Aerosol generating device, preparation method thereof and aerosol generating system
By coating the hollow device of the aerosol generating device with porous particulate materials and loading amino acids and polyethylene glycol, the problem of high glycidol release in heat-not-burn cigarettes is solved, and the safety and quality of smoke are significantly improved.
Patent Information
- Application Number
- CN202411123895.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-10-01
AI Technical Summary
Heat-not-burn cigarette devices release a high amount of harmful substances called glycidol during the heating process, which affects smoke quality.
The porous particulate material is coated in the hollow device of the aerosol generating device to form a composite layer, and amino acids and polyethylene glycol are loaded in the porous particulate material to enhance the physical adsorption and chemical adsorption capacity of glycidol.
It effectively reduces the amount of glycidol released in the aerosol generated by the heat-not-burn cigarette device, and improves the safety and quality of smoke.
Smart Images

Figure CN118716685A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of aerosol generating devices, and in particular to an aerosol generating device and a preparation method thereof, and an aerosol generating system. Background Art
[0002] An aerosol generator is a device that converts liquid or solid substances into aerosols. Heat-not-burn cigarettes are a special type of aerosol generator that produces aerosols by heating tobacco rather than burning it, thus simulating the experience of traditional cigarettes.
[0003] Heat-not-burn (HTB) cigarettes typically heat at temperatures between 200°C and 400°C, far lower than the combustion temperature of traditional cigarettes. This significantly reduces the harmful components produced by heating, leading to their rapid growth. While HNB cigarettes release fewer harmful substances overall than traditional cigarettes, the high concentration of glycerin in their raw materials, a smoking agent, produces harmful substances such as glycidol (propylene oxide) when heated.
[0004] Therefore, it is necessary to improve the traditional technology to reduce the release of glycidol in the aerosol generated by aerosol generating devices such as heat-not-burn cigarettes. Summary of the Invention
[0005] Based on this, one or more embodiments of the present application provide an aerosol generating device and a preparation method thereof, and an aerosol generating system that can reduce the amount of glycidol released.
[0006] According to a first aspect of an embodiment of the present application, an aerosol generating device is provided, comprising a filter, a hollow device, and an aerosol matrix connected in sequence; the hollow device comprises a hollow matrix and a composite layer, the composite layer being located on at least a portion of an inner wall of the hollow matrix;
[0007] Components of the composite layer include composite particles, which include porous particle materials, amino acids loaded on the porous particle materials, and polyethylene glycol loaded on the porous particle materials.
[0008] In one embodiment, a wrapping material is further included, and the wrapping material is wrapped around the outer sides of the filter body, the hollow device and the aerosol matrix which are connected in sequence.
[0009] In one embodiment, the composite layer includes a plurality of strip-shaped regions disposed at intervals, and the composite particles are located in the strip-shaped regions.
[0010] In one embodiment, the loading amount of the polyethylene glycol is 5 wt % to 30 wt % based on the weight of the composite particles.
[0011] In one embodiment, the average molecular weight of the polyethylene glycol is 1000-10000.
[0012] In one embodiment, the loading amount of the amino acid is 1 wt% to 10 wt% based on the weight of the composite particles.
[0013] In one embodiment, the amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
[0014] In one embodiment, the porous particulate material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves.
[0015] In one embodiment, the natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
[0016] In one embodiment, the particle size of the porous granular material is 0.045 mm to 0.425 mm.
[0017] In one embodiment, the porous granular material includes first particles and second particles, the particle size of the first particles is 0.045 mm to 0.15 mm, and the particle size of the second particles is 0.25 mm to 0.425 mm;
[0018] Based on the total weight of the porous granular material, the mass ratio of the first particles is 50 wt % to 90 wt %, and the mass ratio of the second particles is 10 wt % to 50 wt %.
[0019] In one embodiment, in the composite layer, the coating amount of the composite particles is 10 g / m 2 ~60g / m 2 .
[0020] In one embodiment, the components of the composite layer further include a binder mixed with the composite particles.
[0021] In one embodiment, the binder is selected from at least one of gums, cellulose binders, polysaccharides, organic acids and conjugate base salts of organic acids.
[0022] In one embodiment, the amount of the binder added is 0.05 wt % to 10 wt % based on the mass of the composite particles.
[0023] According to a second aspect of an embodiment of the present application, a method for preparing the above-mentioned aerosol generating device is provided, comprising the following steps:
[0024] mixing the composite particles and a solvent to prepare a composite slurry;
[0025] Applying the composite slurry to at least a portion of a surface of a hollow base material and drying the slurry to form a composite layer;
[0026] rolling the hollow base film with the side on which the composite layer is formed as the inner side to obtain the hollow device; and
[0027] The filter body, the hollow device and the aerosol matrix are connected in sequence to prepare the aerosol generating device.
