Non-metal flexible composite pipe connecting structure and connecting method
By welding the non-metallic flexible composite pipe and the electrofusion sleeve into one body, and using the welding surface and annular reinforcement, the problem of sealing and load-bearing capacity of the joints in the non-metallic flexible composite pipe connection structure is solved, and effective sealing and axial The even distribution of load improves the carrying capacity.
Patent Information
- Application Number
- CN202411178110.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-10-15
AI Technical Summary
Existing non-metallic flexible composite pipe connection structures have problems such as ineffective sealing at the joints, stress concentration, and poor load-bearing capacity.
By welding the non-metallic flexible composite pipe and the electrofusion sleeve into one body, and utilizing the welding surface, annular reinforcement and resistance wire of the electrofusion sleeve, the effective sealing of the non-metallic flexible composite pipe and the uniform distribution of axial load are achieved, which avoids The stress is concentrated and the axial load-bearing capacity is increased.
It achieves effective sealing of the non-metallic flexible composite pipe connection structure, avoids the phenomenon of fluid intrusion, evenly distributes the axial load, improves the axial load-bearing capacity of the joint, and solves the problem of stress concentration.
Smart Images

Figure CN118775657A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of composite pipe connection, and in particular to a non-metallic flexible composite pipe connection structure and a connection method. Background Art
[0002] Non-metallic flexible composite pipes usually consist of a three-layer structure, the inner side of which is usually a lining layer made of thermoplastic plastic, usually made of polyethylene, the middle is a reinforcement layer made of continuous fiber, usually made of polyester fiber, and the outer layer is a protective layer of thermoplastic plastic, usually made of polyethylene. Non-metallic flexible composite pipes combine the high strength of fiber with the flexibility and corrosion resistance of polyethylene, and have the advantages of high pressure bearing capacity, large single continuous length, and flexible pipe body for easy construction, so they are widely used in the oil and gas field.
[0003] At present, non-metallic flexible composite pipes generally use metal crimping joints (SY / T 6662.2-2020). The metal crimping joints are used to realize the mechanical connection of two non-metallic flexible composite pipes by fastening the inner lining layer and the outer protective layer. Since the non-metallic flexible composite pipe body at the crimping position is deformed, it is easy to cause stress concentration at the connection joint of the non-metallic flexible composite pipe; and since the end face of the non-metallic flexible composite pipe body is not effectively sealed, there is a hidden danger of fluid entering the pipe body from the crimping surface in the later stage; in addition, ordinary carbon steel requires anti-corrosion treatment, while stainless steel joints have the disadvantages of high cost, low strength and easy damage; metal joints are heavy and inconvenient to use and install, and are especially not suitable for non-metallic flexible composite pipes with large diameters.
[0004] For low-pressure non-metallic flexible composite pipes, the prior art usually uses electric fusion sleeve joints to connect non-metallic flexible composite pipes, but conventional electric fusion sleeve joints completely rely on the fusion surface of the outer protective layer to achieve force conduction. Since the mechanical bearing capacity of pure polyethylene materials is poor, it does not meet the requirements of high-pressure non-metallic flexible composite pipes; for example, the Chinese invention patent with application publication number CN116412307A discloses a RTP pipe connection structure and connection method based on Z-pin implantation. The patent uses the method of implanting Z-pins to improve the connection strength of large-diameter non-metallic flexible composite pipes, but its joint structure is complex, and the implanted Z-pin extends into the continuous fiber reinforced structural layer, which will destroy the structural integrity of the reinforcement layer, and the implantation hole of each Z-pin will destroy the structural integrity of the outer protective layer. Therefore, the prior art non-metallic flexible composite pipe connection structure has the disadvantage that the joint cannot be effectively sealed, and the stress concentration at the joint of the non-metallic flexible composite pipe connection structure is poor in bearing capacity. Summary of the invention
[0005] The present invention aims to solve the problems of ineffective sealing, stress concentration and poor bearing capacity at the joints of the existing non-metallic flexible composite pipe connection structure, and provides a non-metallic flexible composite pipe connection structure and a connection method. By welding the non-metallic flexible composite pipe and the capacitor sleeve into one, the non-metallic flexible composite pipe connection structure can be effectively sealed; and the axial load of the non-metallic flexible composite pipe can be effectively transmitted and evenly distributed at the connection, thereby avoiding the phenomenon of stress concentration. At the same time, the axial deformation at the joint of the non-metallic flexible composite pipe connection structure is limited, thereby improving the axial bearing capacity.
