Soldering system and method for providing reducing gas on soldering system

By using the catalyst's reducing gas conduit in the welding system, the problem of oxidation of semiconductor components and substrate conductive structures is solved, and the welding quality and efficiency are improved.

CN118805249APending Publication Date: 2024-10-18KULICKE & SOFFA IND INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380024582.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-08
Filing Date
2023-03-17
Publication Date
2024-10-18

Smart Images

  • Figure CN118805249A_ABST
    Figure CN118805249A_ABST
Patent Text Reader

Abstract

A seaming system is provided. The soldering system includes: (a) a soldering head assembly configured to transport a soldering tool for soldering a semiconductor element to a substrate; and (b) a reducing gas conduit for transporting reducing gas from (i) a reducing gas source to (ii) a seaming region of the seaming system. The reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering region. The reducing gas conduit contains a catalyst for generating excess reducing species in the reducing gas prior to the reducing gas reaching the seaming region.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to U.S. Provisional Application No. 63 / 328,771, filed on April 8, 2022, the contents of which are incorporated herein by reference. Technical Field

[0003] The present invention relates to welding (bonding) systems and processes, and more particularly, to an improved welding system and process for providing a reducing gas on the welding system. Background Art

[0004] Traditional semiconductor packaging generally involves a bare die attach process and a wire bonding process. Advanced semiconductor packaging techniques (e.g., flip chip bonding, thermocompression bonding, etc.) continue to gain attention in the industry. For example, in thermocompression bonding (TCB), heat and / or pressure (and sometimes ultrasonic energy) are used to form multiple interconnections between (i) conductive structures on a semiconductor element and (ii) conductive structures on a substrate.

[0005] In certain flip chip bonding or thermocompression bonding applications, the conductive structures of the semiconductor element and / or substrate may include copper structures (e.g., copper pillars) or other materials that are subject to oxidation and / or other contamination. In such applications, it is desirable to provide an environment suitable for bonding. Typically, such an environment may be provided by using a reducing gas in the bonding area to reduce potential oxidation and / or contamination of the conductive structures of the semiconductor element or substrate to be bonded.

[0006] It would therefore be desirable to provide improved welding systems, and methods of providing a reducing gas to welding systems. Summary of the invention

[0007] According to an exemplary embodiment, the present invention provides a welding system. The welding system includes: (a) a welding head assembly configured to transport a welding tool for welding a semiconductor element to a substrate; and (b) a reducing gas conduit for transporting a reducing gas from (i) a reducing gas source to (ii) a welding area of ​​the welding system. The reducing gas is configured to be used during welding of the semiconductor element to the substrate at the welding area. The reducing gas conduit includes a catalyst for generating an excess reducing substance in the reducing gas before the reducing gas reaches the welding area.

[0008] According to another exemplary embodiment of the present invention, another welding system is provided. The welding system includes: (a) a welding head assembly configured to transport a welding tool for welding a semiconductor element to a substrate; and (b) a reducing gas conduit for transporting a reducing gas from (i) a reducing gas source to (ii) a welding area of ​​the welding system. The reducing gas is configured to be used during welding of the semiconductor element to the substrate at the welding area. The reducing gas conduit includes a noble metal structure, the noble metal structure being arranged in at least one of the following: (a) a mesh configuration within the reducing gas conduit; (b) a perforated block configuration within the reducing gas conduit; and (c) a configuration covering an inner surface of the reducing gas conduit.

[0009] According to another exemplary embodiment of the present invention, another welding system is provided. The welding system includes: (a) a welding head assembly configured to transport a welding tool, the welding tool being used to weld a semiconductor element to a substrate; and (b) a reducing gas conduit, which is used to transport a reducing gas from (i) a reducing gas source to (ii) a welding area of ​​the welding system. The reducing gas is configured to be used during welding of the semiconductor element to the substrate at the welding area. The reducing gas conduit includes a catalyst, the catalyst being arranged in at least one of the following: (a) a mesh configuration within the reducing gas conduit; (b) a perforated block configuration within the reducing gas conduit; and (c) a configuration covering an inner surface of the reducing gas conduit.

[0010] According to another exemplary embodiment of the present invention, a method for providing a reducing gas on a soldering system is provided. The method includes the following steps: (a) providing a soldering tool for soldering a semiconductor component to a substrate; (b) conveying a reducing gas in a reducing gas conduit, the reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of the soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor component to the substrate at the soldering region; and (c) using a catalyst to generate an excess reducing substance in the reducing gas while the reducing gas is conveyed in the reducing gas conduit.

[0011] According to another exemplary embodiment of the present invention, another method for providing a reducing gas on a welding system is provided. The method includes the following steps: (a) setting up a welding tool for welding a semiconductor component to a substrate; (b) conveying a reducing gas in a reducing gas conduit, the reducing gas conduit extending between (i) a reducing gas source and (ii) a welding area of ​​the welding system, wherein the reducing gas is configured to be used during welding of the semiconductor component to the substrate at the welding area; and (c) when the reducing gas is conveyed in the reducing gas conduit, using a noble metal structure to generate excess reducing species in the reducing gas, the noble metal structure being arranged in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering an inner surface of the reducing gas conduit.

[0012] According to another exemplary embodiment of the present invention, another method for providing a reducing gas on a welding system is provided. The method includes the following steps: (a) providing a welding tool for welding a semiconductor component to a substrate; (b) conveying a reducing gas in a reducing gas conduit, the reducing gas conduit extending between (i) a reducing gas source and (ii) a welding area of ​​the welding system, wherein the reducing gas is configured to be used during welding of the semiconductor component to the substrate at the welding area; and (c) when the reducing gas is conveyed in the reducing gas conduit, using a catalyst to generate excess reducing species in the reducing gas, the catalyst being arranged in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering an inner surface of the reducing gas conduit.

[0013] The method of the present invention may also be embodied as an apparatus (eg, as part of the intelligence of a wire bonding machine) or as computer program instructions on a computer readable carrier (eg, a computer readable carrier containing a wire bonding program for use in connection with a wire bonding machine). BRIEF DESCRIPTION OF THE DRAWINGS

[0014] The following detailed description of the invention is best understood when read in conjunction with the accompanying drawings. It should be emphasized that, according to common practice, the various features of the drawings are not shown to scale. On the contrary, the dimensions of the various features are arbitrarily enlarged or reduced for clarity. The drawings include the following drawings:

[0015] Figures 1 to 4 is a block side view showing a welding system configured to provide a reducing gas to a welding area according to various exemplary embodiments of the present invention;

[0016] FIG. 5A to FIG. 5B and FIG. 6A to FIG. 6B is a block side view showing a welding system configured to provide a reducing gas to a welding area and a substrate oxide reduction chamber according to various exemplary embodiments of the present invention;

[0017] FIG. 7A to FIG. 7B is a cross-sectional side view of a portion of a reducing gas conduit showing a catalyst region according to various exemplary embodiments of the present invention;

[0018] FIG. 7C to FIG. 7E It is along Fig. 7A A cross-sectional view taken along line AA of FIG. 1 , showing an exemplary catalyst configuration according to various exemplary embodiments of the present invention;

[0019] Figure 8 is a cross-sectional side view of a portion of a reducing gas conduit in a serpentine configuration showing a catalyst region according to an exemplary embodiment of the present invention; and

[0020] Figures 9 to 11 are various flow charts of methods of providing a reducing gas on a welding system according to various exemplary embodiments of the present invention. DETAILED DESCRIPTION

[0021] According to an exemplary aspect of the invention, a reducing gas (e.g., formic acid vapor) helps reduce oxides from conductive structures of semiconductor components and conductive structures of substrates to which semiconductor materials are to be soldered. Examples of such conductive structures include conductive pads, conductive leads, conductive traces, and conductive pillars. Examples of materials in the conductive structures include copper, solder, silver-tin, indium-based solder, and the like.

