Polymer nanogel sustained-release agent and production process thereof

By adding diethyl ether to the sustained-release agent to delay evaporation of ethanol, the problem of evaporation of ethanol is solved, which leads to excessive release of drug power, extends the time of the sustained-release agent and improves the disinfection effect. At the same time, safety and cleaning are enhanced through other additives Effect.

CN118873484APending Publication Date: 2024-11-01JIANGSU YINGHUA BIOPHARMACEUTICAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410892672.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-04
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The commonly used ethanol disinfectants in existing sustained-release agents are easy to evaporate and difficult to sustain the effect, resulting in the release of the medicinal power too quickly, which may cause side effects to the human body.

Method used

The additional ether is added to the polymer nanogel sustained release agent, which takes advantage of the easier volatility of ether, and delays the volatility of ethanol through the endothermic heat during volatility, thereby increasing the retention time of ethanol and thus prolongs the effect of the sustained release agent. .

Benefits of technology

The volatile endothermic ether inhibits ethanol volatility, prolongs the action time of the sustained release agent, improves the durability and effect of the disinfectant, and enhances the safety and cleaning effect through other additives such as zinc sulfate and lauric acid.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a high-molecular nanogel sustained-release agent and a production process thereof, and relates to the field of nanogel sustained-release agents, used raw materials comprise a main material and an auxiliary material, the main material comprises the following raw materials in parts by weight: 90-140 parts of water-absorbent resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban; the auxiliary materials comprise the following raw materials in parts by weight: 2-7 parts of diethyl ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid and 5-15 parts of lauric acid. According to the invention, polyethylene glycol and water-absorbent resin are mixed, ethanol and triclocarban are added into the mixture, so that the sterilization and disinfection effects are achieved, ethanol volatilization is delayed by additionally adding diethyl ether, utilizing the characteristic that diethyl ether is more volatile and utilizing heat absorption when diethyl ether volatilizes, so that the retention time of ethanol in the sustained-release agent is prolonged, and the sustained-release effect is improved. Further, the acting time of the slow-release agent is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of nano gel sustained-release agents, in particular to a polymer nano gel sustained-release agent and a production process thereof. Background Art

[0002] Sustained-release agents are a special type of medicine. The so-called sustained-release means that the drug power is released slowly, so it can produce the drug effect for a longer time and continuously. At the same time, the slow release of the drug power can also reduce the impact of the drug power on the human body and avoid side effects that damage the body due to too rapid release of the drug power.

[0003] Sustained-release agents are often used as agents for anti-inflammatory, analgesic, bactericidal and disinfectant purposes that require sustained release of drug power, such as the nano-sustained-release gel bactericide with publication number CN112120017B in the prior art and its preparation method.

[0004] Iodine tincture, ethanol, and hydrogen peroxide are the most commonly used disinfectants and sterilizers in reality. Among them, ethanol has the widest range of applications and is low in cost, but it is extremely volatile during use and is difficult to maintain its effect. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention provides a polymer nanogel sustained-release agent and a production process thereof, which uses the characteristic of ether being more volatile by adding additional ether and utilizing the heat absorption during ether volatilization to delay the volatilization of ethanol, thereby increasing the retention time of ethanol in the sustained-release agent, thereby increasing the duration of action of the sustained-release agent, and can effectively solve the problems in the background technology.

[0006] To achieve the above object, the technical solution adopted by the present invention is: a polymer nanogel sustained-release agent, the raw materials used include a main material and auxiliary materials, the raw materials of the main material include 90-140 parts of water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in terms of weight parts;

[0007] Polyethylene glycol itself is a viscous gel with good water solubility and good compatibility with many organic components. After mixing with absorbent resin, it can be used as a carrier for ethanol and triclocarban. Ethanol and triclocarban are commonly used disinfectants that can play a role in disinfection and sterilization. Applying them to the wound can effectively prevent wound infection.

[0008] The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight, and lauric acid is used as a surfactant.

