Method for treating nanofiltration concentrated solution

Through the combination of selective electrodialysis and advanced oxidation process, monovalent and divalent ions and organic matter in the nanofiltration concentrate are separated and removed, which solves the problems of scaling and organic matter in wastewater concentration, and realizes the production of pure salt and free of charge. Waste technology has good economic and environmental benefits.

CN118724311APending Publication Date: 2024-10-01BAOSHAN IRON & STEEL CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202310339897.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the wastewater concentration process, the concentration of scaling ions and organic matter affects process stability and the quality of crystallized salts. Existing technology is difficult to effectively separate monovalent and divalent ions and remove organic matter, resulting in a large number of impurities in the product and the inability to effectively utilize nanofiltration. Concentrate.

Method used

A selective electrodialysis system is used to separate monovalent and divalent ions, and organic matter is removed through an advanced oxidation process and a catalyst oxidation tower loaded with Fe, Mn and Ce, combined with a disk reverse osmosis and frozen crystallization system to separate sodium sulfate to form pure Sodium chloride and sodium sulfate salts.

Benefits of technology

It realizes waste-free production of sodium chloride and sodium sulfate salts, has dual economic and environmental benefits, and improves the quality and process stability of the concentrate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0004157860440000011
    Figure HDA0004157860440000011
Patent Text Reader

Abstract

The invention discloses a treatment method of a nanofiltration concentrated solution, which comprises the following steps: the nanofiltration concentrated solution enters a selective electrodialysis system for electrodialysis treatment; discharge liquid of the concentration chamber and water produced by the nanofiltration salt separation process are mixed and then enter a sodium chloride concentration, evaporation and crystallization system together to produce sodium chloride salt; discharging liquid of the desalting chamber enters a next treatment process; h2O2 is added into discharge liquid of a desalination chamber to serve as an oxidizing agent, the discharge liquid is pumped into a catalytic oxidation tower, organic matter in the wastewater is oxidized into CO2 and H2O or small-molecular-weight organic matter, effluent of a catalytic oxidation system enters a disc type reverse osmosis (DTRO) system, and water produced by the DTRO system is returned before the DTRO system; the concentrated water enters a freezing crystallization system, the temperature of the concentrated water is reduced to 5-10 DEG C, sodium sulfate crystals are separated from the concentrated water, and crystallization mother liquor obtained after freezing crystallization returns to the nanofiltration concentrated liquor pool. Sodium chloride salt and sodium sulfate salt are generated after treatment by the method, and no waste is generated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of wastewater treatment, and in particular to a treatment process and method for nanofiltration concentrated liquid. Background Art

[0002] Zero wastewater discharge has become a development trend. Desalination and concentration are the main processes to achieve zero wastewater discharge. However, wastewater generally has complex components and contains a variety of inorganic ions, among which the main anions are Cl-, SO4 2- 、CO3 2- etc., the cations are mainly Na + , Ca 2+ Mg 2+ In the process of wastewater concentration, various inorganic ions will be concentrated exponentially, and SO4 2- 、CO3 2- and Ca 2+ Mg 2+ Scaling ions such as Ca and Mg will cause scaling due to exceeding the solubility product, thus affecting the normal operation of the concentration process. Therefore, the wastewater needs to be softened before concentration to reduce the Ca in the wastewater. 2+ Mg 2+ and CO3 2- After softening treatment, the main inorganic ions in the wastewater include Cl-, SO4 2- 、Na + . If direct evaporation and crystallization produces a mixture of sodium chloride and sodium sulfate, that is, impure salts, it cannot be used. Therefore, salt separation is required during the concentration process to separate sodium chloride from sodium sulfate. Nanofiltration is one of the commonly used salt separation processes. After nanofiltration, the water side is pure sodium chloride, which can be produced after evaporation and crystallization. However, the concentrated water side is a mixture of sodium chloride and sodium sulfate, and impure salts of sodium chloride and sodium sulfate will still be produced during evaporation and crystallization. Therefore, it is still necessary to further separate the salt of the nanofiltration concentrate.

