Substrate detection method and system for intelligent Internet of Things bonding silver wire production equipment
Through the intelligent Internet of Things system combined with a variety of detection instruments, automated detection of the substrate surface, oxide layer thickness, dielectric strength, thermal expansion and strength is realized, which solves the instability and subjectivity problems of traditional manual detection methods and improves production efficiency. and product quality.
Patent Information
- Application Number
- CN202410691635.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-30
- Publication Date
- 2024-10-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The traditional substrate inspection method of bonded silver wire production equipment relies on manual visual inspection, which is unstable and susceptible to subjective factors, and is difficult to meet the needs of high efficiency and high stability.
Using an intelligent IoT system, a three-dimensional laser scanner is used to detect the surface of the substrate. Combined with an anodizing thickness gauge, a withstand voltage analyzer, a thermal expansion meter and a push-pull force tester, the substrate's oxide layer thickness, dielectric strength, thermal expansion coefficient and Strength, forming an automated detection process.
It improves the efficiency and stability of substrate detection, can quickly screen out unqualified substrates, and ensures the improvement of product quality.
Smart Images

Figure CN118746321A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of intelligent silver bonding wire processing, and in particular to a substrate detection method and system for intelligent Internet of Things silver bonding wire production equipment. Background Art
[0002] Silver bonding wire is a kind of precision metal wire used in microelectronic packaging and semiconductor manufacturing. It is mainly used to replace traditional gold bonding wire as an interconnection material inside the chip or between the chip and external leads. In recent years, it has gradually attracted attention as a low-cost alternative to gold wire, especially in the LED and integrated circuit (IC) industries.
[0003] The traditional substrate detection method for silver bonding wire production equipment mainly relies on manual visual inspection, which manually identifies whether there are abnormalities in the substrate. Manual visual inspection has problems such as instability and susceptibility to subjective factors, which is not convenient for meeting the needs of high efficiency and high stability in production. Therefore, an intelligent and automated substrate detection method is needed to improve production efficiency and product quality. Based on this, the present application provides a substrate detection method and system for intelligent Internet of Things silver bonding wire production equipment.
[0004] It should be noted that the information disclosed in the background technology section of this application is only intended to deepen the understanding of the general background technology of this application, and should not be regarded as an admission or suggestion in any form that the information constitutes prior art already known to those skilled in the art. Summary of the invention
[0005] The present invention is used to improve the traditional substrate detection method of bonding silver wire production equipment, which mainly relies on manual visual inspection, has problems such as instability and susceptibility to subjective factors, and is not convenient for meeting the needs of high efficiency and high stability in production. Based on this, the present application provides a substrate detection method and system for intelligent Internet of Things bonding silver wire production equipment.
[0006] In the first aspect, the present application provides a substrate detection method for a smart IoT bonding silver wire production equipment, which adopts the following technical solutions, including:
[0007] When it is detected that the substrate moves to the designated position of the detection platform, the three-dimensional point data of the substrate is detected according to the three-dimensional laser scanner, and whether the surface of the substrate is normal is determined according to the three-dimensional point data;
[0008] If the substrate surface is normal, the substrate is sunk into the anodizing solution and the thickness of the oxide layer of the substrate is measured using an anodizing thickness gauge;
[0009] If the oxide layer thickness is within the preset standard thickness range, the breakdown voltage of the substrate is detected by the withstand voltage analyzer, and the dielectric strength of the substrate is determined to be normal based on the breakdown voltage;
[0010] If the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the thermal expansion coefficient of the substrate using a thermal expansion meter;
[0011] If the thermal expansion coefficient is within the preset standard expansion coefficient range, the solder joint position of the substrate is sheared according to the push-pull force tester to obtain the maximum shear force, and whether the substrate strength is normal is determined according to the maximum shear force.
[0012] By adopting the above technical solution, the system obtains three-dimensional point data of the substrate by scanning the substrate in three dimensions, and determines whether the basic surface is abnormal through the three-dimensional point data. Then the system sinks the substrate into the anodizing liquid, and detects the oxide layer thickness of the substrate through the anodizing thickness gauge to determine whether the oxide layer thickness is abnormal. Then the system cleans the substrate and detects the breakdown voltage of the substrate through the voltage analyzer to determine whether the dielectric strength of the substrate is normal. The system then heats the substrate, calculates the thermal expansion coefficient of the substrate according to the deformation of the substrate, and determines whether the thermal expansion of the substrate is normal. Finally, the system shears the solder joint position of the substrate, and determines whether the substrate strength is normal according to the maximum shear force, thereby detecting the surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate, thereby facilitating the rapid screening of unqualified substrates, so as to form an automated substrate detection process, thereby greatly improving the efficiency and stability of substrate detection.
