the substrate 20, and the first dielectric layer 40b is filled between adjacent storage stacks 11 and in a peripheral area P of the storage stack array 10.

[0050] See also Figure 2A First, a base 20 is formed. The base 20 may include a substrate 21 and a control circuit layer 22 located on the substrate 21 . Then, a storage stack array 10 is formed on the control circuit layer 22 .

[0051] like Figure 2A-2B As shown, the steps of forming the memory stack array 10 and the first dielectric layer 40b may include the following steps.

[0052] 1) An initial storage stack and a mask layer are sequentially formed on one side of the substrate 20. Specifically, a bottom electrode 101, a storage material layer and a top electrode 102 may be sequentially formed on the control circuit layer 22 to form an initial storage stack, and then a mask layer is formed on the initial storage stack, and the material of the mask layer may include silicon nitride.

[0053] In some embodiments, the storage material layer may include a gating layer. In other embodiments, such as Figure 2A As shown, the storage material layer may include a gate layer 103 , an intermediate electrode 104 and a phase change layer 105 , wherein the intermediate electrode 104 is located between the phase change layer 105 and the gate layer 103 .

[0054] In some embodiments, the substrate 20 may be a semiconductor substrate, such as silicon (Si), germanium (Ge), SiGe, silicon on insulator (SOI) or germanium on insulator (GOI). The materials of the bottom electrode 101, the middle electrode 104 and the top electrode 102 may be the same, and may include carbon. The material of the gate layer 103 may include Zn x Te y ,Ge x Te y , Nb x O y 、Si x As y 、As x Te y Etc. The material of the phase change layer 105 may include, for example, a chalcogenide-based material including any one of four elements of oxygen (O), sulfur (S), selenium (Se), and tellurium (Te) forming Group VIA of the periodic table.

[0055] In some embodiments, the control circuit layer 22 may include a complementary metal oxide semiconductor (CMOS).

[0056] In some embodiments, an initial memory stack composed of different materials may be formed according to the type of memory, and the present application is not limited in this regard.

[0057] 2) Etching the mask layer and the initial storage stack to form a patterned mask layer 30 and a storage stack 11 , wherein the patterned mask layer 30 is located on a side of the storage stack 11 away from the substrate 20 .

[0058] Specifically, the mask layer can be etched using a mask plate to form a patterned mask layer 30, and then the initial storage stack is etched using the patterned mask layer 30 as a mask to form a storage stack 11 located below the patterned mask layer 30. The patterned mask layer 30 and the storage stack 11 are collectively referred to as a storage stack array 10. Figure 2A As shown, the storage stack 11 may extend along a second direction X, and the second direction X is a direction parallel to the substrate 20. The etching process may adopt a self-aligned double patterning (SADP) process.

[0059] Before forming the initial storage stack, a bit line layer may be formed on the control circuit layer 22. During etching of the initial storage stack, the bit line layer may be etched to form a bit line BL located below the storage stack 11. The bit line BL extends along the second direction X.

[0060] 3) A first dielectric layer 40 b is formed between adjacent storage stacks 11 and around the periphery of the storage stack array 10 .

[0061] Specific examples, such as Figure 2A As shown, an initial first dielectric layer 40 ba is first formed between adjacent storage stacks 11 and around the periphery of the storage stack array 10 . The initial first dielectric layer 40 ba is also formed between adjacent patterned mask layers 30 .

[0062] Step S2: removing the patterned mask layer 30 .

[0063] like Figure 2B As shown, the patterned mask layer 30 and the initial first dielectric layer 40ba can be subjected to a chemical mechanical polishing process to remove the patterned mask layer 30 and form a first dielectric layer 40b. The chemical mechanical polishing process stops at the surface of the storage stack 11, so that the top electrode 102 of the storage stack 11 can be exposed.

[0064] In some embodiments, the initial first dielectric layer 40 ba (or the first dielectric layer 40 b ) is a spin-on dielectric layer (Spin On Dielectrics, SOD), for example, an isolation material is formed between adjacent memory stacks 11 and around the periphery of the memory stack array 10 by spin coating.

