Automatic fire polishing machine for quartz boat surface

By combining a centralized flame shape and light and shadow detection component, the problem of unstable molten layer in fire polishing was solved, achieving efficient and energy-saving quartz boat surface polishing, reducing surface defects and energy consumption.

CN118791217BActive Publication Date: 2024-11-22HANGZHOU HONGXIN MICRO SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411284901.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-11-22
Estimated Expiration
2044-09-13

AI Technical Summary

Technical Problem

In existing flame polishing technology, the lack of flame concentration and uneven flow rate on the polishing surface lead to instability of the molten layer on the surface of the quartz boat, which easily produces surface defects such as scratches and pits, and also consumes a lot of energy.

Method used

Design an automatic flame polishing machine for quartz boat surfaces. Employ a quartz flame head with a concentrated flame shape. By controlling the gas fuel flow rate and wick design, ensure that the flame is evenly distributed on the polished surface. Use a light and shadow detection component to identify and adjust uneven areas in real time.

Benefits of technology

It improves polishing efficiency and energy utilization, reduces surface defects, lowers energy consumption, and ensures the precision and safety of the polishing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118791217B_ABST
    Figure CN118791217B_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of fire polishing devices, and discloses an automatic fire polishing machine for a quartz boat surface, comprising a polishing base and a quartz fire head, wherein a support frame for placing the quartz boat is arranged on the polishing base, and when placed, the end plates at both ends of the quartz boat are located on the outside of the support frame, and a connecting rod for connecting the two end plates is located on the inside, the quartz fire head uses gas fuel for combustion, a light and shadow detection component capable of identifying the projected shadow area is arranged at the bottom of the outer side of the support frame, a light source with a wavelength different from the flame wavelength in the flame polishing process is arranged above the outer side of the support frame, and the light source is directed downward so that the end plate to-be-polished surface of the quartz boat can be projected onto the light and shadow detection component, the quartz fire head is used to polish the end plate to-be-polished surface of the quartz boat, the quartz fire head flame is concentrated, and the flow velocity of the gas fuel on the side close to the polishing surface in the quartz fire head is smaller than that on the side away from the polishing surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fire polishing devices, in particular to an automatic fire polishing machine for the surface of a quartz boat. Background Art

[0002] Quartz boat, as a highly specialized precision ceramic product, is made of high-purity silicon dioxide (SiO2) as its core material. Its purity often reaches extremely high standards to meet the needs of various stringent industrial applications. It is not only an indispensable key component in the field of semiconductor manufacturing, but also an important support for many high-tech industries such as chemical, optics, and aerospace. In the semiconductor industry, quartz boat plays a vital role. As a key carrier in the wafer processing process, it carries the heavy responsibility of chemical vapor deposition, diffusion, etching, annealing and other complex process processing of wafers under high temperature environment. Quartz boat, with its excellent high temperature resistance, excellent chemical stability and extremely low thermal expansion coefficient, ensures that the wafer can maintain extremely high precision and consistency during the processing process, which is a key support for semiconductor It provides a solid foundation for the manufacture of bulk devices. In addition, quartz boats are also widely used in the field of new optical technologies, such as the manufacture of high-end equipment such as radar, infrared tracking and direction finding, astronomical telescopes, etc. Its high light transmittance and good electrical properties make quartz boats an indispensable component. At the same time, in the chemical and metallurgical fields, quartz boats are also widely used in various chemical reactions and molten metal processing processes due to their resistance to acid and alkali corrosion, high temperature and high pressure. Quartz boats are a kind of precision ceramic products that combine high precision, high purity and high temperature resistance. Its appearance has greatly promoted the development of many high-tech industries such as semiconductors, optics, chemicals, aerospace, etc. With the continuous advancement of science and technology and the continuous expansion of application fields, the performance and application scope of quartz boats will continue to upgrade and expand.

