Simulation technical method based on structural characteristics of catalyst layer in electrolyzed water transmission process
Through molecular dynamics simulation method, the microscopic physical model of the anode catalytic layer of the proton exchange membrane electrolytic cell was constructed, and the water molecule transport process and channel formation was studied, which solved the problem of lack of research on structural changes in the permeation and transport process of water molecules in the existing technology, and achieved the The optimized design of electrolytic cell performance reduces experimental costs and time.
Patent Information
- Application Number
- CN202410918718.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-10
- Publication Date
- 2024-11-01
Smart Images

Figure CN118888018A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of electrochemical electrolytic cells, and specifically relates to the simulation of material distribution in a water transmission process and a microscopic physical model of the transmission process in a proton exchange membrane electrolytic cell. Background Art
[0002] The anode catalyst layer of the proton exchange membrane electrolyzer, where the anode oxygen evolution reaction is located, is a key component of the proton exchange membrane electrolyzer. It usually contains electrolyte ions, catalysts and catalyst carriers, providing a place for electrochemical reactions. Water molecules penetrate into the anode catalyst layer, and then the water molecules are decomposed into oxygen and hydrogen ions. The transport rate of reactants in the reaction process is extremely important for its reaction rate, including the transport of electrons, hydrogen ions, water molecules and oxygen molecules. It is precisely because of the resistance of these transport substances that the anode oxygen evolution reaction is slow.
[0003] During the transport of anode reaction substances, water molecules penetrate into the catalyst surface to participate in the chemical reaction. The penetration of water molecules is a crucial process. The formation mechanism of the transport channel of water molecules is very critical to the study of its transport resistance. At present, there is still a lack of research directly targeting the structural changes in microscopic phenomena. A full understanding of the changes in its own structure is more helpful to analyze the causes of its microscopic transport process and its transport resistance. Molecular dynamics simulation can help explore the structure and transport characteristics at the nanoscale, guide the structural design of the electrolytic cell, and thus significantly reduce experimental costs and shorten the R&D cycle.
[0004] At present, there is no method for using molecular dynamics modeling to study the structure of the catalyst layer during the water molecule transport process in the proton exchange membrane electrolyzer. To this end, the present invention provides a molecular dynamics simulation method for exploring the structural changes of the catalyst layer during the reaction process in the anode catalyst layer of the proton exchange membrane electrolyzer, during which water molecules penetrate into the catalyst layer and then reach a stable process for chemical reaction, as well as the formation mechanism of the water molecule channel. The introduction of this method will rapidly promote the technological progress of the proton exchange membrane electrolyzer. Summary of the invention
[0005] The purpose of the present invention is to propose a simulation technology method based on the structural characteristics of the catalytic layer during the electrolytic water transmission process, so as to reveal in detail the local mass transfer process and the process of water molecule channel formation during the water molecule transmission process in the catalytic layer of the electrolytic cell.
[0006] The simulation technology method based on the structural characteristics of the catalytic layer during the electrolytic water transmission process includes: the construction of the catalyst layer model, the construction of the electrolyte film covering the catalyst model, the construction of the water molecule transmission process model, and the acquisition and analysis of material distribution and transmission data. The simulation calculation model uses the LAMMPS software platform to perform all molecular dynamics simulations. The constructed models are all microscopic physical models, which include three parts. The specific modeling steps are as follows:
[0007] (1) Construction of catalyst layer model
[0008] Based on information such as catalyst unit cell parameters, atomic size, atomic mass, etc., molecular dynamics simulation technology was used to construct a catalyst layer model with a length, width and height of 8nm and 6 layers of catalyst atoms in a simulation frame with a length and width of 8nm and a height of 1nm.
[0009] (2) Construction of electrolyte film-covered catalyst model
[0010] First, a preliminary model of the catalyst layer after inserting the electrolyte was constructed, and then a balancing treatment was performed, and finally an electrolyte film-covered catalyst equilibrium microstructure model was obtained. Perfluorosulfonic acid polymer was used as the electrolyte material, and the electrolyte components in the electrolyte film-covered catalyst model included: perfluorosulfonic acid polymer molecules (PFSA), hydronium ions, and water molecules.
[0011] (2.1) The electrolyte in the catalyst layer includes PFSA chains, water molecules, and hydronium ions, so they need to be modeled first. Commercial DuPont proton exchange membrane product materials are used as PFSA models, classic F3C water molecule models, and classic hydronium ion models. The MOLTEMPLATE software platform is used to establish the molecular models of each electrolyte.
