Method and device for efficient resourceful treatment of overhaul slag

The wet roller ball milling method is used to treat overhaul slag, which solves the problems of environmental pollution and resource waste, realizes the extraction and resource utilization of lithium elements, reduces pollution and energy consumption, and improves safety and efficiency.

CN118808307APending Publication Date: 2024-10-22STATE POWER INVESTMENT GRP NINGXIA ENERGY ALUMINUM TECH ENG CO LTD

Patent Information

Application Number
CN202411122988.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

Overhaul slag is produced during the production process of electrolytic aluminum. It contains highly toxic substances and the resource utilization value is not fully utilized, resulting in environmental pollution and resource waste.

Method used

The wet drum ball milling method is used to crush and grind the overhaul slag, and catalytic and harmless agents are added to react. The reaction is strengthened by the mechanical force of the ball mill, and the lithium element and other valuable components are extracted to reduce pollution and realize resource utilization.

Benefits of technology

It effectively reduces secondary pollution during the disposal process, improves operating safety, shortens the process flow, extracts lithium elements, improves resource utilization, and saves energy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808307A_ABST
    Figure CN118808307A_ABST
Patent Text Reader

Abstract

The invention provides an efficient resourceful treatment method and device for overhaul slag. The method comprises the steps that the overhaul slag is fed into a crusher to be crushed to be smaller than 40 meshes, then crushed overhaul slag particles are fed into a wet-process roller ball mill, a catalytic reaction agent is added, after a reaction is conducted for a period of time, a harmless agent is added, and after the reaction is finished, the overhaul slag is recycled. And the undersize slurry is settled, filtered and separated to obtain a filtrate and a harmless filter cake. And adjusting the pH value of the filtrate, adding a lithium extraction reaction agent, and carrying out stirring reaction, sedimentation, filtration and drying to obtain a lithium-containing filter cake and a new filtrate. According to the method, the overhaul slag aluminum ash is treated through a wet method, secondary pollution in the treatment process can be effectively reduced, the operation safety coefficient is increased, and the technological process is shortened. According to the method, mechanical stirring is replaced with wet ball milling, the reaction and leaching effect is enhanced, the reaction is more sufficient, the reaction time is shortened, the lithium element can be extracted, and the resource utilization effect is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of environmentally friendly solid waste treatment, and in particular to a method for efficiently resource-based treatment of overhaul slag. Background Art

[0002] Overhaul slag is the waste slag produced by the maintenance and replacement of the cathode lining of the electrolytic cell during the production of electrolytic aluminum. It is mainly composed of waste cathode carbon blocks, waste refractory materials, waste cathode steel bars and cathode ash. The cathode carbon blocks are immersed in the high-temperature molten salt system for a long time, resulting in a large amount of fluoride in the electrolyte penetrating into the cathode lining. my country is the world's largest producer of electrolytic aluminum. According to statistics, about 15 to 25 kg of overhaul slag is produced for every ton of aluminum produced. Because it contains highly toxic cyanide, fluoride and other toxic substances that seriously affect the ecological environment and human health, overhaul slag solid waste is classified as industrial hazardous waste (waste code 321-023-48) in the latest environmental management.

[0003] Overhaul slag contains a variety of components, which are seriously harmful while also having potential resource utilization value. Among them, the carbonaceous component content accounts for about 30% to 70%, the fluoride component content accounts for about 30% to 50%, and others also contain cyanide, aluminum oxide, iron oxide and other aluminum silicate substances. The fluorine in the overhaul slag mainly exists in the form of crystals NaF, CaF2 and Na3AlF6. When piled in the open air, the F ions will penetrate into the ground with natural rainwater, causing great harm to the environment; the cyanide in the overhaul slag is easily soluble in water, and will dissolve in a humid environment and then diffuse into the body of plants and animals, decomposing CN - In addition, with the development and application of lithium-containing medium- and low-grade bauxite in recent years, the content of Li in alumina, the raw material for electrolytic aluminum, has increased. During the electrolysis process, it penetrates into the tank lining with the electrolyte and gradually accumulates. The concentration of Li in some overhaul slag can reach 1.0-2.7% (in terms of Li + The Li element is active in nature and is not suitable for direct discharge, but it is widely used and can be used to manufacture lithium-ion batteries. Therefore, the harmless treatment and resource utilization of aluminum electrolysis overhaul slag are of great significance. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a method for efficiently disposing overhaul slag in a resource-saving manner, the method comprising the following steps:

[0005] Step 1: Send the overhaul slag into the crusher and crush it into particles below 40 mesh.