[0028] In one embodiment, the method for preparing the composite particles comprises the following steps:
[0029] The amino acid, polyethylene glycol and porous particle material are mixed and dried to prepare the composite particles.
[0030] According to a third aspect of an embodiment of the present application, an aerosol generating system is provided, comprising the above-mentioned aerosol generating device and a heating device.
[0031] In one embodiment, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.
[0032] Compared with traditional technologies, this application has the following beneficial effects:
[0033] The present application forms a composite layer on the inner wall of the hollow device by coating a porous granular material in the hollow device, thereby increasing the residence time of the aerosol matrix in the hollow device and improving the smoke temperature cooling effect; and loads amino acids and polyethylene glycol in the porous granular material. Both amino acids and polyethylene glycol can physically and chemically adsorb harmful substances such as glycidol, thereby reducing the release of harmful substances in the aerosol generated by aerosol generating devices such as heat-not-burn cigarettes. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the following is a brief introduction to the drawings required for use in the specific implementation methods or the description of the prior art. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without any creative work.
[0035] Figure 1 This is a schematic structural diagram of an aerosol generating device prepared in one embodiment of the present application;
[0036] Figure 2 This is a schematic cross-sectional structural diagram of a hollow device according to one embodiment of the present application;
[0037] Figure 3 Schematic diagram of a coating method of a composite layer according to one embodiment of the present application.
[0038] Explanation of reference numerals: 10, aerosol matrix; 20, hollow device; 21, hollow base; 22, composite layer; 30, filter body; 40, wrapping material. DETAILED DESCRIPTION
[0039] In order to make the above-mentioned objects, features and advantages of the present application more clearly understood, the specific embodiments of the present application are described in detail. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways than those described herein, and those skilled in the art can make similar improvements without violating the connotations of the present application. Therefore, the present application is not limited to the specific embodiments disclosed below.
[0040] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art in the technical field of this application. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. Unless otherwise specified, the various raw materials, reagents, instruments and equipment used in this application can be purchased from the market or can be prepared by existing methods.
[0041] Some embodiments of the present application provide an aerosol generating device.
[0042] See also Figure 1 The aerosol generating device includes a filter body 30, a hollow device 20 and an aerosol matrix 21 connected in sequence; the hollow device 20 includes a hollow matrix 21 and a composite layer 22, and the composite layer 22 is located on at least a portion of the inner wall of the hollow matrix 21;
[0043] The components of the composite layer 22 include composite particles, which include a porous particle material, amino acids supported on the porous particle material, and polyethylene glycol supported on the porous particle material.
[0044] It can be understood that the surface of the composite layer containing composite particles is uneven, and the uneven surface will cause turbulence in the aerosol flowing through the hollow device 20, increase the flow route, and correspondingly increase the residence time.
[0045] It can be understood that amino acids include amino acids loaded inside and / or on the surface of porous particle materials; polyethylene glycol includes polyethylene glycol loaded inside and / or on the surface of porous particle materials.
[0046] It is understandable that the aerosol generating device of the present application may be a heat-not-burn cigarette, but is not limited thereto.
[0047] See also Figure 2 The hollow device 20 is a device having a hollow structure in the middle. The shape of the hollow device 20 includes but is not limited to a cylindrical shape. In this specific example, the hollow device 20 includes a hollow base 21 and a composite layer 22 provided on the inner wall of the hollow base 21.
[0048] Understandably, if Figure 3 As shown in FIG. 1A , the composite layer 22 may be provided on the entire inner wall of the hollow substrate 21 ; Figure 3 As shown in FIG. B, it can also be provided on a part of the inner wall of the hollow substrate 21, for example, to form a specific pattern. Figure 3 In the specific example of B, the composite layer 22 includes a plurality of strip-shaped regions arranged at intervals, and the composite particles are located in the strip-shaped regions.
[0049] Furthermore, the extension direction of the strip area intersects with the axial direction of the hollow matrix 21, and the angle of intersection can be >0 and ≤90°. Further, it can be 30°, 45°, 60°, 90° or within the range formed by any two of the above point values. In this specific example, the angle of intersection is 45°. Compared with the setting in which the extension direction of the strip area is parallel to the axial direction of the hollow matrix 21, the convexity and concavity of the composite layer are further increased, thereby increasing the contact time and contact area between the composite layer 22 and the aerosol, thereby improving the adsorption efficiency of harmful substances.
[0050] In some embodiments, the aerosol generating device further includes a wrapping material 40 , which wraps the outer sides of the filter 30 , the hollow device 20 , and the aerosol matrix 10 , which are connected in sequence.
