Method for soaking nylon fastener in water and automatic conveying line for soaking in water

Through intermittent operation and temperature-controlled nylon fastener soaking method, the problem of poor soaking effect of various specifications of nylon fasteners in the existing technology has been solved, and efficient water absorption and mechanical performance improvement have been achieved, and energy consumption has been reduced. and scrap rate, meeting the water-soaking needs of diversified products.

CN118721802AActive Publication Date: 2024-10-01ZHUZHOU TIMES NEW MATERIAL TECHNOLOGY CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410886114.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-03
Publication Date
2024-10-01
Estimated Expiration
2044-07-03

AI Technical Summary

Technical Problem

It is difficult for the existing technology to achieve sufficient water absorption rate for nylon fasteners with various specifications and requirements during the water soaking process. Especially for nylon fasteners with high requirements, the existing automated operation method is difficult to achieve an effective water soaking effect.

Method used

The method of soaking nylon fasteners in water using an intermittent operation method, by controlling the number and time of pauses of the soaking conveyor belt, combined with the length of the water tank and the conveying speed, ensures that the time the nylon fasteners stay in the water tank meets the required water soaking requirements. The water temperature is controlled by a temperature sensor to achieve precise water soaking treatment for different nylon fasteners.

Benefits of technology

It effectively improves the dimensional accuracy and mechanical properties of nylon fasteners, reduces energy consumption and scrap rate, improves production efficiency, meets the water soaking needs of nylon fasteners of various specifications and requirements, and ensures high-quality output of products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118721802A_ABST
    Figure CN118721802A_ABST
Patent Text Reader

Abstract

The invention provides a method for soaking nylon fasteners in water, which comprises the following steps of: bringing the just formed nylon fasteners into a water tank of a water soaking water tank conveying assembly through a material receiving belt section, moving the nylon fasteners in the water tank of a water tank along with a water soaking conveying belt until the water soaking requirement is met, taking the nylon fasteners out of the water tank by the water soaking conveying belt, and enabling the nylon fasteners to fall into a material receiving box; the intermittent operation mode is adopted, and according to the specific requirements of the nylon fasteners, after the determined pause times of the nylon fasteners, the time when the water soaking conveying belt carries the nylon fasteners out of the water tank is just the water soaking time needed by the nylon fasteners. The water soaking effect of the nylon fastener can be guaranteed, the size precision and mechanical performance of the nylon fastener are effectively improved, and meanwhile energy consumption and the rejection rate are reduced. In addition, due to the design of the automatic conveying line, the production efficiency is further improved, and the labor cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method and equipment for processing and manufacturing injection molded parts, and in particular to a method and an automatic conveyor line for processing and manufacturing nylon fasteners soaked in water, belonging to the technical field of nylon parts soaked in water processing and manufacturing. Background Art

[0002] With the continuous development of rail transportation, the use of rails and their accessories is increasing. Rail fasteners are important devices for fixing rails, and they are also consumables with a broad market. At the same time, due to the large market consumption, more and more companies are attracted, and the competition is becoming more and more fierce. The quality and cost of nylon fasteners in fasteners have become key factors in determining market position.

[0003] Nylon is a highly water-absorbent material, with a water absorption rate of more than 1%. This water absorption is due to the amide groups in the nylon molecule. After absorbing moisture, the nylon material will show better toughness and impact strength. However, after injection molding, the nylon material may cause internal stress inside the material due to rapid cooling, which will affect the toughness and durability of the product. Water cooling can help nylon macromolecules tend to natural orientation and crystallization, thereby eliminating internal stress, improving the toughness of the product, and improving the stability of its internal structure, making it more durable during use and reducing the risk of breakage due to brittleness; therefore, more and more cases are currently using nylon fasteners that have been soaked in water.

[0004] However, when using the water soaking process for nylon fasteners, it is necessary to control the soaking temperature and soaking time to ensure that they have an appropriate water absorption rate. However, as the types of fasteners made of nylon increase, the requirements become more and more different, which leads to the need for various soaking conditions. However, most of the current soaking methods are to directly throw the nylon parts into a soaking pool for soaking, and then take them out after a certain period of time. However, this operation method has high labor intensity and is not suitable for mass production. In order to change this situation, it is now proposed to use a conveyor belt method to load the nylon fasteners that have just come out through a water tank through the conveyor belt, soaking them while running, and then take the nylon fasteners out at the end of the water tank. , complete the soaking process; this adopts a continuous soaking process, which uses an operating conveyor belt to pass the nylon parts that need to be soaked through a soaking tank at a uniform speed for soaking; but since the tank is fixed and due to site limitations, the tank cannot be arbitrarily expanded or lengthened, the soaking time is also fixed; this may be easier for a nylon part to meet the soaking requirements, but it is very difficult to use the same tank to meet various requirements for nylon parts of various specifications and requirements, especially for nylon fasteners with very high requirements, it is necessary to ensure sufficient water absorption, which is difficult to achieve using the existing automated soaking method; therefore, it is necessary to improve this.