[0009] Ether has a certain disinfecting effect and is more volatile than ethanol. Menthol can make the sustained-release agent have a cool feeling and a refreshing mint aroma after application, covering up the smell of other substances, and once it accidentally touches the eyes, it can also stimulate the lacrimal glands to secrete tears to clean the eyes. The bitter essence tastes extremely bitter and can effectively prevent children from accidentally ingesting the sustained-release agent. Once accidentally ingested, zinc sulfate can stimulate the digestive tract and act as a vomiting agent, so that the accidentally ingested sustained-release agent will be vomited out in time to avoid further danger. Aloe vera gel, vitamin E, and hyaluronic acid can all protect the skin and moisturize and supplement skin nutrients. Among them, vitamin E can also protect the skin mucosa, promote wound healing, and reduce the irritation of disinfectants to the skin. Lauric acid can produce foam by contacting with water when the sustained-release agent is used and cleaned, so that the residual components in the sustained-release agent can be cleaned more thoroughly.

[0010] Furthermore, the raw materials used include a main material and auxiliary materials, wherein the main material includes 90 parts of a water-absorbing resin, 100 parts of polyethylene glycol, 20 parts of ethanol, and 40 parts of triclocarban in terms of weight;

[0011] The raw materials of the auxiliary material include 2 parts of ether, 20 parts of water, 1 part of menthol, 1 part of bitter essence, 3 parts of zinc sulfate, 40 parts of aloe vera gel, 1 part of vitamin E, 2 parts of hyaluronic acid, and 5 parts of lauric acid in parts by weight.

[0012] Furthermore, the raw materials used include a main material and auxiliary materials, wherein the main material includes 105 parts of a water-absorbing resin, 115 parts of polyethylene glycol, 25 parts of ethanol, and 48 parts of triclocarban in terms of weight;

[0013] The raw materials of the auxiliary material include 4 parts of ether, 23 parts of water, 3 parts of menthol, 2 parts of bitter essence, 5 parts of zinc sulfate, 50 parts of aloe vera gel, 3 parts of vitamin E, 4 parts of hyaluronic acid, and 8 parts of lauric acid in parts by weight.

[0014] Furthermore, the raw materials used include a main material and auxiliary materials, wherein the main material includes 120 parts of a water-absorbing resin, 130 parts of polyethylene glycol, 30 parts of ethanol, and 55 parts of triclocarban in terms of weight;

[0015] The raw materials of the auxiliary material include 6 parts of ether, 27 parts of water, 5 parts of menthol, 4 parts of bitter essence, 8 parts of zinc sulfate, 60 parts of aloe vera gel, 5 parts of vitamin E, 6 parts of hyaluronic acid, and 12 parts of lauric acid in parts by weight.

[0016] Furthermore, the raw materials used include a main material and auxiliary materials, wherein the main material includes 140 parts of a water-absorbing resin, 150 parts of polyethylene glycol, 35 parts of ethanol, and 65 parts of triclocarban in terms of weight;

[0017] The raw materials of the auxiliary material include 7 parts of ether, 30 parts of water, 7 parts of menthol, 5 parts of bitter essence, 10 parts of zinc sulfate, 70 parts of aloe vera gel, 6 parts of vitamin E, 8 parts of hyaluronic acid, and 15 parts of lauric acid in parts by weight.

[0018] The present invention also includes a production process of the polymer nanogel sustained-release agent, and the specific steps are as follows:

[0019] Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing;

[0020] Step 2: adding ethanol and triclocarban to the mixture of water-absorbing resin and polyethylene glycol according to the weight proportions and stirring evenly for standby use; the main material formed after mixing needs to be refrigerated for standby use to prevent ethanol from volatilizing;

[0021] Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir and mix, and refrigerate for use to prevent the ether from volatilizing;

[0022] Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly. After mixing, it will also present a viscous gel state. Slow stirring is to prevent lauric acid from foaming after contacting water and air;

[0023] Step 5: First slowly stir and mix the stirred and mixed aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored in an environment of 2-5°C. The low temperature environment can effectively inhibit the volatilization of ethanol and ether.

[0024] Compared with the prior art, the present invention provides a polymer nanogel sustained-release agent and a production process thereof, which has the following beneficial effects:

[0025] 1. Polymer nanogel is prepared by mixing polyethylene glycol and water-absorbing resin, and ethanol and triclocarban are added thereto to achieve the effect of sterilization and disinfection. By adding additional ether, the ether is more volatile and the heat absorbed during ether volatilization is used to delay the volatilization of ethanol, thereby increasing the retention time of ethanol in the sustained-release agent and thus increasing the duration of action of the sustained-release agent.

