Breakout judgment processing method
By obtaining the surface condition of the billet in real time at the mold outlet and judging the dent parameters, the drawing speed is automatically adjusted, which solves the problems of high cost and inaccurate prediction of the existing steel breakout prediction system, and achieves more efficient and safe steel breakout monitoring and Production adjustments.
Patent Information
- Application Number
- CN202410900912.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-10-15
AI Technical Summary
The existing steel breakage prediction system is costly and inaccurate, resulting in high false alarm and false alarm rates, affecting production efficiency and safety. Especially in slab production, there is a large amount of waste.
By setting a probe at the exit of the mold, the state of the surface of the billet is obtained in real time, and the dent parameters (depth, length and frequency) are extracted to determine whether there is a steel breakout, and the drawing speed is automatically adjusted based on the judgment results to reduce the dents on the surface of the billet and the generation of scrap. .
It achieves timely monitoring of steel leakage, reduces scrap generation, improves product quality and efficiency, and avoids losses caused by rapid changes in production. It is more economical and safer than directly returning to zero pulling speed.
Smart Images

Figure CN118768535A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of steel leakage during billet drawing, and more specifically, relates to a steel leakage determination and processing method. Background Art
[0002] Steel leakage accident is a very harmful production accident in continuous casting production. The occurrence of steel leakage accident will form depressions on the surface of the billet (such as Figure 1 ), which not only affects the continuous casting production, seriously damages the crystallizer and roller table, increases the maintenance workload and maintenance cost of the continuous casting equipment, causes huge economic losses, but also brings huge safety hazards.
[0003] In order to reduce the occurrence of steel leakage, people have been committed to developing a steel leakage prediction system, which effectively reduces the steel leakage rate by installing sensors on the crystallizer and using an automated control system. The most widely used and effective method for predicting bonding steel leakage is to embed thermocouples in the copper plate of the crystallizer to monitor the copper plate thermally. The principle of steel leakage prediction based on temperature detection is: since steel leakage is accompanied by changes in the temperature of the copper plate of the crystallizer, by monitoring the temperature changes of the thermocouples installed on the copper plate, steel leakage judgment is made based on steel leakage characteristic data analysis or fuzzy reasoning of expert systems, big data analysis and other methods.
[0004] The existing steel leakage prediction is based on the temperature change of the thermocouple buried in the copper plate of the crystallizer to analyze the steel leakage. The installation and maintenance costs of the thermocouple are relatively high, especially the later maintenance. Once the maintenance is not in place, the false alarm rate and missed alarm rate of the steel leakage prediction will increase dramatically, thereby affecting the effect of the steel leakage prediction and causing a large amount of waste. In addition, the existing steel leakage prediction does not focus on the historical process of steel casting and the changes in process parameters, but only focuses on the temperature characteristics of the copper plate in a very short period of time. At the same time, although there is also a demand for steel leakage in square billets, due to the small harm of steel leakage and the high maintenance cost of thermocouples, it is generally not used. Therefore, the existing steel leakage prediction is generally only used on slabs. Summary of the invention
[0005] The purpose of the present invention is to provide a method for determining and processing steel leakage in view of the shortcomings of the prior art, so as to solve the problems of high cost of existing steel leakage monitoring and inaccurate prediction that easily causes a large amount of waste.
[0006] In order to achieve the above object, the present invention provides a method for determining and processing steel leakage, comprising:
[0007] S1: Obtain the surface state of the billet at the exit of the crystallizer to confirm whether there is a depression;
[0008] S2: extract the depression parameters and determine whether there is steel leakage according to the depression parameters;
[0009] S3: If steel leakage is determined, the real-time pulling speed of the crystallizer is reduced, and S1-S2 are repeated.
[0010] Optionally, obtaining the surface state of the blank at the crystallizer outlet includes:
[0011] The probe is arranged at the outlet of the crystallizer, and the probe continuously uploads the surface state parameters of the blank to the processor.
[0012] Optionally, extracting the depression parameters and determining whether steel leakage occurs according to the depression parameters comprises:
[0013] determining at least one of a depth, a length, and a frequency of the depressions;
[0014] If the depth of the depression is greater than the first depth and the duration is greater than the first length, it is determined that the steel is leaking;
[0015] If the concave length is greater than the second length, it is determined that the steel is leaking;
[0016] If the frequency of occurrence of the depression is greater than the first frequency, it is determined that steel leakage occurs.
[0017] Optionally, the depression frequency is the percentage ratio of the total length of the depression within the length L along the axial direction of the billet drawing to L.
[0018] Optionally, the first depth is 3-6 mm.