[0022] Oxides from conductive structures can be reduced using a reducing gas by producing an intermediate metal formate species and by subsequent thermal decomposition into metal and other gaseous species. During solder-to-solder, solder-to-metal, and metal-to-metal interconnect bonding (e.g., thermocompression bonding), such processes typically require high temperatures (e.g., 200° C. to 300° C.) to reduce oxides.

[0023] According to certain exemplary embodiments of the present invention, the high temperature requirements for reducing oxides from the surface of the conductive structure can be reduced. For example, the exemplary method utilizes a reaction of a reducing gas (e.g., formic acid vapor) with a catalyst such as a noble metal (e.g., platinum, palladium, gold, etc.). In addition, this reaction can occur at an elevated temperature (e.g., 100° C. to 200° C.). Therefore, due to the catalytic conversion, excess reducing species (e.g., H+ ions) are produced in the reducing gas. The excess reducing species helps to further reduce oxides from the target surface (e.g., from the surface of the conductive structure of the semiconductor element and / or the surface of the substrate to which the semiconductor element will be soldered). The presence of these excess (additional) reducing species further reduces the temperature requirements during the soldering process (e.g., soldering the semiconductor element to the substrate).

[0024] An exemplary welding system according to the present invention may include one or more of the following: a reducing gas conduit for conveying reducing gas; a heater (e.g., an inline heater) for heating at least a portion of the reducing gas conduit (e.g., a catalyst region of the reducing gas conduit); a catalyst (e.g., a noble metal structure such as a mesh, a perforated block, or a covering such as a plating or coating, etc.) disposed in the reducing gas conduit. The temperature of the catalyst may be adjusted, for example, using a closed loop control.

[0025] Each of U.S. Patent No. 10,861,820 (titled “METHODS OF BONDING SEMICONDUCTORELEMENTS TO A SUBSTRATE, INCLUDING USE OF A REDUCING GAS, AND RELATED BONDING MACHINES”), U.S. Patent No. 11,205,633 (titled “METHODS OF BONDING SEMICONDUCTORELEMENTS TO SUBSTRATES, AND RELATED BONDING SYSTEMS”), and U.S. Patent Application Publication No. 2021 / 0265303 (titled “METHODS OF BONDING SEMICONDUCTOR ELEMENTS TO SUBSTRATE, AND RELATED BONDING SYSTEMS”) relates to welding systems using reducing gases, and the present invention references the above in their entireties and incorporates them into the present invention.

[0026] As used herein, the term "semiconductor element" is intended to refer to any structure that includes (or is configured to include in a subsequent step) a semiconductor chip or die. Exemplary semiconductor elements include: bare semiconductor die, semiconductor die on a substrate (e.g., lead frame, PCB, carrier, semiconductor chip, semiconductor wafer, BGA substrate, semiconductor element, etc.), packaged semiconductor device, flip chip semiconductor device, die embedded in a substrate, stack of semiconductor die, etc. In addition, the semiconductor element may include an element that is configured to be soldered to or otherwise included in a semiconductor package (e.g., spacers to be soldered in a stacked die configuration, substrate, etc.).

[0027] As used herein, the term "substrate" is intended to refer to any structure to which a semiconductor component may be soldered. Exemplary substrates include, for example, a lead frame, a PCB, a carrier, a module, a semiconductor chip, a semiconductor wafer, a BGA substrate, another semiconductor component, and the like.

[0028] As used herein, the term "catalyst" is intended to refer to a structure for generating excess reducing species in a reducing gas, for example, in a heated reducing gas conduit. Such a catalyst may be a noble metal structure formed of (or including) ruthenium (Ru), rhodium (Rh), palladium (Pd), iridium (Ir), platinum (Pt) and gold (Au). In addition, depending on the specific application, the catalyst may be formed of (or include) nickel, copper, silver or other suitable materials.

[0029] As used herein, the term "catalyst zone" refers to a portion of a reducing gas conduit (which is any type of tube, conduit or structure that contains reducing gas) that contains catalyst. The catalyst zone may extend along any portion of the length of the reducing gas conduit as required by the application.

[0030] As will be appreciated by those skilled in the art, the reducing gas (e.g., formic acid vapor) contains reducing species. Additional reducing species (also referred to as excess reducing species) are generated in the reducing gas by reaction with the catalyst (e.g., with heat). H+ ions are an example of such additional reducing species.

[0031] Now refer to the accompanying drawings, Figure 1 A welding system 100 is shown (e.g., a flip chip welding machine, a hot press welding machine, etc.). The welding system 100 includes a support structure 102 for supporting a substrate 104 (wherein the substrate 104 includes a plurality of conductive structures 104a) during a welding operation. The support structure 102 can include any suitable structure for a particular application. In the illustrated embodiment, the support structure 102 includes a top plate 102a (configured to directly support the substrate 104), a chuck 102c, and a heater 102b disposed between the top plate and the chuck.

[0032] The welding system 100 also includes a welding head assembly 106, which can be configured to move along (and around) multiple axes of the welding system 100, such as, for example, the x-axis, the y-axis, the z-axis, theta-axis (rotational axis), etc. The welding head assembly 106 contains and / or carries a heater 108 and a welding tool 110. In certain welding machines (e.g., a hot press welder), it may be necessary to heat the welding tool 110. Although Figure 1 A separate heater 108 is shown for heating the bonding tool 110 (for heating the semiconductor element 112 including the plurality of conductive structures 112a), it being understood that the heater 108 and the bonding tool 110 may be integrated into a single element (eg, a heated bonding tool).

[0033] In conjunction with the soldering operation, the semiconductor element 112 is soldered to the substrate 104 using the soldering tool 110. During the soldering operation, corresponding ones of the conductive structures 112a are soldered (e.g., using heat, force, ultrasonic energy, etc.) to corresponding ones of the conductive structures 104a. Figure 1 In FIG. 1 , the conductive structures 112 a include solder material 112 a 1 at a contact portion of each conductive structure 112 a (eg, a portion of the conductive structure 104 a configured to contact the substrate 104 ).

[0034] In certain soldering applications (e.g., thermocompression soldering, flip chip soldering, etc.), it is desirable to provide an environment suitable for soldering. Typically, such an environment can be provided by using a reducing gas in the soldering area to reduce potential oxides of the conductive structure of the semiconductor element or the substrate to which the semiconductor element is to be soldered.

