Operation method for improving blowing rate of air brick

By utilizing the exothermic principle of pre-oxygen oxidation of steel clips and bottom blowing pressure in the breathable bricks in the iron and steel metallurgical industry, combined with the main pipeline and auxiliary pipeline structures, monitoring the air permeability and introducing a mixture of oxygen and argon to remove the steel clips, the problem is solved The problem of poor air permeability of breathable bricks enables efficient stirring of molten steel without the need for pouring. It is suitable for a variety of breathable brick types and prevents the influence of oxygen on the composition of molten steel.

CN118808622APending Publication Date: 2024-10-22LUOYANG LIER REFRACTORY MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410741260.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-11
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

In the iron and steel metallurgical industry, the ventilation channels of the breathable bricks may cause steel clamping due to repeated replacement of gas joints or unstable gas pressure, which affects the air permeability. It may even cause overturning accidents and uneven composition of molten steel, affecting the smelting rhythm and steel quality. .

Method used

By using the principle of pre-oxygen oxidation and heat release of steel clips in the ventilation channel of the breathable brick, and cooperating with the effect of bottom blowing pressure, a pipeline structure is designed, including the main pipeline and the auxiliary pipeline, and the flow meter is used to monitor the ventilation. When the ventilation When the performance is poor, a mixed gas of oxygen and argon is introduced to remove the clamped steel to prevent excessive oxygen from entering the molten steel.

Benefits of technology

It effectively removes the steel clips in the breathable channel, improves the blowing rate of breathable bricks, avoids back-packing processing, is suitable for different types of breathable bricks, and prevents the influence of oxygen on the composition of molten steel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808622A_ABST
    Figure CN118808622A_ABST
Patent Text Reader

Abstract

According to the operation method for improving the blowing rate of the air brick, a main pipeline communicated with an air channel in the air brick is included, and a pressure stabilizer, a first one-way valve and a first valve switch are sequentially arranged on the main pipeline from the side close to the air brick to the side away from the air brick; an auxiliary pipeline is connected in parallel to the main pipeline between the pressure stabilizer and the first one-way valve, and mixed gas of oxygen and argon is introduced into the auxiliary pipeline; the pipeline structure is reasonable in design structure, the clamping steel in the ventilation channel is removed by utilizing the principle that the clamping steel in the ventilation channel of the ventilation brick is subjected to pre-oxygen oxidation heat release in cooperation with the action of bottom blowing pressure, the problem that the ventilation brick is poor in ventilation performance is avoided, ladle-to-ladle treatment is not needed, the pipeline structure can meet use of different types of ventilation bricks, and the application range is wide. The method has the advantage of wide application range, and meanwhile, the problem of component influence of oxygen on the molten steel is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of ladle refining, and in particular relates to an operating method for improving the blowing rate of air permeable bricks. Background Art

[0002] In the iron and steel metallurgical industry, after the molten steel enters the ladle, inert gas is blown into the ladle through the air bricks to stir the molten steel. This can achieve the purpose of stirring the molten steel, even the temperature and chemical composition of the molten steel, promote the floating of inclusions or control the shape of inclusions. This is a technology commonly used in the modern metallurgical industry. The role of air bricks in the metallurgical industry is becoming more and more important.

[0003] There are many types of air bricks on the market, mainly slit type, diffuse type, annular seam type, labyrinth type, etc. The principle is that there is an air passage inside the air brick during the production process. However, during the normal use of the air brick, due to factors such as repeated replacement of gas joints or unstable gas pressure, steel may be trapped in the air passage of the air brick, affecting the air permeability of the air brick. In severe cases, it may cause a bag inversion accident or even uneven composition of molten steel, affecting the smelting rhythm of the steel plant or affecting the quality of steel. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides an operating method for improving the blowing rate of air-permeable bricks. The principle of pre-oxygen oxidation and heat release of clamped steel in the air-permeable channel of the air-permeable brick is utilized. Under the action of bottom blowing pressure, the clamped steel in the air-permeable channel is removed, thereby avoiding the problem of poor air permeability of the air-permeable brick. There is no need to perform a reverse package treatment. Moreover, this pipeline structure can meet the use of different types of air-permeable bricks, has the advantage of a wide range of applications, and also avoids the problem of oxygen affecting the composition of molten steel.

[0005] The technical solution adopted by the present invention is: an operation method for improving the blowing rate of a permeable brick, comprising a main pipeline connected to the permeable passage inside the permeable brick, the main pipeline is provided with a voltage stabilizer, a first one-way valve and a first valve switch in sequence from the side close to the permeable brick to the side far from the permeable brick, a secondary pipeline is connected in parallel to the main pipeline between the voltage stabilizer and the first one-way valve, and a mixed gas of oxygen and argon is introduced into the secondary pipeline; The operation method of the pipeline structure is: using a flow meter to monitor the permeability of the pipeline, when it is monitored that the permeability is poor, the auxiliary pipeline is connected, and the oxygen introduced into the auxiliary pipeline can enter the air permeable channel of the air brick, thereby removing the clamped steel in the air permeable channel; when the flow meter monitors that the permeability meets the requirements, the ventilation of the auxiliary pipeline is stopped to prevent excessive oxygen from entering the molten steel and affecting the composition of the molten steel.

[0006] The secondary pipeline is provided with a second one-way valve and a second valve switch.

