Method for preparing cell membrane by using Pickering emulsion method

The amphiphilic polypeptide of Janus nanofibers with hydrophilic and isooctanol surface characteristics was prepared by the Pickering emulsion method to form stable cell membrane vesicles, which solved the problems of insufficient cell membrane stability and structural authenticity in the existing technology, and achieved Preparation of highly stable and functional biomimetic cell membranes.

CN118725024APending Publication Date: 2024-10-01王子徐
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410625148.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-20
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, lipid vesicles composed of pure phospholipids can only imitate the shape of cells and isolate the contents, but cannot truly simulate the structure of real cells. Moreover, the low stability of fatty acid materials and harsh chemical modification conditions limit their use in artificial cells. applications in.

Method used

The amphiphilic peptides of Janus nanofibers with hydrophilic and isooctanol-loving surface properties were prepared using the Pickering emulsion method, by forming a water-in-oil emulsion in isooctyl alcohol/water, and using the peptide fibers to stabilize the emulsion, followed by in situ cross-fertilization. Combined with solvent replacement, a biomimetic cell membrane with a closed membrane structure is formed.

Benefits of technology

The prepared cell membrane vesicles have high stability. The size change is less than 0.1 μm after five days at room temperature, and the shape remains intact after 360 days at 4°C. More than 70% of the polypeptides are folded as designed, and the cell membrane is permeable to dextran. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

The invention discloses a method for preparing a cell membrane by using a Pickering emulsion method, and belongs to the technical field of Pickering emulsions. The method comprises the following steps: (1) preparing polypeptide: preparing the polypeptide as shown in a formula I by adopting a solid phase method; (2) preparing amphoteric polypeptide: coupling amino undecanoic acid at the amino terminal of the polypeptide I to form the amphoteric polypeptide; (3) preparing isooctanol-philic polypeptide: condensing 4-tetraethylene glycol monomethoxybenzamide at the carboxyl end of the amphoteric polypeptide to obtain the isooctanol-philic polypeptide; (4) purification: purifying the isooctanol-philic polypeptide; (5) folding: folding the purified isooctanol-philic polypeptide by adopting a Pickering emulsion method; and (6) preparing a membrane structure: adding glutaraldehyde into the emulsion obtained in the step (5), and sequentially separating an oil phase and a water phase to obtain the membrane structure. The cell vesicle obtained by the patent is very stable in structure and has selective permeability to glucan.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of Pickering emulsions, and in particular to a method for preparing a cell membrane by using a Pickering emulsion method. Background Art

[0002] There are two main methods for artificially obtaining cell membranes: one is the bottom-up method, which includes preparing a lipid bilayer, and then gradually adding other modification materials such as proteins and nucleic acids, and finally forming a complex structure similar to natural cells. The second is the top-down method, starting from a polymer matrix, gradually introducing low molecular weight components, and finally forming a corresponding complex structure. In terms of the preparation materials of artificial cell membranes: At first, researchers tried to use lipids that constitute cell membranes to make monolayer or multilayer lipid vesicles, and applied them to examine the effects of specific peptide chains on lipid membrane dynamics, function or other characteristics, or to simulate biological forms from eukaryotic cells to organelles or bacteria. Later, phospholipids with high permeability, high lateral mobility and low biological toxicity were widely used as biomimetic materials for assembling GUVs (giant unilamellar vesicles). Studies have found that artificial cells derived from GUVs composed of phospholipid materials have a large enzyme packaging capacity and have certain application prospects. However, lipid vesicles composed of pure phospholipids can only imitate the shape of cells and isolate the contents from the outside world, which is far from the real cell structure. In order to make artificial cells more "realistic" and perform specific cellular functions, researchers will add membrane proteins whose activity can be regulated by adjusting the lipid composition of the membrane to the phospholipid bilayer. After that, researchers try to extract membrane preparations containing natural proteins and small molecules from natural cells as raw materials for assembling artificial cell membranes. In addition, fatty acids have become the focus of studying the initial form of cells. Fatty acids are single-chain amphiphilic molecules that can form bilayers, vesicles, and micelles in water. However, the low stability and harsh chemical modification conditions of this material limit its further development and wider application in artificial cells.

[0003] The applicant used the Pickering emulsion method to enhance the stability of fatty acid-modified polypeptides to prepare artificial cell membranes.