[0035] exist Figure 1 In the embodiment of the present invention, the weld head assembly 106 carries a weld head manifold 114, which is used to receive and distribute fluids (e.g., gas, vapor, liquid, etc.) as required in a given application. Although the weld head manifold 114 is shown in a cross-sectional view, the actual weld head manifold 114 surrounds the welding tool 110 (e.g., the weld head manifold 114 surrounds the welding tool 110 in a coaxial configuration). Of course, the weld head manifold 114 can have a different Figure 1 Furthermore, it should be understood that certain details of the weld head manifold 114 are omitted for simplicity.

[0036] The welding head manifold 114 includes three channels 114a, 114b, and 114c with different functions. The outer channel 114a receives a shielding gas (e.g., nitrogen) from a shielding gas supply source (not shown). The shielding gas 128 is provided from the outer channel 114a of the welding head manifold 114 to protect the welding area 122 from the external environment. The inner channel 114c receives a reducing gas 130 (e.g., wherein the reducing gas 130 may be a saturated vapor, such as formic acid vapor, the reducing gas contains an excess reducing substance, etc.) via the reducing gas conduit 120, and provides the reducing gas 130 to the welding area 122 (e.g., wherein the welding area 122 is the location where the semiconductor element 112 is welded to the substrate 104).

[0037] The reducing gas 130 is provided by a reducing gas source 118 (via a reducing gas conduit 120). For example, the reducing gas source 118 can be a bubbler-type system containing an acidic fluid such as formic acid, acetic acid, or another acidic fluid (where the bubbler-type system can be part of the welding system 100). In another example, the reducing gas source 118 can be a container (e.g., a pressurized container such as a tank), or another source for directing the reducing gas 130 to the welding system 100.

[0038] The reducing gas conduit 120 is configured to transport the reducing gas 130 from the reducing gas source 118 to the soldering area 122 of the soldering system 100, wherein the reducing gas 130 is configured to be used during soldering of the semiconductor device 112 to the substrate 104 at the soldering area 122. Figure 1 In the illustrated embodiment, the reducing gas conduit 120 is configured to provide the reducing gas 130 to the welding head assembly 106 and / or the welding head manifold 114. The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.)) for generating excess reducing species (e.g., H+ ions) in the reducing gas 130 before the reducing gas 130 reaches the welding area 122. The catalyst can be arranged in a variety of different configurations (e.g., in Figure 7C The mesh configuration 120b1, Fig.7D The perforated block configuration 120b2, Fig. 7E The reducing gas 130 is delivered through the catalyst region 120a (i.e., where the catalyst is located) of the reducing gas conduit 120, thereby chemically reacting with the catalyst to produce excess reducing substances. A heater (e.g., an inline heater) may be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ).

[0039] After the reducing gas 130 is distributed in the welding area 122, the reducing gas 130 contacts the surface of each of the conductive structure 104a (of the substrate 104) and the conductive structure 112a (of the semiconductor element 112). The surface of the conductive structure 104a / 112a may then contain reaction products (e.g., where the reaction products are provided due to (i) surface oxides on the conductive structure 104a / 112a and (ii) the reducing gas 130 (and, if necessary, may be heated by the heater 108 and transferred to the conductive structure 104a via contact with the conductive structure 112a). Such reaction products are desirably removed from the welding area 122 using a vacuum provided through the central passage 114b of the weld head manifold 114 via the outlet tube 116).

[0040] See now Figure 2, which shows a soldering system 200. The soldering system 200 is similar in many respects to the soldering system 100, wherein similar components have the same component numbers or numbers beginning with "2" instead of "1" (unless otherwise explicitly stated). The soldering system 200 includes a support structure 202 for supporting the substrate 104. The support structure 202 includes a top plate 202a (configured to directly support the substrate 104), a chuck 202c, and a heater 202b disposed between the top plate and the chuck.

[0041] The welding system 200 also includes a welding head assembly 106, which can be configured to move along (and around) multiple axes of the welding system 200, such as, for example, an x-axis, a y-axis, a z-axis, a theta axis (rotational axis), etc. The welding head assembly 106 includes and / or carries a heater 108 and a welding tool 110. The welding tool 110 is shown carrying a semiconductor component 112 (including a plurality of conductive structures 112a, and the conductive structures 112a include welding material 112a1). The welding head assembly 106 is shown carrying a plate 107, which is used to partially contain at least one of a shielding gas 128 and a reducing gas 130.

[0042] The weld head manifold 114 (eg, Figure 1 On the contrary, Figure 2 A manifold 214 is shown carried by and / or integrated with the support structure 202. The manifold 214 is configured to receive and distribute fluids (e.g., gases, vapors, etc.) as desired in a given application. Although the manifold 214 is shown in cross-section, the actual manifold 214 at least partially surrounds the substrate 104. Of course, the manifold 214 may have a plurality of Figure 2 Furthermore, it should be understood that certain details of the manifold 214 are omitted for simplicity (e.g., details of interconnection with the reducing gas conduit 120, details of structures for distributing the reducing gas 130 within the manifold 214, details of structures for distributing the shielding gas 128 within the manifold 214, details of structures for evacuating the central passage 214b of the manifold 214, etc.).

[0043] The manifold 214 includes three channels 214a, 214b, 214c having different functions. The outer channel 214a receives a shielding gas 128 (e.g., nitrogen) from a shielding gas supply source (e.g., a nitrogen tank, a gas supply, etc.). The shielding gas 128 is provided from the outer channel 214a of the manifold 214 to protect the welding area 222 from the external environment. The inner channel 214c receives a reducing gas 130 via a reducing gas conduit 120 and provides the reducing gas 130 to the welding area 222 in conjunction with the welding operation. The reducing gas 130 is provided by the reducing gas source 118 and carried by the reducing gas conduit 120.

[0044] The reducing gas conduit 120 is configured to transport the reducing gas 130 from the reducing gas source 118 to the soldering area 222 of the soldering system 200, wherein the reducing gas 130 is configured to be used during soldering of the semiconductor device 112 to the substrate 104 at the soldering area 222. Figure 2 In the illustrated embodiment, the reducing gas conduit 120 is configured to provide the reducing gas 130 to the support structure 202 (e.g., via the manifold 214). The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.) for generating excess reducing species (e.g., H+ ions) in the reducing gas 130 before the reducing gas 130 reaches the welding area 222. The catalyst can be arranged in a variety of different configurations (e.g., in Figure 7C The mesh configuration 120b1, Fig.7D The perforated block configuration 120b2, Fig. 7E The reducing gas 130 is delivered through the catalyst region 120a (i.e., where the catalyst is located) of the reducing gas conduit 120, thereby chemically reacting with the catalyst to produce excess reducing substances. A heater (e.g., an inline heater) may be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ).

[0045] After the reducing gas 130 is distributed in the region of the semiconductor element 112 and the substrate 104, the reducing gas 130 contacts the surface of each of the conductive structures 104a and 112a. The surface of the conductive structures 104a / 112a may then contain reaction products (e.g., where the reaction products are provided as a result of: (i) surface oxides on the conductive structures 104a / 112a, and (ii) the reducing gas from the reducing gas 130, (and, if necessary, heat provided by the heater 108). Such reaction products are desirably removed from the soldering region (i.e., the region where the conductive structures 112a of the semiconductor element 112 are soldered to the corresponding conductive structures 104a of the substrate 104) using a vacuum provided through the central passage 214b of the manifold 214 via the outlet tube 216.