[0003] The two ends of the quartz boat are quartz glass plates, which are made by cutting on a large piece of quartz glass. When quartz glass is cut, scratches and pits will appear on the cut surface. Although the outer surface of the quartz boat does not directly contact the material, its appearance quality is also an important reflection of the overall quality of the product. Polishing the outer surface can improve the beauty of the quartz boat, and it also helps to reduce surface defects such as scratches and pits, thereby improving the market competitiveness of the product. Fire polishing mainly uses high-temperature flames to heat and melt the surface of the quartz boat to achieve the polishing effect. The high temperature of the flame melts a layer of material on the surface of the quartz boat, and the molten layer becomes smooth and flat under the action of surface tension. In this process, factors such as the temperature and speed of the flame, as well as the material and thickness of the quartz boat, will affect the polishing effect. Under the action of surface tension, the molten layer will tend to form the most stable form, that is, a smooth and flat surface. This natural flow and redistribution under the action of surface tension, the heating of the quartz fire head is usually heated by gas fuel, so that a fast-flowing airflow will be brought about during the heating process. The airflow may interfere with the melting stability of the quartz glass surface and form defects. Summary of the invention

[0004] (I) Technical problems to be solved: In view of the deficiencies of the prior art, the present invention provides an automatic fire polishing machine for the surface of a quartz boat, which has the advantages of concentrated flame and gentle flow rate to the polishing surface during polishing, thus solving the problem of stability of the molten layer on the polishing surface.

[0005] (ii) Technical solution: In order to achieve the purpose of concentrating the flame and slowing down the flow rate to the polishing surface during the above-mentioned polishing, the present invention provides the following technical solution: an automatic fire polishing machine for a quartz boat surface, comprising a polishing base and a quartz fire head, the polishing base is provided with a support frame for placing the quartz boat, the end plates at both ends of the quartz boat are located on the outside of the support frame when placed, and the connecting rod for connecting the two end plates is located on the inside, the quartz fire head uses gas fuel for combustion, the bottom of the outer side of the support frame is provided with a light and shadow detection component capable of identifying the projected shadow area, and a light source with a wavelength different from the flame wavelength in the flame polishing process is provided above the outer side of the support frame, the light source is directed downward, so that the end plate to be polished surface of the quartz boat can be projected onto the light and shadow detection component.

[0006] The quartz burner is used to polish the end plate to be polished surface of the quartz boat. The flame of the quartz burner is concentrated, and the flow speed of the gas fuel on the side close to the polishing surface in the quartz burner is smaller than that on the side away from the polishing surface.

[0007] Preferably, a circularly distributed wick is vertically arranged inside the quartz burner, and the gas fuel is sprayed out from the wick.

[0008] Preferably, the wick is divided into two parts, left and right, from the central axis, the end of the wick on one side is expanded outwards to increase the diameter of the wick tube, and the end of the wick on the other side is contracted inwards to reduce the diameter of the wick tube.

[0009] Preferably, the diameter of the wick end portion gradually shrinks from one side of the cross-section surface to the other side.

[0010] Preferably, a downwardly recessed arc-shaped groove is provided on the top of the support frame for accommodating the connecting rod.

[0011] Preferably, an air outlet is provided on the arc-shaped groove.

[0012] Preferably, the support frame is directly connected to the polishing base via a screw rod, and the screw rod is driven by a motor.

[0013] Preferably, the light and shadow detection component is provided with a filter capable of filtering the wavelength of flames.

[0014] (III) Beneficial effects: Compared with the prior art, the present invention provides an automatic fire-polishing machine for the surface of a quartz boat, which has the following beneficial effects: 1. The automatic fire-polishing machine for the surface of a quartz boat can minimize the loss of heat in the air through the highly concentrated flame shape designed by the quartz fire head, ensuring that most of the heat directly acts on the end plate to be polished surface of the quartz boat. This design significantly improves the utilization rate of thermal energy in the polishing process, thereby shortening the polishing time and improving production efficiency. The concentrated flame can quickly heat and melt the surface of the quartz glass, making the polishing process faster, which not only reduces the total time required for polishing, but also reduces energy consumption, which is in line with the modern industry's pursuit of high efficiency and energy saving. By controlling the flow rate of the gas fuel, the quartz fire head achieves a soft contact of the flame on the polishing surface. This soft The gentle flame can ensure that the heat is evenly distributed on the polishing surface, avoiding surface defects caused by local overheating, such as cracks and burns. When the soft flame melts the quartz glass surface, it has less interference with the molten layer, which helps to reduce surface defects caused by airflow disturbances, such as white lines and ripples. At the same time, the evenly distributed heat can promote the uniform cooling of the molten layer, further reducing the occurrence of defects. The concentrated flame shape reduces heat loss and improves energy efficiency. Compared with traditional polishing methods, quartz fire head polishing can significantly reduce energy consumption and meet the requirements of sustainable development. Since the heat is mainly concentrated on the polishing surface, the thermal impact on the surrounding environment is relatively small, which helps to reduce potential damage to surrounding equipment and materials during the polishing process and improve the safety and cleanliness of the production site.

