Method of manufacturing microfluidic structure

By using the phase change technology of supporting materials in the microfluidic structure, the problem of difficulty in removing the support structure after curing is solved, and the stable manufacturing and precise removal of complex shape channels are achieved, and the manufacturing accuracy is improved.

CN118876306APending Publication Date: 2024-11-01UNHINDR LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410907374.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2019-09-19
Filing Date
2020-09-18
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

When manufacturing microfluidic structures, the support structure is difficult to remove after curing, especially when the channel shape is complex or long.

Method used

The uncured polymer material is poured into the mold partially cured, the support material is arranged and the uncured material is poured to form a second layer, which is easy to set and remove by phase change of the support material to form a channel in the microfluidic structure. The support material can be phase-transformed by freezing or sublimation, so that it is easy to remove after curing.

Benefits of technology

The stability and removal problems of forming complex shape channels in the microfluidic structure are achieved, the manufacturing accuracy and the certainty of channel shape are improved, and the setting and removal process of support materials is simplified.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876306A_ABST
    Figure CN118876306A_ABST
Patent Text Reader

Abstract

A method of manufacturing a microfluidic structure, the microfluidic structure comprising at least one channel disposed therein, the method comprising: pouring an uncured polymeric material into a mold to produce a first layer; at least partially curing the first layer; and arranging a support material on the first layer; casting an uncured polymeric material onto the first layer to form a second layer, thereby encapsulating the support material; and at least partially curing the second layer such that the first layer and the second layer together form the microfluidic structure to form the at least one channel; wherein the support material undergoes a phase change during formation of the at least one channel.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of Chinese invention patent application No. 202080068667.9. The Chinese invention patent application is based on international application PCT / GB2020 / 052267, with the application date of September 18, 2020, and the invention name is "Method for manufacturing microfluidic structure". Technical Field

[0002] The present invention relates to microfluidic structures, such as microfluidic chips, and methods of making such structures. Such structures include small channels through which fluids can pass, and can be made of polymer materials. The production of such microfluidic structures requires high-precision manufacturing, and the size of the channels that can be incorporated into such structures may be limited by available manufacturing processes and / or materials. Background Art

[0003] When polymer materials are used to produce microfluidic structures, support structures are often used to maintain the shape of channels within the polymeric structure during the curing of the polymer material. However, after curing is complete, it can be difficult to remove the material used to support the channels.

[0004] In some known methods, a soluble material such as sugar can be used as a material to support the channel during curing. Other soluble materials can also be used, such as soluble materials that can be deposited using additive layer manufacturing. In this method, water or another liquid can be used to dissolve the soluble material so that the support material can be removed after curing. However, if the channel has a complex shape or is long, it may be difficult to remove the soluble material due to the length and complexity of the channel.

[0005] The object of the present invention is to at least partially solve the above problems. Summary of the invention

[0006] According to the present disclosure, a method for manufacturing a microfluidic structure is provided, the microfluidic structure including at least one channel disposed therein, the method including pouring an uncured polymer material into a mold to produce a first layer, at least partially curing the first layer, and by disposing a support material on the first layer, pouring an uncured polymer material onto the first layer to form a second layer, thereby encapsulating the support material and at least partially curing the second layer, so that the first layer and the second layer together form the microfluidic structure to form the at least one channel, wherein the support material undergoes a phase change during the formation of the at least one channel. That is, the phase of the support material itself can change from solid, liquid or gas to another of solid, liquid or gas. This can allow the support material to be more easily disposed and / or removed than an arrangement in which a solid material is dissolved by a different liquid.

[0007] Optionally, the first layer comprises at least one open channel, the support material is a fluid when disposed on the first layer, and forming the at least one channel comprises: at least partially filling the open channel with the fluid, curing the fluid, thereby providing the phase change, and enclosing at least a portion of the channel by pouring the uncured polymer material onto the first layer to form the second layer, thereby encapsulating the cured support material. That is, disposing the support material on the first layer comprises at least partially filling the open channel with the fluid. The phase change causes the support material to cure. This can allow the shape of the channel to be determined by a mold and the support material to be easily disposed on the first layer.

[0008] Optionally, the fluid is a liquid and the phase change is solidification of the liquid by freezing.

[0009] Optionally, the support material is solid when provided on the first layer.This may allow the shape of the channel to be pre-formed as a separate component.

[0010] Optionally, wherein the phase change is sublimation. This may allow the support material to be removed more easily than an arrangement in which the material is dissolved in a liquid.

[0011] Optionally, the polymer material is an elastomeric material. Optionally, the elastomeric material includes one or more of silicone, acrylic, nitrile, rubber and polyurethane.

[0012] Optionally, the method further comprises removing the support material from the channel.

[0013] Optionally, the step of removing the support material from the channel and the step of curing the second layer overlap in time.

[0014] Optionally, the method further comprises pouring an uncured polymer material into the mold to produce a third layer, at least partially curing the third layer, disposing the third layer on the second layer before curing of the second layer is complete, and curing the second layer and the third layer together such that a bond is formed between the second layer and the third layer. This may allow for the formation of multiple layered structures.