[0046] See now Figure 3 , which shows a welding system 300. The welding system 300 is similar in many respects to the Figure 1The soldering system 100 of the present invention is shown in the figure, wherein similar components have the same component number or a number beginning with "3" instead of "1" (unless otherwise explicitly stated). The soldering system 300 includes: a substrate source 300a (e.g., a wafer handler or other source) for providing a substrate 104 (e.g., a wafer, a printed circuit board, etc.) on a support structure 300a1; and a processing system 300b. The substrate 104 is configured to be transferred to the processing system 300b (e.g., including an internal environmental chamber 320, including a tunnel portion 302). The tunnel portion 302 includes a substrate oxidation protection chamber 302b and a soldering position 302c (which is a portion of the substrate oxidation protection chamber 302b). A reducing gas delivery system 308 (including a welding head manifold 114, as described herein) is also included in the processing system 300b. Within the processing system 300b (sometimes referred to as a main machine compartment), the internal environmental chamber 320 may include at least a portion of the substrate oxidation protection chamber 302b and the reducing gas delivery system 308.

[0047] The welding system 300 also includes a welding head assembly 106 that includes and / or carries a heater 108 and a welding tool 110. Figure 1 Details of an exemplary bond head assembly 106 are described. Figure 3 Also shown is a main exhaust 304 that extracts exhaust (e.g., gas, such as reducing gas vapor) from the processing system 300b or the internal environmental chamber 320 via conduit 304a and conduit 114b1 (where conduit 114b1 is directly or indirectly coupled to Figure 1 1 and 12. The weld head assembly 106 carries a weld head manifold 114 for receiving and distributing fluids (eg, gases, vapors, etc.) as required in a given application. The weld head manifold 114 receives a reducing gas 130 from a reducing gas source 118 via a reducing gas conduit 120.

[0048] exist Figure 3 In the example shown, the tunnel portion 302 includes an entrance door 302a1 (which closes the opening 302a1a). A substrate conveying system (which may be part of a material handling system, including the support structure 102) is used to convey the substrate 104 through the entrance door 302a1 to the substrate oxidation protection chamber 302b. The substrate oxidation protection chamber 302b includes an inert environment 306 (e.g., supplied by nitrogen, which is not shown in the figure for simplicity). The material handling system is used to move the substrate 104 in the substrate oxidation protection chamber 302b to the welding position 302c. When at the welding position 302c, the reducing gas 130 is provided by the reducing gas delivery system 308. The reducing gas 130 is provided by the reducing gas source 118 and transported by the reducing gas conduit 120.

[0049] The reducing gas conduit 120 is configured to deliver the reducing gas 130 from the reducing gas source 118 to a welding region (e.g., including the welding position 302c) of the welding system 300, wherein the reducing gas 130 is configured to be used during welding of the semiconductor device 112 to the substrate 104 at the welding region. Figure 3 In the illustrated embodiment, the reducing gas conduit 120 is configured to provide the reducing gas 130 to the welding head assembly 106 and / or the welding head manifold 114. The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.)) for generating excess reducing species (e.g., H+ ions) in the reducing gas 130 before the reducing gas 130 reaches the welding area. The catalyst can be arranged in a variety of different configurations (e.g., in Figure 7C The mesh configuration 120b1, Fig.7D The perforated block configuration 120b2, Fig. 7E The reducing gas 130 is delivered through the catalyst region 120a (i.e., where the catalyst is located) of the reducing gas conduit 120, thereby chemically reacting with the catalyst to produce excess reducing substances. A heater (e.g., an inline heater) may be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ).

[0050] In conjunction with the soldering operation, the semiconductor component 112 (which is transported by the soldering head assembly 106 through the opening 302e into the tunnel portion 302) is soldered to the substrate 104 using the soldering tool 110. During the soldering operation, corresponding ones of the conductive structures of the semiconductor component 112 are soldered (e.g., using heat, force, ultrasonic energy, etc.) to corresponding ones of the conductive structures of the substrate 104. The soldering head manifold 114 provides a reducing gas 130 (e.g., the reducing gas can be a saturated vapor gas, such as formic acid vapor) in the region of the semiconductor component 112 and the substrate 104 in conjunction with the soldering operation (in the illustrated example, the reducing gas 130 can enter the tunnel portion 302 through the opening 302e). After the reducing gas 130 is distributed in the region of the semiconductor component 112 and the substrate 104, the reducing gas 130 contacts the surface of each of the conductive structures of the semiconductor component 112 and the substrate 104.

[0051] See now Figure 4 , which shows a welding system 400. The welding system 400 is similar in many respects to the Figure 2 The welding system 200 and Figure 3The welding system 400 is essentially the welding system 300, but has Figure 2 The manifold 214 (and associated structure) is replaced by Figure 1 The weld head manifold 114 (and related structure) is shown.

[0052] The soldering system 400 includes a substrate source 400a (e.g., a wafer handler or other source) for providing a substrate 104 (e.g., a wafer, a printed circuit board, etc.) on a support structure 400a1; and a processing system 400b. The substrate 104 is configured to be transferred to the processing system 400b (e.g., including an internal environmental chamber 420, including a tunnel portion 402). The tunnel portion 402 includes a substrate oxidation protection chamber 402b and a soldering position 402c (which is a portion of the substrate oxidation protection chamber 402b). Within the processing system 400b (sometimes referred to as a main machine compartment), the internal environmental chamber 420 may include at least a portion of the substrate oxidation protection chamber 402b and a reducing gas delivery system 408. The soldering system 400 also includes a solder head assembly 106, which includes and / or transports a heater 108 and a soldering tool 110. In conjunction with the soldering operation, the semiconductor element 112 (which is carried by the soldering tool 110 ) extends through the opening 402 e to be soldered to the substrate 104 .

[0053] exist Figure 4 In the example shown, the tunnel portion 402 includes an entry door 402a1 (which closes the opening 402a1a). A substrate transfer system (which may be part of a material handling system, including the support structure 102) is used to transfer the substrate 104 through the entry door 402a1 to the substrate oxidation protection chamber 402b. The substrate oxidation protection chamber 402b includes an inert environment 406 (e.g., supplied by nitrogen, which is not shown in the figure for simplicity). The material handling system is used to move the substrate 104 in the substrate oxidation protection chamber 402b to the welding position 402c.

[0054] The welding system 400 includes a main exhaust 404 that extracts exhaust gases (e.g., gases such as reducing gas vapor) through conduits 404a and 404b. The processing system 400b is similar to the processing system 300b, except that the processing system 400b includes a reducing gas delivery system 408 (including the manifold 214) instead of the reducing gas delivery system 308 (including the welding head manifold 114). The manifold 214 is configured to receive and distribute fluids (e.g., gases, vapors, etc.) as required in a given application. The manifold 214 receives the reducing gas 130 from the reducing gas source 118 via the reducing gas conduit 120.