[0012] (2.2) Based on the catalyst layer model, PFSA chains, water molecules and hydronium ion electrolyte molecules are inserted above the catalyst layer to construct a preliminary model of the catalyst layer after the electrolyte is inserted. The number of PFSA chains, water molecules and hydronium ion electrolyte molecules is required to conform to the actual situation of the research process.
[0013] (2.3) Perform equilibrium treatment to obtain the equilibrium microstructure model of the electrolyte film covering the catalyst. The equilibrium treatment process is to first perform an energy minimization treatment, then a compression process, and then perform an energy minimization treatment again, followed by an initial deviation elimination treatment, high and low temperature treatment, and a relaxation process, and finally obtain the equilibrium structure.
[0014] (2.4) The energy minimization process is carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process is to set a Lennard-Jones potential wall on the top of the microscopic physical model to interact with each electrolyte component to achieve precise compression control of the catalyst layer. The high and low temperature treatment is a relaxation change process that cycles back and forth between 353.15 Kelvin and 1000 Kelvin for at least four times, with the end temperature being 353.15 Kelvin.
[0015] (3) Construction of water molecule transport process model
[0016] A layer of water molecules at least 3 nm high is placed in the top area of the electrolyte film covering the catalyst equilibrium microstructure model established in step (2), and a Leonard-Jones interaction potential wall that only acts on water molecules is set above all water molecules to allow water molecules to penetrate into the catalytic layer to study the water molecule penetration and transport process.
[0017] (3.1) Insert a number of water molecules that match the water density into a space of 3 nm high that meets the size of the simulation frame. Then perform a balancing treatment to obtain a water molecule layer. Place the water molecule layer into the top area of the electrolyte film covering the catalyst equilibrium microstructure model established above.
[0018] (3.2) Molecular dynamics simulation of the energy minimization, compression, and relaxation processes of the electrolyte film-covered catalyst equilibrium microstructure model is performed to ensure that the entire model structure tends to an equilibrium state.
[0019] (3.3) In all subsequent molecular dynamics simulations, the interactions between catalyst atoms were subjected to static constraints and excluded from the internal force field calculations, so that the relative positions of the catalysts remained unchanged during the simulation, in order to more accurately simulate other dynamic processes.
[0020] (3.4) The energy minimization process is carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process is to set a Lennard-Jones potential wall on the top of the microscopic physical model to interact with each electrolyte component to achieve precise compression control of the catalyst layer.
[0021] (3.5) During the compression process, as the top potential wall gradually moves downward along the thickness direction of the electrolyte membrane, the density of the electrolyte components and the attached water molecules is gradually adjusted to a level that matches the density of the solid electrolyte membrane and water under normal conditions. Afterwards, the potential wall at the top of the model is fixed in the compressed position and the energy minimization process is performed again.
[0022] (3.6) During the relaxation process, all components in the model except the catalyst were subjected to molecular dynamics simulation for at least 1 nanosecond at a constant temperature and constant volume of 1000 Kelvin. The strength of the Lennard-Jones interaction between atoms in the perfluorosulfonic acid polymer molecules in the electrolyte component was reduced by two orders of magnitude to eliminate possible initial errors.
[0023] (3.7) Subsequently, the strength of the Lennard-Jones interaction between the internal atoms of the PFSA chain was adjusted to the initial state, and a molecular dynamics simulation of at least 0.5 ns was performed under a constant temperature and constant volume environment to gradually return the system to the room temperature state of 353.15 Kelvin, ensuring that the entire simulation remained stable after sufficient relaxation.
[0024] (3.8) Finally, a constant temperature and constant volume simulation of at least 5 ns was performed to allow the model to reach the final equilibrium state, at which point the energy of the model and the density distribution along the thickness of the electrolyte no longer changed.
[0025] (4) Material distribution and transport data acquisition and analysis
[0026] The density distribution data of PFSA chains, hydronium ions, and water molecules in the electrolyte film will be obtained using molecular dynamics simulation while ensuring the stable transport of water molecules in the catalyst layer film. The radial distribution function and two-dimensional density cloud map analysis of the water molecule transport process model will be performed to analyze the data.