[0006] Step 2: conveying the crushed overhaul slag particles into a wet drum ball mill, wherein the wet drum ball mill is pre-loaded with grinding balls and water;

[0007] Step 3: Add catalytic reaction reagents into the wet drum ball mill and react for a period of time.

[0008] Step 4: Add harmless agent to the wet drum ball mill, react for a period of time, and collect and treat the gas generated by the reaction.

[0009] Step 5: After the reaction is completed, the grinding balls and the slurry are separated by screening, and the grinding balls are returned to the ball mill for reuse. The slurry is separated by sedimentation and filtration to obtain a primary filtrate and a harmless filter cake.

[0010] Step 6: The primary filtrate is transported to a lithium extraction reaction tank, the pH value of the primary filtrate is adjusted with an alkaline solution, and the precipitate is separated into a solid-liquid state to obtain a secondary filtrate and a precipitate containing aluminum hydroxide.

[0011] Step 7: Add lithium extraction reaction reagent to the secondary filtrate, and obtain filter cake and tertiary filtrate after stirring reaction, sedimentation, filtration and drying. The filter cake mainly contains lithium.

[0012] In some embodiments, sending the overhaul slag into the crusher in step 1 includes allowing the overhaul slag to pass through a box crusher, a jaw crusher, and a first drum ball mill in sequence.

[0013] In some more specific embodiments, the particle size of the overhaul slag after being crushed by a box crusher is controlled at 30-50 mm, the particle size of the overhaul slag after being crushed by a jaw crusher is controlled at 5-30 mm, and the overhaul slag after being ground by the first drum ball mill is passed through a 40-mesh vibrating screen to obtain overhaul slag particles smaller than 40 mesh.

[0014] In some embodiments, the proportion of the water pre-installed in step 2 is 40% to 200% of the mass ratio of the overhaul slag, and the temperature is 25° C. to 100° C.

[0015] In some embodiments, the grinding balls pre-installed in step 2 are one or more of zirconium oxide balls, aluminum oxide balls, and iron balls, and the amount of grinding balls added is 50% to 200% of the mass ratio of the overhaul slag.

[0016] In some embodiments, in steps 2-4, the rotation speed of the wet drum ball mill is 30 r / min to 120 r / min.

[0017] In some embodiments, in step 3, the reaction time is 0.5 h to 5 h.

[0018] In some embodiments, the catalytic reaction agent added in step 3 is one or more of sulfuric acid, aluminum sulfate, aluminum nitrate, and calcium chloride, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

[0019] In some embodiments, in step 4, the reaction time is 0.5 h to 5 h.

[0020] In some embodiments, the harmless agent added in step 4 can be one or more of calcium chloride, calcium hypochlorite, hydrogen peroxide, and sodium hydroxide, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

[0021] In some embodiments, in step 4, after adding the harmless agent, the wet ball mill is sealed with a cover at both ends, and the cover is provided with an exhaust port. The gas generated by the reaction is discharged from the exhaust port, and then absorbed and decontaminated with dilute sulfuric acid before being emptied.

[0022] In some embodiments, the alkaline solution in step 6 is sodium hydroxide solution or ammonia water.

[0023] In some more specific embodiments, the concentration of sodium hydroxide solution is 0.5% to 2%, and the concentration of ammonia water is 5% to 15%.

[0024] In some embodiments, the lithium extraction reaction reagent in step 7 is one or more of sodium carbonate, magnesium carbonate, and potassium carbonate, and the added amount is 1% to 10% of the mass ratio of the overhaul slag, and the filter cake contains lithium carbonate.

[0025] In some embodiments, in step 7, the reaction time is 0.5 h to 5 h.

[0026] In some embodiments, in step 7, the lithium-containing filter cake is dried by one of paddle drying, spray drying, and flash drying.

[0027] On the other hand, the present invention also provides a device for efficiently disposing overhaul slag in a resource-saving manner, which can be used to perform the above-mentioned method, and the device includes the following components:

[0028] Crusher unit is used to crush overhaul slag into particles below 40 mesh.

[0029] The wet drum ball mill is used to mix and react the crushed overhaul slag particles with water, grinding balls and reagents; the reagents include catalytic reaction reagents and harmless reagents added successively.

[0030] The screening device is used to separate the grinding balls and slurry remaining after the reaction in the wet drum ball mill; the remaining grinding balls are returned to the ball mill for reuse.

[0031] The filter is used to settle and filter the slurry screened by the screening device to obtain a primary filtrate and a harmless filter cake.

