Advanced polysilicon resistor and CMOS transistor
By forming the resistor body and the transistor gate on the semiconductor layer, and forming a silicide barrier structure on the sidewall spacers, combined with millisecond annealing technology, the problem of complex steps in the simultaneous formation of polysilicon resistors and transistors in the existing technology is solved. This enables low-cost, efficient resistor manufacturing with better temperature coefficient performance and selectivity.
Patent Information
- Application Number
- CN202380026878.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-06
- Filing Date
- 2023-04-04
- Publication Date
- 2024-10-29
AI Technical Summary
In the existing semiconductor integrated circuit manufacturing process, the simultaneous formation of polysilicon resistors and transistors is complicated, increasing manufacturing costs and complexity, especially for zero temperature coefficient of resistance (ZTCR) resistors that require additional steps such as patterning and resisting. Etchants are removed, resulting in an increase in overall manufacturing costs.
Employing a method that includes forming a resistor body and transistor gate on a semiconductor layer and forming a silicide barrier structure on its sidewall spacers while simultaneously performing a millisecond anneal on the resistor body and transistor gate to achieve resistance temperatures Formation of polysilicon resistors with coefficients in the range of ±100ppm/°C.
This approach reduces manufacturing steps, lowers costs, improves resistor performance and consistency, achieves near-zero temperature coefficient performance at widths smaller than traditional ZTCR resistors, and provides selectivity to resistor types that are suitable for for applications of different IC sizes.
Smart Images

Figure CN118872057A_ABST
Abstract
Description
Background Art
[0001] Examples relate to semiconductor integrated circuit (IC) fabrication, and more particularly, to ICs fabricated in a process that simultaneously forms portions of the IC polysilicon resistors and transistors.
[0002] IC manufacturing of multiple devices such as resistors and transistors involves multiple steps, where the same step can often be used to form a portion of each device at the same time. However, in some instances, one or more additional steps may be required for one device or the other, or a step that is entirely or primarily for one device may have a counter-effect on another device. For example, an example of a polysilicon resistor is called a "zero temperature coefficient of resistance" (ZTCR) resistor, which is sometimes also referred to as having a zero temperature coefficient, meaning that there is little or no change in resistance over a certain temperature range. Some baseline ZTCR resistor manufacturing processes require additional steps, including, for example, patterning, implantation (e.g., with boron), and resist removal, in order to achieve the desired ZTCR, but at the same time increase IC manufacturing complexity and cost. There are many other examples, particularly where one or more steps may be required to form a structure or a group of structures that may affect other structures or affect the overall cost or complexity at the same time. In addition, in the case where steps are required for one device but not the other, the overall manufacturing cost is increased compared to steps that form a portion of two devices at the same time.
[0003] While previously implemented in various baseline arrangements, this document provides examples of how some of the above concepts can be improved upon, as detailed below. Summary of the invention
[0004] A method for forming an integrated circuit includes: first, forming a resistor body and a transistor gate from a semiconductor layer; second, forming a sidewall spacer adjacent to the resistor body and the transistor gate; third, forming a silicide blocking structure above at least a portion of the resistor body; and fourth, simultaneously performing millisecond annealing on the resistor body and the transistor gate.
[0005] Another aspect provides an integrated circuit comprising a semiconductor substrate and a first polysilicon resistor positioned relative to the semiconductor substrate. The first polysilicon resistor comprises a majority dopant concentration of an n-type dopant and has a temperature coefficient of resistance (TC) within a range of ±100 ppm / °C. A second polysilicon resistor is positioned relative to the semiconductor substrate and comprises a majority dopant concentration of a p-type dopant and has a TC of resistance within a range of ±100 ppm / °C.
[0006] Other aspects are also described and claimed. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figures 1 to 10are cross-sectional views showing successive stages of fabrication of a semiconductor structure and the resulting structure.
[0008] Fig.11 is a flow chart of an example embodiment method for manufacturing a semiconductor structure, and its steps correspond to Figures 1 to 10 The corresponding one in .