[0013] Optionally, when detecting that the substrate moves to a specified position of the detection table, detecting three-dimensional point data of the substrate according to a three-dimensional laser scanner, and determining whether the surface of the substrate is normal according to the three-dimensional point data, includes:
[0014] Move the substrate to a designated position of the detection platform, and detect the three-dimensional point data of the substrate using a three-dimensional laser scanner, wherein the three-dimensional point data at least includes three-dimensional point coordinates;
[0015] Determine the abnormal 3D points with differences according to the preset matching standard, the standard 3D point data and the 3D point data;
[0016] Determine the number of abnormal three-dimensional points corresponding to each area according to the different colors of the substrate oxide layer, the coating layer, and the base material and the coordinates of the abnormal three-dimensional points;
[0017] According to the preset number of regional 3D points and the number of abnormal 3D points, the ratio of the number of regional 3D points and the number of abnormal 3D points corresponding to each region is calculated to obtain a difference percentage;
[0018] If the difference percentage is not greater than the preset standard ratio, the substrate surface is judged to be normal, otherwise, the substrate surface is judged to be abnormal.
[0019] By adopting the above technical solution, when the system detects that the substrate moves to the center of the detection table according to the pressure sensor, the system detects the three-dimensional point data of the substrate according to the three-dimensional laser scanner, and determines the area and number of abnormal three-dimensional points according to the matching standard, so as to facilitate the calculation of the proportion of abnormal three-dimensional points in each area, and then facilitate the judgment of whether the surface of the substrate is normal according to the proportion of abnormal three-dimensional points, so as to facilitate the screening of substrates with abnormal surfaces.
[0020] Optionally, if the substrate surface is detected to be normal, the substrate is sunk into an anodic oxidation solution, and the thickness of the oxide layer of the substrate is detected using an anodic oxidation thickness gauge, including:
[0021] If the substrate surface is detected to be normal, the substrate is sunk into the anodizing solution;
[0022] Detecting the thickness of the center and designated points of the oxide layer of the substrate using an anodizing thickness gauge to obtain the oxide layer thickness corresponding to each point;
[0023] If the ratio of the oxide layer thicknesses at each point is within a preset standard thickness ratio range, the average oxide layer thickness is calculated based on the oxide layer thicknesses at each point.
[0024] By adopting the above technical solution, the system sinks the substrate into the anodizing liquid, and detects the thickness of the center and four corners of the substrate oxide layer according to the anodizing thickness gauge, obtains the oxide layer thickness corresponding to the five points, and then calculates the average oxide layer thickness based on the oxide layer thickness, so as to judge whether the substrate oxide layer is normal.
[0025] Optionally, if the oxide layer thickness is within a preset standard thickness range, detecting the breakdown voltage of the substrate using a withstand voltage analyzer, and judging whether the dielectric strength of the substrate is normal according to the breakdown voltage, includes:
[0026] If the average thickness of the oxide layer is within the standard thickness range, the substrate is cleaned and moved to a withstand voltage analyzer;
[0027] Applying a voltage to the substrate oxide layer according to a withstand voltage analyzer until the substrate oxide layer is broken down, thereby obtaining the breakdown voltage;
[0028] Detecting the base thickness of the substrate using a three-dimensional laser scanner;
[0029] Calculating the dielectric strength of the substrate according to the substrate thickness, the breakdown voltage and the average thickness of the oxide layer;
[0030] If the dielectric strength is within a preset strength range, it is determined that the dielectric strength of the substrate is normal; otherwise, it is determined that the dielectric strength of the substrate is abnormal.
[0031] By adopting the above technical solution, after the system detects that the oxide layer of the substrate is normal, the system cleans the substrate to remove the anodic oxidation liquid on the surface of the substrate. The system then applies voltage to the oxide layer of the substrate according to the voltage withstand analyzer until the oxide layer of the substrate is broken down and the breakdown voltage is detected. The system calculates the dielectric strength of the substrate based on the substrate thickness, the breakdown voltage and the average thickness of the oxide layer, thereby determining whether the dielectric strength of the substrate is normal, so as to screen out substrates with abnormal dielectric strength.
[0032] Optionally, if the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the thermal expansion coefficient of the substrate using a thermal expansion meter includes:
[0033] Detect the coating length of the substrate using a three-dimensional laser scanner and determine the corresponding initial temperature;
[0034] If the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the length of the high-temperature coating when the substrate is at a high temperature;
[0035] The thermal expansion coefficient is calculated according to the coating length, the initial temperature, the designated temperature, and the high-temperature coating length.
[0036] By adopting the above technical solution, the system detects the coating length of the substrate and the corresponding initial temperature according to the three-dimensional laser scanner. The system then heats the substrate to a specified temperature in the high-temperature operating state and detects the high-temperature coating length of the substrate, thereby facilitating the system to plan the thermal expansion coefficient of the substrate coating, so as to screen out substrates with abnormal thermal expansion.
[0037] Optionally, before shearing the solder joint position of the substrate according to the push-pull force tester to obtain the maximum shear force if the thermal expansion coefficient belongs to the preset standard expansion coefficient range, and judging whether the strength of the substrate is normal according to the maximum shear force, the method further includes:
[0038] Detecting the areas of the solder joints of the substrate to be detected by the three-dimensional laser scanner, and obtaining the areas of the solder joints corresponding to the solder joints one by one;
[0039] If the ratio of the soldering point area of each soldering point to the preset standard area is within the preset standard area ratio range, then it is determined that the soldering point area is normal.
