By designing an isolation mesh barrel for wafer partition corrosion, using liquid surface tension and regional corrosion technology, the problem of being unable to achieve precision partitioning and isolating the areas to be corroded in the prior art is solved, and higher wafer uniformity and Process stability.
Patent Information
- Application Number
- CN202411267836.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-09-11
AI Technical Summary
The prior art cannot achieve precision partitioning and isolate the areas to be corroded, resulting in uneven thickness or performance in wafer manufacturing and the goal of higher uniformity cannot be achieved.
Design an isolation mesh barrel for wafer partition corrosion. The wafer surface is separated into multiple independent corrosion areas through the cylinder wall and the isolation mesh wall. The liquid surface tension is used to prevent mixing between corrosion liquids, and cooperate with regional corrosion technology. Achieve precision control.
Precision partition corrosion is achieved, corrosion fluid mixing is avoided in adjacent areas, and more stringent wafer uniformity requirements are met, and wafer surfaces are not scratched, which improves process stability.
Smart Images

Figure CN118782507B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductor integrated circuit manufacturing, and in particular relates to an isolation mesh tube used for wafer partition etching and an etching method. Background Art
[0002] The uniformity of wafer thickness or other performance indicators produced in the thin film deposition or growth process on the substrate of semiconductor manufacturing is a key indicator directly related to the consistency of back-end components and is also the goal of its process technology. At present, there are many methods to control the uniformity of the wafer growth process, and they can meet the requirements of general manufacturing. However, with the development and application of semiconductor technology and the increase in cost requirements, the existing technology for optimizing uniformity in the growth link can no longer meet the further demand for wafer uniformity. Especially in the semiconductor wafer manufacturing in the field of sensing, the differences in indicators such as thickness and resistance of sensitive materials will cause the components produced by the same wafer in the back end to have large differences in sensitivity and accuracy. This will lead to the production of components with different performances in the same wafer, and their differences and distribution cannot be controlled, which is an uncontrollable factor that must be solved in product quality control. Therefore, it is necessary to measure the thickness or electrical performance distribution after growth and then use the local corrosion method to achieve a more precise control of wafer uniformity. There are relatively few methods to control uniformity after growth. Currently, they mainly rely on local stress or pressure to adjust the corrosion rate and local spray corrosion during CMP.
[0003] However, the above-mentioned existing technical solutions are unable to achieve precise zoning and isolation of the area to be etched, so the etching effect on the wafer with more detailed uniformity as the goal is less, and a higher uniformity goal cannot be achieved.
[0004] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because they are described in the background technology section of the present application. Summary of the invention
[0005] In view of the above-mentioned shortcomings of the prior art, the purpose of the present invention is to provide an isolation mesh tube and an etching method for wafer partition etching, so as to solve the problem of thickness or performance unevenness that is inevitable in wafer manufacturing in the prior art.
[0006] To achieve the above-mentioned purpose and other related purposes, the present invention provides an isolation mesh cylinder for wafer partition etching, the isolation mesh cylinder comprising: a cylinder wall, which is used to be sleeved on the periphery of the wafer and is adsorbed and fixed together with the wafer by a vacuum adsorption table; an isolation mesh wall, which is fixed in the cylinder wall and is used to separate the wafer surface into a plurality of independent corrosion areas. When the cylinder wall is fixed by the vacuum adsorption table, the isolation mesh wall extends above the wafer surface and has a distance from the wafer surface to form a non-contact air gap. The non-contact air gap is configured so that when the etching liquid enters a certain corrosion area, based on the surface tension of the liquid, the etching liquid will not enter another corrosion area adjacent to the corrosion area.
[0007] Optionally, the radial width of the barrel wall is greater than the radial width of the wafer, and when the barrel wall is sleeved around the periphery of the wafer, the distance between the barrel wall and the edge of the wafer is 30 microns to 500 microns.
[0008] Optionally, the thickness of the isolation network wall ranges from 10 microns to 300 microns.
[0009] Optionally, the height difference between the cylinder wall and the isolation net wall is the sum of the wafer height plus 5 microns to 500 microns.
[0010] Optionally, when the cylinder wall is fixed by the vacuum adsorption table, the distance between the isolation mesh wall and the wafer surface is 5 microns to 500 microns.
[0011] Optionally, the isolation net wall is configured as a square columnar grid.
