Deep ultraviolet LED flip chip p-type reflection electrode structure and preparation method thereof

By forming Ni nanoparticles and coating the reflective metal Rh layer on the p-type GaN contact layer of the deep ultraviolet LED chip, the problem of GaN's UV light absorption and total internal reflection is solved, and the light extraction efficiency and brightness are significantly improved, achieving More efficient deep UV LED light emission.

CN118738236APending Publication Date: 2024-10-01ADVANCED ULTRAVIOLET OPTOELECTRONICS CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410902797.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The external quantum efficiency (EQE) of deep ultraviolet LEDs is low, mainly due to the internal total reflection caused by the refractive index difference between the AlGaN-based material and the sapphire substrate, and the strong absorption of ultraviolet light by the GaN p-type contact layer, resulting in light extraction efficiency (LEE) low.

Method used

Plate a metallic Ni layer on the p-type GaN contact layer and perform high-temperature annealing to form Ni nanoparticles. Use the Ni nanoparticles as a mask to etch the GaN layer to reduce GaN's absorption of ultraviolet light, and evaporate the reflective metal Rh on it. layer to improve light reflectivity and enhance light extraction efficiency.

Benefits of technology

By reducing GaN's absorption of ultraviolet light and increasing light reflectivity, the light extraction efficiency and brightness of deep ultraviolet LEDs are significantly improved, and the luminous efficiency of the chip is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738236A_ABST
    Figure CN118738236A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of deep ultraviolet LED flip chips, and particularly relates to a deep ultraviolet LED flip chip p-type reflection electrode structure and a preparation method thereof, and the preparation method comprises the following steps: preparing an epitaxial wafer structure; preparing a metal Ni layer on the p-type GaN contact layer; performing high-temperature annealing on the metal Ni layer to form p-type ohmic contact, and agglomerating the metal Ni layer to form Ni nanoparticles; etching the p-type GaN contact layer by taking the Ni nanoparticles as a mask; and preparing a reflective metal Rh layer. According to the method, the metal Ni layer is evaporated on the p-type GaN contact layer, the Ni nanoparticles are formed through high-temperature annealing, the Ni nanoparticles serve as a mask, the p-type GaN contact layer is etched, then the reflection metal Rh layer is evaporated, GaN light absorption is reduced, reflection is increased, and therefore the deep ultraviolet LED flip chip with the higher luminous efficiency is obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of deep ultraviolet LED flip chip, and in particular relates to a deep ultraviolet LED flip chip p-type reflective electrode structure and a preparation method thereof. Background Art

[0002] As the most promising new light source, light emitting diodes (LEDs) have the characteristics of high light efficiency, low voltage, long life, small size, low energy consumption, green environmental protection, and short response time. They are widely used in lighting, display, polymer curing, sterilization, communication and other fields. In recent years, in the field of chips, flip chip technology is emerging. Due to the advantages of good heat dissipation, low voltage, high brightness, high reliability, and high saturation current density, LED flip chips are very popular in the application market and are gradually maturing.

[0003] However, deep ultraviolet LEDs are still facing the problem of low external quantum efficiency (EQE). It is reported that the EQE of AlGaN-based deep ultraviolet LEDs grown on sapphire substrates is usually less than 10%. Due to the large difference in refractive index between the AlGaN material, sapphire substrate and air, AlGaN-based deep ultraviolet LEDs cause severe internal total reflection, resulting in low light extraction efficiency (LEE). In addition, in order to obtain good ohmic contact, the p-type contact layer of AlGaN-based deep ultraviolet LEDs mostly uses GaN, but the band gap of GaN is 3.4eV, which will strongly absorb ultraviolet light, which is another important reason for the low LEE. Therefore, reducing the light loss effect caused by the absorption of deep ultraviolet light by the p-GaN layer has become one of the key means to improve the light extraction efficiency of deep ultraviolet LEDs. Summary of the invention

