Amphiphilic polymer, preparation method and application thereof, and drug-loaded nano-micelle dispersion liquid
Drug-loaded nanomicrobes prepared through amphiphilic polymers solve the bioavailability problem of anti-VEGF drugs in the eyes, achieving efficient drug delivery and treatment of retinal neovascular lesions.
Patent Information
- Application Number
- CN202410888266.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-03
- Publication Date
- 2024-11-01
AI Technical Summary
The existing anti-VEGF drugs have poor bioavailability in the eyes and are difficult to effectively penetrate the eye barrier, resulting in poor efficacy in treating retinal neovascular lesions.
Using amphiphilic polymers as hydrophobic drug carriers, drug-loaded nano micelles are prepared through free radical polymerization. The characteristics of their hydrophilic head and hydrophobic tails are used to self-assemble micelles in aqueous solution to form micelles to wrap hydrophobic drugs. , improve the bioavailability of drugs.
It significantly improves the bioavailability and delivery efficiency of drugs, can effectively pass through the cell membrane and enter the cell interior, achieving more efficient drug release and therapeutic effects.
Smart Images

Figure CN118878754A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of drug carriers, and in particular relates to an amphiphilic polymer, a preparation method and application thereof, and a drug-loaded nano-micelle dispersion. Background Art
[0002] Retinal diseases are common ophthalmic diseases with a huge number of patients. Among retinal diseases, neovascularization is one of the main causes of vision loss. Vascular endothelial growth factor (VEGF) is an important vascular endothelial cell growth factor. When retinal diseases occur, VEGF will be produced and released in large quantities, promoting the formation of new blood vessels and enhanced leakage, further aggravating retinal lesions. Therefore, anti-VEGF strategy has become an important way to treat retinal neovascularization and choroidal neovascularization in wet macular degeneration.
[0003] Currently, the most commonly used method in clinical practice is to use anti-VEGF drugs, such as bevacizumab. However, protein monoclonal antibodies usually have poor tissue penetration and bioavailability; and the structure of the eye is complex, with a dense natural barrier system (including corneal barrier, conjunctival barrier and blood-retinal barrier), which greatly limits the penetration ability of drug molecules, especially large molecular protein drugs.
[0004] In the prior art, drug delivery is usually used to improve drug tissue penetration and bioavailability. Although traditional drug delivery methods such as intraocular injection have certain effects, frequent injections can cause discomfort to patients and may be accompanied by many complications, such as infection and retinal detachment. Eye drop technology is a non-invasive method commonly used to deliver drugs directly to the anterior structures of the eye. Its advantages are ease of use, low irritation, high patient compliance, and low risk of systemic side effects. However, due to the ocular barrier and the rapid flushing effect of tears, eye drops are difficult to effectively penetrate the ocular barrier, and there is a problem of poor bioavailability when delivering drugs to the posterior structures of the eye such as the retina and choroid. Summary of the invention
[0005] The purpose of the present invention is to provide an amphiphilic polymer and its preparation method and application, and a drug-loaded nano-micelle dispersion. The amphiphilic polymer of the present invention is used as a hydrophobic drug carrier to significantly improve the bioavailability of the drug when applied to the eye.
[0006] In order to achieve the above object, the present invention provides the following technical solutions:
[0007] An amphiphilic polymer having the following structure:
[0008] Among them, a is 1 to 160, b is 1 to 160, c is 1 to 160, d is 1 to 160, m is 1 to 18, and n is 5 to 90.
[0009] Preferably, the number average molecular weight of the amphiphilic polymer is 10,000-200,000.
[0010] The present invention also provides a method for preparing the amphiphilic polymer described in the above technical solution, comprising the following steps:
[0011] Mixing monomer 1, monomer 2, and methacrylic acid and / or dimethylaminoethyl methacrylate, and performing free radical polymerization to obtain the amphiphilic polymer;
[0012] The monomer 1 is Monomer 2 is
[0013] Preferably, the molar ratio of monomer 1 to monomer 2 is 1 to 6:1;
[0014] Preferably, the molar ratio of the monomer 2, methacrylic acid and dimethylaminoethyl methacrylate is 1:0-6:0-6.
[0015] Preferably, the temperature of the free radical polymerization reaction is 60-80° C., and the time is 24-72 hours.