[0015] Optionally, the method further comprises filling the open channel in the third layer with a fluid, curing the liquid, closing at least a portion of the channel by pouring an uncured polymer material onto the third layer to form a fourth layer, thereby encapsulating the cured fluid, and at least partially curing the fourth layer so that the third layer and the fourth layer are connected to the microfluidic structure. This can allow for the formation of multiple layers of channels in a single structure.

[0016] Optionally, curing of the second layer of polymeric material results in formation of a bond between at least two of the layers.

[0017] Optionally, the passage comprises at least one opening through at least one of the layers.

[0018] Optionally, the channel comprises a plurality of openings through at least one of the layers. This may allow fluid to be introduced into and removed from the structure.

[0019] Optionally, the channel comprises openings at opposite ends of the microfluidic structure.

[0020] Optionally, the method further comprises providing an electronic component through the at least one opening. This may allow the structure to be used as a flow control element.

[0021] Optionally, the cross-section of the open channel is partially elliptical.

[0022] Optionally, the at least one channel is a channel network.

[0023] Optionally, the channel network comprises a manifold arranged to receive and / or store fluid and a plurality of branches fluidly connected to the manifold.

[0024] Optionally, the support material is water.

[0025] Optionally, the freezing step is performed at a temperature of -30 degrees Celsius or lower, preferably at a temperature of -50 degrees Celsius or lower, more preferably at a temperature of -80 degrees Celsius or lower.

[0026] Optionally, the method further comprises disposing an additional support material on the first layer, wherein the additional support material is different from the support material, the additional support material does not undergo a phase change during the forming of the channel, and the additional support material remains between the first layer and the second layer.

[0027] Optionally, the additional support material is a substantially flat sheet, preferably wax paper or metal foil.

[0028] Optionally, the additional support material is arranged to interact with a fluid disposed in the microfluidic structure.

[0029] According to the present disclosure, a method for manufacturing a microfluidic structure is also provided, wherein the microfluidic structure includes at least one channel arranged therein, the method including pouring an uncured polymer material into a mold to produce a first layer, at least partially curing the first layer, encapsulating the support material by setting a support material on the first layer, pouring the uncured polymer material onto the first layer to form a second layer, and at least partially curing the second layer so that the first layer and the second layer together form the microfluidic structure to form the at least one channel, wherein the support material does not undergo a phase change during the formation of the at least one channel, and the support material remains between the first layer and the second layer.

[0030] Optionally, the support material is arranged to interact with a fluid disposed in the microfluidic structure.

[0031] According to the present disclosure, a microfluidic structure obtainable by the above method is also provided.

[0032] According to the present disclosure, a microfluidic structure is also provided, comprising a channel network, wherein the channel network comprises a manifold arranged to receive and / or store fluid and a plurality of branches fluidically connected to the manifold, wherein the microfluidic structure is a flexible sheet.

[0033] Optionally, the microfluidic structure is a microfluidic chip.

[0034] Optionally, the microfluidic structure comprises two channels connected in selective fluid communication via an electronic component.

[0035] Optionally, at least one channel is arranged to receive a fluid to increase at least one of the surface area or volume of the microfluidic structure, and / or at least one channel is arranged to change volume to allow or prevent flow through another channel in the microfluidic structure.

[0036] According to the present disclosure, there is also provided a pad for arranging a device for skin contact, comprising at least one microfluidic structure as described above. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The present invention will now be described, by way of non-limiting example only, with reference to the accompanying drawings, in which:

[0038] Figure 1 A mold for fabricating a microfluidic structure is shown;

[0039] Figure 2 A first layer of uncured polymer material in a mold is shown;

[0040] Figure 3 showing a cured first layer including open channels;

[0041] Figure 4 shows an open channel filled with a liquid Figure 3 Layer;

[0042] Figure 5 Shows Figure 4 an arrangement wherein a second layer of uncured polymer material is added after the liquid has cured;

[0043] Figure 6 Shown after curing the second layer Figure 5 Arrangement;

[0044] Figure 7 shows the microfluidic structure after removal of the liquid;

[0045] Figure 8 Various molds used in methods of manufacturing microfluidic structures are shown;

[0046] Fig. 9 An example of a channel network in a microfluidic structure is shown;

[0047] Fig.10 A structure including a through hole is shown;

[0048] Fig.11 Shown for manufacturing Fig.10 The structure of the mold in the method;

[0049] Fig.12 A pad in a prosthesis is shown;

[0050] Fig.13 A liner in a prosthesis is shown with fluid supplied to its chamber;

[0051] Fig.14 A microfluidic structure having three layers, and interconnections between the layers are shown;

[0052] Fig.15 A cured first layer comprising three open channels is shown;

[0053] Fig.16 Shown with additional support material Fig.15 Arrangement;

[0054] Fig.17 Shows Fig.16 An arrangement in which the open channel is filled with a liquid;

[0055] Fig.18 Shows Fig.17 an arrangement wherein a second layer of uncured polymer material is added after the liquid has cured;

[0056] Fig.19It shows that after removing the liquid Figure 15-18 The structure formed in

[0057] Fig. 20 Shows Fig.19 A structure in which the additional channels are visible and the support material remains in the structure. DETAILED DESCRIPTION

[0058] The present invention provides a method for manufacturing a microfluidic structure, which includes at least one channel within the microfluidic structure. The structure can be a microfluidic chip. This microfluidic chip can have one or more channels arranged inside the chip, which allow fluid to pass through. In particular, the structure can include a channel network that can be used in many different applications. For example, the chip can be formed of a flexible material, such as an elastomeric polymer, particularly an elastomer. This chip can include a flexible manifold. That is, the fluid can be retained in the chip and moved around in the chip and / or moved to other components connected to the chip.

