Iron and manganese cooperated coal gangue thermal disintegration weathering treatment method
The iron-manganese synergistic catalysis method is used to treat coal gangue under high temperature and pressure, which solves the problem of slow conversion rate of carbon-based minerals, achieves efficient humification of coal gangue, and promotes comprehensive utilization of resources and soil improvement.
Patent Information
- Application Number
- CN202411120359.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-10-11
AI Technical Summary
Existing technology is difficult to effectively utilize the carbon-based minerals in coal gangue, resulting in resource waste and slow humus conversion rate, limiting its large-scale comprehensive utilization.
The iron-manganese synergistic catalytic method is used to treat coal gangue by adding water to oxygen, high temperature and high pressure, and uses Fe and Mn elements to catalyze the oxidation of carbon-based minerals into humus to improve the reaction rate and humus conversion efficiency.
It achieves the efficient conversion of carbon-based components inside coal gangue into humus, increases the reaction rate, reduces resource waste and environmental pollution, and produces products rich in humus, which can be used to improve soil fertility.
Smart Images

Figure CN118751668A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of solid waste resource utilization, and specifically relates to a method for treating coal gangue by thermal weathering in cooperation with iron and manganese. Background Art
[0002] As a major industrial solid waste, coal gangue is currently mainly treated and disposed of by stockpiling. How to achieve large-scale comprehensive utilization of coal gangue has become a research hotspot. As a by-product of coal, coal gangue contains a small amount of carbon-based minerals that have been ignored and thus not effectively utilized, resulting in a waste of resources.
[0003] At present, most of the treatment and disposal methods for coal gangue are for the preparation of industrial materials, and there are few patents related to the catalytic heat treatment and humification of coal gangue. Patent CN202310556443.8 introduces a method and application of iron ion catalysis to promote the humification of biomass to synthesize artificial humus. This patent is aimed at using Fe to catalyze biomass materials to accelerate the conversion of humus. Compared with biomass materials, coal gangue is significantly different, and it is difficult to achieve rapid conversion of humus in conventional environments. Patent CN202311098786.0 mentions a method for accelerating the humification of carbon-based minerals in coal gangue based on the use of medium and low temperature heat. The reaction rate of the humification of carbon-based minerals in this method is slow, and it is limited by time cost in actual application.
[0004] Therefore, it is very necessary to develop a method for iron-manganese coordinated coal gangue hot weathering treatment that can solve the above problems. Summary of the invention
[0005] In view of the technical problem that the carbon-based components inside coal gangue cannot be effectively utilized, the purpose of the present invention is to provide a method for iron-manganese coordinated thermal weathering treatment of coal gangue, in which the carbon-based components inside the coal gangue are converted into humus by adding water and oxygen, high temperature and high pressure. Fe and Mn elements have good catalytic properties, which can accelerate the oxidation of carbon-based minerals into humus and increase the reaction rate.
[0006] The object of the present invention is achieved by comprising the following steps: S1. Mix the coal gangue, iron-containing substances and manganese-containing substances evenly, and place the mixture in a closed high-temperature resistant reactor; the even mixing ensures that iron and manganese provide catalysis during the oxidation of carbon-based minerals; S2. Add water and introduce oxygen into the reactor to heat it. Under high temperature and high pressure, the minerals inside the coal gangue expand unevenly, the physical structure is damaged and the cracks increase. The coal gangue becomes obviously pulverized and the particle size decreases significantly. Water vapor and oxygen fully contact with the carbon-based minerals in the coal gangue. The carbon-based minerals are humified under the catalysis of iron-containing and manganese-containing substances, and the humification efficiency is high.
[0007] The gangue used is produced in the coal washing process of coking coal, bituminous coal, anthracite, etc. The heating in step S2 can be external heating, and also utilizes the heat released by spontaneous combustion of the gangue.
[0008] Preferably, the iron-containing substance is iron ore and / or soluble iron salt of iron ore, and the iron ore is one or more of magnetite, hematite, ilmenite, pyrite, limonite and siderite.
[0009] Preferably, the manganese-containing substance is manganese ore and / or a soluble manganese salt of manganese ore, and the manganese ore is one or more of pyrolusite, psilomelane, rhodochrosite, manganese calcite, manganese siderite, rhodonite, and manganese sphene.