[0003] In addition, during the desalination and concentration process, the organic matter in the wastewater will be concentrated exponentially. The organic matter in the wastewater will not only affect the stable operation of the concentration process, but also affect the quality of the crystallized salt. Therefore, the organic matter in the concentrate should be removed.

[0004] CN201410580324.7 The nanofiltration concentrate produced by high-salinity wastewater is fed into an evaporation system to obtain solids. CN201610547062.3 The nanofiltration concentrate and nanofiltration permeate are passed through a membrane concentration device to obtain produced water and concentrated water; the concentrated water is fed into an evaporation system for concentration and crystallization. CN201210028923.9 The nanofiltration concentrate and nanofiltration saline leachate from the nanofiltration membrane device are fed into a forward osmosis membrane device, wherein the nanofiltration concentrate is used as a driving liquid of the forward osmosis membrane device to perform forward osmosis concentration on the nanofiltration saline leachate. Summary of the invention

[0005] Therefore, the technical problem to be solved by the present invention is a process and method for treating nanofiltration concentrated liquid.

[0006] The technical solution of the present invention is a method for treating a nanofiltration concentrate, comprising the following steps:

[0007] a. The nanofiltration concentrate enters the selective electrodialysis system; the electrolyte is injected into the anode chamber and the cathode chamber respectively; the nanofiltration concentrate is injected into the desalination chamber, and pure water is injected into the concentration chamber; the volume ratio of the desalination chamber to the concentration chamber is 1.2:1 to 2:1, and electrodialysis treatment is performed; a monovalent cation selective electrodialysis membrane and a monovalent anion selective electrodialysis membrane are respectively installed in the selective electrodialysis system; the voltage is controlled at 2 to 4V during the electrodialysis process, and the hydraulic retention time is 15 to 90min;

[0008] b. The effluent from the concentration chamber is mixed with the produced water from the nanofiltration salt separation process and then enters the sodium chloride concentration evaporation crystallization system to produce sodium chloride salt; the effluent from the desalination chamber enters the next treatment process;

[0009] c. Add H2O2 as an oxidant to the desalination chamber discharge liquid, and the amount of H2O2 added is 2:1 to 3:1 according to the mass ratio of H2O2:COD; pump the desalination chamber discharge liquid after adding H2O2 into a catalytic oxidation tower placed with a high-efficiency catalyst, and under the catalytic action of the catalyst, the oxidant H2O2 oxidizes the organic matter in the wastewater into CO2 and H2O, or oxidizes it into small molecular organic matter; the hydraulic retention time of the catalytic oxidation tower is 30 to 120 minutes; the catalyst is a molecular sieve catalyst loaded with Fe, Mn and Ce;

[0010] d. The effluent from the catalytic oxidation tower enters the disc-type reverse osmosis DTRO system, and the produced water from the DTRO is returned to the front of the reverse osmosis system; the concentrated water enters the freezing crystallization system, the temperature of the concentrated water is cooled to 5-10°C, sodium sulfate crystals are separated from the concentrated water, and the crystallization mother liquor of the freezing crystallization is returned to the nanofiltration concentrated liquid pool.

[0011] In step a, the monovalent cation selective electrodialysis membrane only allows monovalent cations to pass into the concentrated chamber, while divalent cations cannot pass through and are retained in the dilute chamber; the monovalent anion selective electrodialysis membrane only allows monovalent anions to pass into the concentrated chamber, while divalent anions cannot pass through and are retained in the dilute chamber. The separation of monovalent chloride ions and divalent sulfate ions can be achieved by selective electrodialysis. In addition, since organic matter is uncharged, most of it will also remain in the dilute chamber.

[0012] In step b, the electrodialysis concentration chamber discharges mainly monovalent sodium chloride, and the desalination chamber discharges mainly divalent sulfate and a small amount of monovalent salt and organic matter. In step c, the dosage of H2O2 is two to three times that of COD. For example, if COD is 200 mg / L, the dosage of H2O2 is 400-600 mg / L. The function of the high-efficiency catalyst is to accelerate the oxidation reaction and improve the treatment effect of organic matter. Under the catalytic action of the catalyst, the oxidant H2O2 oxidizes the organic matter in the wastewater into CO2 and H2O, or oxidizes it into small molecular organic matter, thereby reducing the COD concentration in the effluent from the desalination chamber.

