Welding resistance wire printing process, circuit board preparation process and single-sided 6OZ thick copper-aluminum substrate circuit board
By using two steps of screen printing and exposure and development on the thick copper substrate, the problem of uneven solder resist ink thickness is solved, achieving uniform distribution of solder resist ink and improving line insulation performance.
Patent Information
- Application Number
- CN202410859994.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-22
AI Technical Summary
In the existing technology, solder mask screen printing on thick copper substrates is prone to uneven thickness of solder mask ink, resulting in poor development uniformity and affecting the insulation performance of the circuit and product appearance.
Two screen printing processes are used. The first time is to use a 32T dot screen to print A ink only on the line part. The second time is to use a 43T white screen to print B ink on the entire board. The distribution and thickness of the ink are controlled through exposure and development steps. Ensure uniformity of solder mask ink.
It achieves uniform distribution of solder resist ink, ensures sufficient thickness of line surface and line angle ink, solves the problem of uneven development, and improves the insulation performance of the circuit and the appearance quality of the product.
Smart Images

Figure CN118829092A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of single-sided circuit boards, and in particular to a solder resist screen printing process, a circuit board preparation process and a single-sided 6OZ thick copper-aluminum substrate circuit board. Background Art
[0002] Printed Wiring Board (PWB) is a key component in electronic devices, and its quality directly affects the safety performance and service life of electronic devices. Among them, metal-based thick copper circuit boards are widely used in various electronic devices due to their excellent conductivity, heat dissipation and stability. However, with the development of electronic devices towards miniaturization and high integration, the performance requirements for metal-based circuit boards are becoming higher and higher, especially in terms of copper foil thickness, circuit accuracy, solder mask ink thickness and molding accuracy.
[0003] In the prior art, solder resist screen printing generally coats solder resist ink by secondary blank screen printing, and forms a solder resist layer through development and curing steps. However, for thick copper substrates, the secondary blank screen printing ink method is prone to uneven solder resist ink thickness. The solder resist ink at the circuit is stepped, which leads to poor development uniformity, seriously affecting the insulation performance of the circuit and the appearance of the product. Summary of the invention
[0004] In view of the deficiencies in the prior art, the present application provides a solder resist silk screen printing process, a circuit board preparation process and a single-sided 6OZ thick copper-aluminum substrate circuit board.
[0005] According to a first aspect of the present invention, a solder resist screen printing process disclosed in the present application comprises: pre-treating a substrate: cleaning, grinding the substrate and roughening the copper surface;
[0006] The first screen printing is performed on the substrate: ink solution A is prepared, and the circuit part of the substrate is printed with ink solution A using a 32T dot screen, and the substrate is pre-baked;
[0007] Perform the second screen printing on the substrate: prepare the B ink solution, use 43T white screen to print the B ink solution on the substrate, and pre-bake the substrate;
[0008] Expose the substrate with screen printing ink: The substrate with screen printing ink is shielded by a film base, and the circuit diagram part of the substrate is exposed by ultraviolet radiation;
[0009] Developing the exposed substrate: using a developer to rinse the exposed substrate, with the ink side of the substrate facing downward;
[0010] Drying the developed substrate: When baking the board, the temperature gradually increases from low to high;
[0011] Among them, the proportion of open oil water to ink in A ink solution is less than the proportion of open oil water to ink in B ink solution.
[0012] Preferably, in the A ink solution, the ratio of the oil-opening water to the ink is 250±10ml:4Kg; in the B ink solution, the ratio of the oil-opening water to the ink is 300±10ml:4Kg.
[0013] Preferably, when exposing the substrate of the screen printing ink, the substrate is exposed by LDI method, and the exposure energy is 800mj / cm 2 The exposure scale is 9 grids and the positioning accuracy is 35um; during the development of the exposed substrate, the substrate transmission speed is 4m / min.
[0014] Preferably, the substrate after drying and development is baked four times continuously for one hour each time, the first baking temperature is set at 80±5°C, the second baking temperature is set at 100±5°C, the third baking temperature is set at 120±5°C, and the fourth baking temperature is set at 150±5°C.
