Flame-retardant straw composite board and manufacturing method thereof

By combining straw pretreatment with microporous technology, combined with reinforced ribs and phase change particles, the problems of low mechanical properties and single function of straw composite boards are solved, significantly improving the flame retardant performance and diversity, and extending the service life. .

CN118809756AInactive Publication Date: 2024-10-22ANHUI TANHE JIUYUAN AGRICULTURAL TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411199941.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-10-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the production of existing straw composite boards, the wax on the surface of the straw affects the bonding strength of the flame-retardant adhesive and straw debris. The penetration speed of the flame-retardant adhesive is slow, resulting in low mechanical properties and single function of the composite board.

Method used

By pre-processing the straw raw material to remove the wax layer, using microporous technology to enable the flame-retardant adhesive to penetrate deep into the straw, combined with reinforcing ribs and phase change particles, the bonding strength between the adhesive and straw is improved, and the composite board is added sound absorption, heat absorption and flame retardant properties.

Benefits of technology

The mechanical properties, flame retardant performance and functional diversity of the straw composite board are significantly improved, the heat resistance and sound insulation performance of the composite board are enhanced, and the service life is extended.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118809756A_ABST
    Figure CN118809756A_ABST
Patent Text Reader

Abstract

The invention discloses a flame-retardant straw composite board and a manufacturing method thereof, and relates to the technical field of composite boards, the method mainly comprises the following steps: pretreating a straw raw material, crushing, uniformly mixing straw chippings, phase-change particles and a flame-retardant adhesive to form a mixed raw material, wrapping a pretreated reinforcing rib plate with the mixed raw material, and carrying out heat treatment to obtain the flame-retardant straw composite board. And the flame-retardant straw composite board is prepared through pre-pressing molding operation and hot-pressing molding operation. According to the flame-retardant straw composite board and the manufacturing method thereof, through the arrangement of the micropores I, a flame-retardant adhesive can flow into straw chippings, the bonding strength of the straw chippings and the flame-retardant adhesive is improved, and the mechanical property of the flame-retardant straw composite board is improved; according to the flame-retardant straw composite board, straw raw materials are pretreated, so that a wax coat of the straw raw materials can be removed, the bonding strength between straw surface chippings and the flame-retardant adhesive is improved, and the mechanical property of the flame-retardant straw composite board is further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of composite boards, in particular to a flame-retardant straw composite board and a manufacturing method thereof. Background Art

[0002] Straw composite panels are environmentally friendly building materials made from straw and a binder. They are lightweight, high-strength, fire-resistant, and heat-insulating, making them widely used in construction, furniture manufacturing, and other fields. As straw is agricultural waste, its effective utilization can help reduce environmental pollution and resource waste.

[0003] In the related art, the method for making straw composite boards is usually as follows: after the straw raw material is fully crushed, the flame retardant adhesive is fully mixed with the straw debris, and the raw material is solidified and formed to form a flame retardant straw composite board. However, since there is a layer of wax on the surface of the straw, the wax will affect the bonding strength between the flame retardant adhesive and the straw debris, and fully crushing the straw will not destroy the wax layer on the surface of the straw, which will affect the quality of the produced straw composite board; the flame retardant adhesive generally only bonds with the surface of the straw debris, and the flame retardant adhesive penetrates into the interior of the straw debris at a slow speed or cannot penetrate into the interior of the straw debris, affecting the bonding strength between the flame retardant adhesive and the straw debris, and thus affecting the production quality of the straw composite board; and the composite board has low strength and single function; based on this, the present application proposes a flame retardant straw composite board and a manufacturing method thereof. Summary of the Invention

[0004] The present invention provides a flame-retardant straw composite board and a manufacturing method thereof, which solves the problems proposed in the above-mentioned background technology that the wax on the surface of the straw will affect the bonding strength between the flame-retardant adhesive and the straw debris; the flame-retardant adhesive penetrates into the interior of the straw debris slowly or cannot penetrate into the interior of the straw debris, thereby affecting the mechanical properties of the composite board, and the composite board has low strength and single function.

