Device and method for automatically detecting and eliminating metallurgical defects of deposited layer based on temperature field
By using an infrared camera to monitor the temperature field of the molten pool during the laser deposition process and combining it with the PID algorithm to control the process parameters, the problem of difficulty in online detection and control of metallurgical defects in the deposited layer in the existing technology is solved, and the mechanical properties of the laser deposited workpiece are significantly improved. and precision.
Patent Information
- Application Number
- CN202410750832.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-12
- Publication Date
- 2024-10-01
AI Technical Summary
It is difficult to effectively detect and quality control metallurgical defects in the deposition layer produced during the laser deposition process online with existing technology, resulting in reduced mechanical properties.
A device consisting of a laser directional energy deposition system, a temperature detection and control system, and a PID control system is used to obtain the melt pool temperature field information through an infrared camera, set the temperature threshold, and use the PID algorithm to control process parameters to achieve real-time monitoring of the melt pool temperature field. Monitoring and closed-loop control suppress the occurrence and growth of defects.
It achieves real-time monitoring and defect prediction of laser-deposited workpieces, effectively improves mechanical properties, reduces the generation and growth of defects, and improves the geometric accuracy and mechanical properties of workpieces.
Smart Images

Figure CN118720170A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of laser deposition production technology, and in particular to a device and method for automatically detecting and eliminating metallurgical defects of a deposition layer based on a temperature field. Background Art
[0002] At present, the research on defect detection and quality control technology in the process of metal additive manufacturing at home and abroad mainly focuses on online detection and feedback control of the physical parameters of the molten pool, so as to reduce the macro defects such as deformation and dimensional anomaly of additively manufactured parts, and effectively reduce the reduction of mechanical properties caused by macro defects. At present, foreign scholars usually use low-coherence interferometric imaging technology to conduct online detection and feedback control of the molten pool morphology changes and stability in the selective laser melting process to reduce the dimensional deformation of the parts, and in the laser metal deposition forming process, the laser power is adaptively controlled by PID proportional integral differential according to the online detected molten pool thermal radiation intensity value, which improves the dimensional accuracy of the parts. In the direct metal deposition (DMD) system, the dual parameters of molten pool height and molten pool temperature are used to implement hybrid closed-loop control of laser power, which improves the geometric accuracy of parts and reduces the occurrence of dimensional defects. In the laser metal wire deposition process, an online feedback control model of wire feed rate based on iterative learning algorithm is established, which effectively eliminates the dimensional defects caused by the change of forming height due to the mutual influence between adjacent melt channels.
[0003] In China, some scholars have proposed the "thermal stress discrete control" method, which effectively solves the problem of severe warping and cracking during the laser forming process of large titanium alloy structural parts. Through online detection and closed-loop control of the defocus amount of the laser forming molten pool, the appearance defects of the formed parts are effectively reduced. By online detection of the width of the laser cladding molten pool, the surface quality of the laser cladding is evaluated. However, these methods are difficult to effectively detect and control the defects generated during the deposition process online. Summary of the invention
[0004] In order to solve the above technical problems, the purpose of the present invention is to provide a device and method for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field. The technical solutions adopted are as follows:
[0005] This device consists of a laser directed energy deposition system, a temperature detection and control system, a quality database and a PID control system.
[0006] In the laser directed energy deposition system, the laser source provides a high-energy laser beam for the laser processing head installed on the motion mechanism, Ti6Al4V powder is added to the powder feeder, and the process parameters of laser directed energy deposition manufacturing are preset through the CNC platform: powder feeding speed 1rad, laser spot diameter 3mm, and the protective gas cylinder provides inert gas argon as a carrier gas connected to the laser processing head as a protective gas flow to prevent oxidation reaction at high temperature. The processing platform is adjusted and the workpiece is waiting for printing. The high-energy laser beam melts the Ti6Al4V powder into a molten pool. The infrared camera interface consists of an Ethernet connector, an I / O interface, a water cooling interface and a manual focus mechanism. The router is connected to the PC via Ethernet, the manual focus mechanism is mechanically connected to the infrared lamp for focusing, the I / O interface is connected to the infrared camera junction box, and the infrared camera junction box is connected to the power control software on the PC side. The water cooling interface is connected to the water cooling protector, which is used for the heat dissipation protection circuit when the infrared camera is working.