[0016] The present invention also provides the use of the amphiphilic polymer described in the above technical solution or the amphiphilic polymer prepared by the preparation method described in the above technical solution in the preparation of drug-loaded nano micelles.
[0017] The present invention also provides a drug-loaded nano-micelle dispersion, comprising a solvent and drug-loaded nano-micelles dispersed in the solvent;
[0018] The drug-loaded nanomicelles include a hydrophobic drug and an amphiphilic polymer wrapped on the surface of the hydrophobic drug; the amphiphilic polymer is the amphiphilic polymer described in the above technical solution or the amphiphilic polymer prepared by the preparation method described in the above technical solution.
[0019] Preferably, the particle size of the drug-loaded nanomicelles is 5 to 50 nm.
[0020] Preferably, the hydrophobic drug includes a small molecule hydrophobic drug and / or a macromolecular hydrophobic drug; the macromolecular hydrophobic drug includes a hydrophobic protein drug;
[0021] The mass ratio of the amphiphilic polymer to the hydrophobic drug is 100:1-40.
[0022] The present invention provides an amphiphilic polymer having the structure shown above; wherein a is 1 to 160, b is 1 to 160, c is 1 to 160, d is 1 to 160, m is 1 to 18, and n is 5 to 90. The amphiphilic polymer provided by the present invention has a hydrophilic head and a hydrophobic tail, and can self-assemble to form micelles in an aqueous solution. In the drug-loaded nanomicelles prepared by the amphiphilic polymer of the present invention, hydrophobic drugs can be effectively encapsulated in the hydrophobic core of the amphiphilic polymer micelles, while the hydrophilic head shell increases the solubility and stability of the micelles in blood or body fluids; the micelles are both hydrophilic and hydrophobic, and can interact with the phospholipid molecules on the surface of the cell membrane to promote the adsorption and endocytosis of the micelles, thereby improving the bioavailability of the drug.
[0023] The method for preparing the amphiphilic polymer provided by the invention has the advantages of simple operation, low cost, mild reaction conditions and is suitable for industrial batch production.
[0024] At the same time, the drug-loaded nanomicelles in the drug-loaded nanomicelle dispersion provided by the present invention have a diameter of 5 to 50 nm. Due to their extremely small size, they can directly pass through the phospholipid bilayer of the cell membrane and enter the interior of the cell. Compared with larger nanoparticles (with a diameter exceeding 50 nm) that only rely on endocytosis to enter the cell, the process of entering the cell by the present invention does not need to rely on the energy supply of the cell. Not only can they enter the cell more effectively, but they can also release the loaded drug more effectively inside the cell, thereby improving the utilization of the drug, thereby improving the overall efficacy of the drug delivery system; and, the drug-loaded nanomicelles of the present invention have obvious surface charges, which can reduce the repulsion between them and the cell membrane, thereby significantly enhancing the delivery efficiency of the drug-loaded nanomicelles to protein drugs and improving the bioavailability of protein drugs. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0026] Figure 1 The amphiphilic polymer obtained in Example 1 1 H NMR spectrum;
[0027] Figure 2 The amphiphilic polymer obtained in Example 2 1 H NMR spectrum;
[0028] Figure 3 The amphiphilic polymer obtained in Example 3 1 H NMR spectrum;
[0029] Figure 4 This is a test chart of the average molecular weight of the amphiphilic polymers obtained in Examples 1 to 3;
[0030] Figure 5 The particle size distribution diagram of the nanomicelles prepared from the amphiphilic polymers obtained in Examples 1 to 3;
[0031] Figure 6 The surface charge test results of the nanomicelles prepared from the amphiphilic polymers obtained in Examples 1 to 3 are shown in FIG.