[0065] Step S3 : forming a first conductive layer 50 a covering the top electrode 102 of the storage stack 11 .

[0066] Specific examples, such as Figure 2C As shown, tungsten can be directly deposited on the upper surface of the storage stack 11 and the first dielectric layer 40b to form the first conductive layer 50a. The deposition process can be, but is not limited to, chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD) such as thermal oxidation, evaporation, sputtering and other methods.

[0067] Step S4: removing the first conductive layer 50 a and the first dielectric layer 40 b in the peripheral region P, and filling the peripheral region P with a second dielectric layer 60 .

[0068] Specific examples, such as Figure 2D As shown, the first conductive layer 50a and the first dielectric layer 40b in the peripheral region P are removed to form a groove in the peripheral region P, and the remaining portion of the first conductive layer 50a becomes the first conductive layer 50, and the remaining portion of the first dielectric layer 40b becomes the first dielectric layer 40. Figure 2E As shown, an initial second dielectric layer 60a is formed in the groove and on the side of the first conductive layer 50 away from the storage stack 11; Figure 2F As shown, the initial second dielectric layer 60a is subjected to a chemical mechanical polishing process to form the second dielectric layer 60 , and the chemical mechanical polishing process stops at the surface of the first conductive layer 50 away from the storage stack 11 , so that the upper surface of the first conductive layer 50 is flush with the upper surface of the second dielectric layer 60 .

[0069] In some embodiments, the material of the second dielectric layer 60 is different from the material of the first dielectric layer 40 , and the second dielectric layer 60 is a silicon oxide layer.

[0070] In some embodiments, the peripheral region P may be arranged around a storage stack array 10, and a storage stack array 10 is a storage block, and adjacent storage blocks are separated by the second dielectric layer 60 of the peripheral region P. It can be understood that the step of forming the groove or the peripheral region P is actually the step of dividing the storage block, and the step of forming the second dielectric layer 60 is actually the step of isolating the storage block.

[0071] In some embodiments, a dummy storage stack may be present at the periphery of the storage stack array 10 (or between adjacent storage stack arrays 10), and the provision of the dummy storage stack may average the stress of the overall structure. In the step of removing the first conductive layer 50a and the first dielectric layer 40b at the periphery of the storage stack array 10, the dummy storage stack may be removed together, thereby forming a blank peripheral area, which is then filled with the second dielectric layer.

[0072] It should be noted that in some preparation methods, Figure 2AOn the basis of the structure shown, instead of sequentially performing step S3 and step S4, a thin sacrificial layer (e.g., silicon nitride) is covered on the patterned mask layer 30 and the initial first dielectric layer 40a, and then the initial first dielectric layer 40a at the periphery of the storage stack array 10 is removed, and a second dielectric layer (e.g., silicon oxide) is filled at the position, so that a peripheral area located at the periphery of the storage stack array 10 is formed, and the storage stack array surrounded by the second dielectric layer (or peripheral area) is a storage block. Then, a word line contact (including a tungsten deposition process and a CMP process) can be formed in the second dielectric layer in the peripheral area. At this time, the CMP process needs to stop on the sacrificial layer, but because the selectivity ratio of tungsten to silicon nitride is close to 1:1, the problem of over-grinding of silicon nitride will occur, and it is even possible to grind off a portion of the patterned mask layer 30 above the storage stack 11, and it is also possible to grind off the top of the storage stack 11, which not only affects the device reliability and product yield, but also has a great impact on the downstream process. Finally, after forming the word line contacts, the first conductive layer is formed, and the patterned mask layer 30 needs to be removed by a CMP process. The CMP process here involves the word line contacts (tungsten), the second dielectric layer (silicon oxide), the first dielectric layer (SOD), and the patterned mask layer 30 (silicon nitride), and these materials need to have special requirements for the polishing rate selection ratio with the top electrode 102. Involving too many materials will greatly increase the difficulty of the process, easily cause defects in various areas, and affect the uniformity of the top electrode 102.