[0015] 2. The automatic fire polishing machine for the quartz boat surface uses advanced projection and recognition technology through the light and shadow detection component, which can capture and identify the shadow areas on the surface of the quartz boat end plate in real time. These shadow areas directly reflect the unevenness of the surface and provide intuitive feedback information for the operator. By accurately measuring and analyzing the shape, size and position of the shadow area, the light and shadow detection component can quickly locate the specific position of the uneven area. This precise positioning capability helps the operator to adjust the polishing strategy in time to ensure the accuracy and efficiency of the polishing process. The real-time feedback mechanism of the light and shadow detection component enables the operator to discover and deal with surface defects in time, reducing omissions and repeated work in the polishing process, which helps to improve the overall quality of polishing and reduce the rework rate and cost waste caused by quality problems. The wavelength of the projection light source is different from the wavelength of the flame. This design effectively reduces the interference of the flame on the detection process. Even during the flame polishing process, the light and shadow detection component can accurately identify the shadow area, improving the accuracy and reliability of the detection. The automatic recognition function of the light and shadow detection component reduces the burden on the operator and makes the polishing process more convenient and efficient. The operator only needs to pay attention to the detection results to perform subsequent operations without the need for tedious manual detection work.

[0016] 3. The automatic fire polishing machine for the surface of the quartz boat provides a stable support platform for the connecting rod through the design of the arc groove, while reducing the possibility of the flame directly contacting the connecting rod. The relatively slow airflow ejected upward from the air outlet forms a barrier, which effectively prevents the flame from extending to the welding point between the connecting rod and the end plate, which protects the quality of the welding point and avoids the decrease or failure of the welding strength caused by high temperature, thereby ensuring the overall structural stability and service life of the quartz boat. The design of the arc groove and the air outlet simplifies the polishing operation process. The operator does not need to worry about the potential impact of the flame on the connecting rod and can focus more on the polishing itself. In addition, this design also reduces the safety risks during operation and reduces the injury accidents caused by uncontrolled flame or accidental contact. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the structure of the present invention.

[0018] Figure 2 Detailed schematic diagram of the arc groove of the present invention.

[0019] Figure 3 It is a schematic diagram of light source projection of the present invention.

[0020] Figure 4 It is a top view of the structure of the present invention.

[0021] Figure 5 It is a schematic diagram of a quartz fire head of the present invention.

[0022] Figure 6It is a schematic cross-sectional view of a quartz fire head of the present invention.

[0023] In the figure: 1. quartz boat; 2. polishing base; 3. quartz fire head; 21. support frame; 22. light and shadow detection component; 23. arc groove; 24. screw rod; 31. wick; 101. end plate; 102. connecting rod; 231. air outlet. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] Example 1: Please refer to Figure 1-Figure 3 and Figure 5 The automatic fire polishing machine for the surface of a quartz boat comprises a polishing base 2 and a quartz fire head 3. A support frame 21 for placing the quartz boat 1 is arranged on the polishing base 2. When placed, the end plates 101 at both ends of the quartz boat 1 are located on the outside of the support frame 21, and a connecting rod 102 for connecting the two end plates 101 is located on the inside. The quartz fire head 3 uses gas fuel for combustion. A light and shadow detection component 22 capable of identifying the projected shadow area is arranged at the bottom of the outer side of the support frame 21. A light source with a wavelength different from the flame wavelength in the flame polishing process is arranged above the outer side of the support frame 21. The light source is directed downward so that the surface to be polished of the end plate 101 of the quartz boat 1 can be projected onto the light and shadow detection component 22. Because the surface of the end plate 101 is uneven, a shadow area will be formed when the light source is projected downward. By identifying the shadow area, the uneven area can be quickly located, thereby improving the quality of polishing. Moreover, the wavelength of the projected light source is different from the wavelength of the flame, so that even during the flame polishing process, the interference caused by the flame wavelength on the shadow identified by the light and shadow detection component 22 is reduced.

