Schottky barrier diode and manufacturing method thereof
By using indium aluminum zinc oxide (IAZO) material and adjusting its element ratio, combining different electrode materials and structural layers, optimizing the contact type of Schottky barrier diodes solves the problem that single-layer semiconductor structures are difficult to meet Schottky and ohmic contacts. problems, improving the performance and stability of the device.
Patent Information
- Application Number
- CN202310341583.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-01
AI Technical Summary
There is room for improvement in the performance of existing Schottky barrier diodes in terms of materials and structures. In particular, the single-layer semiconductor structure is difficult to meet the requirements of Schottky contact and ohmic contact at the same time, affecting its performance.
Indium aluminum zinc oxide (IAZO) is used as the semiconductor material, and by adjusting the proportions of aluminum, indium, and zinc elements, Schottky contact and ohmic contact semiconductor layers are formed respectively, and different electrode materials and structural layers are combined to optimize device contact. quality.
The performance of the Schottky barrier diode is improved, including increasing its barrier height, ideal factor and operating voltage, enhancing the electrical performance and optical stability, simplifying the preparation process, and achieving more flexible performance control.
Smart Images

Figure CN118738142A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a Schottky barrier diode and a manufacturing method thereof. Background Art
[0002] A Schottky barrier diode (SBD) is a diode fabricated using the metal-semiconductor junction principle, formed when a metal contacts a semiconductor. Currently, high-work-function metals such as gold (Au) and platinum (Pt) are typically used as the anode of an SBD, while N-type semiconductor materials or low-work-function metals are used as the cathode. This creates a Schottky barrier at the interface between the high-work-function metal and the semiconductor. SBDs offer advantages such as high switching frequency and low forward voltage drop, making them suitable for applications in rectifier circuits, protection circuits, and switching circuits.
[0003] In Schottky barrier diode devices, the material forming the Schottky contact and the contact quality of the Schottky contact directly affect its performance. In order to further improve the performance of Schottky barrier diodes, it is necessary to explore new materials and suitable device structures. Summary of the Invention
[0004] The present invention provides a Schottky barrier diode and a manufacturing method thereof, wherein the device performance of the Schottky barrier diode is improved and the device is easy to control during manufacturing.
[0005] A first aspect of the present invention provides a Schottky barrier diode, comprising: a substrate;
[0006] A first electrode structure layer is located on the substrate; the first electrode structure layer includes a first electrode layer;
[0007] a semiconductor structure layer, located on a side of the first electrode layer facing away from the substrate;
[0008] a second electrode structure layer, the second electrode structure layer comprising a second electrode layer, the second electrode layer being located on a side of the semiconductor structure layer facing away from the first electrode structure layer;
[0009] The semiconductor structure layer includes:
[0010] a first semiconductor layer, located on a side of the first electrode layer facing away from the substrate;
[0011] a second semiconductor layer located on a side of the first semiconductor layer facing away from the first electrode layer; the first semiconductor layer and the second semiconductor layer are both made of indium aluminum zinc oxide, and the proportions of aluminum in the first semiconductor layer and the second semiconductor layer are different;
[0012] One semiconductor layer in the semiconductor structure layer forms a Schottky contact with an adjacent electrode layer, and the other semiconductor layer forms an ohmic contact with an adjacent electrode layer.
[0013] In some embodiments of the present invention, the content of aluminum in the semiconductor layer forming a Schottky contact with the adjacent electrode layer is higher than the content of aluminum in the semiconductor layer forming an ohmic contact with the adjacent electrode layer.
[0014] In some embodiments of the present invention, in the semiconductor layer that forms a Schottky contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium, and zinc is higher than 45%; in the semiconductor layer that forms an ohmic contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium, and zinc is lower than 23%.
[0015] In some embodiments of the present invention, the thickness of the semiconductor layer forming an ohmic contact with the adjacent electrode layer is greater than the thickness of the semiconductor layer forming a Schottky contact with the adjacent electrode layer.
[0016] In some embodiments of the present invention, the first electrode structure layer further includes a third electrode layer; the third electrode layer is located between the substrate and the first electrode layer;
[0017] The third electrode layer is made of an adhesive material, and the adhesive material includes silver, indium, magnesium, titanium, aluminum, molybdenum, and copper.
[0018] In some embodiments of the present invention, the second electrode structure layer further includes a fourth electrode layer, and the fourth electrode layer is located on a side of the second electrode layer away from the semiconductor structure layer;
[0019] The fourth electrode layer is used to protect the second electrode layer, and the material used for the fourth electrode includes gold.
[0020] In some embodiments of the present invention, an orthographic projection area of the semiconductor structure layer on the substrate is smaller than an orthographic projection area of the first electrode structure layer on the substrate.
[0021] In some embodiments of the present invention, the orthographic projection of the semiconductor structure layer on the substrate completely covers the orthographic projection of the second electrode structure layer on the substrate.
