Steel forging processing technology capable of rapidly removing oxide skin
Through the alternating spraying technology of pickling liquid and clean water, the chemical components in the pickling liquid are used to complex with the oxide scale and accelerate its dissolution. Combined with the high-pressure spraying technology, the problem of slow removal speed in the high-pressure water descaling technology is solved and the problem is achieved. Rapid removal of scale and assurance of subsequent rolling quality.
Patent Information
- Application Number
- CN202410964601.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing high-pressure water scale removal technology, clean water does not react with the scale, resulting in a slow removal rate of the scale.
The pickling solution and clean water are sprayed alternately, and the ingredients such as hydrochloric acid, sodium lauryl sulfate, oxalic acid, emulsifier and phosphoric acid in the pickling solution are used to accelerate the oxidation through the complexation of oxalic acid in the pickling solution with Fe2 and Fe3. The scale is dissolved and combined with high-pressure spray technology to quickly remove oxide scale.
The oxide scale removal speed is significantly accelerated, and the oxide scale is completely removed within 18-20 minutes without affecting the effect and quality of subsequent rolling processing.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel forging processing, and in particular to a steel forging processing technology for rapidly removing oxide scale. Background Art
[0002] In the traditional hot rolling production line, the temperature of the red steel billet just out of the furnace can reach above 1260℃. The red steel billet is prone to oxidation under high temperature and oxygen, moisture in the air, etc., and a layer of oxide film, also called scale, is produced on the surface. When the red steel billet is rolled on the rough rolling and finishing mill, the scale is easily pressed directly into the steel billet due to the huge pressure of the rolling mill, thus affecting the surface quality of the steel billet. Therefore, it is very important to remove the scale on the surface of the steel billet. There are many traditional methods for dephosphorization of steel billets, such as ultrasonic dephosphorization, water dephosphorization, mechanical dephosphorization, small steel billets will be pickled, peeled by a peeling machine and treated with a steel brush to remove scale, etc. The use of an ultra-high pressure scale cleaning machine can prevent a large amount of scale from being pressed into the steel billet, and the problems of dullness, black spots and color spots on the surface of the steel billet will also be greatly improved.
[0003] The existing high-pressure water descaling technology mainly forms the water flow into a fan-shaped shape like a sharp blade, thereby peeling off the iron oxide scale and the base material. Clean water does not chemically react with the scale, so the speed of removing the scale with clean water alone is slow. Summary of the invention In view of the shortcomings of the prior art, the purpose of the present invention is to provide a steel forging process for quickly removing oxide scale, which aims to solve the technical problems in the prior art that clean water does not react with oxide scale and the oxide scale removal speed is slow.
[0004] The technical solution of the present invention is: a steel forging process for rapidly removing oxide scale, the steps of which are as follows: Step 1: The coking coal is mixed and crushed and then added to the coke oven, where hot coke and coke oven gas are produced through dry distillation at elevated temperatures; Step 2: Powdered iron ore, various fluxes and coke are mixed according to the required proportions. After crushing, screening, mixing and granulation, the mixture is added to the sintering machine through the distribution system. The coke is ignited by the ignition furnace, and the sintering reaction is completed by exhaust windmills. The waste gas generated by sintering is treated with dust removal, desulfurization and denitrification. Step 3: Iron ore, coke and flux are added into the blast furnace from the top according to the required ratio, and high-temperature hot air is blown into the furnace from the blast nozzle at the bottom of the furnace to provide the heat required for smelting. Carbon in the coke reacts with oxygen in the blown air to generate carbon monoxide and hydrogen. Carbon monoxide and hydrogen remove oxygen in the iron ore during their rise in the furnace, thereby reducing it to obtain pig iron. Molten iron is discharged from the tap hole. Gangue in the iron ore, coke and ash in the blown material combine with flux such as limestone added to the furnace to generate slag, which is discharged from the tap hole and slag hole respectively. Coal gas is discharged from the top of the furnace. Step 4: The molten iron tank is transported to the slag removal position and tipped over. After temperature measurement and sampling, the first slag removal is carried out, desulfurizer is added, and the stirring head rises after stirring and desulfurization. The temperature is measured and sampled again, the molten iron tank is tipped over, the second slag removal is carried out, the molten iron tank returns to its original position, and then the molten iron tank is opened to the hanging tank position and added to the converter. High-pressure and high-speed industrial pure oxygen or air is sprayed on the molten crude metal liquid surface through a spray gun to oxidize impurities into gas and escape. After being blown in the converter, it is sent to the secondary refining treatment station for vacuum degassing, blowing treatment and vacuum oxygen blowing decarburization treatment according to the characteristics and quality requirements of the ordered steel grade to adjust the composition of the molten steel; Step 5: Pour the liquid steel into the continuous casting machine to cast the steel billet, and then keep it warm in the soaking furnace without cooling; Step 6: Prepare the pickling solution, put the pickling solution and clean water into different water tanks respectively, turn on the high-pressure water pump to spray the pickling solution evenly and comprehensively on the surface of the billet, then switch to the clean water mode until all the oxide scale is removed, and then directly enter the hot rolling unit for rolling and forming.
