Aerosol generating device, preparation method thereof and aerosol generating system
By coating porous particulate material on the inside of the wrapping material of the aerosol generator and loading amino acids, the problem of high glycidol release in the heating and non-combust cigarettes is solved, significantly reducing the release of harmful substances and improving the safety of tobacco products and healthy.
Patent Information
- Application Number
- CN202411123914.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-05
AI Technical Summary
The release of glycidol in the aerosol generator for heating and non-combust cigarettes is relatively high, which affects the safety and health of tobacco products.
在气溶胶发生装置的包裹材料内侧涂覆多孔颗粒材料,并在多孔颗粒材料中负载氨基酸,增大气溶胶基质与侧壁间隙,提高有害物质的吸附效率,降低缩水甘油的释放量。
It effectively reduces the release of glycidol in heated and non-combust cigarettes, and improves the safety and health of tobacco products.
Smart Images

Figure CN118892224A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of aerosol generating devices, and in particular to an aerosol generating device and a preparation method thereof, and an aerosol generating system. Background Art
[0002] An aerosol generating device is a device that can convert liquid or solid substances into aerosols. It can be applied to tobacco products to heat tobacco using a heating device to generate an aerosol form of tobacco.
[0003] Heat-not-burn cigarettes are a new type of tobacco product containing an aerosol matrix, and their heating temperature is much lower than the burning temperature of traditional cigarettes. Heat-not-burn cigarettes produce fewer harmful ingredients, so they have developed rapidly in recent years.
[0004] In order to pursue a strong smoking effect, it is usually necessary to add glycerin or a mixed solvent containing glycerin as a smoking agent in the aerosol matrix of heat-not-burn cigarettes, and its mass content is usually between 20% and 50%. When heated, glycerin will release harmful substances such as glycidol (propylene oxide), and the amount released can be more than three times that of traditional cigarettes.
[0005] Therefore, it is necessary to improve the traditional technology to reduce the release of glycidol in the aerosol generated by aerosol generating devices such as heat-not-burn cigarettes. Summary of the invention
[0006] Based on this, one or more embodiments of the present application provide an aerosol generating device and a preparation method thereof, and an aerosol generating system that can reduce the amount of glycidol released.
[0007] According to a first aspect of an embodiment of the present application, an aerosol generating device is provided, comprising a wrapping material, a composite layer, a filter body, a hollow device and an aerosol matrix; the wrapping material is wrapped around the outside of the aerosol matrix; the composite layer is located between the aerosol matrix and the wrapping material;
[0008] The components of the composite layer include composite particles, and the composite particles include porous particle materials and amino acids loaded in the porous particle materials.
[0009] In one embodiment, the loading amount of the amino acid is 0.5 wt % to 10 wt % based on the weight of the composite particles.
[0010] In one embodiment, the loading amount of the amino acid is 1 wt% to 5 wt% based on the weight of the composite particles.
[0011] In one embodiment, the amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
[0012] In one embodiment, the amino acid is selected from lysine and threonine.
[0013] In one embodiment, the weight ratio of the lysine to the threonine is (1-3): (1-3).
[0014] In one embodiment, the porous granular material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves.
[0015] In one embodiment, the natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
[0016] In one embodiment, the particle size of the porous granular material is 0.045 mm to 0.25 mm.
[0017] In one embodiment, the coating amount of the composite particles is 3 g / m 2 ~60g / m 2 .
[0018] In one embodiment, the components of the composite layer further include a binder intermixed with the composite particles.
[0019] In one embodiment, the binder is selected from at least one of gums, cellulose binders, polysaccharides, organic acids and conjugate alkali salts of organic acids.
[0020] In one embodiment, the amount of the binder added is 0.05 wt % to 10 wt % based on the mass of the composite particles.
[0021] According to a second aspect of an embodiment of the present application, there is provided a method for preparing an aerosol generating device as described in any one of the above, comprising the following steps:
[0022] Mixing the composite particles and a solvent to prepare a composite slurry;
[0023] Applying the composite slurry to the side of the packaging material in contact with the aerosol substrate, and drying to form a composite layer; and
[0024] The wrapping material is used to wrap the aerosol matrix, and the side of the wrapping material coated with the composite layer is in contact with the aerosol matrix and covers the outer surface of the aerosol matrix. The filter body, the hollow device and the aerosol matrix are connected in sequence to obtain the aerosol generating device.