[0010] Preferably, the mass ratio of coal gangue, iron-containing material and manganese-containing material is 100:0.1~5:0.1~5.
[0011] Preferably, the iron-containing substance, the manganese-containing substance and the coal gangue are mixed simultaneously, or one of the substances is mixed with the coal gangue first, and then the other substance is added and mixed evenly.
[0012] Preferably, the temperature of step S2 is controlled at 90° C. to 400° C., and the reaction time is 0.5 h to 48 h.
[0013] Preferably, the volume mass ratio of oxygen input in step S2 to carbon-based minerals in coal gangue is 16ml~80ml:1g.
[0014] Compared with the prior art, the present invention has the following technical effects: 1. The present invention uses iron and manganese to synergistically treat coal gangue. Iron and manganese can accelerate the electron transfer of each other's catalysts and promote the generation of metal ions. At the same time, the iron-manganese catalyst has double reaction sites and can generate a large number of OH free radicals in the reaction under the interaction, which can effectively promote the catalytic oxidation of high molecular organic matter; 2. The present invention uses hot weathering to treat coal gangue, uses a closed reactor as a container, and provides a high-pressure environment by heating, which can effectively reduce the strength of the coal gangue product and promote structural pulverization; at the same time, by introducing oxygen to control the reaction process, it is avoided that the carbon-based minerals are excessively oxidized to generate a large amount of gaseous products, causing waste of resources and environmental pollution; 3. The method of the present invention is simple and easy to operate, and can fully utilize the carbon-based components inside the coal gangue, so as to convert the coal gangue solid waste into useful resources. The product is rich in humus and can be used to improve soil fertility; 4. The present invention has excellent humification effect on carbon-based components of coal gangue, high reaction rate, and realizes rapid conversion of humus. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic diagram of the process of the present invention. DETAILED DESCRIPTION
[0016] The present invention is further described below in conjunction with the embodiments and drawings, but the present invention is not limited in any way. Any changes or substitutions made based on the teachings of the present invention belong to the protection scope of the present invention.
[0017] Example 1 As attached Figure 1 As shown, the method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Mix gangue, hematite and pyrolusite evenly, wherein the mass ratio of gangue, iron ore and manganese ore is 100:1:1, and the gangue is selected from coking coal associated gangue, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor and heat it. The temperature is controlled at 180°C and the reaction time is 2h. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 16ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, water vapor and oxygen fully contact with the carbon-based minerals in the gangue, and the carbon-based minerals are humified under the catalysis of iron ore and manganese ore. The organic carbon content of the gangue increases from 1.1% to more than 5.6%, the strength of the gangue decreases significantly, and the particle size decreases from 6-10mm to 4-8mm.
[0018] Example 2 The method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Mix gangue, hematite and rhodochrosite evenly, wherein the mass ratio of gangue, iron ore and manganese ore is 100:1:1. Gangue produced in an area mainly producing anthracite is selected, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor for heating. The temperature is controlled at 200°C and the reaction time is 2.5h. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 20ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, water vapor and oxygen fully contact with the carbon-based minerals in the gangue, and the carbon-based minerals are humified under the catalysis of iron ore and manganese ore. The organic carbon content of the gangue is increased from 1.1% to more than 3.0%, the strength of the gangue decreases significantly, and the particle size decreases from 6-10mm to 6-8mm.
[0019] Example 3 The method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Mix gangue, siderite and manganese calcite evenly, the mass ratio of gangue, iron ore and manganese ore is 100:5:5, the gangue is produced in the mining area mainly producing anthracite, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor and heat it. The temperature is controlled at 200°C and the reaction time is 2h. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 20ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, water vapor and oxygen fully contact with the carbon-based minerals in the gangue, and the carbon-based minerals are humified under the catalysis of iron ore and manganese ore. The organic carbon content of the gangue increases from 1.1% to more than 3.2%, the strength of the gangue decreases significantly, and the particle size decreases from 6-10mm to 4-8mm.
[0020] Example 4 The method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Evenly mix gangue, iron ore and manganese ore, wherein the mass ratio of gangue, iron ore and manganese ore is 100:0.1:0.1, wherein the iron ore is obtained by mixing pyrite and magnetite in a mass ratio of 1:1, and the manganese ore is obtained by mixing pyrolusite and rhodonite in a mass ratio of 1:1. The gangue is produced in a mining area mainly producing anthracite, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor and heat it. The temperature is controlled at 90°C and the reaction time is 0.5h. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 16ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, and water vapor and oxygen fully contact with the carbon-based minerals in the gangue. The carbon-based minerals are humified under the catalysis of iron ore and manganese ore.