[0006] In order to achieve the above-mentioned purpose, the technical solution of the present invention is: a non-metallic flexible composite pipe connection structure, including an electric fusion sleeve and two non-metallic flexible composite pipes, the electric fusion sleeve is sleeved on the connection ends of the two non-metallic flexible composite pipes, the non-metallic flexible composite pipe includes an inner lining layer, a reinforcement layer and an outer protective layer arranged in sequence from the inside to the outside, and the connection end of the non-metallic flexible composite pipe is a stepped structure. By fusing two non-metallic meat-flavored composite pipes with an electric fusion sleeve, the effect of effectively sealing the non-metallic flexible connection structure is achieved, and the purpose of the step-shaped connection end of the non-metallic flexible composite pipe is to facilitate fusing with the electric fusion sleeve.
[0007] The inner side wall of the electric fusion sleeve is provided with a welding surface, the inner body of the electric fusion sleeve is inlaid with an annular reinforcement body, and the body of the electric fusion sleeve is spirally wound with a resistance wire; the inner lining layer, the reinforcement layer and the outer protective layer are respectively welded to the electric fusion sleeve through the welding surface. The welding surface facilitates the welding of the electric fusion sleeve with the inner lining layer, the reinforcement layer and the outer protective layer of the non-metallic flexible composite pipe, improves the effect of welding the non-metallic flexible composite pipe with the electric fusion sleeve, and the resistance wire is energized to heat the resistance wire, so that the body of the electric fusion sleeve is melted, expanded and fused, so as to achieve the effect of welding the electric fusion sleeve with the non-metallic flexible composite pipe; the annular reinforcement body ensures the bearing capacity of the connection structure of the non-metallic flexible composite pipe, and also limits the axial deformation at the joint, thereby improving the axial bearing capacity.
[0008] Furthermore, the length of the inner lining layer is greater than that of the reinforcement layer, a lining welding surface is provided at the connecting end of the inner lining layer, the length of the reinforcement layer is greater than that of the outer protective layer, and both the inner lining layer and the outer protective layer are made of thermoplastic plastic material through an extrusion process. The inner lining welding surface cooperates with the welding surface in the electric fusion sleeve to facilitate the welding of the inner lining layer and the electric fusion sleeve, and improve the welding effect of the inner lining layer and the capacitor sleeve.
[0009] Furthermore, the connection end of the reinforcement layer is in a stepped structure, the reinforcement layer includes a plurality of reinforcement single layers, the length of the plurality of reinforcement single layers gradually shortens from the inside to the outside, and the connection end of each reinforcement single layer is provided with a reinforcement welding surface; the winding angle and thickness of two adjacent reinforcement single layers are the same, the winding directions of two adjacent reinforcement single layers are opposite, and the two adjacent reinforcement single layers are hot-melt connected. The reinforcement welding surface of the reinforcement single layer connection end cooperates with the welding surface in the electric fusion sleeve to facilitate the welding of the reinforcement layer and the electric fusion sleeve, and improve the effect of welding the reinforcement layer and the capacitor sleeve.
[0010] Furthermore, the reinforcing single layer includes a reinforcing fiber layer and a plastic film arranged on the upper and lower sides of the reinforcing fiber layer, the reinforcing fiber layer is made of inorganic fiber or organic fiber, and two adjacent reinforcing single layers are welded together by a plastic film, and the plastic film is also made of thermoplastic plastic material; the outermost reinforcing single layer is welded to the outer protective layer, and the innermost reinforcing single layer is welded to the inner lining layer. The plastic mold is used to achieve the effect of mutual welding of two adjacent reinforcing single layers, so that the reinforcing layer is formed by multiple reinforcing single layers, and it is also convenient for the reinforcing layer to be welded to the electric melting sleeve.
[0011] Furthermore, the electric fusion sleeve is made of thermoplastic plastic material through an injection molding process, and the welding surfaces include a first welding surface, a second welding surface and a third welding surface. The inner side wall of the electric fusion sleeve is symmetrically provided with two of the first welding surfaces and the second welding surfaces, and the third welding surface is located between the two second welding surfaces. The first welding surface matches the outer protective layer, the second welding surface matches the reinforced welding surface, and the third welding surface matches the lining welding surface. The purpose is to facilitate the welding of the inner lining layer, the reinforced layer and the outer protective layer of the non-metallic flexible composite pipe with the electric fusion sleeve.