[0007] In the temperature detection and control system, an infrared camera is installed on the side axis of the motion mechanism. The infrared camera obtains high-resolution molten pool images during the directional energy deposition process and obtains molten pool temperature field information; the molten pool temperature field information is transmitted to the PC via USB, and the PC calls the relevant temperature formula to perform online analysis on the molten pool temperature field information and record it in the quality database, set the temperature threshold, and compare the abnormal molten pool temperature field caused by defects with the set temperature threshold. The difference information is transmitted to the CNC platform as a digital signal. The CNC platform uses the PID closed-loop control method to adjust the process parameters, and converts the instructions into analog signals and sends them to the laser source to adjust the laser processing head in real time; the laser process parameters are set to a laser power of 1800W and a scanning speed of 600mm / min; an infrared camera is used to obtain the thermal imaging image of the deposited workpiece, and the two-dimensional temperature field information of the molten pool is used to construct a reference temperature field. The molten pool temperature field is corrected using an image correction method, and the average value of multiple normal molten pool temperature values is obtained to obtain a reference temperature value for the normal molten pool temperature value.
[0008] In the quality database and PID control system, the maximum gradient principle is referred to and the Canny edge detection operator is used to obtain the molten pool boundary. Affected by the gradient temperature field when the molten pool edge state changes, the gradient extreme value feature is used to identify the molten pool boundary. The similarity of the detected molten pool temperature field to the preset molten pool temperature field is calculated to determine the abnormal temperature threshold.
[0009] In order to improve the detection rate in actual detection, the temperature residual mean of the corresponding points in the molten pool can be selected. As similarity.
[0010] Set an abnormal temperature threshold, collect similar points in the molten pool, and if the similarity of the molten pool temperature field is higher than the abnormal temperature field threshold, it is abnormal. Record the time or position of each point of the molten pool temperature field and the evaluation results of the temperature field detection (normal / abnormal) in the quality database. Summarize the temperature field information through similar points to build a three-dimensional information database Q(T) of the molten pool quality. t ), which can quickly locate the molten pool quality management and abnormal temperature field information of the molten pool during the deposition process.
[0011] The PID algorithm is used to adjust the process parameters online, and the process parameter information is fed back to the directed energy deposition manufacturing system to form a closed-loop control to inhibit the generation and growth of defects during the laser deposition process.
[0012] The present invention has at least the following beneficial effects:
[0013] The infrared camera set at the side of the axis is used to obtain the molten pool image during the directed energy deposition process, so as to realize the purpose of real-time monitoring of the molten pool temperature field.
[0014] The thermal image of the workpiece is obtained based on the thermal feedback transmitted by the workpiece received by the infrared camera. The temperature threshold is set, and it is determined whether the workpiece has defects based on the position and size of the abnormal temperature field. The collected temperature data is fed back to the quality database, and the PID algorithm is used to control the process parameters. The controlled process parameter information is fed back to the directed energy deposition system, thereby achieving the purpose of inhibiting the generation and growth of defects in the laser deposition process, which can effectively improve the mechanical properties of the laser deposited workpiece. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions and advantages of the embodiments of the present invention or the prior art, the following briefly introduces the drawings required for use in the description of the embodiments or the prior art.
[0016] Figure 1 It is a flow chart of the device and method for automatically detecting and eliminating metallurgical defects of a deposited layer based on a temperature field of the present invention;
[0017] Figure 2 A schematic diagram of a closed-loop controlled laser directed energy deposition system of the device and method for automatically detecting and eliminating metallurgical defects of a deposited layer based on a temperature field according to the present invention;
[0018] Above Figure 2 In the figure: 1. PC terminal; 2. Powder feeder; 3. Laser source; 4. Motion mechanism; 5. Laser processing head; 6. Workpiece; 7. Processing platform; 8. Infrared camera; 9. Molten pool; 10. Water cooling protector; 11. Protective gas cylinder; 12. CNC platform. DETAILED DESCRIPTION
[0019] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose of the invention, the specific implementation method, structure, characteristics and effects of the device and method for automatically detecting and eliminating metallurgical defects of the deposited layer based on the temperature field proposed by the present invention are described in detail as follows in combination with the accompanying drawings and preferred embodiments.