[0055] The reducing gas conduit 120 is configured to deliver the reducing gas 130 from the reducing gas source 118 to a welding region (e.g., including the welding position 402c) of the welding system 400, wherein the reducing gas 130 is configured to be used during welding of the semiconductor device 112 to the substrate 104 at the welding region. Figure 4 In the illustrated embodiment, the reducing gas conduit 120 is configured to provide the reducing gas 130 to the support structure 102 (e.g., via the manifold 214 of the reducing gas delivery system 408). The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.) for generating excess reducing species (e.g., H+ ions) in the reducing gas 130 before the reducing gas 130 reaches the welding area. The catalyst can be arranged in a variety of different configurations (e.g., in Figure 7C The mesh configuration 120b1, Fig.7D The perforated block configuration 120b2, Fig. 7E The reducing gas 130 is delivered through the catalyst region 120a (i.e., where the catalyst is located) of the reducing gas conduit 120, thereby chemically reacting with the catalyst to produce excess reducing substances. A heater (e.g., an inline heater) may be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ).

[0056] See now Figure 5A , which shows a welding system 500. The welding system 500 includes: a substrate source 500a (e.g., a wafer handler or other source) for providing a substrate 104 (e.g., a wafer, a printed circuit board, etc.) on a support structure 500a1; and a processing system 500b. The substrate 104 is configured to be transferred to the processing system 500b (e.g., including a tunnel portion 502). The tunnel portion 502 includes: a substrate oxide reduction chamber 502a; a substrate oxidation protection chamber 502b; and a welding position 502c (which is a part of the substrate oxidation protection chamber 502b). A reducing gas delivery system 508 (including a welding head manifold 114, as described herein) is also included in the processing system 500b.

[0057] exist Figure 5A In the example shown, at least a portion of the substrate oxide reduction chamber 502a has a common boundary with the substrate oxidation protection chamber 502b. The substrate oxide reduction chamber 502a is closed using an entrance door 502a1 (which closes the opening 502a1a) and an exit door 502a2 (which closes the opening 502a2a). Another reducing gas delivery system 502d provides a reducing gas 130 (e.g., formic acid vapor) to the substrate oxide reduction chamber 502a. Figure 5AIn the example shown, reducing gas delivery system 508 and reducing gas delivery system 502d receive reducing gas from reducing gas source 118 .

[0058] After processing in the substrate oxide reduction chamber 502a (e.g., removing oxide from the conductive structure of the substrate 104), the substrate transfer system (which can be part of the material handling system including the support structure 102) is used to transfer the substrate 104 through the exit door 502a2 to the substrate oxidation protection chamber 502b. The substrate oxidation protection chamber 502b includes an inert environment 506 (e.g., supplied by nitrogen, which is not shown for simplicity). The material handling system (e.g., including the support structure 102) is used to move the substrate 104 in the substrate oxidation protection chamber 502b to the welding position 502c. When at the welding position 502c, the reducing gas 130 is provided by the reducing gas delivery system 508.

[0059] The welding system 500 also includes a welding head assembly 106, which includes and / or carries a heater 108 and a welding tool 110 (for a more detailed description of the welding head assembly 106, see Figure 1 ). Figure 5A Also shown is a main exhaust section 504, which draws exhaust gas (e.g., gas such as reducing gas vapor) through conduit 504a and conduit 114b1 (where conduit 114b1 is directly or indirectly coupled to Figure 1 The weld head assembly 106 carries a weld head manifold 114 that is used to receive and distribute fluids (eg, gas, steam, etc.) as desired in a given application.

[0060] The reducing gas conduit 120 is configured to deliver the reducing gas 130 from the reducing gas source 118 to (i) the reducing gas delivery system 508 (and / or the welding head manifold 114) and (ii) the reducing gas delivery system 502d. Thus, the reducing gas conduit 120 delivers the reducing gas 130 from the reducing gas source 118 to the welding area (e.g., including the welding position 502c) via the reducing gas delivery system 508. The reducing gas 130 is configured to be used during welding (e.g., thermocompression welding, flip chip welding, etc.) the semiconductor element 112 to the substrate 104. Figure 5A (and Figure 5B ), the reducing gas conduit 120 is also configured to deliver the reducing gas 130 to the substrate oxide reducing chamber 502a via the reducing gas delivery system 502d. The substrate oxide reducing chamber 502a is configured to receive the substrate 104 before soldering the semiconductor device 112 to the substrate 104.

[0061] The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.)) for generating excess reducing substances in the reducing gas 130 before the reducing gas 130 reaches the welding position 502c. The reducing gas 130 is transported through the catalyst region 120a (i.e., the location where the catalyst is located) of the reducing gas conduit 120, thereby chemically reacting with the catalyst to generate excess reducing substances. The heater may be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ). The heat provided by the heater can promote the chemical reaction that produces excess reducing species.

[0062] In conjunction with the soldering operation, the semiconductor component 112 (which is transported by the soldering head assembly 106 through the opening 502e into the tunnel portion 502) is soldered to the substrate 104 using the soldering tool 110. During the soldering operation, corresponding ones of the conductive structures of the semiconductor component 112 are soldered (e.g., using heat, force, ultrasonic energy, etc.) to corresponding ones of the conductive structures of the substrate 104. The soldering head manifold 114 provides a reducing gas 130 (e.g., the reducing gas is a saturated vapor gas) in the region of the semiconductor component 112 and the substrate 104 in conjunction with the soldering operation (in the illustrated example, the reducing gas 130 is able to enter the tunnel portion 502 through the opening 502e). After the reducing gas 130 is distributed in the region of the semiconductor component 112 and the substrate 104, the reducing gas 130 contacts the surface of each of the conductive structures of the semiconductor component 112 and the substrate 104.

[0063] Figure 5B A welding system 500' is shown. The welding system 500' is identical to the welding system 500, except that the welding system 500 shows multiple branches of the reducing gas conduit 120 (including multiple catalyst regions 120a) extending from the reducing gas source 118, while the welding system 500' shows a single reducing gas conduit 120 (including a single catalyst region 120a) extending from the reducing gas source 118 and then branching into two portions of the reducing gas conduit 120 (i.e., one branch of the reducing gas conduit 120 extends to the substrate oxide reduction chamber 502a, while the other branch of the reducing gas conduit 120 is connected to the manifold 214). Thus, the reducing gas 130 passes through the single catalyst region 120a in the welding system 500' and through multiple catalyst regions 120a in the welding system 500 while being delivered from the reducing gas source 118.

[0064] See now Fig. 6A , which shows a welding system 600. The welding system 600 is similar in many respects to the Figure 5A The welding system 500 and Figure 2 2 , wherein similar components have the same component numbers or numbers beginning with "6" instead of "5," "2," or "1" (unless otherwise expressly stated). Soldering system 600 is essentially soldering system 500, except that processing system 600b includes reducing gas delivery system 608 (including manifold 214 and associated structures) in place of reducing gas delivery system 508 (including weld head manifold 114 and associated structures) of processing system 500b. Soldering system 600 includes: a substrate source 600a (e.g., a wafer handler or other source) for providing a substrate 104 (e.g., a wafer, a printed circuit board, etc.) on a support structure 600a1. The substrate 104 is configured to be transferred to processing system 600b (e.g., including tunnel section 602). Tunnel section 602 (or other structure, as desired) includes: a substrate oxide reduction chamber 602a; a substrate oxidation protection chamber 602b; and a soldering station 602c (which is a portion of substrate oxidation protection chamber 602b).