[0009] Fig.12 is a resistance plot of three resistor types, including Fig.11 Those resistor types manufactured by this method. DETAILED DESCRIPTION
[0010] Examples are described with reference to the accompanying drawings. The drawings are provided for the purpose of illustrating the examples and may not be drawn to scale. Several aspects are described with reference to the examples for the purpose of illustration, wherein like features correspond to like reference numerals. Many specific details, relationships, and methods are set forth to provide understanding, but the scope is not necessarily limited by the illustrated ordering of actions or events, as some actions may occur in a different order and / or simultaneously with other actions or events. In addition, not all of the illustrated actions or events may be required to implement the methods in one or more examples.
[0011] Figures 1 to 10 are cross-sectional views showing successive stages of fabrication of semiconductor structure 100 and the resulting structure, and Fig.11 1 is a method 1100 in flowchart form outlining the steps of those manufacturing stages. Figure 1 (and method step 1102), a semiconductor structure 100 is provided at an early manufacturing stage. The semiconductor structure 100 includes a semiconductor substrate 102, for example, as part of a silicon wafer. The wafer includes a plurality of locations, each location corresponding to the same or different IC on the wafer, so Figure 1 The illustration of (and later figures) may be repeated in each wafer IC location. The wafer provides either p-type or n-type semiconductors, and semiconductor substrate 102 may represent a portion of the bulk wafer or a region (e.g., a well or buried layer) formed in conjunction with the wafer. As described in detail in the remaining figures, resistors 104 and transistors 106 are ultimately formed in conjunction with semiconductor substrate 102, and those devices are formed only by Figure 1 . Ultimately, these figures and corresponding descriptions provide for efficient, cost-sensitive formation of each of resistor 104 and transistor 106, including, for example, advantageously low resistance in resistor 104, the absence of a separate ZTCR mask and implant, the availability of ZTCR performance in resistor 104 (along with options for different sizes and dopant types), and implementation of transistor 106 without attenuating (or through reactivation) its dopant activation or performance.
[0012] exist Figure 2 (and Fig.11In method step 1104), a surface isolation structure 108, such as a shallow trench isolation (STI), is formed in a portion of the upper surface 102US of the semiconductor substrate 102 corresponding to the region of the resistor 104. The surface isolation structure 108 is, for example, shown as a shallow trench isolation (STI) structure having a thickness in the range of 150nm to 600nm, and it can later conductively isolate the resistor 104 from the substrate 102. Alternative isolation methods may also be used, such as different insulators, local oxidation of silicon (LOCOS) structures, or doped well regions. Subsequently, a threshold voltage (Vt) implant is applied to the semiconductor substrate 102, wherein the dopant type and energy are selected to ultimately adjust the Vt of the transistor 106, for example, to provide a voltage from 1e16 / cm 3 to 1e18 / cm 3 At the same time, in the region of the resistor 104 , the surface isolation structure 108 substantially prevents the implanted dopant from having an effect in the substrate 102 .
[0013] exist Figure 3 (and Fig.11 In method step 1106), a gate oxide layer 110 is formed across a portion of the upper surface 102US, for example, where the surface isolation structure 108 is not located and by oxidizing the remaining exposed portion of the upper surface 102US. The gate oxide layer 110 can have a thickness from 1nm to 5nm. Subsequently, a polysilicon layer 112 is deposited on the entire structure shown, thereby conforming to the gate oxide layer 110 and the upper surface 108US of the surface isolation structure 108. The polysilicon layer 112 is undoped when deposited, but can be in-situ doped in some examples.