[0032] Figure 7 This is a graph showing the toxicity test results of the drug-loaded nanomicelles obtained in Example 4 on ARPE cells;
[0033] Figure 8 The figure is the result of the toxicity test of the drug-loaded nanomicelles obtained in Example 4 on HCEC cells;
[0034] Fig. 9 This is a graph showing the toxicity test results of the drug-loaded nanomicelles obtained in Example 4 on HUVEC cells;
[0035] Fig.10 This is a graph showing the experimental results of the permeability of drug-loaded nanomicelles obtained in Example 4 in the in vitro corneal tissue;
[0036] Fig.11 This is a graph showing the results of the anti-cell growth experiment of the drug-loaded nanomicelles obtained in Example 4;
[0037] Fig.12 This is a graph showing the results of the anti-cell migration experiment of the drug-loaded nanomicelles obtained in Example 4;
[0038] Fig.13 This is a diagram showing the treatment results of the oxygen-induced mouse retinal neovascularization model using the drug-loaded nanomicelles obtained in Example 4;
[0039] Fig.14 This is a graph showing the biocompatibility test results of the drug-loaded nanomicelles obtained in Example 4. DETAILED DESCRIPTION
[0040] The present invention provides an amphiphilic polymer having the following structure:
[0041] Among them, a is 1 to 160, b is 1 to 160, c is 1 to 160, d is 1 to 160, m is 1 to 18, and n is 5 to 90.
[0042] In the present invention, a is 1 to 160, preferably 10 to 100; b is 1 to 160, preferably 5 to 50; c is 1 to 160, preferably 5 to 50; d is 1 to 160, preferably 5 to 50; m is 1 to 18, preferably 3 to 8; and n is 5 to 90, preferably 10 to 45.
[0043] In the present invention, the number average molecular weight of the amphiphilic polymer is preferably 10,000 to 200,000, more preferably 20,000 to 50,000.
[0044] The present invention also provides a method for preparing the amphiphilic polymer described in the above technical solution, comprising the following steps:
[0045] Mixing monomer 1, monomer 2, and methacrylic acid and / or dimethylaminoethyl methacrylate, and performing free radical polymerization to obtain the amphiphilic polymer;
[0046] The monomer 1 is Monomer 2 is
[0047] In the present invention, unless otherwise specified, all preparation raw materials are preferably commercially available products well known to those skilled in the art or prepared by preparation methods well known to those skilled in the art.
[0048] In the present invention, the monomer 1 is preferably an alkyl methacrylate monomer; the monomer 2 is preferably polyethylene glycol monomethyl ether methacrylate; the number average molecular weight (Mn) of the polyethylene glycol monomethyl ether methacrylate is preferably 450 to 4000 g / mol, more preferably 950 to 2000 g / mol; the molar ratio of the monomer 1 to the monomer 2 is preferably 1 to 6:1, more preferably 2 to 3:1.
[0049] In the present invention, the molar ratio of the monomer 2, methacrylic acid and dimethylaminoethyl methacrylate is preferably 1:0-6:0-6, more preferably 1:2-4:2-4, and the amounts of methacrylic acid and dimethylaminoethyl methacrylate are not 0 at the same time.
[0050] In the present invention, the raw materials for the free radical polymerization reaction preferably further include an initiator; the initiator is preferably an azo initiator, a photoinitiator or an ammonium persulfate initiator, more preferably an azo initiator; the azo initiator is preferably azobisisobutyronitrile; the molar amount of the initiator is preferably 3 to 10% of the total molar amount of the raw materials for the free radical polymerization reaction, more preferably 4 to 8%.
[0051] In the present invention, the temperature of the free radical polymerization reaction is preferably 60-80°C, more preferably 65-75°C; the time is preferably 24-72h, more preferably 48-60h; the free radical polymerization reaction is preferably carried out in an organic solvent; the organic solvent is preferably tetrahydrofuran (THF) or N,N-dimethylformamide (DMF), more preferably tetrahydrofuran; the present invention has no special limitation on the amount of the organic solvent.
[0052] In the present invention, the free radical polymerization reaction is preferably carried out under a protective atmosphere; the protective atmosphere is preferably argon or nitrogen, more preferably argon.
[0053] In the present invention, the free radical polymerization product is preferably subjected to post-treatment; the post-treatment preferably includes solvent removal and purification; the method of removing the organic solvent is preferably rotary evaporation; the method of purification is preferably gel column chromatography separation; the mobile phase of the column chromatography separation is preferably methanol or a methane-dichloromethane mixture; the volume ratio of methanol to dichloromethane is preferably 1-4:0-1, more preferably 1:1.
[0054] The amphiphilic polymer provided by the present invention has a hydrophilic head and a hydrophobic tail, and can self-assemble to form micelles in an aqueous solution. The drug-loaded nano-micelles prepared by the amphiphilic polymer of the present invention can effectively encapsulate the hydrophobic drug in the hydrophobic core of the amphiphilic polymer micelle, while the hydrophilic head shell increases the solubility and stability of the micelle in blood or body fluids; the micelle has both hydrophilicity and hydrophobicity, and can interact with the phospholipid molecules on the surface of the cell membrane to promote the adsorption and endocytosis of the micelle, thereby improving the bioavailability of the drug.
