Method for producing photocatalytic multicomponent fibers and photocatalytic multicomponent fibers
Through the combination of the support mixture and the active mixture, multi-component fibers are formed, which solves the problem of low efficiency and easy damage in the air purifier, and achieves the improvement of high-efficiency photocatalyst distribution and mechanical properties.
Patent Information
- Application Number
- CN202380026641.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-11
- Filing Date
- 2023-03-10
- Publication Date
- 2024-11-01
AI Technical Summary
The existing photocatalytic fibers are inefficient and easily damaged in air purifiers, making it difficult to maintain the concentration and uniform distribution of high photocatalysts, and there is also the problem of insufficient aggregate and mechanical characteristics.
Using a combination of carrier mixture and active mixture, including thermoplastic polymers, organic polymers, photocatalysts and antioxidant coupling agents, multicomponent fibers are formed by spinning, and by eliminating surface organic polymers to create an inorganic surface to ensure light The even distribution and high content of the catalyst while maintaining the flexibility and mechanical strength of the fibers.
Efficient photocatalyst distribution and optimized efficiency of air purifiers are achieved, reducing the risk of fiber breakage and damage, while improving the mechanical properties and molding flexibility of the fibers.
Smart Images

Figure CN118891104A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of textiles. In particular, the present invention relates to the field of textile fibers.
[0002] The invention more particularly relates to a method for producing photocatalytic multicomponent fibers and to the photocatalytic multicomponent fibers themselves. Furthermore, the invention relates to a textile comprising photocatalytic multicomponent fibers and to a filter provided with at least one textile according to the invention. Background Art
[0003] The known prior art from which the present invention was developed is described below.
[0004] Air and water pollution has been increasing in recent years. The presence of organic or inorganic molecules in the air and / or water is carefully monitored. In fact, it has been shown that air pollution causes many diseases (for example cardiopulmonary diseases or certain cancers) on the one hand, and leads to aggravated deterioration and pollution of the environment. Similarly, water pollution (groundwater table, lakes, rivers, seas and oceans) continues to increase the harm to fauna and flora. Many purification devices (air and / or water) have also been developed. These devices are particularly intended to be used to eliminate pollutants, pathogens or other allergens.
[0005] These purification devices generally operate by physical methods, such as by filters or electrostatic precipitators, or by absorption of pollutants on materials (such as activated carbon), or by destruction or inactivation using ultraviolet rays or by photocatalysis. Some systems combine more than one technology and each purification device may have different benefits and risks.
[0006] In the field of air treatment, photocatalysts are materials that can decompose substances without emitting secondary pollutants. TiO2 is one of the most commonly used photocatalysts. It is a semiconductor material that allows a variety of redox reactions, including in particular the use of properties regarding light absorption and more precisely in the UV field to decompose pollutants. In addition, TiO2, in addition to its strong photoactivity, is a stable material with a high yield and which is particularly advantageous for industry, being cheap.
[0007] The treatment method implemented by the photocatalytic purifier allows the decomposition and degradation of pollutants on the surface of a photocatalyst, generally titanium dioxide (TiO2), under the action of light rays. The method destroys volatile organic compounds, inorganic pollutants and microorganisms. The final process essentially produces water and carbon dioxide.
[0008] For photocatalytic purifiers, photocatalysts are generally deposited on the surface of a substrate. The photocatalyst can be deposited in the form of a powder, a suspension or a solution. This type of deposition on the surface of the substrate can lead to the formation of photocatalyst aggregates and only partial coverage at a small thickness. In this case, the photocatalyst tends to fall off easily from its substrate, which makes the substrate on which it is deposited deactivated very quickly.
[0009] Furthermore, it has been proposed that binders may be added to improve the adhesion of TiO2 to the substrate. However, such binders may significantly reduce the photocatalytic efficiency.
[0010] Finally, impregnation of a surface with a mixture containing a photocatalyst can strongly change the fluid dynamics at the impregnated surface and drastically reduce the photocatalytic efficiency and increase the pressure drop in the air purifier.
[0011] Recently, it has been proposed to use composite fibers comprising a polymer and a small amount of photocatalyst to form filters for air purifiers. However, with these techniques, the photocatalyst is trapped in the photocatalytic fiber in a random manner, which greatly reduces its efficiency. The fiber may therefore contain TiO2 aggregates, or conversely, areas without TiO2. In addition, when the substrate is in the form of a fiber, the presence of aggregates in the polymer may hinder subsequent manufacturing steps such as spinning.
[0012] In addition, most substrates currently used to fix TiO2 include fibers from glass, ceramics, clay minerals, zeolites, metal plates, cellulose or activated carbon fibers. However, these substrates are particularly fragile on the one hand and very rigid on the other hand (inflexible, inflexible), which leads to limitations in the geometry of purifiers that currently look the same. In fact, during spinning, the fibers are drawn, heated and cooled many times. The fibers can then be damaged, such as cracking or even breaking. In particular, these fibers can be overdrawn and experience mass loss, pressure drop or even a drop in force. This greatly limits the molding and geometry of the textile and thereby limits the photocatalyst.
[0013] Furthermore, during industrialization, it becomes very difficult to ensure good capacity and efficiency of photocatalysts based on fibers containing TiO2. On the one hand, in order to ensure good photocatalytic performance, it is necessary to incorporate a sufficient amount of photocatalyst into the fiber while ensuring sufficient fluidity of the matrix and uniform distribution of the TiO2 during spinning; on the other hand, it is necessary to ensure optimal spinning so that the fiber retains its mechanical characteristics and its manipulability while limiting the pressure drop.
[0014] In order to overcome the problem of aggregates and ensure optimal dispersion of TiO2, for example, a linear titanium oxide polymer is proposed in document US2020282387. In this document, the coating layer is formed by sintering a solution containing the polymer that can be deposited on a substrate in the form of fibers. However, in this document, the substrate is preferably rough with a protruding outer surface. This allows to improve the adhesion of TiO2 to the substrate, but aggravates the formation of TiO2 aggregates on the surface. In addition, sintering gives the structure a high rigidity, which reduces processability and hinders any molding operation. In addition, such a product is very fragile and very fragile, which in particular limits the reduction of its thickness to reduce the pressure drop.
