LDH / ZIF-8 composite protective film on surface of magnesium-lithium alloy micro-arc oxidation film as well as preparation method and application of LDH / ZIF-8 composite protective film
By growing the LDH/ZIF-8 composite film in situ on the surface of the magnesium-lithium alloy micro-arc oxidation film, the problem of poor stability and density of the composite film is solved, effective long-term protection of the substrate is achieved, and the process steps are simplified. , improving the practicality of industrial applications.
Patent Information
- Application Number
- CN202410792024.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-19
- Publication Date
- 2024-10-01
AI Technical Summary
The composite film on the surface of the magnesium-lithium alloy micro-arc oxidation film layer has poor stability and density, which results in the inability to effectively protect the substrate in a long-term corrosion environment. Moreover, the existing sealing process steps are cumbersome, affecting industrial applications.
A one-step method was used to prepare the LDH/ZIF-8 composite film on the surface of the magnesium-lithium alloy micro-arc oxidation film. The LDH and ZIF-8 composite film was grown in situ on the MAO film through hydrothermal reaction. LDH and ZIF- The affinity of 8 forms a strong physical barrier layer, sealing film layer defects and enhancing stability and density.
Significantly improves the stability and density of the magnesium-lithium alloy micro-arc oxidation film, enhances the long-term corrosion protection ability of the substrate, simplifies the process steps, realizes green, efficient and safe sealing treatment, and improves industrial practicality sex.
Smart Images

Figure CN118727095A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of metal surface protection, and specifically relates to an LDH / ZIF-8 composite protective film on the surface of a magnesium-lithium alloy micro-arc oxidation film, and a preparation method and application thereof. Background Art
[0002] As the lightest structural metal, magnesium-lithium alloy is widely favored in the fields of automobiles, aerospace, etc., but its industrial application is limited by its poor corrosion resistance. Micro-arc oxidation technology has attracted widespread attention because the electrolyte is green and environmentally friendly, and the resulting film has excellent corrosion resistance and good adhesion to the substrate. However, due to the high-voltage discharge and gas escape during the micro-arc oxidation process, holes and cracks appear on the surface of the film. The corrosive liquid will penetrate into the substrate through the holes and cracks, causing the substrate to corrode, and the micro-arc oxidation film cannot protect the substrate for a long period of time. Therefore, it is necessary to develop a post-treatment technology to seal the surface of the micro-arc oxidation film of magnesium-lithium alloy.
[0003] At present, the surface of magnesium-lithium alloy micro-arc oxidation film is mainly prepared by preparing layered double hydroxides (LDHs) on its surface to seal its surface, but the stability of MAO-LDH composite film is poor, and the density still needs to be improved. There is also a composite film of LDH and MOFs prepared on the surface of MAO film to improve the comprehensive total energy of the alloy surface protective film, but this method usually prepares LDH film on the surface of MAO film first, and then immerses the composite film in MOF solution, so as to grow MOF film on the surface of LDH. The disadvantage of this method is that the steps are cumbersome, and multiple reactions are not conducive to industrial application. Summary of the invention
[0004] The purpose of the present invention is to solve the technical problem of poor stability and density of the composite film on the surface of the micro-arc oxidation film layer of the magnesium-lithium alloy, and to provide a LDH / ZIF-8 composite protective film on the surface of the micro-arc oxidation film of the magnesium-lithium alloy and a preparation method and application thereof.
[0005] The technical solution of the present invention is as follows:
[0006] One of the purposes of the present invention is to provide a method for preparing a LDH / ZIF-8 composite protective film on the surface of a magnesium-lithium alloy micro-arc oxidation film, the method being carried out according to the following steps:
[0007] Zinc nitrate hexahydrate, aluminum nitrate nonahydrate, 2-methylimidazole and water were mixed and magnetically stirred, and then the pH was adjusted to alkaline. The mixture was then placed in a reactor lined with polytetrafluoroethylene, and a magnesium-lithium alloy sample with a micro-arc oxidation film was added. The mixture was hydrothermally reacted, cooled, washed and dried to obtain a MAO-LDH / ZIF-8 composite protective film.
[0008] It is further defined that the molar ratio of zinc nitrate hexahydrate, aluminum nitrate nonahydrate and 2-methylimidazole is (1-2):1:(70-80).
