A novel radio frequency chip test structure, preparation method and application thereof
By using aluminum metal layer and passivation layer in the RF chip test structure, a high-precision circuit detection unit is solved, and the problems of wear and insufficient accuracy of traditional PCB test substrate probes are achieved, and the use of probes with longer life and improvements are achieved. Low cost high-precision testing.
Patent Information
- Application Number
- CN202411273887.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-12
AI Technical Summary
The metal layer of the traditional PCB test substrate is relatively thick, which leads to severe wear of the probe, short service life, and cannot meet the chip testing needs of smaller pin spacing. At the same time, the cost of high-precision PCB test substrate is relatively high.
Aluminum metal layer is adopted, with a thickness controlled between 1-5um, and a gap is formed with a passivation layer to construct a circuit detection unit, including a pin connection, a needle opening and transmission part, the transmission part is set to a 50ohm impedance line, and the substrate material is high resistance Silicon or glass substrates form metal and passivation layers through sputtering or evaporation processes, and control line width and line spacing to achieve higher accuracy.
It extends the service life of the probe, realizes testing of smaller pin pitch chips, reduces the cost of the test substrate, and has higher accuracy.
Smart Images

Figure CN118800764B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of chip test structures, and in particular to a novel radio frequency chip test structure, a preparation method and application thereof. Background Art
[0002] PCB test substrate is also called printed circuit board substrate. At present, the test substrates in the RF industry are all PCB substrates. By coating copper and printing circuits on substrates such as epoxy resin, the chip is placed on it and the exposed pins are pierced through probes (generally including GSG probes, GS probes, SG probes, etc.) to achieve conduction test. However, the defects of traditional PCB test substrates are:
[0003] a. The metal layer is made of copper foil or electroplated copper, which is thicker, usually more than ten microns. Based on the material and thickness of copper, the entire metal layer is relatively hard, which causes serious wear on the probe. The probe generally needs to be replaced after about half a year, and its service life is extremely short. At the same time, the PCB test substrate has low precision and the seams do not meet the requirements. At present, the minimum line width and line spacing requirement of conventional precision PCB test substrates is 75um, which cannot be applied to the latest module integrated chip testing with ultra-small pin pitch;
[0004] b. The current mainstream solution is to use a high-precision PCB test board supplemented by gold plating to soften the surface, but the cost of this high-precision PCB test substrate is very high, generally costing no less than 150 yuan per square centimeter.
[0005] Starting from the metal layer, this application combines the structure and process to develop a new type of RF chip test structure, preparation method and application to solve the problems existing in the prior art. Summary of the invention
[0006] The purpose of the present invention is to provide a novel radio frequency chip test structure, a preparation method and its application, so as to solve the problem of serious wear of the probe by the PCB test substrate during the application process in the prior art, and further overcome the problem that the PCB test substrate cannot test chips with smaller pin spacing.
[0007] The technical solution of the present invention is: a novel radio frequency chip test structure, comprising a substrate, a metal layer and a passivation layer;
[0008] At least one metal layer is provided, the metal layer is made of aluminum, and the thickness of each metal layer is 1-5 um;
[0009] The passivation layer is formed on each of the metal layers, and the local area where the passivation layer is aligned with the metal layer is peeled off or etched to form a gap, so that the adjacent metal layers are connected, and a detection position is formed on the top layer to expose the metal layer;
[0010] The circuit detection unit is constructed to include a pin connection part, a needle insertion part, and a transmission part; the pin connection part is used to connect to the pin of the chip to be tested, and the needle insertion part is used for the probe to be inserted and turned on; the transmission part connects the pin connection part and the needle insertion part, and is constructed as an impedance line, and the target characteristic impedance is 50ohm.
[0011] Preferably, the minimum spacing between adjacent pin connecting portions is less than 15 um.
[0012] Preferably, the substrate is made of a material with an isotropic dielectric constant.
