Replacing and replacing construction method of elevated bridge stand column
By cutting out the concrete on the top of the viaduct bridge columns, adjusting the steel bars, and re-pouring the repaired concrete, the problem of vertical deviation of the prefabricated columns was solved, construction efficiency was improved, costs were reduced, and the impact on the environment was reduced.
Patent Information
- Application Number
- CN202411206096.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-10-25
AI Technical Summary
The prefabricated installation of existing viaduct bridge columns often causes misalignment of connection positions due to verticality deviation, resulting in extended construction period, increased cost and greater environmental impact.
The method is to cut out part of the concrete on the top of the original column, adjust the exposed steel bars, and re-pour the repair concrete to correct the verticality to form a new column, avoiding the complicated process of complete dismantling and reinstallation.
It improves construction efficiency, reduces costs, reduces the impact on the surrounding environment, and achieves precise correction of column verticality.
Smart Images

Figure CN118835532A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of elevated bridge construction, and in particular to a dismantling and replacement construction method for elevated bridge columns. Background Art
[0002] Columns and cap beams are important components of urban elevated bridges. Columns are vertical load-bearing components of bridges. Cap beams are usually set on top of columns and connect multiple columns. Cap beams play a role in supporting superstructures such as bridge deck beams or bridge decks. However, the existing prefabricated columns often fail to meet the installation verticality requirements, resulting in misalignment of the connection position between the prefabricated columns and the prefabricated cap beams, making it impossible to accurately connect the two.
[0003] In response to this problem, when the verticality deviation of the prefabricated column installation exceeds the design allowable value, the conventional construction method is mainly to completely remove the prefabricated columns that do not meet the verticality requirements, and reinstall new prefabricated columns after all are removed until the verticality requirements are met. This construction method of complete removal and reinstallation not only prolongs the construction period, but also increases the construction cost of the project, and will have a long-term impact on the surrounding environment.
[0004] Therefore, it is urgent to propose a replacement construction method for elevated bridge columns to solve the above technical problems. Summary of the invention
[0005] The object of the present invention is to provide a method for dismantling and replacing a viaduct bridge column, which can avoid the complicated process of complete dismantling and reinstallation, thereby improving construction efficiency, reducing costs, and reducing the impact on the surrounding environment.
[0006] As conceived above, the technical solution adopted by the present invention is:
[0007] The present invention provides a method for dismantling and replacing a column of an elevated bridge, comprising:
[0008] S1. Chisel away part of the original concrete at two ends of the top surface of the original column along the height direction of the original column to a first preset depth, so that the first steel bars inside the original column at the two chiseled positions are exposed;
[0009] The original column is inclined in a first direction, the opposite direction of the first direction is a second direction, one of the two end heads is located at an edge of the top surface facing the first direction, and the other of the two end heads is located at an edge of the top surface facing the second direction;
[0010] S2, cutting off a portion of the length of the top of the first steel bar at the chiseling position, and tilting the remaining first steel bars after cutting off at a preset angle toward the second direction;
[0011] S3, overlapping the second steel bar on the top of the inclined first steel bar, the second steel bar extending in the vertical direction so that the second steel bar can correspond to the position of the sleeve in the cap beam;
[0012] S4, re-pour repair concrete at the two chiseled positions so that the repair concrete wraps the inclined first steel bar, and wait for the repair concrete to solidify to form a new column.
[0013] In some embodiments, the step S1 includes:
[0014] S100, setting up an operating platform on the original column, wherein the operating platform is used to carry operators to perform construction.
[0015] In some embodiments, the operating platform includes a first support member, a second support member, a connecting member and a bearing plate, wherein the first support member is disposed at the bottom of the operating platform, the bearing plate is disposed on the first support member and surrounds the outer periphery of the original column, the second support member is disposed at the top of the original column, and the connecting member is connected between the first support member and the second support member;
[0016] In the step S100, setting up an operating platform on the original column specifically includes:
[0017] S101, cross-arrange the first support members in the longitudinal and transverse directions and connect them to the original columns;
[0018] S102, setting the second support member on the top of the original column;
[0019] S103, using the connecting member to connect the first supporting member and the second supporting member along the height direction of the original column;
[0020] S104, disposing the carrying plate on the first supporting member.
