Circuit board dry film hole sealing method

By optimizing the matching relationship between the board thickness, PTH hole/slot size and dry film thickness of the circuit board, the problems of long production cycle, high cost and poor resolution of the circuit board dry film sealing method in the prior art are solved, and the problem of high production cycle, high cost and poor resolution of the circuit board dry film sealing method in the prior art is improved, The hole sealing ability avoids the problem of line biting and copper-free holes, and improves the electromagnetic shielding effect of the circuit board.

CN118890787APending Publication Date: 2024-11-01JIANG XI XU SHENG DIAN ZI GU FEN YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411155506.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing circuit board dry film sealing methods have problems such as long production cycle, high cost, uneven copper thickness and poor line resolution, which leads to difficulty in installing the electromagnetic interference shield, which is prone to the problem of line biting and copper-free holes.

Method used

By optimizing the matching relationship between the board thickness, PTH hole/slot size, line distance and dry film thickness of the circuit board, 1.5mil or 2mil dry film sealing is used. The specific matching rules include different apertures, line distances, slot lengths and For combination of widths, select the appropriate dry film thickness to improve the sealing capacity.

Benefits of technology

The circuit board dry film sealing ability is improved, and the line biting and copper-free hole problems caused by dry film rupture are avoided, and the line production quality and sealing are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118890787A_ABST
    Figure CN118890787A_ABST
Patent Text Reader

Abstract

The invention discloses a circuit board dry film hole sealing method, which comprises the following steps of: when the aperture d of a PTH hole is less than or equal to 5mm, sealing the hole by adopting a 1.5 mil dry film; when the hole diameter d of the PTH hole is more than 5mm and less than or equal to 6mm and the minimum line distance is more than or equal to 0.075 mm, sealing the hole by adopting a 2mil dry film; when the hole diameter d of the PTH hole is more than 5mm and less than or equal to 6mm and the minimum line distance is less than 0.075 mm, sealing the hole by adopting a 1.5 mil dry film; when the length L of the PTH slot is greater than 5mm and the width D of the PTH slot is greater than 2mm, sealing the hole by adopting a 2mil dry film; and when the length L of the PTH slot is less than or equal to 5mm, sealing the hole by using a 1.5 mil dry film. According to the circuit board dry film hole sealing method provided by the invention, the circuit board dry film hole sealing capability is improved by optimizing the matching relationship among different board thicknesses, the sizes of the PTH holes / the PTH slot holes, the circuit line spacing and the dry film thickness, the problem of dry film breakage during hole sealing is avoided, and the problem of resolution during circuit manufacturing can also be ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of circuit board manufacturing, and in particular to a circuit board dry film sealing method. Background Art

[0002] With the development of the communications industry, the integration of communications equipment is getting higher and higher, such as RRU (radio remote unit), one of the main devices in distributed base stations. There are many kinds of electromagnetic interference between the functional modules of RRU. In order to prevent the interference electromagnetic field from spreading outward and prevent the functional modules from being affected by the external electromagnetic field, the most effective way is to use an electromagnetic shielding cover to surround the interfered module. The installation of the electromagnetic shielding cover requires good grounding effect, good welding sealing and reliability, so it is necessary to open many PTH holes / PTH slots on the PCB to fix the shielding cover.

[0003] In the PCB production process, the conventional method of sealing holes is to use the positive film process, using electroplated tin to protect the copper on the wall of the PTH hole, but the positive film process has problems such as long process, high production cost, uneven electroplated copper thickness and easy film sandwiching; another method is to use the negative film process, using dry film to directly protect the PTH hole and circuit, and the area not covered by the dry film will be etched away. The negative film process can reduce the production cycle and reduce production costs. When sealing with dry film, the selection of dry film will affect the sealing ability of the dry film and the circuit resolution, which is prone to circuit biting and copper-free holes caused by the cracking of the dry film in the etching tank, and poor circuit exposure caused by poor resolution during circuit production.

[0004] In view of this, it is necessary to provide a dry film sealing process to solve the above technical problems. Summary of the invention

[0005] The technical problem to be solved by the present invention is to provide a circuit board dry film sealing method, which improves the circuit board dry film sealing ability by optimizing the matching relationship between different board thicknesses, PTH hole / PTH slot hole sizes, line spacing and dry film thickness.