[0013] Preferably, a passivation layer is formed between the substrate and the metal layer, and the passivation layer directly formed on the substrate is used to adjust the dielectric constant of the substrate;
[0014] The thickness of the passivation layer formed on the metal layer is 0.5-3 um.
[0015] Preferably, the metal layer is primed with titanium, and the thickness of the titanium is 5-100 nm.
[0016] Preferably, the passivation layer is made of any one of silicon nitride and silicon dioxide; and / or,
[0017] The substrate is any one of a high-resistance silicon substrate and a glass substrate.
[0018] Preferably, the target characteristic impedance of the transmission part is 50 ohm, and under the condition of constant relative dielectric constant of the substrate, the line width of the transmission part is positively correlated with the line seam;
[0019] Under the condition that the line width of the transmission part is constant, the dielectric constant of the substrate is positively correlated with the size of the line gap of the transmission part.
[0020] The present invention also discloses a method for preparing a novel radio frequency chip test structure, and the preparation method is as follows:
[0021] S1. Select a substrate, the substrate material can be any one of high-resistance silicon and glass substrate;
[0022] S2, forming a 1-5 um metal base on the substrate by sputtering or evaporation process, and forming a metal layer with a pattern on the metal base by stripping or etching process;
[0023] S3. A sputtering or evaporation process is used in combination with a stripping or etching process to form a passivation layer with a pattern on the surface of the metal layer. The passivation layer is made of any one of silicon nitride and silicon dioxide.
[0024] Preferably, after step S1 is completed, a passivation layer is first formed on the substrate by sputtering or evaporation, and the passivation layer directly formed on the substrate is used to adjust the dielectric constant of the substrate.
[0025] The invention further discloses an application of a novel radio frequency chip testing structure in chip detection.
[0026] Compared with the prior art, the advantages of the present invention are:
[0027] (1) The present invention is applied to chip detection, and combined with the semiconductor manufacturing process, the thickness of the metal layer in the test structure can be controlled between 1-5um. The metal layer is made of aluminum, and combined with the thin and soft characteristics of the metal layer, the wear on the probe during the test is small, and the service life of the probe is longer. At the same time, the limit of the metal line width is also correlated with the thickness of the metal layer. By reducing the thickness of the metal layer, it is possible to form a metal layer with a smaller line width and line spacing by matching the process.
[0028] (2) The circuit detection unit formed by the structure includes a pin connection part, a needle insertion part, and a transmission part. Among them, the pin connection part has the highest requirement for precision. The test structure of the present application can achieve narrower line width and line seam based on the preparation process, and the narrowest can be on the order of microns. It can be used for chip testing with smaller pin spacing. Compared with the line seam condition of about 75um of the traditional PCB test substrate, it has more significant advantages; at the same time, the transmission part has the greatest impact on the final test accuracy. By controlling the target characteristic impedance of the transmission part, the final test requirements can be met.
[0029] (3) The metal layer is primed with titanium, which can improve the connectivity of the metal layer. At the same time, the thickness of titanium is controlled between 5-100 nm, which will not have a significant impact on the thickness of the overall metal layer and can still make the metal layer meet the thin and soft characteristics.