[0014] exist Figure 4 (and Fig.11 In method step 1108), Figure 3 A mask (not shown) is formed and patterned over the polysilicon layer 112, and the polysilicon layer 112 is etched accordingly so that only two portions of the polysilicon layer 112 remain, namely, the polysilicon resistor body portion 112R and the polysilicon gate portion 112G. In addition, the polysilicon etching continues to the upper surfaces 102US and 108US, thereby removing Figure 3 The exposed portion of the gate oxide layer 110 is exposed while leaving an unexposed portion of the oxide layer 110 below the polysilicon gate portion 112G, which is referred to as the gate oxide portion 110GOP hereinafter. Subsequently, a relatively light dopant implant, commonly referred to as a lightly doped drain (LDD) implant, is performed to form a corresponding LDD region 114 below the upper surface 102US and self-aligned to the gate oxide portion 110GOP (and also self-aligned to the lateral edge of the surface isolation structure 108 at one end of the transistor 106). The LDD implant provides, for example, 1e18 / cm 3To 5e20 / cm 3 The LDD implant has an average dopant concentration of 112R, and it is selected to be a dopant type that corresponds to the desired conductivity type of transistor 106. For example, for an n-type metal oxide semiconductor (NMOS) transistor, the LDD implant has an n-type dopant (and alternatively, a complementary p-type for a PMOS transistor). During the LDD implant, the polysilicon resistor body portion 112R may or may not be masked, depending on the desired result for resistor 104. If the resistor body portion 112R is not masked, then the final resistor 104 may have the same dopant type as the LDD implant, for example, if the LDD implant is n-type (sometimes referred to as NLDD), then the resistor 104 may also be n-type, or in a complementary manner, if the LDD implant is p-type (sometimes referred to as PLDD), then the resistor 104 may also be p-type. Alternatively, if the LDD implant is -n-type, a later p-type implant may also be applied to the resistor body portion 112R, for example, during the formation of p-type source / drain regions (sometimes referred to as PSD), so that the later PSD implant counter-dopes with the earlier NLDD implant, in which case the resulting resistor 104 has a relatively high resistance, sometimes referred to as a high sheet resistivity resistor (HSR). The alternative HSR example may also be implemented with the opposite doping type, i.e., first a PLDD implant followed by an n-type (sometimes referred to as NSD) counter-doping.
[0015] exist Figure 5 (and Fig.11 In method step 1110), a plurality of separate layers are formed on Figure 4 10. The structure is formed (e.g., deposited) above the alignment spacers in preparation for forming alignment spacers in a later manufacturing stage. In the example shown, there are three such layers. First, a first spacer oxide layer 116 is formed (e.g., deposited), for example, having a thickness of from 1 nm to 10 nm. Second, a spacer nitride layer 118 is formed (e.g., deposited as (bis-(tert-butylamino)-silane) (BTBAS)), for example, having a thickness of from 10 nm to 50 nm. Third, a second spacer oxide layer 120 is formed (e.g., deposited), for example, having a thickness of from 10 nm to 60 nm. In an alternative example, Figure 6 The plurality of layers may include a different number of layers, such as having only two layers by forming an oxide layer first and then forming a nitride layer.
[0016] exist Figure 6 (and Fig.11 In method step 1112), the first spacer oxide layer 116, the spacer nitride layer 118 and the second spacer oxide layer 120 are provided. Figure 5The three-layer combination (or two layers in an alternative example) is patterned (mask not shown) and etched down to the upper surfaces 102US and 108US, thereby forming corresponding spacers 122R for the resistor 104 and spacers 122T for the transistor 106. Each of the spacers 122R and 122T includes a portion of the first spacer oxide layer 116 and having a first lateral extension 116LE, a portion of the spacer nitride layer 118 and having a second lateral extension 118LE, and a portion of the second spacer oxide layer 120 providing the spacer sidewall 120SW. Also, in an alternative example, the transistor sidewall (adjacent to the gate sidewall) may include one or more additional layers (e.g., silicon oxide, offset nitride, capping oxide). In the example shown in FIG. Figure 5 In another alternative example mentioned, in which only two layers (oxide and then nitride) are formed to provide sidewall spacing, the two layers are etched to form D-shaped sidewall spacers on each of the polysilicon resistor body portion 112R and the polysilicon gate portion 112G. In the example shown, after forming the spacer sidewall 120SW, a concentration ratio is performed. Figure 4 The LDD implantation is a higher source / drain dopant implantation to form corresponding transistor source / drain regions 124 below the upper surface 102US, partially intermixed with the corresponding LDD regions 114 and self-aligned to the spacers 122T (and at one end of the transistor 106, also self-aligned to the surface isolation structure 108). The source / drain implantation provides, for example, 1e19 / cm 3 to 6e21 / cm 3 The average dopant concentration of Figure 4 The LDD implant is selected to be a dopant type corresponding to the desired conductivity type of transistor 106, but the source / drain implant is at a higher energy and dose and forms a dopant concentration deeper below upper surface 102US than the LDD implant. Also, the implant also implants dopants, whether p-type or n-type, into polysilicon resistor body portion 112R to affect its conductivity, such as increasing conductivity in the case of a first dopant implant relative to undoped polysilicon or the same type as an earlier LDD implant, or providing HSR in the case of counter-doping with a previous LDD implant into the same polysilicon resistor body portion 112R.