[0005] Preferably, the dry distillation temperature is 900-1000°C.
[0006] Preferably, a layer of small pieces of sintered ore with a particle size of 10 to 25 mm and a thickness of 20 to 25 mm is first laid as a base material before laying the material.
[0007] Preferably, the temperature of the high-temperature hot air is 1000-1300°C, and the coal gas is used as industrial coal gas or for power generation after being dedusted by a bag filter.
[0008] Preferably, the desulfurizing agent is calcium oxide, calcium carbonate or magnesium oxide, the stirring time during desulfurization is 5 to 8 minutes, and the rotation speed is 80 to 100 r / min; the converter adopts top blowing, bottom blowing or top and bottom combined blowing.
[0009] Preferably, the secondary refining treatment station includes an RH vacuum degassing treatment station, a Ladle Injection ladle injection treatment station, a VOD vacuum oxygen decarburization treatment station and an STN mixing station.
[0010] Preferably, the holding time of the steel billet in the soaking furnace is determined according to the chemical composition, effective thickness and process requirements of the steel grade.
[0011] Preferably, the pickling solution is prepared as follows: hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additive and phosphoric acid are mixed and stirred thoroughly, and the mass ratio of hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additive and phosphoric acid is (80-90):2:1:2:2:(10-12).
[0012] Preferably, the working pressure of the high-pressure water pump is 15-18 MPa.
[0013] Beneficial effects of the present invention: 1. Use a combination of pickling liquid and clean water, and alternate operations to enhance the dephosphorization effect. Since the pH value of the pickling liquid is low, phosphorus substances will be more easily extracted. The addition of phosphoric acid in the pickling liquid can increase the pickling speed and remove the oxide scale without affecting the effect and quality of subsequent rolling treatment; 2. Oxalic acid in the pickling solution can complex with Fe2 and Fe3 to accelerate the dissolution of oxide scale. Additives can also complex with Fe2 and Fe3 to significantly accelerate the dissolution of oxide scale. Sodium dodecyl sulfate has a lubricating and penetrating effect. Emulsifiers have a penetrating effect and also have a fog suppressing effect. DETAILED DESCRIPTION
[0014] The present invention will be further described below in conjunction with the embodiments.
[0015] Example 1 The present invention provides an embodiment: a steel forging process for rapidly removing oxide scale, the steps of which are as follows: Step 1: Mix and crush the coking coal and add it into the coke oven. After heating and dry distillation, hot coke and coke oven gas are produced. The dry distillation temperature is 900℃. Step 2: Powdered iron ore, various fluxes and coke are mixed according to the required ratio. After crushing, screening, mixing and granulation, the mixture is added to the sintering machine through the distribution system. Before distribution, a layer of small pieces of sintered ore with a particle size of 10-25mm and a thickness of 20-25mm is first laid as a base material. The coke is ignited by the ignition furnace, and the sintering reaction is completed by exhaust windmill. The waste gas generated by sintering is treated with dust removal, desulfurization and denitrification; Step 3: Add iron ore, coke and flux into the furnace from the top of the blast furnace according to the ratio requirements, and then blow high-temperature hot air from the blast nozzle at the bottom of the furnace. The temperature of the high-temperature hot air is 1000℃, which provides the heat required for smelting. Carbon in the coke reacts with oxygen in the blown air to generate carbon monoxide and hydrogen. Carbon monoxide and hydrogen remove oxygen in the iron ore during the rising process in the furnace, thereby reducing pig iron. Molten iron is discharged from the iron outlet. Gangue in the iron ore, coke and ash in the blown material combine with flux such as limestone added to the furnace to form slag, which is discharged from the iron outlet and slag outlet respectively. Coal gas is extracted from the top of the furnace. After dust removal by a bag filter, the coal gas is used as industrial gas or for power generation; Step 4: The molten iron tank is transported to the slag position and tipped over. After temperature measurement and sampling, the first slag removal is carried out, the desulfurizer is added, the stirring head rises after stirring and desulfurization, the temperature is measured and sampled again, the molten iron tank is tipped over, the second slag removal is carried out, the molten iron tank returns to its position, and then the molten iron tank is opened to the hanging tank position and added into the converter. The desulfurizer is calcium oxide, calcium carbonate or magnesium oxide. The stirring time during desulfurization is 5 minutes, the speed is 100r / min, and the converter adopts top blowing. High-pressure and high-speed industrial pure oxygen is sprayed on the molten crude metal liquid surface through a spray gun to oxidize impurities into gas and escape. After the converter is blown, it is sent to the secondary refining treatment station for vacuum degassing, blowing treatment and vacuum oxygen blowing decarburization treatment according to the characteristics and quality requirements of the ordered steel grade to adjust the composition of the molten steel. The secondary refining