[0021] In some embodiments, after the carrying plate is arranged on the first supporting member, the method further comprises:
[0022] A guardrail is arranged on the bearing plate.
[0023] In some embodiments, after the guardrail is provided on the carrying plate, the method further comprises:
[0024] A protective net is arranged on the guardrail, and the protective net can shield the chiseling position.
[0025] In some embodiments, when the second steel bar is overlapped to the first steel bar, the net distance between the steel bars is not less than 50 mm, and the steel bar protective layer is not less than 20 mm.
[0026] In some embodiments, before step S4, the method further includes:
[0027] A repair stirrup is connected to the outer periphery of the first steel bar after inclination, and the repair stirrup is fixedly connected to the original stirrup.
[0028] In some embodiments, after step S1, the method further includes:
[0029] The chiseled surface after the original concrete is chiseled is roughened so that the rough surface unevenness difference of the chiseled surface after the roughening treatment is not less than 6 mm, and at least half of the coarse aggregate in the chiseled surface after the roughening treatment is exposed.
[0030] In some embodiments, step S1 further includes:
[0031] The original concrete is chiseled off at the top surface between the two chiseled off positions to a second preset depth, so that the first steel bar inside the top surface between the two chiseled off positions is exposed.
[0032] In some embodiments, step S4 includes:
[0033] S41, setting up a set steel mold on the original column, and the set steel mold and the two chiseled positions are enclosed to form a casting space;
[0034] S42, pouring the repair concrete into the pouring space;
[0035] S43, after the repair concrete solidifies, the shaping steel formwork and the operating platform are removed in sequence.
[0036] Beneficial effects of the present invention:
[0037] The method for replacing the columns of an elevated bridge provided by the present invention can correct or eliminate the verticality deviation of the original column without the complicated process of completely removing the original column and reinstalling the new column, by first chiseling away part of the concrete on the top of the original column, then adjusting the first steel bar exposed at the chiseled away position, and re-pouring the repair concrete. This helps to improve construction efficiency, reduce investment costs, and reduce the impact of the long-term construction of complete removal and reinstallation on the surrounding environment. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.
[0039] Figure 1 It is a schematic diagram of a three-dimensional structure in which an operating platform provided by an embodiment of the present invention is erected on an original column;
[0040] Figure 2 It is a schematic diagram of a three-dimensional structure after a part of the original concrete at the end is chiseled off according to an embodiment of the present invention;
[0041] Figure 3 It is a schematic diagram of a three-dimensional structure after the second steel bar is overlapped to the first steel bar provided by an embodiment of the present invention;
[0042] Figure 4 It is a schematic diagram of a three-dimensional structure after pouring repair concrete from a viewing angle provided by an embodiment of the present invention;
[0043] Figure 5 is a schematic diagram of a three-dimensional structure after pouring repair concrete from another perspective provided by an embodiment of the present invention;
[0044] Figure 6 It is a schematic diagram of the coordination between the original column and the cap beam provided by an embodiment of the present invention;
[0045] Figure 7 is a schematic diagram of the top surface of an original column provided by an embodiment of the present invention;
[0046] Figure 8 It is a schematic diagram of the coordination between the original upright column and the cap beam after correction provided by an embodiment of the present invention;
[0047] Fig. 9 is a schematic diagram of the top surface of the original column after correction provided by an embodiment of the present invention;
[0048] Fig.10 It is an internal schematic diagram of an original column connected to a cap beam after correction provided by an embodiment of the present invention;
[0049] Fig.11 yes Fig.10 The schematic diagram of the cap beam and repaired stirrups is hidden in the figure;
[0050] Fig.12 It is a structural schematic diagram of an original column provided by an embodiment of the present invention;
[0051] Fig.13 It is a schematic diagram of the structure of the column root provided by an embodiment of the present invention.