[0026] 2. By adding zinc sulfate, if accidentally ingested, zinc sulfate can stimulate the digestive tract and induce vomiting, causing the accidentally ingested sustained-release agent to be vomited out in time to avoid further danger.

[0027] 3. By adding lauric acid, when the sustained-release agent is cleaned after use, it can generate foam by contacting with water, so that the residual components in the sustained-release agent can be cleaned more thoroughly. DETAILED DESCRIPTION

[0028] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the present invention will be further described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] Example 1

[0030] The invention provides a polymer nano gel sustained-release agent, the raw materials used include a main material and auxiliary materials, the main material includes 90-140 parts of a water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in parts by weight;

[0031] The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight.

[0032] Specifically in this embodiment, the raw materials used include a main material and an auxiliary material, and the raw materials of the main material include 90 parts of a water-absorbing resin, 100 parts of polyethylene glycol, 20 parts of ethanol, and 40 parts of triclocarban in terms of weight parts;

[0033] The raw materials of the auxiliary material include 2 parts of ether, 20 parts of water, 1 part of menthol, 1 part of bitter essence, 3 parts of zinc sulfate, 40 parts of aloe vera gel, 1 part of vitamin E, 2 parts of hyaluronic acid, and 5 parts of lauric acid in parts by weight.

[0034] The present invention also includes a production process of the polymer nanogel sustained-release agent, and the specific steps are as follows:

[0035] Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing;

[0036] Step 2: adding ethanol and triclocarban to the mixture of water-absorbing resin and polyethylene glycol according to the weight proportions and stirring evenly for standby use; the main material formed after mixing needs to be refrigerated for standby use to prevent ethanol from volatilizing;

[0037] Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir and mix, and refrigerate for use to prevent the ether from volatilizing;

[0038] Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly. After mixing, it will also present a viscous gel state. Slow stirring is to prevent lauric acid from foaming after contacting water and air;

[0039] Step 5: First slowly stir and mix the stirred and mixed aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored at 2°C. The low temperature environment can effectively inhibit the volatilization of ethanol and ether.

[0040] Example 2

[0041] The invention provides a polymer nano gel sustained-release agent, the raw materials used include a main material and auxiliary materials, the main material includes 90-140 parts of a water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in parts by weight;

[0042] The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight.

[0043] Specifically in this embodiment, the raw materials used include a main material and an auxiliary material, and the raw materials of the main material include 105 parts of a water-absorbing resin, 115 parts of polyethylene glycol, 25 parts of ethanol, and 48 parts of triclocarban in terms of weight parts;

[0044] The raw materials of the auxiliary material include 4 parts of ether, 23 parts of water, 3 parts of menthol, 2 parts of bitter essence, 5 parts of zinc sulfate, 50 parts of aloe vera gel, 3 parts of vitamin E, 4 parts of hyaluronic acid, and 8 parts of lauric acid in parts by weight.

[0045] The present invention also includes a production process of the polymer nanogel sustained-release agent, and the specific steps are as follows:

[0046] Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing;

[0047] Step 2: adding ethanol and triclocarban to the mixture of water-absorbing resin and polyethylene glycol according to the weight proportions and stirring evenly for standby use; the main material formed after mixing needs to be refrigerated for standby use to prevent ethanol from volatilizing;

[0048] Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir and mix, and refrigerate for use to prevent the ether from volatilizing;

[0049] Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly. After mixing, it will also present a viscous gel state. Slow stirring is to prevent lauric acid from foaming after contacting water and air;

[0050] Step 5: First slowly stir and mix the stirred aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored at 3°C. The low temperature environment can effectively inhibit the volatilization of ethanol and ether.

[0051] Example 3

[0052] The invention provides a polymer nano gel sustained-release agent, the raw materials used include a main material and auxiliary materials, the main material includes 90-140 parts of a water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in parts by weight;

[0053] The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight.