[0009] It is further defined that the molar ratio of 2-methylimidazole to water is 1:(1.5-2).
[0010] Further defined, magnetic stirring for 8-12 min.
[0011] Further defined, the pH is adjusted to 10-10.5.
[0012] It is further defined that the preparation of the micro-arc oxidation film on the surface of the magnesium-lithium alloy sample is as follows: the magnesium-lithium alloy sample is first surface treated, and then used as the anode and the stainless steel sink as the cathode, and micro-arc oxidation is carried out in the electrolyte using a constant current method.
[0013] Further defining, the surface treatment specifically comprises first grinding with silicon carbide sandpaper, and then ultrasonically treating with acetone and ethanol in sequence.
[0014] It is further defined that the electrolyte composition is: 8-12 g / L Na2SiO3, 4-6 g / L NaF and 1-3 g / L NaOH.
[0015] It is further defined that the temperature of the hydrothermal reaction is 60-80°C and the time is 10-14h.
[0016] The second object of the present invention is to provide a MAO-LDH / ZIF-8 composite protective film prepared according to the above method.
[0017] The third object of the present invention is to provide an application of the MAO-LDH / ZIF-8 composite protective film prepared by the above method in metal surface protection.
[0018] Compared with the prior art, the present invention has the following advantages:
[0019] (1) The present invention provides a one-step method for preparing an LDH / ZIF-8 composite film on the surface of a magnesium-lithium alloy micro-arc oxidation film, which gives full play to the synergistic effect of the ion exchange capacity and stability of the composite film, and constructs a strong physical barrier layer on the surface of the MAO film, thereby effectively enhancing the protective ability of the film to the substrate in a long-term corrosion environment.
[0020] The main means of sealing the pores of the current magnesium-lithium alloy micro-arc oxidation film has many problems such as poor film density, poor stability, complex production process, and poor bonding with the film.
[0021] (2) The present invention utilizes the affinity between the LDH film layer and ZIF-8, and uses the preferentially grown LDH as a sacrificial layer during the hydrothermal process to obtain an LDH / ZIF-8 composite film layer, which not only achieves the purpose of sealing the defects of the MAO film layer, but also enhances the stability and density of the overall film layer, while having excellent bonding strength with the film layer.
[0022] (3) The method of the present invention greatly reduces the steps of preparation, is easy to operate, and is environmentally friendly. It is a green, efficient, and safe magnesium-lithium alloy micro-arc oxidation sealing process, which improves industrial applicability. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 SEM images of the MAO membrane and MAO-LDH / ZIF-8 composite membrane layer in Example 1, wherein (a) is MAO membrane, (b) is MAO-LDH / ZIF-8 composite membrane, and (cd) are enlarged images of (b);
[0024] Figure 2 XRD patterns of the MAO film and the MAO-LDH / ZIF-8 composite film in Example 1;
[0025] Figure 3 FT-IR images of the MAO membrane and the MAO-LDH / ZIF-8 composite membrane layer in Example 1;
[0026] Figure 4 are the polarization curves of the MAO membrane and the MAO-LDH / ZIF-8 composite membrane in Example 1;
[0027] Figure 5 This is the corrosion rate curve of the MAO membrane and MAO-LDH / ZIF-8 composite membrane layer in Example 1 obtained after hydrogen evolution for 14 days. DETAILED DESCRIPTION
[0028] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0029] The experimental methods used in the following examples are conventional methods unless otherwise specified. The materials, reagents, methods and instruments used are conventional materials, reagents, methods and instruments in the art unless otherwise specified, and can be obtained through commercial channels by those skilled in the art.
[0030] The terms "comprising," "including," "having," "containing," or any other variations thereof, as used in the following examples, are intended to cover a non-exclusive inclusion. For example, a composition, step, method, article, or apparatus comprising the listed elements is not necessarily limited to only those elements, but may include other elements not expressly listed or inherent to such composition, step, method, article, or apparatus.