[0012] Optionally, the isolation net wall is configured as a hexagonal columnar grid.
[0013] Optionally, the isolation net wall is configured as a concentric cylindrical grid.
[0014] Optionally, the isolation net wall is configured as a cylindrical fan-shaped grid.
[0015] The present invention also provides an etching method based on an isolation mesh tube for wafer partition etching, the etching method comprising the following steps: grouping a plurality of mutually independent etching areas separated by the isolation mesh wall so that any two etching areas in each group are not adjacent; and etching the wafer surface in the etching area in each group in turn until the etching of the entire wafer is completed.
[0016] Optionally, the etching parameters of each etching area are set according to the etching amount required for the corresponding wafer surface.
[0017] Optionally, after etching the wafer surface in each group of etching areas, the isolation mesh cylinder is taken out and the wafer surface is cleaned, and then the wafer surface in the next group of etching areas is etched.
[0018] As described above, the isolation mesh cylinder and etching method for wafer partition etching of the present invention have the following beneficial effects:
[0019] The present invention utilizes the tension of the solution to design an isolation mesh cylinder for precise partition etching without contacting the wafer surface, and performs partition etching on uneven wafers. The present invention can realize partition etching on a wafer, and the shape and size of each corrosion area can be achieved by designing the isolation mesh cylinder to meet actual needs, and cooperate with regional etching technology (such as applying different concentrations of etching solution or different etching time to each corrosion area) to achieve precise control of the partition, meet more precise control and stricter wafer uniformity requirements, and will not cause scratches on the wafer surface and the situation where the etching solution of adjacent areas is mixed and cannot be distinguished.
[0020] The present invention also realizes a wafer etching method, which groups the multiple independent etching areas separated by the isolation mesh wall so that any two etching areas in each group are not adjacent, and then sequentially etches the wafer surface in the etching area in each group until the etching of the entire wafer is completed. This can further avoid the situation where the etching liquids in adjacent areas are mixed and cannot be distinguished, thereby achieving more accurate partitioned etching. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The included drawings are used to provide a further understanding of the embodiments of the present application, which constitute a part of the specification, are used to illustrate the implementation of the present application, and together with the text description, explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application.
[0022] Figure 1~Figure 2 Shown is a schematic structural diagram of a first isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0023] Figure 3 Shown is a schematic diagram of a first etching method based on an isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0024] Figure 4 Shown is a schematic structural diagram of a second isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0025] Figure 5 It is a schematic diagram showing a second etching method based on an isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0026] Figure 6 Shown is a schematic structural diagram of a third isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0027] Figure 7It is a schematic diagram showing a third etching method based on an isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0028] Figure 8 Shown is a schematic structural diagram of a fourth isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0029] Fig. 9 It is a schematic diagram showing a fourth etching method based on an isolation mesh tube for wafer partition etching according to an embodiment of the present invention.
[0030] Explanation of component numbers: 101 cylinder wall, 102 isolation mesh wall, 103 vacuum adsorption table, 104 wafer, 105 corrosion area. DETAILED DESCRIPTION
[0031] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0032] It should be emphasized that the term “include / comprises” when used herein refers to the presence of features, integers, steps or components, but does not exclude the presence or addition of one or more other features, integers, steps or components.
[0033] Features described and / or illustrated with respect to one embodiment may be used in the same or similar manner in one or more other embodiments, combined with features in other embodiments, or substituted for features in other embodiments.
[0034] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.
[0035] For ease of description, spatially relative terms such as "under," "below," "below," "below," "above," "on," etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or one or more intervening layers may also be present.
[0036] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0037] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0038] Since the existing technical solutions cannot achieve precise partitioning and isolation of the area to be etched, the etching effect on the more delicate wafer with uniformity as the goal is small, and thus a higher uniformity goal cannot be achieved. The present invention uses the tension of the solution to design an isolation mesh cylinder for precise partitioning etching without contacting the wafer surface, and etches the uneven wafer in partitions. The divided small areas can be rectangular, regular hexagonal, or concentric rings. In conjunction with regional etching technology (such as applying different concentrations of etching solution or different etching times to each small area), precise control of the partitions can be achieved to achieve the purpose of uniforming the wafer surface.