[0054] Specifically in this embodiment, the raw materials used include a main material and an auxiliary material, and the raw materials of the main material include 120 parts of a water-absorbing resin, 130 parts of polyethylene glycol, 30 parts of ethanol, and 55 parts of triclocarban in terms of weight parts;

[0055] The raw materials of the auxiliary material include 6 parts of ether, 27 parts of water, 5 parts of menthol, 4 parts of bitter essence, 8 parts of zinc sulfate, 60 parts of aloe vera gel, 5 parts of vitamin E, 6 parts of hyaluronic acid, and 12 parts of lauric acid in parts by weight.

[0056] The present invention also includes a production process of the polymer nanogel sustained-release agent, and the specific steps are as follows:

[0057] Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing;

[0058] Step 2: adding ethanol and triclocarban to the mixture of water-absorbing resin and polyethylene glycol according to the weight proportions and stirring evenly for standby use; the main material formed after mixing needs to be refrigerated for standby use to prevent ethanol from volatilizing;

[0059] Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir and mix, and refrigerate for use to prevent the ether from volatilizing;

[0060] Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly. After mixing, it will also present a viscous gel state. Slow stirring is to prevent lauric acid from foaming after contacting water and air;

[0061] Step 5: First slowly stir and mix the stirred and mixed aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored in an environment of 4°C. The low temperature environment can effectively inhibit the volatilization of ethanol and ether.

[0062] Example 4

[0063] The invention provides a polymer nano gel sustained-release agent, the raw materials used include a main material and auxiliary materials, the main material includes 90-140 parts of a water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in parts by weight;

[0064] The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight.

[0065] Specifically in this embodiment, the raw materials used include a main material and an auxiliary material, and the raw materials of the main material include 140 parts of a water-absorbing resin, 150 parts of polyethylene glycol, 35 parts of ethanol, and 65 parts of triclocarban in terms of weight parts;

[0066] The raw materials of the auxiliary material include 7 parts of ether, 30 parts of water, 7 parts of menthol, 5 parts of bitter essence, 10 parts of zinc sulfate, 70 parts of aloe vera gel, 6 parts of vitamin E, 8 parts of hyaluronic acid, and 15 parts of lauric acid in parts by weight.

[0067] The present invention also includes a production process of the polymer nanogel sustained-release agent, and the specific steps are as follows:

[0068] Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing;

[0069] Step 2: adding ethanol and triclocarban to the mixture of water-absorbing resin and polyethylene glycol according to the weight proportions and stirring evenly for standby use; the main material formed after mixing needs to be refrigerated for standby use to prevent ethanol from volatilizing;

[0070] Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir and mix, and refrigerate for use to prevent the ether from volatilizing;

[0071] Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly. After mixing, it will also present a viscous gel state. Slow stirring is to prevent lauric acid from foaming after contacting water and air;

[0072] Step 5: First slowly stir and mix the stirred aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored at 5°C. The low temperature environment can effectively inhibit the volatilization of ethanol and ether.

[0073] The sustained-release agents prepared according to the formula and method of Examples 1-4 were applied to the skin surfaces of different experimenters respectively. Meanwhile, the sustained-release agent without adding ether was prepared according to the formula and method of Example 4, and the same amount was also applied as a control group. The amount of sustained-release agent of each formula applied was equal, and the ambient temperature of the experimenters during the experiment was maintained at 25° C. The ethanol concentration in the air was detected every 30 minutes. During the detection, the ethanol detection instrument was placed close to the application position of the sustained-release agent, and the air at the position was blown into the ethanol detection instrument to detect the ethanol concentration, and the following table was obtained:

[0074] 30min 60min 90min Example 1 0.35% 0.17% 0.09% Example 2 0.31% 0.19% 0.12% Example 3 0.25% 0.22% 0.19% Example 4 0.27% 0.21% 0.17% Control group 0.46% 0.12% 0%

[0075] It can be seen from the data in the above table that the addition of more volatile ether can absorb heat through the volatilization of ether and inhibit the volatilization of ethanol, thereby increasing the retention time of ethanol in the sustained-release agent, thereby increasing the timeliness of disinfection and improving the effect of disinfection.

[0076] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited by the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, and these changes and improvements all fall within the scope of the present invention to be protected.