[0055] The present invention also provides the use of the amphiphilic polymer described in the above technical solution or the amphiphilic polymer prepared by the preparation method described in the above technical solution in the preparation of drug-loaded nano micelles.
[0056] In the present invention, the drug-loaded nanomicelles are preferably drugs for treating retinal diseases; and the drugs for treating retinal diseases are preferably drugs for inhibiting fundus neovascularization.
[0057] The present invention also provides a drug-loaded nano-micelle dispersion, comprising a solvent and drug-loaded nano-micelles dispersed in the solvent;
[0058] The drug-loaded nanomicelles include a hydrophobic drug and an amphiphilic polymer wrapped on the surface of the hydrophobic drug; the amphiphilic polymer is the amphiphilic polymer described in the above technical solution or the amphiphilic polymer prepared by the preparation method described in the above technical solution.
[0059] In the present invention, the hydrophobic drug preferably includes a small molecule hydrophobic drug and / or a macromolecular hydrophobic drug; the macromolecular hydrophobic drug preferably includes a hydrophobic protein drug; the hydrophobic drug protein includes bevacizumab, aflibercept or ranibizumab, preferably bevacizumab or ranibizumab; the bevacizumab is preferably a commercially available bevacizumab injection, named Avastin; the concentration of the bevacizumab injection is preferably 25 to 50 mg / mL.
[0060] In the present invention, the particle size of the drug-loaded nanomicelles is preferably 5 to 50 nm, more preferably 10 to 30 nm.
[0061] In the present invention, the mass ratio of the amphiphilic polymer to the hydrophobic drug is preferably 100:1-40, more preferably 100:10-20.
[0062] In the present invention, the solvent is preferably water or PBS solution; the mass ratio of the hydrophobic drug to the solvent is preferably 10 to 200:1, more preferably 20 to 100:1.
[0063] In the present invention, the method for preparing the drug-loaded nanomicelle dispersion comprises the following steps:
[0064] The modified amphiphilic polymer, the hydrophobic drug and the solvent are mixed to obtain the drug-loaded nano-micelle dispersion.
[0065] In the present invention, the amphiphilic polymer and methanol are mixed before mixing to obtain an amphiphilic polymer alcohol solution; the amphiphilic polymer alcohol solution is dried to obtain a modified amphiphilic polymer. In the present invention, the concentration of the amphiphilic polymer in the amphiphilic polymer alcohol solution is preferably 0.5-100 mg / mL, more preferably 10-50 mg / mL; the drying is preferably distillation; the distillation is preferably reduced pressure distillation; the present invention removes methanol by distillation. The reason why the amphiphilic polymer is dried after being dissolved in methanol is that the polymer is a viscous liquid and is not easy to weigh. It can be configured into a polymer solution of standard concentration by dissolving.
[0066] In the present invention, the mixing method is preferably ultrasonic mixing; the frequency of the ultrasonic mixing is preferably 20 to 100 KHz, more preferably 30 to 50 KHz; the time is preferably 10 to 60 min, more preferably 20 to 40 min.
[0067] In the present invention, the modified amphiphilic polymer, hydrophobic drug and solvent are preferably filtered after the second mixing; the pore size of the filter head used for the filtration is preferably 200-1000 nm, more preferably 220-250 nm. The function of the filtration is to filter out dust, water-insoluble drug precipitation, etc. in the solution or air.
[0068] In the present invention, the drug-loaded nanomicelles of the present invention are extremely small in size and can directly pass through the phospholipid bilayer of the cell membrane and enter the interior of the cell. Compared with larger nanoparticles (with a diameter exceeding 50 nm) that enter the cell through endocytosis, the process of entering the cell by the present invention does not need to rely on the energy supply of the cell. It can not only enter the cell more effectively, but also release the loaded drug more effectively inside the cell, thereby improving the utilization of the drug, thereby improving the overall efficacy of the drug delivery system; and, the drug-loaded nanomicelles of the present invention have obvious surface charge, which can weaken the repulsion between the drug-loaded nanomicelles and the cell membrane, thereby significantly enhancing the delivery efficiency of the drug-loaded nanomicelles to protein drugs and improving the bioavailability of protein drugs.