[0004] In view of the technical problem that GaN absorbs ultraviolet light and affects the luminous efficiency of LED, the present invention provides a deep ultraviolet LED flip chip p-type reflective electrode structure and a preparation method thereof. The technical principle of the present invention is that metal Ni is prone to agglomeration after high-temperature annealing. By utilizing this feature, the thickness of the plated Ni metal layer and the annealing conditions are controlled to form uniformly distributed Ni nanoparticles with appropriate spacing. Ni metal particles have a large etching selectivity ratio with GaN, and the etching rate of Ni metal particles is slower than that of GaN. During ICP etching, Ni nanoparticles are used as a mask to etch away the exposed GaN not covered by Ni, which is conducive to reducing GaN's absorption of ultraviolet light and improving light extraction efficiency. And the annealed Ni layer can form a good p-type ohmic contact. Then evaporate a layer of reflective metal Rh, which has a high reflectivity in the deep ultraviolet band. In the 260nm~280nm band, the Rh reflectivity is 65%~70%, and the work function (4.98eV) is close to that of the p-type semiconductor layer, which will not lead to an increase in the chip operating voltage. And the reflection of Rh makes the light emitted by the PN junction more emitted from the sapphire surface, thereby obtaining a deep ultraviolet LED chip with higher light efficiency.

[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is: A method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure comprises the following steps: S1, preparing an epitaxial wafer structure, the top layer of the epitaxial wafer structure being a p-type GaN contact layer; S2, preparing a metal Ni layer on the p-type GaN contact layer; S3, annealing the metal Ni layer at high temperature to form a p-type ohmic contact, and the metal Ni layer agglomerates to form Ni nanoparticles; S4, using Ni nanoparticles as a mask to etch the p-type GaN contact layer; S5. Evaporating a reflective metal Rh layer on the Ni nanoparticles and the p-type GaN contact layer, thereby completing the preparation of the p-type reflective electrode structure.

[0006] The method for preparing the epitaxial wafer structure in S1 is: preparing a substrate, an AlN buffer layer, an n-type semiconductor layer, a quantum well layer, a p-type semiconductor layer, and a p-type GaN contact layer in sequence from bottom to top to form an epitaxial wafer structure.

[0007] The thickness of the metal Ni layer in S2 is 1nm-50nm, the metal Ni layer is evaporated on the p-type GaN contact layer, the plating pot speed is 1rpm-20rpm, the coating rate is 0.1Å / s-5Å / s, and the vacuum degree is 2.0×10 -5 Torr-2.0×10 -7 Torr, the coating power is 5%-50% of the electron gun output power.

[0008] The metal Ni layer in S3 is subjected to high temperature annealing in a nitrogen atmosphere, the annealing temperature is 500°C-950°C, the annealing time is 30s-400s, and the nitrogen flow rate is 100cm 3 / min-5000cm 3 / min.

[0009] The Ni nanoparticles are spherical in shape, have an average diameter of 50 nm, and have an average spacing of 0.5 μm.

[0010] In S4, Ni nanoparticles are used as a mask to etch the p-type GaN contact layer to the p-type semiconductor layer using a dry etching device ICP. The etching gas used by the dry etching device ICP is Cl2 and BCl3, and the Cl2 flow rate is 10cm 3 / min-100cm 3 / min, BCl3 flow rate is 1cm 3 / min-40cm 3 / min, working pressure is 1mTorr-20mTorr, SRF power is 100W-500W, BRF power is 100W-300W, SRF Reflect power is 20W-100W, and etching time is 50s-200s.

[0011] The thickness of the reflective metal Rh layer in S5 is 1 nm-200 nm.

[0012] A deep ultraviolet LED flip chip p-type reflective electrode structure comprises an epitaxial wafer structure, Ni nanoparticles and a reflective metal Rh layer, wherein the Ni nanoparticles are grown on the epitaxial wafer structure, and the reflective metal Rh layer is evaporated on the epitaxial wafer structure and the Ni nanoparticles.

[0013] The epitaxial wafer structure comprises a substrate, an AlN buffer layer, an n-type semiconductor layer, a quantum well layer, a p-type semiconductor layer and a p-type GaN contact layer, wherein the AlN buffer layer is grown on the substrate, the n-type semiconductor layer is grown on the AlN buffer layer, the quantum well layer is grown on the n-type semiconductor layer, the p-type semiconductor layer is grown on the quantum well layer, and the p-type GaN contact layer is grown on the p-type semiconductor layer.

[0014] The Ni nanoparticles are grown on the p-type GaN contact layer, the p-type GaN contact layer is etched to the p-type semiconductor layer using the Ni nanoparticles as a mask, and the reflective metal Rh layer is evaporated on the Ni nanoparticles and the p-type GaN contact layer.