[0015] According to a second aspect of the present invention, a circuit board preparation process disclosed in the present application includes: cutting: cutting a 6OZ thick copper-aluminum substrate according to the size requirements of the product drawing;
[0016] The inner layer of the substrate after cutting is made: the substrate is pre-treated, coated, baked, exposed, developed, inner layer etched, film stripped, burr treated and AOI are carried out in sequence;
[0017] The solder resist screen printing process is used to print the solder resist on the inner layer of the substrate;
[0018] Spray tin on the substrate after solder mask silk screen printing;
[0019] The substrate after tin spraying is subjected to forming treatment: the substrate is subjected to target shooting, laser cutting and gong plate in sequence;
[0020] Perform quality test on the formed substrate.
[0021] Preferably, the substrate is exposed by LDI in the inner layer production after cutting, and the exposure energy is 230mj / cm 2 , the exposure scale is 7 and a half stops.
[0022] Preferably, in the inner layer manufacturing of the cut substrate, etching includes:
[0023] The exposed substrate is etched for the first time, and the etching conveying speed is 1.7±1m / min;
[0024] The exposed substrate is etched for the second time, and the etching conveying speed is 2.5±1m / min;
[0025] The exposed substrate is etched for the third time, and the etching transfer speed is 3.5±1m / min.
[0026] Preferably, when etching the exposed substrate, the circuit board surface of the substrate faces downward.
[0027] According to a third aspect of the present invention, the present application discloses a single-sided 6OZ thick copper-aluminum substrate circuit board, which is manufactured using a circuit board manufacturing process.
[0028] The beneficial effects of the present application are as follows: by using a 32T dot screen for the first screen printing to print ink only on the circuit part of the substrate, and using a 43T white screen for the second screen printing to print ink on the entire substrate, the ink is only printed on the circuit part during the first screen printing, ensuring that the line surface and line angle ink thickness of the solder mask ink is sufficient. At the same time, a B ink solution with a lower viscosity is modulated in the second screen printing, so that the ink is easier to flow when the entire substrate is printed. In this way, the solder mask ink is no longer stepped, the solder mask ink is more uniform, and the line surface and line angle ink thickness is sufficient; when the exposed substrate is developed, the ink side of the substrate faces downward, and the developer rinses the substrate from bottom to top. After the developer rinses to the substrate and displays the target area, the developer splashed outside the target area can quickly flow down the substrate, while the developer rinses the substrate from top to bottom, and the developer splashed outside the target area still stays on the substrate, causing the non-target area of the substrate to be over-developed. In this way, the problem of uneven solder mask development is solved. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0030] Figure 1 Schematic diagram of the thickness of solder resist ink for thick copper circuit board in Example 1;
[0031] Figure 2 This is a schematic diagram of the thickness of solder resist ink for a medium-thick copper circuit board in Comparative Example 1;
[0032] Figure 3 This is a schematic diagram of the line width and line spacing of the thick copper circuit board in Example 2;
[0033] Figure 4 This is a schematic diagram of the structure of the thick copper circuit board prepared in Example 2;
[0034] Figure 5 This is a schematic diagram of the structure of the thick copper circuit board prepared in Comparative Example 2;
[0035] Figure 6 This is the second schematic diagram of the structure of the thick copper circuit board prepared in comparative example 2. DETAILED DESCRIPTION
[0036] The following will disclose multiple embodiments of the present application with drawings. For the purpose of clear description, many practical details will be described together in the following description. However, it should be understood that these practical details should not be used to limit the present application. In other words, in some embodiments of the present application, these practical details are not necessary. In addition, in order to simplify the drawings, some conventional structures and components will be depicted in a simple schematic manner in the drawings.
[0037] It should be noted that all directional indications such as up, down, left, right, front, back... in the embodiments of the present application are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture as shown in the accompanying drawings. If the specific posture changes, the directional indication will also change accordingly.
[0038] In addition, in the present application, the descriptions of "first", "second", etc. are only used for descriptive purposes, and do not specifically refer to the order or sequence, nor are they used to limit the present application. They are only used to distinguish components or operations described with the same technical terms, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present application.
[0039] In order to further understand the application content, features and effects of the present application, the following embodiments are cited and described in detail with reference to the accompanying drawings.