[0069] To further illustrate the present invention, the amphiphilic polymer and its preparation method and application, and drug-loaded nanomicelle dispersion provided by the present invention are described in detail below in conjunction with the accompanying drawings and examples, but they should not be construed as limiting the scope of protection of the present invention.
[0070] The examples provided by the present invention synthesize the amphiphilic polymer according to the following synthesis route, wherein P1 is the product obtained in Example 1, P2 is the product obtained in Example 2, and P3 is the product obtained in Example 3.
[0071]
[0072] Example 1
[0073] Decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate (Mn is 950 g / mol) and methacrylic acid are dissolved in THF at a molar ratio of 2:1:2, and AIBN with a total molar amount of 8% of decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate and methacrylic acid monomer is added, and free radical polymerization is carried out under argon gas and 75°C oil bath conditions for 48 hours. After THF is removed by reduced pressure distillation, the resulting product is purified by gel column chromatography (the volume ratio of methanol and dichloromethane is 1:1) to obtain an amphiphilic polymer, which is recorded as P1. Figure 1 Example 1 amphiphilic polymer 1 H NMR spectrum.
[0074] Example 2
[0075] Decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate (Mn is 950 g / mol) and dimethylaminoethyl methacrylate are dissolved in THF at a molar ratio of 2:1:2, and AIBN with a total molar amount of 8% of decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate and methacrylic acid monomer is added, and free radical polymerization is carried out under argon gas and 75°C oil bath conditions for 48 hours. After THF is removed by reduced pressure distillation, the resulting product is purified by gel column chromatography (the volume ratio of methanol and dichloromethane is 1:1) to obtain an amphiphilic polymer, which is recorded as P2. Figure 2 Example 2 amphiphilic polymer 1 HNMR spectrum.
[0076] Example 3
[0077] Decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate (Mn is 950 g / mol), methacrylic acid and dimethylaminoethyl methacrylate are dissolved in THF at a molar ratio of 2:1:2:2, and AIBN with a total molar amount of 8% of decyl methacrylate monomer, polyethylene glycol monomethyl ether methacrylate and methacrylic acid monomer is added, and free radical polymerization is carried out under argon gas and 75° C. oil bath conditions for 48 hours, and THF is removed by reduced pressure distillation. After THF is removed by reduced pressure distillation, the resulting product is purified by gel column chromatography (the volume ratio of methanol and dichloromethane is 1:1) to obtain an amphiphilic polymer, which is recorded as P3. Figure 3 Example 3 amphiphilic polymer 1 HNMR spectrum.
[0078] Figure 4 The average molecular weight test diagram of the amphiphilic polymers of Examples 1 to 3 is shown in FIG. Figure 4 It can be seen that the molecular weights of P1, P2 and P3 are 2.27 kDa, 2.58 kDa and 3.24 kDa, respectively.
[0079] Example 4
[0080] The amphiphilic polymers prepared in Examples 1 to 3 were mixed with methanol to obtain an amphiphilic polymer methanol solution with a concentration of 50 mg / mL; 0.6 mL of the above amphiphilic polymer methanol solution was measured respectively, and the methanol was removed by reduced pressure distillation, and then 0.4 mL of a bevacizumab solution with a concentration of 25 mg / mL and 0.6 mL of water were added, and the mixture was ultrasonically cleaned at a frequency of 40 kHz for 30 min in an ultrasonic cleaning machine, and filtered using a 220 nm filter head to obtain drug-loaded nanomicelle dispersions, which were respectively recorded as PB1, PB2 and PB3.
[0081] Test Example 1
[0082] Nanomicelle particle size test: 1 mL of the amphiphilic polymer prepared in Example 4 was used to prepare the nanomicelle sample (room temperature to 25° C.), and after standing for about 1 hour, the particle size of the micelle was measured at room temperature using a nanoparticle size analyzer.
[0083] Figure 5 The particle size distribution diagram of the drug-loaded amphiphilic polymer nanomicelles obtained in Example 4. Figure 5 The results show that the particle size of micelles is about 10nm, and particles of this size have a strong ability to penetrate the cell membrane.