[0015] Other technologies have also been developed, such as the method for producing macroscopic TiO2 fibers by continuous extrusion in a unidirectional flow described in document EP3126550. Such a method allows the large-scale production of macroscopic TiO2 fibers. However, in order to obtain good photocatalytic properties, after the production of the fibers, the polymer is completely calcined, and the fibers then contain only TiO2 and are extremely brittle. Their mechanical resistance after calcination does not allow the application of a sufficiently strong airflow for use in air purifiers.
[0016] The object of the present invention is to overcome the disadvantages of the prior art. In particular, the object of the present invention is to propose a method for manufacturing a multicomponent fiber with a high surface concentration of a photocatalyst, said multicomponent fiber having a uniform distribution of the photocatalyst so as to optimize the efficiency of a photocatalytic air purifier using the fiber, while maintaining a high air permeability, while allowing to provide an extensible fabric that can support different shaping operations. Summary of the invention
[0017] The present invention aims to overcome these disadvantages.
[0018] The present invention particularly relates to a method for producing a photocatalytic multicomponent fiber comprising the following steps:
[0019] - providing a carrier mixture comprising at least one thermoplastic polymer or a thermoplastic polymer precursor;
[0020] - Providing an active mixture, the active mixture comprising:
[0021] o at least one organic polymer or one organic polymer precursor,
[0022] o at least one photocatalyst in a concentration of at least 10% by weight relative to the weight of the active mixture,
[0023] o at least one antioxidant coupling agent, preferably a silane; or an antioxidant coupling agent precursor,
[0024] - spinning multicomponent fibers from a carrier and an active mixture;
[0025] - eliminating said at least one organic polymer on the surface of the multi-component fiber, so that a photocatalytic multi-component fiber is produced.
[0026] The Applicant has developed a method capable of producing multicomponent photocatalytic fibers having a high photocatalyst content, a homogeneous surface distribution of said photocatalyst, while being deformable and having mechanical properties compatible with its use in air purifiers. In practice, said elimination step allows the formation of an inorganic surface (preferably predominantly inorganic) comprising said photocatalyst in contact with a thermoplastic polymer support.
[0027] The Applicant has in particular developed a carrier mixture and an active mixture, the combination of which allows to ensure the production of flexible fibers having a high content of the photocatalyst on the surface and a uniform distribution of the photocatalyst on the surface, so that aggregates of the photocatalyst are reduced or absent and the surface of the fiber is largely covered with the photocatalyst.
[0028] Furthermore, such a method also makes it possible to spin fibers without breakage, cracking, or loss of force.
[0029] Therefore, the method according to the present invention allows to meet the needs and in particular proposes to generate multicomponent photocatalytic fibers with a high surface concentration of photocatalyst so as to optimize the capacity and efficiency of said photocatalyst and its uniform distribution providing a porous multicomponent fiber surface with almost no or no aggregates, while being extensible to cope with different forming operations.
[0030] According to other optional characteristics of the method, the method may optionally include one or more of the following characteristics alone or in combination:
[0031] - said elimination of said at least one organic polymer on the surface of said multicomponent fiber comprises a surface calcination so as to generate an inorganic surface in contact with the thermoplastic polymer support. This allows on the one hand to activate said photocatalyst and on the other hand to ensure a uniform distribution while providing said photocatalytic multicomponent fiber with a porous surface to improve the exchange with the air;
[0032] - said thermoplastic polymer of said carrier mixture is chosen from thermoplastic polymers having a melting temperature comprised between 100° C. and 350° C. These thermoplastic polymers of said carrier mixture are preferably of biosource and / or biodegradable;
[0033] - it comprises extrusion and / or coextrusion of the carrier mixture and / or the active mixture;
[0034] - the carrier mixture and the active mixture have melt flow indices (hot flow indices), measured according to standard ISO 1133, such that the difference between the melt flow index of the active mixture and the melt flow index of the carrier mixture is less than or equal to 20%. This allows a better control of the viscosity of the carrier and the active mixture, in order to ensure optimal spinning without breakage and / or loss of force. In addition, this ensures optimized mechanical properties of the photocatalytic multicomponent fibers,
[0035] During spinning, the multicomponent fiber has a 2 The calculated sheathing rate is comprised between 5% and 50%. This ensures a uniform distribution of the photocatalyst and reduces the pearl necklace effect.
[0036] According to a second object, the present invention relates to a photocatalytic multicomponent fiber comprising:
[0037] - a thermoplastic polymer carrier, and
[0038] - Inorganic surfaces;
[0039] The thermoplastic polymer support includes at least one thermoplastic polymer, and the inorganic surface includes an oxidation resistant coupling agent network associated with a photocatalyst.
[0040] According to other optional characteristics of the photocatalytic multi-component fiber, the photocatalytic multi-component fiber may optionally include one or more of the following characteristics alone or in combination:
[0041] - it has a diameter less than or equal to 150 μm,
[0042] - said inorganic surface has a thickness of at least 500 nm,
[0043] According to a third object, the present invention relates to a textile comprising at least one photocatalytic multicomponent fiber according to the present invention. Such a textile according to the present invention is flexible and extensible.
[0044] According to a fourth object, the present invention relates to a filter comprising at least one textile according to the invention. Unlike existing filters, such a filter can have a variable geometry, for example pleated. Furthermore, unlike existing filters, the filter according to the invention can have an adapted conformation, for example custom-made.
[0045] According to a fifth object, the present invention relates to a photocatalytic air purifier, which is equipped with at least one filter according to the present invention, a ventilation system and an ultraviolet irradiation system capable of irradiating the at least one filter; the ventilator is arranged to transport air from the inlet of the purification system through the filter to the outlet of the purification system. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Other characteristics and advantages of the invention will be better understood on reading the following description and with reference to the accompanying drawings, given by way of illustration and non-limiting manner.
[0047] [ Figure 1 ] Figure 1 A diagram showing a method for making photocatalytic multi-component fibers according to one embodiment of the present invention.
[0048] [ Figure 2 ] Figure 2 Figures showing different cross sections of a photocatalytic multicomponent fiber according to the present invention.
[0049] [ Figure 3 ] Figure 3 A photograph showing a photocatalytic multi-component fiber according to one embodiment of the present invention is shown by scanning electron microscopy (SEM) at x80 magnification.
[0050] For illustrative purposes, the drawings are not necessarily to scale, particularly with respect to thickness.