[0040] Embodiment 1
[0041] In this example, the solder mask screen printing process is used to screen print ink and form solder pads on a thick copper-aluminum substrate, which includes the following steps:
[0042] Substrate pretreatment: including cleaning the substrate, the substrate conveying speed is 4.0±1.0m / min; grinding, the wear mark thickness is: 12±2mm; roughening the copper surface, the water film time is ≥15s.
[0043] The first screen printing is performed on the substrate after pretreatment: including adjusting the A ink solution: the ink uses green oil, and the ratio of the oil water to the ink in the A ink solution is 250ml:4Kg; printing: using 32T dot screen printing; scraper pressure: 7Kg / cm 2 ; Scraper hardness: 75°; After screen printing the entire substrate, let it stand for 20 minutes and pre-bake it in a tunnel oven for 20 minutes at a temperature of 73°C.
[0044] The substrate after the first screen printing is screen printed for the second time: including adjusting B ink solution: the ink is green oil, and the ratio of oil water to ink in B ink solution is 300ml:4Kg; printing: using 43T white screen printing; scraper pressure: 7Kg / cm 2 ; Scraper hardness: 75°; After screen printing the entire substrate, let it stand for 20 minutes and pre-bake it in a tunnel oven for 30 minutes at a temperature of 73°C.
[0045] Expose the substrate after the second screen printing: including using LDI exposure machine to expose the substrate, the exposure energy is 800mj / cm 2 , the exposure scale is 9 grids and the positioning accuracy is 35um.
[0046] Develop the exposed substrate: including flushing the substrate with developer. When flushing the substrate, the ink side of the substrate is downward, and the developer flushes the substrate from bottom to top. The substrate conveying speed is 5.0m / min; the developing pressure is 2.0±0.5Kg / cm 2 ; The developing temperature is 30±2℃; The drying temperature is 60±5℃.
[0047] The developed substrate is dried: it includes four consecutive baking processes, each time for one hour, the first baking process is set at 80±5°C, the second baking process is set at 100±5°C, the third baking process is set at 120±5°C, and the fourth baking process is set at 150±5°C.
[0048] Comparative Example 1
[0049] Different from the first embodiment, the first screen printing in this embodiment includes: oil mixing, the ink uses green oil, the ratio of oil water to ink in the A ink solution is 300ml:4Kg; printing: using 32T white screen printing; scraper pressure: 7Kg / cm 2 ; Scraper hardness: 75°; After screen printing the entire substrate, let it stand for 15 minutes and pre-bake for 15 minutes at a temperature of 73°C.
[0050] The second screen printing includes: oil mixing, the ink uses green oil, the ratio of oil water to ink in B ink solution is 300ml:4Kg; printing: using 32T white screen printing; scraper pressure: 7Kg / cm 2 ; Scraper hardness: 75°; After screen printing the entire substrate, let it stand for 15 minutes and pre-bake for 25 minutes at a temperature of 73°C.
[0051] Exposure energy is 700 mj / cm 2 , the exposure scale is 9 grids and the positioning accuracy is 50um.
[0052] During development of the substrate, the ink side of the substrate faces upward and the developer flushes the substrate from top to bottom.
[0053] When drying the substrate, bake the plate twice continuously, each time for one hour. The temperature of the first baking plate is set at 100±5℃, and the temperature of the second baking plate is set at 150±5℃.
[0054] See also Figure 1 and Figure 2 , Figure 1 This is a schematic diagram of the thickness of the solder resist ink for the thick copper circuit board in Example 1. Figure 2 Schematic diagram of solder mask ink thickness for medium-thick copper circuit board in comparative example 1. The product obtained by the process of embodiment 1 has uniform ink thickness at the line surface and line foot without obvious protrusions or depressions. However, the product obtained by the process of embodiment 2 has a large ink thickness difference, and the ink at the line is stepped. The first screen printing uses a 32T dot screen to print ink only on the line part of the substrate, and the second screen printing uses a 43T white screen to print ink on the entire substrate, so that the ink is only printed on the line part during the first screen printing, ensuring that the line surface and line corner ink thickness of the solder mask ink is sufficient. At the same time, the B ink with lower viscosity is prepared in the second screen printing to make When the entire substrate is printed, the ink is easier to flow. Thus, compared with the product obtained in comparative example 1, the solder resist ink of the product obtained in embodiment 1 is no longer stepped, the solder resist ink is more uniform, and the thickness of the line surface and line angle ink is sufficient; when the exposed substrate is developed, the ink side of the substrate faces downward, and the developer rinses the substrate from bottom to top. After the developer rinses to the target area of the substrate, the developer splashed outside the target area can quickly flow down the substrate, while the developer rinses the substrate from top to bottom, and the developer splashed outside the target area still stays on the substrate, resulting in over-development of the non-target area of the substrate. In this way, the problem of uneven solder resist development is solved.