treatment station includes RH vacuum degassing treatment station, Ladle Injection ladle blowing treatment station, VOD vacuum oxygen blowing decarburization treatment station and STN mixing station; Step 5: Pour the liquid steel into the continuous casting machine to cast the billet, and then keep it warm in the soaking furnace without cooling. The holding time of the billet in the soaking furnace is determined according to the chemical composition of the steel grade, the effective thickness and the process requirements; Step six: prepare the pickling solution. The preparation method of the pickling solution is as follows: mix hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid and stir them thoroughly. The mass ratio of hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid is 80:2:1:2:2:10. Put the pickling solution and clean water into different water tanks respectively, turn on the high-pressure water pump to spray the pickling solution evenly and comprehensively on the surface of the billet, then switch to the clean water mode until all the oxide scale is removed, and then directly enter the hot rolling mill for rolling and forming. The working pressure of the high-pressure water pump is 15MPa.
[0016] By adopting the process of Example 1, the oxide scale can be completely removed within 18 minutes.
[0017] Example 2 The present invention provides an embodiment: a steel forging process for rapidly removing oxide scale, the steps of which are as follows: Step 1: Mix and crush the coking coal and add it into the coke oven. Then, heat and dry distill it to produce hot coke and coke oven gas. The temperature of dry distillation is 1000℃. Step 2: Powdered iron ore, various fluxes and coke are mixed according to the required ratio. After crushing, screening, mixing and granulation, the mixture is added to the sintering machine through the distribution system. Before distribution, a layer of small pieces of sintered ore with a particle size of 10-25mm and a thickness of 20-25mm is first laid as a base material. The coke is ignited by the ignition furnace, and the sintering reaction is completed by exhaust windmill. The waste gas generated by sintering is treated with dust removal, desulfurization and denitrification; Step 3: Add iron ore, coke and flux into the furnace from the top of the blast furnace according to the ratio requirements, and then blow high-temperature hot air from the blast nozzle at the bottom of the furnace. The temperature of the high-temperature hot air is 1300℃, which provides the heat required for smelting. Carbon in the coke reacts with oxygen in the blown air to generate carbon monoxide and hydrogen. Carbon monoxide and hydrogen remove oxygen in the iron ore during the rising process in the furnace, thereby reducing pig iron. Molten iron is discharged from the iron outlet. Gangue in the iron ore, coke and ash in the blown material combine with flux such as limestone added to the furnace to form slag, which is discharged from the iron outlet and slag outlet respectively. Coal gas is extracted from the top of the furnace. After dust removal by a bag filter, the coal gas is used as industrial gas or for power generation; Step 4: The molten iron tank is transported to the slag position and tipped over. After temperature measurement and sampling, the first slag removal is carried out, the desulfurizer is added, the stirring head rises after stirring and desulfurization, the temperature is measured and sampled again, the molten iron tank is tipped over, the second slag removal is carried out, the molten iron tank returns to its position, and then the molten iron tank is opened to the hanging tank position and added into the converter. The desulfurizer is calcium oxide, calcium carbonate or magnesium oxide. The stirring time during desulfurization is 8 minutes, the speed is 80r / min, and the converter adopts bottom blowing. High-pressure and high-speed air is sprayed on the molten crude metal liquid surface through a spray gun to oxidize impurities into gas and escape. After being blown in the converter, it is sent to the secondary refining treatment station for vacuum degassing, blowing treatment and vacuum oxygen decarburization treatment according to the characteristics and quality requirements of the ordered steel grade to adjust the composition of the molten steel. The secondary refining treatment station includes RH vacuum degassing treatment station, Ladle Injection ladle blowing treatment station, VOD vacuum oxygen decarburization treatment station and STN mixing station; Step 5: Pour the liquid steel into the continuous casting machine to cast the billet, and then keep it warm in the soaking furnace without cooling. The holding time of the billet in the soaking furnace is determined according to the chemical composition of the steel grade, the effective thickness and the process requirements; Step six: prepare the pickling solution. The preparation method of the pickling solution is as follows: mix hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid and stir them thoroughly. The mass ratio of hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid is 90:2:1:2:2:12. Put the pickling solution and clean water into different water tanks respectively, turn on the high-pressure water pump to spray the pickling solution evenly and comprehensively on the surface of the billet, then switch to the clean water mode until all the oxide scale is removed, and then directly enter the hot rolling mill for rolling and forming. The working pressure of the high-pressure water pump is 18MPa.