[0051] Aspects of the present invention are described with reference to flowcharts and / or block diagrams of methods and apparatus (systems) according to embodiments of the invention.
[0052] In the accompanying drawings, flow charts and block diagrams illustrate possible implementations of the system and method according to various embodiments of the present invention, functions and operations. In some implementations, the functions associated with the modules may appear in a different order than shown in the figure. For example, two modules shown in succession may in fact be executed substantially simultaneously, or, depending on the functions involved, the modules may sometimes be executed in the opposite order. DETAILED DESCRIPTION
[0053] In the following, an overview of the present invention and the associated vocabulary are described before introducing the disadvantages of the prior art, and then finally showing in more detail how the present invention overcomes them.
[0054] In the remainder of the description, the expression "multicomponent fibers" may correspond to bicomponent, tricomponent fibers or more.
[0055] Within the meaning of the present invention, the term "support mixture" may correspond to a mixture that is intended to form a network supporting the active mixture so that the active mixture rests on, around or in the support mixture. For example, in a core-sheath fiber configuration, the support mixture may correspond to the fiber core.
[0056] Within the meaning of the present invention, the term "active mixture" may correspond to a mixture intended to form a preferably inorganic network on the surface of the support mixture and intended to interact with a physical stimulus during a photocatalytic reaction. For example, in a core-sheath fiber configuration, the active mixture may correspond to the fiber sheath.
[0057] Within the meaning of the present invention, the term "core" may correspond to an inner part of a fiber, such as the core.
[0058] Within the meaning of the present invention, the term "sheath" may correspond to the outer part of the fiber, such as an envelope.
[0059] Within the meaning of the present invention, the expression "thermoplastic polymer" may correspond to a polymer that can be repeatedly softened or melted under the effect of heat and adopt new shapes by applying heat and pressure.
[0060] Within the meaning of the present invention, the expression "thermoplastic polymer precursor" may correspond to a component allowing to start or initiate the polymerization reaction of one or more monomers.
[0061] Within the meaning of the present invention, the expression "organic polymer" may correspond to a linear, branched or cyclic polymer, the polymer core of which comprises at least one carbon atom.
[0062] Within the meaning of the present invention, the term "polymerization" may correspond to a process allowing a monomer or a mixture of monomers to be converted into a polymer.
[0063] Within the meaning of the present invention, the term "predominantly" may correspond to at least 50%, preferably more than 50%. For example, a predominantly inorganic surface within the meaning of the present invention may correspond to a surface comprising more inorganic polymers by weight than organic polymers, or more inorganic molecules by mole than organic molecules. A predominantly inorganic surface may, for example, comprise at least 50% by weight of photocatalysts and coupling agents.
[0064] Within the meaning of the present invention, the term "antioxidant" may correspond to reducing or limiting the interaction with oxygen, so that redox reactions, in particular during photocatalysis, are reduced.
[0065] Within the meaning of the present invention, the term "substantially equal" may correspond to a value that varies less than 50%, preferably less than 40%, even more preferably less than 30% relative to the value being compared. When substantially equal is used for a comparison value, the comparison value varies less than 50%, preferably less than 40%, even more preferably less than 30% compared to the value used as a reference.
[0066] The present invention proposes taking into account existing difficulties associated with bulky photocatalytic filters and in particular that they may result in pressure drops and / or reduced photocatalyst efficiency.
[0067] In particular, the invention proposes a method for manufacturing multicomponent fibers comprising a polymer support combined with an inorganic surface (preferably predominantly inorganic) surface. Such a method allows the formation of fibers with high mechanical strength, which can be shaped without damaging them and then formed into filters with photocatalytic surfaces, which combine high permeability and high photocatalyst content compared to impregnated textiles with the same characteristics (thickness, density, fiber size).
[0068] Accordingly, the present invention is directed to a process for making multicomponent fibers.
[0069] Figure 1 An example of a method 100 for manufacturing a photocatalytic multi-component fiber is shown. Such a manufacturing method 100 includes a step 110 of supplying a carrier mixture, a step 120 of supplying an active mixture, a spinning step 130, and a step 160 of eliminating at least one organic polymer on the surface of the multi-component fiber. In addition, the manufacturing method 100 according to the present invention may include a step 140 of forming a fabric and a step 150 of shaping the fabric.
[0070] exist Figure 1 In an example of the invention, the method 100 for making a photocatalytic multi-component fiber includes a step 110 of supplying a carrier mixture. The carrier mixture includes at least one thermoplastic polymer. Alternatively, the carrier mixture includes at least one thermoplastic polymer precursor. According to another alternative, the carrier mixture includes at least one thermoplastic polymer and at least one thermoplastic polymer precursor.
[0071] The thermoplastic polymer of the carrier mixture may be chosen from thermoplastic polymers having a melting temperature below 350° C., for example comprised between 100° C. and 350° C. Advantageously, the thermoplastic polymer of the carrier mixture may be chosen from: polypropylene, polyester, polyethylene, polylactic acid, polyamide, polyvinyl, polyacrylate, polybutylene terephthalate, polyhydroxyalkanoate, polybutylene terephthalate-co-adipate and mixtures thereof. For example, the thermoplastic polymer of the carrier mixture may be chosen from: polyethylene terephthalate, biopolyethylene terephthalate, biopolyethylene, biodegradable polyester and polyhydroxyalkanoate.
[0072] Preferably, the thermoplastic polymer of the carrier mixture may be selected from bioderived and / or biodegradable thermoplastic polymers.
[0073] The thermoplastic polymer precursor for the carrier mixture according to the invention may be chosen from all thermoplastic polymer precursors having a melting temperature comprised between 100 and 350° C. Advantageously, the thermoplastic polymer precursor may be chosen from lactides, acrylates, methacrylates, styrenes and / or lactones.
[0074] Advantageously, the thermoplastic polymer of the carrier mixture and / or the thermoplastic polymer formed from a thermoplastic polymer precursor of the carrier mixture has good properties for spinning.
[0075] The step of providing a carrier mixture may, for example, include the preparation of a carrier mixture. In this embodiment, when the carrier mixture comprises a precursor such as at least one thermoplastic polymer monomer, the step of preparing the carrier mixture may include a polymerization step. The polymerization step may be performed using stimulation such as plasma, ion bombardment, electrochemical processes, chemical species (nucleophilic, electrophilic, etc.), light radiation. In addition, the polymerization step may be performed at a predetermined duration and temperature based on the at least one monomer.