[0015] Compared with the prior art, the present invention has the following beneficial effects: The present invention deposits a metal Ni layer on a p-type GaN contact layer, forms Ni nanoparticles by high-temperature annealing, etches the p-type GaN contact layer using the Ni nanoparticles as a mask, and then deposits a reflective metal Rh layer, thereby reducing GaN light absorption and increasing reflection, thereby obtaining a deep ultraviolet LED flip chip with higher light efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.

[0017] The structures, proportions, sizes, etc. illustrated in this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with the technology. They are not used to limit the conditions under which the present invention can be implemented, and therefore have no substantial technical significance. Any structural modification, change in proportion or adjustment of size shall still fall within the scope of the technical contents disclosed in the present invention without affecting the effects and purposes that can be achieved by the present invention.

[0018] Figure 1 It is a schematic diagram of the epitaxial wafer structure of the present invention; Figure 2 A schematic diagram of preparing a metal Ni layer according to the present invention; Figure 3 A schematic diagram of forming Ni nanoparticles according to the present invention; Figure 4 It is a schematic diagram of etching a p-type GaN contact layer according to the present invention; Figure 5 A schematic diagram of preparing a reflective metal Rh layer according to the present invention; Figure 6 This is a surface morphology image of the Ni nanoparticles of the present invention characterized by AFM; Figure 7 This is a height and width curve of the Ni nanoparticles of the present invention characterized by AFM.

[0019] Wherein: 101 is a substrate, 102 is an AlN buffer layer, 103 is an n-type semiconductor layer, 104 is a quantum well layer, 105 is a p-type semiconductor layer, 106 is a p-type GaN contact layer, 201 is a metal Ni layer, 202 is Ni nanoparticles, and 203 is a reflective metal Rh layer. DETAILED DESCRIPTION

[0020] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all the embodiments. These descriptions are only to further illustrate the features and advantages of the present invention, rather than to limit the claims of the present invention. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0021] The specific implementation of the present invention is further described in detail below in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0022] In this embodiment, the method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure includes the following steps: Step 1: Figure 1 As shown, an AlN buffer layer 102, an n-type semiconductor layer 103, a quantum well layer 104, a p-type semiconductor layer 105, and a p-type GaN contact layer 106 are sequentially grown on a sapphire substrate 101, and the thickness of the p-type GaN contact layer 106 is 5nm-50nm.

[0023] Step 2: Figure 2 As shown, a metal Ni layer 201 is evaporated on the p-type GaN contact layer 106. The thickness of the metal Ni layer 201 is 1nm-50nm, the rotation speed of the plating pot is 1rpm-20rpm, the coating rate is 0.1Å / s-5Å / s, and the vacuum degree is 2.0×10 -5 Torr-2.0×10 -7 Torr, the coating power is 5%-50% of the electron gun output power. In view of the island film-forming method during the growth of metal Ni, the coating rate needs to be controlled. If the coating rate is too fast, a uniform film cannot be formed. The thickness of metal Ni is related to the particle size of the Ni nanoparticles 202. If the thickness of the metal Ni film layer is too thick, the electrode will absorb light and cause the brightness to decrease, and the particle size of the formed Ni nanoparticles 202 is too large, and there is a risk of piercing the passivation layer and causing chip leakage; if the thickness of the metal Ni film layer is too thin, the particle size of the formed Ni nanoparticles 202 is too small, and the purpose of a good mask cannot be achieved. Preferably, the thickness of the metal Ni layer 201 is 5nm, the plating pot rotation speed is 7rpm, the coating rate is 0.2Å / s, and the vacuum degree is 2.0×10 -6 Torr, the coating power is 12.5% ​​of the electron gun output power.