[0018] By adopting the process of Example 2, the oxide scale can be completely removed within 20 minutes.
[0019] Example 3 The present invention provides an embodiment: a steel forging process for rapidly removing oxide scale, the steps of which are as follows: Step 1: Mix and crush the coking coal and add it into the coke oven. Then, heat and dry distill it to produce hot coke and coke oven gas. The temperature of dry distillation is 1000℃. Step 2: Powdered iron ore, various fluxes and coke are mixed according to the required ratio. After crushing, screening, mixing and granulation, the mixture is added to the sintering machine through the distribution system. Before distribution, a layer of small pieces of sintered ore with a particle size of 10-25mm and a thickness of 20-25mm is first laid as a base material. The coke is ignited by the ignition furnace, and the sintering reaction is completed by exhaust windmill. The waste gas generated by sintering is treated with dust removal, desulfurization and denitrification; Step 3: Add iron ore, coke and flux into the furnace from the top of the blast furnace according to the ratio requirements, and then blow high-temperature hot air from the blast nozzle at the bottom of the furnace. The temperature of the high-temperature hot air is 1200℃, which provides the heat required for smelting. Carbon in the coke reacts with oxygen in the blown air to generate carbon monoxide and hydrogen. Carbon monoxide and hydrogen remove oxygen in the iron ore during the rising process in the furnace, thereby reducing pig iron. Molten iron is discharged from the iron outlet. Gangue in the iron ore, coke and ash in the injection are combined with flux such as limestone added to the furnace to form slag, which is discharged from the iron outlet and slag outlet respectively. Coal gas is extracted from the top of the furnace. After dust removal by a bag filter, the coal gas is used as industrial gas or for power generation; Step 4: The molten iron tank is transported to the slag position and tipped over. After temperature measurement and sampling, the first slag removal is carried out, the desulfurizer is added, the stirring head rises after stirring and desulfurization, the temperature is measured and sampled again, the molten iron tank is tipped over, the second slag removal is carried out, the molten iron tank returns to its position, and then the molten iron tank is opened to the hanging tank position and added into the converter. The desulfurizer is calcium oxide, calcium carbonate or magnesium oxide. The stirring time during desulfurization is 6 minutes, the speed is 90r / min, and the converter adopts top and bottom composite blowing. High-pressure and high-speed industrial pure oxygen is sprayed on the molten crude metal liquid surface through a spray gun to oxidize impurities into gas and escape. After the converter is blown, it is sent to the secondary refining treatment station for vacuum degassing, blowing treatment and vacuum oxygen blowing decarburization treatment according to the characteristics and quality requirements of the ordered steel grade to adjust the composition of the molten steel. The secondary refining treatment station includes RH vacuum degassing treatment station, Ladle Injection ladle blowing treatment station, VOD vacuum oxygen blowing decarburization treatment station and STN mixing station; Step 5: Pour the liquid steel into the continuous casting machine to cast the billet, and then keep it warm in the soaking furnace without cooling. The holding time of the billet in the soaking furnace is determined according to the chemical composition of the steel grade, the effective thickness and the process requirements; Step six: prepare the pickling solution. The preparation method of the pickling solution is as follows: mix hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid and stir them thoroughly. The mass ratio of hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additives and phosphoric acid is 84:2:1:2:2:10. Put the pickling solution and clean water into different water tanks respectively, turn on the high-pressure water pump to spray the pickling solution evenly and comprehensively on the surface of the billet, and then switch to the clean water mode until all the oxide scales are removed, and then directly enter the hot rolling mill for rolling and forming. The working pressure of the high-pressure water pump is 15-18MPa.
[0020] By adopting the process of Example 3, the oxide scale can be completely removed within 16 minutes.
[0021] The embodiments of the present invention are described in detail above, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of those skilled in the art without departing from the spirit of the present invention.