[0025] In one embodiment, a method for preparing the composite particles is also provided, comprising the following steps:
[0026] The amino acid and the porous particle material are mixed and dried to obtain the composite particles.
[0027] According to a third aspect of an embodiment of the present application, an aerosol generating system is provided, comprising the aerosol generating device described in any one of the above items and a heating device.
[0028] In one embodiment, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.
[0029] Compared with the traditional technology, this application has the following beneficial effects:
[0030] The present application coats a porous granular material on the inner side of a wrapping material in contact with an aerosol matrix, wherein the granular material forms protrusions on the side walls, thereby increasing the gap between the aerosol matrix and the side walls, thereby improving the efficiency of smoke release from the gap; and by loading amino acids in the porous granular material, the amino acids are able to physically and chemically adsorb harmful substances such as glycidol, thereby reducing the release of harmful substances in aerosols generated by aerosol generating devices such as heat-not-burn cigarettes. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0032] Figure 1 This is a schematic diagram of the longitudinal cross-section structure of an aerosol generating device prepared in one embodiment of the present application;
[0033] Figure 2 This is a schematic diagram of the three-dimensional disassembled structure of an aerosol generating device prepared in one embodiment of the present application;
[0034] Figure 3This is a schematic diagram of the longitudinal section structure of an aerosol generating device prepared in another embodiment of the present application;
[0035] Figure 4 This is a schematic diagram of the longitudinal section structure of an aerosol generating device prepared in another embodiment of the present application;
[0036] Figure 5 This is a schematic diagram of the cross-sectional structure of an aerosol matrix according to one embodiment of the present application.
[0037] Explanation of reference numerals: 10, aerosol matrix; 20, hollow device; 30, filter body; 40, composite layer; 50, wrapping material; 60, connecting material. DETAILED DESCRIPTION
[0038] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.
[0039] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art of the present application. The terms used herein in the specification of the present application are only for the purpose of describing specific embodiments and are not intended to limit the present application. Unless otherwise specifically stated, various raw materials, reagents, instruments and equipment used in the present application, etc. can be purchased from the market or can be prepared by existing methods.
[0040] In this application, "optionally", "optional", and "optional" mean optional or dispensable, that is, any one of the two parallel schemes of "yes" or "no". If multiple "options" appear in a technical solution, unless otherwise specified and there is no contradiction or mutual restriction, each "optional" is independent.
[0041] In the present application, the technical features described in an open manner include closed technical solutions composed of the listed features, and also include open technical solutions containing the listed features.
[0042] In a first aspect of the present application, an aerosol generating device is provided.
[0043] In such Figure 1 and Figure 2In the example shown, the aerosol generating device includes a wrapping material 50, a composite layer 40, a filter body 30, a hollow device 20 and an aerosol matrix 10; the wrapping material 50 is wrapped around the outside of the aerosol matrix 10; the composite layer 40 is located between the aerosol matrix 10 and the wrapping material 50;
[0044] The components of the composite layer 40 include composite particles, and the composite particles include a porous particle material and amino acids loaded in the porous particle material.
[0045] It is understandable that the filter body in the present application may include a filter segment and may also include a molded paper that wraps the filter segment.
[0046] In some of the embodiments, the aerosol generating device may be a heat-not-burn cigarette, but is not limited thereto.
[0047] It should be noted that Figure 2 The middle wrapping material layer 50 and the particle layer 40 are both in an unfolded state.
[0048] like Figure 3 As shown, in some embodiments, the aerosol generating device further comprises a tipping material 60, and the tipping material 60 is wrapped around the outer sides of the filter body, the hollow device and the aerosol matrix which are connected in sequence.
[0049] like Figure 4 As shown, the tipping material 60 may also be wrapped around the outer sides of the filter body 30 , the hollow device 20 , and a portion of the aerosol matrix 10 connected to the hollow device 20 , which are connected in sequence.
[0050] Figure 5 It is a cross-sectional schematic diagram of the positional relationship between the aerosol matrix 10, the composite layer 40 and the wrapping material 50; the inner side of the wrapping material 50 in contact with the aerosol matrix 10 is coated with composite particles to form the composite layer 40, thereby enhancing the adsorption of harmful substances such as glycidol and reducing the release of harmful substances in the aerosol.
[0051] In some embodiments, the wrapping material 50 is selected from cigarette paper.