[0022] Some embodiments of the present invention further include: an insulating layer, a first electrode and a second electrode;
[0023] The insulating layer covers the substrate, the first electrode structure layer, the semiconductor structure layer and the second electrode structure layer, and the insulating layer includes a plurality of via holes, and the via holes are used to expose a portion of the first electrode structure layer and a portion of the second electrode structure layer;
[0024] The first electrode and the second electrode are located on a side of the insulating layer away from the substrate. The first electrode is electrically connected to the first electrode structure layer through the via hole, and the second electrode is electrically connected to the second electrode structure layer through the via hole.
[0025] Another aspect of the present invention provides a method for manufacturing a Schottky barrier diode, comprising:
[0026] forming a first conductive material layer on a substrate;
[0027] forming a second conductive material layer on the first conductive material layer;
[0028] forming a first semiconductor material layer on the second conductive material layer;
[0029] forming a second semiconductor material layer on the first semiconductor material layer;
[0030] forming a third conductive material layer on the second semiconductor material layer;
[0031] forming a fourth conductive material layer on the third conductive material layer;
[0032] performing patterning on the fourth conductive material layer, the third conductive material layer, the second semiconductor material layer and the first semiconductor material layer to form a second electrode structure layer, a semiconductor structure layer and a first electrode structure layer;
[0033] covering the substrate, the first electrode structure layer, the semiconductor structure layer and the second electrode structure layer with an insulating layer;
[0034] Punching holes in the insulating layer to expose a portion of the first electrode structure layer and a portion of the second electrode structure layer;
[0035] forming a fifth conductive material layer on the insulating layer;
[0036] The fifth conductive material layer is patterned to form a first electrode and a second electrode; the first electrode is electrically connected to the first electrode structure layer through the via hole of the insulating layer, and the second electrode is electrically connected to the second electrode structure layer through the via hole of the insulating layer.
[0037] The beneficial effects of the present invention are as follows:
[0038] The present invention provides a Schottky barrier diode and a manufacturing method thereof. The Schottky barrier diode comprises: a substrate; a first electrode structure layer located on the substrate; the first electrode structure layer includes a first electrode layer; a semiconductor structure layer located on a side of the first electrode layer facing away from the substrate; a second electrode structure layer, the second electrode structure layer includes a second electrode layer, and the second electrode layer is located on a side of the semiconductor structure layer facing away from the first electrode structure layer; the semiconductor structure layer comprises: a first semiconductor layer located on a side of the first electrode layer facing away from the substrate; a second semiconductor layer located on a side of the first semiconductor layer facing away from the first electrode layer; the materials of the first semiconductor layer and the second semiconductor layer are both indium aluminum zinc oxide, and the proportions of aluminum elements in the first semiconductor layer and the second semiconductor layer are different; one semiconductor layer in the semiconductor structure layer forms a Schottky contact with an adjacent electrode layer, and the other semiconductor layer forms an ohmic contact with the adjacent electrode layer, and the double-layer semiconductor layers are adjusted separately to improve the contact quality of corresponding contact surfaces, which is beneficial to improving the performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments of the present invention. Obviously, the drawings introduced below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0040] Figure 1 A schematic structural diagram of a Schottky barrier diode provided in an embodiment of the present invention;
[0041] Figure 2 A flow chart of a method for manufacturing a Schottky barrier diode provided in an embodiment of the present invention;
[0042] Figure 3 is a schematic diagram of the device structure after forming the first conductive material layer;
[0043] Figure 4 is a schematic diagram of the device structure after forming the second conductive material layer;
[0044] Figure 5 is a schematic diagram of the device structure after forming the first semiconductor material layer;
[0045] Figure 6 is a schematic diagram of the device structure after forming the second semiconductor material layer;
[0046] Figure 7 is a schematic diagram of the device structure after forming the third conductive material layer;
[0047] Figure 8 is a schematic diagram of the device structure after forming the fourth conductive material layer;
[0048] Figure 9 Schematic diagram of the device structure after graphical processing;
[0049] Figure 10 Schematic diagram of the device structure after the insulating layer is formed;
[0050] Figure 11 Schematic diagram of the device structure after forming the connecting wires. DETAILED DESCRIPTION
[0051] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention will be further described below with reference to the accompanying drawings and examples. However, the example embodiments can be implemented in various forms and should not be understood as being limited to the embodiments described herein; on the contrary, these embodiments are provided to make the present invention more comprehensive and complete, and to fully convey the concepts of the example embodiments to those skilled in the art. The same figure marks in the figures represent the same or similar structures, and their repeated descriptions will be omitted. The words expressing position and direction described in the present invention are all explained with reference to the accompanying drawings as examples, but changes can be made as needed, and the changes made are all included in the scope of protection of the present invention. The drawings of the present invention are only used to illustrate the relative position relationship and do not represent the true proportion.
[0052] Circuits usually include four basic components: transistors, diodes, resistors and capacitors. Schottky barrier diodes, as an important type of diode, play a vital role in protecting circuits and components and improving their performance.