[0076] The step of preparing the support mixture may be performed at a temperature of less than or equal to 400°C and greater than or equal to 100°C.
[0077] Optionally, the step of preparing the support mixture may include adding additives, for example to increase the electrical resistance of the flexible support, such as a photocatalytic multi-component fiber core in a core-sheath fiber configuration.
[0078] The method 100 for making a photocatalytic multi-component fiber includes a step 120 of supplying a reactive mixture.
[0079] The reactive mixture comprises at least one organic polymer, for example at least one thermoplastic polymer. Alternatively, the reactive mixture comprises at least one organic polymer precursor. According to another alternative, the reactive mixture comprises at least one organic polymer and at least one organic polymer precursor.
[0080] The polymer of the reactive mixture may be chosen from polymers having a melting temperature comprised between 100° C. and 350° C. Advantageously, the polymer of the reactive mixture may be chosen from: polypropylene, polyester, polyethylene, polylactic acid, polyamide, polyvinyl compounds, polyacrylates, polybutylene terephthalate, polyhydroxyalkanoates, polybutylene terephthalate-co-adipate and mixtures thereof. For example, the polymer of the reactive mixture may be chosen from: polyethylene terephthalate, biopolyethylene terephthalate, biopolyethylene, biodegradable polyesters and polyhydroxyalkanoates.
[0081] Preferably, the polymers of the active mixture may be selected from bioderived and / or biodegradable thermoplastic polymers.
[0082] Furthermore, the polymers of the reactive mixture may contain additional grafting chemical groups.
[0083] The polymer precursor of the reactive mixture according to the invention may for example be chosen from all polymer precursors having a melting temperature comprised between 100 and 350° C. Advantageously, the polymer precursor may be chosen from lactides, acrylates, methacrylates, styrenes and lactones.
[0084] In a specific embodiment of the present invention, the providing of the active mixture may include a step of preparing the active mixture.
[0085] The step of preparing the reactive mixture may be performed at a temperature of less than or equal to 400°C and greater than or equal to 100°C.
[0086] In the case where the preparation of the reactive mixture comprises at least one thermoplastic polymer monomer, the step of preparing the reactive mixture may include a polymerization step. The polymerization step may be performed using stimulation such as plasma, ion bombardment, electrochemical processes, chemical species (nucleophilic, electrophilic, etc.), light radiation. In addition, the polymerization step may be performed at a predetermined duration and temperature according to the at least one monomer.
[0087] In a particular embodiment of the invention, the active mixture comprises the same polymer or polymer precursor as the carrier mixture.
[0088] Advantageously, the polymer (preferably thermoplastic) of the reactive mixture and / or the polymer formed from the polymer precursor (preferably thermoplastic) of the reactive mixture has good properties for spinning.
[0089] The active mixture comprises at least one photocatalyst. Preferably, the active mixture comprises at least one photocatalyst in a concentration of at least 10% by weight relative to the weight of the active mixture, preferably at least 15%, at least 20%, at least 25%, at least 30%, at least 35%, at least 40%. Preferably, the active mixture comprises a photocatalyst in a concentration of less than or equal to 50% by weight relative to the weight of the active mixture, preferably in a concentration of less than or equal to 45%. For example, the photocatalyst will be present in the active mixture in a concentration of 10% to 50% by weight relative to the weight of the active mixture, preferably in a concentration of 15% to 45% by weight relative to the weight of the active mixture, more preferably in a concentration of 20% to 45% by weight relative to the weight of the active mixture and even more preferably in a concentration of 25% to 40%. The photocatalyst can be dosed by a gravimetric dispenser.
[0090] Within the meaning of the present invention, the photocatalyst may be selected from the group consisting of transition metals, poor metals, metalloids and their oxides, preferably having photocatalytic properties. For example, the photocatalyst may be selected from the group consisting of AgBr, AgCl, Ag3PO4, Ag2S, AgI, Bi2O3, Bi2S3, C3N4, CdS, CdSe, CdO, Ce2O3, Ce2S3, CoO, CuO, Cu2O, Cu2S, CulnS2, FeTiO3, Fe2O3, GaAs, GaP, In2S3, MoS2, Nn2O3, NiO, PbO, PdO, RuO2, SnO2, SnS, TiO2, V2O5, WS2, WO3, ZnO, ZnS, ZrS2, ZnSe, ZrO2 and mixtures thereof.
[0091] The photocatalyst may be optionally doped and / or grafted. For example, the photocatalyst may be pre-treated by a hydrophobic treatment.
[0092] Preferably, the photocatalyst is TiO2.
[0093] The photocatalyst may be in crystalline form. In the specific case of TiO2, the photocatalyst may be in the form of anatase or a mixture of anatase and rutile or a mixture of anatase, rutile and limonite.
[0094] The photocatalyst may be in the form of nanoparticles having an average diameter of 2 nm to 100 nm, preferably 5 nm to 75 nm, more preferably 10 nm to 50 nm. The photocatalyst may be in powder form, or in the form of a precursor in solution.
[0095] According to one embodiment, the photocatalyst is incorporated into the active mixture while it is in the molten state. This limits and minimizes the formation of aggregates.
[0096] The reactive mixture comprises at least one coupling agent or coupling agent precursor.Preferably, the coupling agent according to the present invention is resistant to oxidation.
[0097] The coupling agent may comprise a chemical functional group that allows chemical bonding with at least one photocatalyst, preferably with TiO2. The coupling agent may comprise a chemical functional group that allows polymerization of the coupling agent so as to form a network. The coupling agent may comprise a chemical functional group that is capable of chemical bonding with the thermoplastic polymer of the support mixture.
[0098] The coupling agent may be selected from one or more geopolymers (geopolymers, geopolymers, mineral polymers) or one or more geopolymer precursors.
[0099] The coupling agent may be selected from silanes, or for example siloxanes.