[0040] By adopting the above technical solution, the system detects the solder joint area of the substrate through a three-dimensional laser scanner, thereby facilitating the determination of whether the solder joint area of the substrate is normal, so as to facilitate the subsequent calculation of the strength of the substrate.
[0041] Optionally, if the thermal expansion coefficient is within a preset standard expansion coefficient range, shearing the solder joint position of the substrate according to a push-pull force tester to obtain a maximum shear force, and judging whether the strength of the substrate is normal according to the maximum shear force includes:
[0042] If the thermal expansion coefficient is within the standard expansion coefficient range, a horizontal shear force is applied to the solder joint position of the substrate according to the sensor splitter of the push-pull force tester until the solder joint is damaged, thereby obtaining the maximum shear force before the solder joint is damaged;
[0043] If the solder joint area is normal, the maximum shear force corresponding to each solder joint and the solder joint area are divided to obtain the shear strength corresponding to the solder joint;
[0044] If the difference between the shear strength corresponding to each solder joint and the preset standard solder joint strength is within the preset strength difference range, the substrate strength is judged to be normal; otherwise, the substrate strength is judged to be abnormal.
[0045] By adopting the above technical solution, the system applies horizontal shear force to the solder joint position of the substrate according to the sensor chopper of the push-pull force tester until the solder joint is damaged, and obtains the maximum shear force before the solder joint is damaged. The maximum shear force is then divided by the solder joint area to obtain the shear strength. The system determines whether the strength of the substrate is normal based on the shear strength, thereby facilitating the rapid screening of substrates with abnormal strength.
[0046] In the second aspect, the present application provides a substrate detection device for an intelligent Internet of Things bonding silver wire production equipment, which adopts the following technical solutions, including:
[0047] A three-dimensional scanning module is used to detect three-dimensional point data of the substrate according to a three-dimensional laser scanner when the substrate is detected to move to a specified position of the detection table, and determine whether the surface of the substrate is normal according to the three-dimensional point data;
[0048] The substrate oxidation module is used to sink the substrate into the anodic oxidation liquid if the substrate surface is detected to be normal, and detect the thickness of the oxide layer of the substrate according to the anodic oxidation thickness gauge;
[0049] The substrate dielectric module is used to detect the breakdown voltage of the substrate according to the withstand voltage analyzer if the oxide layer thickness is within the preset standard thickness range, and to determine whether the dielectric strength of the substrate is normal according to the breakdown voltage;
[0050] A substrate expansion module, used for heating the substrate to a specified temperature if the dielectric strength of the substrate is normal, and detecting the thermal expansion coefficient of the substrate according to a thermal expansion meter;
[0051] The substrate strength module is used to shear the solder joint position of the substrate according to the push-pull force tester if the thermal expansion coefficient belongs to the preset standard expansion coefficient range, obtain the maximum shear force, and judge whether the substrate strength is normal according to the maximum shear force.
[0052] By adopting the above technical solution, the system obtains three-dimensional point data of the substrate by scanning the substrate in three dimensions, and determines whether the basic surface is abnormal through the three-dimensional point data. Then the system sinks the substrate into the anodizing liquid, and detects the oxide layer thickness of the substrate through the anodizing thickness gauge to determine whether the oxide layer thickness is abnormal. Then the system cleans the substrate and detects the breakdown voltage of the substrate through the voltage analyzer to determine whether the dielectric strength of the substrate is normal. The system then heats the substrate, calculates the thermal expansion coefficient of the substrate according to the deformation of the substrate, and determines whether the thermal expansion of the substrate is normal. Finally, the system shears the solder joint position of the substrate, and determines whether the substrate strength is normal according to the maximum shear force, thereby detecting the surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate, thereby facilitating the rapid screening of unqualified substrates, so as to form an automated substrate detection process, thereby greatly improving the efficiency and stability of substrate detection.
[0053] In a third aspect, the present application further provides a control device, the device comprising:
[0054] It includes a memory and a processor, and the memory stores a computer program that can be loaded and executed by the processor, such as the above-mentioned method for detecting substrates of intelligent Internet of Things bonding silver wire production equipment.
[0055] In a fourth aspect, the present application also provides a computer-readable storage medium storing a computer program that can be loaded by a processor and execute the above-mentioned intelligent Internet of Things bonding silver wire production equipment substrate detection method.
[0056] In summary, the present application includes at least one of the following beneficial technical effects:
[0057] 1. Test the surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate, so as to quickly screen out unqualified substrates and form an automated substrate testing process, which greatly improves the efficiency and stability of substrate testing.
[0058] 2. Calculate the dielectric strength of the substrate based on the substrate thickness, breakdown voltage and average thickness of the oxide layer to determine whether the dielectric strength of the substrate is normal, so as to screen out substrates with abnormal dielectric strength.
[0059] 3. Judge whether the substrate strength is normal based on the shear strength of the solder joint, so as to quickly screen out substrates with abnormal strength.