[0013] In step d, the solubility of sodium sulfate decreases at low temperatures, and sodium sulfate crystallizes out in the form of crystals.

[0014] According to a method for treating a nanofiltration concentrate of the present invention, preferably, the nanofiltration concentrate is a concentrate produced by a nanofiltration salt separation process, and is subjected to softening pretreatment, reverse osmosis concentration and other processes before nanofiltration.

[0015] According to a method for treating a nanofiltration concentrate of the present invention, preferably, the preparation process of the high-efficiency catalyst in step c is as follows:

[0016] (1) Using molecular sieve, first rinse the molecular sieve with water and dry it;

[0017] (2) After rinsing and drying, the molecular sieve is soaked in FeSO4 with a concentration of 0.1 to 0.5 mol at room temperature for 4 to 6 hours, so that the FeSO4 is fully immersed in the molecular sieve; then the mixed solution of the molecular sieve and FeSO4 is placed in a hydrothermal reactor, and the hydrothermal reactor is placed in a heating device, the temperature of the heating device is maintained at 140 to 160°C, maintained for 6 to 8 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4 is taken out of the reactor, rinsed with water, and dried in an oven at 90-120°C;

[0018] (3) The molecular sieve loaded with FeSO4 is soaked in a mixed solution of 0.01-0.03 mol Mn(NO3)2 and 0.01-0.03 mol Ce(NO3)3 at room temperature for 4-6 hours, so that Mn(NO3)2 and Ce(NO3)3 are fully immersed in the molecular sieve; then the molecular sieve and the mixed solution of Mn(NO3)2 and Ce(NO3)3 are placed in a hydrothermal reactor, and the hydrothermal reactor is placed in a heating device, the temperature of the heating device is maintained at 140-160°C, maintained for 6-8 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 is taken out of the reactor, rinsed with water, and dried in an oven at 90-120°C to obtain a high-efficiency catalyst loaded with Fe, Mn and Ce.

[0019] The hydrothermal reactor is sealed and placed in a heating device for the purpose of heating.

[0020] Ferrous sulfate and H2O2 form the Fenton reaction, and Mn and Ce mainly play a catalytic role in the reaction.

[0021] According to a method for treating a nanofiltration concentrate of the present invention, in the preparation of the catalyst, preferably, the molecular sieve in step (1) is a Y-type molecular sieve. The main function of the molecular sieve is to provide a carrier for the catalyst.

[0022] According to a method for treating a nanofiltration concentrate of the present invention, in the preparation of a catalyst, preferably, the drying temperature in step (1) is 90-120° C. More preferably, the drying temperature is 100-110° C.

[0023] According to a method for treating a nanofiltration concentrate of the present invention, in the preparation of a catalyst, preferably, in step (2), the molecular sieve loaded with FeSO4 is rinsed with deionized water and dried in an oven at 100-110°C; in step (3), the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 is rinsed with water and dried in an oven at 100-110°C.

[0024] According to a method for treating a nanofiltration concentrate of the present invention, in the catalyst preparation, it is preferred that the water in steps (1), (2) and (3) is deionized water.

[0025] According to a method for treating a nanofiltration concentrate of the present invention, preferably, in step a, the water quality of the nanofiltration concentrate before water intake is: conductivity 30000-50000 μs / cm, chloride ion 8000-20000 mg / L, sulfate ion 4000-8000 mg / L, COD 200-600 mg / L. This is the water quality of the nanofiltration concentrate after softening pretreatment, reverse osmosis concentration and other processes.

[0026] According to a method for treating a nanofiltration concentrate of the present invention, preferably, the DTRO system described in step d concentrates the effluent from the catalytic oxidation system, and the sulfate content in the concentrated water reaches 100-120 g / L after concentration, and the sulfate concentration in the produced water is 400-800 mg / L.