[0100] The coupling agent is preferably selected from the group consisting of vinyl trimethoxysilane, polydimethylsiloxane, tetraethoxysilane, tetramethoxysilane, tetrapropoxysilane, n-propyl triethoxysilane, ethyl trimethoxysilane, methyl triethoxysilane, propyl trimethoxysilane, propyl triethoxysilane, phenyl trimethoxysilane, phenyl triethoxysilane, trimethoxy vinyl silane, triethoxy vinyl silane, vinyl triethoxy silane, vinyl tri(β-methoxyethoxy)silane, β-(3,4-epoxycyclohexyl)ethyltrimethoxysilane, γ-(2-aziridine)aminopropyltrimethoxysilane, γ-glycidyloxypropyltrimethoxysilane, γ-glycidyloxypropyltrimethyldiethoxysilane, γ-glycidyloxypropyltriethoxysilane, γ-methacrylpropyldimethoxysilane, γ-methacryltrimethoxysilane, γ-methacrylpropyldiethoxysilane, γ-methacrylpropyl Triethoxysilane, N-β (aziridine) γ-aminopropyl methyl dimethoxy silane, N-β (aziridine) γ-aminopropyl trimethoxy silane, N-β (aziridine) γ-aminopropyl triethoxy silane, N-β- (aminoethyl) -γ-aminopropyl trimethoxy silane, 3-acryloxypropyl trimethoxy silane, 3-aminopropyl trimethoxy silane, 3-aminopropyl triethoxy silane, N-phenyl-γ-aminopropyl trimethoxy silane, γ-Chloropropyltrimethoxysilane, γ-mercaptopropyltrimethoxysilane, bis[3-(triethoxysilyl)propyl]tetrasulfide (TESPT) and bis[3-(triethoxysilyl)propyl]disulfide, and preferably 3-acryloxypropyltrimethoxysilane, 3-chloropropyltrimethoxysilane, 3-mercaptopropyltrimethoxysilane, 3-methacryloxypropyltrimethoxysilane, 3-acryloxypropyltrimethoxysilane and combinations thereof. These coupling agents allow a good dispersion of the charges and simplify the compounding process. Preferably, the coupling agents allow the formation of an inorganic network, which allows resistance to photocatalysis. Preferably, the inorganic network is crosslinked. It preferably comprises polymer chains bound together by bonds of low molecular weight. It can then form a three-dimensional network. Advantageously, the inorganic network allows resistance to oxidation and therefore resistance to photocatalysis.
[0101] The coupling agent precursor may be selected from: silica, siloxane, silanol.
[0102] The active mixture comprises at least one coupling agent in a concentration of at least 0.75% by weight, preferably at least 1.5%, at least 2%, at least 2.5%, at least 3% relative to the weight of the active mixture. Preferably, the active mixture comprises a coupling agent in a concentration of less than or equal to 10% by weight, preferably less than or equal to 8%, relative to the weight of the active mixture. For example, the active mixture comprises at least one coupling agent in a concentration of 0.75% to 10% by weight relative to the weight of the active mixture, preferably at least 1.5% to 8% by weight relative to the weight of the active mixture.
[0103] Advantageously, the addition of a coupling agent to the reactive mixture allows reducing the viscosity of the reactive mixture relative to the viscosity of the same reactive mixture in the absence of the coupling agent, measured by rheometer according to ISO 1628 standard.
[0104] The active mixture may include the at least one coupling agent to the at least one photocatalyst in a mass ratio comprised between 1 / 50 and 5 / 1. Preferably, the active mixture may include the at least one coupling agent to the at least one photocatalyst in a mass ratio comprised between 1 / 20 and 2 / 1. More preferably, the active mixture may include the at least one coupling agent to the at least one photocatalyst in a mass ratio comprised between 1 / 10 and 1.
[0105] According to one embodiment, the coupling agent is incorporated into the reactive mixture by injection by means of a pump, such as a peristaltic pump.
[0106] Preferably, the photocatalyst used in the context of the present invention is previously combined with a coupling agent. Therefore, according to a preferred embodiment of the present invention, the coupling agent is added to the active mixture when it is coupled with the photocatalyst. Therefore, in this case, the method may include a step of coupling the photocatalyst to the coupling agent or a step of providing a photocatalyst coupled to the coupling agent.
[0107] The step of supplying the carrier mixture and / or the step of supplying the active mixture can be carried out by means of a mixer (compounder), a kneader, an extruder and / or a gravimetric and / or volumetric dispenser.
[0108] In a preferred embodiment, the step of providing a support mixture and / or the step of providing an active mixture comprises extrusion and / or coextrusion. The step of providing a support mixture and / or the step of providing an active mixture may comprise multiple extrusions. The multiple times may be greater than or equal to two times. Multiple extrusions allow for improved dispersion of the photocatalyst in the active mixture and incorporation of the coupling agent.
[0109] When the step of providing a carrier mixture comprises extrusion of a carrier mixture, the extrusion step is configured such that the carrier mixture has a melt flow index (MFI) substantially equal to the melt flow index of the active mixture, measured according to standard ISO 1133 (as measured at 230° C. for a standard mass of 2160 g). For example, the carrier mixture has a melt flow index (MFI) whose difference from that of the active mixture is less than or equal to 20%, preferably less than or equal to 10%, and even more preferably less than or equal to 5%. Thus, the difference between the MFI of the carrier mixture and the MFI of the active mixture is small and preferably less than or equal to 15%.
[0110] The melt flow index of the active mixture may, for example, be comprised between 5 g / 10 min and 1500 g / 10 min, measured according to standard ISO 1133. For example, the melt flow index of the carrier mixture may be comprised between 9 g / 10 min and 15 g / 10 min. In one embodiment, the MFI of the carrier mixture may be 12 g / 10 min and the MFI of the active mixture may be 27 g / 10 min. In another embodiment, the MFI of the carrier mixture may be 12 g / 10 min and the MFI of the active mixture may be 5 g / 10 min. In another embodiment, the MFI of the carrier mixture may be 12 g / 10 min and the MFI of the active mixture may be 11 g / 10 min.
[0111] The step of preparing the reactive mixture may be performed at a temperature of less than or equal to 400°C and greater than or equal to 100°C, preferably less than or equal to 300°C, more preferably less than or equal to 250°C.
[0112] The method 100 for making a photocatalytic multi-component fiber may include a spinning step 130. The spinning step is preferably performed from a support mixture and an active mixture.
[0113] The spinning step can be carried out hot (hear) by melt spinning (for quenching on a wheel), spunbonding (for cold drawing) and / or melt blowing (for hot drawing).