[0006] The technical solution of the present invention is as follows:

[0007] A circuit board dry film sealing method, comprising:

[0008] When the aperture d of the PTH hole satisfies d≤5mm, a 1.5mil dry film is used to seal the hole;

[0009] When the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing ≥0.075mm, use 2mil dry film to seal the hole; when the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing <0.075mm, use 1.5mil dry film to seal the hole;

[0010] When the length L of the PTH slot is greater than 5mm and the width D is greater than 2mm, a 2mil dry film is used to seal the hole; when the length L of the PTH slot is less than or equal to 5mm, a 1.5mil dry film is used to seal the hole.

[0011] Furthermore, in the PTH slot, 5 mm < L < 8.5 mm.

[0012] Furthermore, in the PTH slot, 2mm<D<5mm.

[0013] Furthermore, when the board thickness is ≤0.4mm, the maximum hole diameter of the PTH hole sealed by the dry film is 2.5mm, and 1.5mil dry film is used for sealing;

[0014] When 0.4mm<board thickness≤0.8mm, the maximum hole diameter of the PTH hole sealed by the dry film is 3.5mm, and 1.5mil dry film is used for sealing;

[0015] When 0.8mm<board thickness≤1.0mm, the maximum hole diameter of the PTH hole sealed by the dry film is 5mm, and 1.5mil dry film is used for sealing;

[0016] When the board thickness is greater than 1.0mm, the aperture diameter of the PTH hole d≤5mm, and 1.5mil dry film is used to seal the hole; when the aperture diameter of the PTH hole d>5mm, 2mil dry film is used to seal the hole.

[0017] Furthermore, when the board thickness is ≤0.6mm, the L of the PTH slot is ≤3mm, D<4.0mm, or 3mm<L≤4mm, D≤3.5mm, 1.5mil dry film is used for sealing;

[0018] When 0.6mm<board thickness≤1.0mm, L≤7mm, D≤5.0mm, or L≤7.5mm, D≤4.5mm, or L<8mm, D≤3.5mm of PTH slot, use 2mil dry film to seal the hole;

[0019] When the board thickness is greater than 1.0mm, and the PTH slot hole has L≤6mm, D≤5.0mm, or L≤8mm, D≤4mm, or L<8.5mm, D≤3mm, use 2mil dry film to seal the hole.

[0020] Compared with the prior art, the circuit board dry film sealing method provided by the present invention has the following beneficial effects:

[0021] The circuit board dry film sealing method provided by the present invention improves the circuit board dry film sealing ability by optimizing the matching relationship between different board thicknesses, PTH hole / PTH slot hole sizes, line spacing and dry film thickness, thereby avoiding the problem of line biting and copper-free holes caused by dry film cracking in the etching tank, and poor line exposure caused by poor resolution during circuit production. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0023] Figure 1 It is a schematic diagram of a PTH slot in the circuit board dry film sealing method of the present invention. DETAILED DESCRIPTION

[0024] In order to enable those skilled in the art to better understand the technical solutions in the embodiments of the present invention and to make the above-mentioned objects, features and advantages of the present invention more obvious and understandable, the specific implementation modes of the present invention are further described below.

[0025] It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in each embodiment of the present invention described below can be combined with each other as long as there is no conflict between them.

[0026] A circuit board dry film sealing method, comprising:

[0027] When the aperture d of the PTH hole satisfies d≤5mm, a 1.5mil dry film is used to seal the hole;

[0028] When the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing ≥0.075mm, use 2mil dry film to seal the hole; when the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing <0.075mm, use 1.5mil dry film to seal the hole;

[0029] When the length L of the PTH slot is greater than 5mm and the width D is greater than 2mm, a 2mil dry film is used to seal the hole. The length L and width D of the PTH slot are expressed as follows: Figure 1 shown.

