Circuit board with signal lines with different impedances and manufacturing method thereof
By covering the protective film on the copper foil layer and performing copper reduction processing, a transition area is formed to achieve the difference in impedance value, which solves the problem that the prior art cannot produce signal lines with the same line width and spacing but different impedance values on the same line layer. The problem of high-quality circuit board product production has been achieved.
Patent Information
- Application Number
- CN202410925279.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-01
AI Technical Summary
The existing printed circuit board processing technology cannot produce signal lines with the same line width and spacing but different impedance values on the same circuit layer, and cannot meet the design needs of some special printed circuit board products.
By covering the copper foil layer with protective function, it is divided into a protective area and a processing area, and copper reduction work is performed in the processing area, so that the copper thickness is smaller than that of the protection area, forming a transition area to achieve impedance value The difference is followed by a different impedance signal line on the copper foil layer after copper reduction.
It has achieved the production of multiple groups of impedance signal lines with the same line width and spacing but different impedance values on the same line layer, which meets the special market needs, and is simple, reasonable, flexible in production, high yield and good quality. .
Smart Images

Figure CN118890797A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of circuit boards, and in particular to a circuit board having different impedance signal lines with the same line width and spacing but different impedance values, and a manufacturing method thereof. Background Art
[0002] With the continuous development of printed circuit board technology, especially when the frequency of the transmitted circuit signal is getting higher and higher, the printed circuit board must not only solve the problem of line conduction and insulation between networks, but also solve the impedance matching problem of the transmitted signal. For conventional printed circuit boards, when the signal frequency is greater than 10MHz, the impedance value of the signal line needs to be controlled. According to the impedance matching principle, there are many factors that affect the impedance value, such as: the line width of the transmission line, the thickness of the line copper layer, the spacing between the lines in the differential impedance line, the distance between the signal layer and the reference layer, the dielectric constant of the dielectric layer material, the thickness of the solder mask layer covering the line, the dielectric constant of the solder mask material, the distance between the signal layer and the shielding layer, and other factors. Among them, the change of each factor will cause the line impedance to change.
[0003] Theoretically, in the same circuit layer, when the line width and line spacing of the designed signal lines are the same, the impedance value of the signal lines is also the same. However, with the development of technology and product usage requirements, in the design of some special printed circuit board products, it is necessary to arrange a set array of signal lines with the same line width and spacing but different impedance values in the same circuit layer. At this time, conventional printed circuit board processing technology cannot meet the design requirements of the above special printed circuit board products.
[0004] In view of this, the present invention is proposed. Summary of the invention
[0005] In order to overcome the above-mentioned defects, the present invention provides a circuit board with signal lines with different impedances and a method for manufacturing the same. The manufacturing method is simple, reasonable, and flexible to operate, and can realize the production of multiple groups of impedance signal lines with "the same line width and spacing but different impedance values" on the same circuit layer of the circuit board product, thereby meeting the special needs of the market.
[0006] The technical solution adopted by the present invention to solve the technical problem is: a method for manufacturing a circuit board with signal lines of different impedances, comprising:
[0007] Providing a first processed board, wherein the outermost layer of the first processed board is a copper foil layer A, which is used to make a circuit pattern;
[0008] A protective film with a protective function is coated on the copper foil layer A to divide the copper foil layer A into a protection area covered by the protective film and a processing area exposed outside the protective film; in addition, an area on the protective film and within a set range outside the processing area is defined as a transition area A, and the protection strength of the transition area A gradually increases from the edge close to the processing area to the direction away from the processing area;
[0009] Performing copper reduction operation on the processing area so that the copper thickness of the processing area is less than the copper thickness of the protection area, and the processing area and the protection area are smoothly transitioned and connected; obtaining a second processed plate;
[0010] Circuit production is performed on the second processed board to produce a circuit pattern on the copper foil layer A after copper reduction; the circuit pattern includes a first impedance signal line arranged in the protection area and a second impedance signal line arranged in the processing area after copper reduction, and the impedance value of the second impedance signal line is greater than the impedance value of the first impedance signal line.
[0011] As a further improvement of the present invention, the protective film has an anti-etching function.
[0012] As a further improvement of the present invention, the first processed plate is subjected to sequential coating pre-treatment, coating with an anti-corrosion photosensitive film, exposure, and development processing to achieve coating of the protective film on the copper foil layer A; in addition, after completing the above-mentioned development processing, the protective film is also subjected to air exposure.