[0004] At the beginning of the twentieth century, Ramsden (1903) discovered that solid particles can stabilize emulsions. Subsequently, Pickering et al. (1907) used colloidal particles such as copper sulfate and iron sulfate to stabilize the water and paraffin system, and systematically explored the application of solid particles in stabilizing emulsions. It was confirmed that ultrafine solid particles can stably exist at the water / oil interface and play a role in stabilizing the emulsion. This emulsion was named "Pickering emulsion", that is, an emulsion stabilized by using solid particles to completely or partially replace surfactants. Pickering emulsions are stable emulsions formed by the irreversible adsorption of solid particles at the oil-water interface. , such as Figure 1As shown, in this patent, the Pickering emulsion method allows polypeptides to fold to form biological structures. Summary of the invention

[0005] This patent can assemble amphiphilic polypeptides of Janus nanofibers with hydrophilic and isooctyl alcohol-philic surface properties as materials for bionic cell membranes. Then, the Pickering emulsion method is used to prepare an oil-in-water emulsion in isooctyl alcohol / water, and the polypeptide fiber is used to stabilize the emulsion; finally, the in-situ cross-linking method is used to generate new chemical bonds between the fibers without changing the original position of the fibers to stabilize the membrane structure and replace the original solvent, ultimately forming a bionic cell membrane with a closed membrane structure.

[0006] The present invention provides a method for preparing a cell membrane by using a Pickering emulsion method, the method comprising: (1) Preparation of polypeptide: A polypeptide as shown in formula I is prepared by a solid phase method. (I).

[0007] (2) Preparation of an amphiphilic polypeptide: aminoundecanoic acid is coupled to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide.

[0008] (3) Preparation of isooctyl alcohol-philic polypeptide: 4-(2,5,8,11-tetraoxatridecan-13-yloxy)benzamide is condensed at the carboxyl end of the amphiphilic polypeptide to obtain an isooctyl alcohol-philic polypeptide (having a hydrophilic and isooctyl alcohol-philic surface and a Janus nanofiber structure).

[0009] (4) Purification: Purify the isooctyl alcohol-philic peptide.

[0010] (5) Folding: The purified isooctyl peptide is folded using the Pickering emulsion method to form a stable solution system.

[0011] (6) Preparation of membrane structure: adding glutaraldehyde to the emulsion obtained in step (5), and then separating the oil phase and the water phase in sequence to obtain a membrane structure.

[0012] Specifically, step (1) adopts Fmoc solid phase synthesis method, using HBTU and DIPEA as catalysts. Fmoc solid phase synthesis method is a conventional method for peptide synthesis, and detailed description is omitted in this embodiment.

[0013] Furthermore, steps (2) and (3) are both carried out on a resin used in a solid phase method (the synthesis method is similar to step (1)). After the reaction is completed, a mixture of trifluoroacetic acid / water / triisopropylsilane is used to cleave the polypeptide molecules from the resin, and then the mixture is distilled under reduced pressure, precipitated with ether, and dried to obtain a crude polypeptide. The volume ratio of trifluoroacetic acid, water, and triisopropylsilane is 92:1-3:2-4.

[0014] Wherein, step (4) specifically comprises: feeding the crude polypeptide into a liquid chromatography column (specifically, C18), using a mixture of water and acetonitrile as a mobile phase, gradient eluting, removing acetonitrile by vacuum distillation, and freeze-drying to obtain a refined polypeptide. Wherein, the volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%; specifically, the volume concentration of acetonitrile is 5%, 20%, 35%, 50%, 65%, 80% and 95%.

[0015] Wherein, step (5) specifically comprises: adding the peptide product to the isooctyl alcohol / water mixed emulsion, stirring at 500-700 rpm for 7-10 hours, wherein the volume ratio of isooctyl alcohol to water is 1-3:10, and the concentration of the peptide product is 0.5-1.0 mg / mL.

[0016] Wherein, step (6) specifically comprises: using 10-30% of glutaraldehyde to the fine polypeptide product, and stirring at a high speed of 10000-12000 rpm for 45-60s.

[0017] Specifically, the method for preparing cell membrane using the Pickering emulsion method provided by the present invention comprises: (1) Preparation of polypeptide: Fmoc solid phase synthesis method was used, HBTU and DIPEA were used as catalysts to prepare the polypeptide as shown in formula I, (I).

[0018] (2) Preparation of an amphiphilic polypeptide: aminoundecanoic acid is coupled to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide.

[0019] (3) Preparation of isooctyl alcohol-philic polypeptide: 4-tetraethylene glycol monomethoxybenzamide is condensed at the carboxyl end of the amphiphilic polypeptide to obtain an isooctyl alcohol-philic polypeptide. After the reaction is completed, the polypeptide molecule is cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, and then distilled under reduced pressure, precipitated with ether, and dried to obtain a crude polypeptide; the volume ratio of the trifluoroacetic acid, water, and triisopropylsilane is 92:1-3:2-4.

