Economical high-standard bearing steel for rolling body and production process of economical high-standard bearing steel

By optimizing the production process of high-standard bearing steel for rolling elements, using converter smelting, LF refining, RH vacuum treatment and continuous casting, combined with electromagnetic stirring technology, the production process consumes time, high energy consumption and carbonization in the existing technology is solved. The problem of widening of the strip shape has achieved efficient and low-cost steel production and excellent segregation quality.

CN118880180APending Publication Date: 2024-11-01NANJING IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411248154.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The production process of existing high-standard bearing steel for rolling elements consumes a long time, has high energy consumption, high cost, and carbide belt widening, making it difficult to meet customer needs.

Method used

The production processes of converter smelting, LF refining, RH vacuum treatment, continuous casting, primary heating, billet rolling, secondary heating, controlled rolling and cold-controlled, and hot-rolled strips are used to control chemical composition and process parameters, such as converter steel output The end point C content, LF white slag time, RH high vacuum degree, continuous casting cooling rate, heating temperature section, combined with the crystallizer electromagnetic stirring technology, optimize the billet forming and rolling process.

Benefits of technology

It shortens the high-temperature diffusion time, reduces cost and energy consumption, improves the yield rate and market competitiveness, better control of carbide belts, and improves segregation quality.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses economical high-standard bearing steel for a rolling body and a production process of the economical high-standard bearing steel, and relates to the technical field of steel production, and the economical high-standard bearing steel comprises the following chemical components in percentage by mass: 0.90-1.05% of C, 0.15-0.45% of Si, 0.20-0.50% of Mn, less than or equal to 0.020% of P, less than or equal to 0.006% of S, 1.35-1.60% of Cr, less than or equal to 0.040% of Al, less than or equal to 0.025% of Ti, less than or equal to 15 ppm of O, less than or equal to 80 ppm of N and the balance of Fe and inevitable impurities. A converter bloom 320 * 420 continuous casting machine is adopted, the section is moderate, and rolled wires also have a large compression ratio. The crystallizer is small in liquid level fluctuation and good in inclusion; and through the advanced technology of crystallizer electromagnetic stirring, tail end electromagnetic stirring, tail end soft reduction and tail end heavy reduction, the segregation quality is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steel production, and in particular to a high-standard bearing steel for economical rolling elements and a production process thereof. Background Art

[0002] The rolling element uses high-standard bearing steel to smelt high-quality alloy with high purity. The electric furnace large square billet continuous casting machine has small crystallizer liquid level fluctuation and good inclusion control; the continuous casting crystallizer has electromagnetic stirring + end electromagnetic stirring + end light pressure, and the segregation quality is good. The large bar billet compression ratio is large, the rolled wire strip meets the requirements of level 2 or below, and the liquid separation is level 0; due to good segregation, the mesh is also easy to control, meeting the requirements of level 2.5 and below 2.0.

[0003] At present, the high-standard bearing steel for rolling elements is all produced by the cross-section of large square billets in electric furnaces, and finally rolled into finished wire rods by high-speed wire after long-term high-temperature diffusion of large bars. The entire production process is time-consuming, energy-intensive, and requires a large proportion of grinding resources, resulting in high costs. In addition, after high-temperature diffusion, the carbide bands also widen, and customers often report that the carbide bands are too wide. Summary of the invention

[0004] The technical problem to be solved by the present invention is to overcome the shortcomings of the prior art and provide an economical high-standard bearing steel for rolling elements and a production process thereof.

[0005] In order to solve the above technical problems, the technical solution of the present invention is as follows: An economical high-standard bearing steel for rolling elements, whose chemical composition and mass percentage are as follows: C: 0.90-1.05%, Si: 0.15-0.45%, Mn: 0.20-0.50%, P≤0.020%, S≤0.006%, Cr: 1.35-1.60%, Al≤0.040%, Ti≤0.025%, O≤15ppm, N≤80ppm, and the balance is Fe and unavoidable impurities.

[0006] The present invention also provides a production process of economical high-standard bearing steel for rolling elements, which comprises in sequence: converter smelting, LF refining, RH vacuum treatment, continuous casting, primary heating, blank rolling, secondary heating, controlled rolling and controlled cooling, and hot-rolled wire rod.