[0027] According to the method for treating a nanofiltration concentrate of the present invention, preferably, the electrolyte in step a is a sodium hydroxide solution. Furthermore, the concentration of the sodium hydroxide solution is preferably 0.01-1 mol / L.

[0028] The beneficial effects of the present invention are:

[0029] The present invention provides a process and method for treating a nanofiltration concentrate. After the nanofiltration concentrate is subjected to selective electrodialysis and salt separation, the concentrated water enters a sodium chloride concentration evaporation crystallization system, and the fresh water is subjected to an advanced oxidation process to remove organic matter, and then DTRO concentration and freezing crystallization are performed to produce sodium sulfate crystals. After the treatment by the invention, sodium chloride salt and sodium sulfate salt are produced, and no waste is generated. The invention has both economic and environmental protection effects, and has good social and environmental benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 The present invention provides a process and method flow chart for treating a nanofiltration concentrated liquid. DETAILED DESCRIPTION

[0031] In order to better understand the present invention, the content of the present invention is further explained below in conjunction with embodiments, but the content of the present invention is not limited to the following embodiments.

[0032] Example 1

[0033] Water quality of nanofiltration concentrate: conductivity 42300μs / cm, chloride ion 13500mg / L, sulfate ion 5820mg / L, COD320mg / L.

[0034] The nanofiltration concentrate was injected into the desalination chamber, and pure water was injected into the concentration chamber. The volume ratio of the desalination chamber to the concentration chamber was 1.8:1, and electrodialysis treatment was performed. A monovalent cation selective electrodialysis membrane and a monovalent anion selective electrodialysis membrane were installed in the selective electrodialysis system. The voltage was controlled at 3V and the hydraulic retention time was 60min during the electrodialysis process.

[0035] The water quality of the electrodialysis concentration chamber is: conductivity 55200μs / cm, chloride ion 18500mg / L, sulfate ion 395mg / L, COD85mg / L; the water quality of the desalination chamber is: conductivity 15600μs / cm, chloride ion 1980mg / L, sulfate ion 5630mg / L, COD260mg / L.

[0036] H2O2 is added as an oxidant to the desalination chamber discharge liquid, and the dosage is 2.5:1. The desalination chamber discharge liquid with H2O2 added is pumped into a catalytic oxidation tower with a high-efficiency catalyst. The hydraulic retention time of the catalytic oxidation tower is 70 minutes. After the catalytic oxidation process, the effluent COD is 56mg / L.

[0037] The preparation process of high-efficiency catalyst is as follows:

[0038] Use Y-type molecular sieve, rinse the molecular sieve with deionized water, and dry it at 105°C. Soak the molecular sieve after rinsing and drying with 0.3 mol FeSO4 at room temperature for 5 hours, so that FeSO4 can fully penetrate into the molecular sieve; then place the mixed solution of molecular sieve and FeSO4 in a hydrothermal reactor, and place the hydrothermal reactor in an oven, keep the temperature of the oven at 150°C for 7 hours, and then cool to room temperature; then rinse the molecular sieve loaded with FeSO4 with deionized water and dry it in an oven at 105°C.

[0039] The molecular sieve loaded with FeSO4 was soaked in a mixed solution of Mn(NO3)2 and Ce(NO3)3 with a concentration of 0.02 mol at room temperature for 5 hours, so that Mn(NO3)2 and Ce(NO3)3 were fully immersed in the molecular sieve; then the molecular sieve and the mixed solution of Mn(NO3)2 and Ce(NO3)3 were placed in a hydrothermal reactor, and the hydrothermal reactor was placed in an oven, the temperature of the oven was maintained at 150°C, maintained for 7 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 was rinsed with deionized water and dried in an oven at 105°C. A highly efficient catalyst loaded with Fe, Mn and Ce was obtained.

[0040] The effluent from the catalytic oxidation system enters the disc-type reverse osmosis DTRO system. After concentration, the sulfate content in the concentrated water is 116g / L, and the sulfate concentration in the produced water is 620mg / L. The DTRO concentrated water enters the freezing crystallization system, where the temperature of the concentrated water is cooled to 7°C, and sodium sulfate is crystallized out in the form of crystals.