[0055] Furthermore, the exposure energy is 700 mj / cm 2 Increased to 800mj / cm 2 The exposure scale is set to 9 grids, the alignment accuracy is set to 35um, and the substrate is developed after exposure. The substrate transmission speed is 4m / min, which makes the target ink exposure more thorough, the ink is more firm, and the hardness of the substrate is still moderate, ensuring the uniformity, integrity and accuracy of the solder mask and enhancing the insulation performance of the circuit.
[0056] Embodiment 2
[0057] The circuit board preparation process in this example is used to prepare a single-sided 6OZ thick copper-aluminum substrate circuit board, which includes the following steps:
[0058] Cutting, board specifications: VT-4B3 (5052-H34), 3.3mm, thermal conductivity 3.0W / mk, 6 / 0OZ, dielectric layer 75um; circuit design: minimum line width and line spacing is 10mil / 20mil, tolerance is ±20%, line width compensation is 10.24mil, the minimum line width and line spacing after compensation is 20.24mil / 9.76mil, and the circuit is made in negative film form.
[0059] The inner layer of the substrate after cutting is made: including
[0060] The substrate is subjected to wet film pretreatment after cutting, substrate conveying speed: 3.5m / min, wear scar thickness: 12±2mm, drying temperature: 85℃±5℃, water film test: water film duration ≥15s.
[0061] Coating the substrate after wet film pretreatment: coating 2 times, coating speed: 20±5 yards, wet film thickness: 14±2um.
[0062] The coated substrate is baked: the substrate is baked in a tunnel furnace once: the speed is 7±2m / min, and the six consecutive temperatures in the tunnel furnace are 100°C, 110°C, 120°C, 120°C, 110°C, and 100°C respectively.
[0063] Expose the substrate after baking using an LDI exposure machine with an exposure energy setting of 230 mj / cm 2 , exposure scale 7.5 grids, let stand for 15 minutes after exposure.
[0064] Develop the exposed substrate with a developing pressure of 2.0±0.5Kg / cm 2 , the developing temperature is 30±2℃, the developing speed is 2.4m / min, and the Na2CO3 concentration range in the developer is 0.8-1.2%.
[0065] Let the developed substrate stand or dry for 15±5min.
[0066] Perform inner layer etching on the substrate after static or drying, and the etching pressure is 2.0±0.5Kg / cm 2 , the temperature is 50±5℃, the Cu2+ concentration range is 130-160g / L, the Cl- concentration range is 170~210g / L, the pH value range is 7.5-8.2, and the specific gravity range is 1.17-1.2g / cm 3 Under the above conditions, the substrate is etched three times in sequence. In the first etching, the substrate conveying speed is 1.7±1m / min, in the second etching, the substrate conveying speed is 2.5±1m / min, and in the third etching, the substrate conveying speed is 3.5±1m / min. During the three etchings of the exposed substrate, the circuit board surface of the substrate is facing downward.
[0067] After the inner layer is etched, the substrate is stripped with a stripping pressure of 1.5±0.5kg / cm 2 The stripping temperature is 55±5℃, the substrate conveying speed is 2.2m / min, and the NaOH concentration range in the stripping solution is 0.8-1.2%.
[0068] The burrs of the substrate after film removal are processed, and the burr control range is ≤2.5mil on one side.
[0069] Perform AOI inspection on the substrate after burr treatment.
[0070] Targeting is performed on the substrate after the inner layer is manufactured, and positioning holes are opened on the substrate;
[0071] The solder resist screen printing in the first embodiment is performed on the substrate after the positioning holes are opened.