[0065] exist Fig. 6A In the example shown, at least a portion of the substrate oxide reduction chamber 602a has a common boundary with the substrate oxidation protection chamber 602b. A reducing gas delivery system 608 is also included in the processing system 600b. The substrate oxide reduction chamber 602a is closed using an entrance door 602a1 (which closes the opening 602a1a) and an exit door 602a2 (which closes the opening 602a2a). Another reducing gas delivery system 602d (which is shown as being indirectly interconnected with the reducing gas delivery system 608 to use a common reducing gas source, i.e., the reducing gas source 118) provides a reducing gas 130 (e.g., formic acid vapor) in the substrate oxide reduction chamber 602a. After processing in the substrate oxide reduction chamber 602a (e.g., removing oxide from the conductive structure of the substrate 104), a substrate conveying system (which can be part of a material handling system including the support structure 102) is used to convey the substrate 104 through the opening 602a2a to the substrate oxidation protection chamber 602b. The substrate oxidation protection chamber 602b includes an inert environment 606 (e.g., supplied by nitrogen, which is not shown for simplicity). A material handling system (e.g., including the support structure 102) is used to move the substrate 104 in the substrate oxidation protection chamber 602b to the welding position 602c. When at the welding position 602c, the reducing gas 130 is provided by the reducing gas delivery system 608.

[0066] Fig. 6A Also shown is a welding head assembly 106, which contains and / or carries a heater 108 and a welding tool 110 (see also FIG. Figure 1 In conjunction with the soldering operation, the soldering tool 110 is capable of transporting the semiconductor component 112 through the opening 602e. Fig. 6AAlso shown is a main exhaust 604 that draws exhaust (eg, gases such as reducing gas vapor) through conduit 604a and conduit 604b. Manifold 214 is configured to receive and distribute fluids (eg, gases, vapors, etc.) as required in a given application.

[0067] The reducing gas conduit 120 is configured to carry the reducing gas 130 from the reducing gas source 118 to the reducing gas delivery system 608 and then to the bonding area (e.g., including the bonding location 602c), wherein the reducing gas 130 is configured to be used during bonding (e.g., thermocompression bonding, flip chip bonding, etc.) of the semiconductor element 112 to the substrate 104. Fig. 6A (and Figure 6B ), the reducing gas conduit 120 is configured to deliver the reducing gas 130 to the substrate oxide reduction chamber 602a (which is configured to receive the substrate 104) before the semiconductor element 112 is welded to the substrate 104. In addition, the reducing gas conduit 120 is configured to deliver the reducing gas 130 to the support structure 102 (e.g., via the manifold 214). The reducing gas conduit 120 includes a catalyst (e.g., wherein the catalyst is formed of or includes at least one noble metal (e.g., platinum, palladium, gold, etc.)) that is used to produce excess reducing substances in the reducing gas 130 before the reducing gas 130 reaches the welding position 602c. The reducing gas 130 is delivered through the catalyst region 120a of the reducing gas conduit 120 (i.e., the location where the catalyst is located), thereby chemically reacting with the catalyst to produce excess reducing substances. The heater can be used in conjunction with the reducing gas conduit 120, and more specifically, in conjunction with the catalyst region 120a (e.g., see FIG. 7A to FIG. 7B and Figure 8 ). The heat provided by the heater can promote the chemical reaction that produces excess reducing species.

[0068] Figure 6B A welding system 600' is shown. The welding system 600' is identical to the welding system 600, except that the welding system 600 shows multiple branches of the reducing gas conduit 120 (including multiple catalyst regions 120a) extending from the reducing gas source 118, while the welding system 600' shows a single reducing gas conduit 120 (including a single catalyst region 120a) extending from the reducing gas source 118 and then branching into two portions of the reducing gas conduit 120 (i.e., one branch of the reducing gas conduit 120 extends to the substrate oxide reduction chamber 602a, while the other branch of the reducing gas conduit 120 is connected to the manifold 214). Thus, the reducing gas 130 passes through the single catalyst region 120a in the welding system 600' and through multiple catalyst regions 120a in the welding system 600 while being delivered from the reducing gas source 118.

[0069] See now Fig. 7A , showing a cross-section of a portion of an exemplary reducing gas conduit 120 (e.g., wherein FIG. 7A to FIG. 7B and Figure 8 The reducing gas conduit 120 and FIG. 7C to FIG. 7E The catalyst configuration shown in is an example of a reducing gas conduit 120 illustrated and described throughout this application. The reducing gas conduit 120 includes a catalyst region 120a1 (which may extend along any portion of the reducing gas conduit 120 as desired in a particular application). The catalyst region 120a1 includes a catalyst 120b. The catalyst 120b is housed within the reducing gas conduit 120 and may be constructed in a variety of different configurations (e.g., see Figure 7C Mesh configuration 120b1, Fig.7D The perforated block configuration 120b2 and Fig. 7E The reducing gas conduit 120 further includes a heater 120c. The heater 120c is shown as a block diagram, which is connected to the reducing gas conduit 120 and more specifically to the catalyst region 120a1. Fig. 7A In the embodiment, the heater 120c is configured to heat the catalyst 120b to a temperature (e.g., 100°C, 150°C, 200°C) that helps produce excess reducing species in the reducing gas. The heater 120c can be used to control the temperature, for example, using closed loop control (e.g., simultaneously measuring the temperature for controlling the heating).

[0070] See now Figure 7B , showing a cross-section of a portion of another exemplary reducing gas conduit 120. The reducing gas conduit 120 includes a catalyst region 120a2. The catalyst region 120a2 includes a catalyst 120b. The catalyst 120b is contained within the reducing gas conduit 120 and can be constructed in a variety of different configurations (e.g., see Figure 7C Mesh configuration 120b1, Fig.7D The perforated block configuration 120b2 and Fig. 7E The reducing gas conduit 120 further includes a heater 120d (or a plurality of heaters). Fig. 7A In contrast to heater 120c in FIG. 1 , heater 120d is shown as an inline heater connected to catalyst region 120a2. Figure 7B In the embodiment, heater 120d is configured to heat catalyst 120b to a temperature (e.g., 100°C, 150°C, 200°C) that helps produce excess reducing species in the reducing gas. Heater 120d can be used to control temperature, for example, using closed loop control (e.g., simultaneously measuring temperature for controlling heating).

[0071] As described above, the reducing gas conduit 120 Fig. 7AThe catalyst region 120a1 (or Figure 7B The catalyst 120a2) and the catalyst 120b can be arranged in a variety of different configurations. Examples of such catalyst configurations are FIG. 7C to FIG. 7E Display (such as Fig. 7A AA). According to certain exemplary embodiments of the present invention, the entire structure of the catalyst can be formed of a noble metal. In other exemplary embodiments, the structure of the catalyst can include a noble metal (e.g., a noble metal coating on another structure).