[0031] When equivalent, concentration or other value or parameter is represented by the range limited by range, preferred range or a series of upper preferred value and lower preferred value, this should be understood as specifically disclosing all ranges formed by any pairing of any upper range limit or preferred value and any lower range limit or preferred value, regardless of whether the scope is disclosed separately. For example, when disclosing range "1 to 5", described range should be interpreted as including range "1 to 4", "1 to 3", "1 to 2", "1 to 2 and 4 to 5", "1 to 3 and 5" etc. When numerical range is described in this article, unless otherwise stated, the scope is intended to include its end value and all integers and fractions within the scope. In the present application specification and claims, range limitation can be combined and / or interchanged, if these ranges are not otherwise stated, include all sub-ranges contained therein.
[0032] The indefinite articles "a" and "an" before the elements or components of the present invention have no limitation on the quantity requirements (i.e. the number of occurrences) of the elements or components. Therefore, "a" or "an" should be interpreted as including one or at least one, and the elements or components in the singular form also include the plural form, unless the quantity obviously refers to the singular form only.
[0033] The "one embodiment" or "embodiment" of the present invention refers to a specific feature, structure or characteristic that can be included in at least one implementation of the present invention. The "in one embodiment" that appears in different places in this specification does not refer to the same embodiment, nor is it a separate or selective embodiment that is mutually exclusive with other embodiments.
[0034] The endpoints and any values of the ranges disclosed in the invention are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be regarded as specifically disclosed in this article.
[0035] Example 1: The preparation method of the LDH / ZIF-8 composite protective film on the surface of the magnesium-lithium alloy micro-arc oxidation film of this example is carried out according to the following steps:
[0036] (1) Preparation of micro-arc oxidation film on Mg-9Li-3Al alloy surface:
[0037] The surface of the Mg-9Li-3Al alloy was polished with 320#, 800# and 2000# silicon carbide sandpaper to remove the oxide film and stains. Then, acetone and ethanol were used for ultrasonic treatment for 10 minutes each, and the treated magnesium-lithium alloy was obtained by drying.
[0038] The treated magnesium-lithium alloy was used as the anode and the stainless steel water tank was used as the cathode. The constant current method was used for micro-arc oxidation treatment. The electrical parameters were 5A / dm 2 , frequency 600Hz, duty cycle 20%, oxidation time 10min, electrolyte composition 10g / L Na2SiO3, 5g / L NaF and 2g / L NaOH. The sample with micro-arc oxidation film was obtained, and its SEM is as follows Figure 1 (a) shown.
[0039] (2) In situ growth of LDH / ZIF-8 composite membrane:
[0040] The mixed solution was prepared according to the molar ratio of zinc nitrate hexahydrate: aluminum nitrate nonahydrate: 2-methylimidazole: water of 3:2:150:278, and then magnetically stirred for 10 minutes. -1 Adjust the pH to 10.3 with NaOH solution.
[0041] The solution was transferred to the polytetrafluoroethylene liner, and the micro-arc oxidation sample in step (1) was placed vertically in the polytetrafluoroethylene liner. The reactor was placed in an oven at 70°C for hydrothermal reaction for 12 hours. After the reaction, it was cooled to room temperature in the air, taken out, washed with deionized water and ethanol, and blown dry to obtain an LDH / ZIF-8 composite film layer in situ grown on the surface of the magnesium-lithium alloy micro-arc oxidation film layer, namely, a MAO-LDH / ZIF-8 composite protective film.
[0042] The SEM image of the in-situ grown LDH / ZIF-8 composite film on the surface of the magnesium-lithium alloy micro-arc oxidation film prepared in this example is as follows: Figure 1 As shown in (b)-(d), it can be seen that LDH / ZIF-8 grows uniformly and densely on the surface of the micro-arc oxidation film, and the defects of the micro-arc oxidation film are blocked by the LDH / ZIF-8 composite film.
[0043] like Figure 2 As shown, the XRD diffraction pattern shows that the main components of the composite film layer are Mg-Zn-Al-NO3(LDH), ZIF-8, MgO and Mg2SiO4.
[0044] like Figure 3 As shown in the FT-IR spectrum, the composite film layer has -1 and 1362cm-1 OH appeared - The broad peak and NO3 - The absorption vibration peak at 995cm -1 , 1146cm -1 , 1575cm -1 and 2922cm -1 The peaks correspond to the plane bending and plane vibration of the imidazole ring and the stretching vibration of the CH bond in ZIF-8. The absorption bands of the imidazole ring and nitrate ion appeared simultaneously in the composite film, indicating that the LDH / ZIF-8 composite film was successfully prepared.