[0032] A lithium extraction reaction pool is used to adjust the pH value of the primary filtrate with an alkaline solution, separate the precipitate into solid and liquid, and obtain a secondary filtrate and a precipitate containing aluminum hydroxide; and to react the secondary filtrate with a lithium extraction agent, and the product of the reaction is filtered and dried to obtain a filter cake and a tertiary filtrate, wherein the filter cake contains lithium.

[0033] The present invention adopts wet method to treat overhaul slag aluminum ash, which can effectively reduce secondary pollution in the disposal process, improve the operation safety factor, and shorten the process flow. The present invention adopts wet ball milling instead of mechanical stirring to strengthen the reaction and leaching effect, make the reaction more complete, shorten the reaction time, and can also extract lithium elements, thereby improving the resource utilization effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0035] Figure 1 A process flow chart for efficiently resource-based disposal of overhaul slag provided by the present invention is shown. DETAILED DESCRIPTION

[0036] The solution provided in this specification is described below in conjunction with the accompanying drawings.

[0037] In order to make the purpose, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be described below in conjunction with the accompanying drawings.

[0038] In the description of the embodiments of the present application, words such as "exemplary", "for example" or "for example" are used to indicate examples, illustrations or descriptions. Any embodiment or design described as "exemplary", "for example" or "for example" in the embodiments of the present application should not be interpreted as being more preferred or more advantageous than other embodiments or designs. Specifically, the use of words such as "exemplary", "for example" or "for example" is intended to present related concepts in a concrete way.

[0039] In the description of the embodiments of the present application, the term "and / or" is merely a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B may represent: A exists alone, B exists alone, and A and B exist at the same time. In addition, unless otherwise specified, the term "plurality" means two or more.

[0040] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. The terms "include", "comprises", "has" and their variations all mean "including but not limited to", unless otherwise specifically emphasized.

[0041] The present invention provides a method for efficiently disposing of overhaul slag in a resource-based manner. The method accelerates the harmless reaction process of the overhaul slag by a wet chemical ball milling process, and further adds a catalyst, a reactant, etc. to extract valuable elements in the overhaul slag. While disposing of the overhaul slag in a harmless manner, effective resources in the overhaul slag are utilized to solve the problem that a large amount of waste overhaul slag generated in aluminum industry production is difficult to efficiently dispose of and effectively utilize as a resource.

[0042] The following is a further explanation of the overhaul slag disposal method provided by the present invention in conjunction with the accompanying drawings. A flow chart of a method for efficiently recycling overhaul slag provided by the present invention is shown in FIG. Figure 1 As shown, the method comprises the following steps:

[0043] Step 1: Send the overhaul slag into the crusher and crush it into particles below 40 mesh.

[0044] In some embodiments, sending the overhaul slag into the crusher in step 1 includes allowing the overhaul slag to pass through a box crusher, a jaw crusher, and a first drum ball mill in sequence.

[0045] In some more specific embodiments, the particle size of the overhaul slag after being crushed by a box crusher is controlled at 30-50 mm, the particle size of the overhaul slag after being crushed by a jaw crusher is controlled at 5-30 mm, and the overhaul slag after being ground by the first drum ball mill is passed through a 40-mesh vibrating screen to obtain overhaul slag particles smaller than 40 mesh.

[0046] The overhaul slag is fully crushed in this step so that the overhaul slag particles can fully contact and react with the solution during the subsequent wet treatment of the overhaul slag, thereby improving the treatment efficiency.

[0047] Step 2: conveying the crushed overhaul slag particles into a wet drum ball mill, wherein the wet drum ball mill is pre-loaded with grinding balls and water.

[0048] In some embodiments, the proportion of the water pre-installed in step 2 is 40% to 200% of the mass ratio of the overhaul slag, and the temperature is 25° C. to 100° C.

[0049] In some embodiments, the grinding balls pre-installed in step 2 are one or more of zirconium oxide balls, aluminum oxide balls, and iron balls, and the amount of grinding balls added is 50% to 200% of the mass ratio of the overhaul slag.

[0050] In some embodiments, in step 2, the rotation speed of the wet drum ball mill is 30 r / min to 120 r / min.