[0012] Furthermore, the annular reinforcement body includes a plurality of reinforcement body layers stacked in sequence, the lengths of the plurality of reinforcement body layers gradually increase from the inside to the outside; two adjacent reinforcement body layers are fused to each other, and the reinforcement body layers are fused to the barrel of the electric melting sleeve. The annular reinforcement body is formed by a plurality of reinforcement body layers, and the annular reinforcement body improves the axial bearing capacity of the joint of the non-metallic flexible composite pipe connection structure.
[0013] Furthermore, two terminals are symmetrically arranged on the outer side of the electric fusion sleeve, and the two ends of the resistance wire are respectively connected to the two terminals. The terminals can be connected to an electric fusion welding machine to supply power to the resistance wire through the terminals, so that the resistance wire heats up and melts the electric fusion sleeve.
[0014] A connection method based on a non-metallic flexible composite pipe connection structure includes the following steps: Step 1: Insert the two non-metallic flexible composite pipes to be connected into the electric fusion sleeve respectively, so that the outer protective layer of the non-metallic flexible composite pipe matches the first welding surface, the reinforced welding surface of the reinforcing layer matches the second welding surface, and the lining welding surface matches the third welding surface, and connect the two terminal blocks to the electric fusion welding machine.
[0015] Step 2: Check whether the non-metallic flexible composite pipe is inserted tightly, whether the two non-metallic flexible composite pipes are coaxial, and whether the ends of the inner lining layers of the two non-metallic flexible composite pipes are in contact. After checking that everything is correct, power on the electric fusion welding machine.
[0016] Step 3: The resistance wire generates heat to melt, expand and fuse the electrofusion sleeve body in the first welding surface, the second welding surface and the third welding surface area.
[0017] Step 4: After the electric fusion sleeve is fused with the inner lining layer, reinforcement layer and outer protective layer of the non-metallic flexible composite pipe, the electric fusion welding machine is powered off and the electric fusion welding is completed.
[0018] Step 5: After the electric fusion sleeve and the non-metallic flexible composite pipe have been cooled, the connection of the two non-metallic flexible composite pipes is completed.
[0019] Furthermore, in step 4, the electric fusion sleeve, inner lining layer, plastic film and outer protective layer are all made of thermoplastic plastic materials. After the electric fusion welding is completed, the inner lining layer, reinforcement layer and outer protective layer of the non-metallic flexible composite pipe are welded into one with the electric fusion sleeve.
[0020] Through the above technical solution, the beneficial effects of the present invention are: 1. The non-metallic flexible composite pipe connection structure of the present invention has a reasonable structure and good use effect. The non-metallic flexible composite pipe and the capacitor sleeve are welded together by electric fusion, which can effectively seal the non-metallic flexible composite pipe connection structure to prevent the fluid from entering the non-metallic flexible composite pipe. At the same time, the axial load of the non-metallic flexible composite pipe can be effectively transmitted and evenly distributed at the connection, avoiding stress concentration. At the same time, the axial deformation of the non-metallic flexible composite pipe connection structure joint is limited, thereby improving the axial bearing capacity.
[0021] 2. The present invention achieves the effect of effectively sealing the non-metallic flexible composite pipe connection structure by matching the outer protective layer of the non-metallic flexible composite pipe with the first welding surface, matching the reinforced welding surface of the reinforcing layer with the second welding surface, and matching the lining welding surface with the third welding surface, so as to respectively fuse the inner lining layer, the reinforcing layer and the outer protective layer of the non-metallic flexible composite pipe with the electric fusion sleeve.
[0022] 3. The present invention strengthens the welding surface of the single-layer connection end so that the single-layer reinforcement of the reinforcement layer is respectively welded to the electric fusion sleeve, so that the axial load of the non-metallic flexible composite pipe can be effectively transmitted and evenly distributed at the joint, thereby achieving the effect of avoiding stress concentration.
[0023] 4. The present invention uses the annular reinforcement in the body of the electric fusion sleeve to ensure the pressure bearing capacity of the joint of the non-metallic flexible composite pipe connection structure, while limiting the axial deformation at the joint, thereby improving its axial bearing capacity.