[0059] Now refer to Figure 1-7 The method of manufacturing a microfluidic structure is described, wherein a simplified representation including a single channel is shown. However, it should be understood that the channel can form a channel network of any suitable shape, such as Figure 8 and Fig. 9 shown.

[0060] The mold 10 is used to produce the first layer of the structure. Figure 1 As shown, the mold may have raised portions 11 which correspond to the desired shape and position of the channels in the structure. Fig.11 A single raised portion corresponding to a single channel is shown in FIG, but a more complex shaped mold may be used to produce a corresponding more complex shaped channel, e.g. Figure 8 Such molds are those shown in , in which a network of channels is provided spanning from one side of the mold to the other.

[0061] like Figure 2 As shown, an uncured polymer material is poured into a mold 10 to form a first layer 12. The first layer is then at least partially cured so that it retains the shape defined by the mold 10. The curing process can be performed using any suitable method known in the art, including chemically initiated curing or (for example, thermosetting materials) induced curing by heat or radiation. If the first layer is partially cured, once it is removed from the mold, the layer can retain the shape defined by the mold, but can still retain the ability to form further bonds with (i.e., connect to) additional layers of polymer material, as will be described below.

[0062] like Figure 3, which shows the first layer 12 after (partial) curing and removal from the mold 10, forming open channels 13 at the locations of the raised portions 11 of the mold. It should be noted that the first layer 12 Figure 3 The first layer 12 has been flipped so that the open channels face upward. At this stage, the first layer 12 can be placed in a second mold 14 for subsequent steps, or as described below, this can be done later in the process. Figure 3 As shown, the open channel opens to one surface of the first layer 12 and appears in cross section as a depression in the surface of the first layer 12. Figure 3 In the arrangement shown, the top surface of the first layer 12 is narrower than the bottom surface of the first layer. This is because when pouring the uncured elastomer, a meniscus may form, such as Figure 2 This can result in Figure 3 The bottom surface of the first layer 12 (ie, Figure 2 The top surface of the first layer 12 in Figure 3 The top surface of the first layer 12 is long, resulting in Figure 3 However, depending on the material used, the meniscus may not be formed, or it may be negligible, and therefore Figure 3 In contrast to the trapezoidal shape shown in FIG. 1 , the cross section of the first layer 12 may also be rectangular.

[0063] Usually, if Figure 3 As shown, the cross-section of the open channel is a portion of an ellipse, such as a semicircle or an ellipse with a portion of its circumference removed. Depending on the material used, channels with different cross-sectional shapes can be used. For substantially flexible materials, a channel such as Figure 3 The cross-sectional shape shown is an ellipse having less than half of its circumference. In this case, the flexibility of the material can allow the first layer 12 to be removed from the mold. For less flexible materials, a semi-ellipse or an ellipse shape with more than half of its circumference removed can be used to facilitate the removal of the first layer 12 from the mold 10. It should be understood that a circle is a specific example of an ellipse. It should also be understood that the cross-section can have any other geometric shape depending on the desired shape of the channel.

[0064] The open channel 13 is then at least partially filled with a liquid, such as Figure 4As shown. Liquid is used as a support material. The liquid may be water, or may be any other suitable liquid that can be frozen at an appropriate temperature. For example, an additive that changes the physical or chemical properties of the liquid may be added to the liquid. Such an additive may, for example, react with the liquid to lower its temperature to freeze the liquid, or may change the freezing point of the liquid. The open channel may be completely filled with liquid, or, for a liquid that expands when frozen, may be partially filled with enough liquid so that once the liquid freezes, it forms the desired shape of the rest of the channel. The degree to which the open channel is filled with liquid may be selected to take into account the change in volume of the liquid when it is frozen. In addition, when the liquid is disposed in the open channel, the surface tension of the liquid may form a meniscus that may have a convex shape when viewed from a cross section. That is, the channel is filled so that its surface extends above the surface of the layer in which the channel is disposed. When the liquid freezes, the change in volume may cause the frozen liquid to expand or contract, thereby providing a support material of the desired shape in the channel.

[0065] The liquid in the open channel is then frozen (i.e., undergoes a phase change). The frozen liquid serves as a support material, which allows a second polymer layer to be disposed on top of the first layer and to form a closed channel between the first layer and the second layer. In other words, once the structure has been formed, the frozen liquid fills the space that will form the channel. It should be understood that the terms "frozen" and "freezing" generally refer to solidified liquids. The term is not limited to the use of any particular temperature or liquid, and can be used to describe the process of changing the temperature of any liquid so that it changes phase to a solid phase.

[0066] Freezing can be performed at any suitable temperature, but the temperature is preferably low enough so that the liquid remains frozen during at least a portion of the subsequent process of solidifying the second layer, so that the frozen liquid can support the unsolidified liquid layer in the region of the channel. In particular, freezing can be performed at a temperature of -30 degrees Celsius or lower, preferably at a temperature of -50 degrees Celsius or lower, and more preferably at a temperature of -80 degrees Celsius or lower.