[0073] In the method for preparing the memory provided in the embodiment of the present application, step S3 is performed after step S2, and then step S4 is performed, that is, after the top electrode 102 of the storage stack 11 is exposed, the first conductive layer 50 is first formed, and then the peripheral area P is formed. In this way, the first conductive layer 50 can protect the first dielectric layer 40 between adjacent storage stacks 11 from being removed, and there is no need to add a sacrificial layer to etch to form the peripheral area P, which can simplify the process and reduce costs, and also solves (or does not exist) the problem of excessive grinding of the sacrificial layer in some preparation methods.

[0074] In this embodiment of the present application, a CMP process is performed in step S2 (see Figure 2B ), the patterned mask layer 30 on the storage stack 11 is removed to expose the top electrode 102. This CMP process only involves the initial first dielectric layer 40a (SOD) and the patterned mask layer (silicon nitride). Compared with the four film layers involved in the CMP process for exposing the top electrode 102 in some preparation methods, the CMP process of the present application is easier to control, can reduce defects, reduce process difficulty, and improve the uniformity of the top electrode 102.

[0075] See also Figure 3 , Figure 3is a flow chart of a method for preparing a memory provided in some embodiments of the present application. Please also refer to Figures 4A-4C , Figures 4A-4C 1 is a schematic diagram of the structure of the memory provided in some embodiments of the present application during the preparation process. For ease of understanding and brief description, the same reference numerals are used for the same structures in this embodiment as in the above embodiment, and the same structures are not described in detail. Only the different structures are described in detail in this embodiment.

[0076] The method for preparing the memory includes steps S1-S7, wherein steps S1-S4 can refer to the above description, and this embodiment focuses on steps S5-S7.

[0077] Step S5: forming a through hole V in the peripheral region P penetrating the second dielectric layer 60 .

[0078] See also Figure 4A , a through hole V can be formed in the second dielectric layer 60 in the peripheral area P by an etching process.

[0079] Step S6 : forming a second conductive layer 52 covering the first conductive layer 50 and a conductive contact CT filling the through hole V.

[0080] See also Figure 4B Tungsten can be deposited in the through hole V, on the first conductive layer 50 and on the second dielectric layer 60, so as to form a conductive contact CT in the through hole V, and the second conductive layer 52 connects the first conductive layer 50 and the conductive contact CT.

[0081] Step S7: performing a chemical mechanical polishing process on the second conductive layer 52 .

[0082] Specifically, the second conductive layer 52 is subjected to CMP to reduce the thickness of the second conductive layer 52. When the second conductive layer 52 is subsequently used as a word line, it is equivalent to reducing the thickness of the word line and improving the flatness of the word line, so that the electrical performance of the word line meets the requirements.

[0083] Step S8: Etching the second conductive layer 52 to form a plurality of second conductive lines 52a parallel to each other, and etching the first conductive layer 50 to form a plurality of first conductive lines 50a parallel to each other, wherein the first conductive lines 50a correspond one-to-one to the second conductive lines 52a and are self-aligned with the corresponding second conductive lines 52a.

[0084] See also Figure 4CThe etching of the second conductive layer 52 and the first conductive layer 50 can be completed in one etching process, and the second conductive layer 52 is etched to form a plurality of second conductive lines 52a, and the first conductive layer 50 is etched to form a plurality of first conductive lines 50a. The first conductive lines 50a and the second conductive lines 52a can both extend along the first direction Y.

[0085] In some embodiments, after forming the first conductive line 50a, the method for manufacturing the memory may further include: etching the memory stack 11 using the second conductive line 52a as a mask to form a memory cell C.

[0086] The memory cells C are distributed in an array along the first direction Y and the second direction X, and a plurality of the memory cells C are arranged in a row along the first direction Y, and one first conductive line 50a connects the memory cells C in a row. Therefore, the memory cell C is located at the intersection of the first conductive line 50a and the bit line BL, and the control signal is transmitted from the conductive contact CT to the memory cell C through the second conductive line 52a and the first conductive line 50a. Since the thickness of the conductive line increases and the resistance decreases after the control signal reaches the top of the memory cell C, the voltage drop decreases.