[0024] 5. The non-metallic flexible composite pipe and the electric fusion sleeve of the present invention are both made of non-metallic materials, thereby solving the corrosion problem of existing carbon steel joints. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a structural schematic diagram of a non-metallic flexible composite pipe connection structure of the present invention; Figure 2 It is a structural schematic diagram of the electric fusion sleeve of the present invention; Figure 3 It is a schematic diagram of the structure of the non-metallic flexible composite pipe body of the present invention; Figure 4 It is a schematic diagram of the reinforced single-layer structure of the reinforcing layer of the present invention.
[0026] The numbers in the accompanying drawings are: 1 is the inner lining layer, 101 is the inner lining welding surface, 2 is the reinforcement layer, 3 is the reinforcement single layer, 4 is the reinforcement welding surface, 5 is the plastic film, 6 is the reinforcement fiber layer, 7 is the outer protective layer, 8 is the electric fusion sleeve, 9 is the annular reinforcement body, 10 is the reinforcement body layer, 11 is the first welding surface, 12 is the second welding surface, 13 is the third welding surface, 14 is the resistance wire, and 15 is the terminal. DETAILED DESCRIPTION
[0027] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments: like Figure 1 to Figure 4 As shown, a non-metallic flexible composite pipe connection structure includes an electric fusion sleeve 8 and two non-metallic flexible composite pipes, the electric fusion sleeve 8 is sleeved on the connection ends of the two non-metallic flexible composite pipes, the non-metallic flexible composite pipes include an inner lining layer 1, a reinforcing layer 2 and an outer protective layer 7 arranged in sequence from the inside to the outside, and the connection ends of the non-metallic flexible composite pipes are in a stepped structure. In this embodiment, the two non-metallic flexible composite pipes are tubular structures of the same size and structure, wherein the two non-metallic flexible composite pipes are inserted into the electric fusion sleeve 8 with the same length, the reinforcing layer 2 is fused with the inner lining layer 1 and the outer protective layer 7, the reinforcing layer 2 is formed by winding reinforcing fibers layer by layer, and is used to bear the load generated by fluid pressure, and the number of winding layers is usually an even number, and the outer protective layer 7 is used to protect the reinforcing layer 2 and the inner lining layer 1 structure.
[0028] The inner side wall of the electric fusion sleeve 8 is provided with a welding surface, the body of the electric fusion sleeve 8 is inlaid with an annular reinforcement body 9, and the body of the electric fusion sleeve 8 is spirally wound with a resistance wire 14; the inner lining layer 1, the reinforcement layer 2 and the outer protective layer 7 are respectively welded to the electric fusion sleeve 8 through the welding surface. In this embodiment, the annular reinforcement body 9 is coated inside the body of the electric fusion sleeve 8, which is composed of multiple layers of annularly wound fiber-reinforced thermoplastic plastic belts; the resistance wire 14 is placed in the body of the electric fusion sleeve 8 in a spirally wound manner, and the resistance wire 14 is powered to heat the resistance wire 14, so that the electric fusion sleeve 8 at the welding surface is melted, expanded and fused, wherein the electric melting temperature is 160°C±10°C, thereby achieving the purpose of welding the non-metallic flexible composite pipe and the electric fusion sleeve 8.
[0029] The length of the inner lining layer 1 is greater than that of the reinforcing layer 2, and a lining welding surface 101 is provided at the connecting end of the inner lining layer 1. The length of the reinforcing layer 2 is greater than that of the outer protective layer 7. The inner lining layer 1 and the outer protective layer 7 are both made of thermoplastic plastic material through an extrusion process. In this embodiment, the inner lining welding surface 101 is formed by making the length of the inner lining layer 1 greater than that of the reinforcing layer 2. The inner lining welding surface 101 is closely fitted with the welding surface of the inner wall of the electric fusion sleeve 8, so that the inner lining layer 1 and the electric fusion sleeve 9 can be welded together. The inner lining layer 1 and the outer protective layer 7 can both be made of PE (polyethylene), PA (polyamide) and other materials. In this embodiment, the inner lining layer 1 and the outer protective layer 7 are both made of PE100 material.