[0060] Explanation of reference numerals: 210, three-dimensional scanning module; 220, substrate oxidation module; 230, substrate dielectric module; 240, substrate expansion module; 250, substrate strength module. BRIEF DESCRIPTION OF THE DRAWINGS
[0061] Figure 1 This is a flow chart of a method for detecting substrates of a smart Internet of Things bonding silver wire production equipment according to the present application.
[0062] Figure 2 This is a structural block diagram of a substrate detection device for intelligent Internet of Things bonding silver wire production equipment in the present application. DETAILED DESCRIPTION
[0063] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0064] The working principle of 3D laser scanners is mainly based on laser ranging technology. This device emits a laser pulse, which is reflected back when it encounters the surface of an object and is captured by the scanner's receiver. By measuring the time from the laser pulse being emitted to the time it is reflected back to the scanner, combined with the principle of constant light speed, the distance between the scanner and the object being measured can be calculated. In order to obtain more comprehensive data, 3D laser scanners are usually equipped with mechanical components that can guide the laser beam scanning, such as reflective prisms or rotating plane mirrors. These mechanical components rotate at high speed, allowing the scanner to obtain a large amount of dense point cloud data in a short period of time. These point cloud data include information such as the 3D coordinates, reflectivity, and texture of each point. By processing this data, the 3D model of the target being measured and various drawing data such as lines, surfaces, and bodies can be quickly reconstructed.
[0065] The embodiment of the present application adopts a sensor network of an intelligent production system. By installing suitable sensors in the production system, the parameters in the production process can be monitored in real time. The system obtains the three-dimensional point data of the substrate by scanning the three-dimensional substrate, detects the oxide layer thickness of the substrate by an anodizing thickness gauge, detects the breakdown voltage of the substrate by a withstand voltage analyzer, heats the substrate, calculates the thermal expansion coefficient of the substrate according to the deformation of the substrate, judges whether the thermal expansion of the substrate is normal, and judges whether the substrate strength is normal according to the maximum shear force by shearing the solder joint position of the substrate, thereby detecting the surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate, and then facilitates the rapid screening of unqualified substrates, so as to form an automated substrate detection process, which greatly improves the efficiency and stability of substrate detection. It should be understood that the various preset standards and ranges mentioned in the embodiment of the present application are all set in advance by the manufacturer according to the test.
[0066] Reference Figure 1 , a method for detecting a substrate of an intelligent Internet of Things bonding silver wire production equipment, comprising at least steps S10 to S50.
[0067] S10, when it is detected that the substrate moves to the designated position of the detection platform, the three-dimensional point data of the substrate is detected according to the three-dimensional laser scanner, and whether the surface of the substrate is normal is determined according to the three-dimensional point data.
[0068] S20, if the substrate surface is detected to be normal, the substrate is sunk into the anodizing solution, and the thickness of the oxide layer of the substrate is detected by an anodizing thickness gauge;
[0069] S30, if the oxide layer thickness is within a preset standard thickness range, detecting the breakdown voltage of the substrate using a withstand voltage analyzer, and determining whether the dielectric strength of the substrate is normal based on the breakdown voltage;
[0070] S40, if the dielectric strength of the substrate is normal, heating the substrate to a specified temperature, and detecting the thermal expansion coefficient of the substrate using a thermal expansion meter;
[0071] S50, if the thermal expansion coefficient is within the preset standard expansion coefficient range, shear the solder joint position of the substrate according to the push-pull force tester to obtain the maximum shear force, and judge whether the strength of the substrate is normal according to the maximum shear force.
[0072] Specifically, the system obtains three-dimensional point data of the substrate by scanning the substrate in three dimensions, and determines whether the basic surface is abnormal through the three-dimensional point data. Then the system sinks the substrate into the anodizing liquid, and detects the thickness of the oxide layer of the substrate through the anodizing thickness gauge to determine whether the oxide layer thickness is abnormal. Then the system cleans the substrate and detects the breakdown voltage of the substrate through the voltage analyzer to determine whether the dielectric strength of the substrate is normal. The system then heats the substrate, calculates the thermal expansion coefficient of the substrate according to the deformation of the substrate, and determines whether the thermal expansion of the substrate is normal. Finally, the system shears the solder joint position of the substrate and determines whether the substrate strength is normal according to the maximum shear force. The surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate are detected, which facilitates the rapid screening of unqualified substrates, so as to form an automated substrate detection process, which greatly improves the efficiency and stability of substrate detection.
[0073] In some embodiments, step S10 includes at least the following steps: moving the substrate to a specified position on the detection table, and detecting the three-dimensional point data of the substrate according to a three-dimensional laser scanner, the three-dimensional point data including at least the three-dimensional point coordinates; determining the abnormal three-dimensional points where differences occur according to a preset matching standard, standard three-dimensional point data and three-dimensional point data; determining the number of abnormal three-dimensional points corresponding to each area according to the different colors of the substrate's oxide layer, coating, and base material and the coordinates of the abnormal three-dimensional points; calculating the ratio of the number of regional three-dimensional points corresponding to each area and the number of abnormal three-dimensional points according to the preset number of regional three-dimensional points and the number of abnormal three-dimensional points, and obtaining the difference percentage; if the difference percentage is not greater than the preset standard ratio, the substrate surface is judged to be normal, otherwise, the substrate surface is judged to be abnormal.