[0051] In some embodiments, the wrapping material 50 is selected from cigarette paper.
[0052] The composite coating 21 provided within the hollow device of an aerosol generating device enhances the physical and chemical adsorption of harmful substances such as glycidol, thereby reducing their release into cigarette aerosols and improving safety. The porous granular material forms protrusions within the hollow device. When smoke generated by the aerosol matrix passes through the hollow device, the smoke is adsorbed and trapped by the protrusions, increasing the smoke's residence time within the hollow device and thereby reducing the smoke temperature. The amino acids and polyethylene glycol loaded within the porous granular material can adsorb smoke generated by the aerosol matrix, thereby reducing its release.
[0053] In some embodiments, the polyethylene glycol loading is 5 wt % to 30 wt % based on the weight of the composite particles, for example, 5 wt %, 6 wt %, 7 wt %, 8 wt %, 9 wt %, 10 wt %, 11 wt %, 12 wt %, 13 wt %, 14 wt %, 15 wt %, 16 wt %, 17 wt %, 18 wt %, 19 wt %, 20 wt %, 21 wt %, 22 wt %, 23 wt %, 24 wt %, 25 wt %, 26 wt %, 27 wt %, 28 wt %, 29 wt %, or 30 wt %.
[0054] In some optional examples, the loading amount of polyethylene glycol is 10 wt % to 20 wt %.
[0055] In some optional examples, the loading amount of polyethylene glycol is 10 wt % to 15 wt %.
[0056] In some embodiments, the average molecular weight of polyethylene glycol is 1000 to 10000, for example, 1000, 2000, 3000, 4000, 5000, 6000, 7000, 8000, 9000 or 10000.
[0057] In some optional examples, the loading amount of polyethylene glycol is 4000-8000.
[0058] In some optional examples, the loading amount of polyethylene glycol is 6000-8000.
[0059] In some embodiments, the amino acid loading is 1 wt % to 10 wt % based on the weight of the composite particle, for example, 1 wt %, 1.5 wt %, 2 wt %, 2.5 wt %, 3 wt %, 3.5 wt %, 4 wt %, 4.5 wt %, 5 wt %, 5.5 wt %, 6 wt %, 6.5 wt %, 7 wt %, 7.5 wt %, 8 wt %, 8.5 wt %, 9 wt %, 9.5 wt %, or 10 wt %.
[0060] In some optional examples, the loading amount of amino acids is 2 wt% to 8 wt%.
[0061] In some optional examples, the loading amount of amino acids is 3 wt% to 6 wt%.
[0062] In some embodiments, the amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
[0063] In some optional examples, the amino acid is selected from at least one of lysine, threonine, methionine, and arginine.
[0064] In some alternative examples, the amino acid is selected from lysine and threonine.
[0065] In some optional examples, the weight ratio of lysine to threonine is (1-3):(1-3). For example, it can be 1:1, 1:2, 1:3, 2:1, 2:3, 3:1, or 3:2. It is understood that when lysine and threonine are mixed in the above specific ratios, the synergistic effect of the two can further enhance the adsorption of harmful substances.
[0066] Understandably, by loading amino acids in the porous particulate material, the amino acids can physically and chemically adsorb harmful substances such as glycidol, thereby reducing the release of harmful substances in the heat-not-burn cigarette aerosol.
[0067] In some embodiments, the porous particulate material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon, and molecular sieves.
[0068] In some specific examples, the natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite, and kaolin; the metal oxide includes calcium oxide; the hydroxide includes calcium hydroxide; the carbonate includes calcium carbonate; and the sulfate includes calcium sulfate.
[0069] In some optional examples, the porous particulate material is selected from activated carbon or diatomaceous earth.
[0070] In some embodiments, the particle size of the porous particulate material is 0.045 mm to 0.425 mm. For example, it can be 0.045 mm, 0.055 mm, 0.065 mm, 0.075 mm, 0.085 mm, 0.095 mm, 0.10 mm, 0.11 mm, 0.12 mm, 0.13 mm, 0.14 mm, 0.15 mm, 0.16 mm, 0.17 mm, 0.18 mm, 0.19 mm, 0.20 mm, 0.21 mm, 0.22 mm, 0. 23mm, 0.24mm, 0.25mm, 0.26mm, 0.27mm, 0.28mm, 0.29mm, 0.30mm, 0.31mm, 0.32mm, 0.33mm, 0.34mm, 0.35mm, 0.36mm, 0.37mm, 0.38mm, 0.39mm, 0.40mm, 0.41mm, 0.42mm or 0.425mm.