[0114] Figure 2 Examples of spinning configurations according to the present invention are shown. The figure shows some possible configurations: Figure 2 The core-sheath configuration in A; Figure 2 The island-in-the-sea configuration in B; Figure 2 C in a side-by-side configuration.
[0115] Figure 2The configurations shown in A and 2B allow the formation of one or more fibers comprising a thermoplastic polymer carrier 11 of the core type and an inorganic surface 12 (preferably predominantly inorganic) of the inorganic sheath type. Figure 2 As shown in FIG. 1B , the multicomponent fiber may include three phases: a thermoplastic polymer carrier 11, an inorganic (preferably predominantly inorganic) surface 12, and a sacrificial matrix 13. Indeed, in certain embodiments, the multicomponent fiber may include a sacrificial matrix that is generally removed prior to the step of eliminating at least one organic polymer.
[0116] like Figure 2 As shown in FIG. 4C , the multicomponent fiber may include a support 11 in contact with an inorganic (preferably predominantly inorganic) surface 12 .
[0117] In order to reduce the diameter of the obtained wire (wire web), an additional wire drawing step can be carried out under cold and / or hot conditions.
[0118] Preferably, a spinning step is carried out in order to achieve a fiber diameter comprised between 2 μm and 150 μm.
[0119] In order to avoid damage such as cracking, breaking, or loss of mass or decrease in strength, the spinning step is performed so that the fiber has a ratio according to the formula 4e*(D*e) / D 2 The sheath fraction measured by microscopy (SEM) is comprised between 5% and 50%, preferably between 7% and 30%. In the case where the percentage of sheath is equal to the surface area of the sheath (Sg) divided by the total surface area (St), Sg = St-Score, that is to say Sg = π*D2 / 4-π*(D-2e) 2 / 4 or Sg = π*(4De-4e 2 ) / 4 or Sg = π*e*(De), and thus the percentage of sheath corresponds to 4e*(De) / D 2 Where D is the outer diameter of the sheath and e is the thickness of the sheath. Thanks to the controlled sheath ratio, the pearl necklace effect (uneven distribution of the photocatalyst) is minimized.
[0120] Advantageously, the spinning step may be performed by melting and may include hot drawing, which may be performed by at least one extruder comprising one or more heating zones.Preferably, the melt spinning step comprises an extruder for the carrier mixture and an extruder for the reactive mixture.
[0121] The spinning step can be configured to change the ratio (e.g., mass) of the carrier mixture relative to the active mixture. This can allow the diameter of the fiber to be reduced and, for example, for core-sheath fibers, the core ratio relative to the sheath ratio to be changed. In addition, the fibers obtained due to the preparation steps of the carrier mixture and the active mixture have a uniform texture (measured by SEM microscopy) during the spinning step, which indicates a good dispersion of the charges and a uniform distribution of the photocatalyst on the surface. The fibers can be air cooled and directly wound.
[0122] The spinning step may include a drawing step. Drawing may preferably be carried out at a temperature between the glass transition temperature and the melting temperature of the polymer contained in the carrier and / or the active mixture. In this embodiment, the coil is unwound and passed through a first drawing station at a speed V1, the fiber is reheated, preferably 80° C. to 140° C., and drawn again at a speed V2 using a second drawing station before being wound again. The drawing ratio V2 / V1 allows the diameter to be varied. Drawing allows the diameter of the fiber to be refined and its mechanical properties to be improved.
[0123] The method 100 for making multi-component fibers may include a step 140 of forming a fabric from the multi-component fibers. The step 140 of forming a fabric from the multi-component fibers may or may not include a weaving or knitting step.
[0124] The step 140 of forming a fabric can be performed from a single multicomponent fiber, a plurality of multicomponent fibers, or a sheet of a plurality of multicomponent fibers. The fabric formed can correspond to a nonwoven fabric or a woven fabric in a planar, tubular, or other three-dimensional pattern. As with other textile structures, a variety of properties can be incorporated into the mesh structure to meet design objectives that may include: increased flexibility, increased strength, reduced thickness, improved maneuverability, and improved mechanical strength.
[0125] The method 100 for making multicomponent fibers may include a step of forming a fabric 150. Due to the flexibility of multicomponent fibers including thermoplastic polymers, the forming step 150 allows the formation of fabrics having a wide variety of configurations.
[0126] The method 100 for making a multicomponent fiber comprises a step 160 of eliminating at least one polymer on the surface of said multicomponent fiber. Preferably an organic polymer. Said elimination step allows the generation of a photocatalytic multicomponent fiber. Advantageously, said elimination step comprises a surface treatment of the multicomponent fiber.
[0127] Preferably, said step of eliminating said at least one polymer, preferably an organic polymer, on the surface of the multicomponent fiber allows the generation of an inorganic surface (preferably a predominantly inorganic surface) in contact with the thermoplastic polymer support. This allows, for example, the formation of an inorganic sheath around a thermoplastic polymer core in a core-sheath fiber configuration. The generated inorganic (preferably predominantly inorganic) surface may contain the presence of organic polymer. However, the remaining organic polymer is a minority by weight in the inorganic surface. In practice, the inorganic surface preferably comprises at least 50% by weight of photocatalyst and coupling agent.
[0128] The step of eliminating the at least one, preferably organic, polymer on the surface may comprise a thermal treatment, a chemical treatment, a plasma treatment, preferably locally, that is to say on the surface of the multicomponent fiber. Preferably, the treatment allows to eliminate at least part of the organic polymer from the active mixture at a depth of at least 500 nm, more preferably at least 1 μm, even more preferably at least 2 μm. Preferably, the treatment allows to eliminate at least part of the organic polymer from the active mixture at a depth of at most 50 μm, more preferably at most 30 μm, even more preferably at most 20 μm. For example, the elimination step allows to degrade at least part of at least one organic polymer of the active mixture at a depth of 500 nm to 50 μm, preferably 1 μm to 30 μm, and therefore more preferably 2 μm to 20 μm.
[0129] In combination Figure 2 In the specific embodiment shown in B, the sacrificial matrix may be removed prior to the removal step 160 by chemical, thermal or plasma treatment.
[0130] Furthermore, the elimination step of eliminating at least one polymer (preferably organic) from the surface of the multicomponent fiber may be partial or total. A partial elimination may correspond to the elimination of the restriction of the organic polymer at the depth of the multicomponent fiber.