[0005] The search did not find the same technical solution as the present invention, but only found some related comparative technical documents, mainly the following: 1. The patent with application number 202223054261.0 discloses an automatic conveying and cooling machine for injection molded parts, including a rectangular plate, a conveyor belt is arranged on the upper surface of the rectangular plate, the upper surface of the rectangular plate and the symmetrical positions on the front and rear sides of the conveyor belt are respectively fixedly connected to the limit plate, a plurality of circular holes are opened on one side of the limit plate, the inside of the circular holes is fixedly connected to the mounting plate, a fan is fixedly connected to one side of the mounting plate, the symmetrical positions on the front and rear sides of the upper surface of the rectangular plate and the position outside the limit plate are respectively fixedly connected to the vertical rod, and the upper ends of the opposite sides of the two vertical rods are fixedly connected to the horizontal plate. The device can facilitate the conveying and cooling of injection molded parts, facilitate the movement of injection molded parts, save the cooling time of injection molded parts, facilitate quick collection, and avoid damage. By setting the conveyor belt, the conveying of injection molded parts can be facilitated, and by setting the fan and the atomizer, the injection molded parts can be quickly cooled, which is convenient for use.

[0006] 2. The patent with application number 202222914344.6 discloses a rapid condensation injection molding machine, which relates to the technical field of injection molding machines and aims to solve the problem that the cooling and demolding efficiency of injection molding machines is low and adjacent molds are easily fused. The key points of its technical solution are: it includes a machine body and a demolding mechanism installed in the machine body, the bottom wall of the machine body is fixedly connected to a cooling box, the cooling box is provided with a feed inlet and a discharge port, the demolding mechanism is located directly above the feed inlet, the inner wall of the cooling box is rotatably connected to a conveyor belt for transporting plastic parts, the demolding mechanism is located directly above the conveyor belt, and a number of separation parts are fixedly connected to the outer surface of the conveyor belt, and gaps for accommodating plastic parts are formed between adjacent separation parts. The utility model is fixedly connected to a spray assembly in the cooling box, and the spray port of the spray assembly is arranged toward the conveyor belt. The spray assembly sprays water to the plastic parts on the conveyor belt through the spray port, which can accelerate the condensation of the plastic parts, thereby improving the product quality.

[0007] 3. The patent with application number 202021019342.5 discloses a cooling pool for the water quenching process of reflective materials, including: a water pool and a transmission device. The inner wall of the water pool is provided with a plurality of mounting seats, the side wall of the water pool is provided with an inlet pipe and an outlet pipe, the outlet pipe is provided with a filter screen, the water pool is provided with a detachable feed trough, and the bottom of the front end of the water pool is a concave structure; the transmission device is detachably arranged on the mounting seat, the transmission device is inclined, the transmission belt of the transmission device is a filter screen structure for easy drainage, the bottom is located in the water pool, the outlet end of the transmission device is located outside the water pool, the transmission device is driven by a motor, the motor is arranged at the front end of the water pool, and the motor and the transmission device are connected by a joint. It improves production efficiency, prevents a large amount of crystals from falling into the water pool, reduces the workload of cleaning the water pool in the later stage, and avoids personal injury.

[0008] Through the analysis of the above patents, it can be confirmed that the prior art for the process of soaking plastic parts in water has always remained in the simple soaking method or simple water spray cooling, and has not paid attention to the process or method of soaking in water. For the automatic conveying soaking in water, it is only simply considered as a continuous operation method, and the plastic parts to be cooled are passed through a fixed water tank. Therefore, the plastic is only soaked in water, but it does not meet the real soaking requirements; therefore, it is still necessary to improve it. Summary of the invention

[0009] The technical problem to be solved by the present invention is: In order to improve the quality of rail transit fasteners and reduce production costs, this patent proposes a nylon fastener soaking process method and an automatic conveyor line. This method effectively improves the dimensional accuracy and mechanical properties of nylon fasteners by optimizing the soaking process of nylon fasteners, while reducing energy consumption and scrap rate. In addition, the design of the automatic conveyor line further improves production efficiency and reduces labor costs.

[0010] The technical solution proposed by the present invention is: a method for soaking nylon fasteners in water, which brings the newly formed nylon fasteners into the water tank of the soaking tank conveying assembly through the material receiving belt section, and places the nylon fasteners on the soaking conveyor belt, so that all the nylon fasteners are immersed in water as a whole, and move with the soaking conveyor belt in the water tank until the soaking requirement is reached, and then the soaking conveyor belt brings the nylon fasteners out of the water tank and drops them into the receiving box; its characteristics are: using an intermittent operation mode, first according to the specific needs of the nylon fasteners, determine the required soaking temperature and time, and then according to the length of the water tank and the conveying speed of the soaking conveyor belt, determine the required pause time and number, so that after the nylon fasteners have passed the determined number of pauses, the time when the soaking conveyor belt brings the nylon fasteners out of the water tank is exactly the soaking time required by the nylon fasteners. This method can ensure that the soaking time of the nylon fasteners meets the requirements.