[0026] The quartz burner 3 is used to polish the end plate 101 of the quartz boat 1. The flame of the quartz burner 3 is concentrated. Figure 6, and the flow velocity of the gas fuel on the side close to the polished surface of the quartz burner 3 is smaller than that on the side far from the polished surface. Because there is a certain difference in the flow velocity of the gas, the gas pressure also has a difference. Due to the Bernoulli principle, that is, the flow velocity is inversely proportional to the pressure, the gas velocity in the lower area with a larger diameter is relatively slow, while the gas velocity in the upper area with a smaller diameter is relatively fast. The pressure on the side with slow gas flow velocity is greater than that on the side with fast gas flow velocity. The gas fuel on the side with slow gas flow velocity will move to the side with fast flow velocity, making the flame convergent. The convergent flame shape can transfer heat to the quartz glass more concentratedly. The flame shape helps to melt the glass surface quickly and improve polishing efficiency. At the same time, because the flame on the side in contact with the polished surface flows more slowly and more gently, the softness of the flame is crucial to the polishing effect. Soft flame contact can ensure that heat is evenly distributed on the polished surface, avoiding local overheating or surface defects. When the soft flame melts the quartz glass surface, it has less interference with the molten layer, avoiding the formation of white lines due to excessive air flow speed when the molten layer cools down. At the same time, the flame temperature is controlled to avoid extreme conditions of being too high or too low.

[0027] See also Figure 6 A circularly distributed wick 31 is vertically arranged inside the quartz burner 3, and the gas fuel is ejected from the wick 31. The wick 31 is divided into two parts on the left and right sides from the central axis. The end of the wick 31 on one side is in an outward expansion shape, so that the diameter of the wick 31 increases, and the end of the wick 31 on the other side is in an inward contraction shape, so that the diameter of the wick 31 decreases. Since the end of the wick 31 on this side expands outward and the diameter increases, according to the continuity principle of the fluid (that is, the volume of the fluid flowing through any cross section of the pipeline per unit time is equal), the gas fuel needs to occupy a larger space when passing through this side. In order to maintain the continuity of the fluid volume, the flow rate of the gas fuel on this side will be reduced accordingly. On the contrary, the end of the wick 31 on the other side contracts inwardly and the diameter decreases. Also according to the continuity principle of the fluid, the gas fuel needs to occupy a smaller space when passing through this side. In order to maintain the continuity of the fluid volume, the flow rate of the gas fuel on this side will be increased accordingly. The slower air flow speed means that the impact of the flame on the polished surface is smaller, reducing the surface defects caused by air flow disturbance.

[0028] The top of the support frame 21 is provided with a downwardly recessed arc groove 23 for placing the connecting rod 102. The arc groove 23 is provided with an air outlet 231. The air outlet 231 can spray a slow airflow upward to prevent the flame of the quartz fire head 3 from extending to the welding point between the connecting rod 102 and the end plate 101 when polishing the end plate 101 of the quartz boat 1, thereby reducing the connection quality. In addition, the slow airflow has little interference with the polishing surface.

[0029] The support frame 21 is directly connected to the polishing base 2 via a screw rod 24 . The screw rod 24 is driven by a motor. The position of the support frame 21 can be adjusted by rotating the screw rod 24 to adapt to quartz boats 1 of different specifications.

[0030] The light and shadow detection component 22 is provided with a filter capable of filtering the flame wavelength, so as to reduce the interference of the light waves of the quartz flame head 3 on the light and shadow detection component 22 .

[0031] Example 2: Please refer to Figure 1-Figure 3 and Figure 5 The automatic fire polishing machine for the surface of a quartz boat comprises a polishing base 2 and a quartz fire head 3. A support frame 21 for placing the quartz boat 1 is arranged on the polishing base 2. When placed, the end plates 101 at both ends of the quartz boat 1 are located on the outside of the support frame 21, and a connecting rod 102 for connecting the two end plates 101 is located on the inside. The quartz fire head 3 uses gas fuel for combustion. A light and shadow detection component 22 capable of identifying the projected shadow area is arranged at the bottom of the outer side of the support frame 21. A light source with a wavelength different from the flame wavelength in the flame polishing process is arranged above the outer side of the support frame 21. The light source is directed downward so that the surface to be polished of the end plate 101 of the quartz boat 1 can be projected onto the light and shadow detection component 22. Because the surface of the end plate 101 is uneven, a shadow area will be formed when the light source is projected downward. By identifying the shadow area, the uneven area can be quickly located, thereby improving the quality of polishing. Moreover, the wavelength of the projected light source is different from the wavelength of the flame, so that even during the flame polishing process, the interference caused by the flame wavelength on the shadow identified by the light and shadow detection component 22 is reduced.