[0027] The present invention focuses on the microscopic scale and explores the electrolyte structure mass transfer characteristics and water channel formation characteristics of the water transport process under different membrane thicknesses and different catalysts, laying an important foundation for further optimizing the performance of the electrolytic cell.
[0028] The characteristics and benefits of the present invention are:
[0029] (1) A high-precision microscopic physical model of the catalytic layer of the water molecule transport process is constructed through molecular dynamics simulation. This model studies the electrolyte structure mass transfer characteristics and water channel formation characteristics of the water molecule transport process by constructing models of different catalysts and different film thicknesses. This makes it possible to study the influence of water molecule transport efficiency under different conditions, and thus provides a basis for optimizing the catalytic layer design.
[0030] (2) The simulation method can not only provide guidance for experiments and reduce the blindness of experiments, but also adjust the experimental design based on the simulation results, thereby saving R&D costs and time. Moreover, the method is also applicable to mass transfer research under different catalysts and different electrolytes, which helps to further guide the optimization design of catalytic layer materials and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1(a) Construction diagram of the catalyst layer model.
[0032] Figure 1(b) Construction diagram of the electrolyte film covering the catalyst model.
[0033] Fig. 1(c) Construction diagram of the water molecule transport process model before water molecules penetrate.
[0034] Fig. 1(d) Construction diagram of the water molecule transport process model after water molecules penetrate.
[0035] Figure 2 Model of water molecule transport process for thicker film groups showing iridium catalyst.
[0036] Figure 3 A model showing the water molecule transport process for a thicker film set of iridium oxide catalysts.
[0037] Figure 4 It is a conceptual diagram of the model of the water molecule transport process - a water channel display.
[0038] FIG. 5( a ) is a graph showing the density distribution of perfluorosulfonic acid in an electrolyte film-covered catalyst model of an iridium catalyst.
[0039] FIG5( b ) is a graph showing the water density distribution of the electrolyte film-covered catalyst model of the iridium catalyst.
[0040] FIG5( c ) is a graph showing the full electrolyte density distribution of the electrolyte film-covered catalyst model of the iridium catalyst.
[0041] Figure 6 (a) and (b) are two-dimensional density distribution diagrams of thin films in the electrolyte film covering catalyst model of iridium catalyst.
[0042] Figure 6(c) and (d) are two-dimensional density distribution diagrams of medium-thickness films in the electrolyte thin film covering catalyst model of iridium catalyst.
[0043] Figure 6(e) and (f) are two-dimensional density distribution diagrams of thicker films in the electrolyte thin film covering catalyst model of iridium catalyst.
[0044] FIG. 7( a ) is a graph showing the density distribution of perfluorosulfonic acid in an electrolyte film-covered catalyst model of an iridium oxide catalyst.
[0045] FIG. 7( b ) is a graph showing the water density distribution of the electrolyte film-covered catalyst model of iridium oxide catalyst.
[0046] FIG. 7( c ) is a graph showing the full electrolyte density distribution of the electrolyte film-covered catalyst model of the iridium oxide catalyst.
[0047] Figure 8 (a) and (b) are two-dimensional density distribution diagrams of thin films in the electrolyte film covering catalyst model of iridium oxide catalyst.
[0048] Figure 8(c) and (d) are two-dimensional density distribution diagrams of medium-thickness films in the electrolyte thin film covered catalyst model of iridium oxide catalyst.
[0049] Figure 8(e) and (f) are two-dimensional density distribution diagrams of thicker films in the electrolyte thin film covered catalyst model of iridium oxide catalyst.
[0050] 9(a) and (b) are two-dimensional density distribution diagrams of the initial state of the thicker film group in the water molecule transport process model of the iridium catalyst.
[0051] Figure 9 (c) and (d) are two-dimensional density distribution diagrams of the final state of the thicker film group in the water molecule transport process model of the iridium catalyst.
[0052] 10(a) and (b) are two-dimensional density distribution diagrams of the initial state of the thicker film group in the water molecule transport process model of iridium oxide catalyst.
[0053] Figure 10 (c) and (d) are two-dimensional density distribution diagrams of the final state of the thicker film group in the water molecule transport process model of iridium oxide catalyst.