[0011] Furthermore, the intermittent operation method is to arrange a soaked conveyor belt through a water trough, one end of the conveyor belt is set in the water trough below the material receiving belt, for receiving the nylon fasteners coming out of the molding equipment; the other end of the conveyor belt is raised from the end of the water trough and extends out of the water trough to bring the nylon fasteners soaked in water out of the water trough; a baffle is set at a certain distance on the conveyor belt, and the material receiving belt brings the newly formed nylon fasteners into the baffle space; the distance of each intermittent operation of the soaked conveyor belt is an integer multiple of the baffle spacing, and the soaking time is controlled by intermittent operation.

[0012] Furthermore, the time and number of pauses required are determined by controlling the conveyor belt from the material receiving belt to the nylon fastener in the water tank through an electrical control box, moving the conveyor belt to the other end, driving the nylon fastener to the raised end, and making the nylon fastener out of the water pause for a certain number of times and time to meet the time control requirement for soaking the nylon fastener in water.

[0013] Furthermore, the time and number of pauses required are determined based on the soaking time required for different nylon fasteners at the determined soaking temperature, the length of the water tank and the speed at which the conveyor belt is connected from the material receiving belt to the nylon fasteners in the water tank, and moves to the other end of the conveyor belt to drive the nylon fasteners to the raised end, and the required number of pauses and pause time are calculated according to the integer multiples of the baffle spacing for each operation to ensure that the soaking time of the nylon fasteners when they are out of water is the required control time.

[0014] Furthermore, the method of calculating the required number of pauses and the pause time according to the integer multiples of the baffle spacing in each operation is to distribute the number of pauses and the pause time to ensure that the shipment volume of each movement can meet the product shipment volume of the molding equipment.

[0015] Furthermore, the water temperature in the water tank is controlled by a temperature sensor. A water inlet and a water outlet are provided at both ends of the water tank. When the temperature is over or the water level is too low, water is replenished through the water inlet. If the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 40-70℃.

[0016] Furthermore, the temperature of the nylon fastener when it comes out of water is controlled at 50-60°C, the water absorption rate of the nylon fastener reaches 0.3%-0.5%, and the flatness of the nylon fastener reaches 0.5mm.

[0017] Furthermore, the nylon fastener water-immersing automatic conveyor line of the nylon fastener water-immersing method includes a water trough, a material receiving belt, and a water-immersing conveyor belt. One end of the water-immersing conveyor belt is arranged at the bottom of one end of the water trough, below the material receiving belt, and the other end of the water-immersing conveyor belt extends from the bottom of the water trough to the other end of the water trough, and is upward from the end to expose the water surface and the upper surface of the water trough, and extend outside the water trough.

[0018] Furthermore, a plurality of baffles are provided on the upper surface of the water-soaked conveyor belt, so that the water-soaked conveyor belt forms a spaced conveyor belt in sections, and the conveyor belt runs intermittently in the water tank in multiples of the spacing distance formed by the baffles.

[0019] Furthermore, a temperature controller is provided in the water tank, and the temperature control range is 40-70°C, which is the most suitable temperature for nylon parts to be soaked in water.

[0020] Furthermore, a water shield is arranged at the connection part between the water-soaked conveyor belt and the material receiving belt section, which can shield the splashes generated by the nylon fastener falling into the water; the raised part of the water-soaked conveyor belt is connected to the material dropping chute, and the material dropping chute is connected to the material receiving box.

[0021] The beneficial effects of the present invention are: The present invention adopts an intermittent operation mode to soak the nylon fasteners in water, and controls the soaking time by controlling the number of pauses or time, so that different soaking operations can be effectively performed on different nylon fasteners, and has the following advantages: (1) The intermittent operation mode is adopted, and the time that the nylon fastener stays in the water tank can be adjusted arbitrarily. Therefore, for the same equipment and the same water tank length, different products can be soaked in water; the soaking process of nylon fasteners is optimized, and the demand for the site of the soaking process is reduced; (2) Through the intermittent operation of the conveyor belt, the pause time or number of the conveyor belt can be controlled. Both can be flexibly selected to meet the product output needs of various molding equipment. According to the size of product shipments and the soaking time requirements, the pause number and pause time of the intermittent operation can be matched respectively to find the most suitable matching pause time and number; effectively improve the water absorption rate and mechanical properties of nylon fasteners, while reducing energy consumption and scrap rate; (3) The intermittent operation described above adopts the method of setting partitions on the conveyor belt and allowing the conveyor belt to run intermittently in the water tank according to the multiple of the conveyor belt interruption, which can ensure that the nylon fasteners can be effectively soaked in water in batches. The soaking time of each batch of nylon fasteners is uniform and there will be no confusion, thereby ensuring the soaking effect of the nylon fasteners; (4) Thermometers are set at both ends of the water tank to control the water temperature at any time, further improving the water absorption accuracy of the water, and achieving the accurate water absorption rate required for each type of nylon fastener; (5) By arranging a water shield at the connection part between the soaked conveyor belt and the receiving belt section, it is possible to effectively prevent water splashing when the products coming out of the molding equipment fall into the water tank and pollute the production site. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a top view structural diagram of the nylon parts soaking and automatic conveying equipment; Figure 2 This is a front view structural diagram of the nylon parts soaking and automatic conveying equipment; Explanation of the reference numerals: (1) water trough conveying assembly; (2) material receiving belt; (3) electrical control box; (4) material receiving box; (5) water shield; (6) drain mesh plate; (7) material drop chute; (8) conveyor belt. DETAILED DESCRIPTION