[0030] Specific:

[0031] When the board thickness is ≤0.4mm, the maximum diameter of the PTH hole sealed by the dry film is 2.5mm, and 1.5mil dry film is used for sealing;

[0032] When 0.4mm<board thickness≤0.8mm, the maximum hole diameter of the PTH hole sealed by the dry film is 3.5mm, and 1.5mil dry film is used for sealing;

[0033] When 0.8mm<board thickness≤1.0mm, the maximum hole diameter of the PTH hole sealed by the dry film is 5mm, and 1.5mil dry film is used for sealing;

[0034] When the plate thickness is greater than 1.0mm, the hole diameter of the PTH hole d≤5mm, and 1.5mil dry film is used to seal the hole; when the hole diameter of the PTH hole d>5mm, 2mil dry film is used to seal the hole;

[0035] When the board thickness is ≤0.6mm, the PTH slot L≤3mm, D<4.0mm, or 3mm<L≤4mm, D≤3.5mm, use 1.5mil dry film to seal the hole;

[0036] When 0.6mm<board thickness≤1.0mm, L≤7mm, D≤5.0mm, or L≤7.5mm, D≤4.5mm, or L<8mm, D≤3.5mm of PTH slot, use 2mil dry film to seal the hole;

[0037] When the board thickness is greater than 1.0mm, and the PTH slot hole has L≤6mm, D≤5.0mm, or L≤8mm, D≤4mm, or L<8.5mm, D≤3mm, use 2mil dry film to seal the hole.

[0038] In the present invention, when the minimum line spacing is less than 0.075 mm, 1.5 mil dry film is used for sealing; when the minimum line spacing is greater than or equal to 0.075 mm, 2 mil dry film is preferably used for sealing to meet the sealing capacity.

[0039] The circuit board dry film sealing method provided by the present invention improves the circuit board dry film sealing ability by optimizing the matching relationship between different board thicknesses, PTH hole / PTH slot hole sizes, line spacing and dry film thickness, thereby avoiding the problem of line biting and copper-free holes caused by dry film cracking in the etching tank, and poor line exposure caused by poor resolution during circuit production.

[0040] The embodiments of the present invention are described in detail above, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations made to these embodiments without departing from the principles and spirit of the present invention are still within the protection scope of the present invention.

Claims

1. A circuit board dry film sealing method, characterized in that: include: When the aperture d of the PTH hole satisfies d≤5mm, a 1.5mil dry film is used to seal the hole; When the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing ≥0.075mm, use 2mil dry film to seal the hole; when the hole diameter d of the PTH hole meets 5mm<d≤6mm and the minimum line spacing <0.075mm, use 1.5mil dry film to seal the hole; When the length L of the PTH slot is greater than 5mm and the width D is greater than 2mm, a 2mil dry film is used to seal the hole; when the length L of the PTH slot is less than or equal to 5mm, a 1.5mil dry film is used to seal the hole.

2. The circuit board dry film sealing method according to claim 1, characterized in that: In the PTH slot, 5mm<L<8.5mm.

3. The circuit board dry film sealing method according to claim 2, characterized in that: In the PTH slot, 2mm<D<5mm.

4. The circuit board dry film sealing method according to claim 1, characterized in that: When the board thickness is ≤0.4mm, the maximum diameter of the PTH hole sealed by the dry film is 2.5mm, and 1.5mil dry film is used for sealing; When 0.4mm<board thickness≤0.8mm, the maximum hole diameter of the PTH hole sealed by the dry film is 3.5mm, and 1.5mil dry film is used for sealing; When 0.8mm<board thickness≤1.0mm, the maximum hole diameter of the PTH hole sealed by the dry film is 5mm, and 1.5mil dry film is used for sealing; When the board thickness is greater than 1.0mm, the aperture of the PTH hole d≤5mm, and 1.5mil dry film is used to seal the hole; when the aperture of the PTH hole d>5mm, 2mil dry film is used to seal the hole.

5. The circuit board dry film sealing method according to claim 1, characterized in that: When the board thickness is ≤0.6mm, the PTH slot L≤3mm, D<4.0mm, or 3mm<L≤4mm, D≤3.5mm, use 1.5mil dry film to seal the hole; When 0.6mm<board thickness≤1.0mm, L≤7mm, D≤5.0mm, or L≤7.5mm, D≤4.5mm, or L<8mm, D≤3.5mm of PTH slot, use 2mil dry film to seal the hole; When the board thickness is greater than 1.0mm, and the PTH slot hole has L≤6mm, D≤5.0mm, or L≤8mm, D≤4mm, or L<8.5mm, D≤3mm, use 2mil dry film to seal the hole.