[0041] Example 2

[0042] Water quality of nanofiltration concentrate: conductivity 31200μs / cm, chloride ion 8230mg / L, sulfate ion 4150mg / L, COD226mg / L.

[0043] Inject nanofiltration concentrate into the desalination chamber and pure water into the concentration chamber. The volume ratio of the desalination chamber to the concentration chamber is 2:1, and electrodialysis treatment is performed. A monovalent cation selective electrodialysis membrane and a monovalent anion selective electrodialysis membrane are installed in the selective electrodialysis system. During the electrodialysis process, the voltage is controlled at 2V and the hydraulic retention time is 15min.

[0044] The water quality of the electrodialysis concentration chamber is: conductivity 41200μs / cm, chloride ion 12600mg / L, sulfate ion 312mg / L, COD62mg / L; the water quality of the desalination chamber is: conductivity 11200μs / cm, chloride ion 1350mg / L, sulfate ion 3920mg / L, COD185mg / L.

[0045] H2O2 is added as an oxidant to the desalination chamber discharge liquid, and the dosage is 2:1. The desalination chamber discharge liquid with H2O2 added is pumped into a catalytic oxidation tower with a high-efficiency catalyst. The hydraulic retention time of the catalytic oxidation tower is 30 minutes. After the catalytic oxidation process, the effluent COD is 48mg / L.

[0046] The preparation process of high-efficiency catalyst is as follows:

[0047] Use Y-type molecular sieve, rinse the molecular sieve with deionized water, and dry it at 100°C. Soak the molecular sieve after rinsing and drying with 0.5 mol FeSO4 at room temperature for 4 hours to allow FeSO4 to fully penetrate the molecular sieve; then place the mixed solution of molecular sieve and FeSO4 in a hydrothermal reactor, and place the hydrothermal reactor in an oven, keep the temperature of the oven at 160°C for 6 hours, and then cool to room temperature; then rinse the molecular sieve loaded with FeSO4 with deionized water and dry it in an oven at 110°C.

[0048] The molecular sieve loaded with FeSO4 was soaked in a mixed solution of Mn(NO3)2 and Ce(NO3)3 with a concentration of 0.01 mol at room temperature for 6 hours, so that Mn(NO3)2 and Ce(NO3)3 were fully immersed in the molecular sieve; then the molecular sieve and the mixed solution of Mn(NO3)2 and Ce(NO3)3 were placed in a hydrothermal reactor, and the hydrothermal reactor was placed in an oven, the temperature of the oven was maintained at 140°C, maintained for 8 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 was rinsed with deionized water and dried in an oven at 105°C. A highly efficient catalyst loaded with Fe, Mn and Ce was obtained.

[0049] The effluent from the catalytic oxidation system enters the disc-type reverse osmosis DTRO system. After concentration, the sulfate content in the concentrated water is 103g / L, and the sulfate concentration in the produced water is 450mg / L. The DTRO concentrated water enters the freezing crystallization system, where the temperature of the concentrated water is cooled to 5°C, and sodium sulfate crystallizes out in the form of crystals.

[0050] Example 3

[0051] Water quality of nanofiltration concentrate: conductivity 48600μs / cm, chloride ion 18500mg / L, sulfate ion 7520mg / L, COD535mg / L.

[0052] The nanofiltration concentrate was injected into the desalination chamber, and pure water was injected into the concentration chamber. The volume ratio of the desalination chamber to the concentration chamber was 1.2:1, and electrodialysis treatment was performed. A monovalent cation selective electrodialysis membrane and a monovalent anion selective electrodialysis membrane were installed in the selective electrodialysis system. The voltage was controlled at 4V and the hydraulic retention time was 90min during the electrodialysis process.