Claims
1. A steel forging process for rapidly removing oxide scale; characterized in that: The steps are as follows: Step 1: The coking coal is mixed and crushed and then added to the coke oven, where hot coke and coke oven gas are produced through dry distillation at elevated temperatures; Step 2: Powdered iron ore, various fluxes and coke are mixed according to the required proportions. After crushing, screening, mixing and granulation, the mixture is added to the sintering machine through the distribution system. The coke is ignited by the ignition furnace, and the sintering reaction is completed by exhaust windmills. The waste gas generated by sintering is treated with dust removal, desulfurization and denitrification. Step 3: Iron ore, coke and flux are added into the blast furnace from the top according to the required ratio, and high-temperature hot air is blown into the furnace from the blast nozzle at the bottom of the furnace to provide the heat required for smelting. Carbon in the coke reacts with oxygen in the blown air to generate carbon monoxide and hydrogen. Carbon monoxide and hydrogen remove oxygen in the iron ore during their rise in the furnace, thereby reducing it to obtain pig iron. Molten iron is discharged from the tap hole. Gangue in the iron ore, coke and ash in the blown material combine with flux such as limestone added to the furnace to generate slag, which is discharged from the tap hole and slag hole respectively. Coal gas is discharged from the top of the furnace. Step 4: The molten iron tank is transported to the slag removal position and tipped over. After temperature measurement and sampling, the first slag removal is carried out, desulfurizer is added, and the stirring head rises after stirring and desulfurization. The temperature is measured and sampled again, the molten iron tank is tipped over, the second slag removal is carried out, the molten iron tank returns to its original position, and then the molten iron tank is opened to the hanging tank position and added to the converter. High-pressure and high-speed industrial pure oxygen or air is sprayed on the molten crude metal liquid surface through a spray gun to oxidize impurities into gas and escape. After being blown in the converter, it is sent to the secondary refining treatment station for vacuum degassing, blowing treatment and vacuum oxygen blowing decarburization treatment according to the characteristics and quality requirements of the ordered steel grade to adjust the composition of the molten steel; Step 5: Pour the liquid steel into the continuous casting machine to cast the steel billet, and then keep it warm in the soaking furnace without cooling; Step 6: Prepare the pickling solution, put the pickling solution and clean water into different water tanks respectively, turn on the high-pressure water pump to spray the pickling solution evenly and comprehensively on the surface of the billet, then switch to the clean water mode until all the oxide scale is removed, and then directly enter the hot rolling unit for rolling and forming.
2. A steel forging process for rapid descaling according to claim 1, characterized in that: The temperature of carbonization is 900-1000°C.
3. The steel forging process for rapid descaling according to claim 1, characterized in that: Before laying the material, a layer of small pieces of sintered ore with a particle size of 10 to 25 mm and a thickness of 20 to 25 mm is laid as the base material.
4. The steel forging process for rapid descaling according to claim 1, characterized in that: The temperature of the high-temperature hot air is 1000-1300℃. After the gas is dedusted by a bag filter, it can be used as industrial gas or for power generation.
5. The steel forging process for rapid descaling according to claim 1, characterized in that: The desulfurizer is calcium oxide, calcium carbonate or magnesium oxide. The stirring time during desulfurization is 5 to 8 minutes, and the rotation speed is 80 to 100 r / min. The converter adopts top blowing, bottom blowing or top and bottom combined blowing.
6. The steel forging process for rapid descaling according to claim 1, characterized in that: The secondary refining treatment station includes RH vacuum degassing treatment station, Ladle Injection ladle injection treatment station, VOD vacuum oxygen decarburization treatment station and STN mixing station.
7. The steel forging process for rapid descaling according to claim 1, characterized in that: The holding time of the steel billet in the soaking furnace is determined according to the chemical composition of the steel grade, effective thickness and process requirements.
8. The steel forging process for rapid descaling according to claim 1, characterized in that: The preparation method of the pickling solution is as follows: mix hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additive and phosphoric acid and stir them evenly. The mass ratio of hydrochloric acid, sodium dodecyl sulfate, oxalic acid, emulsifier, additive and phosphoric acid is (80-90):2:1:2:2:(10-12).
9. The steel forging process for rapid descaling according to claim 1, characterized in that: The working pressure of the high-pressure water pump is 15~18MPa.
Citation Information
Patent Citations
Additive for pickling scales on surface of stainless steel material as well as preparation of additive and pickling method
CN104195580A
High-strength special steel material and preparation process thereof
CN108893685A
Pickling coil preparation technology
CN109695038A
High-strength H-shaped steel for prefabricated buildings and production technology of high-strength H-shaped steel
CN112593152A
Groove type pickling process for 022Cr11Ti ferritic stainless steel hot-rolled coiled and cut plate
CN115369409A