[0053] Schottky barrier diodes are a type of diode made based on the characteristic of Schottky barrier formed by the contact between metal and semiconductor. They can be divided into two structures: point contact type and surface bonding type. The performance of surface bonding Schottky barrier diodes is generally better than that of point contact type Schottky barrier diodes. Among them, the materials on both sides of the contact surface and the contact quality are important factors affecting the performance of Schottky barrier diodes.
[0054] Compared with traditional silicon materials commonly used in the semiconductor field, multi-metal oxide amorphous semiconductor materials have begun to be used in the preparation of Schottky barrier diodes due to their advantages such as high mobility and simple process. Schottky barrier diodes based on semiconductor materials such as indium gallium zinc oxide (IGZO) have appeared in related technologies, but they are usually single-layer semiconductor structures. In Schottky barrier diodes, the semiconductor material forming the Schottky contact needs to have a relatively larger resistance, and the semiconductor material forming the ohmic contact needs to have a relatively smaller resistance. It is difficult for a single-layer semiconductor material to meet the above requirements at the same time. In order to further improve the performance of Schottky barrier diodes, it is necessary to explore new materials and suitable device structures.
[0055] In view of this, an embodiment of the present invention provides a Schottky barrier diode, which can improve device performance by adjusting semiconductor materials and device structure.
[0056] Figure 1 A schematic structural diagram of a Schottky barrier diode provided in an embodiment of the present invention.
[0057] like Figure 1 As shown, the Schottky barrier diode provided by the embodiment of the present invention includes a substrate 100, a first electrode structure layer 200, a semiconductor structure layer 300, and a second electrode structure layer 400. The first electrode structure layer 200 is located on the substrate 100, the semiconductor structure layer 300 is located on the side of the first electrode structure layer 200 facing away from the substrate 100, and the second electrode structure layer 400 is located on the side of the semiconductor structure layer 300 facing away from the first electrode structure layer 200.
[0058] Specifically, the first electrode structure layer 200 includes at least a first electrode layer 102, and the semiconductor structure layer 300 is located on a side of the first electrode layer 102 facing away from the substrate 100. The semiconductor structure layer 300 includes a first semiconductor layer 103 and a second semiconductor layer 104, wherein the first semiconductor layer 103 is located on a side of the first electrode layer 102 facing away from the substrate 100, and the second semiconductor layer 104 is located on a side of the first semiconductor layer 103 facing away from the first electrode layer 102. The second electrode structure layer 400 includes at least a second electrode layer 105, which is located on a side of the semiconductor structure layer 300 facing away from the first electrode structure layer 200.
[0059] The first electrode layer 102 is in contact with the first semiconductor layer 103, and the second electrode layer 105 is in contact with the second semiconductor layer 104. One semiconductor layer in the semiconductor structure layer 300 can form a Schottky contact with the adjacent electrode layer, and the other semiconductor layer can form an ohmic contact with the adjacent electrode layer. That is, the first electrode layer 102 can form a Schottky contact with the first semiconductor layer 103, and the second electrode layer 105 can form an ohmic contact with the second semiconductor layer 104. In this case, the device is a bottom-contact Schottky barrier diode. Alternatively, the first electrode layer 102 can form an ohmic contact with the first semiconductor layer 103, and the second electrode layer 105 can form a Schottky contact with the second semiconductor layer 104. In this case, the device is a top-contact Schottky barrier diode.
[0060] In an embodiment of the present invention, the materials of the first electrode layer 102 and the second electrode layer 105 need to be adjusted according to the corresponding contact type. To achieve Schottky contact, the materials used in the corresponding electrode layer may include platinum (Pt) or gold (Au) with a high work function and not easily oxidized. To achieve ohmic contact, the materials used in the corresponding electrode layer include at least silver (Ag), indium (In), magnesium (Mg), titanium (Ti), aluminum (Al), molybdenum (Mo), copper (Cu) and other metals with good adhesion, low resistance and low work function, as well as one of the semiconductor materials with good conductivity such as indium zinc oxide, indium tin oxide, aluminum zinc oxide, fluorine-doped tin oxide, etc.
[0061] In an embodiment of the present invention, the materials for both the first semiconductor layer 103 and the second semiconductor layer 104 are indium aluminum zinc oxide (IAZO). The atomic ratio of indium, aluminum, and zinc can be adjusted as needed, specifically including ratios such as 1:1:1, 2:2:1, or 2:1:1. This allows for the regulation of properties such as the conductivity of the IAZO material. IAZO is a semiconductor material with an optical band gap and electron control capabilities far superior to IGZO. Therefore, IAZO can exhibit superior electrical performance and optical stability. Schottky barrier diodes fabricated using IAZO as the material for the first and second semiconductor layers 103 and 104 exhibit significantly superior barrier height, ideality factor, operating voltage, and other properties to conventional Schottky barrier diodes and PN junction diodes.