[0024] Step 3: Figure 3As shown, the metal Ni layer 201 is subjected to high temperature annealing in a nitrogen atmosphere, the annealing temperature is 500°C-950°C, the annealing time is 30s-400s, and the nitrogen flow rate is 100 cm 3 / min -5000cm 3 / min. If the annealing temperature is low, the metal Ni layer 201 tends to form blunt balls, which are connected together and cannot expose the p-type GaN contact layer 106 to be etched. If the annealing temperature is too high, the metal Ni layer 201 tends to form sharp balls, which may pierce the passivation layer and cause the chip to leak. The formed Ni nanoparticles 202 can be used as a p-type ohmic contact electrode and as a mask for etching the exposed p-type GaN contact layer 106, breaking through the limitation of the accuracy of photoresist as an etching mask and achieving the purpose of nanometer-level etching. Preferably, the annealing temperature is 600°C, the annealing time is 180s, and the nitrogen flow rate is 2000cm 3 / min. Figure 6 , Figure 7 As shown, uniformly distributed Ni nanoparticles 202 with appropriate spacing are formed on the surface of the p-type GaN contact layer 106. The Ni nanoparticles 202 are spherical in shape, with an average diameter of 50 nm and an average spacing of 0.5 μm.

[0025] Step 4: Figure 4 As shown, the Ni nanoparticles 202 are used as a mask, and the exposed p-type GaN contact layer 106 is etched by dry etching equipment ICP. The thickness of the p-type GaN contact layer 106 is 5nm-20nm. The etching gas used by ICP is Cl2 and BCl3, and the Cl2 flow rate is 10cm 3 / min-100cm 3 / min, BCl3 flow rate is 1cm 3 / min-40cm 3 / min, working pressure is 1mTorr-20mTorr, SRF power is 100W-500W, BRF power is 100W-300W, SRFReflect power is 20W-100W, etching time is 50s-200s. Preferably, Cl2 flow rate is 85cm 3 / min, BCl3 flow rate is 5cm 3 / min, working pressure is 2mTorr, SRF power is 400W, BRF power is 185W, SRF Reflect power is 50W, and etching time is 50s.

[0026] Step 5: Figure 5As shown, a reflective metal Rh layer 203 is evaporated, and the thickness of the reflective metal Rh layer 203 is 1 nm-100 nm. Rhodium (Rh) has a high reflectivity in the deep ultraviolet band. In the 260nm-280nm band, the reflectivity of metal Rh is 65%-70%, and the work function (4.98 eV) is close to that of the p-type semiconductor layer 105, which will not lead to an increase in the chip operating voltage. And due to the reflection of metal Rh, the light emitted by the PN junction is emitted more from the sapphire surface, thereby improving the luminous efficiency of the deep ultraviolet LED flip chip. Preferably, the thickness of the reflective metal Rh layer 203 is 100 nm.

[0027] A deep ultraviolet LED flip chip p-type reflective electrode structure includes a substrate 101, an AlN buffer layer 102, an n-type semiconductor layer 103, a quantum well layer 104, a p-type semiconductor layer 105, a p-type GaN contact layer 106, Ni nanoparticles 202, and a reflective metal Rh layer 203. The AlN buffer layer 102 is grown on the substrate 101, the n-type semiconductor layer 103 is grown on the AlN buffer layer 102, the quantum well layer 104 is grown on the n-type semiconductor layer 103, the p-type semiconductor layer 105 is grown on the quantum well layer 104, and the p-type GaN contact layer 106 is grown on the p-type semiconductor layer 105. The Ni nanoparticles 202 are grown on the p-type GaN contact layer 106, the p-type GaN contact layer 106 is etched to the p-type semiconductor layer 105 using the Ni nanoparticles 202 as a mask, and the reflective metal Rh layer 203 is evaporated on the Ni nanoparticles 202 and the p-type GaN contact layer 106.

[0028] Taking a 20mil×20mil chip as an example, the deep ultraviolet LED flip chip with a p-type reflective electrode structure in this embodiment and the deep ultraviolet LED flip chip with a conventional structure in the prior art are packaged into lamp beads, and the brightness and electro-optical conversion efficiency are tested using an integrating sphere, with an integration time of 500ms and a test current of 100mA. Through the test, as shown in Table 1, compared with the deep ultraviolet LED flip chip with a conventional structure in the prior art packaged into a lamp bead, the brightness and electro-optical conversion efficiency of the lamp bead equipped with the deep ultraviolet LED flip chip with a p-type reflective electrode structure in this embodiment are greatly improved.

[0029] Table 1 Integrating sphere test results of control example and this embodiment

[0030] Only the preferred embodiments of the present invention are described in detail above, but the present invention is not limited to the above embodiments. Various changes can be made within the knowledge scope of ordinary technicians in this field without departing from the purpose of the present invention, and various changes should be included in the protection scope of the present invention.