[0020] The present invention provides a specific implementation method of a device and method for automatically detecting and eliminating metallurgical defects of a deposited layer based on a temperature field. The method is suitable for the scene of automatic detection and elimination of metallurgical defects in a laser deposition process. In this scene, the workpiece being inspected will produce various defects due to external factors. The present invention performs online detection of the temperature field of the molten pool during the laser deposition process and combines the PID algorithm to perform closed-loop control of the process parameters, thereby effectively improving the mechanical properties of the laser deposited workpiece and inhibiting and eliminating the formation and growth of defects during the laser deposition process.
[0021] The specific scheme of the device and method for automatically detecting and eliminating metallurgical defects of a deposited layer based on a temperature field provided by the present invention is described in detail below in conjunction with the accompanying drawings.
[0022] This device consists of a laser directed energy deposition system, a temperature detection and control system, a quality database and a PID control system.
[0023] In the laser directed energy deposition system, Ti6Al4V powder is added to the powder feeder 2, and the process parameters of laser directed energy deposition manufacturing are preset through the CNC platform 12: powder feeding speed 1rad, laser spot diameter 3mm, the protective gas cylinder 11 provides inert gas argon as a carrier gas connected to the laser processing head 5 as a protective gas flow to prevent oxidation reaction at high temperature, adjust the processing platform 7, wait for the workpiece 6 to be printed, the laser source 3 provides a high-energy laser beam to the laser processing head 5, melts the Ti6Al4V powder into a molten pool 9, the water cooling interface is connected to the water cooling protector 10, and the router is connected to the control software of the PC end 1 through Ethernet to perform directed energy deposition manufacturing.
[0024] In the temperature detection and control system, an infrared camera 8 is installed on the side axis of the motion mechanism 4. The infrared camera 8 obtains a high-resolution molten pool image during the directional energy deposition process to obtain the molten pool temperature field information; the molten pool temperature field information is transmitted to the PC terminal 1 via USB, and the PC terminal 1 calls the relevant temperature formula to perform online analysis on the molten pool temperature field information and records it to the quality database, sets a temperature threshold, and compares the abnormal molten pool temperature field caused by defects with the set temperature threshold. The difference information is transmitted as a digital signal to the electronic numerical control platform 12, and the electronic numerical control platform 12 adopts the PID closed-loop control method to adjust the process parameters, and converts the instructions into analog signals and sends them to the laser source 3 to adjust the laser processing head 5 in real time; the laser process parameters are set to a laser power of 1800W and a scanning speed of 600mm / min.
[0025] The temperature detection and control system consists of a PC terminal 1, an infrared camera 8, and the control software of the PC terminal 1. The infrared camera 8 is installed on the motion mechanism 4, and the lens is aimed at the workpiece 6 placed on the processing platform 7, which is used to capture dynamic images of the molten pool solidification process and obtain temperature field information. The temperature threshold and related temperature formula are set in the control software of the PC terminal 1 to obtain temperature information in the laser deposition workpiece.
[0026] The quality database and PID control system consists of PC-side 1 acquisition and control software and PC-side quality database software. The powder feeding speed, laser power, scanning speed, laser spot diameter, molten pool width and PID parameters of the laser directional energy deposition system are set in the display window of the PC-side acquisition and control software to facilitate the adjustment of laser process parameters. The molten pool image during the laser deposition process is obtained using an infrared camera 8. Since it will be affected by external environments such as smoke and dirt in an industrial production environment, it is necessary to correct the acquired molten pool image to make the image conform to the actual situation.
[0027] Under the same laser deposition conditions, an infrared camera 8 is used to obtain a thermal image of the deposited workpiece, and the two-dimensional temperature field information of the molten pool is used to construct a preset temperature field. The average value of multiple normal molten pool temperature values is obtained to obtain a preset temperature value of the normal molten pool temperature value; the similarity between the preset temperature value of the normal molten pool temperature field and the detected real-time molten pool temperature field is calculated to obtain the abnormal temperature threshold. A series of temperature similarities in the laser deposition process are obtained in the PC-side quality database software to facilitate subsequent analysis. Generally, during the laser deposition process, the edge state of the molten pool changes from liquid to solid, and from melting to solidification. Its temperature field will be affected by the gradient temperature field. Referring to the maximum gradient principle, the molten pool boundary is obtained in combination with the Canny edge detection operator, and the gradient extreme value feature is used to identify the boundary of the molten pool.