[0062] In IAZO materials, a higher indium content improves IAZO's conductivity, while a higher aluminum content reduces IAZO's conductivity while improving its stability. Therefore, by adjusting the ratio of indium to aluminum in IAZO, the electrical properties of the material can be adjusted. In this embodiment of the present invention, the first semiconductor layer 103 and the second semiconductor layer 104 have different aluminum ratios, resulting in different resistances in the first and second semiconductor layers 103 and 104.
[0063] Moreover, the content of aluminum in the semiconductor layer that forms a Schottky contact with the adjacent electrode layer is higher than the content of aluminum in the semiconductor layer that forms an ohmic contact with the adjacent electrode layer. In the semiconductor layer that forms a Schottky contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium, and zinc is higher than 45%, and the corresponding sum of the proportions of indium and zinc is lower than 55%, thereby making the corresponding semiconductor layer have a higher resistance, which helps the semiconductor layer to form a Schottky contact with the corresponding electrode layer with a higher potential barrier; in the semiconductor layer that forms an ohmic contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium, and zinc is lower than 23%, and the corresponding sum of the proportions of indium and zinc is higher than 77%, thereby making the corresponding semiconductor layer have a lower resistance, which helps the semiconductor layer to form an ohmic contact with the corresponding electrode layer with a lower resistance.
[0064] In an embodiment of the present invention, by adjusting the ratio of aluminum in the IAZO material in the first semiconductor layer and the second semiconductor layer to the three elements of aluminum, indium, and zinc, the resistance of the first semiconductor layer and the second semiconductor layer can be adjusted respectively, so that the first semiconductor layer and the second semiconductor layer form a Schottky contact with a higher potential barrier or an ohmic contact with a lower resistance with the corresponding electrode layer, respectively. Compared with a Schottky barrier diode with a single-layer semiconductor structure, the embodiment of the present invention can more flexibly change the preparation parameters, and more simply and effectively regulate the device performance, thereby making the device performance better.
[0065] In an embodiment of the present invention, the thicknesses of the first semiconductor layer 103 and the second semiconductor layer 104 may be different, wherein the thickness of the semiconductor layer forming an ohmic contact with the adjacent electrode layer is greater than the thickness of the semiconductor layer forming a Schottky contact with the adjacent electrode layer, that is, the semiconductor layer with better conductivity has a larger thickness, which can make the electron concentration in the Schottky barrier diode device higher, the resistance lower, and the current that can pass through it larger, thereby further improving the device performance.
[0066] like Figure 1 As shown, in an embodiment of the present invention, the first electrode structure layer 200 may further include a third electrode layer 101. The third electrode layer 101 is located between the substrate 100 and the first electrode layer 102. The material used for the third electrode layer 101 may include at least one of a metal with good adhesion, low resistance, and low work function, such as silver (Ag), indium (In), magnesium (Mg), titanium (Ti), aluminum (Al), molybdenum (Mo), and copper (Cu), and a semiconductor material with good conductivity, such as indium zinc oxide, indium tin oxide, aluminum zinc oxide, and fluorine-doped tin oxide. The third electrode layer 101 can adhere to the substrate 100, preventing the various film layers from falling off the substrate and preventing phenomena such as bulging during the preparation process, which is beneficial for increasing the stability of the Schottky barrier diode.
[0067] The second electrode structure layer 400 may further include a fourth electrode layer 106, which is located on the side of the second electrode layer 105 away from the semiconductor structure layer 300. The material used for the fourth electrode layer 106 may include gold (Au) with relatively low resistance and strong antioxidant ability. The fourth electrode layer 106 can be used to protect the second electrode layer 105, and can prevent the second electrode layer 105 from being scratched during subsequent testing and affecting its performance.
[0068] The Schottky barrier diode may further include an insulating layer 107, a first electrode 108, and a second electrode 109. The insulating layer 107 covers the substrate 100, the first electrode structure layer 200, the semiconductor structure layer 300, and the second electrode structure layer 400. The insulating layer 107 isolates the above structure from the external environment, effectively preventing the effects of oxygen, water vapor, and the like on the semiconductor and electrode materials, thereby improving the stability of the device.
[0069] The insulating layer 107 includes a plurality of vias, which are used to expose a portion of the first electrode structure layer 200 and a portion of the second electrode structure layer 400. A conductive material can be used to form a connecting line 110 in each via. A first electrode 108 and a second electrode 109 are located on a side of the insulating layer 107 facing away from the substrate 100. The first electrode 108 is electrically connected to the first electrode structure layer 200 via the connecting line 110 in the corresponding via, and the second electrode 109 is electrically connected to the second electrode structure layer 400 via the connecting line 110 in the corresponding via.
[0070] In some embodiments of the present invention, Figure 1 As shown, the orthographic projection area of the semiconductor structure layer 300 on the substrate 100 can be smaller than the orthographic projection area of the first electrode structure layer 200 on the substrate 100, and the orthographic projection of the semiconductor structure layer 300 on the substrate 100 completely covers the orthographic projection of the second electrode structure layer 400 on the substrate 100, so that the via hole in the insulating layer 107 can expose part of the first electrode layer 102 and part of the fourth electrode layer 106, and the first electrode 108 is electrically connected to the first electrode layer 102 through the connecting line 110 in the corresponding via hole, and the second electrode 109 is electrically connected to the fourth electrode layer 106 through the connecting line 110 in the corresponding via hole. At this time, the length of the connecting line in the via hole of the Schottky barrier diode is shorter, which can save manufacturing materials and reduce costs.