[0039] like Figure 1~Figure 2 As shown, this embodiment provides an isolation mesh cylinder for zoned etching of a wafer 104, the isolation mesh cylinder comprising: a cylinder wall 101, which is used to be sleeved on the periphery of the wafer 104 and is adsorbed and fixed together with the wafer 104 by a vacuum adsorption platform 103; an isolation mesh wall 102, which is fixed in the cylinder wall 101, and is used to separate the surface of the wafer 104 into a plurality of mutually independent corrosion areas 105. When the cylinder wall 101 is fixed by the vacuum adsorption platform 103, the isolation mesh wall 102 extends above the surface of the wafer 104 and has a distance from the surface of the wafer 104 to form a non-contact air gap. The non-contact air gap is configured such that when the etching liquid enters a certain corrosion area 105, based on the surface tension of the liquid, the etching liquid will not enter another corrosion area 105 adjacent to the corrosion area 105.
[0040] like Figure 1As shown, in one embodiment, the material of the barrel wall 101 can be a corrosion-resistant material such as polymer, ceramic, metal, etc., and the shape of the barrel wall 101 can be, for example, cylindrical. The radial width of the barrel wall 101 is greater than the radial width of the wafer 104. When the barrel wall 101 is sleeved on the periphery of the wafer 104, the distance D2 between the barrel wall 101 and the edge of the wafer 104 is 30 microns to 500 microns, such as 100 microns, 200 microns, 300 microns, etc., to avoid collision with the wafer 104 during sleeve installation and cause damage to the wafer 104 or the barrel wall 101.
[0041] like Figure 1 As shown, in one embodiment, the thickness of the cylinder wall 101 is relatively thick so that it can be adsorbed and fixed by the vacuum adsorption platform 103. For example, the thickness of the cylinder wall 101 can be between 1 mm and 30 mm, so that it can be adsorbed and fixed by the vacuum adsorption platform 103 while ensuring its mechanical strength and not being easily deformed.
[0042] like Figure 1 As shown, the thickness of the isolation mesh wall 102 is small to ensure that the area of the wafer 104 occupied by the isolation mesh wall 102 is small, thereby ensuring the integrity of the surface corrosion of the wafer 104. In one embodiment, the thickness of the isolation mesh wall 102 ranges from 10 microns to 300 microns, for example, 50 microns, 200 microns, etc. The material of the isolation mesh wall 102 can be a corrosion-resistant material such as polymer, ceramic, metal, etc. The isolation mesh wall 102 can be integrally formed with the cylinder wall 101, or fixedly connected to the cylinder wall 101 by welding, pasting, etc.
[0043] like Figure 1 As shown, in one embodiment, the height difference between the cylinder wall 101 and the isolation mesh wall 102 is the height of the wafer 104 plus the sum of 5 microns to 500 microns. When the cylinder wall 101 is fixed by the vacuum adsorption platform 103, the spacing D1 between the isolation mesh wall 102 and the non-contact air gap on the surface of the wafer 104 is 5 microns to 500 microns. The non-contact air gap of the present invention is configured so that when the corrosive liquid enters a certain corrosion area 105, the corrosive liquid will not enter the adjacent corrosion area 105 based on the surface tension of the liquid, which can avoid the isolation mesh wall 102 from damaging the wafer 104, greatly improve the process stability, and at the same time, it can eliminate the situation where some direct contact is caused by the height difference caused by the direct contact due to the uneven surface of the wafer 104.
[0044] like Figure 2 As shown, in one embodiment, the isolation mesh wall 102 is configured as a square column grid.
[0045] like Figure 4As shown, in one embodiment, the isolation mesh wall 102 is configured as a concentric cylindrical grid. For this configuration, the concentric cylinders can be fixed to each other by providing one or more beams (such as along the diameter direction) on the top of the isolation mesh wall 102. The beams are only provided on the top of the isolation mesh wall 102 and will not affect the actual corrosion area.
[0046] like Figure 6 As shown, in one embodiment, the isolation mesh wall 102 is configured as a cylindrical fan-shaped grid.
[0047] like Figure 8 As shown, in one embodiment, the isolation mesh wall 102 is configured as a hexagonal columnar grid.
[0048] Of course, in other embodiments, the isolation mesh wall 102 may also be configured as a grid of other shapes, such as a rhombus, a triangle, a mixed grid of the above-listed shapes, or an irregular shape, etc., and is not limited to the examples listed here.