[0019] Optionally, the second length is 1-20m.
[0020] Optionally, the first length is 0.01-10m.
[0021] Optionally, the first frequency is 20% to 100%.
[0022] Optionally, reducing the pulling speed of the crystallizer includes:
[0023] Reduce speed by △V, △V=0.2m / min.
[0024] Optionally, it also includes:
[0025] If the speed is lower than the preset speed after multiple speed reductions, an alarm and / or shutdown will occur.
[0026] The present invention provides a method for determining and processing steel leakage, which has the following beneficial effects:
[0027] This method can monitor whether leakage occurs in time by directly obtaining the surface state of the billet at the exit of the crystallizer. Compared with finished product detection, it is more timely and reduces the generation of waste. At the same time, the drawing speed is automatically adjusted according to the judgment result to reduce the generation of billet depression, so that the subsequent billet can be automatically adjusted to qualified, thereby improving product quality and efficiency and reducing the generation of waste and inferior products. At the same time, repeated step deceleration is more economical and safer than directly returning the drawing speed to zero. Directly returning the drawing speed to zero will cause a sharp change in the production process, and a large section of the billet will inevitably be scrapped, resulting in a decline in production and quality. Gradual deceleration can adapt to the automatic adjustment of the drawing speed, avoid the influence of distance changes, and minimize the impact on production.
[0028] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present invention, but do not constitute a limitation of the present invention. The above and other purposes, features and advantages of the present invention will become more apparent by describing the exemplary embodiments of the present invention in more detail in conjunction with the accompanying drawings, wherein the same reference numerals generally represent the same components in the exemplary embodiments of the present invention.
[0030] Figure 1 A schematic diagram showing the steel breakout depression during casting is shown.
[0031] Figure 2 The figure shows a schematic flow chart of the method for determining and processing steel leakage provided by the present invention. DETAILED DESCRIPTION
[0032] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to make the present invention more thorough and complete, and to fully convey the scope of the present invention to those skilled in the art.
[0033] like Figure 1 As shown, a method for determining and processing steel leakage includes:
[0034] S1: Obtain the surface state of the billet at the exit of the crystallizer to confirm whether there is a depression;
[0035] S2: extract the depression parameters and determine whether there is steel leakage according to the depression parameters;
[0036] S3: If steel leakage is determined, the real-time pulling speed of the crystallizer is reduced, and S1-S2 are repeated.
[0037] Specifically, by obtaining the surface state of the billet in time at the exit of the crystallizer, it is possible to monitor whether leakage occurs in time, which is more timely than finished product detection and reduces the generation of waste. At the same time, the drawing speed is automatically adjusted according to the judgment result to reduce the generation of billet depression, so that the subsequent billet can be automatically adjusted to qualified, thereby improving product quality and efficiency and reducing the generation of waste and inferior products. At the same time, repeated step deceleration is more economical and safer than directly returning the drawing speed to zero. Directly returning the drawing speed to zero will cause a sharp change in the production process, and a large section of the billet will inevitably be scrapped, resulting in a decline in production and quality. Gradual deceleration can adapt to the automatic adjustment of the drawing speed, avoid the impact of distance changes, and minimize the impact on production.
[0038] Furthermore, the method uses depression as an example for judgment. If there is a bulge, the parameter value can be adaptively adjusted or an alarm or shutdown can be directly issued.
[0039] In this embodiment, obtaining the surface state of the blank at the crystallizer outlet includes:
[0040] The probe is arranged at the outlet of the crystallizer, and the probe continuously uploads the surface state parameters of the billet to the processor.
[0041] Specifically, the throwing state parameters are acquired in real time through the probe and uploaded to the processor for display and / or further artificial intelligence judgment.
[0042] Furthermore, the probe can shoot video recordings, and the length of the billet can be calculated in combination with the drawing speed information, and then the video of any period of time can be intercepted and matched with the corresponding length of the billet. At the same time, one probe corresponds to one side, and multiple probes can correspond to multiple sides and be used simultaneously.
[0043] In this embodiment, extracting the depression parameters and determining whether steel leakage occurs according to the depression parameters includes:
[0044] determining at least one of a depth, a length, and a frequency of the depressions;
[0045] If the depth of the depression is greater than the first depth and the duration is greater than the first length, it is determined that the steel is leaking;
[0046] If the concave length is greater than the second length, it is determined that the steel is leaking;
[0047] If the frequency of occurrence of the depression is greater than the first frequency, it is determined that steel leakage occurs.