[0071] Based on the same inventive concept, an embodiment of the present invention further provides a method for manufacturing a Schottky barrier diode. Figure 2 A flow chart of a method for manufacturing a Schottky barrier diode provided in an embodiment of the present invention.
[0072] like Figure 2 As shown, the steps for manufacturing the Schottky barrier diode provided by the embodiment of the present invention are as follows:
[0073] S01, forming a first conductive material layer on a substrate;
[0074] S02, forming a second conductive material layer on the first conductive material layer;
[0075] S03, forming a first semiconductor material layer on the second conductive material layer;
[0076] S04, forming a second semiconductor material layer on the first semiconductor material layer;
[0077] S05, forming a third conductive material layer on the second semiconductor material layer;
[0078] S06, forming a fourth conductive material layer on the third conductive material layer;
[0079] S07, performing patterning on the fourth conductive material layer, the third conductive material layer, the second semiconductor material layer, and the first semiconductor material layer to form a second electrode structure layer, a semiconductor structure layer, and a first electrode structure layer;
[0080] S08, covering the substrate, the first electrode structure layer, the semiconductor structure layer, and the second electrode structure layer with an insulating layer;
[0081] S09, punching holes in the insulating layer to expose a portion of the first electrode structure layer and a portion of the second electrode structure layer;
[0082] S10, forming a fifth conductive material layer on the insulating layer;
[0083] S11 , patterning the fifth conductive material layer to form a first electrode and a second electrode; the first electrode is electrically connected to the first electrode structure layer through a via hole in the insulating layer, and the second electrode is electrically connected to the second electrode structure layer through a via hole in the insulating layer.
[0084] Figure 3 is a schematic diagram of the device structure after forming the first conductive material layer; Figure 4 is a schematic diagram of the device structure after forming the second conductive material layer; Figure 5 is a schematic diagram of the device structure after forming the first semiconductor material layer;
[0085] Figure 6 is a schematic diagram of the device structure after forming the second semiconductor material layer; Figure 7 is a schematic diagram of the device structure after forming the third conductive material layer; Figure 8 is a schematic diagram of the device structure after forming the fourth conductive material layer; Figure 9 Schematic diagram of the device structure after graphical processing; Figure 10 Schematic diagram of the device structure after the insulating layer is formed; Figure 11 Schematic diagram of the device structure after forming the connecting wires.
[0086] Figures 3 to 10 The structure of the device after completing steps S01 to S08 is shown in sequence. After completing step S09, the via hole is filled with electrode material to form a Figure 11 The device structure shown in FIG. 1 can be formed after completing step S11. Figure 1 The Schottky barrier diode shown.
[0087] Specifically, in step S01, substrate 100 can be a clean, hard substrate with a flat surface, such as SiO2 / p-Si, SiO2 / n-Si, transparent glass, or quartz. Alternatively, it can be a flexible substrate, such as polyimide (PI), polyethersulfone (PES), polyethylene naphthalate (PEN), polycarbonate (PC), or polyethylene terephthalate (PET). Schottky barrier diodes using IAZO semiconductor materials can be applied to transparent circuit substrates without being restricted by substrate material, thus offering a wider range of applications.
[0088] In step S01, the first conductive material layer uses at least one of metal materials with good adhesion, low resistance and low work function, such as silver (Ag), indium (In), magnesium (Mg), titanium (Ti), aluminum (Al), molybdenum (Mo), and copper (Cu), and semiconductor materials with good conductivity, such as indium zinc oxide, indium tin oxide, aluminum zinc oxide, and fluorine-doped tin oxide, which helps to increase the stability of the Schottky barrier diode.
[0089] In step S02 and step S05, the materials of the second conductive material layer and the third conductive material layer need to be adjusted according to the device structure. When the device is a bottom-contact Schottky barrier diode, the second conductive material layer can be made of platinum (Pt) or gold (Au) with a high work function and not easily oxidized, which helps to form a Schottky contact with a high barrier between the semiconductor structure layer. The third conductive material layer is made of at least one metal material with good adhesion, low resistance and low work function, such as silver (Ag), indium (In), magnesium (Mg), titanium (Ti), aluminum (Al), molybdenum (Mo), copper (Cu), and indium zinc oxide, indium tin oxide, aluminum zinc oxide, fluorine-doped tin oxide, and other semiconductor materials with good conductivity, which helps to An ohmic contact with good conductivity is formed between the semiconductor material layer; when the device is a top-contact Schottky barrier diode, the second conductive material layer uses at least one of metal materials with good adhesion, low resistance and low work function, such as silver (Ag), indium (In), magnesium (Mg), titanium (Ti), aluminum (Al), molybdenum (Mo), copper (Cu), and semiconductor materials with good conductivity, such as indium zinc oxide, indium tin oxide, aluminum zinc oxide, and fluorine-doped tin oxide, which helps to form an ohmic contact with good conductivity between the semiconductor material layer. The third conductive material layer can use materials such as platinum (Pt) or gold (Au) with a higher work function and not easily oxidized, which helps to form a Schottky contact with a higher barrier between the semiconductor structure layer.