[0071] In some optional examples, the porous granular material may include first particles with a particle size of 0.045 mm to 0.15 mm and second particles with a particle size of 0.25 mm to 0.425 mm.
[0072] In some optional examples, the porous granular material includes first particles and second particles; based on the total weight of the porous granular material, the mass ratio of the first particles is 50 wt% to 90 wt%, and the mass ratio of the second particles is 10 wt% to 50 wt%. Further optionally, the mass ratio of the first particles is 60 wt% to 80 wt%, and the mass ratio of the second particles is 20 wt% to 40 wt%.
[0073] In some embodiments, in the composite layer, the coating amount of the composite particles is 10 g / m 2 ~60g / m 2 . For example, it can be 10g / m 2 , 11g / m 2 , 12g / m 2 , 13g / m 2 , 14g / m 2 , 15g / m 2 , 16g / m 2 , 17g / m 2 , 18g / m 2 , 19g / m 2 , 20g / m 2 , 25g / m 2 , 30g / m 2 , 35g / m 2 , 40g / m 2 , 45g / m 2 , 50g / m 2 , 55g / m 2 or 60g / m 2 .
[0074] It should be noted that, unless otherwise specified, the coating amount of the composite particles in this application is calculated based on the total area of the composite layer, that is, based on the entire inner wall area of the hollow substrate.
[0075] In some optional examples, the coating amount of the composite particles is 15 g / m 2 ~50g / m 2 .
[0076] In some optional examples, the coating amount of the composite particles is 20 g / m 2 ~40g / m 2 .
[0077] In some embodiments, the components of the composite layer further include a binder intermixed with the composite particles.
[0078] In some embodiments, the binder is selected from at least one of a gum, a cellulose binder, a polysaccharide, an organic acid, and a conjugate base salt of an organic acid.
[0079] In some specific examples, the gum is selected from at least one of guar gum, xanthan gum, gum arabic and locust bean gum; the cellulose binder is selected from at least one of hydroxypropyl cellulose, carboxymethyl cellulose, hydroxyethyl cellulose, methyl cellulose and ethyl cellulose; the polysaccharide is selected from starch; the organic acid is selected from alginic acid; and the conjugate base salt of the organic acid is selected from at least one of sodium alginate, agar and pectin.
[0080] In one embodiment, the amount of binder added is 0.05 wt % to 10 wt % based on the total weight of the composite particles, for example, 0.05 wt %, 0.06 wt %, 0.07 wt %, 0.08 wt %, 0.09 wt %, 0.1 wt %, 0.2 wt %, 0.3 wt %, 0.4 wt %, 0.5 wt %, 0.6 wt %, 0.7 wt %, 0.8 wt %, 0.9 wt %, 1.0 wt %, 2.0 wt %, 3.0 wt %, 4.0 wt %, 5.0 wt %, 6.0 wt %, 7.0 wt %, 8.0 wt %, 9.0 wt %, or 10 wt %.
[0081] In some optional examples, the added amount of the binder is 0.5 wt % to 3 wt %.
[0082] The aerosol generating device of the present application has the advantages of low aerosol smoke temperature and low release of harmful substances.
[0083] A second aspect of the present application provides a method for preparing the aerosol generating device of the first aspect, comprising steps S10 to S40.
[0084] Step S10: mixing the composite particles and the solvent to prepare a composite slurry;
[0085] Step S20: applying the composite slurry to at least a portion of a surface of the hollow base material 21 and drying it to form a composite layer 22;
[0086] Step S30: rolling the hollow base film with the side on which the composite layer is formed as the inner side to obtain the hollow device; and
[0087] Step S40: connecting the filter 30, the hollow device 20 and the aerosol matrix 10 in sequence to prepare an aerosol generating device.
[0088] In some embodiments, in step S10, the method for preparing the composite particles includes the following steps: mixing amino acids, polyethylene glycol and porous particle materials, and drying to prepare composite particles.
[0089] In some embodiments, the method for preparing the aerosol generating device further includes step S50.
[0090] Step S50 : using a wrapping material 40 to wrap the filter body 30 , the hollow device 20 and the aerosol matrix 10 that are connected in sequence.
[0091] A third aspect of the present application provides an aerosol generating system, comprising the aerosol generating device of the first aspect and a heating device.
[0092] In one embodiment, a heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.
[0093] The present application does not impose any particular limitation on the heating component, battery component, control component and housing, and they may be made of materials and in shapes commonly used in the art.
[0094] The aerosol generating system of the present application has the advantages of low release of harmful substances such as glycidol and good safety.