[0017] exist Figure 7 (and Fig.11 In method step 1114), first Figure 6 A conformal capping layer 126 is formed over the structure. In a first example, the capping layer 126 may be a highly tensile silicon oxide or silicon nitride or silicon carbide or a combination thereof having a thickness from 10 nm to 100 nm. In a second example, and as Figure 7As shown by dashed line 126D along the capping layer 126, the capping layer 126 may be a dual layer, first comprising a thin oxide and then comprising a stress memory nitride (e.g., silicon-rich nitride). Next, a relatively long stabilization ("stab") anneal is performed on the semiconductor structure 100, followed by a spike anneal. For example, the stabilization anneal may be at a stabilization temperature in a range from 500° C. to 600° C. for a period in a range from 20 seconds to 240 seconds. The stabilization anneal may improve cross-wafer (e.g., resistance) uniformity, for example to achieve a more uniform temperature distribution across the wafer. The spike anneal is followed by a stabilization anneal, the spike anneal ramping up to a spike peak temperature of, for example, 1,000°C to 1,050°C, with a spike anneal ramp time of approximately three seconds at a ramp rate of approximately 170°C per second, sometimes referred to as a refinement spike anneal where the ramp rate exceeds 100°C per second, and the spike peak temperature is followed by a ramp down of approximately 65°C to 70°C per second, for example, to return to the stabilization temperature or lower. The refinement spike anneal implements a stress memory technology (SMT) for the semiconductor structure 100, i.e., stress from the capping layer 126 is transferred to and retained (memorized) in the polysilicon components beneath the conformal capping layer 126, such as the polysilicon resistor body portion 112R and the polysilicon gate portion 112G. Additionally, the refinement spike anneal may also activate implanted dopants, such as from Figure 4 and 6 , and in fact the spike anneal may have a higher degree of activation due to the higher peak temperature, thereby further reducing the resistance of resistor 104 and partially assisting the resistor in achieving ZTCR performance, as further enhanced by the additional millisecond anneal described later, even if a separate ZTCR mask and implant step is not previously provided. If multiple resistors are formed as resistor 104 or between different resistors in different corresponding areas on a wafer providing substrate 102, the stabilization anneal and the spike anneal may also improve resistance uniformity. The stabilization anneal immediately following the refinement spike anneal may be referred to as a "stabilization spike anneal."
[0018] exist Figure 8 (and Fig.11 In method step 1116), if it is a single material layer, the SMT is completely removed. Figure 7The capping layer 126, or if the capping layer 126 is a bilayer as mentioned above as an alternative, the nitride portion can be removed, for example, using hot phosphoric acid. Subsequently, a multilayer silicide barrier (SiBLK) stack 128 is formed, which in one example includes a SiBLK thin oxide layer 130 (which can remain as part of the previously formed bilayer for the capping layer 126, thereby avoiding additional formation / etching steps) and a SiBLK thin nitride / carbide / SiCN layer 132. The SiBLK thin oxide layer 130 can be grown or deposited, and it has a thickness from 1nm to 100nm. The SiBLK thin nitride / carbide / SiCN layer 132 can be deposited, for example, by BTBAS at 550°C, or by plasma enhanced chemical vapor deposition (PECVD) at 350°C to 400°C, and has a thickness from 5nm to 40nm.
[0019] exist Fig. 9 (and Fig.11 In method step 1118), mask 134 is formed in the region of resistor 104. Figure 7 The SiBLK stack 128 is formed above the transistor 106, while no such mask is formed in the region of the transistor 106. Subsequently, the SiBLK etch is performed in the exposed regions outside the region covered by the mask 134, and the etching is performed in the region of the transistor 106. Figure 8 The etching stops at the SiBLK thin oxide layer 130 of the SiBLK stack 128, so that the etching removes the exposed portion of the SiBLK thin nitride / carbide / SiCN layer 132. Thus, the polysilicon resistor body portion 112R remains covered by the layer from the SiBLK stack 128, while the polysilicon gate portion 112G remains covered only by the oxide layer 130 of the SiBLK stack 128. Subsequently, the mask 134 (e.g., Fig.10 ), and as Fig. 9 As shown in the legend at the top of , the millisecond anneal is performed, for example, at 1,200° C. to 1,350° C. and for a duration of less than one second, for example, 1 millisecond to 100 milliseconds. The millisecond anneal can be performed by various equipment alternatives, such as using a laser or a flash lamp.