[0052] In the figure:
[0053] 1. Original column; 11. Top surface; 111. End; 12. Column base;
[0054] 2. The first steel bar;
[0055] 3. Second steel bar;
[0056] 4. Cap beam; 41. Sleeve;
[0057] 5. Operating platform; 51. First support member; 52. Second support member; 53. Connecting member; 54. Loading plate; 55. Guardrail;
[0058] 6. Repair stirrups;
[0059] 7. Finalize the steel mold. DETAILED DESCRIPTION
[0060] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0061] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0062] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0063] In the description of the present invention, it should be noted that the terms "upper", "lower", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or are the positions or positional relationships in which the inventive product is usually placed when in use. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance. In the description of the present invention, unless otherwise specified, "multiple" means two or more.
[0064] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "disposed" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0065] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0066] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0067] like Figures 1 to 11 As shown, the method for dismantling and replacing the viaduct bridge column provided in this embodiment includes:
[0068] S1, along the height direction of the original column 1, chisel away part of the original concrete at the two ends 111 of the top surface 11 of the original column 1 to a first preset depth, so that the first steel bars 2 inside the original column 1 at the two chiseled positions are exposed;
[0069] The original column 1 is inclined in a first direction, the opposite direction of the first direction is a second direction, one of the two end heads 111 is located at an edge of the top surface 11 facing the first direction, and the other of the two end heads 111 is located at an edge of the top surface 11 facing the second direction;
[0070] S2, cutting off a portion of the length of the top of the first steel bar 2 at the chiseled position, and tilting the remaining first steel bars 2 after cutting off toward the second direction at a preset angle;
[0071] S3, overlapping the second steel bar 3 on the top of the inclined first steel bar 2, the second steel bar 3 extending in the vertical direction so that the second steel bar 3 can correspond to the position of the sleeve 41 in the cap beam 4;
[0072] S4, re-pour the repair concrete at the two chiseled positions so that the repair concrete wraps the inclined first steel bar 2, and wait for the repair concrete to solidify to form a new column. Among them, the repair concrete can be made of UHPC (Ultra-High Performance Concrete), which has higher strength, durability and crack resistance than traditional concrete.
[0073] After the new column is formed, the verticality deviation of the new column is corrected or eliminated. After confirming that the new column meets the design strength, the cap beam 4 can be hoisted for the new column to connect the exposed second steel bar 3 to the sleeve 41 in the cap beam 4. In step S3, when the second steel bar 3 is overlapped on the top of the inclined first steel bar 2, a positioning plate or a limit plate can be used to match the position of the sleeve 41 to ensure the accuracy of the position of the second steel bar 3 and ensure that the second steel bar 3 does not shift during the subsequent pouring of repair concrete.
[0074] For example, Figure 6 to Figure 11 As shown, the first direction is along the longitudinal direction of the bridge toward the side with a large pile number, and the second direction is toward the side with a small pile number. It can be understood that: at this time, the original column 1 with a deviation in verticality is inclined toward the side with a large pile number, and the original column 1 is biased toward the side with a large pile number relative to the cap beam 4, resulting in the original column 1 and the cap beam 4 being unable to be effectively connected due to misalignment. Therefore, when part of the original concrete is chiseled off in step S1, in order to ensure that the internal first steel bars 2 at the two chiseling positions are effectively exposed and to prevent eccentricity in the subsequent correction process, from the top view of the top surface 11, the chiseled area at the end 111 on the side with a large pile number is larger than the chiseled area at the end 111 on the side with a small pile number (such as Figure 7The shaded area shown is the chiseled area). After the subsequent correction steps S2 to S4 are executed, since the remaining first steel bars 2 after being cut are all tilted toward the second direction at a preset angle, that is, tilted toward the side of the small pile number at a preset angle, after the repair concrete is re-poured, the re-poured areas at the two chiseled positions are substantially the same (e.g. Fig. 9 The shaded area shown is the area where the repair concrete is re-poured), that is, the new column formed after the re-pour is offset to the side of the small pile number, so as to achieve the purpose of correcting or eliminating the verticality deviation of the original column 1.