[0007] In the secondary pipeline, the oxygen content is 0.01%-100%.

[0008] A flow meter is also installed on the main pipe.

[0009] The beneficial effects of the present invention are: The invention has a reasonable design structure, utilizes the principle of heat release by pre-oxidation of steel clamps in the air passage of the air brick by oxygen, and removes the steel clamps in the air passage under the action of bottom blowing pressure, thereby avoiding the problem of poor air permeability of the air brick, and does not need to perform reverse bagging treatment. Moreover, the pipeline structure can meet the use of different types of air bricks, has the advantage of a wide range of applications, and also avoids the problem of oxygen affecting the composition of molten steel. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 It is a structural schematic diagram of the present invention.

[0011] Among them: 1. Main pipeline; 2. First valve switch; 3. First one-way valve; 4. Secondary pipeline; 5. Second one-way valve; 6. Second valve switch; 7. Voltage stabilizer; 8. Flow meter. DETAILED DESCRIPTION

[0012] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0013] As shown in the figure, an operating method for improving the blowing rate of a breathable brick comprises a main pipe 1 connected to the internal air permeable channel of the breathable brick, the main pipe 1 is provided with a voltage stabilizer 7, a first non-return valve 3 and a first valve switch 2 in sequence from the side close to the breathable brick to the side far from the breathable brick, wherein the main pipe 1 is an argon gas pipeline, the purity of argon gas can reach above 99.999%, and the argon gas is introduced into the air permeable channel of the breathable brick as the main gas for stirring molten steel; a flow meter 8 is also installed on the main pipe 1, and the flow meter 8 is arranged on the main pipe between the voltage stabilizer 7 and the breathable brick, and is used to monitor in real time whether the gas in the pipeline is unobstructed.

[0014] A secondary pipeline 4 is connected in parallel to the main pipeline 1 between the voltage stabilizer 7 and the first one-way valve 3, and a mixed gas of oxygen and argon is introduced into the secondary pipeline 4. A second one-way valve 5 and a second valve switch 6 are provided on the secondary pipeline 4. The second valve switch 6 is a high-temperature resistant valve to avoid failure due to high temperature during operation. Specifically, in the secondary pipeline 4, the oxygen content is 0.01%-100%, and the rest is argon. The amount of oxygen introduced can be selected according to actual needs. In this example, the oxygen content is 1% and the argon content is 99%. This arrangement utilizes the oxidation exothermic reaction of the steel clamps in the air permeable channel when encountering oxygen, and at the same time, under the action of the bottom blowing pressure, the steel clamps in the air permeable channel can be removed, thereby ensuring the air permeability of the air brick. When the flow rate in the pipeline reaches the requirement, the oxygen introduction can be stopped, the purpose is to prevent too much oxygen from entering the molten steel and affecting the composition of the molten steel, and also to prevent excessive melting loss of the air brick itself by oxygen.

[0015] The operation method of the pipeline structure is as follows: the flow meter is used to monitor the air permeability of the pipeline. When the air permeability is poor, the auxiliary pipeline 4 is turned on, and the oxygen introduced into the auxiliary pipeline 4 can enter the air permeable channel of the air permeable brick, thereby removing the clamped steel in the air permeable channel. When the flow meter monitors that the air permeability meets the requirements, the ventilation of the auxiliary pipeline 4 is stopped to prevent excessive oxygen from entering the molten steel and affecting the composition of the molten steel. This method of improving the blowing rate of the air brick is operated by using a double pipeline at the rear of the air brick. The main pipeline 1 is normally used to introduce argon to stir the molten steel. When the air permeability is normal, there is no need to open the auxiliary pipeline 4 and normal operation is sufficient. However, when the air permeability is insufficient, the auxiliary pipeline 4 needs to be opened. When the oxygen in the auxiliary pipeline 4 meets the steel clamps in the air passage of the air brick core at high temperature, the steel clamps are oxidized and burned, thereby ensuring the smooth flow of the air passage and ensuring the air permeability.

[0016] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. An operating method for improving the blowing rate of air permeable bricks, characterized in that: It includes a main pipeline connected to the air permeable channel inside the air permeable brick, the main pipeline is provided with a voltage stabilizer, a first one-way valve and a first valve switch in sequence from the side close to the air permeable brick to the side far from the air permeable brick, and a secondary pipeline is connected in parallel to the main pipeline between the voltage stabilizer and the first one-way valve, and a mixed gas of oxygen and argon is passed into the secondary pipeline; The operation method of the pipeline structure is: using a flow meter to monitor the permeability of the pipeline, when it is monitored that the permeability is poor, the auxiliary pipeline is connected, and the oxygen introduced into the auxiliary pipeline can enter the air permeable channel of the air brick, thereby removing the clamped steel in the air permeable channel; when the flow meter monitors that the permeability meets the requirements, the ventilation of the auxiliary pipeline is stopped to prevent excessive oxygen from entering the molten steel and affecting the composition of the molten steel.

2. The method for improving the blowing rate of air-permeable bricks according to claim 1, characterized in that: The secondary pipeline is provided with a second one-way valve and a second valve switch.

3. The method for improving the blowing rate of air-permeable bricks according to claim 1, characterized in that: In the secondary pipeline, the oxygen content is 0.01%-100%.

4. The method for improving the blowing rate of air-permeable bricks according to claim 1, characterized in that: A flow meter is also installed on the main pipe.