[0090] Furthermore, when a Schottky contact is formed between the conductive material layer and the semiconductor structure layer, an appropriate amount of oxygen can be introduced into the preparation environment during the formation of the conductive material layer to adsorb oxygen atoms on the surface of the conductive material layer. Alternatively, the conductive material layer can be subjected to an oxidation treatment after formation. Treatment methods such as ultraviolet ozone, oxygen plasma, and oxygen environment annealing can be used to increase the potential barrier at the contact surface, facilitating the formation of a Schottky contact while avoiding the formation of an ohmic contact that affects product yield.
[0091] In step S03 and step S04, the first semiconductor material layer and the second semiconductor material layer both use IAZO material, but the atomic ratios of the three elements In, Al, and Zn of the IAZO material in the first semiconductor material layer and the second semiconductor material layer can be different, so that the resistance of the first semiconductor material layer and the second semiconductor material layer can be different. When the device is a bottom-contact Schottky barrier diode, the content of Al in the first semiconductor material layer is higher than the content of Al in the second semiconductor material layer, the proportion of Al among the three elements In, Al, and Zn in the first semiconductor material layer is higher than 45%, and the corresponding sum of the proportions of In and Zn elements is lower than 55%, and the proportion of Al among the three elements In, Al, and Zn in the second semiconductor material layer is lower than 23%, and the corresponding sum of the proportions of In and Zn elements is higher than 77%; when the device is a top-contact Schottky barrier diode, the content of Al in the second semiconductor material layer is higher than the content of Al in the first semiconductor material layer, the proportion of Al among the three elements In, Al, and Zn in the first semiconductor material layer is lower than 23%, and the corresponding sum of the proportions of In and Zn elements is higher than 77%, and the proportion of Al among the three elements In, Al, and Zn in the second semiconductor material layer is higher than 45%, and the corresponding sum of the proportions of In and Zn elements is lower than 55%.
[0092] The first semiconductor material layer and the second semiconductor material layer are prepared by at least one method selected from magnetron sputtering, pulsed laser deposition, sol-gel and the like, and the first semiconductor material layer and the second semiconductor material layer can be prepared by different methods.
[0093] In the embodiment of the present invention, the Schottky barrier diode has different performance requirements for the first semiconductor material layer and the second semiconductor material layer. Selecting a suitable IAZO material component and a preparation method thereof helps to improve the device performance of the Schottky barrier diode.
[0094] In step S06 , the material used for the fourth conductive material layer may include gold (Au) or the like, which has relatively low resistance and strong oxidation resistance.
[0095] In steps S01, S02, S05, and S06, the first conductive material layer, the second conductive material layer, the third conductive material layer, and the fourth conductive material layer are prepared by at least one of magnetron sputtering, electron beam evaporation, thermal evaporation, pulsed laser deposition, chemical vapor deposition, and sol-gel methods. Furthermore, the first conductive material layer, the second conductive material layer, the third conductive material layer, and the fourth conductive material layer may be prepared using different methods.
[0096] In the embodiment of the present invention, selecting a suitable conductive material and its preparation method can reduce the overall resistance of the Schottky barrier diode device and lower the power consumption of the circuit.
[0097] In step S07 , the patterning process may be performed by dry etching or wet etching.
[0098] In step S08, the insulating layer material may include one or more materials selected from the group consisting of Ta2O5, SiO2, Al2O3, HfO2, silicon nitride, and silicon oxynitride. The insulating layer is prepared using at least one of the following methods: magnetron sputtering, pulsed laser deposition, atomic layer deposition, plasma-enhanced atomic layer deposition, thermal oxidation, chemical vapor deposition, and plasma-enhanced chemical vapor deposition. Selecting an appropriate insulating layer material and its preparation method can effectively prevent the effects of oxygen, water vapor, and other environmental factors on the semiconductor structure layer of the Schottky barrier diode, thereby improving the stability of the Schottky barrier diode and the display substrate.
[0099] After completing step S09, it is necessary to form connecting wires in the via holes after drilling the insulating layer. The connecting wires can be formed first and then proceed to step S10, or the connecting wires and the fifth conductive material layer in step S10 can be formed simultaneously. The connecting wires and the fifth conductive material layer can be made of one or more metal materials with low resistance, such as tungsten, aluminum, copper, gold, and indium, or semiconductor materials with excellent conductivity, such as indium zinc oxide, indium tin oxide, aluminum zinc oxide, and fluorine-doped tin oxide. The connecting wires and the fifth conductive material layer are prepared by at least one method, such as magnetron sputtering, pulsed laser deposition, chemical vapor deposition, atomic layer deposition, and sol-gel deposition. Selecting appropriate connecting wire materials and conductive materials, as well as their preparation methods, helps reduce the overall power consumption of the circuit and display substrate.