[0020] exist Fig.10 (and Fig.11 In method step 1120), the remaining exposed portions of SiBLK layer 128 are removed, thereby removing the exposed SiBLK thin oxide layer 130. The oxide removal also removes the exposed spacer sidewalls 120SW for transistor 106, but does not remove the exposed spacer sidewalls for resistor 104 because the spacer sidewalls 120SW of resistor 104 remain covered by the remaining portions of SiBLK thin nitride / carbide / SiCN layer 132. It should be noted that Fig.10A millisecond anneal legend is also included at the top thereof as an alternative example indicating that the millisecond anneal described above may occur after the SiBLK layer 128 is completely removed, rather than as shown in FIG. Fig. 9 The millisecond annealing occurs once the SiBLK layer 128 has been deposited but not yet removed as indicated in FIG. Fig.10 Continuing in the process, a silicidation step is performed to form silicide on the exposed semiconductor structure. Specifically, gate silicide 136 is formed along the upper surface of polysilicon gate portion 112G, and source / drain silicide 138 is formed along the upper surface of transistor source / drain region 124. However, at the same time, the remaining portion of SiBLK structure 128 in the area of resistor 104 prevents silicide of polysilicon resistor body portion 112R. Note also that Fig.10 and the previous figures show a cross section including only a portion of the polysilicon resistor body portion 112R; with respect to other resistor portions, some may receive silicide as Fig.10 Silicidated portions, such as at the resistor head, or in the case of a serpentine resistor, at the portion where the resistor turns, where any of those locations remain unsilicided. Fig.10 1. The layer coverage of silicide masking the polysilicon resistor body portion 112R is shown in FIG.
[0021] Finish Fig.11 However, in the absence of corresponding cross-sectional views, additional steps of fabricating the semiconductor structure 100 are contemplated. For example, in step 1122, portions of which may have been performed earlier in the method 1100, one or more additional semiconductor features are formed on or in a layer of the semiconductor substrate 102, with similar copies of each feature being formed into each corresponding IC on a semiconductor wafer that includes the semiconductor substrate 102. The step 1122 of forming the one or more additional semiconductor features may include nearly any process for forming any feature. For example, step 1122 may include patterning one or more photoresist features on or in conjunction with the semiconductor substrate 102, including in conjunction with various layers and levels. Also, step 1122 may include forming one or more interconnect features. Step 1122 may also include other process steps, or a series of different process steps, such that all features for the functional operation of the semiconductor structure 100 are ultimately completed.
[0022] Next, in step 1124, the semiconductor wafer including the semiconductor substrate 102 may be coupled to a test device and tested, after which each IC is cut (singulated) from the semiconductor wafer. Subsequently, some or all of the ICs (e.g., those that passed the test) are packaged. The package provides a housing that surrounds (or encapsulates) the IC, and further provides an external interface, such as a number of conductive pins fixed relative to pads on the die, and conductors such as bonding wires, lands, or balls are formed between the IC pads and the package pins. Subsequently, any packaged IC with acceptable test results is ready for sale and shipment to customers.
[0023] Fig.12 is a resistance graph 1200 of three resistor types including Fig.11 The graph 1200 includes normalized resistor size (e.g., resistor line width, e.g., in nanometers up to micrometers) on the horizontal axis and a logarithmic scale, and it includes normalized temperature coefficient, i.e., resistor temperature variable resistance (e.g., parts per million per ° C.) on the vertical axis. The graph 1200 includes plots of three resistor types, the three resistor types including Fig.11 The example method 1100 produces two of the resistors 104, namely, a PSD resistor resistance plot 1202 and a NSD resistor resistance plot 1204. The graph 1200 also includes a ZTCR resistance plot 1206, which represents a temperature variable resistance of a ZTCR that can be constructed using prior art techniques.