[0049] The present invention utilizes the tension of the solution to design an isolation mesh cylinder for precise partition etching without contacting the surface of the wafer 104, and performs partition etching on the uneven wafer 104. The present invention can realize partition etching on a wafer 104, and the shape and size of each etching area 105 can be achieved to meet actual needs through the design of the isolation mesh cylinder, and the precise control of the partition is achieved in conjunction with the regional etching technology (such as applying different concentrations of etching solution or different etching time to each etching area), so as to meet the requirements of more precise control and more stringent uniformity of the wafer 104, and will not cause scratches on the wafer surface and the situation where the etching solutions of adjacent areas are mixed and cannot be distinguished.
[0050] In the isolation mesh cylinder for etching the wafer 104 in different areas of the present invention, when the etching liquid enters a certain etching area 105, due to the surface tension of the liquid, the etching liquid will not enter the adjacent etching area 105. When there are etching liquids in adjacent etching areas 105, the liquids may merge and form a mixture. For accurate etching, this embodiment proposes an etching method that can ensure the independence of each etching area 105, and when in use, etching liquid is not added to adjacent areas at the same time. Figure 3 , Figure 5 , Figure 7 , Fig. 9 As shown, this embodiment also provides an etching method based on an isolation mesh tube for zone etching of the wafer 104, the etching method comprising the following steps:
[0051] Step 1), grouping the multiple independent corrosion regions 105 separated by the isolation mesh wall 102 so that any two corrosion regions 105 in each group are not adjacent;
[0052] Step 2) etching the surface of the wafer 104 in the etching area 105 in each group in turn until the etching of the entire wafer 104 is completed.
[0053] In one embodiment, after the surface of the wafer 104 in each group of corrosion areas 105 is corroded, the isolation mesh tube is taken out and the surface of the wafer 104 is cleaned, and then the isolation mesh tube is aligned and put back in its original position, and then the surface of the wafer 104 in the next group of corrosion areas is corroded.
[0054] In a specific example, if Figure 3 As shown, for the isolation net cylinder in which the isolation net wall 102 is set as a square column grid, each corrosion area can be numbered. For example, the 14 grids in the upper part are numbered 1 to 14. The corrosion liquid of the corrosion areas 1, 3, 5, 7, 9, 11, and 13 are first filled to perform the first major step of local corrosion. After completion, the isolation net cylinder is taken out, and the surface of the wafer 104 is cleaned and then loaded. Alternatively, the isolation net cylinder is not taken out, and the local corrosion of the corrosion areas 2, 4, 6, 8, 10, 12, and 14 is directly performed after local cleaning and drying. In this way, the purpose of separate parameterized corrosion of each corrosion area is achieved, and the corrosion liquid of adjacent areas will not be mixed and cannot be distinguished, and the partitioned corrosion of the entire wafer 104 is completed. Of course, the above numbering number is only for the convenience of explanation. In fact, according to the above explanation principle, more numbers can be added to the same group to etch more corrosion areas at the same time, thereby improving the corrosion efficiency.
[0055] like Figure 5 As shown, when the key parameter distribution of the material growth process on the wafer 104 determines its uniformity is in a ring shape, it is suitable to Figure 5 The isolation mesh wall 102 shown is configured as an isolation mesh cylinder of concentric cylindrical grids, which can divide the wafer 104 into a number of concentric rings, and etch each ring portion at intervals. For example, the etching areas 1, 3, and 5 can be etched first, and then the etching areas 2, 4, and 6 can be etched after cleaning. Figure 7 As shown, if the angular non-uniformity also occurs, the angular division can be further divided into Figure 7 The sector area shown, i.e., the isolation mesh cylinder with the isolation mesh wall 102 set as a cylindrical sector mesh, can be etched in the order of first etching the etching areas 1, 7, 3, and 9, then etching the etching areas 2, 4, 6, and 8, and then etching 5 and 10 respectively. The above numbering numbers are only for the convenience of description. In fact, according to the above description principle, more numbers can be added in the same group to etch more etching areas at the same time, thereby improving the etching efficiency.