[0051] In this step, water is pre-added to the wet drum ball mill to facilitate the dissolution of the subsequent addition of catalytic reaction agents and harmless agents. This part of the pre-added water can be replaced by the subsequent 3rd filtrate, and recycled to improve resource output. The present invention uses wet ball milling to replace mechanical stirring. During the stirring process, the mechanical force of the ball mill is used to enhance the reaction and leaching effect. While the ball mill is crushing, the overhaul slag particles can also be further refined to make the reaction more complete, improve the leaching effect of the harmless reaction, shorten the reaction time, and greatly save energy in industrial production.

[0052] Step 3: Add catalytic reaction reagents into the wet drum ball mill and react for a period of time.

[0053] In some embodiments, in step 3, the reaction time is 0.5 h to 5 h.

[0054] In some embodiments, in step 3, the rotation speed of the wet drum ball mill is 30 r / min to 120 r / min.

[0055] In some embodiments, the catalytic reaction agent added in step 3 is one or more of sulfuric acid, aluminum sulfate, aluminum nitrate, and calcium chloride, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

[0056] The catalytic reaction agent starts to react with the overhaul slag after being added. The catalytic reaction agent can be used for the initial defluorination of the overhaul slag, and can also accelerate the subsequent harmless reaction and improve the treatment efficiency.

[0057] Step 4: Add harmless agent to the wet drum ball mill, react for a period of time, and collect and treat the gas generated by the reaction.

[0058] In some embodiments, in step 4, the reaction time is 0.5 h to 5 h.

[0059] In some embodiments, in step 4, the rotation speed of the wet drum ball mill is 30 r / min to 120 r / min.

[0060] In some embodiments, the harmless agent added in step 4 can be one or more of calcium chloride, calcium hypochlorite, hydrogen peroxide, and sodium hydroxide, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

[0061] In some embodiments, in step 4, after adding the harmless agent, the wet ball mill is sealed with a cover at both ends, and the cover is provided with an exhaust port. The gas generated by the reaction is discharged from the exhaust port, and then absorbed and decontaminated with dilute sulfuric acid before being emptied.

[0062] This step is mainly used to decontaminate the overhaul slag. In this step, the wet drum ball mill contains pre-loaded water, and the decontamination agents calcium chloride and calcium hypochlorite are added according to the ratio concentration requirements. They generate oxidizing hypochlorous acid and calcium ions in the solution. The hypochlorous acid completely oxidizes the cyanide in the overhaul slag into carbon dioxide and nitrogen, thereby removing the cyanide. Calcium ions combine with fluoride ions to form calcium fluoride precipitation, thereby further defluorinating the overhaul slag.

[0063] Step 5: After the reaction is completed, the grinding balls and the slurry are separated by screening, and the grinding balls are returned to the ball mill for reuse. The slurry is separated by sedimentation and filtration to obtain a primary filtrate and a harmless filter cake.

[0064] The harmless filter cake obtained in this step contains calcium fluoride and can be used as building materials.

[0065] Step 6: The primary filtrate is transported to a lithium extraction reaction tank, the pH value of the primary filtrate is adjusted with an alkaline solution, and the precipitate is separated into a solid-liquid state to obtain a secondary filtrate and a precipitate containing aluminum hydroxide.

[0066] In some embodiments, the alkaline solution in step 6 is sodium hydroxide solution or ammonia water.

[0067] In some more specific embodiments, the concentration of the sodium hydroxide solution is 0.5% to 2%, and the concentration of the ammonia solution is 5% to 15%.

[0068] In other embodiments, the alkaline solution in step 6 may also be an alkaline substance such as sodium bicarbonate, potassium hydroxide, sodium carbonate, etc.

[0069] Step 7: Add lithium extraction reaction reagent to the secondary filtrate, and obtain filter cake and tertiary filtrate after stirring reaction, sedimentation, filtration and drying. The filter cake mainly contains lithium.

[0070] In some embodiments, the lithium extraction reaction reagent in step 7 is one or more of sodium carbonate, magnesium carbonate, and potassium carbonate, and the added amount is 1% to 10% of the mass ratio of the overhaul slag, and the filter cake contains lithium carbonate.

[0071] In some embodiments, in step 7, the reaction time is 0.5 h to 5 h.

[0072] In some embodiments, in step 7, the lithium-containing filter cake is dried by one of paddle drying, spray drying, and flash drying.

[0073] The overhaul slag disposal method provided by the present invention is specifically described below in conjunction with embodiments.