[0032] The quartz burner 3 is used to polish the end plate 101 of the quartz boat 1. The flame of the quartz burner 3 is concentrated. Figure 6, and the flow velocity of the gas fuel on the side close to the polished surface of the quartz burner 3 is smaller than that on the side far from the polished surface. Because there is a certain difference in the flow velocity of the gas, the gas pressure also has a difference. Due to the Bernoulli principle, that is, the flow velocity is inversely proportional to the pressure, the gas velocity in the lower area with a larger diameter is relatively slow, while the gas velocity in the upper area with a smaller diameter is relatively fast. The pressure on the side with slow gas flow velocity is greater than that on the side with fast gas flow velocity. The gas fuel on the side with slow gas flow velocity will move to the side with fast flow velocity, making the flame convergent. The convergent flame shape can transfer heat to the quartz glass more concentratedly. The flame shape helps to melt the glass surface quickly and improve polishing efficiency. At the same time, because the flame on the side in contact with the polished surface flows more slowly and more gently, the softness of the flame is crucial to the polishing effect. Soft flame contact can ensure that heat is evenly distributed on the polished surface, avoiding local overheating or surface defects. When the soft flame melts the quartz glass surface, it has less interference with the molten layer, avoiding the formation of white lines due to excessive air flow speed when the molten layer cools down. At the same time, the flame temperature is controlled to avoid extreme conditions of being too high or too low.

[0033] See also Figure 6 A circularly distributed wick 31 is vertically arranged inside the quartz fire head 3, and the gas fuel is sprayed from the wick 31. The diameter of the end of the wick 31 gradually shrinks from one side of the cross-section to the other side (not shown). According to the continuity principle of the fluid, the mass (or volume) of the fluid passing through any cross-section of the pipeline per unit time is constant, which means that if the cross-sectional area of ​​the pipeline changes, the flow rate of the fluid will also change accordingly to maintain the continuity of the flow rate. At the end of the wick 31, the diameter gradually shrinks from one side of the cross-sectional surface to the other side. When the gas fuel passes through this gradually shrinking pipeline, in order to maintain the continuity of the flow rate, the flow rate of the gas fuel in the area with a smaller diameter (i.e., the side away from the polishing surface) must be increased to pass the same volume of gas in a smaller cross-sectional area. At the same time, the linear change of the wick 31 reduces the difference in the flow rate and pressure change of the airflow in adjacent wicks 31, reduces the occurrence of turbulence and turbulence, and makes the flame more stable.

[0034] The top of the support frame 21 is provided with a downwardly recessed arc groove 23 for placing the connecting rod 102. The arc groove 23 is provided with an air outlet 231. The air outlet 231 can spray a slow airflow upward to prevent the flame of the quartz fire head 3 from extending to the welding point between the connecting rod 102 and the end plate 101 when polishing the end plate 101 of the quartz boat 1, thereby reducing the connection quality. In addition, the slow airflow has little interference with the polishing surface.

[0035] The support frame 21 is directly connected to the polishing base 2 via a screw rod 24 . The screw rod 24 is driven by a motor. The position of the support frame 21 can be adjusted by rotating the screw rod 24 to adapt to quartz boats 1 of different specifications.

[0036] The light and shadow detection component 22 is provided with a filter capable of filtering the flame wavelength, so as to reduce the interference of the light waves of the quartz flame head 3 on the light and shadow detection component 22 .