Claims

1. A method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure, It is characterized in that The following steps are involved: S1, preparing an epitaxial wafer structure, wherein the top layer of the epitaxial wafer structure is a p-type GaN contact layer (106); S2, preparing a metal Ni layer (201) on the p-type GaN contact layer (106); S3, performing high temperature annealing on the metal Ni layer (201) to form a p-type ohmic contact, and at the same time the metal Ni layer (201) agglomerates to form Ni nanoparticles (202); S4, using the Ni nanoparticles (202) as a mask, etching the p-type GaN contact layer (106); S5. Evaporating a reflective metal Rh layer (203) on the Ni nanoparticles (202) and the p-type GaN contact layer (106), thereby completing the preparation of the p-type reflective electrode structure.

2. A method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: The method for preparing the epitaxial wafer structure in S1 is: preparing a substrate (101), an AlN buffer layer (102), an n-type semiconductor layer (103), a quantum well layer (104), a p-type semiconductor layer (105), and a p-type GaN contact layer (106) in sequence from bottom to top to form an epitaxial wafer structure.

3. The method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: The thickness of the metal Ni layer (201) in S2 is 1 nm-50 nm. The metal Ni layer (201) is evaporated on the p-type GaN contact layer (106). The rotation speed of the plating pot is 1 rpm-20 rpm, the coating rate is 0.1 Å / s-5 Å / s, and the vacuum degree is 2.0×10 -5 Torr-2.0×10 -7 Torr, the coating power is 5%-50% of the electron gun output power.

4. The method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: The metal Ni layer (201) in S3 is subjected to high temperature annealing in a nitrogen atmosphere, the annealing temperature is 500°C-950°C, the annealing time is 30s-400s, and the nitrogen flow rate is 100cm 3 / min-5000cm 3 / min.

5. The method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: The Ni nanoparticles (202) are spherical in shape, the average diameter of the Ni nanoparticles (202) is 50 nm, and the average spacing between the Ni nanoparticles (202) is 0.5 μm.

6. The method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: In S4, Ni nanoparticles (202) are used as a mask, and a dry etching device ICP is used to etch the p-type GaN contact layer (106) to the p-type semiconductor layer (105). The etching gas used by the dry etching device ICP is Cl 2 and BCl 3 , Cl 2 Flow rate is 10cm 3 / min-100cm 3 / min, BCl 3 Flow rate is 1cm 3 / min-40cm 3 / min, working pressure is 1mTorr-20mTorr, SRF power is 100W-500W, BRF power is 100W-300W, SRF Reflect power is 20W-100W, and etching time is 50s-200s.

7. The method for preparing a deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 1, Features: The thickness of the reflective metal Rh layer (203) in S5 is 1 nm-200 nm.

8. A deep ultraviolet LED flip chip p-type reflective electrode structure, Features: The invention comprises an epitaxial wafer structure, Ni nanoparticles (202) and a reflective metal Rh layer (203), wherein the Ni nanoparticles (202) are grown on the epitaxial wafer structure, and the reflective metal Rh layer (203) is evaporated on the epitaxial wafer structure and the Ni nanoparticles (202).

9. A deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 8, Features: The epitaxial wafer structure comprises a substrate (101), an AlN buffer layer (102), an n-type semiconductor layer (103), a quantum well layer (104), a p-type semiconductor layer (105) and a p-type GaN contact layer (106); the AlN buffer layer (102) is grown on the substrate (101), the n-type semiconductor layer (103) is grown on the AlN buffer layer (102), the quantum well layer (104) is grown on the n-type semiconductor layer (103), the p-type semiconductor layer (105) is grown on the quantum well layer (104), and the p-type GaN contact layer (106) is grown on the p-type semiconductor layer (105).

10. A deep ultraviolet LED flip chip p-type reflective electrode structure according to claim 9, Features: The Ni nanoparticles (202) are grown on a p-type GaN contact layer (106); the p-type GaN contact layer (106) is etched to the p-type semiconductor layer (105) using the Ni nanoparticles (202) as a mask; and the reflective metal Rh layer (203) is evaporated on the Ni nanoparticles (202) and the p-type GaN contact layer (106).