[0024] For each of the three plots 1202, 1204, and 1206, the temperature-based performance of the resistor can be evaluated when each plot is close to zero or within a certain range of zero, where the closer the resistance is to zero or within a relatively small range of zero, the better the resistor qualifies as a zero temperature coefficient resistor. In addition, the resistor can still be used for zero temperature coefficient (or near zero temperature coefficient) performance if it falls within a temperature coefficient range suitable for the application. For example, consider a range of normalized temperature coefficients of ±0.2, which can correspond to a practical range of ±100ppm / °C, for example. In this range, a ZTCR resistor with a normalized width of at least approximately 8 has a -0.2 normalized temperature coefficient, and the temperature coefficient approaches zero for larger widths (reaching zero at an approximate normalized width of 36). In contrast, for the PSD resistor 104 constructed by method 1100, it achieves the same -0.2 normalized temperature coefficient at a significantly smaller width than the ZTCR, and therefore, the PSD resistor achieves this temperature coefficient at a normalized width of approximately 1.0, and the other PSD resistors remain within the range of ±0.2 normalized temperature coefficients up to a normalized width of at least 100. Similarly, for the NSD resistor 104 constructed by method 1100, it achieves the same normalized temperature coefficient of -0.2 at a normalized width of approximately 2.0, and the other NSD resistors also remain within the range of ±0.2 normalized temperature coefficients up to a normalized width of at least 100. Therefore, an IC can be constructed using method 1100 to implement one or both of the PSD and NSD resistors having these properties. Some of the previous observations also occur for narrower temperature coefficient ranges. For example, consider a ±0.1 normalized temperature coefficient range, which may, for example, correspond to a practical range of ±50ppm / °C. In this range, the PSD resistor resistance plot 1202 shows that the range is achieved at normalized widths of approximately 1.3 up to approximately 6.0, while the NSD resistor resistance plot 1202 shows that the range is achieved at normalized widths of approximately 6.0 or greater.
[0025] Thus, while the above example provides a method 1100 for constructing resistors and / or transistors with advantageous efficiency (e.g., number and order of steps plus reduced cost), an additional and unintended consequence is that the method 1100 provides a selection of one or both types of resistors, each having advantageous temperature coefficient (or near temperature coefficient) performance, where both PSD and NSD resistors approach zero temperature coefficient at a width that is less than the width of a conventional ZTCR resistor. Thus, a designer may achieve ZTCR performance or better using a smaller width NSD or PSD resistor. Furthermore, a designer may choose to implement both PSD and NSD resistors in a single IC, e.g., using PSD resistors where a relatively smaller width is desired or required and using NSD resistors where a relatively larger width is desired or required.
[0026] As can be seen from the above, those skilled in the art will understand examples of semiconductor IC manufacturing provided, for example, with respect to ICs that include both polysilicon resistors and transistors. Such examples provide various benefits, some of which are described above and still include other benefits. The examples are formed using a resistor SiBLK structure formation that is relatively late in the manufacturing steps, preferably after the transistor source / drain implantation, whereby the transistor source / drain implantation can simultaneously implant dopants into the resistor body. Therefore, the source / drain implantation of the resistor body, in particular by subsequent annealing, can improve performance relative to other ZTCR methods while reducing or eliminating the need for separate and earlier ZTCR masking and implantation steps in the process. In addition, the examples include millisecond anneals after SiBLK deposition and before or after its removal, and in either case the millisecond annealing will remove potential damage from SiBLK formation and reactivate dopants that are potentially deactivated by SiBLK formation, which in turn can reduce resistor conductivity and make the temperature coefficient negative. Another example is expected to achieve a ZTCR (or better) metric with a p-type or n-type dopant, and in fact, one or other dopant type may correspond to the zero temperature coefficient performance of resistors of different width sizes, so that a p-type doped resistor may have a zero temperature coefficient for a first size range, and an n-type doped resistor may have a zero temperature coefficient for a second size range different from the first size range. Therefore, the IC can be implemented by the selectivity of the appropriate dopant type for the ZTCR zero temperature coefficient polysilicon resistor according to the size considerations of the IC. Another example implemented as an n-type polysilicon resistor is expected to provide an extremely low drift comparable to the baseline ZTCR. Another example implemented as a p-type polysilicon resistor is expected to provide a match comparable to or exceeding the baseline ZTCR. These benefits can be achieved for more complex structures of multiple devices on the same substrate (and IC), thereby achieving improvements in scaling across devices. Additional modifications to the described examples are possible within the scope of the appended claims, and other examples are possible.