[0095] The present application will be further described below in conjunction with specific examples and comparative examples, but they should not be construed as limiting the scope of protection of the present application. The raw materials involved in the following specific examples, unless otherwise specified, can all be sourced from commercial sources, the instruments used, unless otherwise specified, can all be sourced from commercial sources, and the processes involved, unless otherwise specified, are all routinely selected by those skilled in the art.
[0096] Example 1:
[0097] (1) Arginine is dissolved in water to obtain an arginine solution, and the arginine solution is mixed with molten polyethylene glycol 1000 to obtain a mixed solution; activated carbon particles are immersed in the mixed solution, and dried at 100°C to obtain composite particles (i.e., activated carbon particles loaded with arginine and polyethylene glycol 1000).
[0098] Wherein, based on the total weight of the composite particles, the loading amount of arginine is 1wt%, the loading amount of polyethylene glycol 1000 is 30wt%; and the particle size of the activated carbon particles is 0.25mm~0.425mm.
[0099] (2) The composite particles, a binder (carboxymethyl cellulose), and water are mixed to obtain a composite slurry. The binder is added in an amount of 2 wt% based on the total weight of the composite particles.
[0100] (3) The composite slurry is evenly applied to the entire area of one surface of the cigarette paper, and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of the composite particles on the inner surface of the hollow device is 60 g / m 2 .
[0101] (4) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0102] Example 2:
[0103] The method is basically the same as Example 1, except that 1 wt% of arginine is replaced by 8 wt% of lysine, and 30 wt% of polyethylene glycol 1000 is replaced by 5 wt% of polyethylene glycol 10000; the particle size of the activated carbon particles is 0.15 mm to 0.25 mm; the coating amount of the composite particles on the inner surface of the hollow device is 40 g / m 2 .
[0104] Example 3:
[0105] The method is basically the same as Example 1, except that the activated carbon is replaced by montmorillonite; 1 wt% of arginine is replaced by 3 wt% of arginine, and 30 wt% of polyethylene glycol 1000 is replaced by 5 wt% of polyethylene glycol 6000; the coating amount of the composite particles on the inner surface of the hollow device is 10 g / m 2 .
[0106] Example 4:
[0107] The method is basically the same as Example 1, except that the activated carbon is replaced by sepiolite, and the particle size of the sepiolite particles is 0.15 mm to 0.25 mm; 1 wt % of arginine is replaced by 5 wt % of threonine, and 30 wt % of polyethylene glycol 1000 is replaced by 10 wt % of polyethylene glycol 2000.
[0108] Example 5:
[0109] The method is basically the same as Example 1, except that the activated carbon is replaced by kaolin, and the particle size of the kaolin particles is 0.045 mm to 0.15 mm; 1 wt% of arginine is replaced by 6 wt% of lysine, and 30 wt% of polyethylene glycol 1000 is replaced by 10 wt% of polyethylene glycol 4000; the coating amount of the composite particles on the inner surface of the hollow device is 50 g / m 2 .
[0110] Example 6:
[0111] The method is basically the same as Example 1, except that the activated carbon is replaced by diatomaceous earth, and the particle size of the diatomaceous earth particles is 0.045 mm to 0.15 mm; 1 wt% of arginine is replaced by 8 wt% of arginine, and 30 wt% of polyethylene glycol 1000 is replaced by 10 wt% of polyethylene glycol 6000; the coating amount of the composite particles on the inner surface of the hollow device is 15 g / m 2 .
[0112] Example 7:
[0113] The method is basically the same as Example 1, except that the activated carbon is replaced by diatomaceous earth, and the particle size of the diatomaceous earth particles is 0.15 mm to 0.25 mm; 1 wt% of arginine is replaced by 5 wt% of threonine, and 30 wt% of polyethylene glycol 1000 is replaced by 10 wt% of polyethylene glycol 8000; the coating amount of the composite particles on the inner surface of the hollow device is 20 g / m 2 .
[0114] Example 8:
[0115] The method is basically the same as Example 1, except that the activated carbon is replaced by calcium oxide, and the particle size of the calcium oxide particles is 0.15 mm to 0.25 mm; 1 wt% of arginine is replaced by 3 wt% of an amino acid mixture (threonine and lysine are mixed in a mass ratio of 1:1); 30 wt% of polyethylene glycol 1000 is replaced by 10 wt% of polyethylene glycol 8000; the coating amount of the composite particles on the inner surface of the hollow device is 45 g / m 2 .
[0116] Example 9:
[0117] The method is basically the same as Example 1, except that the activated carbon is replaced by ZSM-5 molecular sieve, and the particle size of the ZSM-5 molecular sieve particles is 0.15 mm to 0.25 mm; 1 wt% of arginine is replaced by 3 wt% of an amino acid mixture (threonine and lysine are mixed in a mass ratio of 1:1), and 30 wt% of polyethylene glycol 1000 is replaced by 10 wt% of polyethylene glycol 4000; the coating amount of the composite particles on the inner surface of the hollow device is 25 g / m 2 .