[0021] Example 5 The method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Evenly mix gangue, iron ore and manganese ore, wherein the mass ratio of gangue, iron ore and manganese ore is 100:5:5, wherein the iron ore is obtained by mixing magnetite and limonite in a mass ratio of 2:1, and the manganese ore is obtained by mixing pyrolusite and psilomelane in a mass ratio of 1:3. The gangue is produced in a mining area mainly producing anthracite, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor and heat it. The temperature is controlled at 400°C and the reaction time is 48h. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 80ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, and water vapor and oxygen fully contact with the carbon-based minerals in the gangue. The carbon-based minerals are humified under the catalysis of iron ore and manganese ore.
[0022] Example 6 The method for treating coal gangue by hot weathering with iron and manganese in this embodiment comprises the following steps: S1. Evenly mix the gangue, iron ore and manganese ore, wherein the mass ratio of the gangue, iron ore and manganese ore is 100:2.5:2.5, wherein the iron ore is obtained by mixing pyrite, ilmenite and siderite in a mass ratio of 3:1:2, and the manganese ore is obtained by mixing pyrolusite, psilomelane and manganese siderite in a mass ratio of 1:1.5:1. The gangue is produced in a mining area mainly producing anthracite, and the mixture is placed in a closed high temperature resistant reactor; S2. Add water and introduce oxygen into the reactor and heat it. The temperature is controlled at 245°C. The reaction time is 24h15min. The volume mass ratio of oxygen input to carbon-based minerals in the gangue is 48ml:1g. Under high temperature and high pressure, the gangue undergoes physical deformation, the cracks increase, and water vapor and oxygen fully contact with the carbon-based minerals in the gangue. The carbon-based minerals are humified under the catalysis of iron ore and manganese ore.
Claims
1. A method for treating coal gangue by hot weathering with iron and manganese, characterized in that The following steps are involved: S1. Mix the coal gangue, iron-containing substances and manganese-containing substances evenly, and place the mixture in a closed high-temperature resistant reactor; S2. Add water and introduce oxygen into the reactor to heat it. Under high temperature and high pressure, the coal gangue undergoes physical deformation, the cracks increase, and the water vapor and oxygen fully contact with the carbon-based minerals in the coal gangue. The carbon-based minerals are humified under the catalysis of iron-containing substances and manganese-containing substances.
2. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The iron-containing substance is iron ore and / or soluble iron salt of iron ore, and the iron ore is one or more of magnetite, hematite, ilmenite, pyrite, limonite and siderite.
3. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The manganese-containing substance is manganese ore and / or soluble manganese salt of manganese ore, and the manganese ore is one or more of pyrolusite, psilomelane, rhodochrosite, manganese calcite, manganese siderite, rhodonite, and manganese sphene.
4. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The mass ratio of coal gangue, iron-containing substances and manganese-containing substances is 100:0.1~5:0.1~5.
5. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The iron-containing substance, the manganese-containing substance and the coal gangue are mixed at the same time, or one of the substances is mixed with the coal gangue first, and then the other substance is added and mixed evenly.
6. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The temperature of step S2 is controlled at 90°C to 400°C, and the reaction time is 0.5h to 48h.
7. The method for treating coal gangue by hot weathering with iron and manganese according to claim 1, characterized in that The volume mass ratio of oxygen input in step S2 to carbon-based minerals in coal gangue is between 16ml and 80ml:1g.
Citation Information
Patent Citations
Process for preparing humic acid from residue after extraction of coal humic acid
CN101289474A
Desulphurization and denitrification agent and preparation method thereof
CN107899596A
Preparation method and application of magnetic nano iron-manganese double metal oxide composite catalyst
CN108404929A
Copper-manganese-doped iron metal organic framework material, preparation method thereof and method for treating organic wastewater by catalytically activating persulfate
CN113351254A
Method for preparing humic acid through microbial decomposition and conversion of coal gangue as well as product and application thereof
CN116200449A
Cited By
High-temperature and high-pressure synergistic treatment method for red mud and coal or coal gangue
CN119368550A