[0030] (4) The test structure formed through the preparation process has a lower cost for the entire structure. Taking a 6-inch wafer as an example, the cost can be controlled within 20 yuan per square centimeter. Combined with its precision advantage and less wear on the probe, it has significant advantages over traditional PCB test substrates. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] The present invention will be further described below in conjunction with the accompanying drawings and embodiments:
[0032] Figure 1 A cross-sectional view of a novel radio frequency chip test structure according to Embodiment 1 of the present invention;
[0033] Figure 2 This is a schematic diagram of a novel radio frequency chip test structure according to Embodiment 1 of the present invention;
[0034] Figure 3This is a schematic diagram of the distribution of the pin connection part, the needle insertion part, and the transmission part in a novel radio frequency chip test structure according to Example 1 of the present invention;
[0035] Figure 4 A schematic diagram of the spacing between a pair of pin connection parts in a novel radio frequency chip test structure according to Embodiment 1 of the present invention;
[0036] Figure 5 A diagram showing the relationship between the line width of a metal layer and a line seam in a novel radio frequency chip test structure according to Embodiment 1 of the present invention;
[0037] Figure 6 A cross-sectional view of a novel radio frequency chip test structure according to Embodiment 2 of the present invention;
[0038] Figure 7 A diagram showing the relationship between the relative dielectric constants of a seam and a substrate in a novel radio frequency chip test structure according to Embodiment 2 of the present invention;
[0039] Figure 8 A cross-sectional view of a stacked structure formed according to a process sequence of a novel radio frequency chip test structure according to Embodiment 3 of the present invention;
[0040] Fig. 9 A cross-sectional view of a stacked structure corresponding to the function of a novel radio frequency chip test structure described in Example 3 of the present invention;
[0041] Fig.10 This is a cross-sectional view of a new type of radio frequency chip test structure described in Example 4 of the present invention.
[0042] Wherein: 1. substrate;
[0043] 2. Metal layer, 21. First metal layer, 22. Second metal layer, 23. Third metal layer, 2a. Ground layer, 2b. Signal layer;
[0044] 3. passivation layer, 31. first passivation layer, 32. second passivation layer, 33. third passivation layer;
[0045] 4. Notch, 5. Pin connection part, 6. Needle insertion part, 7. Transmission part. DETAILED DESCRIPTION
[0046] The present invention is further described in detail below in conjunction with specific embodiments: Example 1
[0047] A method for preparing a novel radio frequency chip test structure, the preparation method is as follows:
[0048] S1. Select the substrate, the substrate material is high-resistance silicon;
[0049] S2. A metal base of 1-5um is formed on the substrate by sputtering or evaporation process, and a metal layer with a pattern is formed on the metal base by lift-off process or etching process. The metal layer can also be primed with titanium to improve the connectivity of the metal layer. The thickness of titanium is controlled between 5-100nm, which has little effect on the overall thickness of the metal layer.
[0050] S3. A sputtering or evaporation process is used in combination with a stripping or etching process to form a passivation layer with a graphic appearance on the surface of the metal layer. The passivation layer uses silicon nitride, and the thickness of the passivation layer is controlled between 0.5-3um.
[0051] Of course, in other embodiments, the substrate may also be a glass substrate, and the passivation layer may also be silicon dioxide.
[0052] Based on the preparation method of the new RF chip test structure, a new RF chip test structure is obtained, such as Figure 1 As shown, it includes a substrate 1, a metal layer 2 and a passivation layer 3.
[0053] The substrate 1 is made of a material with isotropic dielectric constant, such as silicon, which has a high resistivity and avoids leakage. Of course, a glass substrate can also be used. In this embodiment, the substrate is made of high-resistance silicon, whose relative dielectric constant is 11.9.
[0054] The metal layer 2 is provided with one layer, and the metal layer is made of aluminum with a thickness of 1-5um. In the present application, based on the adopted preparation process, aluminum can be used to form the metal layer. The thin and soft aluminum can ensure that the wear on the probe is small during the test process, and the service life of the probe is longer.
[0055] It should be noted that the metal layer of the traditional PCB test substrate generally uses harder and thicker copper instead of aluminum because the surface of aluminum is easily oxidized, resulting in poor contact. However, in this application, even if the surface of the thinner metal layer is slightly oxidized, it is relatively soft and the probe used in the test process has a pointed head. Therefore, during the actual measurement process, the pointed head can pierce the surface and penetrate into the metal layer, and thus the problem of poor contact will not occur.
[0056] The passivation layer 3 is formed on the metal layer 2. The local area where the passivation layer 3 is aligned with the metal layer 2 is peeled off or etched to form a notch 4, forming a detection position, so that the corresponding area of the metal layer 2 is exposed.
[0057] like Figure 2 , Figure 3 As shown, the circuit detection unit is constructed to include a pin connection portion 5 , a needle piercing portion 6 , and a transmission portion 7 .