[0053] The water quality of the electrodialysis concentration chamber is: conductivity 43500μs / cm, chloride ion 16600mg / L, sulfate ion 830mg / L, COD126mg / L; the water quality of the desalination chamber is: conductivity 15600μs / cm, chloride ion 2150mg / L, sulfate ion 6780mg / L, COD406mg / L.

[0054] H2O2 is added as an oxidant to the desalination chamber discharge liquid, and the dosage is 3:1. The desalination chamber discharge liquid with H2O2 added is pumped into a catalytic oxidation tower with a high-efficiency catalyst. The hydraulic retention time of the catalytic oxidation tower is 120 minutes. After the catalytic oxidation process, the effluent COD is 78mg / L.

[0055] The preparation process of high-efficiency catalyst is as follows:

[0056] Use Y-type molecular sieve, rinse the molecular sieve with deionized water, and dry it at 110°C. Soak the molecular sieve after rinsing and drying with 0.1 mol FeSO4 at room temperature for 6 hours to allow FeSO4 to fully penetrate the molecular sieve; then place the mixed solution of molecular sieve and FeSO4 in a hydrothermal reactor, and place the hydrothermal reactor in an oven, keep the temperature of the oven at 140°C for 8 hours, and then cool to room temperature; then rinse the molecular sieve loaded with FeSO4 with deionized water and dry it in an oven at 105°C.

[0057] The molecular sieve loaded with FeSO4 was soaked in a mixed solution of Mn(NO3)2 and Ce(NO3)3 with a concentration of 0.03 mol at room temperature for 4 hours, so that Mn(NO3)2 and Ce(NO3)3 were fully immersed in the molecular sieve; then the molecular sieve and the mixed solution of Mn(NO3)2 and Ce(NO3)3 were placed in a hydrothermal reactor, and the hydrothermal reactor was placed in an oven, the temperature of the oven was maintained at 160°C, maintained for 6 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 was rinsed with deionized water and dried in an oven at 115°C. A highly efficient catalyst loaded with Fe, Mn and Ce was obtained.

[0058] The effluent from the catalytic oxidation system enters the disc-type reverse osmosis DTRO system. After concentration, the sulfate content in the concentrated water is 116g / L, and the sulfate concentration in the produced water is 780mg / L. The DTRO concentrated water enters the freezing crystallization system, where the temperature of the concentrated water is cooled to 10°C, and sodium sulfate crystallizes out in the form of crystals.

Claims

1. A method for treating a nanofiltration concentrate, characterized in that: The steps include: a. The nanofiltration concentrate enters the selective electrodialysis system; the electrolyte is injected into the anode chamber and the cathode chamber respectively; the nanofiltration concentrate is injected into the desalination chamber, and pure water is injected into the concentration chamber; the volume ratio of the desalination chamber to the concentration chamber is 1.2:1 to 2:1, and electrodialysis treatment is performed; a monovalent cation selective electrodialysis membrane and a monovalent anion selective electrodialysis membrane are respectively installed in the selective electrodialysis system; the voltage is controlled at 2 to 4V during the electrodialysis process, and the hydraulic retention time is 15 to 90min; b. The effluent from the concentration chamber is mixed with the produced water from the nanofiltration salt separation process and then enters the sodium chloride concentration evaporation crystallization system to produce sodium chloride salt; the effluent from the desalination chamber enters the next treatment process; c. Add H2O2 as an oxidant to the desalination chamber discharge liquid, and the amount of H2O2 added is 2:1 to 3:1 according to the mass ratio of H2O2:COD; pump the desalination chamber discharge liquid after adding H2O2 into a catalytic oxidation tower placed with a high-efficiency catalyst, and under the catalytic action of the catalyst, the oxidant H2O2 oxidizes the organic matter in the wastewater into CO2 and H2O, or oxidizes it into small molecular organic matter; the hydraulic retention time of the catalytic oxidation tower is 30 to 120 minutes; the catalyst is a molecular sieve catalyst loaded with Fe, Mn and Ce; d. The effluent from the catalytic oxidation tower enters the disc-type reverse osmosis DTRO system, and the produced water from the DTRO is returned to the front of the reverse osmosis system; the concentrated water enters the freezing crystallization system, the temperature of the concentrated water is cooled to 5-10°C, sodium sulfate crystals are separated from the concentrated water, and the crystallization mother liquor of the freezing crystallization is returned to the nanofiltration concentrated liquid pool.