[0056] like Fig. 9As shown, for an isolation mesh cylinder in which the isolation mesh wall 102 is set as a hexagonal columnar grid, the partition etching can be performed in multiple steps. In the first step, the corrosion area marked as 1 is etched, and after cleaning, the second step is performed, and the corrosion area marked as 2 is etched, and after cleaning again, the third step is performed, and the corrosion area marked as 3 is etched. The above numbering number is only for the convenience of description. In fact, according to the above description principle, more numbers can be added in the same group to etch more corrosion areas at the same time, thereby improving the etching efficiency.
[0057] As described above, the isolation mesh tube and etching method for wafer 104 partition etching of the present invention have the following beneficial effects:
[0058] The present invention utilizes the tension of the solution to design an isolation mesh cylinder for precise partition etching without contacting the surface of the wafer 104, and performs partition etching on the uneven wafer 104. The present invention can realize partition etching on a wafer 104, and the shape and size of each etching area can be achieved to meet actual needs through the design of the isolation mesh cylinder, and the precise control of the partition is achieved in conjunction with the regional etching technology (such as applying different concentrations of etching solution or different etching time to each etching area, etc.), so as to meet the requirements of more precise control and more stringent uniformity of the wafer 104, and will not cause scratches on the wafer surface and the situation where the etching solutions of adjacent areas are mixed and cannot be distinguished.
[0059] The present invention also realizes a method for etching the wafer 104, by grouping the multiple independent etching areas separated by the isolation mesh wall 102 so that any two etching areas in each group are not adjacent, and then etching the surface of the wafer 104 in the etching area in each group in turn until the etching of the entire wafer 104 is completed, which can further avoid the situation where the etching liquids in adjacent areas are mixed and cannot be distinguished, thereby achieving more accurate partitioned etching.
[0060] Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.
[0061] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. An isolation mesh cylinder for wafer partition etching, characterized in that: The isolation net cylinder comprises: The cylinder wall is used to be sleeved on the periphery of the wafer and is adsorbed and fixed together with the wafer by the vacuum adsorption table; The isolation mesh wall is fixed in the cylinder wall and is used to separate the wafer surface into a plurality of independent corrosion areas. When the cylinder wall is fixed by the vacuum adsorption table, the isolation mesh wall extends above the wafer surface and has a distance from the wafer surface to form a non-contact air gap. The non-contact air gap is configured so that when the etching liquid enters a certain corrosion area, the etching liquid will not enter another corrosion area adjacent to the corrosion area based on the surface tension of the liquid.
2. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The radial width of the barrel wall is greater than the radial width of the wafer. When the barrel wall is sleeved on the periphery of the wafer, the distance between the barrel wall and the edge of the wafer is 30 microns to 500 microns.
3. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The thickness of the isolation net wall ranges from 10 microns to 300 microns.
4. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The height difference between the cylinder wall and the isolation net wall is the sum of the wafer height plus 5 microns to 500 microns.
5. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: When the cylinder wall is fixed by the vacuum adsorption platform, the distance between the isolation mesh wall and the wafer surface is 5 microns to 500 microns.
6. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The isolation net wall is arranged as a square columnar grid.
7. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The isolation net wall is arranged as a hexagonal columnar grid.
8. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The isolation net wall is arranged as a concentric cylindrical grid.
9. The isolation mesh cylinder for wafer partition etching according to claim 1, characterized in that: The isolation net wall is arranged as a cylindrical fan-shaped grid.
10. An etching method for an isolation mesh cylinder for wafer partition etching according to any one of claims 1 to 9, characterized in that: include: Grouping the multiple independent corrosion areas separated by the isolation mesh wall so that any two corrosion areas in each group are not adjacent; The wafer surface within the etching area in each group is etched in turn until the etching of the entire wafer is completed.
11. The etching method based on the isolation mesh cylinder for wafer partition etching according to claim 10, characterized in that: The etching parameters of each etching area are set according to the required etching amount of the corresponding wafer surface.
12. The etching method based on the isolation mesh tube for wafer partition etching according to claim 10, characterized in that: After etching the wafer surface in each group of etching areas, the isolation mesh cylinder is taken out and the wafer surface is cleaned, and then the wafer surface in the next group of etching areas is etched.
Citation Information
Patent Citations
Corrosion method and device for silicon carbide wafers
CN103866398A
Etching method and etching device for third-generation semiconductor
CN111668096A
Wafer processing apparatus and semiconductor manufacturing apparatus
CN116705644A
Chemical mechanical polishing apparatus
KR1020050024100A
Modulated metal removal using localized wet etching
US20100029088A1