[0058] The pin connection part 5 is used to connect to the pin of the chip to be tested, so the distribution of the pin connection part 5 needs to be compatible with the pin distribution of the chip; as the current chip precision becomes higher and higher, the chip pin spacing gradually decreases, and at this time the spacing between the pin connection parts 5 also needs to be reduced, and the accuracy requirement is higher. Through the preparation method of the new RF chip test structure in this application, the spacing between the pin connection parts 5 can be less than 15um. For the spacing between the pin connection parts 5, please refer to Figure 4 As shown, the distance L is the width of the grounding metal between a pair of pin connectors 5, and the distance S corresponding to the blank area is the line spacing, so the distance between the edges of a pair of pin connectors 5 is 2S+L. Using the preparation method of the present application, the spacing 2S+L between the pin connectors 5 can be less than 15um. At the same time, the limit of the metal line width and line spacing is also related to the thickness of the metal layer. Only by thinning the thickness of the metal layer can the manufacturing process be matched to achieve a smaller line width and line spacing. In this application, based on the thinner thickness of the metal layer and the manufacturing process, the test of the latest module integrated chip with ultra-small pin pitch is met.
[0059] The puncture part 6 is for the probe to pierce and conduct. The probe pierces the metal layer 2. Since the thickness of the metal layer 2 can be controlled between 1-5um and the metal layer is made of aluminum, the metal layer 2 can be made relatively thin and soft. The wear on the probe is small during the test, and the service life of the probe is longer. The transmission part 7 connects the pin connection part 5 and the puncture part 6. Due to the distribution of the pin connection part 5, the distance of the transmission part 7 is generally set to be longer, and it is constructed as an impedance line, which has the greatest impact on the accuracy of the final test result. Its target characteristic impedance needs to be controlled at 50ohm.
[0060] During the application process, the pin connection part 5 has the highest precision requirement, which needs to ensure that the chip pins can be brought out without interference; the precision requirement of the needle insertion part 6 is relatively low, as long as it ensures that there is no short circuit after the probe is inserted; the transmission part 7 has the greatest impact on the final test results, and the test structure needs to meet the impedance and resistance requirements to ensure the final test performance. The transmission part 7 is an impedance line with a target characteristic impedance of 50ohm. Under a constant relative dielectric constant (high-resistance silicon substrate, relative dielectric constant of 11.9), the line width corresponding to the transmission part 7 is positively correlated with the line seam.
[0061] The specific relationship between line width and seam can be referred to Figure 5 And Table 1:
[0062] Table 1: Relationship between metal layer line width and line gap under constant relative dielectric constant:
[0063]
[0064] Therefore, by controlling the line width and line seam of the transmission part 7, the target impedance of the transmission part 7 can be adjusted to meet the requirement of the target characteristic impedance of 50ohm and ensure the final test performance; at the same time, the line width and line seam of the transmission part 7 can also meet higher precision requirements.
[0065] Based on the above, it can be found that the new RF chip test structure provided by the present invention can achieve narrower line widths and line gaps compared to traditional PCB test substrates, with the narrowest being on the order of microns, and can be used for chip testing with smaller pin pitches.
[0066] During the test, the chip is placed on the passivation layer, the pins of the chip are connected to the pin connection part 5, and the probe is inserted into the needle insertion part 6 to achieve conduction between the chip and the test structure, thereby completing the test of the chip.
[0067] The advantages of adopting the solution of the present application, based on the preparation process of the test structure and the soft and thin characteristics of the metal layer, are: first, the wear on the probe can be greatly reduced; second, higher precision can improve the performance consistency of the test substrate; third, it can be used for chip testing with smaller pin spacing; fourth, the cost is greatly reduced. Example 2
[0068] Since different chips need to be tested using substrates with different dielectric constants, in this embodiment, a passivation layer (also called a dielectric layer) is first formed on the substrate to adjust the dielectric constant of the substrate.