[0020] (4) Purification: The crude polypeptide is sent to a liquid chromatography column, and a mixture of water and acetonitrile is used as the mobile phase for gradient elution. The acetonitrile is removed by vacuum distillation, and the polypeptide is freeze-dried to obtain a refined product; the volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%.

[0021] (5) Folding: Add the polypeptide product to an isooctyl alcohol / water mixed emulsion, and stir at 500-700 rpm for 7-10 hours to obtain a polypeptide emulsion containing β-folding, wherein the volume ratio of isooctyl alcohol to water is 1-3:10, and the concentration of the polypeptide product is 0.5-1.0 mg / mL.

[0022] (6) Preparation of membrane structure: Add glutaraldehyde to the emulsion obtained in step (5), the amount of glutaraldehyde is 10-30% of the polypeptide fine product, stir at high speed at 10000-12000 rpm for 45-60s, and then separate the oil phase and the water phase in turn to obtain the membrane structure.

[0023] The cell membrane prepared by this patent has the following advantages: (1) The cell membrane vesicles prepared by this patent are spherical, with an average size of 7-12μm and a membrane thickness of 3-7nm. At room temperature, the average size of the cell membrane vesicles is 0.1-0.3μm smaller after five days, and there is no fusion or fragmentation of the cell membrane vesicles. At 4°C, the morphology of the cell membrane vesicles remains intact after 360 days of storage, and the average size of the cell membrane vesicles changes by less than 1μm. That is, the cell membrane vesicles of this patent are very stable.

[0024] (2) After step (5), a transmission electron microscope was used to observe the aggregation (the polypeptide was observed to be fibrous and aggregated, which was a Janus structure) and folding of the polypeptide. Uranyl acetate was used to stain the polypeptide structure, and circular dichroism spectroscopy was used to detect the folding of the polypeptide. It was observed that more than 70% of the polypeptides were folded according to the design requirements.

[0025] (3) Fluorescently labeled dextran can enter the cell membrane vesicles from the outside, proving that the cell membrane is permeable to dextran. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is the schematic diagram of this patent; Figure 2 This is the fluorescence absorption diagram of the cell membrane without the addition of this patent; Figure 3 This is the fluorescence absorption diagram of the cell membrane added with this patent. DETAILED DESCRIPTION

[0027] Example 1 Example 1 provides a method for preparing a cell membrane using a Pickering emulsion method, comprising: (1) Preparation of polypeptide: The polypeptide represented by formula I was prepared by Fmoc solid phase synthesis method with HBTU and DIPEA as catalysts.

[0028] (2) Preparation of an amphiphilic polypeptide: aminoundecanoic acid is coupled to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide.

[0029] (3) Preparation of isooctyl peptide: 4-tetraethylene glycol monomethoxybenzamide is condensed at the carboxyl end of the amphiphilic peptide to obtain an isooctyl peptide. After the reaction is completed, the peptide molecule is cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, and then distilled under reduced pressure, precipitated with ether, and dried to obtain a crude peptide. The volume ratio of trifluoroacetic acid, water, and triisopropylsilane is 92:2:3.

[0030] (4) Purification: The crude polypeptide is sent to a liquid chromatography column, and a mixture of water and acetonitrile is used as the mobile phase, and gradient elution is performed. The acetonitrile is removed by vacuum distillation, and the polypeptide is freeze-dried to obtain the refined product. The volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%.

[0031] (5) Folding: Add the peptide product to the isooctyl alcohol / water mixed emulsion and stir at 600 rpm for 8 hours to obtain a peptide emulsion containing β-folding, wherein the volume ratio of isooctyl alcohol to water is 1:5 and the concentration of the peptide product is 1 mg / mL.

[0032] (6) Preparation of membrane structure: Glutaraldehyde was added to the emulsion obtained in step (5), the amount of glutaraldehyde was 25% of the polypeptide concentrate, high-speed stirring was performed at 10,000 rpm for 60 seconds, and then the oil phase and the water phase were separated in turn to obtain a membrane structure.

[0033] The structure of the cell membrane was observed using an electron microscope: the cell membrane vesicles were spherical, with an average size of 8.4μm and a membrane thickness of 3.7nm. A fluorescein isothiocyanate-dextran solution with a concentration of 1mg / mL was prepared, and the molecular weight of fluorescein isothiocyanate-dextran was 100kDa-500kDa. It was added to the aqueous solution of this product, and the fluorescence absorption (wavelength of 520 nanometers) was detected to determine the permeability of this cell membrane. It was found that dextran could penetrate this cell membrane.