[0075] Among them, large pile numbers and small pile numbers are commonly used in bridge construction and will not be introduced in detail here.
[0076] The method for replacing the columns of an elevated bridge provided in this embodiment can correct or eliminate the verticality deviation of the original column 1 without the complicated process of completely removing the original column 1 and reinstalling a new column, by first chiseling away part of the concrete on the top of the original column 1, then adjusting the exposed first steel bar 2 at the chiseled-away position, and re-pouring the repair concrete. This helps to improve construction efficiency, reduce investment costs, and reduce the impact of the long-term construction of complete removal and reinstallation on the surrounding environment.
[0077] Optionally, in step S1, the first preset depth can be 50 cm to 80 cm, such as 50 cm, 60 cm, 70 cm, 80 cm, etc., which can be determined according to actual conditions and is not specifically limited here. Preferably, in this embodiment, the first preset depth is set to 60 cm, that is, 60 cm of the original concrete is chiseled downward from the top surface 11.
[0078] When the original concrete is chiseled off in step S1, the first steel bar 2 inside needs to be retained and cannot be removed as a whole by a chain saw. Therefore, a large water-grinding drill is used to perform row drilling to remove the original concrete, and a pneumatic pick is used to perform local processing on the reserved position of the first steel bar 2.
[0079] Optionally, in step S2, the cut-off length of the top of the first steel bar 2 can be 10 cm to 20 cm, such as 10 cm, 15 cm, 20 cm, etc., which can be determined according to actual conditions and is not specifically limited here. Preferably, in this embodiment, the cut-off length of the top of the first steel bar 2 is set to 15 cm. The preset angle of inclination of the remaining first steel bar 2 in the second direction after truncation can be 5° to 8°, such as 5°, 6°, 7°, 8°, etc., which can be determined according to the degree of vertical deviation of the original column 1, and is not specifically limited here. Preferably, in this embodiment, the preset angle of inclination of the first steel bar 2 is set to 6°.
[0080] It should be noted that the cut-off length of the top of the first steel bar 2 and the preset angle at which the remaining first steel bar 2 after truncation is inclined in the second direction both need to be designed and selected based on the degree of verticality deviation of the original column 1 to ensure the verticality correction effect and to ensure that the new column has sufficient strength.
[0081] In order to ensure that the new column and the cap beam 4 can be stably connected, in some embodiments, step S1 further includes:
[0082] The original concrete is chiseled off at the top surface 11 between the two chiseled positions to a second preset depth, so that the first steel bars 2 inside the top surface 11 between the two chiseled positions are exposed. In this way, if the connection length of the second steel bars 3 inserted into the sleeve 41 is insufficient, the exposed first steel bars 2 between the two chiseled positions can have a sufficient length to achieve a stable connection with the cap beam 4.
[0083] Optionally, the second preset depth can be 9cm to 12cm, for example, 9cm, 10cm, 11cm, 12cm, etc., which can be determined according to actual conditions and is not specifically limited here; preferably, in this embodiment, the second preset depth is set to 10cm, that is, 10cm deep of original concrete is chiseled downward at the top surface 11 between the two chiseling positions.
[0084] In specific implementation, in order to facilitate construction, the top surface 11 of the original column 1 can be chiseled downward to the second preset depth as a whole, and then the two end heads 111 can be chiseled downward to the first preset depth.