[0023] The present invention is a technical improvement made by the inventor in the actual work process in order to solve specific problems. In the existing nylon parts soaking in water, the inventor also set up a continuous automatic soaking line in order to realize the automatic soaking operation. Initially, a continuous soaking process was adopted, that is, the conveyor belt in the water tank was driven by a motor to run continuously. Since the speed of the motor is constant, the speed of the conveyor belt driven by the reducer in the water tank is also constant. In this way, for a single nylon fastener, the length of the water tank can be adjusted according to requirements, or the reduction rate of the motor and the reducer can be adjusted to meet the soaking requirements; but for a variety of nylon fasteners with different soaking requirements, it is difficult to meet the soaking requirements of various nylon fasteners; there are two main reasons: First, the length of the water tank is difficult to change, especially for workplaces with limited space. It is difficult to meet the water requirements of various nylon fasteners by adjusting the length of the water tank. The second is to adjust the speed of the motor to change the moving speed of the conveyor belt in the water tank to meet the soaking requirements of various nylon fasteners. It is necessary to use a variable speed motor, but it is difficult to determine the motor speed change conditions for specific nylon fasteners, and it is also difficult to accurately control the motor speed; on the other hand, even if the speed conditions are met, after actual testing, it is found that this continuous operation still has a big problem, that is, in order to ensure that the conveyor belt can drive the nylon fasteners to move upward when the water is discharged, a partition must be added to the conveyor belt, but when the conveyor belt moves at a uniform speed, it is easy for the formed nylon fasteners brought down by the material receiving belt to fall on the partition, which will cause some nylon fasteners in the same period to fall in front of the partition, and some to fall behind the partition, so that there will be two different soaking results in the same period, thereby affecting the soaking effect of the product. For this reason, after repeated research, the inventor proposed an intermittent operation method for soaking operations; the following will be combined with the attached Figure 1~2 The present invention is further described. Specific embodiment one:

[0024] A method for soaking nylon fasteners in water, wherein the soaked nylon fasteners involved are straight-insert nylon lock buckles. According to the water absorption rate requirements of the straight-insert nylon lock buckles, it is necessary to soak the products in water at a water temperature of 40 degrees after they are formed, so that the water absorption rate of the nylon fasteners reaches 0.3%, and the flatness of the nylon fasteners reaches 0.5 mm. According to calculations, the soaking time required is 60 minutes; injection molding is used for production, and the production batch size is 10 products per minute; the water tank length selected according to the site size is 6 meters, and the interruption of the conveyor belt 8 is 0.5 meters long per section. The nylon fastener soaking method of this embodiment includes the following steps: A. Determine the relevant soaking parameters: for the straight-insert nylon lock, the required soaking time is 60 minutes, and the water tank length is 6 meters; the soaking temperature is 40°; the conveying speed of the soaking conveyor belt 8 is determined to be 0.1 m / s; the production batch size is 10 products per minute.

[0025] B. Determine the intermittent operation mode according to the required soaking time: according to the production batch size of 10 products per minute, the conveyor belt 8 has an interval of 0.5 meters, and the conveyor belt 8 needs to run at least once every 10 minutes; otherwise, there will be too many products in the same interval; according to the length of the water tank of 6 meters, the effective soaking length of the conveyor belt 8 in the water tank is only 5 meters (with a 1-meter water outlet section), and the conveying speed of the soaked conveyor belt 8 is 0.1 meters per second; the running time of each interval from beginning to end is 45 seconds; there are 10 intervals in the water; according to the interval of pausing once each time it runs, the number of pauses of the conveyor belt 8 in the water tank is 9 times; in order to meet the soaking time of 60 minutes, each pause time should be 7 minutes.

[0026] C. The conveying speed of the conveyor belt 8 is controlled by the electrical control box 3 to be 0.1 m / s. The conveyor belt 8 adopts an intermittent operation mode. It runs for 5 seconds and travels a discontinuity of 0.5 m, so that the next discontinuity is just under the material receiving belt 2. It pauses for 7 minutes. No matter how many products are in the discontinuity at this time, it will run for another 5 seconds and travel a discontinuity of 0.5 m, so that the next discontinuity is just under the material receiving belt 2. This is repeated. After 9 pauses, the first discontinuity reaches the tail end of the water tank, and then runs for another discontinuity to bend up and out of water. The soaking is completed, and the water is drained during the pause of the upturn. After reaching the top of the conveyor belt 8, it will fall into the material receiving box 4 to complete the soaking operation of the entire product. The soaking length is 5 meters, and the number of pauses is 9 times.

[0027] Note when working: 1) The 2 sections of the material receiving belt bring the newly formed straight-insert nylon lock into the baffles of the water tank of the water tank conveying assembly 1, and place the straight-insert nylon lock on the water tank conveying belt 8, so that all the straight-insert nylon locks are immersed in water as a whole.