[0013] As a further improvement of the present invention, a positive image film is provided, on which a specific film area corresponding to the transition area A is provided, and the shading rate of the specific film area gradually decreases along the increasing direction of the protection strength of the transition area A.
[0014] As a further improvement of the present invention, the specific area of the film is polished with metallographic sandpaper so that the shading rate of the specific area of the film is gradually reduced from 100% to 5%.
[0015] As a further improvement of the present invention, the transition area A is an area within 2 mm from the edge of the processing area surrounded by the protective film and close to the processing area to the direction away from the processing area.
[0016] As a further improvement of the present invention, the copper reduction operation is performed by using an etching process, and the copper reduction amount in the processing area is 15 to 20 μm;
[0017] In addition, the area on the copper foil layer A and corresponding to the transition area A is defined as a transition area B, the copper reduction amount of the transition area B is less than the copper reduction amount of the processing area, and the transition area B forms an inclined surface after etching and copper reduction treatment.
[0018] As a further improvement of the present invention, after the copper reduction operation is completed, the protective film is removed and the plate is ground in sequence, so that the processing area and the protection area are smoothly transitioned and connected.
[0019] As a further improvement of the present invention, the first processing plate is provided with an inner layer circuit;
[0020] The second processed board is processed in sequence by drilling, copper electroplating, pre-film treatment, anti-plating photosensitive film coating, exposure, development, pattern electroplating copper layer, electroplating tin layer, film stripping, alkaline etching copper, and removing tin layer to produce the circuit pattern;
[0021] The second processed board that has completed the circuit production is subjected to conventional impedance testing, AOI inspection, solder mask, character printing, leveling, molding, cleaning, and electrical testing processes in sequence to complete the production of the subsequent circuit board finished product required.
[0022] The present invention further provides a circuit board with signal lines having different impedances, which is manufactured by using the method for manufacturing a circuit board with signal lines having different impedances described in the present invention.
[0023] The beneficial effects of the present invention are as follows: 1) Through technical innovation, the present invention can realize the production of multiple groups of impedance signal lines with "same line width and spacing but different impedance values" on the same circuit layer of the circuit board product, which well meets the special needs of the market. 2) The circuit board production method provided by the present invention is simple, reasonable, flexible in operation, easy to produce and implement, and the resulting circuit board has a high yield and good quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 A process flow chart of a method for manufacturing a circuit board having signal lines with different impedances according to the present invention;
[0025] Figure 2 It is a schematic diagram of the cross-sectional structure of the double-sided copper-clad substrate of the present invention;
[0026] Figure 3 is a schematic diagram of the cross-sectional structure of the first processed plate of the present invention;
[0027] Figure 4 The cross-sectional structure diagram of the present invention after the protective film is covered on the copper foil layer A;
[0028] Figure 5 is a schematic cross-sectional structural diagram of the second processed plate of the present invention;
[0029] Figure 6 It is a partial top view structural schematic diagram of the second processed plate of the present invention;
[0030] Figure 7 This is a schematic diagram of the cross-sectional structure of the second processing board after circuit manufacturing is completed according to the present invention.
[0031] Combined with the attached drawings, the following description is given:
[0032] 1. First processing board; 10. Copper foil layer A; 11. First insulating layer; 12. Copper foil layer B; 13. Inner layer circuit; 14. Second insulating layer; 100. Protection area; 101. Processing area; 102. Transition area B; 2. Protective film; 20. Transition area A; 3. Second processing board; 4. Build-up copper layer; 51. First impedance signal line; 52. Second impedance signal line. DETAILED DESCRIPTION
[0033] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings.
[0034] Embodiment 1:
[0035] Please see attached Figure 1 To Attachment Figure 7 As shown, this embodiment 1 provides a method for manufacturing a circuit board with signal lines of different impedances, including the following manufacturing steps:
[0036] S1: Provide a first processed board 1, wherein the outermost layer of the first processed board 1 is a copper foil layer A10, which is used to make a circuit pattern.
