Forging method for improving yield of large-specification free cutting steel

By peeling off the iron oxide scale and impurities in the forging of large-size easy-cut steel, preliminary pressing and chopping of the large and small head ends, and positioning, enlarging forging and grinding during forging, the problem of low yield of easy-cut steel is solved and significantly improved. The yield rate and steel utilization rate are improved, and surface defects and waste are reduced.

CN118744216APending Publication Date: 2024-10-08SHOUGANG GUIYANG SPECIAL STEEL
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410915433.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-09
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The yield rate of large-sized easy-to-cut steel is too low. The surface defects of the steel after forging are large, difficult to grind and do not meet the delivery size, which affects the yield rate.

Method used

During the forging process, the iron oxide scale and impurities are peeled off, and the large and small head ends are initially pressed and chopped. The large head end is retained, and then is positioned and enlarged during the forging, and the size is adjusted after grinding so that the large and small head ends are in line with the middle. Partially consistent.

Benefits of technology

It improves the yield rate of easy-to-cut steel, reduces surface defects and slag inclusions, improves steel utilization, reduces cutting waste, and increases the yield rate by 1 to 2 points.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744216A_ABST
    Figure CN118744216A_ABST
Patent Text Reader

Abstract

The invention discloses a forging method for improving the yield of large-specification free cutting steel. The forging method comprises the following steps: (1) firstly stripping oxide scale and impurities on the surface of a steel ingot during cogging; (2) pressing downwards from the large-head end of the steel ingot at a certain distance, forging from inside to outside, cutting off slag inclusion at the tail part of the large-head end and retaining most of the large-head end, and then cogging the rest part; (3) positioning the large end and the small end of the steel ingot during forging, and performing size amplification forging on the end parts positioned at the two ends during forging; and (4) the amplified and forged part is ground on a round steel grinding machine, and the ground size is kept consistent with the size of the middle part of the steel ingot. The steel utilization rate of the ends of the two ends of the free-cutting steel is increased, waste of cut ends is reduced, the yield of steel ingots is high, the yield of large-specification free-cutting steel can be increased by 1-2 points, and the yield of the steel ingots is maximized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a forging method for improving the yield rate of large-size free-cutting steel, belonging to the technical field of metallurgy. Background Art

[0002] For a long time, the yield rate of die-cast free-cutting steel ingots after heating and forging has been too low. This is mainly manifested in that after the large and small heads at both ends of the ingot are cut off on the forging machine, the yield rate of free-cutting steel produced by the remaining steel is low. However, after retaining the large and small heads at both ends and producing large-size forgings, the forgings produced have large surface defects due to the large slag inclusions at the large and small heads at both ends. Grinding is difficult and the grinding depth is too deep. After grinding, the delivery size cannot be met, and the parts that do not meet the delivery requirements must be cut off on the sawing machine, which has a particularly large impact on the yield rate of free-cutting steel. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a forging method for improving the yield rate of large-size (φ300-φ600) free-cutting steel, thereby solving the problem of too low yield rate of large-size (φ300-φ600) free-cutting steel after forging.

[0004] In order to solve the above technical problems, the technical solution of the present invention is as follows:

[0005] A forging method for improving the yield rate of large-size free-cutting steel comprises the following steps:

[0006] (1) When forging, the steel ingot is hammered lightly and slowly on the forging machine to peel off the iron oxide scale and impurities on the surface of the steel ingot;

[0007] (2) Press down a certain distance from the big end of the ingot, and forge from the inside to the outside. After the initial pressing down of the distance is completed, the big end is chopped on the hammer, and the chopping length is 50mm-500mm. The slag at the tail of the big end is cut off and most of the big end is retained. Then the remaining part of the blank is opened, and the small end is not chopped;

[0008] (3) The finished steel ingot is returned to the furnace for heating, and then taken out of the furnace for forging after the holding time is reached; during forging, the large end and the small end of the steel ingot are first positioned, and the end parts positioned at both ends are enlarged and forged during forging, with the positioning length being 500mm-1500mm, and the middle part of the steel ingot is forged according to the required size;

[0009] (4) Grind the enlarged forged parts of the large and small ends on a round steel grinding machine so that the size after grinding is consistent with the size of the middle part of the ingot.

[0010] Preferably, in step (2), the distance measured from the large end of the steel ingot is 50 mm to 500 mm.

[0011] As a preferred embodiment, in step (3), the positioning distance between the large end and the small end is 0.5m-1.5m.