[0030] The connection end of the reinforcement layer 2 is a stepped structure. The reinforcement layer 2 includes a plurality of reinforcement single layers 3. The length of the plurality of reinforcement single layers 3 gradually shortens from the inside to the outside. The connection end of each reinforcement single layer 3 is provided with a reinforcement welding surface 4. The winding angle and thickness of two adjacent reinforcement single layers 3 are the same. The winding directions of the two adjacent reinforcement single layers 3 are opposite. The two adjacent reinforcement single layers 3 are connected by hot melt. In this embodiment, the number of reinforcement single layers 3 of the reinforcement layer 2 is four, wherein the winding angle is the angle between the reinforcement single layer 3 and the axial direction of the non-metallic flexible composite pipe. The purpose of the length of the plurality of reinforcement single layers 3 gradually shortening from the inside to the outside is to make the connection end of each reinforcement single layer 3 constitute a reinforcement welding surface 4, and the reinforcement welding surface 4 cooperates with the welding surface of the inner wall of the electric melting sleeve 8, so as to facilitate the welding of the reinforcement layer 2 and the electric melting sleeve 9.
[0031] The reinforcing single layer 3 includes a reinforcing fiber layer 6 and a plastic film 5 arranged on the upper and lower sides of the reinforcing fiber layer 6. The reinforcing fiber layer 6 is made of inorganic fiber or organic fiber. The two adjacent reinforcing single layers 3 are welded together by the plastic film 5. The plastic film 5 is also made of thermoplastic plastic material; the outermost reinforcing single layer 3 is welded to the outer protective layer 7, and the innermost reinforcing single layer 3 is welded to the inner lining layer 1. The plastic film 5 is also made of PE (polyethylene), PA (polyamide) and other materials. The reinforcing fiber layer 6 can be made of polyester fiber, aramid fiber, glass fiber and other materials. In this embodiment, the plastic film 5 is also made of PE100 material, and the reinforcing fiber layer 6 is made of polyester fiber. The plastic film 5 is wound together with the reinforcing fiber layer 6. When winding the plastic film 5 and the reinforcing fiber layer 6, the winding forming part is heated by a hot air gun, such as Figure 4 As shown, the heating temperature is 160°C ± 10°C, which is higher than the melting point of the plastic film 5 but does not exceed the melting point of the reinforcing fiber layer 6. Since the melting point of PE100 is 120°C and the melting point of polyester yarn is 225°C, 160°C ± 10°C can ensure effective welding of the local plastic film 5 without causing damage to the reinforcing fiber layer 6.
[0032] The electric fusion sleeve 8 is made of thermoplastic plastic material through an injection molding process. The welding surfaces include a first welding surface 11, a second welding surface 12 and a third welding surface 13. The inner side wall of the electric fusion sleeve 8 is symmetrically provided with two of the first welding surfaces 11 and the second welding surfaces 12. The third welding surface 13 is located between the two second welding surfaces 12. The first welding surface 11 matches the outer protective layer 7, the second welding surface 12 matches the reinforced welding surface 4, and the third welding surface 13 matches the lining welding surface 101. The body of the electric fusion sleeve 8 is also made of materials such as PE (polyethylene) and PA (polyamide). In this embodiment, the body of the electric fusion sleeve 8 is also made of PE100 material, and the welding surfaces include a first welding surface 11, a second welding surface 12 and a third welding surface 13 arranged in sequence from the outside to the inside. The diameter of the second welding surface 12 gradually decreases from the outside to the inside, and the diameters of the two ends of the second welding surface 12 are respectively the same as the diameters of the first welding surface 11 and the third welding surface 13; when the non-metallic flexible composite pipe is inserted into the electric fusion sleeve 8, the outer protective layer 7 is tightly fitted with the first welding surface 11, the reinforced welding surface 4 of the connecting end of the reinforcing layer 2 cooperates with the second welding surface 12, and the inner lining welding surface 101 of the inner lining layer 1 is tightly fitted with the third welding surface 13.
[0033] The annular reinforcement body 9 includes a plurality of reinforcement body layers 10 stacked in sequence, and the length of the plurality of reinforcement body layers 10 gradually increases from the inside to the outside; two adjacent reinforcement body layers 10 are fused to each other, and the reinforcement body layer 10 is fused to the barrel of the electric melting sleeve 8. In this embodiment, the annular reinforcement body 9 includes four reinforcement body layers 10, and the annular reinforcement body 9 is composed of multiple layers of circumferentially wound reinforcing fiber thermoplastic plastic tapes, and the reinforcing fibers include organic fibers and inorganic fibers, such as polyester fibers, aramid fibers, glass fibers, etc. The annular reinforcement body 9 is formed by circumferentially winding aramid fiber reinforced PE100 material tapes.