2. The method for treating a nanofiltration concentrate according to claim 1, characterized in that: Nanofiltration concentrate is the concentrate produced by the nanofiltration salt separation process.

3. The method for treating a nanofiltration concentrate according to claim 1, characterized in that: The preparation process of the high-efficiency catalyst in step c is as follows: (1) Using molecular sieve, first rinse the molecular sieve with water and dry it; (2) After rinsing and drying, the molecular sieve is soaked in FeSO4 with a concentration of 0.1 to 0.5 mol at room temperature for 4 to 6 hours, so that the FeSO4 is fully immersed in the molecular sieve; then the mixed solution of the molecular sieve and FeSO4 is placed in a hydrothermal reactor, and the hydrothermal reactor is placed in a heating device, the temperature of the heating device is maintained at 140 to 160°C, maintained for 6 to 8 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4 is taken out of the reactor, rinsed with water, and dried in an oven at 90-120°C; (3) The molecular sieve loaded with FeSO4 is soaked in a mixed solution of 0.01-0.03 mol Mn(NO3)2 and 0.01-0.03 mol Ce(NO3)3 at room temperature for 4-6 hours, so that Mn(NO3)2 and Ce(NO3)3 are fully immersed in the molecular sieve; then the molecular sieve and the mixed solution of Mn(NO3)2 and Ce(NO3)3 are placed in a hydrothermal reactor, and the hydrothermal reactor is placed in a heating device, the temperature of the heating device is maintained at 140-160°C, maintained for 6-8 hours, and then cooled to room temperature; then the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 is taken out of the reactor, rinsed with water, and dried in an oven at 90-120°C to obtain a high-efficiency catalyst loaded with Fe, Mn and Ce.

4. The method for treating a nanofiltration concentrate according to claim 3, characterized in that: The molecular sieve in step (1) is a Y-type molecular sieve.

5. The method for treating a nanofiltration concentrate according to claim 3, characterized in that: The drying temperature in step (1) is 90-120°C.

6. The method for treating a nanofiltration concentrate according to claim 3, characterized in that: Step (2) rinse the molecular sieve loaded with FeSO4 with deionized water and dry it in an oven at 100-110°C; Step (3) rinse the molecular sieve loaded with FeSO4, Mn(NO3)2 and Ce(NO3)3 with water and dry it in an oven at 100-110°C.

7. The method for treating a nanofiltration concentrate according to claim 3, characterized in that: The water in steps (1), (2) and (3) is deionized water.

8. The method for treating a nanofiltration concentrate according to claim 1, characterized in that: In step a, the water quality of the nanofiltration concentrate before water inlet is: conductivity 30000-50000 μs / cm, chloride ion 8000-20000 mg / L, sulfate ion 4000-8000 mg / L, COD 200-600 mg / L.

9. The method for treating a nanofiltration concentrate according to claim 1, characterized in that: The DTRO system described in step d concentrates the effluent from the catalytic oxidation system. After concentration, the sulfate content in the concentrated water reaches 100-120 g / L, and the sulfate concentration in the produced water is 400-800 mg / L.

10. The method for treating a nanofiltration concentrate according to claim 1, characterized in that: The electrolyte in step a is sodium hydroxide solution.

Citation Information

Patent Citations

  • Fe-Mn double-metal heterogeneous Fenton catalyst taking molecular sieve as carrier as well as preparation method and application of catalyst

    CN104209138A

  • Method for pretreating wastewater from 2, 4-D acid synthesizing process

    CN106365366A

  • Resourceful treatment method for high-salt wastewater containing sodium chloride and sodium sulfate

    CN107304090A

  • Freezing salt separation system and freezing salt separation method

    CN111908677A

  • Preparation method and application of Fe-Ce-LDH / 13X granular catalyst for heterogeneous electro-Fenton system

    CN113842942A