[0012] Beneficial effect: The present invention takes the retention of large free-cutting steel risers as a breakthrough for improving the yield rate of free-cutting steel, and is a new method for improving the forging of large free-cutting steel. This method performs a small amount of chopping of the cut heads at the ends of the large and small heads to retain the excess cut heads, and then enlarges the two ends of the large and small heads during forging, and then grinds them, so that the surface defects of the free-cutting steel after grinding are greatly reduced, and the ends of the large and small heads are free of inclusions and defects, thereby greatly improving the yield rate of free-cutting steel.

[0013] Compared with the prior art, the present invention has a high steel utilization rate at both ends of the easy-to-cut steel forged by this "enlargement method", a high steel ingot yield rate, reduced waste of cut heads, and improved steel utilization rate at large and small heads. The yield rate of large-size easy-to-cut steel can be increased by 1 to 2 points, thereby maximizing the steel ingot yield rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a photo of the forging site of the present invention. DETAILED DESCRIPTION

[0015] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation mode, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.

[0016] Example 1: Take the die-cast 1141 large free-cutting steel with a forging diameter of φ400 as an example. The raw material ingot of the die-cast steel ingot is an 11-ton ingot. During production, the steel ingot is first heated and then blanked. The ingot is blanked to 550 cubic meters and then returned to the furnace for heating. The specific steps are:

[0017] The first step is to hammer the steel ingot slowly on the forging machine to peel off the oxidized iron scale and impurities, and then press down from one end (usually the big end) at a distance of 500mm. The amount of pressure should not be too large, and forging should be performed from the inside to the outside until the initial pressure of 500mm is completed. The big end is chopped on the hammer, but no extra chopping is done. The chopping length is 50mm-500mm. Most of the big end should be retained, and the slag at the tail of the big end should be cut off (depending on the amount of slag). After the slag is cut off, the remaining part of the blank is opened. The blank is opened to 550 square meters uniformly, and the small end is not chopped, but it should also be opened in this way;

[0018] The second step is to return the steel ingot to the furnace for heating, and then take it out of the furnace for forging after the insulation time is reached. When forging, the large end and the small end should be positioned first. For the easy-to-cut steel with a diameter of φ400, the distance of 0.5m to 1m should be measured at the end for positioning. After positioning, attention should be paid to the forging size during forging. The end parts located at both ends should be enlarged and forged to φ450 circle, and the middle part can be forged according to the size of φ400 circle;

[0019] In the third step, the free-cutting steel after forging will appear large at both ends and small in the middle. When it is ground on the round steel grinding machine later, the enlarged (enlarged forging) part will be ground. The grinding standard is based on the outer diameter of the φ400 circle.

[0020] After inspection, it was found that the surface defects of the free-cutting steel were greatly reduced after grinding, and the steel utilization rate of the large and small heads was high. After ultrasonic testing, there were no inclusions and defects in the large and small heads, which fully met the use requirements.

[0021] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A forging method for improving the yield rate of large-size free-cutting steel, characterized in that: The following steps are involved: (1) When forging, the steel ingot is hammered lightly and slowly on the forging machine to peel off the iron oxide scale and impurities on the surface of the steel ingot; (2) Press down a certain distance from the big end of the ingot, and forge from the inside to the outside. After the initial downward pressing is completed, the big end is chopped on the hammer, and the chopping length is 50mm-500mm. The slag at the tail of the big end is cut off and most of the big end is retained. Then the remaining part of the blank is opened, and the small end is not chopped; (3) The steel ingot is returned to the furnace for heating and then taken out of the furnace for forging after the holding time is reached; during forging, the large end and the small end of the steel ingot are first positioned, and the end parts positioned at both ends are enlarged and forged during forging, and the middle part of the steel ingot is forged according to the required size; (4) Grind the enlarged forged parts of the large and small ends on a round steel grinding machine so that the size after grinding is consistent with the size of the middle part of the steel ingot.

2. The forging method for improving the yield rate of large-size free-cutting steel according to claim 1, characterized in that: In the step (2), the distance measured from the large end of the steel ingot is 300-500 mm.

3. The forging method for improving the yield rate of large-size free-cutting steel according to claim 1, characterized in that: In the step (3), the positioning distance between the large end and the small end is 0.5m-1m.

Citation Information

Patent Citations

  • Hot extrusion forging equipment and method for axle tube

    CN102248111A

  • Forging method of cylindrical slide sleeve and reverse extrusion mould

    CN102814440A

  • Forging method for improving yield of 30CrNiMo8 motor rotating shaft steel billet

    CN118268821A

  • Method for the manufacture of heavy-duty components by precision forging

    EP1671719A1