[0052] In some embodiments, the amino acid loading is 0.5 wt% to 10 wt% based on the weight of the composite particles, for example, 0.5 wt%, 1 wt%, 1.5 wt%, 2 wt%, 2.5 wt%, 3 wt%, 3.5 wt%, 4 wt%, 4.5 wt%, 5 wt%, 5.5 wt%, 6 wt%, 6.5 wt%, 7 wt%, 7.5 wt%, 8 wt%, 8.5 wt%, 9 wt%, 9.5 wt% or 10 wt%.
[0053] In some optional examples, the loading amount of amino acids is 1 wt%~5 wt%.
[0054] In some optional examples, the loading amount of amino acids is 2 wt% to 3 wt%.
[0055] In some embodiments, the amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
[0056] In some optional examples, the amino acid is selected from lysine and threonine.
[0057] In some optional examples, the weight ratio of lysine to threonine is (1-3):(1-3), for example, 1:1, 1:2, 1:3, 2:1, 2:3, 3:1 or 3:2.
[0058] Understandably, by loading amino acids in the porous particulate material, the amino acids can physically and chemically adsorb harmful substances such as glycidol, thereby reducing the release of harmful substances in the aerosol of heat-not-burn cigarettes.
[0059] In some embodiments, the porous particulate material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves.
[0060] In some specific examples, the natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin; the metal oxide includes calcium oxide; the hydroxide includes calcium hydroxide; the carbonate includes calcium carbonate; and the sulfate includes calcium sulfate.
[0061] In some optional examples, the porous particulate material is selected from activated carbon or diatomaceous earth.
[0062] In some embodiments, the coating weight of the composite particles is 3 g / m 2 ~60g / m 2 For example, it can be 3g / m 2 , 4g / m 2 , 5g / m 2 , 6g / m 2 , 7g / m 2 , 8g / m 2 , 9g / m 2 , 10g / m 2 , 15g / m 2 , 20g / m 2 , 25g / m 2 , 30g / m2 , 35g / m 2 , 40g / m 2 , 45g / m 2 , 50g / m 2 , 55g / m 2 Or 60g / m 2 .
[0063] In some optional examples, the coating amount of the composite particles is 5 g / m 2 ~50g / m 2 .
[0064] In some optional examples, the coating amount of the composite particles is 8 g / m 2 ~30g / m 2 .
[0065] It is understandable that when the composite is coated on the inner surface of the wrapping material, it may be coated on a partial area of the inner surface of the wrapping material or on the entire area of the inner surface of the wrapping material.
[0066] In one example, the composite is coated on all or part of the inner surface of the packaging material except for the lap joint.
[0067] In some embodiments, the particle size of the porous granular material is 0.045 mm to 0.25 mm, for example, 0.045 mm, 0.055 mm, 0.065 mm, 0.075 mm, 0.085 mm, 0.095 mm, 0.10 mm, 0.11 mm, 0.12 mm, 0.13 mm, 0.14 mm, 0.15 mm, 0.16 mm, 0.17 mm, 0.18 mm, 0.19 mm, 0.20 mm, 0.21 mm, 0.22 mm, 0.23 mm, 0.24 mm, 0.25 mm.
[0068] In some optional examples, the particle size of the porous granular material is 0.075 mm to 0.15 mm.
[0069] It can be understood that porous granular material is coated on the inner surface of the wrapping material, and the granular material forms protrusions on the inner wall, which increases the gap between the aerosol matrix and the side wall, thereby improving the smoke release efficiency and making the heat-not-burn cigarette have good smoke richness and smoke fullness.
[0070] In some embodiments, the components of the composite layer further include a binder intermixed with the composite particles.
[0071] In some embodiments, the binder is selected from at least one of a gum, a cellulose binder, a polysaccharide, an organic acid, and a conjugate base salt of an organic acid.
[0072] In some specific examples, the gum is selected from at least one of guar gum, xanthan gum, gum arabic and locust bean gum; the cellulose binder is selected from at least one of hydroxypropyl cellulose, carboxymethyl cellulose, hydroxyethyl cellulose, methyl cellulose and ethyl cellulose; the polysaccharide is selected from starch; the organic acid is selected from alginic acid; and the conjugate base salt of the organic acid is selected from at least one of sodium alginate, agar and pectin.
[0073] In one embodiment, the amount of binder added is 0.05 wt% to 10 wt% based on the total weight of the composite particles, for example, 0.05 wt%, 0.06 wt%, 0.07 wt%, 0.08 wt%, 0.09 wt%, 0.1 wt%, 0.2 wt%, 0.3 wt%, 0.4 wt%, 0.5 wt%, 0.6 wt%, 0.7 wt%, 0.8 wt%, 0.9 wt%, 1.0 wt%, 2.0 wt%, 3.0 wt%, 4.0 wt%, 5.0 wt%, 6.0 wt%, 7.0 wt%, 8.0 wt%, 9.0 wt% or 10 wt%.