[0034] Two wiring terminals 15 are symmetrically arranged on the outer side of the electric fusion sleeve 8, and the two ends of the resistance wire 14 are respectively connected to the two wiring terminals 15. In this embodiment, the wiring terminals 15 can be connected to an electric fusion welding machine to supply power to the resistance wire 14 through the wiring terminals 15, so that the resistance wire 14 heats up and electrically fuses the electric fusion sleeve 8.
[0035] A connection method based on a non-metallic flexible composite pipe connection structure includes the following steps: Step 1: Insert the two non-metallic flexible composite pipes to be connected into the electric fusion sleeve 8 respectively, so that the outer protective layer 7 of the non-metallic flexible composite pipe matches the first welding surface 11, the reinforced welding surface 4 of the reinforcing layer 2 matches the second welding surface 12, and the lining welding surface 101 matches the third welding surface 13, and connect the two terminal blocks 15 to the electric fusion welding machine.
[0036] Step 2: Check whether the non-metallic flexible composite pipe is inserted tightly, whether the two non-metallic flexible composite pipes are coaxial, and whether the ends of the inner lining layer 1 of the two non-metallic flexible composite pipes are in contact. After checking that everything is correct, power on the electric fusion welding machine.
[0037] Step 3: The resistance wire 14 generates heat to melt, expand and fuse the body of the electric fusion sleeve 8 in the first welding surface 11 , the second welding surface 12 and the third welding surface 13 .
[0038] Step 4: After the electric fusion sleeve 8 is welded with the inner lining layer 1, the reinforcement layer 2 and the outer protective layer 7 of the non-metallic flexible composite pipe, the electric fusion welding machine is powered off and the electric fusion welding is completed. The electric fusion sleeve 8, the inner lining layer 1, the plastic film 5 and the outer protective layer 7 are all made of thermoplastic plastic materials. After the electric fusion welding is completed, the inner lining layer 1, the reinforcement layer 2 and the outer protective layer 7 of the non-metallic flexible composite pipe are welded to the electric fusion sleeve 8 as a whole; the electric fusion temperature is 160℃±10℃. Since the melting point of PE100 is 120℃, the melting point of polyester fiber is 225℃, and the melting point of aramid fiber is greater than 300℃, it can be ensured at 160℃±10℃ that the reinforcing fiber is not damaged under the premise of effective welding of the local PE100 material.
[0039] Step 5: After the electric fusion sleeve 8 and the non-metallic flexible composite pipe have been cooled, the connection of the two non-metallic flexible composite pipes is completed.
[0040] The embodiments described above are only preferred embodiments of the invention and are not intended to limit the scope of implementation of the invention. Therefore, any equivalent changes or modifications made according to the technical solutions described in the patent scope of the present invention should be included in the scope of the patent application of the present invention.
Claims
1. A non-metallic flexible composite pipe connection structure, characterized in that: It comprises an electric fusion sleeve (8) and two non-metallic flexible composite pipes, wherein the electric fusion sleeve (8) is sleeved on the connecting ends of the two non-metallic flexible composite pipes, the non-metallic flexible composite pipes comprise an inner lining layer (1), a reinforcement layer (2) and an outer protective layer (7) which are arranged in sequence from the inside to the outside, and the connecting ends of the non-metallic flexible composite pipes are in a stepped structure; The inner side wall of the electric fusion sleeve (8) is provided with a welding surface, the barrel of the electric fusion sleeve (8) is embedded with an annular reinforcement body (9), and the barrel of the electric fusion sleeve (8) is spirally wound with a resistance wire (14); the inner lining layer (1), the reinforcement layer (2) and the outer protective layer (7) are respectively welded to the electric fusion sleeve (8) via the welding surface.
2. A non-metallic flexible composite pipe connection structure according to claim 1, characterized in that: The length of the inner lining layer (1) is greater than the length of the reinforcing layer (2); a lining welding surface (101) is provided at the connecting end of the inner lining layer (1); the length of the reinforcing layer (2) is greater than the length of the outer protective layer (7); and both the inner lining layer (1) and the outer protective layer (7) are made of thermoplastic plastic material through an extrusion process.
3. A non-metallic flexible composite pipe connection structure according to claim 2, characterized in that: The connection end of the reinforcement layer (2) is in a stepped structure. The reinforcement layer (2) comprises a plurality of reinforcement single layers (3). The lengths of the plurality of reinforcement single layers (3) gradually decrease from the inside to the outside. The connection end of each reinforcement single layer (3) is provided with a reinforcement welding surface (4). The winding angle and thickness of two adjacent reinforcement single layers (3) are the same. The winding directions of two adjacent reinforcement single layers (3) are opposite. The two adjacent reinforcement single layers (3) are connected by hot melt.