[0131] The heat treatment may be selected from: UV (ultraviolet) or IR (infrared) radiation treatment, convection heating, conduction heating. Preferably, the heat treatment comprises calcination. The heat treatment is preferably localized on the surface and more preferably at a depth of at least 500 nm. The heat treatment may be carried out at a temperature comprised between 350° C. and 550° C. The heat treatment may be applied for a duration comprised between 0.5 hours and 7 hours.
[0132] The chemical treatment may be chosen from treatments using reactive species in solid, liquid or gaseous form and which will allow the elimination of the polymer from the reactive mixture, for example, treatment in oxidizing liquids of the oxygenated water type.
[0133] Plasma treatment generally involves ionization of a gas. Plasma treatment may, for example, involve applying an electric or magnetic field through a gas such that a plasma is formed that is capable of oxidizing the surface of the multicomponent fiber.
[0134] Eliminating the preferably organic polymer on the surface allows increasing the level of photocatalyst on the surface, which allows increasing the photocatalytic efficiency and thus greatly improving the photocatalytic properties of the multicomponent fibers.
[0135] According to another aspect, the present invention relates to a photocatalytic multicomponent fiber.
[0136] The multicomponent photocatalytic fiber according to the invention is obtainable by the method according to the invention. Preferably, it is directly obtainable by the method according to the invention.
[0137] The multicomponent fibers include a support comprising at least one thermoplastic polymer and an inorganic surface, preferably a predominantly inorganic surface.
[0138] In a particular embodiment, the photocatalytic multicomponent fibers according to the present invention comprise a thermoplastic polymer core and an inorganic sheath.
[0139] In an optional embodiment, the photocatalytic multi-component fiber may include, preferably between the core and the sheath, at least one intermediate sheath. The intermediate sheath may include another thermoplastic polymer, an inorganic material (e.g., silica), and / or a coupling agent. The intermediate sheath may, for example, help protect the core and increase the life of the multi-component fiber. The multi-component fiber may also include a sacrificial matrix.
[0140] The thermoplastic polymer core of the multicomponent fiber comprises a thermoplastic polymer.The polymer core of the multicomponent fiber may comprise additives.The thickness of the core of the multicomponent fiber may be comprised between 1 μm and 150 μm.
[0141] The sheath of the multi-component fiber comprises a network of an antioxidant coupling agent and a photocatalyst. Preferably a network of silica and titanium. The surface thickness of the photocatalyst is preferably comprised between 300nm and 20μm. Advantageously, the sheath of the multi-component fiber is at least 50% inorganic, preferably at least 60%, more preferably at least 70%, and even more preferably at least 80%. The sheath of the multi-component fiber may be less than 100% inorganic, for example preferably less than 95%. Advantageously, the inorganic sheath has at least 5% by weight of photocatalyst, preferably at least 10% by weight of photocatalyst, preferably at least 15% by weight of photocatalyst, more preferably at least 20% by weight of photocatalyst and even more preferably at least 25% of photocatalyst. For example, preferably after removing the organic polymer from the reactive mixture, the inorganic sheath has less than 95% by weight of photocatalyst, preferably less than 90% by weight of photocatalyst and more preferably less than 85% by weight of photocatalyst. The thickness of the sheath of the multi-component fiber may be comprised between 300nm and 20μm. The photocatalytic multi-component fiber according to the present invention has a thickness, preferably a diameter, of less than or equal to 150 μm, preferably less than or equal to 100 μm, more preferably less than or equal to 50 μm, even more preferably less than or equal to 10 μm. For example, the photocatalytic multi-component fiber has a thickness, preferably a diameter, of at least 1 μm.
[0142] Preferably, the multicomponent fibers have a predominantly inorganic surface thickness greater than or equal to 500 nm.
[0143] The multicomponent fiber has a surface. Preferably, the surface of the multicomponent fiber is uniform in composition (for energy dispersive X-ray MEB / EDX). Preferably, after treatment, the multicomponent fiber is porous with a surface area of at least 10 m 2 The multicomponent fibers may have a specific surface area of up to 500 m / g (measured by BET analysis). 2 / g specific surface area. Preferably, the multi-component fiber may have a surface area of 2 / g and 500m 2 / g specific surface area.
[0144] According to another aspect, the present invention relates to a textile comprising at least one photocatalytic multicomponent fiber according to the present invention.
[0145] The textile according to the invention may correspond to textiles that can be used in all sectors, such as clothing, furnishing or the industrial sector. They can be used in water and / or air treatment methods, in particular for water and / or air purification via photocatalysis, or for their antimicrobial and self-cleaning properties. Such textiles can be involved in the destruction of preferably volatile organic compounds.
[0146] Advantageously, the textile according to the invention is deformable in order to have different geometries. Thus, the textile according to the invention is flexible, in particular before the step of eliminating at least one polymer, preferably organic, on the surface. The deformation may be by folding, twisting, twisting without breaking or losing photocatalytic efficiency. Thus, the filter according to the invention has an increased efficiency and photocatalytic capacity.
[0147] According to another aspect, the invention relates to a filter comprising at least one textile according to the invention.
[0148] According to another aspect, the present invention relates to a photocatalytic fluid purifier, comprising at least one filter according to the present invention. The fluid may be, for example, air or water, preferably air. Preferably, the filter is arranged between a fluid inlet and a fluid outlet of the purifier.
[0149] The purifier may also include a ventilation system.
[0150] The ventilation system may be arranged to transport a fluid from the inlet of the purifier to the outlet of the purifier. The ventilation system is particularly arranged to generate an air flow through the filter according to the present invention. The ventilation system may, for example, comprise at least one ventilator, the ventilator being equipped with one or more propellers, blades and / or turbines that may be arranged at different positions. Preferably, the ventilation system is arranged so that the air flow (preferably filtered) leaving the purifier contains a reduced level of VOCs, allergens, pollutants and / or pathogens compared to the air entering the purifier. Advantageously, the speed of the ventilation system may be adjusted. Therefore, different power levels of the purifier may be defined. This allows, for example, in the case of severe pollution, to increase the power of the purifier without it running continuously at maximum power.
[0151] The purifier may also include an illumination system.