[0028] 2) The newly formed straight-insert nylon lock falls into the water tank to increase the water temperature, which is controlled by a temperature sensor. There are water inlets and outlets at both ends of the water tank. When the temperature is over or the water level is too low, water is replenished through the water inlet. When the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 40°.

[0029] 3) The soaked conveyor belt 8 operates intermittently at a conveying speed of 0.1 m / s. It pauses for 7 minutes after running 0.5 m. The length of the soaked conveyor belt 8 is 5 m. After 9 pauses, the straight-insert nylon lock is brought from the water tank to the raised end. At this time, the soaking time of the straight-insert nylon lock is 30 minutes.

[0030] 4) The straight-insert nylon lock is dried on the drain mesh plate 6, and the water drops hung on the straight-insert nylon lock drip from the holes at the upper end of the drain mesh plate 6.

[0031] 5) The conveyor belt 8 continues to move, and the straight-insert nylon lock falls from the raised section of the conveyor belt 8 into the receiving box 4. Specific embodiment 2:

[0032] The nylon fastener soaking method of this embodiment includes the following steps: A method for soaking nylon fasteners in water, wherein the soaked nylon fasteners involved are spring bar type I fasteners. According to the water absorption rate requirements of spring bar type I fasteners, it is necessary to soak the products in water at a water temperature of 50 degrees after they are formed, so that the water absorption rate of the nylon fasteners reaches 0.4%, and the flatness of the nylon fasteners reaches 0.5 mm. According to calculations, the soaking time required is 90 minutes; injection molding is used for production, and the production batch size is 8 products per minute; the water trough length selected according to the site size is 7 meters, and the interruption of the conveyor belt 8 is 0.5 meters long per section. The nylon fastener soaking method of this embodiment includes the following steps: A. Determine the relevant soaking parameters: For spring bar type I fasteners, the required soaking time is 90 minutes and the water tank length is 7 meters; the soaking temperature is 50°; the conveying speed of the soaking conveyor belt 8 is determined to be 0.1 m / s; the production batch size is 10 products per minute.

[0033] B. Determine the intermittent operation mode according to the required soaking time: according to the production batch size of 8 products per minute, the conveyor belt 8 has an interval of 0.5 meters, and the conveyor belt 8 needs to run at least once every 10 minutes; otherwise, there will be too many products in the same interval; according to the length of the water tank of 7 meters, the effective soaking length of the conveyor belt 8 in the water tank is only 6 meters, and the conveying speed of the soaked conveyor belt 8 is 0.1 meters per second; the running time of each interval from beginning to end is 55 seconds; there are 12 intervals in the water; according to the pause of one interval each time the conveyor belt 8 runs, the number of pauses in the water tank is 11 times; in order to meet the soaking time of 90 minutes, each pause time should be 8.5 minutes.

[0034] C. The conveying speed of the conveyor belt 8 is controlled by the electrical control box 3 to be 0.1 m / s. The conveyor belt 8 adopts an intermittent operation mode. It runs for 5 seconds and travels a 0.5 m interval so that the next interval is just opposite to the bottom of the material receiving belt 2. It then pauses for 8.5 minutes. No matter how many products are in the interval at this time, it will run for another 5 seconds and travel a 0.5 m interval so that the next interval is just opposite to the bottom of the material receiving belt 2. This is repeated. After 11 pauses, the first interval reaches the tail end of the water tank. Then the interval is tilted upward to discharge water, and the soaking is completed. The water is drained during the upward pause. After reaching the top of the conveyor belt 8, it will fall into the material receiving box 4 to complete the soaking operation of the entire product. The soaking length is 6 meters, and the number of pauses is 11 times.

[0035] Note when working: 1) The 2 sections of the material receiving belt bring the newly formed spring bar type I fasteners into the baffles of the water tank of the water tank conveying assembly 1, and place the spring bar type I fasteners on the water tank conveying belt 8, so that all the spring bar type I fasteners are immersed in water as a whole.

[0036] 2) The newly formed spring bar I type fastener falls into the water tank to increase the water temperature, which is controlled by a temperature sensor. There are water inlets and outlets at both ends of the water tank. When the temperature is over or the water level is too low, water is replenished through the water inlet. When the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 50°.

[0037] 3) The water-soaked conveyor belt 8 operates at a conveying speed of 0.1 m / s in an intermittent manner, pausing for 7 minutes after running 0.5 m. The length of the water-soaked conveyor belt 8 is 6 m. After 11 pauses, the spring bar type I fastener is brought from the water tank to the raised end. At this time, the immersion time of the spring bar type I fastener is 90 minutes.

[0038] 4) The spring bar type I fastener is dried on the drain mesh plate 6, and the water drops hung on the spring bar type I fastener drip from the holes at the upper end of the drain mesh plate 6.