[0085] In some embodiments, when the second steel bar 3 is overlapped with the first steel bar 2, the clear distance between the steel bars is not less than 50 mm, and the steel bar protective layer is not less than 20 mm. The structure formed after the second steel bar 3 is overlapped with the first steel bar 2 is regarded as an integral steel bar, which means that for multiple integral steel bars, the clear distance between the steel bars is not less than 50 mm, and the steel bar protective layer is not less than 20 mm.
[0086] Among them, the clear distance between the steel bars refers to the distance between the outer surfaces of two adjacent steel bars. The steel bar protection layer refers to the thickness of the concrete between the outer surface of the steel bar and the outer surface of the concrete structure. In other words, the steel bar protection layer is the thickness of the concrete layer wrapped around the steel bar. When setting the steel bars, the distance must be controlled to ensure the thickness of the steel bar protection layer formed by subsequent pouring.
[0087] With this setting, the minimum clear distance between the steel bars is 50mm, ensuring that the subsequent pouring of repair concrete can be fully filled between the steel bars to form a strong bond. The steel bar protective layer of not less than 20mm helps prevent corrosion of the steel bars and increase the durability of the structure.
[0088] like Fig.10 As shown, in some embodiments, before step S4, the method further includes:
[0089] The repair stirrups 6 are connected to the outer periphery of the inclined first steel bar 2, and the repair stirrups 6 are fixedly connected to the original stirrups. That is, the repair stirrups 6 need to be connected in place before pouring the repair concrete.
[0090] Through such a setting, the repair stirrups 6 are connected to the adjusted first steel bars 2, which can provide support and reinforcement for the adjusted first steel bars 2, and further fix the repair stirrups 6 to the original stirrups, forming an overall support and reinforcement system, which can ensure that after the repair concrete is poured, the entire repair area has good strength and durability, and avoid structural defects after the repair concrete hardens.
[0091] Optionally, the repair stirrup 6 is connected to the original stirrup by welding. Specifically, when double-sided welding is used, the welding length is 5 times the diameter of the steel bar, while when single-sided welding is used, the welding length is 10 times the diameter of the steel bar. For example, if the diameter of the steel bar is 20 mm, the welding length of double-sided welding is 100 mm, and the welding length of single-sided welding is 200 mm.
[0092] In some embodiments, after step S1, the method further includes:
[0093] The chiseled surface after the original concrete is chiseled is roughened so that the rough surface unevenness difference of the chiseled surface after the chiseling treatment is not less than 6mm, and at least half of the coarse aggregate in the chiseled surface after the chiseling treatment is exposed.
[0094] Among them, coarse aggregate refers to the larger particles of stone in concrete. They are one of the basic components of concrete. Coarse aggregate plays the role of "skeleton" in concrete, supporting and dispersing the load, thereby increasing the strength of concrete.
[0095] Through such a setting, the surface roughness of the chiseled surface is increased and the coarse aggregate is exposed, so that the repair concrete can not only be better embedded in these chiseled surfaces with irregular surfaces during pouring, but also directly contact with the coarse aggregate, which is conducive to forming a strong mechanical lock and enhancing the bonding strength between the new and old concrete.
[0096] In some embodiments, step S1 includes:
[0097] S100, an operating platform 5 is set up on the original column 1, and the operating platform 5 is used to carry operators to perform construction. Since the height of the original column 1 is generally high, and the correction and remedial work in this embodiment is performed at the top of the column, the operating platform 5 provides a convenient and safe working platform for the operators to perform construction work.
[0098] like Figure 1 to Figure 3As shown, in some embodiments, the operating platform 5 includes a first support member 51, a second support member 52, a connecting member 53 and a bearing plate 54. The first support member 51 is arranged at the bottom of the operating platform 5, and the bearing plate 54 is arranged on the first support member 51 and surrounds the outer periphery of the original column 1. The bearing plate 54 is for operators to stand during construction. The second support member 52 is arranged on the top of the original column 1, and the connecting member 53 is connected between the first support member 51 and the second support member 52.