[0074] Specifically, when the system detects that the substrate has moved to the center of the inspection table according to the pressure sensor, the system detects the three-dimensional point data of the substrate according to the three-dimensional laser scanner, and determines the area and number of abnormal three-dimensional points according to the matching criteria, so as to facilitate calculation of the proportion of abnormal three-dimensional points in each area, and then to judge whether the surface of the substrate is normal according to the proportion of abnormal three-dimensional points, so as to screen out substrates with abnormal surfaces.
[0075] In some embodiments, step S20 includes at least the following steps: if the substrate surface detection is normal, sinking the substrate into the anodizing liquid; detecting the thickness of the center and the specified point of the substrate oxide layer according to the anodizing thickness gauge, and obtaining the oxide layer thickness corresponding to each point; if the ratio of the oxide layer thickness of each point is within the preset standard thickness ratio range, calculating the average oxide layer thickness according to the oxide layer thickness of each point.
[0076] Specifically, the system sinks the substrate into the anodizing liquid, and uses the anodizing thickness gauge to detect the thickness of the substrate's oxide layer at the center and four corners, obtains the oxide layer thickness corresponding to the five points, and then calculates the average oxide layer thickness based on the oxide layer thickness, so as to determine whether the substrate's oxide layer is normal.
[0077] In some embodiments, step S30 includes at least the following steps: if the average thickness of the oxide layer is within the standard thickness range, the substrate is cleaned and the substrate is moved to a withstand voltage analyzer; a voltage is applied to the oxide layer of the substrate according to the withstand voltage analyzer until the oxide layer of the substrate is broken down to obtain a breakdown voltage; the substrate thickness is detected according to a three-dimensional laser scanner; the dielectric strength of the substrate is calculated based on the substrate thickness, the breakdown voltage and the average thickness of the oxide layer; if the dielectric strength is within the preset strength range, the dielectric strength of the substrate is judged to be normal, otherwise, the dielectric strength of the substrate is judged to be abnormal.
[0078] The calculation formula of dielectric strength is: A = U / (d*0.782+d0*0.218);
[0079] A-dielectric strength (kV / mm), U-breakdown voltage (kV), d-substrate oxide layer thickness (mm) d0-substrate thickness (mm).
[0080] Specifically, after detecting that the oxide layer of the substrate is normal, the system cleans the substrate to remove the anodic oxidation liquid on the surface of the substrate. The system then applies voltage to the oxide layer of the substrate according to the voltage withstand analyzer until the oxide layer of the substrate is broken down and the breakdown voltage is detected. The system calculates the dielectric strength of the substrate based on the substrate thickness, breakdown voltage and average thickness of the oxide layer, thereby determining whether the dielectric strength of the substrate is normal, so as to screen out substrates with abnormal dielectric strength.
[0081] In some embodiments, step S40 includes at least the following steps: detecting the coating length of the substrate according to a three-dimensional laser scanner and determining the corresponding initial temperature; if the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the high-temperature coating length when the substrate is at high temperature; calculating the thermal expansion coefficient according to the coating length, initial temperature, specified temperature and high-temperature coating length.
[0082] The calculation formula of thermal expansion coefficient is:
[0083]
[0084] α—thermal expansion coefficient ( / ℃); L0—coating length of substrate (μm); L—high-temperature coating length of substrate at specified temperature (μm); T0—initial temperature of substrate coating (℃); T—specified temperature of substrate coating (℃).
[0085] Specifically, the system detects the coating length of the substrate and the corresponding initial temperature based on the 3D laser scanner. The system then heats the substrate to a specified temperature in the high-temperature operating state and detects the high-temperature coating length of the substrate, thereby facilitating the system to plan the thermal expansion coefficient of the substrate coating, so as to screen out substrates with abnormal thermal expansion.
[0086] In some embodiments, considering the detection of the area of the solder joint, the corresponding processing steps are as follows: the area of the solder joint of the substrate to be detected is detected by a three-dimensional laser scanner to obtain the solder joint area corresponding to the solder joint one by one; if the ratio of the solder joint area of each solder joint to the preset standard area is within the preset standard area ratio range, then the solder joint area is judged to be normal.
[0087] Specifically, the system detects the solder joint area of the substrate through a three-dimensional laser scanner, thereby facilitating the determination of whether the solder joint area of the substrate is normal, so as to facilitate the subsequent calculation of the strength of the substrate.
[0088] In some embodiments, step S50 includes at least the following steps: if the thermal expansion coefficient is within the standard expansion coefficient range, a horizontal shear force is applied to the solder joint position of the substrate according to the sensor splitter of the push-pull force tester until the solder joint is damaged, thereby obtaining the maximum shear force before the solder joint is damaged; if the solder joint area is normal, the maximum shear force corresponding to each solder joint and the solder joint area are divided to obtain the shear strength corresponding to the solder joint; if the difference between the shear strength corresponding to each solder joint and the preset standard solder joint strength is within the preset strength difference range, the substrate strength is judged to be normal; otherwise, the substrate strength is judged to be abnormal.