[0005] The present invention provides the following technical solution: a method for manufacturing a flame-retardant straw composite board, comprising the following steps:

[0006] Step 1: Prepare straw raw materials, flame retardant adhesive, phase change particles and reinforcing ribs;

[0007] The straw raw material has undergone basic processing such as dust removal and sorting. The reinforcing rib plate is in a grid shape and includes transverse reinforcing ribs, vertical reinforcing ribs and connecting ribs. The ends of the vertical reinforcing ribs are fixed with transverse reinforcing ribs. Two adjacent vertical reinforcing ribs and two adjacent transverse reinforcing ribs are connected by connecting ribs. The transverse reinforcing ribs and the vertical reinforcing ribs each include a straight portion and a bent portion. The straight portion is located between the two bent portions, and the convex side of the bent portion is inserted into the concave side of the adjacent bent portion.

[0008] Step 2: pre-treating the straw raw material to destroy the wax layer on the surface of the straw raw material; pre-treating the reinforcing rib plate, filling the inner cavity of the reinforcing rib plate with a flame retardant, and providing a diaphragm between the flame retardant and the reinforcing rib plate;

[0009] Step 3: Wash and dry the straw obtained in step 2, and punch micropores on the straw using a micropore puncher, wherein there are two types of micropores on the surface of the straw, namely micropore 1 and micropore 2, wherein the size of micropore 1 is not less than the diameter of the flame retardant adhesive molecule, and the size of micropore 2 is less than the diameter of the flame retardant adhesive molecule;

[0010] Step 4: Fully crush the punched straw to obtain straw debris;

[0011] Step 5: After fully mixing the phase change particles and the straw chips, they are further fully mixed with a flame retardant adhesive to obtain a mixed raw material;

[0012] Step 6: After laying a layer of mixed raw materials in the straw composite board forming mold to form a bottom layer, the reinforcing rib plate is placed on the bottom layer, and the mixed raw materials are continued to be added so that the reinforcing rib plate is wrapped by the mixed raw materials. The raw materials in the mold are pre-pressed and thermoset in sequence to obtain a composite board;

[0013] Step 7: Place the composite board at room temperature for 3-5 days to obtain a finished flame-retardant composite board.

[0014] Preferably, in step 2, the methods used to destroy the wax layer on the surface of the straw raw material include but are not limited to: caustic soda solution treatment, lime solution treatment and mixed solution treatment.

[0015] Preferably, in step three, micropore one and micropore two are alternately arranged, and both micropore one and micropore two are through holes, and the straw is penetrated by micropore one and micropore two.

[0016] Preferably, the mass ratio of the flame retardant adhesive, the phase change particles and the straw chips is 1:20:79.

[0017] Preferably, holes are provided on the side walls of the reinforcing rib plate, and the diaphragm decomposes when heated.

[0018] Preferably, the size of the phase change particles is the same as that of the straw debris, and the outer surface of the phase change particles is wrapped with an isolation shell, and the isolation shell has flame retardant and high temperature resistant properties.

[0019] Preferably, the pre-pressing is performed at room temperature and pressure, and the hot pressing is performed at 9-12 MPa and 130-150° C. for 60-90 min.

[0020] A flame-retardant straw composite board manufactured by a manufacturing method includes a wrapping system and a reinforcing rib plate, wherein the reinforcing rib plate is located inside the wrapping system, and the wrapping system includes a flame-retardant adhesive, phase-change particles and straw debris, and the phase-change particles and straw debris are connected by the flame-retardant adhesive.

[0021] Preferably, the reinforcing rib plate is a hollow structure, the inner cavity of the reinforcing rib plate is filled with a flame retardant, and holes are provided on the side walls of the reinforcing rib plate. An isolation membrane is fixed to the inner wall of the reinforcing rib plate, and the flame retardant is wrapped by the isolation membrane.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. The flame-retardant straw composite board and its manufacturing method, through the setting of micropores 1, allow the flame-retardant adhesive to flow into the interior of the straw debris, thereby improving the bonding strength between the straw debris and the flame-retardant adhesive and improving the mechanical properties of the flame-retardant straw composite board; by pre-treating the straw raw material, the wax layer of the straw raw material can be removed, the bonding strength between the straw surface debris and the flame-retardant adhesive can be increased, and the mechanical properties of the flame-retardant straw composite board can be further improved.