[0087] The preparation method of the memory provided in the embodiment of the present application optimizes the process sequence and specific steps, that is, after the top electrode 102 of the storage stack 11 is exposed, the first conductive layer 50 is formed first, and then the peripheral area P is formed, so that the first conductive layer 50 can protect the first dielectric layer 40 between the adjacent storage stacks 11 from being removed, and there is no need to add a sacrificial layer to etch and form the peripheral area P, which can simplify the process and reduce costs, and also solve (or do not exist) the problem of excessive grinding of the sacrificial layer in some preparation methods. In addition, the conductive contact CT is finally formed, which can increase the thickness of the conductive line above the storage stack 11 and reduce the resistance, and the final tungsten CMP process only involves tungsten, and the process difficulty is greatly reduced. Furthermore, in the preparation method provided in the embodiment of the present application, the CMP process for removing the patterned mask layer 30 on the storage stack 11 to expose the top electrode 102 only involves the initial first dielectric layer 40a (SOD) and the patterned mask layer 30 (silicon nitride). Compared with the four film layers involved in the CMP process for exposing the top electrode 102 in some preparation methods, the process is easier to control, which can reduce defects, reduce process difficulty, and improve the uniformity of the top electrode 102.

[0088] An embodiment of the present application also provides a memory, which can be prepared by the preparation method provided by any of the above embodiments.

[0089] See also Figure 4B and Figure 4CThe memory 100 includes a memory cell C, a first dielectric layer 40 and a second dielectric layer 60, a plurality of first conductive lines 50a and a plurality of second conductive lines 52a. The memory cell C is located on a substrate 20, the first dielectric layer 40 and the second dielectric layer 60 are located on the substrate 20, and the first dielectric layer 40 is located between the adjacent memory cells C, and the second dielectric layer 60 is located on the first dielectric layer 40 and in a peripheral region P of the memory cell C. The plurality of first conductive lines 50a are located on the first dielectric layer 40 and the side of the memory cell C away from the substrate 20, and each of the first conductive lines 50a covers the top electrodes 102 of a row or a column of the memory cells C. The plurality of second conductive lines 52a correspond to the first conductive lines 50a one by one, cover the corresponding first conductive lines 50a, and extend to the peripheral region P.

[0090] In some embodiments, the memory 100 further includes a bit line BL extending along the second direction X. The memory cell C is located between the bit line BL and the first conductive line 50 a , and the first conductive line 50 a is disposed at the intersection of the bit line BL and the word line.

[0091] In some embodiments, the peripheral region P is disposed around the periphery of the plurality of memory cells C.

[0092] In some embodiments, the base 20 includes a substrate 21 and a control circuit layer 22 , and the control circuit layer 22 is located between the bit line BL and the substrate 21 .

[0093] In some embodiments, a surface of the first conductive line 50 a away from the substrate 20 is flush with a surface of the second dielectric layer 60 away from the substrate.

[0094] In some embodiments, the memory 100 further includes a conductive contact CT, which is disposed in the peripheral region P and penetrates the second dielectric layer 60 , and the conductive contact CT is connected to the second conductive line 52 a .

[0095] In the memory 100 provided in the embodiment of the present application, since the thickness H1 of the conductive line on the memory cell C is greater than the thickness H2 of the conductive line in the peripheral area P (such as Figure 4B As shown), the resistance can be reduced, thereby reducing the voltage drop.

[0096] See also Figure 5 , Figure 5 2 is a schematic diagram of a storage system provided in some embodiments of the present application. The storage system 200 includes a memory 201 and a controller 202. The memory 201 may be a memory in any of the above embodiments. The controller 202 is connected to the memory 201 and is used to control the memory 201 to store data. The memory 201 may perform an operation of storing data based on the control of the controller 202.

[0097] In some embodiments, the storage system may be implemented as a storage device such as a universal flash storage (UFS) device, a solid state drive (SSD), a multimedia card in the form of MMC, eMMC, RS-MMC and micro MMC, a secure digital card in the form of SD, mini SD and micro SD, a Personal Computer Memory Card International Association (PCMCIA) card type storage device, a peripheral component interconnect (PCI) type storage device, a high-speed PCI (PCI-E) type storage device, a compact flash (CF) card, a smart media card or a memory stick, etc.