[0037] Specifically, in this embodiment 1, according to the design requirements of the finished circuit board, the first processed board 1 can adopt a double-sided copper clad plate structure, or can also adopt a laminate structure with inner layer circuits. The following takes the finished circuit board as a four-layer board structure, and the first processed board 1 adopts a laminate structure with two layers of inner layer circuits as an example to illustrate the circuit board manufacturing method of this application. Of course, when this application is actually used, the finished circuit board is not limited to a four-layer board structure, and the first processed board 1 is not limited to a laminate structure with two layers of inner layer circuits.
[0038] In addition, the manufacturing method of the first processed plate 1 is:
[0039] S11: Provide a double-sided copper-clad substrate, the double-sided copper-clad substrate comprising a first insulating layer 11 and two copper foil layers B12 respectively attached to opposite sides of the first insulating layer 11. Figure 2 shown.
[0040] S12: The double-sided copper-clad substrate is sequentially subjected to baking, anti-corrosion photosensitive film coating, exposure, development, etching and film stripping to achieve the production of inner layer circuits 13 on the two copper foil layers B12. Figure 3 As shown; it can be understood that the inner layer circuit 13 is integrally formed on the copper foil layer B12.
[0041] S13: After the double-sided copper-clad substrate with the inner layer circuit fabricated is subjected to AOI inspection and browning processing in sequence, a second insulating layer 14 (prepreg sheet may be used) and the copper foil layer A10 are sequentially laminated on each of the copper foil layers B12 (including the inner layer circuit 13), and then hot pressing is performed to obtain the first processed board 1, which can be referred to in the attached drawing. Figure 3 shown.
[0042] Note: The processing steps of "baking the board, coating the anti-corrosion photosensitive film, exposing, developing, etching, film stripping, AOI inspection, browning and hot pressing" described in S12 and S13 above are all common technical means in the field of circuit board processing technology, so they are not described in detail here, but only briefly described as follows:
[0043] ① Baking board: baking the double-sided copper-clad substrate to age the first insulating layer 11 and release the stress in the double-sided copper-clad substrate.
[0044] ② Coating with anti-corrosion photosensitive film: coating the anti-corrosion photosensitive dry film A on the two copper foil layers B12.
[0045] ③Exposure and development: Exposure is to expose part of the area of the resist photosensitive dry film A according to the work data of the circuit board; development is to remove the unexposed area of the resist photosensitive dry film A. Understandably, the pattern formed by the resist photosensitive dry film A obtained after development is also called a negative image in the industry.
[0046] ④ Etching and film stripping: Etching is to remove the local area of the copper foil layer B12 exposed outside the anti-corrosion photosensitive dry film A, and film stripping is to remove the anti-corrosion photosensitive dry film A using a strong alkaline solution, then the inner layer circuit 13 is obtained in a bare state.
[0047] ⑤AOI inspection: the inner layer circuit 13 is inspected by an optical scanning method.
[0048] ⑥ Browning: Browning is performed on the inner layer circuit 13 to increase the bonding force between the inner layer circuit 13 and the second insulating layer 14 in the subsequent process.
[0049] ⑦ Hot pressing: heating, pressurizing and curing the double-sided copper-clad substrate, the second insulating layer 14 and the copper foil layer A10 stacked together to firmly combine them together to obtain the first processed board 1.
[0050] S2: A protective film 2 with a protective function is provided on the copper foil layer A10 to divide the copper foil layer A10 into a protection area 100 covered by the protective film 2 and a processing area 101 exposed outside the protective film 2; in addition, the area on the protective film 2 and within a set range surrounding the processing area 101 is defined as a transition area A20. According to the design requirements of the circuit board product, the transition area A20 is also optimally controlled to be processed as follows: its protection strength gradually increases from its edge close to the processing area 101 to the direction away from the processing area 101; so that when the copper reduction operation is performed in the later process, the processing area 101 and the protection area 100 are smoothly transitioned and connected without forming obvious steps.
[0051] Specifically, in this embodiment 1, according to the circuit board processing requirements, the protective film 2 preferably adopts an anti-etching (or anti-etching) photosensitive dry film, and is coated on the copper foil layer A10 through a negative image pattern making process. Further, the specific manufacturing method of coating the protective film 2 on the copper foil layer A10 through the negative image pattern making process is as follows:
[0052] S20: Pre-treatment before coating; including: a) drilling a positioning target hole on the first processing plate 1 using an X-Ray target drilling machine; b) positioning through the positioning target hole, and using a milling machine to mill away the waste material around the edge of the first processing plate 1; c) grinding, cleaning, heating and drying the first processing plate 1 after the milling / gonging plate edge processing is completed to facilitate the post-processing operation.