[0072] During the solder mask screen printing on the substrate, before the substrate is dried and developed, it also includes printing characters on the substrate, and the text ink is LJM-300.
[0073] Spray tin on the substrate after solder mask screen printing.
[0074] The substrate after tin spraying is subjected to forming treatment: the substrate is subjected to target shooting, laser cutting and gong plate in sequence. During target shooting, the aluminum surface of the substrate is downward, the coated drill tip is 1.80φmm, the upper drilling height is 9mm, the processing starting point is mm, the feed speed is 0.6m / min, the retracting speed is 5m / min, and the hole limit is 2000hit; during laser cutting, the aluminum surface of the substrate is upward, the cutting speed is 1m / min, the lifting height is 10mm, the nozzle height is 0.3mm, the air pressure is 1.50Bar, the peak power is 95%, the duty cycle is 70%, and the pulse frequency is 6700Hz; in gong surface, the aluminum surface of the substrate is downward, the tool diameter is 2.0mm, the rotation speed is 40m / min, the lowering speed is 0.5m / min, the retracting speed is 15m / min, and the tool life is 10m.
[0075] The quality test of the formed substrate is carried out, and the formed substrate is washed, electrically tested, FQC and FQA are carried out in sequence.
[0076] Comparative Example 2
[0077] Different from the second embodiment, in the inner layer of the substrate in this embodiment, the exposure energy is 210 mj / cm 2, 7 grids of exposure scale; etching is directly carried out after substrate development, and etching includes two times. The conveying speed of the substrate for the first etching is 1.5m / min, and the conveying speed of the substrate for the second etching is 2.3m / min. In addition, the circuit surface of the substrate is facing upward for both the first etching and the second etching; during molding, the substrate is drilled and laser cut in turn. The aluminum surface of the substrate faces upward during drilling and the aluminum surface of the substrate faces upward during laser cutting.
[0078] See also Figure 3 , Figure 4 , Figure 5 and Figure 6 , Figure 3 This is a schematic diagram of the line width and line spacing of the thick copper circuit board in the second embodiment. Figure 4 This is a schematic diagram of the structure of the thick copper circuit board prepared in Example 2. Figure 5 This is a schematic diagram of the structure of the thick copper circuit board prepared in Comparative Example 2. Figure 6 This is the second schematic diagram of the thick copper circuit board structure prepared in comparative example 2, Figure 3 It can be seen that the line width and line spacing of the thick copper circuit board meet the design requirements. Figure 4 The medium-thick copper circuit board does not have the dielectric layer falling off the hole edge or the ink falling off the board edge. Figure 5 Medium-thick copper circuit boards have dielectric layers falling off the edge of the holes. Figure 6 The medium-thick copper circuit board has ink falling off the board edge. Compared with the product obtained in comparative example 2, the product obtained in embodiment 2 further solidifies the wet film by increasing the exposure energy parameters during the inner layer production and adding a standing or drying step after development to prevent the wet film from falling off the substrate after development; the substrate etching speed is increased and the substrate conveying speed is accelerated, so that the etching liquid will not excessively erode the substrate each time the substrate is etched, and the substrate etching is more uniform, effectively solving the problem of line width, line spacing and burrs of the circuit, thereby improving the accuracy of the circuit; when etching, the circuit surface of the substrate is downward, and the etching liquid washes the substrate from bottom to top, and the sputtered etching liquid can quickly flow down the substrate, further avoiding excessive etching of the etching liquid; by optimizing the substrate drilling and laser forming into target shooting, laser, and gong plate forming, a new process of pre-cutting and then CNC gong plate is used to solve the problems of excessive accuracy of positioning holes in the substrate, loss of dielectric layer at the hole edge, no blackening at the board edge, and no ink falling at the board edge, which not only improves the performance of the product, but also improves the appearance and reliability of the product, and has significant advantages.
[0079] Embodiment 3
[0080] The single-sided 6OZ thick copper-aluminum substrate circuit board in this example is manufactured by the circuit board manufacturing process in Example 2.