[0034] Example 2 Example 2 provides a method for preparing a cell membrane using a Pickering emulsion method, comprising: (1) Preparation of polypeptide: The polypeptide represented by formula I was prepared by Fmoc solid phase synthesis method with HBTU and DIPEA as catalysts.

[0035] (2) Preparation of an amphiphilic polypeptide: aminoundecanoic acid is coupled to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide.

[0036] (3) Preparation of isooctanol-philic polypeptide: 4-tetraethylene glycol monomethoxybenzamide is condensed at the carboxyl end of the amphiphilic polypeptide to obtain an isooctanol-philic polypeptide. After the reaction is completed, the polypeptide molecule is cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, and then distilled under reduced pressure, precipitated with ether, and dried to obtain a crude polypeptide. The volume ratio of trifluoroacetic acid, water, and triisopropylsilane is 92:3:3.

[0037] (4) Purification: The crude polypeptide is sent to a liquid chromatography column, and a mixture of water and acetonitrile is used as the mobile phase, and gradient elution is performed. The acetonitrile is removed by vacuum distillation, and the polypeptide is freeze-dried to obtain the refined product. The volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%.

[0038] (5) Folding: Add the peptide product to the isooctyl alcohol / water mixed emulsion and stir at 600 rpm for 9 hours to obtain a peptide emulsion containing β-folding, wherein the volume ratio of isooctyl alcohol to water is 1:4 and the concentration of the peptide product is 1 mg / mL.

[0039] (6) Preparation of membrane structure: Glutaraldehyde was added to the emulsion obtained in step (5), the amount of glutaraldehyde was 15% of the polypeptide fine product, high-speed stirring was performed at 12000 rpm for 60 seconds, and then the oil phase and the water phase were separated in turn to obtain a membrane structure.

[0040] The structure of the cell membrane was observed using an electron microscope: the cell membrane vesicles were spherical, with an average size of 8.3μm and a membrane thickness of 3.9nm. A fluorescein isothiocyanate-dextran solution with a concentration of 1mg / mL was prepared, and the molecular weight of fluorescein isothiocyanate-dextran was 100kDa-500kDa. It was added to the aqueous solution of this product, and the fluorescence absorption (wavelength of 520 nanometers) was detected to determine the permeability of the cell membrane. It was found that dextran could penetrate the cell membrane.

[0041] Example 3 Example 3 provides a method for preparing a cell membrane using a Pickering emulsion method, comprising: (1) Preparation of polypeptide: The polypeptide represented by formula I was prepared by Fmoc solid phase synthesis method with HBTU and DIPEA as catalysts.

[0042] (2) Preparation of an amphiphilic polypeptide: aminoundecanoic acid is coupled to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide.

[0043] (3) Preparation of isooctanol-philic polypeptide: 4-tetraethylene glycol monomethoxybenzamide is condensed at the carboxyl end of the amphiphilic polypeptide to obtain an isooctanol-philic polypeptide. After the reaction is completed, the polypeptide molecule is cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, and then distilled under reduced pressure, precipitated with ether, and dried to obtain a crude polypeptide. The volume ratio of trifluoroacetic acid, water, and triisopropylsilane is 92:2:4.

[0044] (4) Purification: The crude polypeptide is sent to a liquid chromatography column, and a mixture of water and acetonitrile is used as the mobile phase, and gradient elution is performed. The acetonitrile is removed by vacuum distillation, and the polypeptide is freeze-dried to obtain the refined product. The volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%.

[0045] (5) Folding: Add the peptide product to the isooctyl alcohol / water mixed emulsion and stir at 550 rpm for 10 hours to obtain a peptide emulsion containing β-folding, wherein the volume ratio of isooctyl alcohol to water is 1:5 and the concentration of the peptide product is 0.8 mg / mL.

[0046] (6) Preparation of membrane structure: Glutaraldehyde was added to the emulsion obtained in step (5), the amount of glutaraldehyde was 30% of the polypeptide concentrate, high-speed stirring was performed at 10,000 rpm for 55 seconds, and then the oil phase and the water phase were separated in turn to obtain a membrane structure.