[0007] As a preferred solution of the production process of economical high-standard bearing steel for rolling elements described in the present invention, in the converter smelting process, the C content at the steel tapping end point is controlled to be greater than or equal to 0.10%, the target P content is less than or equal to 0.018%, and the target temperature is greater than or equal to 1620°C.

[0008] As a preferred solution of the production process of the economical high-standard bearing steel for rolling elements of the present invention, in the LF refining process, the white slag time is controlled to be ≥20 min, and the smelting time is controlled to be ≥40 min.

[0009] As a preferred solution of the production process of economical high-standard bearing steel for rolling elements described in the present invention, in the RH vacuum treatment process, the RH high vacuum degree is controlled to be ≤2.5 mbar, the holding time is ≥20 min, and the soft blowing time is ≥15 min.

[0010] As a preferred solution for the production process of high-standard bearing steel for economical rolling elements described in the present invention, wherein: in the continuous casting process, constant pulling speed casting is adopted, and cooling is in the form of water cooling, including primary cooling and secondary cooling. The rate of the primary cold water cooling is 170t / h, and the rate of the secondary cold water cooling is 0.15L / kg. The current of the electromagnetic stirring of the crystallizer is 250A, and the frequency is 2Hz. The current of the end electromagnetic stirring is 700 A, and the frequency is 8Hz.

[0011] As a preferred solution of the production process of economical high-standard bearing steel for rolling elements described in the present invention, in the primary heating process, the preheating stage temperature is less than 900°C, the heating stage temperature is 1000-1300°C, the heating stage temperature is 1200-1260°C, and the soaking stage temperature is 1200-1260°C.

[0012] As a preferred solution of the production process of economical high-standard bearing steel for rolling elements of the present invention, in the secondary heating process, the temperature of the first heating stage is 800-1000°C, the temperature of the second heating stage is 1000-1100°C, and the temperature of the soaking stage is 1000-1080°C.

[0013] The beneficial effects of the present invention are: (1) The present invention adopts a converter bloom 320*420 continuous casting machine with a moderate cross section and a large compression ratio for the rolled wire. The crystallizer liquid level fluctuates little and the inclusions are good; the crystallizer electromagnetic stirring + end electromagnetic stirring + end light pressure + end heavy pressure advanced technology has better segregation quality.

[0014] (2) The blank of the present invention has moderate shape and good segregation, and does not require a long high temperature time. The high temperature diffusion time of the large bar blanking is more than 2 hours. There is less oxidation and decarburization during the blanking process, and the yield rate is high.

[0015] (3) The present invention fully peels the blank, with a peeling depth of ≥0.5 mm. After being rolled into wire rod, ferrite decarburization is hardly observed on the surface. DETAILED DESCRIPTION

[0016] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific implementation methods.

[0017] The embodiment of the present application provides an economical high-standard bearing steel for rolling elements, whose chemical composition and mass percentage are as follows: C: 0.90-1.05%, Si: 0.15-0.45%, Mn: 0.20-0.50%, P≤0.020%, S≤0.006%, Cr: 1.35-1.60%, Al≤0.040%, Ti≤0.025%, O≤15ppm, N≤80ppm, and the remainder is Fe and unavoidable impurities.

[0018] The present application also provides a production process of economical high-standard bearing steel for rolling elements, which includes: converter smelting, LF refining, RH vacuum treatment, continuous casting, primary heating, blank rolling, secondary heating, controlled rolling and controlled cooling, and hot-rolled wire rod. The details are as follows: Converter steelmaking process: Control the C content at the end of steel tapping to be greater than or equal to 0.10% to prevent overoxidation of molten steel and facilitate the removal of inclusions. The target P content is less than or equal to 0.018%, and the target temperature is greater than or equal to 1620℃. Control the appropriate steel tapping temperature to effectively control the return of molten steel to P. At the same time, alloying is carried out according to 200kg-400kg of lime / furnace and 100-200kg of aluminum blocks / furnace.

[0019] LF refining process: control the white slag time to be greater than or equal to 20 minutes, and the smelting time to be greater than or equal to 40 minutes. The oxygen content in the molten steel can be fully removed by sufficient white slag time, and the white slag and smelting time can be controlled. Through the appropriate smelting cycle, the alloy composition can be accurately controlled and the inclusions can be fully floated and removed. Auxiliary material dosage: Silicon carbide 100-140kg / furnace, used for deoxidation.