[0054] Attached Figure 4 As the abstract drawings of the present invention, it should be noted that: in the embodiments, Figures 6, 8, 9 and 10 express the two-dimensional image density distribution of the simulation results. These four figures are all color images. If converted to black and white images, it is impossible to clearly express the two-dimensional image density (difference) distribution characteristics in each case. DETAILED DESCRIPTION
[0055] The specific modeling method of the present invention is further described below with reference to the accompanying drawings and examples. It should be noted that this example is a narrative description for the purpose of clearly explaining the simulation steps, and does not limit the protection scope of the method of the present invention.
[0056] Based on the simulation technology method of the structural characteristics of the catalytic layer during the electrolysis of water, the constructed models are all microscopic physical models. Figure 1 clearly shows the flow of the modeling process of the present invention. The specific modeling steps are as follows:
[0057] (1) Construction of catalyst layer model
[0058] Through the information of catalyst unit cell parameters, atomic size, atomic mass, etc., molecular dynamics simulation technology is used to construct a catalyst layer model with a length and width of 8nm and a height of 6 layers of catalyst atoms in a simulation frame with a length and width of 8nm and a height of 1nm. This implementation method uses two catalysts: iridium and iridium oxide. This implementation method uses two catalysts, one is a pure iridium model, which consists of 6 layers of Ir (111) planes composed of iridium atoms. The other is a more common iridium oxide catalyst, which is composed of a rutile structure lattice, in which there are six-coordinated iridium and three-coordinated oxygen, and a structure of three layers of iridium atoms and three layers of oxygen atoms is established.
[0059] (2) Construction of electrolyte film-covered catalyst model
[0060] First, a preliminary model of the catalyst layer after inserting the electrolyte was constructed, and then a balancing treatment was performed, and finally an electrolyte film-covered catalyst equilibrium microstructure model was obtained. Perfluorosulfonic acid polymer was used as the electrolyte material, and the electrolyte components in the electrolyte film-covered catalyst model included: perfluorosulfonic acid polymer molecules (PFSA), hydronium ions, and water molecules.
[0061] (2.1) The electrolyte in the catalyst layer includes PFSA chains, water molecules, and hydronium ions, so they need to be modeled first. The commercial DuPont proton exchange membrane product material was used as the PFSA model (composed of 10 repeating monomers and 16CF, with groups and side chains in its chemical structure), the classic F3C water molecule model, and the classic hydronium ion model. The MOLTEMPLATE software platform was used to establish the molecular models of each electrolyte.
[0062] (2.2) Based on the catalyst layer model, PFSA chains, water molecules and hydronium ions are inserted above the catalyst layer to construct a preliminary model of the catalyst layer after the electrolyte is inserted. The number of each electrolyte molecule is required to meet the actual situation of the research process. Three experimental groups are used in this implementation method: a relatively thin film (6 perfluorosulfonic acid polymer molecules, 60 hydronium ions and 500 water molecules), a medium thickness membrane (10 perfluorosulfonic acid polymer molecules, 100 hydronium ions and 900 water molecules) and a relatively thick membrane (14 perfluorosulfonic acid polymer molecules, 140 hydronium ions and 1300 water molecules).
[0063] (2.3) Perform equilibrium treatment to obtain the equilibrium microstructure model of the electrolyte film covering the catalyst. The equilibrium treatment process is to first perform an energy minimization process, then a compression process, and then perform an energy minimization process again, followed by an initial deviation elimination process, a high and low temperature treatment, and a 2 nanosecond relaxation process, and finally obtain the equilibrium structure.
[0064] (2.4) The energy minimization process was carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process was to set a Lennard-Jones potential wall on the top of the model to interact with each electrolyte component to achieve precise compression control of the catalyst layer. The high and low temperature treatment was a relaxation change process with at least four cycles between 353.15 Kelvin and 1000 Kelvin, with the end temperature being 353.15 Kelvin.
[0065] (3) Construction of water molecule transport process model
[0066] A layer of water molecules at least 3 nm high is placed in the top area of the electrolyte film-covered catalyst equilibrium microstructure model established in step (2), and a Leonard-Jones interaction potential wall that only acts on water molecules is set above all water molecules to allow water molecules to penetrate into the catalyst layer to study the water molecule penetration and transport process, and the following is obtained: Figure 2 and Figure 3 Model, Figure 4 A conceptual diagram of the water channel during the osmotic transport process of water molecules is given.
[0067] (3.1) Insert 6400 water molecules that meet the water density into the space that meets the frame size of 8nm×8nm×3nm. Then perform equilibrium treatment to obtain a water molecule layer. Place the water molecule layer into the top area of the electrolyte film covering the catalyst equilibrium microstructure model established above.