[0100] According to the first inventive concept, the materials for both the first and second semiconductor layers are indium aluminum zinc oxide (IAZO), wherein the atomic ratio of indium, aluminum, and zinc can be set as desired, specifically including ratios such as 1:1:1, 2:2:1, or 2:1:1. This allows the conductivity and other properties of the IAZO material to be regulated. IAZO is a semiconductor material with an optical band gap and electron control capabilities far superior to IGZO. Therefore, IAZO can have better electrical properties and optical stability. Schottky barrier diodes made using IAZO as the material for the first and second semiconductor layers have significantly better barrier height, ideality factor, operating voltage, and other properties than traditional Schottky barrier diodes and PN junction diodes.
[0101] According to the second inventive concept, the electrical properties of the IAZO material can be adjusted by adjusting the ratio of indium and aluminum in IAZO. The ratio of aluminum in the first semiconductor layer and the second semiconductor layer is different, so that the resistance of the first semiconductor layer and the second semiconductor layer can be different.
[0102] According to the third inventive concept, the content of aluminum in the semiconductor layer forming a Schottky contact with the adjacent electrode layer is higher than the content of aluminum in the semiconductor layer forming an ohmic contact with the adjacent electrode layer. By adjusting the ratio of aluminum in the IAZO material to the three elements of aluminum, indium and zinc in the first semiconductor layer and the second semiconductor layer, the resistance of the first semiconductor layer and the second semiconductor layer can be adjusted respectively, so that the first semiconductor layer and the second semiconductor layer form a Schottky contact with a higher potential barrier or an ohmic contact with a lower resistance with the corresponding electrode layer respectively. Compared with the Schottky barrier diode with a single-layer semiconductor structure, the preparation parameters can be changed more flexibly, and the device performance can be regulated more simply and effectively, thereby making the device performance better.
[0103] According to the fourth inventive concept, the thickness of the semiconductor layer that forms an ohmic contact with the adjacent electrode layer is greater than the thickness of the semiconductor layer that forms a Schottky contact with the adjacent electrode layer, that is, the thickness of the semiconductor layer with better conductivity is greater, which can make the electron concentration in the Schottky barrier diode device higher, the resistance lower, and the current that can pass through it greater, thereby further improving the device performance.
[0104] According to the fifth inventive concept, the first electrode structure layer also includes a third electrode layer located between the substrate and the first electrode layer. The third electrode layer is made of an adhesive material. The third electrode layer can be adhered to the substrate, which can prevent the film layers from falling off from the substrate and avoid the occurrence of bulging and other phenomena during the preparation process, which is beneficial to increasing the stability of the Schottky barrier diode.
[0105] According to the sixth inventive concept, the second electrode structure layer further includes a fourth electrode layer, which can be used to protect the second electrode layer and prevent the second electrode layer from being scratched during subsequent testing processes, thereby affecting its performance.
[0106] According to the seventh inventive concept, the insulating layer covers the substrate, the first electrode structure layer, the semiconductor structure layer and the second electrode structure layer, which can isolate the above structures from the external environment and effectively prevent the influence of oxygen, water vapor, etc. on the semiconductor material and the electrode material, thereby improving the stability of the device.
[0107] According to the eighth inventive concept, the orthographic projection area of the semiconductor structure layer on the substrate is smaller than the orthographic projection area of the first electrode structure layer on the substrate, and the orthographic projection of the semiconductor structure layer on the substrate completely covers the orthographic projection of the second electrode structure layer on the substrate, so that the vias in the insulating layer can expose part of the first electrode layer and part of the fourth electrode layer, and the first electrode is electrically connected to the first electrode layer through the connecting wires in the corresponding vias, and the second electrode is electrically connected to the fourth electrode layer through the connecting wires in the corresponding vias. At this time, the length of the connecting wires in the vias of the Schottky barrier diode is shorter, which can save manufacturing materials and reduce costs.
[0108] According to the ninth inventive concept, a Schottky barrier diode using IAZO semiconductor material can be applied to a transparent circuit substrate without being restricted by substrate materials, and has a wider range of application scenarios.
[0109] According to the tenth inventive concept, when a Schottky contact is formed between the conductive material layer and the semiconductor structure layer, an appropriate amount of oxygen can be introduced into the preparation environment during the formation of the conductive material layer to allow oxygen atoms to be adsorbed on the surface of the conductive material layer. Alternatively, the conductive material layer can be subjected to an oxidation treatment after formation. Treatment methods can include ultraviolet ozone, oxygen plasma, oxygen environment annealing, and the like, thereby increasing the potential barrier at the contact surface, facilitating the formation of a Schottky contact and avoiding the formation of an ohmic contact that affects product yield.