[0028] Affected by uncertain factors, such as irregular movement and splashing of powder, the temperature of the molten pool fluctuates. The average processing of the temperature field of the molten pool at multiple different times t makes the molten pool temperature field close to the ideal temperature field and has a relatively stable two-dimensional near-Gaussian distribution, thereby reducing the fluctuation of the molten pool temperature field caused by external factors. For the two-dimensional temperature distribution, at time t, the molten pool temperature field T(x,y) can be expressed as:
[0029] T(x,y) t ={T ide (x,y),T sf (x,y),T abn (x,y)}
[0030] The xy coordinate system is set on the plane where the molten pool is located, and the observation area is set to M×N. The obtained molten pool temperature field information is divided into three parts: T ide(x, y) is the two-dimensional temperature field distribution of the molten pool under ideal conditions, T sf (x, y) is the temperature change caused by heat accumulation during the deposition process, T abn (x, y) is the temperature anomaly of the deposition process; the formula for the preset temperature value T0 is: The formula for calculating the gradient direction of the molten pool temperature field is:
[0031]
[0032] The formula for calculating the gradient direction is:
[0033]
[0034] Among them, the temperature field of the molten pool is placed in the coordinate axis, and the gradient g in the x-axis direction is x (x,y) and the gradient g in the y-axis direction y (x,y) is combined into a two-dimensional gradient distribution g xy (x, y), the gradient direction of each point is θ(x, y), and the gradient amplitude is calculated by linear interpolation to determine the maximum value of the gradient at each point.
[0035] The formula for calculating the similarity of the detected molten pool temperature field to the preset molten pool temperature field at time t is:
[0036]
[0037] Among them, the observed area is M×N, T t (x, y) is the temperature value of the molten pool temperature field to be measured at time t, T0(x, y) is the temperature value of the preset molten pool temperature field, and are the preset temperature value of the molten pool temperature field and the average value of the actually measured molten pool temperature field, and is a constant, obtained by detecting the changing distribution of the temperature field.
[0038] In order to improve the detection rate in actual detection, the temperature residual mean of the corresponding points in the molten pool can be selected. As similarity, the formula is:
[0039]
[0040] Among them, T t (x, y) is the temperature value of the molten pool temperature field to be measured at time t, and T0(x, y) is the temperature value of the preset molten pool temperature field.
[0041] During the laser deposition process, abnormal points are generated near the molten pool temperature field. According to the preset molten pool temperature field, it can be considered that this abnormal point is about to produce defects. Since the number of abnormal points cannot be estimated, the average value of the abnormal point temperature field is set as the abnormal temperature threshold Thr(P) to construct the quality database Q(Tt) during the laser deposition process. The formula is:
[0042]
[0043] In the laser deposition process, a series of similarities of the molten pool can be obtained by the above method. The similarity of the molten pool temperature field is abnormal when it is higher than the abnormal temperature threshold Thr(P), and it is normal when it is lower than the abnormal temperature threshold Thr(P). t )=1 means outputting abnormal molten pool information at time t.
[0044] An abnormal temperature threshold is set and similar points in the molten pool are collected. If the similarity of the molten pool temperature field is higher than the abnormal temperature field threshold, it is abnormal. The time or position of each point of the molten pool temperature field and the evaluation results of the temperature field detection (normal / abnormal) are recorded in the quality database. The temperature field information is summarized through similar points to build a three-dimensional information library of molten pool quality. This can quickly locate the molten pool quality management and abnormal molten pool temperature field information during the deposition process.
[0045] The infrared camera 8 transmits the collected real-time molten pool temperature field data to the quality database and PID control system. The quality database processes the data, obtains the temperature similarity, and thus sets the temperature threshold. The PID control system converts the difference between the real-time molten pool temperature and the preset molten pool temperature into an analog signal as feedback input.