[0068] (3.2) Molecular dynamics simulations of the energy minimization, compression, and relaxation processes were performed on the above model to ensure that the structure of the entire model tends to an equilibrium state.
[0069] (3.3) In all subsequent molecular dynamics simulations, the interactions between catalyst atoms were subjected to static constraints and excluded from the internal force field calculations, so that the relative positions of the catalysts remained unchanged during the simulation, in order to more accurately simulate other dynamic processes.
[0070] (3.4) The energy minimization process is carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process is to set a Lennard-Jones potential wall on the top of the microscopic physical model to interact with each electrolyte component to achieve precise compression control of the catalyst layer.
[0071] (3.5) During the compression process, as the top potential wall gradually moves downward along the thickness direction of the electrolyte membrane, the density of the electrolyte components and the attached water molecules is gradually adjusted to a level that matches the density of the physical electrolyte membrane and water under normal conditions. Afterwards, the potential wall at the top of the microscopic physical model is fixed in the compressed position and the energy minimization process is performed again.
[0072] (3.6) During the relaxation process, all components in the model except the catalyst are subjected to molecular dynamics simulation for at least 1 nanosecond at a constant temperature and constant volume environment of 1000 Kelvin, in which the Lennard-Jones interaction strength between atoms within the perfluorosulfonic acid polymer molecules in the electrolyte component is reduced by two orders of magnitude to eliminate possible initial errors.
[0073] (3.7) Subsequently, the strength of the Lennard-Jones interaction between the internal atoms of the PFSA chain was adjusted to the initial state, and a molecular dynamics simulation of at least 0.5 ns was performed under a constant temperature and constant volume environment to gradually return the system to the room temperature state of 353.15 Kelvin, ensuring that the entire simulation remained stable after sufficient relaxation.
[0074] (3.8) Finally, a constant temperature and constant volume simulation of at least 5 ns was performed to allow the model to reach the final equilibrium state, at which point the energy of the model and the density distribution along the thickness of the electrolyte no longer changed.
[0075] (4) Material distribution and transport data acquisition and analysis
[0076] For the catalyst surface film structure model, this implementation method performs radial distribution function and two-dimensional density cloud map analysis: the final 2 nanosecond relaxation process of the electrolyte film covering the catalyst model and the final 5 nanosecond constant temperature and constant volume simulation process of the water molecule transport process model. For the final 5 nanosecond constant temperature and constant volume simulation process of the water molecule transport process model, the average data of 0-0.2 nanoseconds is counted as the instantaneous initial 0.1 nanosecond density distribution and the average data of 4.8-5.0 nanoseconds is counted as the instantaneous final 4.9 nanosecond density distribution. The density distribution function calculation formula is as follows,
[0077]
[0078] Among them, ρ ab (r) means the number density of the particles in the calculation group in the spherical layer at a distance r from the reference particle. The denominator N b / V is the average number density of particles in the calculation group.
[0079] The density distribution data of PFSA chains, hydronium ions, and water molecules in the electrolyte film will be obtained using molecular dynamics simulation while ensuring the stable transport of water molecules in the catalyst layer film.
[0080] Figures 5 and 6 show the density distribution of the electrolyte film covering the catalyst model of the iridium catalyst. Figures 7 and 8 show the density distribution of the electrolyte film covering the catalyst model of the iridium oxide catalyst. According to the comparative analysis of the results of the iridium catalyst and the iridium oxide catalyst, it can be seen that the electrolyte film on the catalyst surface presents a multilayer structure.
[0081] When the electrolyte layer is thin, the film structure is mainly divided into two layers, namely the catalyst-PFSA contact interface region (region I) and the PFSA-pore transition interface region (region III). It can be seen from Figures 6 and 8 that region I is a very dense ultra-thin layer with tightly arranged PFSA chains, while region III is a thin layer with loosely arranged PFSA chains. As the film becomes thicker, it changes from a two-layer structure to a three-layer structure. In addition to region I and region III, there is also a water-PFSA stable region (region II) with uniform material distribution between the two.
[0082] It can be seen from FIG. 5 and FIG. 7 that as the electrolyte film becomes thicker, the structure and thickness of regions I and III change slightly, while region II gradually becomes thicker.