[0072] See Figure 7C , showing a mesh configuration 120b1 of a catalyst 120b. In this embodiment, the catalyst 120b (e.g., formed of or including a noble metal) is formed into a staggered structure having openings to allow a reducing gas (e.g., reducing gas 130) to flow through the reducing gas conduit 120. This embodiment is expected to provide a catalyst with a large surface area to interact with the reducing gas.

[0073] See now Fig.7D , showing a perforated block configuration 120b2 of a catalyst 120b. In this configuration, the catalyst 120b (eg, formed of or including a noble metal) is formed into a structure having a plurality of through slots (or orifices) to allow a reducing gas to flow therethrough.

[0074] See now Fig. 7E , showing the inner surface configuration 120b3 of the catalyst 120b. In this configuration, the catalyst 120b is disposed on the inner surface of the reducing gas conduit 120. This configuration can provide a smaller surface area (with a smaller surface area) that can interact with the reducing gas. FIG. 7C to FIG. 7D configuration) but allows for a larger reducing gas flow rate.

[0075] It should be understood that these configurations are exemplary in nature and are not intended to limit the configuration of the catalyst to the examples shown. For example, a combination of one or more configurations (e.g., a combination of a mesh configuration 120b1 and an inner surface configuration 120b3) and one or more materials may be contemplated.

[0076] See now Figure 8 , showing a cross-section of a portion of the reducing gas conduit 120 in a "meandering configuration." The reducing gas conduit 120 includes a catalyst region 120a3 (including a catalyst 120b) and a heater 120c. In certain applications, a "meandering configuration" may be desirable. For example, such a configuration provides a more efficient use of space in a welding system. In addition, such a configuration provides a circuitous path for the reducing gas, allowing the reducing gas to better interact with the catalyst 120b (e.g., by increasing surface area, increasing the duration of flow through the conduit, increasing the non-laminar flow of the reducing gas, increasing the friction between the reducing gas and the catalyst, etc.). Although Figure 8 A "serpentine configuration" is shown, but the invention is not limited thereto (e.g., alternative configurations include spirals / helices, right-angle turn joints, return branches (to increase turbulence), etc.). A circuitous path configuration may include FIG. 7C to FIG. 7E One or more of the configurations illustrated and described in the above.

[0077] Figures 9 to 11 is a flow chart showing various methods of providing a reducing gas on a welding system. As will be appreciated by those skilled in the art: certain steps contained in the flow chart may be omitted; certain additional steps may be added; and the order of the steps may be altered from that shown, all within the scope of the present invention.

[0078] See now Fig. 9 At step 902, a soldering tool for soldering a semiconductor element to a substrate is provided (e.g., see soldering tool 110, semiconductor element 112, and substrate 104 throughout the figures). At step 904, a reducing gas is transported in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of the soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering region (e.g., see reducing gas 130, reducing gas conduit 120, reducing gas source 118, and soldering region throughout the figures). At step 906, excess reducing species (e.g., H+ ions) are generated in the reducing gas using a catalyst (e.g., the catalyst is formed of or includes at least one noble metal, such as platinum, palladium, gold, etc.) while the reducing gas is transported in the reducing gas conduit (e.g., the reducing gas 130 passes through catalyst region 120a and thus includes excess reducing species, as shown throughout the various figures). During step 906, a heating element (e.g., an inline heater, Fig. 7A The heater 120c, Figure 7B The catalyst may be heated by heating the catalyst 120d, etc. Such heating may improve the chemical process associated with the generation of excess reducing species.

[0079] In optional step 908, a reducing gas is provided to a weld head assembly that carries the welding tool, and the reducing gas is provided to the welding area via the weld head assembly (e.g., see Figure 1 , Figure 3 and FIG. 5A to FIG. 5B In optional step 910, a reducing gas is provided to a support structure for supporting the substrate, and the reducing gas is provided to the welding area via the support structure (eg, see Figure 2 , Figure 4 and FIG. 6A to FIG. 6B In optional step 912, reducing gas is passed through a reducing gas conduit (eg, see FIG. 5A to FIG. 5B and FIG. 6A to FIG. 6B ) is provided to a substrate oxide reduction chamber of a soldering system, and before soldering the semiconductor element to the substrate, the substrate is received at a soldering area via the substrate oxide reduction chamber.

[0080] See now Fig.10 At step 1002, a soldering tool for soldering a semiconductor component to a substrate is provided (e.g., see soldering tool 110, semiconductor component 112, and substrate 104 throughout the drawings). At step 1004, a reducing gas is delivered in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of the soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor component to the substrate at the soldering region (e.g., see reducing gas 130, reducing gas conduit 120, reducing gas source 118, and soldering region throughout the drawings). In step 1006, when the reducing gas is transported in the reducing gas conduit, an excess reducing species (e.g., H+ ions) is generated in the reducing gas using a noble metal structure (e.g., a catalyst formed of or including at least one noble metal, such as platinum, palladium, gold, etc.), the noble metal structure being arranged in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering the inner surface of the reducing gas conduit (e.g., see FIG. 7C to FIG. 7E ).

[0081] See now Fig.11 At step 1102, a soldering tool for soldering a semiconductor component to a substrate is provided (e.g., see soldering tool 110, semiconductor component 112, and substrate 104 throughout the drawings). At step 1104, a reducing gas is delivered in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of the soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor component to the substrate at the soldering region (e.g., see reducing gas 130, reducing conduit 120, reducing gas source 118, and soldering region 122 throughout the drawings). In step 1106, while the reducing gas is transported in the reducing gas conduit, excess reducing species (e.g., H+ ions) are generated in the reducing gas using a catalyst (e.g., the catalyst is formed of or includes at least one noble metal, such as platinum, palladium, gold, etc.), the catalyst being disposed in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering the inner surface of the reducing gas conduit (e.g., see FIG. 7C to FIG. 7E ).

[0082] Although the invention is illustrated and described herein with reference to specific embodiments, the invention is not intended to be limited to the details shown, but rather various modifications may be made to the details within the scope and range of equivalents of the claims and without departing from the invention.

Claims

1. A welding system, comprising: a bonding head assembly configured to carry a bonding tool for bonding a semiconductor element to a substrate; as well as A reducing gas conduit for conveying reducing gas from (i) a reducing gas source to (ii) a soldering area of ​​a soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering area, and the reducing gas conduit includes a catalyst for generating excess reducing species in the reducing gas before the reducing gas reaches the soldering area.

2. The welding system according to claim 1, wherein: The catalyst comprises a noble metal.

3. The welding system according to claim 1, wherein: The reducing gas conduit is configured to provide the reducing gas to the welding head assembly that carries the welding tool.

4. The welding system according to claim 1, wherein: The reducing gas conduit is configured to provide the reducing gas to a support structure for supporting the substrate.

5. The welding system according to claim 1, wherein: The reducing gas conduit comprises a heating element.

6. The welding system according to claim 1, wherein: The excess reducing species comprises H+ ions.

7. The welding system according to claim 1, wherein: The catalyst is disposed in a mesh configuration in the reducing gas conduit.

8. The welding system according to claim 1, wherein: The catalyst is disposed in the reducing gas conduit in a perforated block configuration.

9. The welding system according to claim 1, wherein: The catalyst is disposed on an inner surface of the reducing gas conduit.