[0053] S21: coating with an anti-corrosion photosensitive film; coating the anti-corrosion photosensitive dry film B on the two copper foil layers A10; and performing alignment based on the positioning target hole during the film coating process.
[0054] S22: Exposure and development; exposure is to expose part of the area of the anti-etching photosensitive dry film B according to the operation data of the circuit board; development is to remove the unexposed area of the anti-etching photosensitive dry film B; then the protective film 2 is obtained, and the details can be referred to in the attached Figure 4 shown.
[0055] It can be understood that according to the impedance matching principle (see background technology) and by optimizing the operating data of the circuit board, the area on the copper foil layer A10 used to make impedance signal lines with large impedance values (defined as processing area 101) can be exposed outside the protective film 2, and the area on the copper foil layer A10 used to make impedance signal lines with small impedance values and other lines (defined as protection area 100) can be covered by the protective film 2.
[0056] Supplementary explanation: Based on the practice in the circuit board industry, the pattern of the protective film 2 obtained after development is called a negative image.
[0057] S23: After completing the above-mentioned development process, the protective film 2 is also subjected to a blank exposure (i.e., exposure without superimposing any negative film with any pattern) to further enhance the curing of the protective film 2 and prevent the protective film 2 from falling off from the copper foil layer A10; and further improve the anti-etching ability of the protective film 2.
[0058] In addition, according to the impedance matching principle, the post-process needs to perform copper reduction operation on the processing area 101. In order to ensure that the processing area 101 after copper reduction is smoothly transitioned and connected with the protection area 100, so as to facilitate the post-process to make circuit patterns on the copper foil layer A10 after copper reduction, this embodiment 1 also makes the following preferred design: the area on the protective film 2 and within the set range surrounding the processing area 101 is defined as the transition area A20, and the protection strength of the transition area A20 gradually increases from the edge close to the processing area 101 to the direction away from the processing area 101, that is, the protection strength of the transition area A20 gradually decreases from the edge of one side away from the processing area 101 to the edge of the other side close to the processing area 101; in this way, when the copper reduction operation is performed in the post-process, the copper foil layer can be made The area on the copper foil layer A10 and corresponding to the transition area A20 is also subjected to copper reduction. If the area on the copper foil layer A10 and corresponding to the transition area A20 is defined as the transition area B102 (the transition area B102 actually belongs to a special part of the protection area 100), based on the protection strength characteristics of the transition area A20, the transition area B102 can present: the copper thickness of the transition area B102 gradually increases from the edge of one side close to the processing area 101 to the direction away from the processing area 101, that is, the copper reduction of the transition area B102 is less than the copper reduction of the processing area 101; the transition area B102 is also formed with an inclined surface that is gently inclined upward, so that the processing area 101 and the protection area 100 can be smoothly transitioned and connected, please refer to the attached Figure 5 and attached Figure 6 shown.
[0059] Furthermore, in this embodiment 1, the method for gradually increasing the protection strength of the transition area A20 from the edge close to the processing area 101 to the direction away from the processing area 101 is:
[0060] S220: A positive image film is also provided, on which a specific film area corresponding to the transition area A20 is provided, and the shading rate of the specific film area gradually decreases along the increasing direction of the protection strength of the transition area A20.
[0061] Specifically, in this embodiment 1, the specific area of the film is polished with 2500 (i.e., 2500 mesh) metallographic sandpaper so that the shading rate of the specific area of the film gradually decreases from 100% to 5% along the direction of increasing protection strength of the transition area A20.
[0062] S221: After the anti-etching photosensitive dry film B is attached to the copper foil layer A10, the positive film is placed on the anti-etching photosensitive dry film B, and then exposed and developed to obtain the protective film 2 with the transition area A20.
[0063] It is understandable that since the shading rate of the specific area of the film gradually decreases from 100% to 5%, the protection strength of the transition area A20 will inevitably not be unique during the exposure processing, and will show a protection strength enhancement change pattern in the same direction as the shading rate of the specific area of the film.