[0039] 5) The conveyor belt 8 continues to move, and the spring bar type I fastener falls from the raised section of the conveyor belt 8 into the receiving box 4. Specific embodiment three:

[0040] The nylon fastener soaking method of this embodiment includes the following steps: A method for soaking nylon fasteners in water, wherein the soaked nylon fastener involved is a Type II fastener baffle seat. According to the water absorption rate requirement of the Type II fastener baffle seat, it is necessary to soak the product in water at a water temperature of 50 degrees after the product is formed, so that the water absorption rate of the nylon fastener reaches 0.5%, and the flatness of the nylon fastener reaches 0.5mm. According to calculation, the soaking time required is 100 minutes; injection molding is used for production, and the production batch size is 10 products per minute; the water trough length selected according to the site size is 8 meters, and the interruption of the conveyor belt 8 is 0.5 meters long per section. The nylon fastener soaking method of this embodiment includes the following steps: A. Determine the relevant soaking parameters: Type II fastener baffle seat, the required soaking time is 100 minutes, the water tank length is 8 meters; the soaking temperature is 50°; the conveying speed of the soaking conveyor belt 8 is determined to be 0.1 m / s; the production batch size is 10 products per minute.

[0041] B. Determine the intermittent operation mode according to the required soaking time: according to the production batch size of 10 products per minute, the conveyor belt 8 has an interval of 0.5 meters, and the conveyor belt 8 needs to run at least once every 10 minutes; otherwise, there will be too many products in the same interval; according to the length of the water tank of 8 meters, the effective soaking length of the conveyor belt 8 in the water tank is only 7 meters, and the conveying speed of the soaked conveyor belt 8 is 0.1 meters per second; the running time of each interval from beginning to end is 65 seconds; there are 14 intervals in the water; according to the pause of one interval each time the conveyor belt 8 runs, the number of pauses in the water tank is 13 times; in order to meet the soaking time of 100 minutes, each pause time should be 8 minutes.

[0042] C. The conveying speed of the conveyor belt 8 is controlled by the electrical control box 3 to be 0.1 m / s. The conveyor belt 8 adopts an intermittent operation mode, first pauses for 8 minutes and then runs for 5 seconds, moves a break of 0.5 m, so that the next break is just under the material receiving belt 2, and then pauses for 8.5 minutes. No matter how many products are in the break at this time, it will run for another 5 seconds, move a break of 0.5 m, so that the next break is just under the material receiving belt 2, and repeat this process. After 13 pauses, the first break reaches the tail end of the water tank, and then the break is upturned to discharge water, and the soaking is completed. The water is drained during the upturned pause, and after reaching the top of the conveyor belt 8, it will fall into the material receiving box 4, completing the soaking operation of the entire product. The soaking length is 7 meters, and the number of pauses is 13 times.

[0043] Note when working: 1) The 2 sections of the material receiving belt bring the newly formed Type II fastener baffle seat into the baffles of the water tank of the water tank conveying assembly 1, and place the Type II fastener baffle seat on the water tank conveying belt 8, so that all the Type II fastener baffle seats are immersed in water as a whole.

[0044] 2) The newly formed Type II fastener baffle seat falls into the water tank to increase the water temperature, which is controlled by a temperature sensor. A water inlet and a water outlet are provided at both ends of the water tank. When the temperature is over or the water level is too low, water is replenished through the water inlet. When the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 50°.

[0045] 3) The soaked conveyor belt 8 operates at a conveying speed of 0.1 m / s in an intermittent manner, pausing for 9 minutes after running 0.5 m. The length of the soaked conveyor belt 8 is 7 m. After 13 pauses, the Type II fastener baffle seat is brought from the water tank to the raised end. At this time, the soaking time of the Type II fastener baffle seat is 100 minutes.

[0046] 4) The type II fastener baffle seat is dried on the drain mesh plate 6, and the water drops hanging on the type II fastener baffle seat drip from the holes at the upper end of the drain mesh plate 6.

[0047] 5) The conveyor belt 8 continues to move, and the Type II fastener baffle seat falls from the raised section of the conveyor belt 8 into the receiving box 4.

[0048] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.

[0049] It can be seen from the above embodiments that the present invention also relates to a method for soaking nylon fasteners in water, wherein the newly formed nylon fasteners are brought into the water tank of the soaking tank conveying assembly 1 through the two sections of the material receiving belt, and the nylon fasteners are placed on the soaking conveyor belt 8, so that all the nylon fasteners are immersed in water as a whole, and move along with the soaking conveyor belt 8 in the water tank until the soaking requirement is reached, and then the soaking conveyor belt 8 takes the nylon fasteners out of the water tank and drops them into the material receiving box 4; the characteristic is that: an intermittent operation mode is adopted, and the required soaking temperature and time are determined according to the specific needs of the nylon fasteners, and then the required pause time and number are determined according to the length of the water tank and the conveying speed of the soaking conveyor belt 8, so that after the nylon fasteners have passed the determined number of pauses, the time when the soaking conveyor belt 8 takes the nylon fasteners out of the water tank is exactly the soaking time required by the nylon fasteners. This method can ensure that the soaking time of the nylon fasteners meets the standard.

[0050] Furthermore, the intermittent operation mode is to arrange the soaked conveyor belt 8 through the water trough, one end of the conveyor belt 8 is set in the water trough below the receiving belt 2, for receiving the nylon fasteners coming out of the molding equipment; the other end of the conveyor belt 8 is raised from the end of the water trough and extends out of the water trough to bring the nylon fasteners soaked in water out of the water trough; a baffle is set at a certain distance on the conveyor belt 8, and the receiving belt 2 brings the newly formed nylon fasteners into the baffle space; the distance of each intermittent operation of the soaked conveyor belt 8 is an integer multiple of the baffle spacing, and the soaking time is controlled by intermittent operation.