[0089] Specifically, the system applies horizontal shear force to the solder joint position of the substrate according to the sensor chopper of the push-pull force tester until the solder joint is destroyed, and obtains the maximum shear force before the solder joint is destroyed. The maximum shear force is then divided by the solder joint area to obtain the shear strength. The system determines whether the strength of the substrate is normal based on the shear strength, thereby facilitating the rapid screening of substrates with abnormal strength.
[0090] In summary, the implementation principle of the substrate detection method of an intelligent Internet of Things bonding silver wire production equipment in an embodiment of the present application is as follows: the system obtains three-dimensional point data of the substrate by scanning the substrate in three dimensions, and determines whether the basic surface is abnormal through the three-dimensional point data. Then the system sinks the substrate into the anodizing liquid, and detects the oxide layer thickness of the substrate through an anodizing thickness gauge to determine whether the oxide layer thickness is abnormal. Then the system cleans the substrate and detects the breakdown voltage of the substrate through a withstand voltage analyzer to determine whether the dielectric strength of the substrate is normal. The system then heats the substrate, calculates the thermal expansion coefficient of the substrate according to the deformation of the substrate, and determines whether the thermal expansion of the substrate is normal. Finally, the system shears the solder joint position of the substrate, and determines whether the substrate strength is normal according to the maximum shear force, thereby detecting the surface, oxide layer thickness, dielectric strength, thermal expansion and substrate strength of the substrate, thereby facilitating the rapid screening out of unqualified substrates, so as to form an automated substrate detection process, which greatly improves the efficiency and stability of substrate detection.
[0091] Figure 1 FIG. 1 is a flow chart of a method for detecting a substrate of a silver wire production equipment for bonding in an intelligent Internet of Things in one embodiment. It should be understood that although Figure 1 The steps in the flowchart are shown in sequence as indicated by the arrows, but the steps are not necessarily executed in the order indicated by the arrows; unless otherwise specified in this document, there is no strict order restriction for the execution of the steps, and the steps may be executed in other orders; and Figure 1 At least part of the steps may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least part of the sub-steps or stages of other steps.
[0092] Based on the same technical concept, Figure 2 The embodiment of the present application also provides a substrate detection device for an intelligent Internet of Things bonding silver wire production equipment, which adopts the following technical solution, and the device includes:
[0093] The three-dimensional scanning module 210 is used to detect the three-dimensional point data of the substrate according to the three-dimensional laser scanner when the substrate is detected to move to the specified position of the detection table, and determine whether the surface of the substrate is normal according to the three-dimensional point data;
[0094] The substrate oxidation module 220 is used to sink the substrate into the anodic oxidation liquid if the substrate surface is detected to be normal, and detect the thickness of the oxide layer of the substrate using an anodic oxidation thickness gauge;
[0095] The substrate dielectric module 230 is used to detect the breakdown voltage of the substrate according to the withstand voltage analyzer if the oxide layer thickness is within the preset standard thickness range, and determine whether the dielectric strength of the substrate is normal according to the breakdown voltage;
[0096] The substrate expansion module 240 is used to heat the substrate to a specified temperature if the dielectric strength of the substrate is normal, and detect the thermal expansion coefficient of the substrate according to a thermal expansion meter;
[0097] The substrate strength module 250 is used to shear the solder joint position of the substrate according to the push-pull force tester to obtain the maximum shear force if the thermal expansion coefficient is within the preset standard expansion coefficient range, and determine whether the substrate strength is normal according to the maximum shear force.
[0098] In some embodiments, the 3D scanning module 210 is specifically used to move the substrate to a specified position of the detection platform, and detect the 3D point data of the substrate according to the 3D laser scanner, and the 3D point data at least includes the 3D point coordinates;
[0099] According to the preset matching standard, the standard 3D point data and the 3D point data, determining the abnormal 3D points with differences;
[0100] According to the different colors of the substrate oxide layer, the coating layer, and the base material and the coordinates of the abnormal three-dimensional points, the number of abnormal three-dimensional points corresponding to each area is determined;
[0101] According to the preset number of regional 3D points and the number of abnormal 3D points, the ratio of the number of regional 3D points and the number of abnormal 3D points corresponding to each region is calculated to obtain the difference percentage;
[0102] If the difference percentage is not greater than the preset standard ratio, the substrate surface is judged to be normal, otherwise, the substrate surface is judged to be abnormal.
[0103] In some embodiments, the substrate oxidation module 220 is specifically used to sink the substrate into the anodic oxidation solution if the substrate surface is detected to be normal;
[0104] The thickness of the oxide layer center and designated points of the substrate is detected by an anodizing thickness gauge to obtain the oxide layer thickness corresponding to each point;
[0105] If the ratio of the oxide layer thicknesses at each point is within a preset standard thickness ratio range, the average oxide layer thickness is calculated based on the oxide layer thicknesses at each point.