[0064] Furthermore, according to the design requirements of the circuit board product, the transition area A20 is optimized as follows: the transition area A20 is an area within 2 mm from the edge of the protective film 2 surrounding and close to the processing area 101 to the direction away from the processing area 101. It is understandable that the present application is not limited to the above-mentioned design of the transition area A20, which can be specifically determined according to the design requirements of the circuit board product.
[0065] S3: performing copper reduction operation on the processing area 101, so that the copper thickness of the processing area 101 is less than the copper thickness of the protection area 100, and the processing area 101 and the protection area 100 are smoothly transitioned and connected; obtaining a second processed plate 3, which can be referred to in the attached Figure 5 shown.
[0066] Specifically, since the protective film 2 is preferably an anti-corrosion photosensitive dry film, the present embodiment 1 preferably uses an etching process to perform copper reduction. According to the design requirements of the circuit board product, the copper reduction amount of the processing area 101 is also optimally controlled to be 15-20 μm.
[0067] In addition, it can be seen from the above that based on the configuration of the transition area A20, a transition area B102 that can smoothly transition and connect with the processing area 101 can be formed on the protection area 100 and close to the processing area 101; and in order to further optimize the subsequent process to produce circuit patterns on the copper foil layer A10 after copper reduction, this embodiment 1 also removes the protective film 2 and grinds the first processing board 1 after the copper reduction operation, so that the processing area 101 and the protection area 100 can smoothly transition and connect.
[0068] Furthermore, the protective film 2 can be removed by using a strong alkaline solution; and the copper foil layer A10 after copper reduction can be ground by using a non-woven grinding machine.
[0069] S4: Circuit production is performed on the second processed board 3 to produce a circuit pattern on the copper foil layer A10 after copper reduction; the circuit pattern includes a first impedance signal line 51 provided in the protection area 100 and a second impedance signal line 52 provided in the processed area 101 after copper reduction, and the impedance value of the second impedance signal line 52 is greater than the impedance value of the first impedance signal line 51; for details, please refer to the attached Figure 7 shown.
[0070] Specifically, the specific production method for circuit production on the second processing board 3 in this embodiment 1 is: the second processing board 3 is subjected to drilling, copper electroplating, lamination pretreatment, anti-plating photosensitive film coating, exposure, development, graphic electroplating copper layer, electroplating tin layer, film stripping, alkaline etching copper, and removal of tin plating layer in sequence to produce the circuit pattern.
[0071] Note: The processing steps of "drilling, copper electroplating, pre-treatment of coating, coating of photosensitive film for resist plating, exposure, development, pattern electroplating of copper layer, electroplating of tin layer, film stripping, alkaline etching of copper, and removal of tin layer" described in S4 above are all common technical means in the field of circuit board processing technology, so they will not be described in detail here, but only briefly described as follows:
[0072] ① Drilling: drilling the second processing plate 3 with a drilling machine to obtain through holes on the effective area of the second processing plate 3.
[0073] ② Copper electroplating: a connecting copper body of a set thickness is plated on the inner wall of the through hole through chemical copper plating and electroplating process; the two copper foil layers A10 can be connected to the inner layer circuit 13 by means of the connecting copper body.
[0074] It is understandable that, according to processing requirements, the connecting copper body can be a copper column structure or a copper ring structure. However, when the connecting copper body adopts a copper ring structure, resin plugging operations need to be performed accordingly.
[0075] ③ Pre-coating treatment, coating with anti-plating photosensitive film, exposure, and development: Pre-coating treatment is to clean, heat and dry the second processed board 3; coating with anti-plating photosensitive film is to stick the anti-plating photosensitive dry film on the copper foil layer A10 after copper reduction; exposure is to expose part of the anti-plating photosensitive dry film according to the operating data of the circuit board; development is to remove the unexposed area of the anti-plating photosensitive dry film.
[0076] ④ Graphic electroplated copper layer, electroplated tin layer: The graphic electroplated copper layer is formed by electroplating a build-up copper layer 4 having a thickness of more than 20 μm on the copper foil layer A10 and in the area exposed outside the anti-plating photosensitive dry film. Figure 7 As shown; it can be understood that the line width and line spacing of each part of the build-up copper layer 4 can be designed to be consistent or inconsistent, depending on the design requirements of the circuit board product;
[0077] The patterned electroplated tin layer is a tin layer with a thickness of 4 to 6 μm plated on the build-up copper layer 4 by electroplating. The tin layer is a protective layer and will be removed after the circuit is completed.