[0051] Furthermore, the time and number of pauses required are determined by controlling the conveyor belt 8 from the receiving belt 2 to the nylon fastener in the water tank through the electrical control box 3, moving to the other end of the conveyor belt 8, driving the nylon fastener to the raised end, so that the number of pauses and time for the nylon fastener to exit the water is increased to meet the time control requirement for the nylon fastener to be soaked in water.

[0052] Furthermore, the time and number of pauses required are determined based on the soaking time required for different nylon fasteners at the determined soaking temperature, according to the length of the water tank and the conveyor belt 8, from the receiving belt 2 to the nylon fasteners such as the water tank, and move to the other end of the conveyor belt 8 to drive the nylon fasteners to the tilted end. The required number of pauses and pause time are calculated according to the integer multiples of the baffle spacing of each operation to ensure that the soaking time of the nylon fasteners when they are out of water is the required control time.

[0053] Furthermore, the method of calculating the required number of pauses and the pause time according to the integer multiples of the baffle spacing in each operation is to distribute the number of pauses and the pause time to ensure that the shipment volume of each movement can meet the product shipment volume of the molding equipment.

[0054] Furthermore, the water temperature in the water tank is controlled by a temperature sensor. A water inlet and a water outlet are provided at both ends of the water tank. When the temperature is over or the water level is too low, water is replenished through the water inlet. If the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 40-70℃.

[0055] Furthermore, the temperature of the nylon fastener when it comes out of water is controlled at 50-60°C, the water absorption rate of the nylon fastener reaches 0.3%-0.5%, and the flatness of the nylon fastener reaches 0.5mm.

[0056] Furthermore, the nylon fastener water-immersed automatic conveyor line of the nylon fastener water-immersed method includes a water trough, a material receiving belt 2, and a water-immersed conveyor belt 8. One end of the water-immersed conveyor belt 8 is arranged at the bottom of one end of the water trough, below the material receiving belt 2, and the other end of the water-immersed conveyor belt 8 extends from the bottom of the water trough to the other end of the water trough, and is tilted upward from the end to expose the water surface of the water trough and the upper surface of the water trough, and extends outside the water trough. It is characterized in that: a plurality of baffles are arranged on the upper surface of the water-immersed conveyor belt 8, so that the water-immersed conveyor belt 8 forms a section of spaced conveyor belt 8, and the conveyor belt 8 runs intermittently in the water trough according to the spacing formed by the baffles. The tilted part of the water-immersed conveyor belt 8 is connected to the blanking chute 7, and the blanking chute 7 is connected to the receiving box 4).

[0057] Furthermore, a temperature controller is provided in the water tank, and the temperature control range is 40-70°C.

[0058] Furthermore, a water shield 5 is arranged at the connection part between the water-soaked conveyor belt 8 and the material receiving belt 2, which can block the splashes caused by the nylon fastener falling into the water; the raised part of the water-soaked conveyor belt 8 is connected to the drain mesh plate 7, and the drain mesh plate 7 is connected to the material receiving box 4.

[0059] The beneficial technical effects of the present invention are: The present invention adopts an intermittent operation mode to soak the nylon fasteners in water, and controls the soaking time by controlling the number of pauses or time, so that different soaking operations can be effectively performed on different nylon fasteners, and has the following advantages: (1) The intermittent operation mode can adjust the time that the nylon fastener stays in the water tank at will. Therefore, the same equipment and the same water tank length can be used for soaking different products. The soaking process of nylon fasteners is optimized, reducing the demand for the site for the soaking process. (2) Through the intermittent operation of the conveyor belt, the pause time or number of the conveyor belt can be controlled. Both can be flexibly selected to meet the product output needs of various molding equipment. According to the size of product shipments and the soaking time requirements, the pause number and pause time of the intermittent operation can be matched respectively to find the most suitable matching pause time and number; effectively improving the water absorption rate and mechanical properties of nylon fasteners, while reducing energy consumption and scrap rate; (3) The intermittent operation is to set partitions on the conveyor belt, and allow the conveyor belt 8 to run intermittently in the water tank according to the multiple of the conveyor belt 8 interruption, which can ensure that the nylon fasteners can be effectively soaked in water in batches. The soaking time of each batch of nylon fasteners is uniform and there will be no confusion, thereby ensuring the soaking effect of the nylon fasteners; (4) Thermometers are set at both ends of the water tank to control the water temperature at any time, further improving the water absorption accuracy of the soaking water to achieve the accurate soaking water absorption rate required for each type of nylon fastener; (5) By arranging a water shield 5 at the connection portion between the soaking conveyor belt 8 and the receiving belt 2, it is possible to effectively prevent water splashing when the products coming out of the molding equipment fall into the water tank, thereby polluting the production site.