[0067] Freezing may be performed by placing the first layer and the liquid in the channel in an atmosphere of appropriate temperature. Alternatively or additionally, local cooling may be applied to the liquid in the channel to bring it to the desired temperature.

[0068] After the step of freezing the liquid, as Figure 5As shown, an uncured polymer material is poured onto the first layer 12 to form the second layer 16. Thus, the frozen liquid is encapsulated between the first layer and the second layer, and a closed channel is formed around the frozen liquid, which is defined between the first layer 12 and the second layer 16. In other words, the frozen liquid supports a portion of the second layer 16 located above the open portion of the channel, and the portion of the second layer closes the channel. The second layer 16 can be poured into the second mold 14, and the first layer 12 is set in the second mold 14 before the second layer 16 is poured.

[0069] The second layer 16 is then at least partially cured. During the curing process of the second layer, crosslinks (i.e., chemical bonds) may be formed between the first layer 12 and the second layer 16 to connect the first layer and the second layer. This may result in a structure that forms a continuous block 1, such as Figure 6 and Figure 7 In other words, once curing of the structure has been completed, the first layer and the second layer may no longer be individually identifiable, particularly if the first layer and the second layer are formed using the same material. It should be understood that if the first layer and the second layer have different mechanical properties or are formed from different materials from each other, the layers are still connected together but can still be individually identifiable.

[0070] After the second layer solidifies, or during the process of solidifying the second layer, the frozen liquid (i.e., support material) undergoes another phase change. The frozen liquid can be allowed to return to a liquid state (i.e., melt) and removed from the channel. Alternatively, the solid can change phase directly to a gas (i.e., sublime). The support material can be removed using air, by suction or by blowing air through the channel or by any other suitable process. Figure 7 The finished structure with the liquid removed is shown in .

[0071] The method described above allows very small diameter channels to be formed in microfluidic structures. In addition, because the substance supporting the channel (ie, the support material) is liquid when the second layer of uncured polymer is cast, it can be easily removed once it melts.

[0072] In the above arrangement, a liquid is used as the support material, and thus the liquid is solidified by freezing. However, the support material may be initially a gas, and the phase change may be from gas to liquid and then to solid, or may be directly from gas to solid.

[0073] In another arrangement, when the support material is provided on the first layer, the support material may be solid, rather than liquid or gas. For example, the support material may be used to form a pattern, wherein the shape of the pattern corresponds to the shape of the channel to be formed. The first polymer material layer is formed by pouring an uncured polymer material into a mold, and the first layer is at least partially cured. In contrast to the above arrangement, during the formation of the first layer, no (open) channel is required to be formed in the first layer by the mold.

[0074] After the first layer is at least partially solidified, the pattern is placed on the first layer, and an uncured elastomer is poured on top of the first layer and the pattern to encapsulate the support material, thereby forming the second layer. The second layer is then at least partially solidified. Then, after forming the second layer and / or during the curing process of the second layer, the support material can undergo a phase change. In some arrangements, the solid can become a liquid phase (i.e., a melt, as described above). In other arrangements, the solid can sublime (i.e., directly change from a solid phase to a gas phase). In both cases, once the support material undergoes a phase change, the support material can be removed. Phase change can be caused by exposing the structure to a change in temperature or pressure, or phase change can occur at ambient temperature. Suitable materials that can be used for sublimable support materials include, but are not limited to, naphthalene and dry ice (solid carbon dioxide).

[0075] The above arrangement in which the support material is solid when provided on the first layer also allows very small diameter channels to be formed in the microfluidic structure. In addition, because the substance supporting the channel (i.e., the support material) undergoes a phase change, it can be easily removed after the phase change. It will be appreciated that such a phase change can provide easier removal of the support material than known arrangements, for example in which the material is dissolved.

[0076] Both of the above approaches can be extended to include forming additional layers on the structure. This can allow layers to be "stacked" on top of each other, with multiple channels or networks of channels provided in the same structure. Channels in different layers can also be interconnected through openings between those layers, allowing fluid communication between channels in different layers. Such a configuration can be Fig.14 shown and described below.

[0077] To form this structure, an uncured polymer material can be poured into a mold to produce a third layer including at least one open channel. It should be understood that the mold can have the same shape as the mold used to form the first layer, or can have a different shape, depending on the desired shape of the channel in the third layer. The mold can include one or more raised portions in the mold that extend above the level to which the uncured polymer is poured to provide an opening as described below. These can allow interconnection between the third layer and the other layers.

[0078] The third layer is then at least partially cured so that it retains the shape defined by the mold. As with the first layer, if the third layer is partially cured, once it is removed from the mold, the layer may retain the shape defined by the mold, but may still retain the ability to form further bonds with (i.e., connect to) further layers of polymeric material.

[0079] Once formed, the third layer is then disposed on the second layer, with the surface of the third layer that does not have an open channel in contact with the second layer. This can be done while the second layer is partially cured. This allows the second and third layers to subsequently cure together so that a bond is formed between the second and third layers. That is, the third layer is connected to the second layer.

[0080] After the third layer has been connected to the second layer, the step of closing the open channels in the third layer as described above with respect to the first and second layers is performed. That is, the open channels in the third layer are at least partially filled with a liquid (which is an example of a fluid), and the liquid in the open channels is then frozen (i.e., solidified).