[0083] Figures 9 and 10 show the two-dimensional density distribution maps of the thicker group in the water molecule transport process model for iridium and iridium oxide catalysts, respectively.
[0084] According to the analysis and comparison of the two, it can be seen that the water channels are mainly formed in regions II and III, and there are two water channel modes. In the model of the iridium catalyst surface film after water infiltration in Figure 9, there is only a water channel mode in which water molecules penetrate downward with the help of weak connections between dispersed water clusters. In the model of the iridium oxide catalyst surface film after water infiltration in Figure 10, there is an additional water channel mode that is directly connected to the top water layer, and the second water channel mode is more advantageous in the process of water molecule penetration and transmission.
[0085] Throughout the simulation, the interaction between the Lennard-Jones interaction potential wall and atoms is as follows:
[0086]
[0087] In the formula, E wall is the potential energy of the potential wall and the atom, ε wall is the potential well depth, σ wall is the collision distance, r wall is the distance between the potential wall and the atom, r c is the cutoff distance for interaction, set to 1.5 nm. The potential energy between all atoms in the model is calculated as follows:
[0088]
[0089] In the formula, U is the potential energy between all atoms, and K on the right is b (b i -b0) 2 is used to calculate the bond stretch, K θ (θ i -θ0)2 It is used to calculate the bond angle bending, K d [1+dcos(nφ)] is used to calculate the dihedral torsion, is used to calculate the van der Waals potential, It is used to calculate the long-range electrostatic potential. The interaction between two different types of atoms is obtained according to the Lennard-Jones mixing rule:
[0090]
[0091] Where ε is the potential well depth, σ is the collision distance, subscripts ii and jj represent the van der Waals interactions with atoms of the same type, and subscripts ij represent the van der Waals interactions with atoms of different types. The potential energy parameters between atoms are shown in Table 1. The particle-particle-particle-mesh method was selected as the long-range electrostatic calculation method, and the specified tolerance of the error was set to 0.0001. The Nose-Hoover constant temperature method was used to control the system temperature, the relaxation time was 0.1 picoseconds, and the time step of the simulation process was set to 1 femtosecond.
[0092] Table 1 Correlation potential parameters of molecular dynamics simulation
[0093]
[0094]
[0095] The method of the present invention can not only effectively guide the experimental process and significantly reduce the blindness and uncertainty of the experiment, but also make fine adjustments to the experimental design based on the simulation results, which helps to significantly save costs and time in the research and development process. In addition, the scope of application of this method is not limited to the catalysts, electrolytes, etc. used in the catalytic layer of the electrolytic cell. It is also applicable to mass transfer research of other types of catalysts, electrolytes, and other catalytic layers, thereby providing important theoretical support and guidance for the optimization design of the entire process. Its unique methodology and wide applicability have opened up new paths for its research and development and application, showing that this method has very broad application prospects in the field of electrochemical science.
Claims
1. A simulation technology method based on the structural characteristics of the catalytic layer during the electrolytic water transmission process, characterized in that: The construction of the catalyst layer model, the construction of the electrolyte film covering the catalyst model, the construction of the water molecule transport process model, and the acquisition and analysis of material distribution and transport data. The simulation calculation model uses the LAMMPS software platform to perform all molecular dynamics simulations. The constructed models are all microscopic physical models, which include three parts. The specific modeling steps are as follows: (1) Construction of catalyst layer model Based on the information of catalyst unit cell parameters, atomic size, atomic mass, etc., molecular dynamics simulation technology was used to construct a catalyst layer model with a length and width of 8nm and a height of 6 layers of catalyst atoms in a simulation frame with a length and width of 8nm and a height of 1nm. (2) Construction of electrolyte film-covered catalyst model Firstly, a preliminary model of the catalyst layer after inserting the electrolyte is constructed, and then a balancing treatment is performed, and finally a balanced microstructure model of the electrolyte film-covered catalyst is obtained. Perfluorosulfonic acid polymer is used as the electrolyte material. The electrolyte components in the electrolyte film-covered catalyst model include: perfluorosulfonic acid polymer molecules, hydronium ions and water molecules. (2.1) The electrolyte in the catalyst layer includes perfluorosulfonic acid polymer molecular chains, water molecules, and hydronium ions. Therefore, it is necessary to first model the perfluorosulfonic acid polymer molecular chains, water molecules, and hydronium ions. The commercial DuPont proton exchange membrane product material is used