[0046] The difference formula is: t(k) = T i (k)-T r (k), where T i (k) is the preset molten pool temperature, T r (k) is the real-time molten pool temperature; according to the difference in molten pool temperature, the PID control system uses a PID algorithm to control the laser source 3 to adjust the laser power in real time.
[0047] The laser power variation is Where K p is the proportional gain, T1 is the integration time, T D For the differential time, set the PID parameters: K p is 200, T1 is 0.5, T D is 0.5.
[0048] Set the melt pool temperature change rate By keeping the real-time temperature change rate of the molten pool within ±3%, it can be considered that the temperature field of the molten pool remains stable and no abnormal temperature field caused by defects is generated, thereby inhibiting the generation and growth of defects in the laser directed energy deposition process.
[0049] In this embodiment, preferably, the infrared camera 8 can measure the temperature field of the molten pool simultaneously with the movement of the print head.
[0050] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A device for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature fields, characterized in that: This device consists of a laser directed energy deposition system, a temperature detection and control system, a quality database and a PID control system; The laser directed energy deposition system is composed of a PC terminal, a laser source, a water-cooled protector, a CNC platform, a powder feeder, a protective gas cylinder, a laser processing head, a motion mechanism, a processing platform, a molten pool, and a workpiece; the laser processing head is installed below the motion mechanism, the laser source provides a high-energy laser beam for the laser processing head, Ti6Al4V powder is added to the powder feeder, the process parameters of laser directed energy deposition manufacturing are preset through the CNC platform, the protective gas cylinder provides inert gas argon as a carrier gas connected to the laser processing head as a protective gas flow to prevent oxidation reaction at high temperature, the processing platform is adjusted, and the workpiece is waiting for printing, and the high-energy laser beam melts the Ti6Al4V powder into a molten pool; The temperature detection and control system consists of a PC, an infrared camera and control software on the PC; an infrared camera is installed on the motion mechanism, and the infrared camera and the laser processing head perform paraxial motion, and the lens is aimed at the workpiece placed on the processing table, so as to capture dynamic images during the solidification process of the molten pool and obtain temperature field information; the interface of the infrared camera consists of an Ethernet connector, an I / O connector, a water cooling connector and a manual focus mechanism, the infrared camera is connected to the router to the PC via the Ethernet connector, the manual focus mechanism is mechanically connected to the infrared lamp for focusing, the I / O connector is connected to the infrared camera junction box, the infrared camera junction box is connected to the power control software on the PC, and the water cooling connector is connected to the water cooling protector, which is used for the heat dissipation protection circuit when the infrared camera is working; the temperature threshold and related temperature formulas are set in the PC control software to obtain temperature information in the laser deposition workpiece; The quality database and PID control system consists of PC-side acquisition and control software and PC-side quality database software. The powder feeding speed, laser power, scanning speed, laser spot diameter, molten pool width and PID parameters of the laser directional energy deposition system are set in the display window of the PC-side acquisition and control software to facilitate the adjustment of laser process parameters. A series of temperature similarities in the laser deposition process are obtained in the PC-side quality database software to facilitate subsequent analysis.
2. The device for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field according to claim 1, characterized in that: The preset process parameters of laser directed energy deposition manufacturing are: powder feeding speed 1 rad, laser spot diameter 3 mm, laser power 1800 W, and scanning speed 600 mm / min.
3. The device for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field according to claim 1, characterized in that: The infrared camera obtains high-resolution dynamic molten pool images and temperature field information during the directed energy deposition process, and obtains the molten pool temperature field information; the molten pool temperature field information is transmitted to the PC via USB, and the PC calls the relevant temperature formula to perform online analysis on the molten pool temperature field information and records it in the quality database, sets the temperature threshold, and compares the abnormal molten pool temperature field caused by defects with the set temperature threshold. The difference information is transmitted to the electronic numerical control platform as a digital signal. The electronic numerical control platform uses the PID closed-loop control method to adjust the process parameters, and converts the instructions into analog signals and sends them to the laser source for real-time regulation of the laser processing head. The laser process parameters are set to 1rad, laser power 1800W, and scanning speed 600mm / min.