[0081] After the step of freezing the liquid, an uncured polymer material is poured onto the third layer to form a fourth layer. Thus, the frozen liquid is encapsulated between the third layer and the fourth layer, and a closed channel defined between the third layer and the fourth layer is formed around the frozen liquid. In other words, the frozen liquid supports a portion of the fourth layer above the opening portion of the channel. Thus, a closed channel is formed.

[0082] The fourth layer is then at least partially cured. During the curing process of the fourth layer, crosslinks (i.e., chemical bonds) can be formed between the third layer and the fourth layer so that the structure forms a continuous block. In other words, once the structure is complete, the third layer and the fourth layer are interconnected. During this step, additional crosslinks can also be formed between the second layer and the third layer. In some arrangements, the third layer and the fourth layer may no longer be individually identifiable. It should be understood that if the third layer and the fourth layer have different mechanical properties or are formed of different materials from each other, these layers are connected together, but can still be individually identifiable.

[0083] After the fourth layer solidifies, or during the process of solidifying the fourth layer, the frozen liquid returns to a liquid state and is removed from the channel. The liquid may be removed using air, by suction or by blowing air through the channel, or by any other suitable process.

[0084] When the third and fourth layers are added to the structure as described above, the steps of curing the various layers can be timed to provide crosslinks between each layer that contacts each other. That is, all layers can be partially cured when they are first formed, and each subsequent layer can be placed on the previous layer before the curing of the previous layer is complete. This can ensure the structural integrity of the block and allow the properties of the block to be controlled during manufacturing by controlling the curing of each layer.

[0085] It should be understood that the above steps can be performed as many times as necessary to provide additional channel groups stacked in additional layers in the structure. In other words, the steps of adding additional layers as described above with respect to the third and fourth layers can be repeated multiple times to create a multilayer structure. It should also be understood that an arrangement using an initial solid support material can be used for some layers, and an arrangement using an initial liquid support material can be used for other layers in the same structure.

[0086] Fig.14 A schematic representation of such a multilayer structure comprising three structural layers is shown in FIG. Figure 7 , but with a plurality of channels 31 and interconnections 32 between some of the channels in the same layer and between the layers 30a, 30b, 30c. It should be understood that each of the structural layers 30a, 30b, 30c in the finished structure can be produced by the above method, so that each layer is made by combining two separate layers of polymer material. That is, the above first and second layers constitute the first structural layer 30a, and the above third and fourth layers constitute the second structural layer 30b. Although Fig.14 30a, 30b, 30c, but it should be understood that these connections may not be individually identifiable in the finished structure. The interconnect 32 can be formed using the same process as the channel 31 itself. Therefore, the interconnect can also be considered as an additional channel provided in the structure.

[0087] Fig.14 The arrangement in comprises three structural layers 30a, 30b, 30c, wherein there is an interconnection between a channel in the second layer and a channel in the third layer, and an interconnection between two channels in the third layer. However, it should be understood that this is merely an exemplary arrangement, and any other combination of interconnections between channels in the same structural layer and in different structural layers is possible.

[0088] In addition to the above methods including support materials that undergo phase change, in some arrangements, additional support materials that do not undergo phase change can be used. In one arrangement, the additional support material can be retained inside the finished structure. In this arrangement, the additional support material can be a substantially flat flexible sheet. Such a sheet can be a sheet of wax paper, waxy plastic, or a paper or plastic material coated with another organic coating, a sheet of metal foil (e.g., aluminum foil), or a sheet formed by or comprising an organic polymer. The thickness of this flat flexible sheet can be less than 1 mm, and preferably 0.3-0.7 mm, more preferably substantially 0.5 mm.

[0089] The use of additional support materials that do not undergo phase changes can be particularly useful for forming structures in which channels extend in different directions within a given structural layer. In some arrangements, it may be desirable for such channels to intersect each other without being fluidly connected to each other. This may be difficult to achieve in arrangements in which the support material is initially fluid during channel formation, because channels within the same structural layer are filled with a single continuous fluid extension, which causes the finished channels to merge with each other (i.e., fluidly connected). In addition, it may be desirable to provide channels that bridge two of the individual layers 12, 16 formed during the process of manufacturing a single structural layer, or bridge channels between finished structural layers.

[0090] In order to provide separation of channels that cross each other or bridge layers as described above in the same structural layer, additional support materials as described above can be used. The process of using such additional support materials is as follows Figure 15-20 shown and described below.

[0091] In addition to the (primary) support material 15, additional support material is provided on the first layer 12 during the process. When a flat sheet is used, this can provide "breaks" in the polymer that are formed during the casting of the polymer, which form discontinuities in the polymer of the finished structure. Such discontinuities can in turn form additional channels.

[0092] exist Figure 15-20 In the process shown in Fig.15 A first layer 12 is shown, which is similar to Figure 3 The first layer shown in FIG. 1 has three channels 13a, 13b, 13c. It should be understood that in the finished structure, the channel 13 is Fig.15 The cross-section shown extends in the direction "into the page".

[0093] The use of additional support material 40 allows the formation of additional channels 40a (e.g. Fig. 20 ), which spans between the two outer channels 13a and 13c and bypasses the middle channel 13b. Fig. 20In the view of FIG. 1 , the additional channel 40a extends in a direction from left to right. That is, the additional channel 40a extends in a direction perpendicular to the channel 13. In other words, as described above, the additional channel 40a intersects the channel 13b without being fluidically connected thereto, and connects or bridges between the channels 13a and 13c.