Claims

1. A polymer nanogel sustained-release agent, characterized in that: The raw materials used include a main material and auxiliary materials, wherein the main material includes 90-140 parts of a water-absorbing resin, 100-150 parts of polyethylene glycol, 20-35 parts of ethanol, and 40-65 parts of triclocarban in terms of weight. The raw materials of the auxiliary material include 2-7 parts of ether, 20-30 parts of water, 1-7 parts of menthol, 1-5 parts of bitter essence, 3-10 parts of zinc sulfate, 40-70 parts of aloe vera gel, 1-6 parts of vitamin E, 2-8 parts of hyaluronic acid, and 5-15 parts of lauric acid in parts by weight.

2. A polymer nanogel sustained-release agent according to claim 1, characterized in that: The raw materials used include main materials and auxiliary materials. The main materials include 90 parts of water-absorbing resin, 100 parts of polyethylene glycol, 20 parts of ethanol, and 40 parts of triclocarban in terms of weight. The raw materials of the auxiliary material include 2 parts of ether, 20 parts of water, 1 part of menthol, 1 part of bitter essence, 3 parts of zinc sulfate, 40 parts of aloe vera gel, 1 part of vitamin E, 2 parts of hyaluronic acid, and 5 parts of lauric acid in parts by weight.

3. A polymer nanogel sustained-release agent according to claim 1, characterized in that: The raw materials used include main materials and auxiliary materials. The main materials include 105 parts of water-absorbing resin, 115 parts of polyethylene glycol, 25 parts of ethanol, and 48 parts of triclocarban in terms of weight. The raw materials of the auxiliary material include 4 parts of ether, 23 parts of water, 3 parts of menthol, 2 parts of bitter essence, 5 parts of zinc sulfate, 50 parts of aloe vera gel, 3 parts of vitamin E, 4 parts of hyaluronic acid, and 8 parts of lauric acid in parts by weight.

4. The polymer nanogel sustained-release agent according to claim 1, characterized in that: The raw materials used include main materials and auxiliary materials. The main materials include 120 parts of water-absorbing resin, 130 parts of polyethylene glycol, 30 parts of ethanol, and 55 parts of triclocarban in terms of weight. The raw materials of the auxiliary material include 6 parts of ether, 27 parts of water, 5 parts of menthol, 4 parts of bitter essence, 8 parts of zinc sulfate, 60 parts of aloe vera gel, 5 parts of vitamin E, 6 parts of hyaluronic acid, and 12 parts of lauric acid in parts by weight.

5. The polymer nanogel sustained-release agent according to claim 1, characterized in that: The raw materials used include main materials and auxiliary materials. The main materials include 140 parts of water-absorbing resin, 150 parts of polyethylene glycol, 35 parts of ethanol, and 65 parts of triclocarban in terms of weight. The raw materials of the auxiliary material include 7 parts of ether, 30 parts of water, 7 parts of menthol, 5 parts of bitter essence, 10 parts of zinc sulfate, 70 parts of aloe vera gel, 6 parts of vitamin E, 8 parts of hyaluronic acid, and 15 parts of lauric acid in parts by weight.

6. A production process for the polymer nanogel sustained-release agent according to any one of claims 1 to 5, characterized in that: The specific steps are as follows: Step 1: firstly mix the water-absorbing resin and polyethylene glycol according to weight proportions, and the two are in a gel state after mixing; Step 2: Add ethanol and triclocarban according to weight proportions to the mixture of water-absorbing resin and polyethylene glycol and stir evenly for use; the main material formed after mixing needs to be refrigerated for use; Step 3: Add menthol, bitter essence and zinc sulfate according to their weight parts into water and stir to dissolve, then add ether according to their weight parts, stir to mix and refrigerate for later use; Step 4: Add corresponding weight portions of vitamin E, hyaluronic acid and lauric acid to corresponding weight portions of aloe vera gel, and slowly stir to mix evenly; Step 5: First slowly stir and mix the stirred and mixed aloe vera gel and the main ingredients, then add the solution in step 3 and continue to slowly stir and mix. After mixing, the polymer nanogel sustained-release agent can be prepared and the sustained-release agent can be stored in an environment of 2-5°C.