[0084] Nanomicelle surface charge test: 1 mL of the amphiphilic polymer prepared in Examples 1 to 3 was used to prepare the nanomicelle sample (room temperature to 25° C.), and after standing for about 1 hour, the surface charge of the micelle was measured at room temperature using a nanoparticle size analyzer.
[0085] Figure 6 The surface charge test results of the nanomicelles prepared from the amphiphilic polymers of Examples 1 to 3 are shown in FIG. Figure 6 It can be seen that the three micelles have very obvious differences in surface charges, all of which can weaken the repulsion with the cell membrane, thereby significantly enhancing the drug delivery efficiency of the drug-loaded nanomicelles. Among them, the drug delivery capacity of positively charged and zwitterionicly charged micelles is slightly higher than that of negatively charged micelles.
[0086] Test Example 2
[0087] Cytotoxicity test: Cell Counting Kit-8 (CCK-8) was used to detect the cytotoxicity of the amphiphilic polymers prepared in Examples 1 to 3 on retinal pigment epithelial cell line (ARPE), human corneal endothelial cell line (HCEC) and human umbilical vein endothelial cell line (HUVEC).
[0088] The above cell lines are all commonly used in ophthalmic experiments. The cell culture conditions are: DMEM medium + 15% FBS + 1% streptomycin-penicillin, and the cells are cultured at 1×10 4 The cells were inoculated at a density of 100 μL / well in a 96-well culture plate and incubated for 48 hours for cell attachment and recovery. Different concentrations of P1, P2 and P3 material dilutions (0.25-50 mg / mL) were prepared using fresh culture medium. After 24 hours of culture, the plate was taken out and 100 μL of the prepared material dilutions were added to each well. After continuing to be placed in the incubator for 24 hours, the old culture medium was aspirated with a pipette, and 100 μL of the basic culture medium containing 10% CCK-8 was added to each well. After the plate was placed in a cell culture incubator and incubated for 2 hours in the dark, the absorbance value at 450 nm was detected by an ELISA instrument, and the survival rate of cells at different concentrations was calculated by comparison with the control group.
[0089] Figures 7 to 9The figure shows the cytotoxicity test results of the drug-loaded nanomicelles obtained in Example 4 on ARPE cells, HCEC cells and HUVEC cells. Figures 7 to 9 It can be seen that the amphiphilic polymers of Examples 1 to 3 have a survival rate of about 100% below a concentration of 25 mg / mL, indicating that the amphiphilic polymers obtained in Examples 1 to 3 have very low cytotoxicity and are a material with relatively good safety.
[0090] Test Example 3
[0091] Corneal permeability test: After an overdose of sodium pentobarbital was injected into healthy adult New Zealand white rabbits through the ear vein, the rabbits were killed and fresh cornea / conjunctiva-sclera-choroid tissues were dissected. These tissues were placed between the donor and receiver chambers of the Franz diffusion cell. After confirming that the diffusion cell had no leakage, 0.1 mL of bevacizumab and the drug-loaded nanomicelle dispersion described in Example 4 (the final concentration of bevacizumab was 10 mg / mL) were added to the donor chamber, and 5 mL of PBS solution was added to the receiver chamber. Subsequently, the Franz diffusion cell was placed on a constant temperature stirrer at 36.8°C, and 0.2 mL of liquid in the receiver chamber was collected at 0h, 1h, 2h, 3h, 4h, 5h and 6h, and the same volume of PBS solution was added. The bevacizumab concentration in the collected fluid was determined by a UV spectrophotometer, and the cumulative total permeation was calculated according to the following formula:
[0092] Total cumulative penetration = R n ×V1+(R n-1 +R n-2 +R n-3 ……+R1)×V2;
[0093] Where V1 is the volume of the receiver chamber (5 mL), V2 is the volume of the liquid collected each time (0.2 mL), R1 is the concentration value of the receiving solution collected for the first time, and R n is the concentration value of the receiving solution collected for the nth time, R n-1 is the concentration value of the receiving solution collected for the (n-1)th time.
[0094] Fig.10 The figure is the experimental result of corneal tissue permeability of drug-loaded nano-micelles obtained in Example 4. Fig.10 It can be seen that Beva itself is difficult to penetrate the cornea. With the assistance of P1, P2, and P3, the permeability of Beva is significantly increased, that is, the drug-loaded nanomicelles obtained in Example 4 have better permeability than pure bevacizumab, among which PB2 and PB3 show better permeability on the cornea than PB1.