[0099] In step S100, an operating platform 5 is set up on the original column 1, which specifically includes:
[0100] S101, cross-arrange the first support member 51 along the longitudinal and transverse directions and connect it to the original column 1; wherein the longitudinal and transverse directions refer to the longitudinal bridge direction and the transverse bridge direction; specifically, the first support member 51 can be fastened and locked to the original column 1 by using fine-rolled threaded steel bars;
[0101] S102, setting the second support member 52 on the top of the original column 1;
[0102] S103, using the connecting member 53 to connect the first supporting member 51 and the second supporting member 52 along the height direction of the original column 1;
[0103] S104 , disposing a carrying plate 54 on the first supporting member 51 .
[0104] Through such an arrangement, the connecting member 53 connects the first supporting member 51 and the second supporting member 52 to form a whole, so that the overall stability of the operating platform 5 is better, thereby improving the safety performance during construction.
[0105] Optionally, the contact surface between the first support member 51 and the original column 1, and the contact surface between the second support member 52 and the original column 1 are padded with rubber material to increase friction resistance and improve connection stability.
[0106] Optionally, the first support member 51 and the second support member 52 include but are not limited to square steel.
[0107] Optionally, the connecting member 53 includes but is not limited to being a precision-rolled threaded steel bar.
[0108] Optionally, the bearing plate 54 can be configured as a patterned steel plate, and the patterned steel plate can increase a certain contact friction force.
[0109] In some embodiments, after the supporting plate 54 is arranged on the first supporting member 51 , the method further includes: arranging a guardrail 55 on the supporting plate 54 .
[0110] By providing the guardrail 55 , the safety of the operating platform 5 is further improved.
[0111] In some embodiments, after the guardrail 55 is arranged on the bearing plate 54 , the method further includes: arranging a protective net on the guardrail 55 , and the protective net can shield the chiseling position.
[0112] Specifically, the protective net is configured as a dense mesh net, and the dense mesh net is wrapped around and covers the guardrail 55 .
[0113] This arrangement can effectively prevent waste and debris generated during the concrete removal process from splashing onto the driveway, thus protecting the safety of pedestrians and vehicles under the driveway.
[0114] like Figure 4 and Figure 5 As shown, in some embodiments, step S4 includes:
[0115] S41, setting up a set steel formwork 7 on the original column 1, and the set steel formwork 7 and the two chiseled positions are enclosed to form a casting space;
[0116] S42, pouring repair concrete into the pouring space; illustratively, a hopper may be used to pour the repair concrete;
[0117] S43, after the repaired concrete solidifies, the shaping steel formwork 7 and the operating platform 5 are removed in sequence.
[0118] Specifically, when the shaping steel mold 7 is erected in step S41, flanges and pull rods may be provided at the top and bottom of the shaping steel mold 7 for locking until the shaping steel mold 7 remains stable, and then step S42 is performed.
[0119] By using the shaped steel formwork 7, the shape of the repair concrete after pouring can be effectively controlled to be consistent with the design expectations, which not only improves the accuracy of the construction, but also ensures the safety and reliability of the structure.
[0120] The method for dismantling and replacing the columns of the viaduct bridge in the above embodiment can avoid the long-term construction of complete dismantling and reinstallation by first chiseling away part of the concrete on the top of the original column 1, then adjusting the first steel bar 2 exposed at the chiseled position, and re-pouring the repair concrete. However, this method is well applicable to the case where the verticality deviation of the original column 1 is small. When the verticality deviation of the original column 1 is large, that is, when the inclination angle of the original column 1 is large, at this time, if the above method is adopted, it is necessary to deepen the chiseling depth of the part of the concrete on the top of the original column 1, and the subsequent steel bar correction and re-pouring of the repair concrete are also difficult.