10. The welding system according to claim 1, wherein: The reducing gas conduit is further configured to deliver the reducing gas to a substrate oxide reduction chamber configured to receive the substrate prior to soldering the semiconductor component to the substrate.

11. A welding system, comprising: a bonding head assembly configured to carry a bonding tool for bonding a semiconductor element to a substrate; as well as A reducing gas conduit for conveying reducing gas from (i) a reducing gas source to (ii) a welding area of ​​a welding system, wherein the reducing gas is configured for use during welding of the semiconductor element to the substrate at the welding area, the reducing gas conduit comprising a precious metal structure, the precious metal structure being arranged in at least one of: (a) a mesh configuration within the reducing gas conduit; (b) a perforated block configuration within the reducing gas conduit; and (c) a configuration covering an inner surface of the reducing gas conduit.

12. The welding system according to claim 11, wherein: The noble metal structure is a catalyst for generating excess reducing species in the reducing gas.

13. The welding system according to claim 12, wherein: The excess reducing species comprises H+ ions.

14. The welding system according to claim 11, wherein: The reducing gas conduit is configured to provide the reducing gas to the welding head assembly that carries the welding tool.

15. The welding system according to claim 11, wherein: The reducing gas conduit is configured to provide the reducing gas to a support structure for supporting the substrate.

16. The welding system of claim 11, wherein: The reducing gas conduit comprises a heating element.

17. The welding system of claim 11, wherein: The reducing gas conduit is further configured to deliver the reducing gas to a substrate oxide reduction chamber configured to receive the substrate prior to soldering the semiconductor component to the substrate.

18. A welding system comprising: a bonding head assembly configured to carry a bonding tool for bonding a semiconductor element to a substrate; as well as A reducing gas conduit for conveying reducing gas from (i) a reducing gas source to (ii) a welding area of ​​a welding system, wherein the reducing gas is configured for use during welding of the semiconductor element to the substrate at the welding area, the reducing gas conduit comprising a catalyst, the catalyst being arranged in at least one of: (a) a mesh configuration within the reducing gas conduit; (b) a perforated block configuration within the reducing gas conduit; and (c) a configuration covering an inner surface of the reducing gas conduit.

19. The welding system of claim 18, wherein: The catalyst comprises a noble metal.

20. The welding system of claim 18, wherein: The reducing gas conduit is configured to provide the reducing gas to the welding head assembly that carries the welding tool.

21. The welding system of claim 18, wherein: The reducing gas conduit is configured to provide the reducing gas to a support structure for supporting the substrate.

22. The welding system of claim 18, wherein: The reducing gas conduit comprises a heating element.

23. The welding system of claim 18, wherein: The catalyst is used to generate excess reducing species in the reducing gas.

24. The welding system of claim 23, wherein: The excess reducing species comprises H+ ions.

25. The welding system of claim 18, wherein: The reducing gas conduit is further configured to deliver the reducing gas to a substrate oxide reduction chamber configured to receive the substrate prior to soldering the semiconductor component to the substrate.

26. A method for providing a reducing gas in a welding system, the method comprising the steps of: (a) providing a soldering tool for soldering a semiconductor element to a substrate; (b) conveying a reducing gas in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of a soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering region; and (c) using a catalyst to generate excess reducing substances in the reducing gas while the reducing gas is transported in the reducing gas conduit.

27. The method according to claim 26, wherein: The catalyst comprises a noble metal.

28. The method of claim 26, further comprising the step of providing the reducing gas to a weld head assembly that carries the welding tool, the reducing gas being provided to the welding area via the weld head assembly.

29. The method of claim 26, further comprising the step of providing the reducing gas to a support structure for supporting the substrate, the reducing gas being provided to the welding area via the support structure.

30. The method of claim 26, wherein: Step (c) comprises heating the catalyst with a heater.

31. The method of claim 26, wherein: The excess reducing species produced in step (c) comprises H+ ions.

32. The method of claim 26, wherein: The catalyst is disposed in a mesh configuration in the reducing gas conduit.

33. The method of claim 26, wherein: The catalyst is disposed in the reducing gas conduit in a perforated block configuration.

34. The method of claim 26, wherein: The catalyst is disposed on an inner surface of the reducing gas conduit.

35. The method of claim 26, further comprising step (d) of providing the reducing gas to a substrate oxide reduction chamber of the soldering system via the reducing gas conduit, and step (e) of receiving the substrate at the soldering area via the substrate oxide reduction chamber before soldering the semiconductor element to the substrate.

36. A method of providing a reducing gas in a welding system, the method comprising the steps of: (a) providing a soldering tool for soldering a semiconductor element to a substrate; (b) conveying a reducing gas in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of a soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering region; and (c) when the reducing gas is transported in the reducing gas conduit, an excess reducing substance is generated in the reducing gas using a precious metal structure, wherein the precious metal structure is arranged in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering the inner surface of the reducing gas conduit.

37. The welding system of claim 36, wherein: The noble metal structure is a catalyst for generating the excess reducing species in the reducing gas.

38. The welding system of claim 36, wherein: The excess reducing species comprises H+ ions.

39. The method of claim 36, further comprising the step of providing the reducing gas to a weld head assembly that carries the welding tool, the reducing gas being provided to the welding area via the weld head assembly.

40. The method of claim 36, further comprising the step of providing the reducing gas to a support structure for supporting the substrate, the reducing gas being provided to the welding area via the support structure.

41. The method of claim 36, wherein: Step (c) comprises heating the noble metal structure with a heater.

42. The method of claim 36, further comprising step (d) of providing the reducing gas to a substrate oxide reduction chamber of the soldering system via the reducing gas conduit, and step (e) of receiving the substrate at the soldering area via the substrate oxide reduction chamber before soldering the semiconductor element to the substrate.

43. A method of providing a reducing gas in a welding system, the method comprising the steps of: (a) providing a soldering tool for soldering a semiconductor element to a substrate; (b) conveying a reducing gas in a reducing gas conduit extending between (i) a reducing gas source and (ii) a soldering region of a soldering system, wherein the reducing gas is configured to be used during soldering of the semiconductor element to the substrate at the soldering region; and (c) when the reducing gas is transported in the reducing gas conduit, using a catalyst to produce excess reducing substances in the reducing gas, the catalyst is arranged in at least one of the following: (i) a mesh configuration within the reducing gas conduit; (ii) a perforated block configuration within the reducing gas conduit; and (iii) a configuration covering the inner surface of the reducing gas conduit.

44. The welding system of claim 43, wherein: The excess reducing species comprises H+ ions.

45. The method of claim 43, further comprising the step of providing the reducing gas to a weld head assembly that carries the welding tool, the reducing gas being provided to the welding area via the weld head assembly.

46. ​​The method of claim 43, further comprising the step of providing the reducing gas to a support structure for supporting the substrate, the reducing gas being provided to the welding area via the support structure.

47. The method of claim 43, wherein: Step (c) comprises heating the catalyst with a heater.

48. The method of claim 43, further comprising step (d) of providing the reducing gas to a substrate oxide reduction chamber of the soldering system via the reducing gas conduit, and step (e) of receiving the substrate at the soldering area via the substrate oxide reduction chamber before soldering the semiconductor element to the substrate.