[0118] Example 10:
[0119] The method is basically the same as Example 1, except that: the activated carbon particles include first particles with a particle size of 0.045 mm to 0.15 mm and second particles with a particle size of 0.25 mm to 0.425 mm, and the mass ratio of the first particles to the second particles is 6.5:3.5; 1 wt% of arginine is replaced by 3 wt% of an amino acid mixture (threonine and lysine are mixed in a mass ratio of 1:1), and 30 wt% of polyethylene glycol 1000 is replaced by 15 wt% of polyethylene glycol 6000; the coating amount of the composite particles on the inner surface of the hollow device is 30 g / m 2 .
[0120] Example 11:
[0121] The method is basically the same as Example 1, except that: the activated carbon is replaced with diatomaceous earth, and the diatomaceous earth particles include first particles with a particle size of 0.045 mm to 0.15 mm and second particles with a particle size of 0.25 mm to 0.425 mm, and the mass ratio of the first particles to the second particles is 7.5:2.5; 1 wt% of arginine is replaced with 3 wt% of an amino acid mixture (threonine and lysine are mixed in a mass ratio of 1:1), and 30 wt% of polyethylene glycol 1000 is replaced with 10 wt% of polyethylene glycol 8000; the coating amount of the composite particles on the inner surface of the hollow device is 35 g / m 2 .
[0122] Example 12:
[0123] The same as Example 11, except that the composite slurry was applied to a partial area of one surface of the cigarette paper; the coating amount of the composite particles was 35 g / m2 based on the entire area of the cigarette paper. 2 Based on the area of the coated area on the cigarette paper, the coating amount of the composite particles is 50g / m 2 ;
[0124] Example 13:
[0125] The same as Example 11, except that the composite slurry was applied to a partial area of one surface of the cigarette paper; the coating amount of the composite particles was 15 g / m2 based on the entire area of the cigarette paper. 2 Based on the area of the coated area on the cigarette paper, the coating amount of the composite particles is 30g / m 2 ;
[0126] Comparative Example 1:
[0127] (1) Threonine is dissolved in water to obtain a threonine solution, which is then mixed with a binder (carboxymethyl cellulose) and water to obtain a composite slurry. The binder is added in an amount of 2.2 wt% based on the total weight of the threonine.
[0128] (3) The composite is evenly coated on one surface of the cigarette paper and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of threonine on the inner surface of the hollow device is 2 g / m 2 .
[0129] (4) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0130] Comparative Example 2:
[0131] The same as the comparative example 1, the difference is: the coating amount is 2g / m 2 The threonine is replaced with a coating amount of 6g / m 2 of lysine.
[0132] Comparative Example 3:
[0133] (1) Activated carbon particles, a binder (carboxymethyl cellulose), and water were mixed to obtain a composite slurry. The binder was added in an amount of 2.2 wt% based on the total weight of the activated carbon particles. The particle size of the activated carbon particles was 0.125 mm to 0.18 mm.
[0134] (2) The composite slurry is evenly coated on one surface of the cigarette paper and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of activated carbon particles on the inner surface of the hollow device is 30 g / m 2 .
[0135] (3) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0136] Comparative Example 4:
[0137] The same as the comparative example 3, the difference is: the coating amount is 30g / m 2 The activated carbon particles are replaced with a coating amount of 35g / m 2 of diatomaceous earth particles.
[0138] Comparative Example 5:
[0139] (1) Threonine is dissolved in water to obtain a threonine solution; activated carbon particles are immersed in the threonine solution and dried at 100°C to obtain composite particles (i.e., activated carbon particles loaded with threonine).
[0140] The loading amount of threonine is 2 wt % based on the total weight of the composite particles; and the particle size of the activated carbon particles is 0.025 mm to 0.15 mm.
[0141] (2) The composite particles, a binder (carboxymethyl cellulose), and water were mixed to obtain a composite slurry. The binder was added in an amount of 1.8 wt% based on the total weight of the composite particles.
[0142] (3) The composite slurry is evenly coated on one surface of the cigarette paper and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of the composite particles on the inner surface of the hollow device is 50 g / m 2 .
[0143] (4) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0144] Comparative Example 6:
[0145] The same as comparative example 5, the changes are: activated carbon is replaced by diatomaceous earth, the loading amount of 2wt% threonine is replaced by 3wt% lysine, and the final coating amount of the composite particles is 50g / m 2 .