[0094] In the already formed Fig.15 After the first layer 12 shown in Figure 3 The same process described above is followed by providing additional support material 40 on the first layer 12, inside the channel 13 and in the desired shape of the additional channel 40a. It will be appreciated that the additional support material need not extend along the entire length of the channel 13, but only partially along the length of the channel in the direction "into the page".

[0095] Once the additional support material 40 is provided, the support material 15 (which in this arrangement can be considered the "primary" support material) is provided, as in the above process. For example, a liquid can be poured into the channel 13 and the liquid support material frozen, as described above with respect to Figure 4 described. Fig.17 shows the support material 15 after it has been added Fig.16 , in which the additional support material 40 is arranged within the (main) support material 15 and thus within the channel 13.

[0096] Fig.18 shows the second layer 16 after it has been provided. Fig.17 The arrangement is similar to Figure 5 Add to Figure 4 The presence of additional support material 40 in the first and second layers creates the above-mentioned discontinuity.

[0097] Fig.19 The finished structure is shown, wherein the three channels 13a, 13b, 13c and the additional support material 40 remain in the finished structure. Fig. 20 As shown, additional channels 40a may be naturally formed around additional support material 40, or may open around discontinuities caused by additional support material when fluid is provided in the structure.

[0098] In one arrangement, the additional support material is shaped so that one channel extends in a direction perpendicular to the direction in which the channel extends (i.e., in Figure 7The additional support material is a substantially flat flexible sheet, so once a closed channel is formed, it can abut the wall of the channel and not interfere with the channel, or it can remain disposed within the channel without preventing flow through the channel due to its thickness. Therefore, it does not need to be removed from the structure and remains in the finished structure. As described above, the support material that does undergo a phase change (i.e., the primary support material) can be removed while retaining the additional support material in place.

[0099] In addition, the additional support material can have another function of interacting with the fluid in the channel in a favorable manner. The interaction can be a chemical interaction or a physical interaction. For example, the additional support material can have a substance embedded therein, which can be absorbed from the additional support material by the fluid in the channel. This can allow the properties of the fluid to be changed. In another example, the additional support material can be used as a filter to remove substances from the fluid in the channel (i.e., absorbing substances from the fluid, rather than absorbing fluid substances from the additional support material). In another example, the additional support material can contain substances that are retained in the additional support material, but chemical reactions occur in the fluid in the structure. Therefore, the additional support material can have two functions, namely its function in forming the channel as described above, and the function of interacting with the fluid in the finished structure.

[0100] It should also be understood that in some arrangements, a support material that does not undergo a phase change during the process of forming a channel may be used instead of a support material that does undergo a phase change during the process of forming a channel. Such a support material may be, for example, a substantially flat flexible sheet (as described above as an "additional support material"). It should be understood that in such an arrangement, the flexible sheet is used as the (primary) support material, rather than the additional support material. In other words, a support material that does not undergo a phase change during the process of forming at least one channel and that remains between the first layer and the second layer replaces the support material that undergoes a phase change.

[0101] The polymer material used in the above method can be any curable polymer. In particular, a polymer elastomeric material (i.e., an elastomer) or a thermosetting material. The elastomeric material can be (but is not limited to) one or more of silicone, PDMS (polydimethylsiloxane), acrylic resin, nitrile, rubber, and polyurethane. The materials used for the first layer and the second layer can be the same or different, and any combination of the materials mentioned below can be used. The polymer material can be selected according to the desired properties of the microfluidic structure. For example, if a flexible structure is required, silicone may be particularly suitable, or if a more rigid structure is required, a more rigid polymer (e.g., acrylic resin) can be used. Different materials can be used for different layers, which can be used to combine the properties of different materials (e.g., to produce a semi-rigid structure in which one layer and therefore a portion of the structure has a different rigidity from another layer).

[0102] The mold used in the above method can be manufactured using additive layer manufacturing (3-D printing), and the mold can be produced as part of the method to provide the desired channel layout. However, the mold can also be produced by any other suitable method. Examples of suitable molds are Figure 8 shown.

[0103] The microfluidic structure produced by the above method can form a flexible sheet. In other words, the sheet can have two main surfaces separated in the thickness direction. The two main surfaces can extend substantially parallel to each other. The remaining one or more surfaces can extend in the thickness direction (i.e., the direction perpendicular to the direction in which the main surfaces extend). These remaining surfaces can have a smaller area than the main surface and can be considered as the side surface or edge of the sheet. In some arrangements, the sheet can have a square or rectangular shape so that the structure has a cubic shape, in which two faces are much larger than the remaining faces, and the remaining (smaller) faces form edges in the thickness direction.

[0104] It should be understood that the flexible sheet is not limited to this particular shape, but different geometries of the flexible sheet are within the scope of the present disclosure. The flexible sheet can be any shape suitable for use as an interface between rigid surfaces, including parabolic, annular, flat, or a combination of some or all of these geometries.

[0105] In some arrangements, the structure includes one or more openings into the channel. That is, the one or more openings allow fluid to be introduced into or removed from the structure.