[0024] 2. The flame-retardant straw composite board and its manufacturing method have the following advantages: through the setting of micropores 2, the composite board has a sound-absorbing function, which improves the sound insulation performance of the composite board and facilitates the use of the composite board; through the setting of phase change particles, the composite board has a heat-absorbing function, which improves the heat resistance of the composite board and further improves the flame-retardant performance of the composite board; through the setting of flame retardants, the flame-retardant performance of the composite board is further improved.

[0025] 3. The flame-retardant straw composite board and its manufacturing method, through the provision of a reinforcing rib plate, can support the composite board and improve the compression resistance of the composite board, thereby extending the service life of the composite board. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a front view of a flame-retardant straw composite board prepared by a method for manufacturing a flame-retardant straw composite board provided by the present invention;

[0027] Figure 2 The structure of the present invention Figure 1 Front view schematic diagram;

[0028] Figure 3 This is a schematic diagram of the structural reinforcement plate of the present invention;

[0029] Figure 4 The structure of the present invention Figure 3 Top view schematic diagram.

[0030] In the figure: 1. Flame retardant binder; 2. Phase change particles; 3. Straw chips; 4. Vertical reinforcement ribs; 5. Horizontal reinforcement ribs; 6. Connecting ribs. DETAILED DESCRIPTION

[0031] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0032] The present invention provides a method for manufacturing a flame-retardant straw composite board, comprising the following steps:

[0033] Step 1: Prepare straw raw materials, flame retardant adhesive, phase change particles and reinforcing ribs;

[0034] The straw raw materials have undergone basic processing such as dust removal and sorting, and the reinforcing ribs are in a grid shape; the phase change particles are wrapped with an isolation shell, which has flame retardant and high temperature resistant properties. The phase change particles can be solid-liquid phase change particles, and the isolation shell can wrap the phase change particles that have become liquid, so as to facilitate the reuse of the phase change particles.

[0035] Step 2: Pre-treat the straw raw material to destroy the waxy layer on the surface of the straw raw material. The methods used to destroy the waxy layer on the surface of the straw raw material include but are not limited to: caustic soda solution treatment, lime solution treatment, and mixed liquid treatment. When using the caustic soda solution treatment method to remove the waxy layer on the surface of the straw, the ratio of caustic soda to straw is 1:20-25, and the ratio of caustic soda to water is 1:20-25. The caustic soda aqueous solution is sprayed onto the surface of the straw raw material and left at room temperature for 8-10 hours. When using the lime solution treatment method to remove the waxy layer on the surface of the straw, the raw materials used are lime, water, and salt, wherein the weight ratio of lime, straw raw material, water, and salt is: 1:50-100:150-300:0.5-1. The lime aqueous solution is sprayed onto the surface of the straw and piled for 24-36 hours. The mixed liquid treatment method is to mix 15% caustic soda solution and lime water solution of the same concentration evenly, spray them on the surface of the straw together, with the ratio of the mixed liquid to the straw being 4:5, and pile them for 7-10 days.

[0036] The reinforcing rib plate is pretreated, and the inner cavity of the reinforcing rib plate is filled with a flame retardant, and a diaphragm is provided between the flame retardant and the reinforcing rib plate. Holes are provided on the side walls of the reinforcing rib plate, and the diaphragm decomposes when heated. The material of the diaphragm can be selected according to needs and is not restricted here. Through the setting of the holes, the diaphragm and the flame retardant, when the reinforcing rib plate is heated and the diaphragm decomposes when heated, the holes are in an open state, and the flame retardant flows out, thereby improving the flame retardant performance of the composite board.

[0037] Step three, the straw obtained in step two is cleaned and dried, and micropores are punched on the straw using a micropore puncher. There are two types of micropores on the surface of the straw, namely micropore one and micropore two. The size of micropore one is not less than the diameter of the flame retardant adhesive molecule, and the size of micropore two is less than the diameter of the flame retardant adhesive molecule. Micropore one and micropore two are alternately arranged, and micropore one and micropore two are both through holes. The straw is penetrated by micropore one and micropore two, and micropore two is a honeycomb hole. Through the setting of micropore one, the flame retardant adhesive molecules can enter micropore one, thereby improving the connection strength between the flame retardant adhesive and the straw debris, while the flame retardant adhesive cannot enter micropore two, so that the composite board prepared using straw debris is provided with multiple micropores, so that the prepared composite board has a sound insulation function, thereby improving the functionality of the composite board.