[0146] Comparative Example 7:
[0147] (1) Threonine is dissolved in water to obtain a threonine solution, which is then mixed with molten polyethylene glycol 6000 to obtain a mixed solution. The mixed solution, a binder (carboxymethyl cellulose), and water are then mixed to obtain a composite slurry. The binder is added in an amount of 2 wt% based on the total weight of the composite slurry.
[0148] (3) The composite slurry is evenly coated on one surface of the cigarette paper and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of threonine on the inner surface of the hollow device is 2 g / m 2 The coating amount of polyethylene glycol 6000 on the inner surface of the hollow device is 5g / m 2 .
[0149] (4) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0150] Comparative Example 8:
[0151] The same as the comparative example 7, the difference is: the coating amount is 2g / m 2The threonine is replaced with a coating amount of 6g / m 2 Lysine; the coating amount is 5g / m 2 The polyethylene glycol 6000 is replaced with a coating amount of 20g / m 2 of polyethylene glycol 4000.
[0152] Comparative Example 9:
[0153] (1) The activated carbon granules are immersed in molten polyethylene glycol 6000 and dried at 100°C to obtain composite particles (i.e., activated carbon granules loaded with polyethylene glycol 600).
[0154] Wherein, based on the total weight of the composite particles, the loading amount of polyethylene glycol 1000 is 25wt%; and the particle size of the activated carbon particles is 0.045mm~0.15mm.
[0155] (2) The composite particles, a binder (carboxymethyl cellulose), and water are mixed to obtain a composite slurry. The binder is added in an amount of 2.5 wt% based on the total weight of the composite particles.
[0156] (3) The composite slurry is evenly coated on one surface of the cigarette paper and dried to form a composite layer; the surface coated with the composite layer faces inward, and the paper is rolled and bonded to form a hollow device. The coating amount of the composite particles on the inner surface of the hollow device is 50 g / m 2 .
[0157] (4) The filter body, the hollow device, and the aerosol matrix are sequentially connected, and the filter body, the hollow device, and the aerosol matrix connected in sequence are connected together using a wrapping material to obtain a heat-not-burn cigarette.
[0158] Comparative Example 10:
[0159] The same as comparative example 9, the changes are: activated carbon is replaced by diatomaceous earth, polyethylene glycol 6000 with a loading amount of 25wt% is replaced by polyethylene glycol 8000 with a loading amount of 15wt%, and the final coating amount of the composite particles is 50g / m 2 .
[0160] The method parameters for preparing the heat-not-burn cigarettes in the above-mentioned Examples 1-13 and Comparative Examples 1-10 are shown in Table 1 below; and the GC-MS method described in the literature (Chen X, Bailey PC, Yang C, et al. Targeted characterization of the chemical composition of JUUL systems aerosol and comparison with 3R4Freference cigarettes and IQOS heat sticks[J]. Separations, 2021, 8(10): 168.) was used to test the glycidol content released by the above-mentioned Examples, Comparative Examples and Control Samples (the Control Sample is a heat-not-burn cigarette whose inner wall of the hollow device is not coated with composite particles), and the results are shown in Table 1.
[0161] A central heating method was used, with the heating temperature set at 310°C. A linear smoking machine was used to smoke heat-not-burn cigarettes, with the following smoking parameters: puff volume of 55 mL; puff time of 2 s; puff interval of 30 s; number of puffs of 8 times; preheating time of 18 s; and a bell-shaped puff curve.
[0162] Table 1
[0163]
[0164]
[0165] As shown in the table above, the heat-not-burn cigarettes prepared using the specific method of this application exhibit significantly reduced glycidol release. Examples 10-13 demonstrate that the combination of two porous granular materials with different particle sizes can create a rugged surface on the composite layer, increasing the contact area between the smoke and the composite layer and further improving the adsorption efficiency of harmful substances.
[0166] The inner walls of the hollow devices of the heat-not-burn cigarettes prepared in Comparative Examples 1 and 2 were coated only with amino acids; the inner walls of the hollow devices of the heat-not-burn cigarettes prepared in Comparative Examples 3 and 4 were coated only with porous granular materials; the inner walls of the hollow devices of the heat-not-burn cigarettes prepared in Comparative Examples 5 and 6 were coated only with porous granular materials loaded with amino acids; the inner walls of the hollow devices of the heat-not-burn cigarettes prepared in Comparative Examples 7 and 8 were coated only with amino acids and polyethylene glycol; the inner walls of the hollow devices of the heat-not-burn cigarettes prepared in Comparative Examples 9 and 10 were coated only with granular materials loaded with polyethylene glycol; although the glycidol content released by the heat-not-burn cigarettes finally prepared in the above comparative examples was lower than that of the control sample, the improvement effect was not good.