[0106] In some arrangements, there may be two openings on opposite sides of the structure. These may be on the side surfaces in the thickness direction. This may allow a fluid to be introduced into the structure and flow through the channel. For example, the openings may be provided on opposite edge surfaces of the sheet so that a fluid may be introduced through one opening and removed through the other opening.

[0107] As mentioned above, at least one channel may be a channel network. That is, a number of different channels may be provided in the structure, which channels may be connected together or may be separated from each other. Fig. 9 An example of such a channel network is shown in FIG. In some arrangements, the channel network may include a manifold and a number of branch pipes connected to the manifold fluid. The manifold may be a channel forming a space arranged to store and / or retain fluid therein. The branch pipes may be connected to the manifold directly or indirectly (e.g., via valves) so that fluid can be supplied from the manifold to the branch pipes.

[0108] Additionally, one or more openings may be provided on a major surface of the structure, such as Fig.10 Such openings may be formed during the formation of the first layer by providing raised portions in the mould extending above the level to which the uncured polymer is poured. These may take the form of posts (or columns) 18 extending from the base of the mould. Fig.11 A corresponding mold that can be used to produce such a layer is shown. Thus, when the cured first layer is removed from the mold, through holes 17 are present in the first layer, which then form openings in the channels in the main surface of the structure. The raised portions in the mold can also be used for other purposes. For example, when a layer with through holes entering the channels has been formed, they can be used to block the holes when the channels are filled with liquid to prevent the liquid from leaking before freezing. In addition, the mold for forming subsequent layers (e.g., the second mold 14 as described above) can include posts 18, which correspond to the through holes 17 in the layers that have been formed. These posts can be used to block the holes during the casting of the uncured polymer of the subsequent layers, and to form additional holes in the subsequent layers that align with the holes in the layers that have been formed.

[0109] The openings in the major surfaces of the structure can be used for a variety of purposes. For example, other components such as electronic components or fluid control components can be mounted to the structure (i.e., disposed through at least one of the openings). For example, a valve can be inserted into a through hole (i.e., mounted to the structure) to control flow through the passage. Electronic components can also be mounted to the structure via a conduit that is in fluid communication with the opening.

[0110] In some arrangements, there may be one or more channels (e.g., branches as described above) that are not directly linked together (i.e., linked together inside the structure). Instead, one or more valves may be provided, which may be arranged so that the valve selectively allows or prevents fluid communication between two channels. In some arrangements, the valve may be an electronic valve or a pneumatic valve mounted to (or in) the structure. This may allow the structure to be used as a flow control element.

[0111] Furthermore, in some arrangements, a channel of the structure itself can be used as a valve to allow or prevent flow through another channel of the structure. That is, one channel can be arranged so that when it is filled with fluid, its volume changes so that it blocks another channel. Again, this can allow the structure to act as a flow control element and control the flow of fluid through the structure itself.

[0112] The microfluidic structure can be used in a cushion for a device such as a prosthesis or other device that contacts a body part. For example, the object or surface can be a medical or non-medical device arranged for skin contact. The cushion can also include a plurality of chambers arranged to store or retain fluids. In some arrangements, the channels are arranged to receive the fluid so that at least one of the surface area or volume of the microfluidic structure is increased, which can provide improved cushioning of the body part or gripping of the body part. Fig.12 and 13 Explain its examples.

[0113] Fig.12 and Fig.13 An example of a cushion 19 having a plurality of chambers 20 implemented in a prosthesis 21 is shown. The chambers 20 are connected by channels and in fact the chambers and channels together can be considered as a network of channels as described above. That is, the chambers themselves are also channels. Fig.12 The chamber 20 is shown in a state where it is not filled with fluid and therefore has a small volume. Fig.13 The state of fluid supply to chamber 20 is shown. Fluid may be supplied through one or more openings as described above, and any number of chambers may be supplied through any number of openings.

[0114] When the fluid is supplied to the opening, the chamber 20 may be partially or completely filled with the fluid. If the fluid is a gas, the fluid may fill the entire volume of the chamber 20. When the fluid is supplied, the volume of the chamber may increase. The increase in the volume of the chamber may result in an increase in the surface area and / or volume of the pad (i.e., structure) at the local area of ​​the pad corresponding to the corresponding chamber. This increase in volume may be at the inner surface of the pad and / or at the outer surface of the pad. In some examples, the chamber 20 may extend beyond the thickness of the unfilled pad (i.e., unfilled structure) when filled with fluid. The increase in volume and / or surface area is caused by the increase in pressure in the chamber caused by the fluid supply. Therefore, it is obvious that by changing the fluid supplied to the chamber, the increase in the surface area and / or volume of the pad at the local area of ​​the chamber can be controlled.

[0115] Furthermore, the structure is not limited to use as a cushion between a body part and a prosthesis, but is suitable for use as an interface between any suitable objects. In some non-limiting examples, the structure can be used to provide cushioning in a ski boot, a wheelchair, a mattress, or a helmet.

[0116] It should be understood by those skilled in the art that, although the present invention has been described with reference to exemplary embodiments, the present invention is not limited to the disclosed exemplary embodiments. Various modifications, combinations, sub-combinations, and variations may be made, depending on design requirements and other factors, as long as they are within the scope of the appended claims or their equivalents. Features from any example or embodiment of the present disclosure may be combined with features from any other example or embodiment of the present disclosure.