[0074] Example 1

[0075] Take 1000kg of overhaul slag to be treated, add it to a box crusher, crush it to 30-50mm, then send it to a jaw crusher through a belt conveyor, crush it to 5-30mm, then send it to a drum ball mill through a belt conveyor, place a 40-mesh vibrating screen at the end of the drum ball mill, screen and obtain 1000kg of overhaul slag particles smaller than 40 mesh, and send it to a wet drum ball mill through a bucket elevator. Pre-add 1500kg of water to the wet drum ball mill (which can be supplemented to 1500kg by filtrate later), 2000kg of grinding steel balls, start the wet drum ball mill, and run it at a speed of 60r / min. First, add 50kg of catalytic reaction agent industrial concentrated sulfuric acid and 30kg of aluminum nitrate. After running for 30 minutes, add 80kg of harmless agent mixed with calcium chloride and calcium hypochlorite, and continue the reaction for 2h. The gas generated by the reaction is discharged from the exhaust port and absorbed by dilute sulfuric acid. After the reaction is completed, the mixture of slurry and grinding balls is poured into a screening machine, and through a 40-mesh sieve, about 2050 kg of grinding balls (a small amount of slurry is attached, and it is returned to the wet drum ball mill for continued use) and the slurry to be treated (2580 kg) are screened, and the slurry is transported to a belt filter for filtration to obtain 1620 kg of filter cake with a moisture content of 30% and 960 kg of primary filtrate. The filter cake is sent to a temporary storage warehouse for temporary storage, and the primary filtrate is transported to a reaction tank, and a 0.5% concentration of sodium hydroxide solution is gradually added to adjust the pH of the filtrate until white turbidity appears, and the pH value of the filtrate is adjusted with a 5% concentration of ammonia solution, and the precipitate (the precipitate is mainly aluminum hydroxide, about 1.3 kg) is filtered and separated to obtain a secondary filtrate. 8 kg of industrial sodium carbonate is added to the secondary filtrate, and stirred for 1 hour. After the reaction is complete, 8 kg of filter cake containing crude lithium carbonate and about 958 kg of the 3rd filtrate can be obtained by filtering. The first filtrate, the second filtrate and the third filtrate are sent to the evaporation crystallizer for 10 cycles each, and the evaporation liquid is continuously circulated after the salts therein are crystallized.

[0076] In summary, compared with the prior art, the overhaul slag treatment method provided by the present invention has the following beneficial effects:

[0077] 1) The wet method is used to treat the aluminum ash from overhaul slag, which can effectively reduce the secondary pollution in the disposal process and improve the safety factor of operation; the wet ball milling method is used instead of mechanical stirring. During the stirring process, the mechanical force of the ball mill is used to enhance the reaction and leaching effect.

[0078] 2) The wet ball milling method is used to harmlessly treat the overhaul slag, which shortens the process flow. While the ball mill is crushing, the overhaul slag particles can be further refined to make the reaction more complete, improve the leaching effect of the harmless reaction, shorten the reaction time, and greatly save energy in industrial production.

[0079] 3) The wet process helps to extract lithium and improve resource utilization. The particle size distribution of overhaul slag after wet ball milling can reach below 50μm, and the filter cake is more conducive to the use of subsequent products.

[0080] On the other hand, the present invention also provides a device for efficiently disposing overhaul slag in a resource-saving manner, which can be used to perform the above-mentioned method, and the device includes the following components:

[0081] Crusher unit, used to crush overhaul slag into particles below 40 mesh;

[0082] A wet drum ball mill is used to mix and react the crushed overhaul slag particles with water, grinding balls and reagents; the reagents include catalytic reaction reagents and harmless reagents added successively;

[0083] The screening device is used to separate the grinding balls and slurry remaining after the reaction in the wet drum ball mill; the remaining grinding balls are returned to the ball mill for reuse;

[0084] A filter is used to settle and filter the slurry screened by the screening device to obtain a primary filtrate and a harmless filter cake;

[0085] A lithium extraction reaction pool is used to adjust the pH value of the primary filtrate with an alkaline solution, separate the precipitate into solid and liquid, and obtain a secondary filtrate and a precipitate containing aluminum hydroxide; and to react the secondary filtrate with a lithium extraction agent, and the product of the reaction is filtered and dried to obtain a filter cake and a tertiary filtrate, wherein the filter cake contains lithium.

[0086] It should be noted that the above components can be assembled into a production line to realize the automated processing of overhaul slag. In addition, the functions of each component can also refer to the relevant embodiments when introducing the method above, and no further description is given.