[0106] In some embodiments, the substrate dielectric module 230 is specifically used to clean the substrate if the average thickness of the oxide layer is within the standard thickness range, and move the substrate to the withstand voltage analyzer;
[0107] Applying voltage to the substrate oxide layer according to the withstand voltage analyzer until the substrate oxide layer is broken down to obtain a breakdown voltage;
[0108] Detecting the base thickness of the substrate using a three-dimensional laser scanner;
[0109] The dielectric strength of the substrate is calculated based on the substrate thickness, breakdown voltage, and average thickness of the oxide layer;
[0110] If the dielectric strength is within the preset strength range, the dielectric strength of the substrate is determined to be normal; otherwise, the dielectric strength of the substrate is determined to be abnormal.
[0111] In some embodiments, the substrate expansion module 240 is specifically used to detect the coating length of the substrate according to the three-dimensional laser scanner and determine the corresponding initial temperature;
[0112] If the dielectric strength of the substrate is normal, the substrate is heated to a specified temperature, and the length of the high-temperature coating when the substrate is at high temperature is detected;
[0113] Calculates the coefficient of thermal expansion based on the coating length, initial temperature, specified temperature, and elevated temperature coating length.
[0114] In some embodiments, the substrate strength module 250 is specifically used to detect the area of the substrate solder joints to be detected by the three-dimensional laser scanner, and obtain the solder joint areas corresponding to the solder joints one by one;
[0115] If the ratio of the solder joint area of each solder joint to the preset standard area is within the preset standard area ratio range, the solder joint area is judged to be normal.
[0116] In some embodiments, the substrate strength module 250 is specifically used for applying a horizontal shear force to the substrate solder joint position according to the sensor splitter of the push-pull force tester when the thermal expansion coefficient falls within the standard expansion coefficient range until the solder joint is damaged, and obtaining the maximum shear force before the solder joint is damaged;
[0117] If the solder joint area is normal, the maximum shear force corresponding to each solder joint and the solder joint area are divided to obtain the shear strength corresponding to the solder joint;
[0118] If the difference between the shear strength corresponding to each solder joint and the preset standard solder joint strength is within the preset strength difference range, the substrate strength is judged to be normal; otherwise, the substrate strength is judged to be abnormal.
[0119] The embodiment of the present application also discloses a control device.
[0120] Specifically, the control device includes a memory and a processor, and the memory stores a computer program that can be loaded by the processor and execute the above-mentioned intelligent Internet of Things bonding silver wire production equipment substrate detection method.
[0121] The embodiment of the present application also discloses a computer-readable storage medium.
[0122] Specifically, the computer-readable storage medium stores a computer program that can be loaded by a processor and executed such as the above-mentioned intelligent Internet of Things bonding silver wire production equipment substrate detection method. The computer-readable storage medium includes, for example: U disk, mobile hard disk, read-only memory (Read-Only Memory, ROM), random access memory (Random Access Memory, RAM), magnetic disk or optical disk and other media that can store program codes.
[0123] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.
Claims
1. A method for detecting substrates of intelligent Internet of Things bonding silver wire production equipment, characterized in that: include: When it is detected that the substrate moves to the designated position of the detection platform, the three-dimensional point data of the substrate is detected according to the three-dimensional laser scanner, and whether the surface of the substrate is normal is determined according to the three-dimensional point data; If the substrate surface is normal, the substrate is sunk into the anodizing solution and the thickness of the oxide layer of the substrate is measured using an anodizing thickness gauge; If the oxide layer thickness is within the preset standard thickness range, the breakdown voltage of the substrate is detected by the withstand voltage analyzer, and the dielectric strength of the substrate is determined to be normal based on the breakdown voltage; If the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the thermal expansion coefficient of the substrate using a thermal expansion meter; If the thermal expansion coefficient is within the preset standard expansion coefficient range, the solder joint position of the substrate is sheared according to the push-pull force tester to obtain the maximum shear force, and whether the substrate strength is normal is determined according to the maximum shear force.
2. The method according to claim 1, characterized in that: When it is detected that the substrate moves to the designated position of the detection platform, the three-dimensional point data of the substrate is detected according to the three-dimensional laser scanner, and whether the surface of the substrate is normal is determined according to the three-dimensional point data, including: Move the substrate to a designated position of the detection platform, and detect the three-dimensional point data of the substrate using a three-dimensional laser scanner, wherein the three-dimensional point data at least includes three-dimensional point coordinates; Determine the abnormal 3D points with differences according to the preset matching standard, the standard 3D point data and the 3D point data; Determine the number of abnormal three-dimensional points corresponding to each area according to the different colors of the substrate oxide layer, the coating layer, and the base material and the coordinates of the abnormal three-dimensional points; According to the preset number of regional 3D points and the number of abnormal 3D points, the ratio of the number of regional 3D points and the number of abnormal 3D points corresponding to each region is calculated to obtain a difference percentage; If the difference percentage is not greater than the preset standard ratio, the substrate surface is judged to be normal, otherwise, the substrate surface is judged to be abnormal.