Claims

1. A method for manufacturing a microfluidic structure, the microfluidic structure comprising at least one channel disposed therein, the method include: pouring uncured polymer material into the mold to produce a first layer; at least partially curing the first layer; as well as The at least one channel is formed by: disposing a support material on the first layer; pouring an uncured polymer material onto the first layer to form a second layer, thereby encapsulating the support material; as well as at least partially curing the second layer such that the first layer and the second layer together form the microfluidic structure; Wherein, the support material undergoes a phase change during the process of forming the at least one channel.

2. The method according to claim 1, in: The first layer includes at least one open channel; When disposed on the first layer, the support material is a fluid; as well as Forming the at least one channel comprises: at least partially filling the open channel with the fluid; solidifying the fluid, thereby providing the phase change; and The cured support material is encapsulated by casting the uncured polymer material onto the first layer to form the second layer to close at least a portion of the channel.

3. The method according to claim 2, in, The fluid is a liquid, and the phase change is solidification of the liquid by freezing.

4. The method according to claim 1, in, The support material is solid when disposed on the first layer.

5. The method according to claim 1 or 4, in, The phase change is sublimation.

6. The method according to any one of the preceding claims, in, The polymer material is an elastomeric material, preferably comprising one or more of silicone, acrylic, nitrile, rubber and polyurethane.

7. A method according to any one of the preceding claims, further comprising removing the support material from the channel.

8. The method according to claim 7, in, The steps of removing the support material from the channels and curing the second layer overlap in time.

9. The method according to any one of the preceding claims, further comprising: include: pouring uncured polymer material into the mold to create a third layer; at least partially curing the third layer; before the curing of the second layer is completed, disposing the third layer on the second layer; as well as The second layer and the third layer are cured together such that a bond is formed between the second layer and the third layer.

10. The method according to claim 9, further comprising: include: filling the open channels in the third layer with a fluid; solidifying the liquid; encapsulating the solidified fluid by casting an uncured polymer material onto the third layer to form a fourth layer to close at least a portion of the channel; as well as The fourth layer is at least partially cured such that the third layer and the fourth layer are connected to the microfluidic structure.

11. The method according to any one of the preceding claims, in, Solidification of the second layer of polymeric material results in the formation of a bond between at least two of the layers.

12. The method according to any one of the preceding claims, in, The passage comprises at least one opening through at least one of the layers, and preferably comprises a plurality of openings through at least one of the layers.

13. The method according to any one of the preceding claims, in, The channel includes openings at opposite ends of the microfluidic structure.

14. The method of claim 12 or 13, further comprising positioning an electronic component through the at least one opening.

15. The method according to any one of the preceding claims, in, The cross section of the open channel is partially elliptical.

16. A method according to any one of the preceding claims, in, The at least one channel is a channel network.

17. The method according to claim 16, in, The channel network includes a manifold arranged to receive and / or store a fluid and a plurality of branches fluidly connected to the manifold.

18. A method according to any one of the preceding claims, in, The supporting material is water.

19. The method according to any one of claims 3 to 18, in, The freezing step is performed at a temperature of -30 degrees Celsius or lower, preferably at a temperature of -50 degrees Celsius or lower, and more preferably at a temperature of -80 degrees Celsius or lower.

20. The method of any of the preceding claims, further comprising providing an additional support material on the first layer, wherein the additional support material is different from the support material, the additional support material does not undergo a phase change during the forming of the channel, and the support material remains between the first layer and the second layer.

21. The method according to claim 20, in, The additional support material is a substantially flat sheet, preferably wax paper or metal foil.

22. The method according to claim 20 or 21, in, The additional support material is arranged to interact with a fluid disposed in the microfluidic structure.

23. A method of manufacturing a microfluidic structure, the microfluidic structure comprising at least one channel disposed therein, the method include: pouring uncured polymer material into the mold to produce a first layer; at least partially curing the first layer; as well as The at least one channel is formed by: disposing a support material on the first layer; pouring an uncured polymer material onto the first layer to form a second layer, thereby encapsulating the support material; as well as at least partially curing the second layer such that the first layer and the second layer together form the microfluidic structure; Wherein, the support material does not undergo a phase change during the formation of the at least one channel, and the support material remains between the first layer and the second layer.

24. The method according to claim 23, in, The support material is arranged to interact with a fluid disposed in the microfluidic structure.

25. A microfluidic structure obtainable by the method of any of the preceding claims.

26. Microfluidic structures, including channel networks, in, The channel network includes a manifold arranged to receive and / or store a fluid and a plurality of branches fluidly connected to the manifold, Wherein, the microfluidic structure is a flexible sheet.

27. The microfluidic structure according to claim 25 or 26, in, The microfluidic structure is a microfluidic chip.

28. The microfluidic structure according to any one of claims 25 to 27, in, The microfluidic structure includes two channels connected in selective fluid communication by an electronic component.

29. The microfluidic structure according to any one of claims 25 to 28, in, At least one channel is arranged to receive a fluid to increase at least one of a surface area or a volume of the microfluidic structure, and / or at least one channel is arranged to change volume to allow or prevent flow through another channel in the microfluidic structure.

30. Pad for arranging a device for skin contact, comprising at least one microfluidic structure according to any one of claims 25 to 29.