as the perfluorosulfonic acid polymer molecular model, the classic F3C water molecule model, and the classic hydronium ion model. The MOLTEMPLATE software platform is used to establish the molecular models of each electrolyte. (2.2) Based on the catalyst layer model, perfluorosulfonic acid polymer molecular chains, water molecules and hydronium ion electrolyte molecules are inserted above the catalyst layer to construct a preliminary model of the catalyst layer after the electrolyte is inserted. The number of perfluorosulfonic acid polymer molecular chains, water molecules and hydronium ion electrolyte molecules is required to conform to the actual situation of the calculation and analysis process. (2.3) Perform equilibrium treatment to obtain the equilibrium microstructure model of the electrolyte film covering the catalyst. The equilibrium treatment process is to first perform an energy minimization treatment, then a compression process, and then perform an energy minimization treatment again, followed by an initial deviation elimination treatment, high and low temperature treatment and a relaxation process, and finally obtain the equilibrium structure. (2.4) The energy minimization process is carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process is to set a Lennard-Jones potential wall on the top of the microscopic physical model to interact with each electrolyte component to achieve precise compression control of the catalyst layer. The high and low temperature treatment is a relaxation change process between 353.15 Kelvin and 1000 Kelvin for at least four cycles, and the end temperature is 353.15 Kelvin. (3) Construction of water molecule transport process model A layer of water molecules at least 3 nm high is placed in the top area of the electrolyte film covering the catalyst equilibrium microstructure model established in step (2), and a Leonard-Jones interaction potential wall that only acts on water molecules is set above all water molecules to allow water molecules to penetrate into the catalyst layer to study the water molecule penetration and transport process. (3.1) Insert a number of water molecules that match the water density into a space of 3 nm high that meets the size of the simulation frame, and then obtain a water molecule layer after balancing. Place the water molecule layer into the top area of the electrolyte film covering the catalyst equilibrium microstructure model established above. (3.2) Perform molecular dynamics simulations of the energy minimization, compression, and relaxation processes of the electrolyte film-covered catalyst equilibrium microstructure model to ensure that the entire model structure tends to an equilibrium state. (3.3) In all subsequent molecular dynamics simulations, the interactions between catalyst atoms were statically constrained and excluded from the internal force field calculations, so that the relative positions of the catalysts remained unchanged during the simulation, in order to more accurately simulate other dynamic processes. (3.4) The energy minimization process is carried out at a constant temperature and constant volume of 1000 Kelvin. The compression process is carried out by setting a Lennard-Jones potential wall on the top of the model to interact with each electrolyte component to achieve precise compression control of the catalyst layer. (3.5) During the compression process, as the top potential wall gradually moves downward along the thickness direction of the electrolyte membrane, the density of the electrolyte components and the attached water molecules is gradually adjusted to a level that matches the density of the solid electrolyte membrane and water under normal conditions. Afterwards, the potential wall at the top of the model is fixed in the compressed position and the energy minimization process is performed again. (3.6) During the relaxation process, all components in the model except the catalyst were subjected to molecular dynamics simulation for at least 1 nanosecond at a constant temperature and constant volume of 1000 Kelvin. The strength of the Lennard-Jones interaction between atoms in the perfluorosulfonic acid polymer molecules in the electrolyte component was reduced by two orders of magnitude to eliminate possible initial errors. (3.7) Then, the intensity of the Lennard-Jones interaction between the internal atoms of the perfluorosulfonic acid polymer molecular chain was adjusted to the initial state, and a molecular dynamics simulation was performed for at least 0.5 nanoseconds under a constant temperature and constant volume environment to gradually return the system to a room temperature of 353.15 Kelvin to ensure that the entire simulation remained stable after sufficient relaxation. (3.8) Finally, a constant temperature and constant volume simulation of at least 5 nanoseconds was performed to allow the model to reach the final equilibrium state, at which point the energy of the model and the density distribution along the thickness of the electrolyte no longer changed; (4) Material distribution and transport data acquisition and analysis The density distribution data of perfluorosulfonic acid polymer molecular chains, hydronium ions and water molecules in the electrolyte film will be obtained using molecular dynamics simulation while ensuring the stable transmission of water molecules in the catalyst layer film. The radial distribution function and two-dimensional density cloud map analysis of the water molecule transmission process model will be carried out for data analysis.