[0069] Specifically, a method for preparing a novel radio frequency chip test structure is as follows:
[0070] S1. Select the substrate, the substrate material is high-resistance silicon;
[0071] S2, forming a passivation layer on the substrate by sputtering or evaporation process to adjust the dielectric constant of the substrate;
[0072] S3, forming a 1-5 um metal base on the substrate by sputtering or evaporation process, and combining a lift-off process or an etching process to form a metal layer with a pattern on the metal base;
[0073] S4. A sputtering or evaporation process is used in combination with a stripping or etching process to form a passivation layer with a graphic appearance on the surface of the metal layer. The passivation layer uses silicon nitride, and the thickness of the passivation layer is controlled between 0.5-3um. Of course, in other embodiments, the passivation layer can also use silicon dioxide.
[0074] like Figure 6 As shown, a novel radio frequency chip test structure includes a substrate 1, a first passivation layer 31, a metal layer 2 and a second passivation layer 32.
[0075] The first passivation layer 31 is used to adjust the dielectric constant of the substrate 1 .
[0076] The metal layer 2 is made of aluminum and has a thickness of 1-5 um.
[0077] The second passivation layer 32 covers the metal layer 2 , and its main function is to form a protective film on the metal surface to reduce corrosion. It is very thin, dense, and has good covering properties, and can be firmly adsorbed on the surface of the metal layer 2 .
[0078] Since the dielectric constant of the substrate in this embodiment can be adjusted through the first passivation layer 31, the target characteristic impedance of the transmission part 7 in the metal layer 2 is set to 50ohm. Under the condition of a constant line width of the transmission part 7 (line width = 150um), the adjustment of the line seam design parameters can be achieved by adjusting the relative dielectric constant.
[0079] Through a large number of experiments, it is found that the relationship between the relative dielectric constant of the seam and the substrate can be referred to Figure 7 and Table 2:
[0080] Table 2: Relationship between the relative dielectric constant of the line gap and the substrate under the condition of constant line width
[0081]
[0082] From the above, it can be found that under the condition that the line width of the transmission part 7 is constant, the dielectric constant of the substrate 1 is positively correlated with the size of the line gap of the transmission part 7. By reducing the dielectric constant, the line gap can be made less than 10um. Example 3
[0083] In the present application, in different application scenarios, multiple metal layers can also be used to implement chip testing. In this embodiment, three metal layers are used.
[0084] Specifically, Figure 8 As shown, a new type of RF chip test structure, according to the preparation and molding process, its structure includes a substrate 1, three metal layers 2 and a passivation layer 3, the thickness of the first metal layer 21, the second metal layer 22, and the third metal layer 23 are all controlled between 1-5um, and the thickness of the first passivation layer 31, the second passivation layer 32, and the third passivation layer 33 are controlled between 0.5-3um; each metal layer 2 and passivation layer 3 are formed into a specific graphic appearance by a process. The new type of RF chip test structure corresponding to the three metal layers can realize high-isolation multiplexer testing, combined with Fig. 9 As shown, it includes a ground layer 2a for grounding and a signal layer 2b for signal transmission. Example 4
[0085] like Fig.10As shown, a novel radio frequency chip test structure includes a substrate 1, a metal layer 2 and a passivation layer 3; the metal layer 2 is provided with three layers, and a passivation layer 3 is formed on each metal layer 2. In the preparation method, a passivation layer 3 is first formed on the substrate 1 to adjust the dielectric constant of the substrate.
[0086] In summary, the present invention is applied to chip detection, combined with the semiconductor manufacturing process, so that the thickness of the metal layer in the test structure can be controlled between 1-5um, and the metal layer is made of aluminum, combined with the thin and soft characteristics of the metal layer, the wear on the probe during the test process is small, and the service life of the probe is longer. At the same time, the accuracy of the entire test structure is higher, and narrower line widths and line seams can be achieved, the narrowest can be in the micron level, and can be used for chip testing with smaller pin spacing; and the test structure formed by the manufacturing process has a lower cost for the entire structure.