[0038] Step 4: Fully crushing the punched straw to obtain straw debris, wherein the size of the phase change particles is the same as that of the straw debris;

[0039] Step 5: Thoroughly mix the phase-change particles with the straw scraps and then with the flame-retardant binder to create a mixed material. The phase-change particles provide a heat-absorbing composite board, further enhancing its flame-retardant properties. The mass ratio of the flame-retardant binder, phase-change particles, and straw scraps is 1:20:79.

[0040] Step 6: After laying a layer of mixed raw materials in the straw composite board forming mold to form a bottom layer, place the reinforcing rib plate on the bottom layer, and then continue to add mixed raw materials so that the reinforcing rib plate is wrapped by the mixed raw materials. The raw materials in the mold are pre-pressed and thermoset in turn to obtain a composite board. In this way, the wrapping system formed by the mixed raw materials can completely wrap the reinforcing rib plate, and the reinforcing rib plate is in a grid shape, which improves the strength of the composite board. Pre-pressing is carried out at room temperature and pressure, and hot pressing is carried out at 9-12MPa and 130-150℃ for 60-90min.

[0041] Step 7: Place the composite board at room temperature for 3-5 days to obtain a finished flame-retardant composite board.

[0042] The present invention provides a flame-retardant composite panel, which is prepared using the above-mentioned manufacturing method. The flame-retardant composite panel includes a wrapping system and a reinforcing rib plate, wherein the reinforcing rib plate is located inside the wrapping system. The wrapping system includes a flame-retardant adhesive 1, phase change particles 2 and straw debris 3, and the phase change particles 2 and straw debris 3 are connected by the flame-retardant adhesive 1.

[0043] The flame retardant binder 1, the phase change particles 2 and the straw chips 3 are fully and evenly mixed in a mass ratio of 1:20:79 to form a wrapping system.

[0044] The reinforcing rib plate includes transverse reinforcing ribs 5, vertical reinforcing ribs 4 and connecting ribs 6. The ends of the vertical reinforcing ribs 4 are fixed with transverse reinforcing ribs 5. The adjacent two vertical reinforcing ribs 4 and the adjacent two transverse reinforcing ribs 5 are connected by connecting ribs 6, so that the reinforcing rib plate forms a grid structure.

[0045] Both the transverse ribs 5 and the vertical ribs 4 consist of a straight portion and a bent portion. The straight portion is located between the two bent portions, with the convex side of the bent portion inserted into the concave side of the adjacent bent portion. The bent portion has elasticity, which reduces the force applied to the rib plate, improving the compressive resistance of the rib plate and, consequently, the composite panel.

[0046] The reinforcing rib plate has a hollow structure, the inner cavity of the reinforcing rib plate is filled with flame retardant, and holes are provided on the side wall of the reinforcing rib plate. An isolation membrane is fixed to the inner wall of the reinforcing rib plate, and the flame retardant is wrapped by the isolation membrane.

[0047] In summary, the present invention allows the flame-retardant adhesive and straw debris to be fully mixed, thereby improving the connection strength between the flame-retardant adhesive and the straw debris, and further improving the mechanical properties of the manufactured flame-retardant straw composite board; the setting of phase change particles and flame retardants enables the composite board to have the function of absorbing heat and releasing flame retardants, further improving the flame retardant properties of the straw composite board; the setting of micropore 2 enables the composite board to have a sound insulation function, increases the function of the composite board, and makes the composite board multifunctional, and the setting of the reinforcing rib plate improves the mechanical properties of the composite board.