[0167] The technical features of the above-mentioned embodiments can be combined arbitrarily. In order to make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0168] The above-described embodiments merely represent several implementation methods of the present application. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the present invention. It should be noted that a person skilled in the art may make various modifications and improvements without departing from the spirit of the present application, and these modifications and improvements fall within the scope of protection of the present application. Therefore, the scope of protection of the present application shall be determined by the appended claims.
Claims
1. An aerosol generating device, characterized in that: It comprises a filter body, a hollow device and an aerosol matrix connected in sequence; the hollow device comprises a hollow matrix and a composite layer, and the composite layer is located on at least part of the inner wall of the hollow matrix; The components of the composite layer include composite particles, which include porous particle materials, amino acids loaded on the porous particle materials, and polyethylene glycol loaded on the porous particle materials.
2. The aerosol generating device according to claim 1, characterized in that: It also includes a wrapping material, which wraps the outer sides of the filter body, the hollow device and the aerosol matrix which are connected in sequence.
3. The aerosol generating device according to claim 1, characterized in that: The composite layer comprises a plurality of strip-shaped regions arranged at intervals, and the composite particles are located in the strip-shaped regions.
4. The aerosol generating device according to any one of claims 1 to 3, characterized in that: Based on the weight of the composite particles, the loading amount of the polyethylene glycol is 5wt% to 30wt%.
5. The aerosol generating device according to any one of claims 1 to 3, characterized in that: The average molecular weight of the polyethylene glycol is 1000-10000.
6. The aerosol generating device according to any one of claims 1 to 3, characterized in that: Based on the weight of the composite particles, the loading amount of the amino acid is 1 wt% to 10 wt%.
7. The aerosol generating device according to any one of claims 1 to 3, characterized in that: The amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
8. The aerosol generating device according to any one of claims 1 to 3, characterized in that: The porous particle material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves.
9. The aerosol generating device according to claim 8, characterized in that: The natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
10. The aerosol generating device according to any one of claims 1 to 3 and 9, characterized in that: The particle size of the porous granular material is 0.045 mm to 0.425 mm.
11. The aerosol generating device according to claim 10, characterized in that: The porous granular material comprises a first particle and a second particle, the particle size of the first particle is 0.045 mm to 0.15 mm, and the particle size of the second particle is 0.25 mm to 0.425 mm; Based on the total weight of the porous particle material, the mass ratio of the first particles is 50wt% to 90wt%, and the mass ratio of the second particles is 10wt% to 50wt%.
12. The aerosol generating device according to any one of claims 1 to 3, 9 and 11, characterized in that: In the composite layer, the coating amount of the composite particles is 10 g / m 2 ~60g / m 2 .
13. The aerosol generating device according to any one of claims 1 to 3, 9 and 11, characterized in that: The components of the composite layer also include a binder intermixed with the composite particles.
14. The aerosol generating device according to claim 13, characterized in that: The binder is selected from at least one of gums, cellulose binders, polysaccharides, organic acids and conjugate alkali salts of organic acids.
15. The aerosol generating device according to claim 13, characterized in that: The amount of the binder added is 0.05wt% to 10wt% based on the mass of the composite particles.
16. A method for preparing an aerosol generating device according to any one of claims 1 to 15, characterized in that: The steps include: Mixing the composite particles and a solvent to prepare a composite slurry; Applying the composite slurry to at least a portion of a surface of a hollow base material, and drying to form a composite layer; Rolling the hollow substrate film with the side on which the composite layer is formed as the inner side to obtain the hollow device; and The filter body, the hollow device and the aerosol matrix are connected in sequence to obtain the aerosol generating device.
17. The method for preparing an aerosol generating device according to claim 16, characterized in that: The method for preparing the composite particles comprises the following steps: The amino acid, polyethylene glycol and porous particle material are mixed and dried to prepare the composite particles.
18. An aerosol generating system, characterized in that: It comprises the aerosol generating device and heating device as described in any one of claims 1 to 15.
19. The aerosol generating system according to claim 18, characterized in that: The heating device comprises a heating component, a battery component for supplying power to the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component and the control component.
Citation Information
Patent Citations
Complex adsorbent capable of reducing release amount of heavy metals in mainstream smoke of cigarettes, preparation method for complex adsorbent and application of complex adsorbent
CN102499479A
Aerosol generating article having cavity with particulate aerosol altering material
CN111148440A
Cigarette and preparation method thereof
CN117617551A
Filter medium for reducing harmful substance in tobacco smoke fog
CN1267488A
Filter for a smoking article
WO2011015861A2