[0121] To this end, this embodiment also provides a method for dismantling and replacing an elevated bridge column when the verticality deviation of the original column 1 is large, comprising the following steps:
[0122] Cut and hoist the original column 1 in sections, and retain the column base 12 of the original column 1;
[0123] Chisel downwards from the top of the column root 12 to a third preset depth, retaining the main reinforcement during the chiseling;
[0124] Reinstall the upper post on top of the post base.
[0125] For example, Fig.12 and Fig.13 As shown, to ensure the safety of the cutting construction, it can be divided into 2 sections for cutting, which are planned to be divided into 9.5-meter and 10.4-meter sections, with a total of 2 sections for cutting and hoisting. The remaining last 2.6 meters of the column root 12 is chiseled out, and 0.42 meters is chiseled down from the top to retain the main reinforcement. After grinding the contact surface, the upper column is reinstalled. Before reinstalling the upper column, the position of the main reinforcement retained on site must be matched when prefabricating the upper column.
[0126] The column root 12 after chiseling from the top downwards is as follows Fig.13 As shown, the height of the retained column root 12 is 2.2 meters, and there is still a certain verticality deviation. Here, the slurry layer is used to adjust the positioning of the upper column so that the verticality of the upper column no longer expands in the inclined direction of the column root 12 when the upper column is positioned. The reinstalled upper column and the column root 12 together form a new column, so that the verticality of the new column meets the design requirements.
[0127] With such an arrangement, only the upper part of the original column 1 needs to be cut and removed, and the column root 12 of the original column 1 can be retained. Compared with the method of completely removing the original column 1, the construction workload can be reduced and the construction efficiency can be improved.
[0128] Specifically, when cutting and hoisting the original column 1, the cutting is carried out by using a diamond chain process, and the hoisting is carried out by using a crawler crane.
[0129] The details of the removal of the original column 1 are as follows:
[0130] Step 1: Use a climbing vehicle to wind the diamond rope around the driving wheel and auxiliary wheel in a certain order according to the determined cutting form. Note that the direction of the rope should be consistent with the driving direction of the driving wheel. Pre-temporarily fix the cutting segment through the lifting point, and use the crawler crane to pre-load 50% of the body weight. At this time, the load rate of the crawler crane is 45%.
[0131] Step 2: Start the electric motor, adjust the driving wheel lifting tension through the control panel, ensure that the diamond rope is properly tightened, supply circulating cooling water, and then start another electric motor to drive the driving wheel to drive the diamond rope to rotate and cut. During the cutting process, the stability of the machine base must be closely observed, and the offset of the guide wheel must be adjusted at any time to ensure that the cutting rope is in the same plane.
[0132] During the cutting process, the cutting parameters are adjusted by operating the control panel. The speed of the diamond rope is about 20m / s. On the other hand, sufficient flushing liquid should be ensured during the cutting process to cool the diamond rope and take away the grinding chips. The cutting operation should be stable in speed, parameters and equipment.
[0133] When the cutting depth reaches half of the original column 1, insert a steel plate of about 10mm to fill the gap. In addition, prepare 1mm / 3mm / 5mm adjustment steel plates to ensure that the gap can be filled.
[0134] When cutting to the outermost steel bars on the side of the original column 1, slow down the cutting progress, pay close attention to the status of the column, and continue after inserting steel plates to cushion the side.
[0135] Step 3: After cutting is completed, lift each cut segment.