[0047] The structure of the cell membrane was observed using an electron microscope: the cell membrane vesicles were spherical, with an average size of 8.7 μm and a membrane thickness of 3.6 nm. A fluorescein isothiocyanate-dextran solution with a concentration of 1 mg / mL was prepared, and the molecular weight of fluorescein isothiocyanate-dextran was 100 kDa-500 kDa. It was added to the aqueous solution of this product, and the fluorescence absorption (wavelength of 520 nanometers) was detected to determine the permeability of the cell membrane. It was found that dextran could penetrate the cell membrane.

[0048] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. Method for preparing cell membrane using Pickering emulsion method, It is characterized in that The method comprises: (1) Preparation of polypeptide: A polypeptide as shown in formula I is prepared by a solid phase method. (I); (2) preparing an amphiphilic polypeptide: coupling aminoundecanoic acid to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide; (3) preparing an isooctyl alcohol-philic polypeptide: condensing 4-tetraethylene glycol monomethoxybenzamide at the carboxyl end of the amphiphilic polypeptide to obtain an isooctyl alcohol-philic polypeptide; (4) Purification: purifying the isooctyl alcohol-philic polypeptide; (5) Folding: The purified isooctyl peptide is folded using the Pickering emulsion method; (6) Preparation of membrane structure: adding glutaraldehyde to the emulsion obtained in step (5), and then separating the oil phase and the water phase in sequence to obtain a membrane structure.

2. The method according to claim 1, It is characterized in that Step (1) adopts Fmoc solid phase synthesis method, using HBTU and DIPEA as catalysts.

3. The method according to claim 1, It is characterized in that Steps (2) and (3) are both carried out on the resin used in the solid phase method. After the reaction is completed, the polypeptide molecules are cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, distilled under reduced pressure, precipitated with ether, and dried to obtain a crude polypeptide; the volume ratio of the trifluoroacetic acid, water, and triisopropylsilane is 92:1-3:2-4.

4. The method according to claim 1, It is characterized in that Step (4) specifically comprises: feeding the crude polypeptide into a liquid chromatography column, using a mixture of water and acetonitrile as a mobile phase, gradient eluting, removing the acetonitrile by vacuum distillation, and freeze-drying to obtain a refined polypeptide; the volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%.

5. The method according to claim 1, It is characterized in that Step (5) specifically includes: adding the polypeptide product to an isooctyl alcohol / water mixed emulsion, stirring at 500-700 rpm for 7-10 hours, wherein the volume ratio of the isooctyl alcohol to water is 1-3:10, and the concentration of the polypeptide product is 0.5-1.0 mg / mL.

6. The method according to claim 1, It is characterized in that Step (6) specifically includes: the amount of glutaraldehyde used is 10-30% of the polypeptide product, and high-speed stirring is performed at 10000-12000 rpm for 45-60 seconds.

7. The method according to claim 1, It is characterized in that The method comprises: (1) Preparation of polypeptide: Fmoc solid phase synthesis method was used, HBTU and DIPEA were used as catalysts to prepare the polypeptide shown in formula I, (I); (2) preparing an amphiphilic polypeptide: coupling aminoundecanoic acid to the amino terminus of the polypeptide of I to form an amphiphilic polypeptide; (3) Preparation of isooctyl alcohol-philic polypeptide: 4-tetraethylene glycol monomethoxybenzamide is condensed at the carboxyl end of the amphiphilic polypeptide to obtain an isooctyl alcohol-philic polypeptide. After the reaction is completed, the polypeptide molecule is cleaved from the resin using a mixture of trifluoroacetic acid / water / triisopropylsilane, and then distilled under reduced pressure, and then precipitated with ether and dried to obtain a crude polypeptide. The volume ratio of the trifluoroacetic acid, water and triisopropylsilane is 92:1-3:2-4; (4) Purification: The crude polypeptide is sent to a liquid chromatography column, and a mixture of water and acetonitrile is used as the mobile phase, and gradient elution is performed. The acetonitrile is removed by vacuum distillation, and the polypeptide is freeze-dried to obtain a refined product; the volume concentration of acetonitrile in the mixture of water and acetonitrile is 5-95%; (5) Folding: Add the peptide product to an isooctyl alcohol / water mixed emulsion, and stir at 500-700 rpm for 7-10 hours to obtain a peptide emulsion containing β-folding, wherein the volume ratio of isooctyl alcohol to water is 1-3:10, and the concentration of the peptide product is 0.5-1.0 mg / mL; (6) Preparation of membrane structure: Add glutaraldehyde to the emulsion obtained in step (5), wherein the amount of glutaraldehyde is 10-30% of the polypeptide fine product, stir at a high speed of 10000-12000 rpm for 45-60 s, and then separate the oil phase and the water phase in turn to obtain a membrane structure.