Claims

1. A method for soaking nylon fasteners in water, wherein a newly formed nylon fastener is brought into a water tank of a soaking tank conveying assembly (1) through a material receiving belt (2), and the nylon fastener is placed on a soaking conveyor belt (8), so that all the nylon fasteners are immersed in water as a whole, and move along the soaking conveyor belt (8) in the water tank until the soaking requirement is met, and then the soaking conveyor belt (8) brings the nylon fasteners out of the water tank and drops them into a material receiving box (4); the method is characterized in that: An intermittent operation method is adopted. First, the required soaking temperature and time are determined according to the specific needs of the nylon fasteners. Then, according to the length of the water tank, the conveying speed of the soaking conveyor belt (8), the required pause time and number of times are determined, so that after the nylon fasteners have stopped for the determined number of times, the time when the soaking conveyor belt (8) takes the nylon fasteners out of the water tank is exactly the soaking time required for the nylon fasteners.

2. The method for soaking nylon fasteners in water according to claim 1, characterized in that: The intermittent operation method is to arrange a soaked conveyor belt (8) through a water tank, one end of the conveyor belt (8) is arranged in the water tank below the receiving belt (2) for receiving the nylon fasteners coming out of the molding equipment; the other end of the conveyor belt (8) is tilted from the end of the water tank and extends out of the water tank to bring the soaked nylon fasteners out of the water tank; a baffle is arranged at a certain distance on the conveyor belt (8), and the receiving belt (2) brings the newly formed nylon fasteners into the baffle space; the distance of each intermittent operation of the soaked conveyor belt (8) is an integer multiple of the baffle spacing, and the soaking time is controlled by intermittent operation.

3. The method for soaking nylon fasteners in water according to claim 1, characterized in that: The time and number of pauses required are determined by controlling the conveyor belt (8) from the material receiving belt (2) to the nylon fastener connected to the water tank through the electrical control box (3), moving to the other end of the conveyor belt (8), driving the nylon fastener to the raised end, so that the number and time of pauses for the nylon fastener to exit the water are controlled to meet the time control requirement for the nylon fastener to be soaked in water.

4. The method for soaking nylon fasteners in water according to claim 3, characterized in that: The time and number of pauses required are determined based on the soaking time required for different nylon fasteners at the determined soaking temperature, the length of the water tank and the conveyor belt (8) from the receiving belt (2) to the nylon fasteners such as the water tank, and the running speed at which the nylon fasteners are driven to the tilted end at the other end of the conveyor belt (8), and the required number of pauses and pause time are calculated according to the integer multiples of the baffle spacing of each operation, so as to ensure that the soaking time of the nylon fasteners when they are out of water is the required control time.

5. The method for soaking nylon fasteners in water according to claim 3, characterized in that: The method of calculating the required number of pauses and the pause time according to the integer multiples of the baffle spacing in each operation is to distribute the number of pauses and the pause time to ensure that the shipment volume of each movement can meet the product shipment volume of the molding equipment.

6. The method for soaking nylon fasteners in water according to claim 4, characterized in that: The water temperature in the water tank is controlled by a temperature sensor. There are water inlet and outlet at both ends of the water tank. When the temperature is over or the water level is too low, water is added through the water inlet. When the water level is too high, water is discharged through the water outlet. The water temperature is controlled at 40-70℃.

7. The method for soaking nylon fasteners in water according to claim 6, characterized in that: The temperature of the nylon fasteners when they are out of water is controlled at 50-60°C, the water absorption rate of the nylon fasteners reaches 0.3%-0.5%, and the flatness of the nylon fasteners reaches 0.5mm.

8. A nylon fastener soaking automatic conveyor line for realizing the nylon fastener soaking method according to any of claims 1 to 7, comprising a water tank, a material receiving belt (2), and a soaking conveyor belt (8), wherein one end of the soaking conveyor belt (8) is arranged at the bottom of one end of the water tank, below the material receiving belt (2), and the other end of the soaking conveyor belt (8) extends from the bottom of the water tank to the other end of the water tank, and is tilted upward from the end to expose the water surface of the water tank and the upper surface of the water tank, and extends outside the water tank, the tilted part of the soaking conveyor belt (8) is connected to the blanking chute (7), and the blanking chute (7) is connected to the material receiving box (4), characterized in that: A plurality of baffles are arranged on the upper surface of the water-soaked conveyor belt (8), so that the water-soaked conveyor belt (8) forms a segmented conveyor belt (8), and the conveyor belt (8) runs intermittently in the water tank according to the intervals formed by the baffles.

9. The nylon fastener soaking automatic conveying line as claimed in claim 8, characterized in that: A temperature controller is provided in the water tank, and the temperature control range is 40-70°C.

10. The nylon fastener soaking automatic conveying line as claimed in claim 8, characterized in that: The connection portion between the water-soaked conveyor belt (8) and the material receiving belt (2) is provided with a water shield (5) which can shield the splashes generated when the nylon fastener falls into the water.

Citation Information

Patent Citations

  • Novel energy-saving flat-lying film cooling device

    CN112060430A

  • Railway fastener elastic strip quenching conveying device

    CN115196267A

  • Mobile Phone Case with Bottle Opener

    KR1020240157224A