[0087] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with this technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the scope of protection of the present invention. For those skilled in the art, it is obvious that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is limited by the attached claims rather than the above description, and it is intended to include all changes within the meaning and scope of the equivalent elements of the claims in the present invention.
Claims
1. A new type of radio frequency chip test structure, characterized in that: It comprises a substrate (1), a metal layer (2) and a passivation layer (3); At least one metal layer (2) is provided, the metal layer (2) is made of aluminum, and the thickness of each metal layer (2) is 1-5 um; The passivation layer (3) is formed on each metal layer (2), and a local area where the passivation layer (3) is aligned with the metal layer (2) is peeled off or etched to form a notch (4), so that the adjacent metal layers (2) are connected, and a detection position is formed on the top layer, so that the metal layer (2) is exposed; The circuit detection unit is constructed to include a pin connection portion (5), a needle insertion portion (6), and a transmission portion (7); the pin connection portion (5) is used to connect to the pin of the chip to be tested, and the needle insertion portion (6) is used for the probe to be inserted and turned on; the transmission portion (7) connects the pin connection portion (5) and the needle insertion portion (6), and is constructed as an impedance line, and the target characteristic impedance is 50 ohm.
2. A novel radio frequency chip test structure according to claim 1, characterized in that: The minimum spacing between adjacent pin connection portions (5) is less than 15 um.
3. A novel radio frequency chip test structure according to claim 2, characterized in that: The substrate (1) is made of a material with an isotropic dielectric constant.
4. A novel radio frequency chip test structure according to claim 3, characterized in that: A passivation layer (3) is also formed between the substrate (1) and the metal layer (2), and the passivation layer (3) directly formed on the substrate (1) is used to adjust the dielectric constant of the substrate (1); The thickness of the passivation layer (3) formed on the metal layer (2) is 0.5-3 um.
5. The novel radio frequency chip test structure according to claim 1, characterized in that: The metal layer (2) is based on titanium, and the thickness of the titanium is 5-100 nm.
6. The novel radio frequency chip test structure according to claim 1, characterized in that: The passivation layer (3) is made of any one of silicon nitride and silicon dioxide; and / or, The substrate (1) is any one of a high-resistance silicon substrate and a glass substrate.
7. The novel radio frequency chip test structure according to claim 2, characterized in that: The target characteristic impedance of the transmission part (7) is 50 ohm; When the relative dielectric constant of the substrate (1) is constant, the line width of the transmission portion (7) is positively correlated with the line gap; Under the condition that the line width of the transmission portion (7) is constant, the dielectric constant of the substrate (1) is positively correlated with the size of the line gap of the transmission portion (7).
8. A method for preparing a novel radio frequency chip test structure according to any one of claims 1 to 7, characterized in that: The preparation method is as follows: S1. Select a substrate, the substrate material can be any one of high-resistance silicon and glass substrate; S2, forming a 1-5 um metal base on the substrate by sputtering or evaporation process, and forming a metal layer with a pattern on the metal base by stripping or etching process; S3. Sputtering or evaporation combined with a stripping or etching process is used to form a passivation layer with a graphic appearance on the surface of the metal layer, and the passivation layer is made of any one of silicon nitride and silicon dioxide.
9. The method for preparing a novel radio frequency chip test structure according to claim 8, characterized in that: After step S1 is completed, a passivation layer is first formed on the substrate by sputtering or evaporation. The passivation layer directly formed on the substrate is used to adjust the dielectric constant of the substrate.
10. Application of a novel radio frequency chip test structure as claimed in any one of claims 1 to 7 in chip detection.
Citation Information
Patent Citations
Sample applied to atomic force nano probe test and manufacturing method thereof
CN103364594A
Wafer acceptance test key for aluminum wire resistance
CN108831841A
Test disc and chip failure analysis test method
CN116338262A
Wafer packaging body capable of preventing aluminum crystal pad of chip from being damaged in probe detection operation
CN219998219U