3. The method according to claim 1, characterized in that If the substrate surface is detected to be normal, the substrate is sunk into the anodizing solution, and the thickness of the oxide layer of the substrate is detected by an anodizing thickness gauge, including: If the substrate surface is detected to be normal, the substrate is sunk into the anodizing solution; Detecting the thickness of the center and designated points of the oxide layer of the substrate using an anodizing thickness gauge to obtain the oxide layer thickness corresponding to each point; If the ratio of the oxide layer thicknesses at each point is within a preset standard thickness ratio range, the average oxide layer thickness is calculated based on the oxide layer thicknesses at each point.
4. The method according to claim 3, characterized in that If the oxide layer thickness is within the preset standard thickness range, the breakdown voltage of the substrate is detected by a withstand voltage analyzer, and whether the dielectric strength of the substrate is normal is determined according to the breakdown voltage, including: If the average thickness of the oxide layer is within the standard thickness range, the substrate is cleaned and moved to a withstand voltage analyzer; Applying a voltage to the substrate oxide layer according to a withstand voltage analyzer until the substrate oxide layer is broken down, thereby obtaining the breakdown voltage; Detecting the base thickness of the substrate using a three-dimensional laser scanner; Calculating the dielectric strength of the substrate according to the substrate thickness, the breakdown voltage and the average thickness of the oxide layer; If the dielectric strength is within a preset strength range, it is determined that the dielectric strength of the substrate is normal; otherwise, it is determined that the dielectric strength of the substrate is abnormal.
5. The method according to claim 1, characterized in that If the dielectric strength of the substrate is normal, the substrate is heated to a specified temperature, and the thermal expansion coefficient of the substrate is detected using a thermal expansion meter, including: Detect the coating length of the substrate using a three-dimensional laser scanner and determine the corresponding initial temperature; If the dielectric strength of the substrate is normal, heating the substrate to a specified temperature and detecting the length of the high-temperature coating when the substrate is at a high temperature; The thermal expansion coefficient is calculated according to the coating length, the initial temperature, the designated temperature, and the high-temperature coating length.
6. The method according to claim 1, characterized in that If the thermal expansion coefficient is within the preset standard expansion coefficient range, the method further includes shearing the solder joint position of the substrate according to the push-pull force tester to obtain the maximum shear force, and judging whether the strength of the substrate is normal according to the maximum shear force: Detecting the areas of the solder joints of the substrate to be detected by the three-dimensional laser scanner, and obtaining the areas of the solder joints corresponding to the solder joints one by one; If the ratio of the soldering point area of each soldering point to the preset standard area is within the preset standard area ratio range, then it is determined that the soldering point area is normal.
7. The method according to claim 6, characterized in that If the thermal expansion coefficient is within the preset standard expansion coefficient range, shearing the solder joint position of the substrate according to the push-pull force tester to obtain the maximum shear force, and judging whether the strength of the substrate is normal according to the maximum shear force, including: If the thermal expansion coefficient is within the standard expansion coefficient range, a horizontal shear force is applied to the solder joint position of the substrate according to the sensor splitter of the push-pull force tester until the solder joint is damaged, thereby obtaining the maximum shear force before the solder joint is damaged; If the solder joint area is normal, the maximum shear force corresponding to each solder joint and the solder joint area are divided to obtain the shear strength corresponding to the solder joint; If the difference between the shear strength corresponding to each solder joint and the preset standard solder joint strength is within the preset strength difference range, the substrate strength is judged to be normal; otherwise, the substrate strength is judged to be abnormal.
8. A substrate detection device for intelligent Internet of Things bonding silver wire production equipment, characterized in that: The device comprises: A three-dimensional scanning module is used to detect three-dimensional point data of the substrate according to a three-dimensional laser scanner when the substrate is detected to move to a specified position of the detection table, and determine whether the surface of the substrate is normal according to the three-dimensional point data; The substrate oxidation module is used to sink the substrate into the anodic oxidation liquid if the substrate surface is detected to be normal, and detect the thickness of the oxide layer of the substrate according to the anodic oxidation thickness gauge; The substrate dielectric module is used to detect the breakdown voltage of the substrate according to the withstand voltage analyzer if the oxide layer thickness is within the preset standard thickness range, and to determine whether the dielectric strength of the substrate is normal according to the breakdown voltage; A substrate expansion module, used for heating the substrate to a specified temperature if the dielectric strength of the substrate is normal, and detecting the thermal expansion coefficient of the substrate according to a thermal expansion meter; The substrate strength module is used to shear the solder joint position of the substrate according to the push-pull force tester if the thermal expansion coefficient belongs to the preset standard expansion coefficient range, obtain the maximum shear force, and judge whether the substrate strength is normal according to the maximum shear force.
9. A control device, characterized in that: The device comprises: The method comprises a memory and a processor, wherein the memory stores a computer program that can be loaded by the processor and execute the method according to any one of claims 1 to 7.
10. A computer-readable storage medium, characterized in that: A computer program is stored which can be loaded by a processor and execute the method as claimed in any one of claims 1 to 7.