[0136] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for dismantling and replacing a column of an elevated bridge, characterized in that: include: S1, chiseling away part of the original concrete at two ends (111) of the top surface (11) of the original column (1) to a first preset depth along the height direction of the original column (1), so that the first steel bars (2) inside the original column (1) at the two chiseled positions are exposed; The original column (1) is inclined in a first direction, the opposite direction of the first direction is a second direction, one of the two end heads (111) is located at an edge of the top surface (11) facing the first direction, and the other of the two end heads (111) is located at an edge of the top surface (11) facing the second direction; S2, cutting off a portion of the length of the top of the first steel bar (2) at the chiseled-off position, and tilting the remaining first steel bar (2) after cutting off toward the second direction at a preset angle; S3, overlapping the second steel bar (3) on the top of the inclined first steel bar (2), wherein the second steel bar (3) extends in a vertical direction and enables the second steel bar (3) to correspond to the position of the sleeve (41) in the cap beam (4); S4, re-pour repair concrete at the two chiseled positions so that the repair concrete wraps the inclined first steel bar (2), and wait for the repair concrete to solidify to form a new column.
2. The method for dismantling and replacing a viaduct bridge column according to claim 1, characterized in that: The step S1 includes: S100, setting up an operating platform (5) on the original column (1), wherein the operating platform (5) is used to carry operators to perform construction.
3. The method for dismantling and replacing a viaduct bridge column according to claim 2, characterized in that: The operating platform (5) comprises a first supporting member (51), a second supporting member (52), a connecting member (53) and a bearing plate (54); the first supporting member (51) is arranged at the bottom of the operating platform (5); the bearing plate (54) is arranged on the first supporting member (51) and surrounds the outer periphery of the original column (1); the second supporting member (52) is arranged at the top of the original column (1); and the connecting member (53) is connected between the first supporting member (51) and the second supporting member (52); In the step S100, setting up an operating platform (5) on the original column (1) specifically includes: S101, cross-arrange the first support member (51) in the longitudinal and transverse directions and connect it to the original column (1); S102, placing the second support member (52) on the top of the original column (1); S103, using the connecting member (53) to connect the first supporting member (51) and the second supporting member (52) along the height direction of the original column (1); S104, arranging the carrying plate (54) on the first supporting member (51).
4. The method for dismantling and replacing a viaduct bridge column according to claim 3, characterized in that: After the carrying plate (54) is arranged on the first supporting member (51), the method further comprises: A guardrail (55) is arranged on the carrying plate (54).
5. The method for dismantling and replacing a viaduct bridge column according to claim 4, characterized in that: After the guardrail (55) is arranged on the bearing plate (54), the method further comprises: A protective net is arranged on the guardrail (55), and the protective net can shield the chiseling position.
6. The method for dismantling and replacing a viaduct bridge column according to claim 1, characterized in that: When the second steel bar (3) is overlapped to the first steel bar (2), the net distance between the steel bars is not less than 50 mm and the steel bar protective layer is not less than 20 mm.
7. The method for dismantling and replacing a viaduct bridge column according to any one of claims 1 to 6, characterized in that: Before step S4, the method further includes: A repair stirrup (6) is connected to the outer periphery of the tilted first steel bar (2), and the repair stirrup (6) is fixedly connected to the original stirrup.
8. The method for dismantling and replacing a viaduct bridge column according to any one of claims 1 to 6, characterized in that: After step S1, the method further includes: The chiseled surface after the original concrete is chiseled is roughened so that the rough surface unevenness difference of the chiseled surface after the roughening treatment is not less than 6 mm, and at least half of the coarse aggregate in the chiseled surface after the roughening treatment is exposed.
9. The method for dismantling and replacing a viaduct bridge column according to any one of claims 1 to 6, characterized in that: The step S1 further comprises: The original concrete is chiseled off at the top surface (11) between the two chiseling positions to a second preset depth, so that the first steel bar (2) inside the top surface (11) between the two chiseling positions is exposed.
10. The method for dismantling and replacing a viaduct bridge column according to any one of claims 2 to 5, characterized in that: The step S4 comprises: S41, placing a set steel mold (7) on the original column (1), wherein the set steel mold (7) and the two chiseled-out positions are enclosed to form a casting space; S42, pouring the repair concrete into the pouring space; S43, after the repair concrete solidifies, the shaping steel formwork (7) and the operating platform (5) are removed in sequence.