4. A non-metallic flexible composite pipe connection structure according to claim 3, characterized in that: The reinforced single layer (3) comprises a reinforced fiber layer (6) and a plastic film (5) arranged on the upper and lower sides of the reinforced fiber layer (6), the reinforced fiber layer (6) is made of inorganic fiber or organic fiber, two adjacent reinforced single layers (3) are welded together by the plastic film (5), and the plastic film (5) is also made of thermoplastic plastic material; the outermost reinforced single layer (3) is welded to the outer protective layer (7), and the innermost reinforced single layer (3) is welded to the inner lining layer (1).
5. The non-metallic flexible composite pipe connection structure according to claim 3, characterized in that: The electric fusion sleeve (8) is made of thermoplastic material through an injection molding process, and the welding surface comprises a first welding surface (11), a second welding surface (12) and a third welding surface (13). The inner side wall of the electric fusion sleeve (8) is symmetrically provided with two of the first welding surfaces (11) and the second welding surfaces (12), and the third welding surface (13) is located between the two second welding surfaces (12). The first welding surface (11) matches the outer protective layer (7), the second welding surface (12) matches the reinforced welding surface (4), and the third welding surface (13) matches the inner lining welding surface (101).
6. The non-metallic flexible composite pipe connection structure according to claim 1, characterized in that: The annular reinforcement body (9) comprises a plurality of reinforcement body layers (10) stacked in sequence, the lengths of the plurality of reinforcement body layers (10) gradually increasing from the inside to the outside; two adjacent reinforcement body layers (10) are fused to each other, and the reinforcement body layers (10) are fused to the barrel of the electric fusion sleeve (8).
7. The non-metallic flexible composite pipe connection structure according to claim 1, characterized in that: Two wiring terminals (15) are symmetrically arranged on the outer side of the electric fusion sleeve (8), and two ends of the resistance wire (14) are respectively connected to the two wiring terminals (15).
8. A connection method for a non-metallic flexible composite pipe connection structure according to claims 1-7, characterized in that: The following steps are involved: Step 1: insert two non-metallic flexible composite pipes to be connected into the inside of the electric fusion sleeve (8) respectively, so that the outer protective layer (7) of the non-metallic flexible composite pipe matches the first welding surface (11), the reinforced welding surface (4) of the reinforcement layer (2) matches the second welding surface (12), and the lining welding surface (101) matches the third welding surface (13), and connect the two terminal blocks (15) to the electric fusion welding machine; Step 2: Check whether the non-metallic flexible composite pipes are inserted tightly, whether the two non-metallic flexible composite pipes are coaxial, and whether the ends of the inner lining layers (1) of the two non-metallic flexible composite pipes are in contact with each other. After the inspection is correct, power on the electric fusion welding machine; Step 3: The resistance wire (14) generates heat to melt, expand and fuse the body of the electric fusion sleeve (8) in the areas of the first fusion surface (11), the second fusion surface (12) and the third fusion surface (13); Step 4: After the electric fusion sleeve (8) is fused with the inner lining layer (1), the reinforcement layer (2) and the outer protective layer (7) of the non-metallic flexible composite pipe, the electric fusion welding machine is powered off, and the electric fusion welding is completed; Step 5: After the electric fusion sleeve (8) and the non-metallic flexible composite pipe are cooled, the connection of the two non-metallic flexible composite pipes is completed.
9. A connection method for a non-metallic flexible composite pipe connection structure according to claim 8, characterized in that: In step 4, the electric fusion sleeve (8), the inner lining layer (1), the plastic film (5) and the outer protective layer (7) are all made of thermoplastic plastic material. After the electric fusion welding is completed, the inner lining layer (1), the reinforcement layer (2) and the outer protective layer (7) of the non-metallic flexible composite pipe are welded to the electric fusion sleeve (8) as a whole.
Citation Information
Patent Citations
Connecting structure and connecting method for reinforced composite pipes
CN105402542A
Continuous fiber pre-impregnated stirrup belt ring thermoplastic composite oil and gas gathering and transportation pipeline
CN112833263A
Coupling sleeve for high-pressure pipe
CN1300357A
Pored steel frame reinforced composite polymer pipeline adaptor
CN2608804Y