[0078] ⑤ Stripping, alkaline copper etching, and removing the tin-plated layer: Stripping is to remove the anti-plating photosensitive dry film with a strong alkaline solution; alkaline copper etching is to etch away the area on the copper foil layer A10 that is not covered and protected by the tin-plated layer with a strong alkaline solution; removing the tin-plated layer is to remove the tin-plated layer; that is, to obtain the circuit pattern. It can be understood that the circuit pattern is composed of the build-up copper layer 4 and the part of the copper foil layer A10 located directly below the build-up copper layer 4, and the periphery of the build-up copper layer 4 is flush with the periphery of the part of the copper foil layer A10 located directly below it.
[0079] As can be seen from the above, the actual copper thickness of the circuit pattern (including the first impedance signal line 51) arranged on the protection area 100 is: the sum of the copper thickness of the protection area 100 and the copper thickness of the build-up copper layer 4; Figure 7 The actual copper thickness of the circuit pattern (including the second impedance signal line 52) set on the processing area 101 after copper reduction is: the sum of the copper thickness of the processing area 101 after copper reduction and the copper thickness of the added copper layer 4; please refer to the attached Figure 7 shown.
[0080] Since the copper thickness of the processing area 101 after copper reduction is less than the copper thickness of the protection area 100, the copper thickness of the second impedance signal line 52 is less than the copper thickness of the first impedance signal line 51; based on the premise that the line width and line spacing of the first impedance signal line 51 and the second impedance signal line 52 remain the same (which can be achieved by designing the operation data when manufacturing the build-up copper layer 4), it can be obtained that: the impedance value of the second impedance signal line 52 is greater than the impedance value of the first impedance signal line 51.
[0081] S5: The second processed board 3 that has completed the circuit production is subjected to conventional impedance testing, AOI testing, solder masking, character printing (printing text logos), hot air leveling, edge milling, cleaning (soft brush cleaning and ultrasonic cleaning), electrical testing (open circuit, short circuit and insulation testing), and packaging processes in sequence to complete the production of the subsequent circuit board finished product required.
[0082] As can be seen from the above, the present invention can realize the production of multiple groups of impedance signal lines with "same line width and spacing, but different impedance values" on the same circuit layer of the circuit board product through technical innovation, which well meets the special needs of the market. In addition, the circuit board production method provided by the present invention is simple, reasonable, flexible in operation, easy to produce and implement, and the resulting circuit board has a high yield and good quality.
[0083] Embodiment 2:
[0084] The second embodiment provides a circuit board with signal lines having different impedances, which is manufactured by using the method for manufacturing a circuit board with signal lines having different impedances described in the first embodiment.
[0085] Specifically, the circuit board structure is as follows: Figure 7 As shown, the circuit board includes the first insulating layer 11, the inner layer circuit 13, the second insulating layer 14 and the circuit pattern which are stacked in sequence from the inside to the outside, and the circuit pattern includes the first impedance signal line 51 and the second impedance signal line 52. The line width and line spacing of the first impedance signal line 51 and the second impedance signal line 52 are the same, and the impedance value of the second impedance signal line 52 is greater than the impedance value of the first impedance signal line 51.
[0086] Note: In this specification, the prefixes "first", "second", etc. of the component names (such as the first processed board, the second processed board, etc.), and the suffixes "A", "B", etc. of the component names (such as copper foil layer A, copper foil layer B, etc.) are only for the convenience of description and are not used to limit the scope of implementation of the patent of this invention.
[0087] To sum up, the circuit board manufacturing method described in the present invention is simple, reasonable, and flexible to operate. It can realize the production of multiple groups of impedance signal lines with "the same line width and spacing but different impedance values" on the same circuit layer of the circuit board product, which well meets the special needs of the market.
[0088] Many specific details are described in the above description to facilitate a full understanding of the present invention. However, the above description is only a preferred embodiment of the present invention. The present invention can be implemented in many other ways different from those described herein, so the present invention is not limited to the specific implementation disclosed above. At the same time, any person familiar with the art can make many possible changes and modifications to the technical solution of the present invention using the methods and technical contents disclosed above without departing from the scope of the technical solution of the present invention, or modify it into an equivalent embodiment of equivalent changes. Any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of protection of the technical solution of the present invention.