[0020] RH vacuum treatment process: control RH high vacuum degree ≤ 2.5 mbar, high vacuum holding time ≥ 20 min, soft blowing time ≥ 15 min. It is beneficial to remove H in molten steel and promote the full floating of inclusions.

[0021] Continuous casting process: constant pulling speed casting is adopted. Cooling is divided into primary cooling and secondary cooling, both of which are water-cooled. The rate of primary cold water cooling is 170t / h. The proportion of columnar crystals is increased by rapid cooling of primary cold water, which improves the density of the billet. The rate of secondary cold water cooling is 0.15L / kg. The current of electromagnetic stirring of the crystallizer is 250A, the frequency is 2Hz, and the current of electromagnetic stirring at the end is 700A, the frequency is 8Hz. The electromagnetic stirring technology is beneficial to the shrinkage of molten steel and improves the center defects of continuous casting billets.

[0022] Primary heating process: The heating temperature and heating time of the steel billet are as follows: the temperature of the preheating section is less than 900℃, and the preheating of the billet reduces the risk of billet cracking. The temperature of the first heating section is 1000-1300℃, the temperature of the second heating section is 1200-1260℃, and the temperature of the soaking section is 1200-1260℃. Through two-stage heating and one-stage soaking, the temperature inside and outside the round billet is uniform.

[0023] Secondary heating process: The heating temperature and heating time for steel wire rolling are as follows: the temperature of the first heating stage is 800-1000℃, the temperature of the second heating stage is 1000-1100℃, and the temperature of the soaking stage is 1000-1080℃.

[0024] Therefore, the technical solution of this application develops a process path of 320×420 section of converter → rapid billeting (high temperature period ≥ 2h) → high-speed wire rolling, which reduces costs, saves energy and reduces emissions, and improves the delivery efficiency and market competitiveness of Nangang products. The high-standard bearing steel of converter reduces the cost by 283 yuan / ton compared with the high-standard bearing steel of electric furnace. Cost reduction of high-speed wire rolling: The actual yield rate of high-standard bearing steel is 94.04%, which is about 1.25% higher than the 92.78% of high-standard bearing steel of electric furnace two-fire, and the actual cost reduction is about 30 yuan / ton.

[0025] In addition to the above embodiments, the present invention may also have other implementation modes; any technical solutions formed by equivalent replacement or equivalent transformation shall fall within the protection scope required by the present invention.

Claims

1. An economical high-standard bearing steel for rolling elements, characterized by: Its chemical composition and mass percentage are as follows: C: 0.90-1.05%, Si: 0.15-0.45%, Mn: 0.20-0.50%, P≤0.020%, S≤0.006%, Cr: 1.35-1.60%, Al≤0.040%, Ti≤0.025%, O≤15ppm, N≤80ppm, and the balance is Fe and unavoidable impurities.

2. A production process of high-standard bearing steel for economical rolling elements according to claim 1, characterized in that: Including: Converter smelting, LF refining, RH vacuum treatment, continuous casting, primary heating, billet rolling, secondary heating, controlled rolling and cooling, hot rolled wire rod.

3. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the converter smelting process, the C content at the steel tapping end point is controlled to be greater than or equal to 0.10%, the target P content is less than or equal to 0.018%, and the target temperature is greater than or equal to 1620°C.

4. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the LF refining process, the white slag time is controlled to be ≥20 min and the smelting time is controlled to be ≥40 min.

5. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the RH vacuum treatment process, the RH high vacuum degree is controlled to be ≤2.5 mbar, the holding time is ≥20 min, and the soft blowing time is ≥15 min.

6. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the continuous casting process, constant pulling speed casting is adopted, and cooling is in the form of water cooling, including primary cooling and secondary cooling. The rate of the primary cold water cooling is 170t / h, the rate of the secondary cold water cooling is 0.15L / kg, the current of the electromagnetic stirring of the crystallizer is 250A, the frequency is 2Hz, and the current of the terminal electromagnetic stirring is 700A, the frequency is 8Hz.

7. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the primary heating process, the temperature of the preheating section is less than 900°C, the temperature of the first heating section is 1000-1300°C, the temperature of the second heating section is 1200-1260°C, and the temperature of the soaking section is 1200-1260°C.

8. The production process of economical high-standard bearing steel for rolling elements according to claim 2 is characterized in that: In the secondary heating process, the temperature of the first heating stage is 800-1000°C, the temperature of the second heating stage is 1000-1100°C, and the temperature of the soaking stage is 1000-1080°C.