[0048] The standard parts used in the present invention can all be purchased from the market, and special-shaped parts can be customized according to the description in the specification and the drawings. The specific connection methods of each part adopt conventional means such as mature bolts, rivets, welding, etc. in the existing technology. The machinery, parts and equipment all adopt conventional models in the existing technology and will not be described in detail here. The contents not described in detail in this specification belong to the existing technology known to professional and technical personnel in this field. Although the embodiments of the present invention have been shown and described, it can be understood by ordinary technicians in this field that various changes, modifications, substitutions and modifications can be made to these embodiments without departing from the principles and spirit of the present invention. The scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for manufacturing a flame retardant straw composite board, characterized in that: The following steps are involved: Step 1: prepare straw raw materials, flame retardant adhesives, phase change particles and reinforcing rib plates; The straw raw material has undergone basic processing such as dust removal and sorting. The reinforcing rib plate is in a grid shape and comprises transverse reinforcing ribs (5), vertical reinforcing ribs (4) and connecting ribs (6). The ends of the vertical reinforcing ribs (4) are fixed with transverse reinforcing ribs (5). Two adjacent vertical reinforcing ribs (4) and two adjacent transverse reinforcing ribs (5) are connected by connecting ribs (6). The transverse reinforcing ribs (5) and the vertical reinforcing ribs (4) both comprise a straight portion and a bent portion. The straight portion is located between the two bent portions, and the convex side of the bent portion is inserted into the concave side of the adjacent bent portion. Step 2: pre-treating the straw raw material to destroy the wax layer on the surface of the straw raw material; pre-treating the reinforcing rib plate, filling the inner cavity of the reinforcing rib plate with a flame retardant, and providing a diaphragm between the flame retardant and the reinforcing rib plate; Step 3, washing and drying the straw obtained in step 2, punching micropores on the straw using a micropore puncher, wherein there are two types of micropores on the surface of the straw, namely micropore 1 and micropore 2, wherein the size of micropore 1 is not less than the molecular diameter of the flame retardant adhesive, and the size of micropore 2 is less than the molecular diameter of the flame retardant adhesive; Step 4: Fully crush the punched straw to obtain straw debris; Step 5: After the phase change particles and the straw debris are fully mixed, they are further fully mixed with a flame retardant adhesive to obtain a mixed raw material; Step 6: After laying a layer of mixed raw materials in the straw composite board forming mold to form a bottom layer, the reinforcing rib plate is placed on the bottom layer, and then the mixed raw materials are continued to be added so that the reinforcing rib plate is wrapped by the mixed raw materials. The raw materials in the mold are pre-pressed and thermoset in sequence to obtain a composite board; Step 7: Place the composite board at room temperature for 3-5 days to obtain a finished flame-retardant composite board.

2. The method for manufacturing a flame retardant straw composite board according to claim 1, characterized in that: In the step 2, the methods used to destroy the wax layer on the surface of the straw raw material include but are not limited to: caustic soda solution treatment method, lime solution treatment method and mixed solution treatment method.

3. The method for manufacturing a flame retardant straw composite board according to claim 1, characterized in that: In the step three, micropore one and micropore two are arranged alternately, and both micropore one and micropore two are through holes, and the straw is penetrated by micropore one and micropore two.

4. The method for manufacturing a flame retardant straw composite board according to claim 1, characterized in that: The mass ratio of the flame retardant adhesive, the phase change particles and the straw chips is 1:20:

79.

5. The flame retardant straw composite board and the manufacturing method thereof according to claim 1, characterized in that: The side wall of the reinforcing rib plate is provided with holes, and the diaphragm is decomposed by heat.

6. The method for manufacturing a flame retardant straw composite board according to claim 1, characterized in that: The size of the phase change particles is the same as that of the straw debris. The outer surface of the phase change particles is wrapped with an isolation shell, and the isolation shell has flame retardant and high temperature resistant properties.

7. The method for manufacturing a flame retardant straw composite board according to claim 1, characterized in that: The pre-pressing is performed at room temperature and pressure, and the hot pressing is performed at 9-12 MPa and 130-150° C. for 60-90 min.

8. The flame retardant straw composite board manufactured by the method for manufacturing a flame retardant straw composite board according to any one of claims 1 to 7, characterized in that: The invention comprises a wrapping system and a reinforcing rib plate, wherein the reinforcing rib plate is located inside the wrapping system, and the wrapping system comprises a flame retardant adhesive (1), phase change particles (2) and straw debris (3), wherein the phase change particles (2) and the straw debris (3) are connected via the flame retardant adhesive (1).

9. The flame retardant straw composite board manufactured by the method for manufacturing a flame retardant straw composite board according to claim 8, characterized in that: The reinforcing rib plate is a hollow structure, the inner cavity of the reinforcing rib plate is filled with a flame retardant, and holes are provided on the side wall of the reinforcing rib plate. An isolation membrane is fixed to the inner wall of the reinforcing rib plate, and the flame retardant is wrapped by the isolation membrane.