[0098] The memory 201 includes: a storage unit located on a substrate; a first dielectric layer and a second dielectric layer located on the substrate, wherein the first dielectric layer is located between adjacent storage units, and the second dielectric layer is located on the first dielectric layer and in a peripheral area of ​​the storage unit; a plurality of first conductive lines located on the first dielectric layer and on a side of the storage unit away from the substrate, wherein each of the first conductive lines covers a top electrode of a row or a column of the storage units; and a plurality of second conductive lines corresponding to the first conductive lines one by one, covering corresponding first conductive lines and extending to the peripheral area.

[0099] The description of the above embodiments is only used to help understand the technical solutions and core ideas of the present application. Ordinary technical personnel in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. A method for preparing a memory, characterized in that: include: forming a storage stack array and a first dielectric layer on a substrate; The storage stack array includes storage stacks arranged at intervals and a patterned mask layer located on a side of the storage stack away from the substrate, and the first dielectric layer is filled between adjacent storage stacks and in a peripheral area of ​​the storage stack array; removing the patterned mask layer; forming a first conductive layer covering a top electrode of the memory stack; The first conductive layer and the first dielectric layer in the peripheral area are removed, and a second dielectric layer is filled in the peripheral area.

2. The method for preparing a memory according to claim 1, characterized in that: The step of removing the patterned mask layer comprises: The patterned mask layer and the first dielectric layer are subjected to chemical mechanical polishing to remove the patterned mask layer and a portion of the first dielectric layer.

3. The method for preparing a memory according to claim 1, characterized in that: The steps of removing the first conductive layer and the first dielectric layer in the peripheral area to form the peripheral area, and filling the second dielectric layer in the peripheral area include: removing the first conductive layer and the first dielectric layer in the peripheral area to form a trench in the peripheral area; forming an initial second dielectric layer in the trench and on a side of the first conductive layer away from the storage stack; The initial second dielectric layer is subjected to chemical mechanical polishing to form the second dielectric layer, wherein the chemical mechanical polishing stops at a surface of the first conductive layer away from the storage stack.

4. The method for preparing a memory according to claim 1, characterized in that: Also includes: forming a through hole penetrating the second dielectric layer in the peripheral region; A second conductive layer covering the first conductive layer and a conductive contact filling the through hole are formed.

5. The method for preparing a memory according to claim 4, characterized in that: Also includes: The second conductive layer is etched to form a plurality of second conductive lines parallel to each other, and the first conductive layer is etched to form a plurality of first conductive lines parallel to each other, wherein the first conductive lines correspond to the second conductive lines one by one and are self-aligned with the corresponding second conductive lines.

6. The method for preparing a memory according to claim 5, characterized in that: Also includes: Using the second conductive line as a mask, etching the storage stack to form a storage unit; Wherein, a plurality of the memory cells are arranged in a row along a first direction, and one of the first conductive lines connects the memory cells in one row.

7. The method for preparing a memory according to claim 1, characterized in that: The first dielectric layer is a spin-coated dielectric layer, and the second dielectric layer is a silicon oxide layer.

8. A memory, characterized in that: include: A storage unit is located on the substrate; A first dielectric layer and a second dielectric layer are located on the substrate, wherein the first dielectric layer is located between adjacent storage units, and the second dielectric layer is located in a peripheral area of ​​the storage unit; A plurality of first conductive lines are located on the first dielectric layer and a side of the memory cells away from the substrate, each of the first conductive lines covering a top electrode of a row or a column of the memory cells; A plurality of second conductive lines correspond one-to-one to the plurality of first conductive lines, and the first conductive lines are self-aligned with the corresponding second conductive lines, and the second conductive lines cover the corresponding first conductive lines and extend to the peripheral area.

9. The memory according to claim 8, characterized in that: A surface of the first conductive line away from the substrate is flush with a surface of the second dielectric layer away from the substrate.

10. The memory according to claim 8, characterized in that: Also includes: A conductive contact is located in the peripheral area and penetrates the second dielectric layer, and the conductive contact is connected to the second conductive line.