Claims
1. A method for manufacturing a circuit board having signal lines with different impedances, characterized in that: include: Providing a first processed board (1), wherein the outermost layer of the first processed board (1) is a copper foil layer A (10) which is used to make a circuit pattern; A protective film (2) having a protective function is provided on the copper foil layer A (10) to divide the copper foil layer A (10) into a protection area (100) covered by the protective film (2) and a processing area (101) exposed outside the protective film (2); in addition, an area on the protective film (2) and within a set range surrounding the processing area (101) is defined as a transition area A (20), and the protection strength of the transition area A (20) gradually increases from its edge close to the processing area (101) to a direction away from the processing area (101); Performing a copper reduction operation on the processing area (101) so that the copper thickness of the processing area (101) is less than the copper thickness of the protection area (100), and the processing area (101) and the protection area (100) are smoothly transitioned and connected; obtaining a second processed plate (3); Circuit fabrication is performed on the second processed board (3) to produce a circuit pattern on the copper foil layer A (10) after copper reduction; the circuit pattern comprises a first impedance signal line (51) provided in the protection area (100) and a second impedance signal line (52) provided in the processed area (101) after copper reduction, wherein the impedance value of the second impedance signal line (52) is greater than the impedance value of the first impedance signal line (51).
2. The method for manufacturing a circuit board having signal lines with different impedances according to claim 1, characterized in that: The protective film (2) has an anti-etching function.
3. The method for manufacturing a circuit board having signal lines with different impedances according to claim 2, characterized in that: The first processed plate (1) is sequentially subjected to pre-coating treatment, anti-corrosion photosensitive film coating, exposure, and development processing, so as to coat the protective film (2) on the copper foil layer A (10); In addition, after the above-mentioned development process is completed, the protective film (2) is also subjected to air exposure.
4. The method for manufacturing a circuit board having signal lines with different impedances according to claim 3, characterized in that: A positive image film is also provided, on which a specific film area corresponding to the transition area A (20) is provided, and the light shielding rate of the specific film area gradually decreases along the increasing direction of the protection strength of the transition area A (20).
5. The method for manufacturing a circuit board having signal lines with different impedances according to claim 4, characterized in that: The specific area of the film is polished with metallographic sandpaper so that the light shielding rate of the specific area of the film is gradually reduced from 100% to 5%.
6. The method for manufacturing a circuit board having signal lines with different impedances according to claim 4, characterized in that: The transition area A (20) is an area within 2 mm from the edge of the protective film (2) surrounding the processing area (101) and close to the processing area (101) in the direction away from the processing area (101).
7. The method for manufacturing a circuit board having signal lines with different impedances according to claim 2, characterized in that: The copper reduction operation is performed by using an etching process, and the copper reduction amount of the processing area (101) is 15 to 20 μm; In addition, an area on the copper foil layer A (10) and corresponding to the transition area A (20) is defined as a transition area B (102), the copper reduction amount of the transition area B (102) is less than the copper reduction amount of the processing area (101), and the transition area B (102) forms an inclined surface after etching copper reduction treatment.
8. The method for manufacturing a circuit board having signal lines with different impedances according to claim 7, characterized in that: After the copper reduction operation is completed, the protective film (2) is removed and the plate is ground in sequence, so that the processing area (101) and the protection area (100) are smoothly transitioned and connected.
9. The method for manufacturing a circuit board having signal lines with different impedances according to claim 1, characterized in that: The first processing board (1) is provided with an inner layer circuit; The second processed board (3) is subjected to drilling, copper electroplating, lamination pretreatment, anti-plating photosensitive film coating, exposure, development, pattern electroplating copper layer, electroplating tin layer, film stripping, alkaline copper etching, and tin layer removal processing in sequence to produce the circuit pattern; The second processed board (3) that has completed the circuit production is subjected to conventional impedance testing, AOI testing, solder masking, character printing, leveling, molding, cleaning, and electrical testing processes in sequence to complete the production of the subsequent required circuit board finished product.
10. A circuit board having signal lines with different impedances, characterized in that: The circuit board is manufactured by the method for manufacturing a circuit board having signal lines with different impedances as described in any one of claims 1 to 9.
Citation Information
Cited By
Multi-layer circuit board impedance precision improving method and device, electronic equipment and medium
CN121692529A