[0037] Working principle: The worker places the quartz boat 1 on the polishing base 2. Because the end plate 101 of the quartz boat 1 is formed by cutting, there is a rough surface on the edge formed by cutting. From a microscopic perspective, the rough surface is the depression formed by the uneven surface of the quartz glass. Fire polishing mainly uses a high-temperature flame to heat and melt the surface of the quartz boat to achieve the polishing effect. The high temperature of the flame causes a layer of material on the surface of the quartz boat to melt, and the molten layer becomes smooth and flat under the action of surface tension. In this process, factors such as the temperature and speed of the flame, as well as the material and thickness of the quartz boat, will affect the polishing effect. Under the action of surface tension, the molten layer will tend to form the most stable form, that is, a smooth and flat surface. The natural flow and redistribution under the action of surface tension is the key to achieving surface smoothness by fire polishing. The quartz fire head 3 of the device uses gas fuel for combustion, and the flow speed of the flame is related to the flow speed of the gas fuel. The quartz fire head 3 is used to polish the end plate 101 to be polished of the quartz boat 1, and the flow speed of the gas fuel on the side close to the polishing surface in the quartz fire head 3 is smaller than that on the side away from the polishing surface. Because there is a certain difference in the flow speed of the gas, there is also a difference in the gas pressure. Due to the Bernoulli principle, that is, the flow speed is inversely proportional to the pressure, the air flow speed in the lower area with a larger diameter is relatively slow, while the air flow speed in the upper area with a smaller diameter is relatively fast. The pressure on the side with slow gas flow is greater than that on the side with fast gas flow. The gas fuel on the side with slow gas flow will move toward the side with fast flow, making the flame convergent. The convergent flame shape can transfer heat to the quartz glass surface more concentratedly, reducing heat loss and thermal impact on the surrounding environment. This flame shape helps to quickly melt the glass surface and improve polishing efficiency. At the same time, because the flame flow speed on the side in contact with the polishing surface is slower and more moderate, the softness of the flame is crucial to the polishing effect. Soft flame contact can ensure that the heat is evenly distributed on the polishing surface, avoiding local overheating or surface defects, and the soft flame produces During melting, the interference to the molten layer is small, which avoids the formation of white lines due to excessively fast air flow speed when the molten layer is cooled. At the same time, the flame temperature is controlled to avoid extreme conditions of being too high or too low. A downward light source is arranged above the end plate 101 of the quartz boat 1, and a light and shadow detection component 22 is arranged below the end plate 101. Because the surface of the end plate 101 is uneven, a shadow area will be formed when the light source is projected downward. The shadow area can be identified, and the uneven area can be quickly located, thereby improving the polishing quality. The wavelength of the projected light source is different from the flame wavelength, so that even during the flame polishing process, the interference caused by the flame wavelength on the shadow identified by the light and shadow detection component 22 is reduced.

[0038] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0039] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. An automatic fire-polishing machine for the surface of a quartz boat, comprising a polishing base (2) and a quartz fire head (3), wherein the polishing base (2) is provided with a support frame (21) for placing the quartz boat (1), and when placed, the end plates (101) at both ends of the quartz boat (1) are located outside the support frame (21), and a connecting rod (102) for connecting the two end plates (101) is located inside, and the quartz fire head (3) uses gas fuel for combustion, characterized in that: A light and shadow detection component (22) capable of identifying a projected shadow area is arranged at the bottom of the outer side of the support frame (21); a light source having a wavelength different from the wavelength of the flame during the flame polishing process is arranged above the outer side of the support frame (21); the light source is directed downward so that the surface to be polished of the end plate (101) of the quartz boat (1) can be projected onto the light and shadow detection component (22); the quartz fire head (3) is used to polish the surface to be polished of the end plate (101) of the quartz boat (1); the flame of the quartz fire head (3) is concentrated, and the flow speed of the gas fuel on the side of the quartz fire head (3) close to the polishing surface is smaller than that on the side away from the polishing surface.

2. The automatic fire polishing machine for the surface of a quartz boat according to claim 1, characterized in that: A circularly distributed wick (31) is vertically arranged inside the quartz burner (3), and gas fuel is sprayed out from the wick (31).

3. The automatic fire polishing machine for the surface of a quartz boat according to claim 2, characterized in that: The wick (31) is divided into two parts, left and right, from the central axis. The end of the wick (31) on one side is in an outward expansion shape, so that the diameter of the wick (31) increases, and the end of the wick (31) on the other side is in an inward contraction shape, so that the diameter of the wick (31) decreases.

4. The automatic fire polishing machine for quartz boat surface according to claim 2, characterized in that: The diameter of the end of the wick (31) gradually shrinks from one side of the cross-section to the other side.

5. The automatic fire polishing machine for quartz boat surface according to claim 1, characterized in that: The top of the support frame (21) is provided with a downwardly recessed arc-shaped groove (23) for accommodating the connecting rod (102).

6. The automatic fire polishing machine for the surface of a quartz boat according to claim 5, characterized in that: The arc-shaped groove (23) is provided with an air outlet (231).

7. The automatic fire polishing machine for the surface of a quartz boat according to claim 6, characterized in that: The support frame (21) is directly connected to the polishing base (2) via a screw rod (24), and the screw rod (24) is driven by a motor.

8. An automatic fire polishing machine for the surface of a quartz boat according to any one of claims 1 to 7, characterized in that: The light and shadow detection component (22) is provided with a filter capable of filtering the wavelength of flames.