[0152] The irradiation system preferably comprises an ultraviolet irradiation system capable of irradiating at least one filter according to the invention. Preferably, the wavelength of the irradiation system is comprised in the range of UVA, UVB and / or UVC, that is to say 100nm to 400nm. Advantageously, the irradiation system may be focused on one or more bands, for example 100nm to 280nm, 280nm to 320nm, 320nm to 400nm or any other band allowing the concentration of UVA and UVB, or UVB and UVC, or any other combination between UVA, UVB, UVC, the UV radiation allowing the activation of the photocatalyst. For example, the irradiation system may comprise a UV lamp.
[0153] The purifier may include one or more sensors. For example, it may be a pressure sensor, a pollution sensor, a temperature sensor, a particle detection sensor, a concentration sensor, a consumption sensor, and an obstruction sensor.
[0154] The purifier may include a processing module configured to adjust the speed of the ventilation system and / or the intensity of the illumination system.
[0155] The purifier may include a communication module configured to communicate between the sensor and the ventilation and / or illumination system via a communication network. For example, the communication module may be configured to transmit information containing at least one indication of: a measured pressure difference, a filter blockage level, an indication of a contamination level, an indication of a decontamination level, a type of particles detected, an abnormal increase in temperature within the purifier, and / or an abnormal current consumption by the purifier.
[0156] Example
[0157] Components
[0158] Thermoplastic polymer of carrier mixture: Polypropylene
[0159] Reactive mixture of organic polymers: Polypropylene
[0160] Photocatalyst: TiO2 40%, crystalline form: mixture of anatase and rutile
[0161] Coupling agent: polysiloxane
[0162] Mixing
[0163] Compounding is carried out using a co-kneader with mixing capabilities. It can be a single-screw co-kneader driven by rotation and translation motion, or a twin-screw co-kneader.
[0164] The co-blender may include multiple (gravimetric and / or volumetric) dispensers and one or more heating zones.
[0165] The polymer, coupling agent and possible additives of the active mixture are introduced into a blending kneader using a hopper and produce a dry mixture. The photocatalyst is introduced using a gravimetric dispenser and a transverse feed device to ensure that the photocatalyst is incorporated in the molten state.
[0166] Fill the second weight dispenser with the active mix.
[0167] The carrier mixture is also produced using single-screw or twin-screw extruders.
[0168] The mixing is carried out at a temperature comprised between 150 and 300°C.
[0169] Spinning
[0170] At the mixture end, the spinning step is carried out using conveyor belts and spools. The speed of each extruder allows to vary the polymer ratio of the carrier mixture / polymer of the active mixture.
[0171] The mechanical characterization of the fibers was carried out according to standard ISO 5079.
[0172] like Figure 3 As shown in , the photocatalytic multicomponent fibers according to the invention are much more homogeneous in composition, carry more photocatalyst, and have fewer aggregates (MEB). They can therefore provide more active material, even in the case of a sheath fraction greater than 25%. Moreover, their diameter decreases with the presence of a drawing step while maintaining good mechanical properties. In fact, the fibers are more flexible and more resistant while having a diameter less than 150 μm.
[0173] Furthermore, when the fabrication method includes a preliminary step of grafting the photocatalyst via a coupling agent, the draw ratio is optimized (8 vs. 6), and the diameter is also reduced.
[0174] The photocatalytic multi-component fiber according to the present invention has improved mechanical properties. The multi-component fiber has optimized flexibility and improved ductility.
[0175] [Table 1]
[0176]
[0177] The present invention may be the subject of many variations and applications other than those described above. In particular, unless otherwise indicated, the different structural and functional characteristics of each of the embodiments described above should not be considered as combined and / or closely and / or inseparably related to each other, but rather as simple juxtapositions. Furthermore, the structural and / or functional characteristics of the different embodiments described above may be the subject of any different juxtapositions or any different combinations, in whole or in part.
Claims
1. A method (100) for making a photocatalytic multi-component fiber, comprising the steps of: - providing a carrier mixture (110), said carrier mixture comprising at least one thermoplastic polymer or a thermoplastic polymer precursor; - providing a reactive mixture (120), the reactive mixture comprising: o at least one organic polymer or organic polymer precursor, o at least one photocatalyst in a concentration of at least 10% by weight relative to the weight of the active mixture, o at least one antioxidant coupling agent, preferably a silane; or an antioxidant coupling agent precursor, - spinning (130) a multicomponent fiber from the carrier and the reactive mixture; - eliminating (160) said at least one organic polymer on the surface of said multi-component fiber so as to produce a photocatalytic multi-component fiber.
2. The method (100) for manufacturing a photocatalytic multi-component fiber according to claim 1 is characterized in that the elimination of at least one organic polymer on the surface of the multi-component fiber includes surface calcination to generate an inorganic surface in contact with a thermoplastic polymer carrier.
3. Method (100) for manufacturing a photocatalytic multicomponent fiber according to claim 1 or 2, characterized in that the thermoplastic polymer of the support mixture is selected from thermoplastic polymers having a melting temperature comprised between 100°C and 350°C.
4. The method (100) for producing a photocatalytic multicomponent fiber according to one of the preceding claims, characterized in that it comprises extrusion and / or coextrusion of the carrier mixture and / or the active mixture.
5. The method (100) for producing a photocatalytic multicomponent fiber according to one of the preceding claims, characterized in that, during spinning, the multicomponent fiber has a photocatalytic multicomponent fiber having ... 2 The calculated sheath ratio was comprised between 5% and 50%.
6. Photocatalytic multi-component fibers, comprising: - a thermoplastic polymer carrier, and - Inorganic surfaces; The thermoplastic polymer support includes at least one thermoplastic polymer, and the inorganic surface includes a network of an oxidation resistant coupling agent and a photocatalyst.
7. Photocatalytic multicomponent fiber according to claim 6, characterized in that it has a diameter less than or equal to 150 μm.
8. Photocatalytic multicomponent fiber according to claim 6 or 7, characterized in that it has an inorganic surface with a thickness of at least 500 nm.
9. Textile comprising at least one photocatalytic multicomponent fiber according to one of claims 6 to 8.
10. Filter comprising at least one textile according to claim 9.
11. A photocatalytic air purifier provided with at least one filter according to claim 10, a ventilation system and a UV irradiation system capable of irradiating at least one filter; the ventilator being arranged to transport air from an inlet of the purification system through the filter to an outlet of the purification system.