[0095] Test Example 4
[0096] Anti-cell migration performance test: HUVEC cells were plated at 5×10 5 The cells were seeded in a 12-well plate at a density of 100 cells. The cells were cultured in an incubator for about 48 hours until they were fully fused. After the cells were fused, a sterile 100 μL pipette tip was used to scratch the cell monolayer in each well, and the initial width of the scratch was recorded by an inverted microscope. The cells were divided into the following groups: blank control group, Beva group, experimental group (PB1 group, PB2 group and PB3 group), and each group was added with substances diluted in serum-free medium. The final concentration of Beva in the Beva group was 50 μg / mL, while the P group was a blank micelle group without a carrier, with a concentration of 150 μg / mL. The cells were then cultured for an additional 24 hours. Afterwards, the final width of the scratch was recorded by an upright microscope, and the captured images were analyzed and the scratch width was calculated using ImageJ. The cell mobility of each group was calculated using the following formula:
[0097] Cell mobility (%) = (final scratch width / initial scratch width) × 100%;
[0098] Figures 11-12 The results of the anti-cell growth and anti-cell migration experiments of the drug-loaded nanomicelles obtained in Example 4 are shown in FIG. Figures 11-12 It can be seen that Beva, PB1, PB2, and PB3 all have inhibitory effects on cell migration and growth. At the same concentration of bevacizumab, PB1, PB2, and PB3 all show better anti-cell migration ability than bevacizumab alone; among them, the anti-cell migration ability of PB2 and PB3 is more advantageous than that of PB1. This proves that the drug-loaded nanomicelles of the present invention have no effect on the functionality of bevacizumab, and they can enter cells, which can further enhance the drug effect of bevacizumab.
[0099] Test Example 5
[0100] Testing of treatment conditions for retinal diseases in mice: Establishment of an oxygen-induced mouse retinal neovascularization model: Newborn mice were housed with lactating mothers in standard animal facilities under normoxic conditions until P7. At P7, to induce retinal neovascularization, mice were assigned to two environmental conditions: one group was placed in a hyperbaric oxygen chamber containing 70% oxygen for hyperoxia treatment, and the other group was maintained in normoxic conditions at ambient oxygen levels. After five days of exposure, both groups of animals were returned to normoxic conditions from P12 onwards to induce retinal ischemia and subsequent pathological neovascularization.
[0101] Treatment of diseased mice: The mice were divided into the following treatment groups: NS group, Beva group, intravitreal bevacizumab (IVT) group and experimental group (including PB1 group, PB2 group and PB3 group). The IVT group received a single intravitreal injection of bevacizumab (0.5 μL, 10 mg / mL) at P12, while the other groups received 5 μL of eye drops twice a day. The final concentration of bevacizumab in both the bevacizumab group and the experimental group was 10 mg / mL, and the concentration of the amphiphilic polymer in the experimental group was 30 mg / mL. At P17, the mice were euthanized by cervical dislocation after air anesthesia, and the eyeballs were removed and fixed in 4% formaldehyde for 1 h. The retinal tissue was then gently separated and cut into a four-leaf clover shape. The tissue was washed three times in PBS and transferred to a 96-well plate. Then, GS-IB4 working solution (0.5% Isolectin-GS B4, Invitrogen I21413; 0.5% Triton-X100; 1mM CaCl2) was added and incubated overnight on a shaker in the dark at 4°C. After washing, the retinal tissue was transferred to a slide with the inner limiting membrane facing up, and the tissue was allowed to dry naturally, and anti-fading agent was added for preservation. Images were captured using a confocal laser scanning microscope and processed using Adobe Photoshop software. The avascular area, neovascular area, and the entire retinal tissue were manually outlined, and the corresponding pixel values were recorded for analysis.
[0102] Fig.13 The figure is a diagram showing the therapeutic results of the oxygen-induced mouse retinal neovascularization model using the drug-loaded nanomicelles obtained in Example 4. Fig.13 It can be seen that the IVT group, PB1 group, PB2 group and PB3 group all had different degrees of retinal recovery compared with the modeling group and bevacizumab group; among them, the treatment conditions of PB2 and PB3 were better than those of the PB1 group, and even comparable to the gold standard IVT group for clinical treatment, which indicates that PB2 and PB3 are very efficient in delivering bevacizumab from the ocular surface to the retina.