[0087] The specific implementation methods described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific implementation method of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made on the basis of the technical solution of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for efficiently disposing overhaul slag as a resource, characterized in that: The following steps are involved: Step 1: Send the overhaul slag into the crusher and crush it into particles below 40 mesh; Step 2: conveying the crushed overhaul slag particles into a wet drum ball mill, wherein the wet drum ball mill is pre-loaded with grinding balls and water; Step 3: Add catalytic reaction reagents to the wet drum ball mill and react for a period of time; Step 4: Add the harmless agent to the wet drum ball mill, react for a period of time, and collect and treat the gas generated by the reaction; Step 5: After the reaction is completed, the grinding balls and the slurry are separated by screening, the grinding balls are returned to the ball mill for reuse, and the slurry is separated by sedimentation and filtration to obtain a primary filtrate and a harmless filter cake; Step 6: transporting the primary filtrate to a lithium extraction reaction tank, adjusting the pH value of the primary filtrate with an alkaline solution, and performing solid-liquid separation on the precipitate to obtain a secondary filtrate and a precipitate containing aluminum hydroxide; Step 7: Add lithium extraction reaction reagent to the secondary filtrate, and obtain a lithium-containing filter cake and a tertiary filtrate after stirring reaction, sedimentation, filtration and drying.

2. The method according to claim 1, characterized in that In the step 1, sending the overhaul slag into the crusher includes allowing the overhaul slag to pass through a box crusher, a jaw crusher, and a first drum ball mill in sequence.

3. The method according to claim 2, characterized in that The particle size of the overhaul slag after being crushed by the box crusher is controlled at 30-50mm, and the particle size of the overhaul slag after being crushed by the jaw crusher is controlled at 5-30mm. The overhaul slag ground by the first drum ball mill is passed through a 40-mesh vibrating screen to obtain overhaul slag particles smaller than 40 mesh.

4. The method according to claim 1, characterized in that The proportion of the pre-installed water is 40% to 200% of the mass ratio of the overhaul slag, and the temperature is 25°C to 100°C.

5. The method according to claim 1, characterized in that The pre-installed grinding balls are one or more of zirconium oxide balls, aluminum oxide balls and iron balls, and the added amount of the grinding balls is 50% to 200% of the mass ratio of the overhaul slag.

6. The method according to claim 1, characterized in that The catalytic reaction agent is one or more of sulfuric acid, aluminum sulfate, aluminum nitrate, and calcium chloride, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

7. The method according to claim 1, characterized in that In step 4, after adding the harmless agent, the wet ball mill is sealed with a cover at both ends, and the cover is provided with an exhaust port. The gas generated by the reaction is discharged from the exhaust port, and then absorbed by dilute sulfuric acid to remove impurities and harmlessness, and then emptied.

8. The method according to claim 1, characterized in that The harmless agent is one or more of calcium chloride, calcium hypochlorite, hydrogen peroxide and sodium hydroxide, and the added amount is 2% to 15% of the mass ratio of the overhaul slag.

9. The method according to claim 1, characterized in that The lithium extraction reaction reagent is one or more of sodium carbonate, magnesium carbonate and potassium carbonate, and the added amount is 1% to 10% of the mass ratio of the overhaul slag, and the filter cake contains lithium carbonate.

10. A device for efficiently disposing overhaul slag in a resource-saving manner, characterized in that: Includes the following components: Crusher unit, used to crush overhaul slag into particles below 40 mesh; A wet drum ball mill is used to mix and react the crushed overhaul slag particles with water, grinding balls and reagents; the reagents include catalytic reaction reagents and harmless reagents added successively; The screening device is used to separate the grinding balls and slurry remaining after the reaction in the wet drum ball mill; the remaining grinding balls are returned to the ball mill for reuse; A filter is used to settle and filter the slurry screened by the screening device to obtain a primary filtrate and a harmless filter cake; A lithium extraction reaction tank, in which the pH value of the primary filtrate is adjusted by using an alkaline solution, and the precipitate is separated into a solid and a liquid to obtain a secondary filtrate and a precipitate containing aluminum hydroxide; And, the secondary filtrate is reacted with a lithium extraction agent, and the product of the reaction is filtered and dried to obtain a filter cake and a tertiary filtrate, wherein the filter cake contains lithium.

Citation Information

Patent Citations

  • Method for preparing lithium carbonate from coal ash

    CN103101935A

  • Harmless treatment method of aluminum electrolysis overhaul slag

    CN109332350A

  • Method for treating aluminum ash in aluminum industrial production

    CN112142353A

  • Lithium slag treatment method

    CN116651903A

  • Resource recycling method for overhaul slag

    CN116715262A

Cited By

  • Method for treating overhaul slag by alkaline process and recycling

    CN121589112A