[0081] In summary, the first screen printing uses a 32T dot screen to print ink only on the circuit part of the substrate, and the second screen printing uses a 43T white screen to print ink on the entire substrate, so that the ink is only printed on the circuit part during the first screen printing, ensuring that the line surface and line angle ink thickness of the solder mask ink is sufficient. At the same time, the B ink solution with lower viscosity is modulated in the second screen printing, so that the ink is easier to flow when the entire substrate is printed. In this way, the solder mask ink is no longer stepped, the solder mask ink is more uniform, and the line surface and line angle ink thickness is sufficient; when the exposed substrate is developed, the ink side of the substrate faces downward, and the developer rinses the substrate from bottom to top. After the developer rinses to the substrate and displays the target area, the developer splashed outside the target area can quickly flow down the substrate, while the developer rinses the substrate from top to bottom, and the developer splashed outside the target area still stays on the substrate, causing the non-target area of the substrate to be over-developed. In this way, the problem of uneven solder mask development is solved.
[0082] The above is only the implementation mode of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present application should be included in the scope of the claims of the present application.
Claims
1. A solder resist screen printing process, characterized in that: include: Pre-process the substrate: clean, grind and roughen the copper surface; The first screen printing is performed on the substrate: ink solution A is prepared, and the circuit part of the substrate is printed with ink solution A using a 32T dot screen, and the substrate is pre-baked; Perform the second screen printing on the substrate: prepare the B ink solution, use 43T white screen to print the B ink solution on the substrate, and pre-bake the substrate; Expose the substrate with screen printing ink: The substrate with screen printing ink is shielded by a film base, and the circuit diagram part of the substrate is exposed by ultraviolet radiation; Developing the exposed substrate: using a developer to rinse the exposed substrate, with the ink side of the substrate facing downward; Drying the developed substrate: When baking the board, the temperature gradually increases from low to high; Among them, the proportion of open oil water to ink in A ink solution is less than the proportion of open oil water to ink in B ink solution.
2. The solder resist screen printing process according to claim 1, characterized in that: In ink solution A, the ratio of oil-opening water to ink is 250±10ml:4Kg; in ink solution B, the ratio of oil-opening water to ink is 300±10ml:4Kg.
3. The solder resist screen printing process according to claim 1, characterized in that: When exposing the substrate of the screen printing ink, the LDI method is used to expose the substrate, and the exposure energy is 800mj / cm 2 The exposure scale is 9 grids and the positioning accuracy is 35um. During the development of the exposed substrate, the substrate transmission speed is 4m / min.
4. The solder resist screen printing process according to claim 1, characterized in that: After drying and development, the substrate is baked four times continuously, each time for one hour. The temperature of the first baking is set to 80±5℃, the second baking is set to 100±5℃, the third baking is set to 120±5℃, and the fourth baking is set to 150±5℃.
5. A circuit board preparation process, characterized in that: Cutting: Cut out 6OZ thick copper-aluminum substrate; The inner layer of the substrate after cutting is made: the substrate is pre-treated, coated, baked, exposed, developed, inner layer etched, film stripped, burr treated and AOI are carried out in sequence; Using any solder resist screen printing process in claims 1-4 to perform solder resist screen printing on the substrate having the inner layer manufactured; Spray tin on the substrate after solder mask silk screen printing; The substrate after tin spraying is subjected to forming treatment: the substrate is subjected to target shooting, laser cutting and gong plate in sequence; Perform quality tests on the formed substrates.
6. The circuit board preparation process according to claim 5, characterized in that: After cutting, the substrate is exposed to the inner layer by LDI method, and the exposure energy is 230mj / cm 2 , the exposure scale is 7 and a half stops.
7. The circuit board preparation process according to claim 6, characterized in that: In the inner layer production of the substrate after cutting, etching includes: The exposed substrate is etched for the first time, and the etching conveying speed is 1.7±1m / min; The exposed substrate is etched for the second time, and the etching conveying speed is 2.5±1m / min; The exposed substrate is etched for the third time, and the etching transfer speed is 3.5±1m / min.
8. The solder resist screen printing process according to claim 7, characterized in that: When etching the exposed substrate, the circuit board side of the substrate faces downward.
9. A single-sided 6OZ thick copper-aluminum substrate circuit board, characterized in that: The circuit board is manufactured by any circuit board manufacturing process according to claims 5-8.
Citation Information
Cited By
Method and device for improving flatness of PCB white oil block
CN120692772A