[0103] Test Example 6
[0104] Biocompatibility test: Healthy C57 mice were divided into NS group and experimental group (including PB1 group, PB2 group and PB3 group, the final concentration of bevacizumab was 10mg / mL, and the concentration of amphiphilic polymer was 30mg / mL). Mice were instilled with 10μL eye drops in each eye twice a day for one week, and the ocular surface integrity and potential irritation were monitored using a slit lamp biomicroscope, which can examine the anterior structure of the eye in detail. In addition, fluorescein sodium staining was used to detect any damage to the corneal epithelium, after which the mice were killed by cervical dislocation after isoflurane anesthesia, and the eyeballs of mice in each group were collected and fixed overnight in FAS eyeball fixative (prepared with 40% formaldehyde / glacial acetic acid / 80% ethanol at a volume ratio of 10:10:80). Subsequently, the fixed eyeballs were embedded in paraffin and cut into 5-micron thick sections, which were then stained with hematoxylin-eosin (HE). After staining, the sections were dehydrated and washed with gradient alcohol and xylene, and then covered with mounting solution to preserve tissue sections and staining. Finally, the sections were observed under a bright field microscope by a scanner.
[0105] Fig.14 The figure is the result of the biocompatibility test of the drug-loaded nanomicelles obtained in Example 4. Fig.14 The results showed that the mice in the experimental groups (PB1, PB2 and PB3) had no signs of corneal opacity, neovascularization or defects, and the anterior chamber depth was comparable to that of the PBS control group. Histological examination of the retina by HE staining further confirmed the safety of these amphiphilic polymers. In addition, the morphology of the retina (including the hierarchical structure of the retina and its structural organization) did not change, and there were no signs of tissue damage or inflammation, confirming the non-toxicity of these amphiphilic polymers when applied topically.
[0106] Although the above embodiment describes the present invention in detail, it is only a part of the embodiments of the present invention, not all of the embodiments. Other embodiments can be obtained based on this embodiment without creativity, and these embodiments all fall within the protection scope of the present invention.
Claims
1. An amphiphilic polymer, characterized in that It has the following structure: Among them, a is 1 to 160, b is 1 to 160, c is 1 to 160, d is 1 to 160, m is 1 to 18, and n is 5 to 90.
2. The amphiphilic polymer according to claim 1, characterized in that The number average molecular weight of the amphiphilic polymer is 10,000 to 200,000.
3. The method for preparing the amphiphilic polymer according to claim 1 or 2, characterized in that: The following steps are involved: Mixing monomer 1, monomer 2, and methacrylic acid and / or dimethylaminoethyl methacrylate, and performing free radical polymerization to obtain the amphiphilic polymer; The monomer 1 is Monomer 2 is 4. The preparation method according to claim 3, characterized in that: The molar ratio of the monomer 1 to the monomer 2 is 1 to 6:
1.
5. The preparation method according to claim 3, characterized in that: The molar ratio of the monomer 2, methacrylic acid and dimethylaminoethyl methacrylate is 1:0-6:0-6.
6. The preparation method according to any one of claims 3 to 5, characterized in that: The temperature of the free radical polymerization reaction is 60-80° C. and the time is 24-72 hours.
7. Use of the amphiphilic polymer according to claim 1 or 2 or the amphiphilic polymer prepared by the preparation method according to any one of claims 3 to 7 in the preparation of drug-loaded nanomicelles.
8. A drug-loaded nanomicelle dispersion, characterized in that: It includes a solvent and drug-loaded nano-micelles dispersed in the solvent; The drug-loaded nanomicelles include a hydrophobic drug and an amphiphilic polymer wrapped on the surface of the hydrophobic drug; the amphiphilic polymer is the amphiphilic polymer described in claim 1 or 2 or the amphiphilic polymer prepared by the preparation method described in any one of claims 3 to 7.
9. The drug-loaded nanomicelle dispersion according to claim 8, characterized in that: The particle size of the drug-loaded nano micelles is 5 to 50 nm.
10. The drug-loaded nanomicelle dispersion according to claim 8, characterized in that: The hydrophobic drugs include small molecule hydrophobic drugs and / or macromolecular hydrophobic drugs; the macromolecular hydrophobic drugs include hydrophobic protein drugs; The mass ratio of the amphiphilic polymer to the hydrophobic drug is 100:1-40.