4. A method for automatically detecting and eliminating metallurgical defects of a deposited layer based on a temperature field using the device as claimed in claim 1, characterized in that: The molten pool image is acquired by a rangefinder infrared camera to monitor the molten pool temperature field in real time, obtain the thermal image of the workpiece, set the temperature threshold, and judge whether the workpiece has defects based on the abnormal temperature field caused by the defects. The collected temperature data is recorded in the quality database, and the process parameters are regulated by the PID closed-loop control method, which is then fed back to the laser directed energy deposition system to inhibit the generation and growth of defects during the laser deposition process and improve the mechanical properties of the laser deposited workpiece. The specific steps are as follows: (1) An infrared camera is installed on the laser directed energy deposition system to obtain high-resolution images of the molten pool during the directed energy deposition process and obtain information on the temperature field of the molten pool; (2) constructing a reference temperature field based on the collected two-dimensional temperature field information of the molten pool, correcting the molten pool temperature field using an image correction method, obtaining an average value of multiple normal molten pool temperature values, and obtaining a reference temperature value of the normal molten pool temperature value; Referring to the maximum gradient principle, the molten pool boundary is obtained by combining the Canny edge detection operator. Affected by the gradient temperature field when the edge state of the molten pool changes, the gradient extreme value feature is used to identify the boundary of the molten pool. (3) Setting an abnormal temperature threshold, collecting similar points in the molten pool, if the similarity of the molten pool temperature field is higher than the abnormal temperature field threshold, it is abnormal, and if the similarity of the molten pool temperature field is lower than the abnormal temperature field threshold, it is normal. Record the time or position of each point of the molten pool temperature field and the evaluation result of the temperature field detection (normal / abnormal) in the quality database, summarize the temperature field information through similar points, and build a three-dimensional information database of the molten pool quality, which can quickly locate the molten pool quality management and abnormal molten pool temperature field information during the deposition process; (4) The PID algorithm is used to adjust the process parameters online, and the process parameter information is fed back to the directed energy deposition manufacturing system to form a closed-loop control to inhibit the generation and growth of defects during the laser deposition process.
5. The method for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field according to claim 4, characterized in that: Identify the boundary of the molten pool according to the gradient extreme value characteristics, including: The formula for calculating the gradient direction of the molten pool temperature field is: The formula for calculating the gradient direction is: Among them, the temperature field of the molten pool is placed in the coordinate axis, and the gradient g in the x-axis direction is x (x,y) and the gradient g in the y-axis direction y (x,y) is combined into a two-dimensional gradient distribution g xy (x, y), the gradient direction of each point is θ(x, y), and the gradient amplitude is calculated by linear interpolation to determine the maximum value of the gradient at each point; The formula for calculating the similarity of the detected molten pool temperature field to the reference preset molten pool temperature field at time t is: Among them, the observed area is M×N, T t (x, y) is the temperature value of the molten pool temperature field to be measured at time t, T0(x, y) is the temperature value of the preset molten pool temperature field, and are the reference temperature value of the molten pool temperature field and the average value of the actually measured molten pool temperature field, and is a constant, obtained by detecting the changing distribution of the temperature field.
6. The method for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field according to claim 4, characterized in that: In order to improve the detection rate in actual detection, the similarity calculation is based on the mean temperature residual of the corresponding points in the molten pool. As similarity, the formula is: Among them, T t (x, y) is the temperature value of the molten pool temperature field to be measured at time t, and T0(x, y) is the temperature value of the preset molten pool temperature field.
7. The method for automatically detecting and eliminating metallurgical defects of deposited layers based on temperature field according to claim 4, characterized in that: The quality database 4Q(Tt) in the laser deposition process is constructed, and its formula is: In the laser deposition process, a series of similarities of the molten pool are obtained. The molten pool temperature field similarity higher than the abnormal temperature threshold Thr(P) is considered abnormal, and the molten pool temperature field similarity lower than the abnormal temperature threshold Thr(P) is considered normal. t )=1 means outputting abnormal molten pool information at time t.
Citation Information
Cited By
Laser cutting machine
CN119794615A
Quality detection method in functionally graded material preparation process
CN120992694A