[0045] The corrosion resistance of the MAO film and the MAO-LDH / ZIF-8 composite film of this embodiment was characterized by using a Zahner IM6ex electrochemical workstation in a three-electrode system (saturated calomel electrode as reference electrode, platinum electrode as counter electrode, and sample as working electrode). The corrosion resistance of the film was studied by potentiodynamic polarization curve test at room temperature in a 3.5wt.% NaCl solution with a scanning rate of 1mV / s. The results are shown in Figure 2. Figure 4 As shown in the results, the corrosion current density of the MAO-LDH / ZIF-8 composite film obtained in this example is 3.098×10 -9 Compared with the corrosion current density of MAO film layer, 1.986×10 -7 , reduced by about two orders of magnitude.
[0046] The MAO film layer and the MAO-LDH / ZIF-8 composite film layer of this embodiment were subjected to hydrogen evolution tests. The results are as follows: Figure 5 As shown in the figure, the corrosion rate of the MAO film increases rapidly with time, and decreases after 4 days. This may be due to the formation of the corrosion product Mg(OH)2, which seals the corrosion channel and blocks the penetration of the corrosive liquid. However, since the corrosion product Mg(OH)2 is loose and porous, it is quickly corroded and falls off, thereby accelerating the corrosion rate. The hydrogen evolution rate of MAO-LDH / ZIF-8 remains basically stable, which shows that the film has good density and stability. The corrosion rates of the MAO film and the MAO-LDH / ZIF-8 composite film are 0.093 ml·cm -2 ·day -1 and 0.011 ml cm -2 ·day -1 Compared with the MAO film, the average HER of the MAO-LDH / ZIF-8 film within 14 days was significantly reduced, proving that the MAO-LDH / ZIF-8 composite film has good protection ability for the substrate in a long-term environment.
[0047] The above are only preferred specific embodiments of the present invention, which are all different implementations based on the overall concept of the present invention, and the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A method for preparing a LDH / ZIF-8 composite protective film on the surface of a magnesium-lithium alloy micro-arc oxidation film, characterized in that: The method: Zinc nitrate hexahydrate, aluminum nitrate nonahydrate, 2-methylimidazole and water were mixed and magnetically stirred, and then the pH was adjusted to alkaline. The mixture was then placed in a reactor lined with polytetrafluoroethylene, and a magnesium-lithium alloy sample with a micro-arc oxidation film was added. The mixture was hydrothermally reacted, cooled, washed and dried to obtain a MAO-LDH / ZIF-8 composite protective film.
2. The method according to claim 1, characterized in that: The molar ratio of zinc nitrate hexahydrate, aluminum nitrate nonahydrate and 2-methylimidazole is (1-2):1:(70-80).
3. The method according to claim 1, characterized in that The molar ratio of 2-methylimidazole to water is 1:(1.5-2).
4. The method according to claim 1, characterized in that: Stir magnetically for 8-12 minutes.
5. The method according to claim 1, characterized in that Adjust pH to 10-10.
5.
6. The method according to claim 1, characterized in that Preparation of micro-arc oxidation film on the surface of magnesium-lithium alloy samples: The magnesium-lithium alloy samples were first surface treated, and then used as the anode and the stainless steel sink as the cathode, and micro-arc oxidation was carried out in the electrolyte using a constant current method.
7. The method according to claim 6, characterized in that Electrolyte composition: 8-12g / LNa2SiO3, 4-6g / LNaF and 1-3g / LNaOH.
8. The method according to claim 1, characterized in that The temperature of the hydrothermal reaction is 60-80°C and the time is 10-14h.
9. MAO-LDH / ZIF-8 composite protective film prepared by the method according to any one of claims 1 to 8.
10. Use of the MAO-LDH / ZIF-8 composite protective film prepared by the method according to any one of claims 1 to 8 in metal surface protection.
Citation Information
Cited By
LDH / ZIF-8 composite protective film for surface of micro-arc oxidation film of magnesium-lithium alloy, and preparation method therefor and use thereof
WO2025260745A1