[0110] According to the eleventh inventive concept, selecting a suitable conductive material and its preparation method can reduce the overall resistance of the Schottky barrier diode device and lower the power consumption of the circuit.
[0111] Although the preferred embodiments of the present invention have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0112] Obviously, those skilled in the art may make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if such changes and modifications fall within the scope of the claims and their equivalents, the present invention is intended to include such changes and modifications.
Claims
1. A Schottky barrier diode, characterized in that: include: substrate; A first electrode structure layer, located on the substrate; The first electrode structure layer includes a first electrode layer; A semiconductor structure layer, located on a side of the first electrode layer away from the substrate; a second electrode structure layer, the second electrode structure layer comprising a second electrode layer, and the second electrode layer is located on a side of the semiconductor structure layer away from the first electrode structure layer; The semiconductor structure layer comprises: A first semiconductor layer, located on a side of the first electrode layer facing away from the substrate; a second semiconductor layer, located on a side of the first semiconductor layer away from the first electrode layer; the first semiconductor layer and the second semiconductor layer are both made of indium aluminum zinc oxide, and the first semiconductor layer and the second semiconductor layer have different proportions of aluminum; One semiconductor layer in the semiconductor structure layer forms a Schottky contact with an adjacent electrode layer, and the other semiconductor layer forms an Ohmic contact with an adjacent electrode layer.
2. The Schottky barrier diode according to claim 1, characterized in that: The content of aluminum in the semiconductor layer forming a Schottky contact with the adjacent electrode layer is higher than the content of aluminum in the semiconductor layer forming an ohmic contact with the adjacent electrode layer.
3. The Schottky barrier diode according to claim 2, characterized in that: In the semiconductor layer forming Schottky contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium and zinc is higher than 45%; in the semiconductor layer forming ohmic contact with the adjacent electrode layer, the proportion of aluminum among the three elements of aluminum, indium and zinc is lower than 23%.
4. The Schottky barrier diode according to claim 1, wherein: The thickness of the semiconductor layer forming an ohmic contact with the adjacent electrode layer is greater than the thickness of the semiconductor layer forming a Schottky contact with the adjacent electrode layer.
5. The Schottky barrier diode according to claim 1, wherein: The first electrode structure layer further includes a third electrode layer; the third electrode layer is located between the substrate and the first electrode layer; The third electrode layer is made of an adhesive material, and the adhesive material includes silver, indium, magnesium, titanium, aluminum, molybdenum, and copper.
6. The Schottky barrier diode according to claim 1, characterized in that: The second electrode structure layer further includes a fourth electrode layer, and the fourth electrode layer is located on a side of the second electrode layer away from the semiconductor structure layer; The fourth electrode layer is used to protect the second electrode layer, and the material used for the fourth electrode includes gold.
7. The Schottky barrier diode according to claim 1, characterized in that: The orthographic projection area of the semiconductor structure layer on the substrate is smaller than the orthographic projection area of the first electrode structure layer on the substrate.
8. The Schottky barrier diode according to claim 7, characterized in that: The orthographic projection of the semiconductor structure layer on the substrate completely covers the orthographic projection of the second electrode structure layer on the substrate.
9. The Schottky barrier diode according to claim 7 or 8, characterized in that: Also includes: an insulating layer, a first electrode and a second electrode; The insulating layer covers the substrate, the first electrode structure layer, the semiconductor structure layer and the second electrode structure layer, and the insulating layer includes a plurality of via holes, and the via holes are used to expose a portion of the first electrode structure layer and a portion of the second electrode structure layer; The first electrode and the second electrode are located on a side of the insulating layer away from the substrate. The first electrode is electrically connected to the first electrode structure layer through the via hole, and the second electrode is electrically connected to the second electrode structure layer through the via hole.
10. A method for manufacturing a Schottky barrier diode, characterized in that: include: forming a first conductive material layer on a substrate; forming a second conductive material layer on the first conductive material layer; forming a first semiconductor material layer on the second conductive material layer; forming a second semiconductor material layer on the first semiconductor material layer; forming a third conductive material layer on the second semiconductor material layer; forming a fourth conductive material layer on the third conductive material layer; Performing patterning on the fourth conductive material layer, the third conductive material layer, the second semiconductor material layer and the first semiconductor material layer to form a second electrode structure layer, a semiconductor structure layer and a first electrode structure layer; Covering the substrate, the first electrode structure layer, the semiconductor structure layer and the second electrode structure layer with an insulating layer; Punching holes in the insulating layer to expose a portion of the first electrode structure layer and a portion of the second electrode structure layer; forming a fifth conductive material layer on the insulating layer; Performing patterning on the fifth conductive material layer to form a first electrode and a second electrode; The first electrode is electrically connected to the first electrode structure layer through the via hole of the insulating layer, and the second electrode is electrically connected to the second electrode structure layer through the via hole of the insulating layer.
Citation Information
Cited By
Molybdenum disulfide-based asymmetric structure Schottky diode
CN119603980A