[0048] Specifically, whether there is steel leakage is judged according to at least one of the depth, length and frequency of the depression. If at least one of them meets the judgment criteria, there is steel leakage. This method can be used to solve steel leakage problems caused by different reasons and forms. At the same time, the frequency parameter is added to make the judgment more accurate and effective, avoiding the problem of failing the casting when there are multiple longer cracks that are shorter than the second length or the first length.
[0049] Furthermore, specific parameters are determined according to the specifications and uses of the casting.
[0050] In this embodiment, the depression frequency is the percentage ratio of the total length of the depression within the length L along the axial direction of the billet drawing to L.
[0051] Specifically, the calculation method adds up the total lengths of the depressions within a certain length and then confirms whether there is steel leakage based on the total length. This is more accurate and effective than simply calculating the number of depressions within a fixed length.
[0052] Furthermore, simply calculating the number of depressions within a fixed length is easily affected by multiple small and dense cracks that can be removed, and the value range of L is 1m to 20m.
[0053] In this embodiment, the first depth is 3-6 mm.
[0054] In this embodiment, the second length is 1-20m.
[0055] In this embodiment, the first length is 0.01-10 m.
[0056] In this embodiment, the first frequency is 20% to 100%.
[0057] In this embodiment, reducing the pulling speed of the crystallizer includes:
[0058] Reduce speed by △V, △V=0.2m / min.
[0059] Specifically, the speed reduction difference is consistent each time, and the average speed reduction is convenient for ensuring quality while producing efficiently.
[0060] In this embodiment, it also includes:
[0061] If the speed is lower than the preset speed after multiple speed reductions, an alarm and / or shutdown will occur.
[0062] Specifically, the preset pulling speed is the pulling speed of the water exchange port, and if it is too low, an alarm will be issued and the machine will be shut down.
[0063] In this embodiment, a method for determining and processing steel leakage is used, taking a small slab as an example:
[0064] Since small slabs are more sensitive to dents, the first depth of steel leakage is 5mm. If this value is small, steel leakage alarms are likely to occur frequently; the second length is 5m; the frequency of dent warning on long slabs with L=10m is 50%. The normal production speed of the casting machine is 1.5-1.8m / min, and the speed is 0.8m / min during normal water change.
[0065] When steel leakage is judged to occur, the casting speed is reduced in steps; first, the current production casting speed is reduced by 0.2m / min, and the sinking is observed to see whether steel leakage is still judged. If it is no longer judged to be steel leakage, production can be carried out at this casting speed. If it is still judged to be steel leakage, it is further reduced by 0.2m / min until the casting speed is reduced to 0.8m / min at the water exchange port. If it is still judged to be steel leakage, the alarm is stopped.
[0066] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments.
Claims
1. A method for determining and processing steel leakage, characterized in that: include: S1: Obtain the surface state of the billet at the exit of the crystallizer to confirm whether there is a depression; S2: extract the depression parameters and determine whether there is steel leakage according to the depression parameters; S3: If steel leakage is determined, the real-time pulling speed of the crystallizer is reduced, and S1-S2 are repeated.
2. The method for determining steel leakage according to claim 1, characterized in that: The obtaining of the casting surface state at the crystallizer outlet comprises: The probe is arranged at the outlet of the crystallizer, and the probe continuously uploads the surface state parameters of the blank to the processor.
3. The method for determining steel leakage according to claim 1, characterized in that: The extracting of the depression parameters and determining whether the steel is leaking according to the depression parameters include: determining at least one of a depth, a length, and a frequency of the depressions; If the depth of the depression is greater than the first depth and the duration is greater than the first length, it is determined that the steel is leaking; If the concave length is greater than the second length, it is determined that the steel is leaking; If the frequency of occurrence of the depression is greater than the first frequency, it is determined that steel leakage occurs.
4. The method for determining steel leakage according to claim 3, characterized in that: The depression frequency is the percentage ratio of the total length of the depression to L within the length L along the axial direction of the billet.
5. The method for determining steel leakage according to claim 3, characterized in that: The first depth is 3-6 mm.
6. The method for determining steel leakage according to claim 3, characterized in that: The second length is 1-20m.
7. The method for determining steel leakage according to claim 3, characterized in that: The first length is 0.01-10m.
8. The method for determining steel leakage according to claim 4, characterized in that: The first frequency is 20% to 100%.
9. The method for determining steel leakage according to claim 1, characterized in that: The method of reducing the pulling speed of the crystallizer comprises: Reduce speed by △V, △V=0.2m / min.
10. The method for determining steel leakage according to claim 1, characterized in that: Also includes: If the speed is lower than the preset speed after multiple speed reductions, an alarm and / or shutdown will occur.