Claims
1. A method of forming an integrated circuit, wherein include: First, forming the resistor body and transistor gate from a semiconductor layer; second, forming sidewall spacers adjacent to the resistor body and the transistor gate; third, forming a silicide blocking structure over at least a portion of the resistor body; as well as Fourth, the resistor body and the transistor gate are millisecond annealed simultaneously.
2. The method according to claim 1: wherein the step of forming a silicide blocking structure comprises depositing a silicide blocking material; and The step of simultaneously performing the millisecond annealing occurs while at least a portion of the silicide blocking material covers the transistor gate.
3. The method according to claim 1: wherein the step of forming a silicide blocking structure comprises depositing a silicide blocking material; and The step of simultaneously performing a millisecond anneal occurs after all of the silicide blocking material is removed from the transistor gate. 4 . The method according to claim 1 , further comprising a stable spike annealing after forming the sidewall spacer and before forming a silicide blocking pattern. The method of claim 1 , wherein the millisecond annealing step comprises laser annealing. The method of claim 1 , wherein the millisecond annealing step comprises a flash lamp anneal.
7. The method of claim 1, wherein the millisecond annealing step comprises annealing at a temperature of at least 1,000°C and for a duration of less than one second.
8. The method of claim 1, further comprising simultaneously implanting dopants into the resistor body and into source / drain regions adjacent to the transistor gate.
9. The method of claim 8, further comprising, after the simultaneous implantation step and before the third step, annealing the source / drain regions.
10. The method of claim 9, wherein the step of annealing the source / drain regions comprises a steady anneal at a first temperature and for a first duration followed by a spike anneal at a second temperature greater than the first temperature and for a second duration less than the first duration.
11. The method of claim 9, further comprising, before annealing the source / drain regions, forming a stress-memory capping layer in a fixed position relative to the transistor gate. 12 . The method according to claim 11 , further comprising removing the stress memory capping layer after forming the stress memory layer and before the third step.
13. A method of forming an integrated circuit, wherein include: forming a resistor body relative to a semiconductor substrate; forming a transistor gate relative to the semiconductor substrate; forming a first source / drain region and a second source / drain region in a fixed position relative to the transistor gate, comprising a first implant having a first dopant dose and a second implant having a larger second dopant dose; forming a silicide blocking structure over at least a portion of the resistor body after forming the first source / drain region and the second source / drain region; as well as After forming the silicide blocking structure, millisecond annealing is performed on the first source / drain region and the second source / drain region.
14. The method of claim 13, further comprising removing the silicide blocking structure prior to the millisecond anneal.
15. The method of claim 13, further comprising performing a refinement spike anneal prior to the millisecond anneal, the refinement spike anneal comprising ramping a substrate temperature from a steady temperature to a spike peak temperature at a ramp rate exceeding 100°C per second.
16. The method of claim 13, further comprising forming sidewall spacers on sidewalls of the resistor body, wherein the silicide blocking structure contacts silicon oxide spacer sidewalls and silicon oxide lateral extensions of the sidewall spacers.
17. An integrated circuit, wherein include: Semiconductor substrate; a first polysilicon resistor positioned relative to the semiconductor substrate, the first polysilicon resistor comprising a majority dopant concentration of an n-type dopant and having a temperature coefficient of resistance (TC) within a range of ±100 ppm / °C; as well as A second polysilicon resistor is positioned relative to the semiconductor substrate, the second polysilicon resistor including a majority dopant concentration of a p-type dopant and having a temperature coefficient of resistance within a range of ±100 ppm / °C.
18. The integrated circuit of claim 17, wherein each of the first polysilicon resistor and the second polysilicon resistor each has a temperature coefficient within a range of ±50 ppm / °C.
19. The integrated circuit of claim 17, wherein the first polysilicon resistor has a first width and the second polysilicon resistor has a second, different width.
20. The integrated circuit of claim 17, wherein the first polysilicon resistor has a first width that is greater than a second width of the second polysilicon resistor.