[0074] In some optional examples, the added amount of the binder is 0.5wt%~3wt%.
[0075] The aerosol generating device of the present application has the advantages of less release of harmful substances.
[0076] In a second aspect of the present application, a method for preparing the above-mentioned aerosol generating device is provided, comprising steps S10 to S30:
[0077] Step S10: Mixing composite particles, a binder and a solvent to prepare a composite slurry.
[0078] Step S20: coating the composite slurry onto the side of the packaging material 50 that contacts the aerosol matrix 10, and drying to form a composite layer.
[0079] Step S30: Use a wrapping material 50 to wrap the aerosol matrix 10, and the side of the wrapping material 50 coated with the composite layer 40 contacts the aerosol matrix 10 and covers the outer surface of the aerosol matrix 10, and the filter body 30, the hollow device 20 and the aerosol matrix 10 are connected in sequence to prepare an aerosol generating device.
[0080] In some embodiments, in step S10, the method for preparing the composite particles comprises the following steps: mixing the amino acid and the porous particle material, and drying to obtain the composite particles.
[0081] A third aspect of the present application provides an aerosol generating system, comprising the aerosol generating device of the first aspect and a heating device.
[0082] In one embodiment, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.
[0083] The present application does not impose any particular limitation on the heating component, battery component, control component and housing, and they may be made of materials and in shapes commonly used in the art.
[0084] The aerosol generating system of the present application has the advantages of low release of harmful substances such as glycidol and good safety.
[0085] The present application will be further described below in conjunction with specific examples and comparative examples, but they should not be construed as limiting the scope of protection of the present application. The raw materials involved in the following specific examples, unless otherwise specified, can all be sourced from commercial sources, the instruments used, unless otherwise specified, can all be sourced from commercial sources, and the processes involved, unless otherwise specified, are all conventionally selected by those skilled in the art.
[0086] Embodiment 1:
[0087] (1) Methionine is provided and dissolved in water to obtain a methionine solution, an activated carbon particle material is immersed in the methionine solution, and the activated carbon particle material is dried at 100° C. to obtain composite particles (i.e., activated carbon particle material loaded with methionine). The loading amount of methionine is 4 wt % based on the total weight of the composite particles.
[0088] (2) Mixing the activated carbon particles loaded with methionine with a binder (carboxymethyl cellulose) to obtain a composite. The amount of the binder added is 2 wt % based on the total weight of the composite particles.
[0089] (3) The composite material is uniformly coated on the surface of the aerosol matrix section of the cigarette paper; the side coated with the composite material is brought into contact with the aerosol matrix (comprising reconstituted tobacco leaves, 20 wt% glycerin and flavoring substances), and the filter body, hollow device and aerosol matrix connected in sequence are wrapped with tipping paper to obtain a heat-not-burn cigarette. The coating amount of the composite particles on the inner surface of the cigarette paper is 40 g / m 2 .
[0090] Embodiment 2:
[0091] The same as Example 1, except that the methionine with a loading amount of 4 wt% was replaced by threonine with a loading amount of 5 wt%, and the coating amount of the composite particles on the inner surface of the cigarette paper was 30 g / m 2 .
[0092] Embodiment 3:
[0093] The method is basically the same as Example 1, except that the methionine with a loading amount of 4 wt% is replaced by lysine with a loading amount of 1 wt%, and the coating amount of the composite particles on the inner surface of the cigarette paper is 8 g / m 2 .
[0094] Embodiment 4:
[0095] The method is basically the same as Example 1, except that the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 1:1), and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0096] Embodiment 5:
[0097] The method is basically the same as Example 1, except that the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 2:1), and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0098] Embodiment 6:
[0099] The method is basically the same as Example 1, except that the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 1:2), and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0100] Embodiment 7:
[0101] The method is basically the same as Example 1, except that the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 3:1), and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0102] Embodiment 8:
[0103] The method is basically the same as Example 1, except that the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 1:3), and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0104] Embodiment 9:
[0105] The method is basically the same as Example 1, except that the methionine with a loading amount of 4 wt% is replaced by lysine with a loading amount of 3 wt%, and the coating amount of the composite particles on the inner surface of the cigarette paper is 15 g / m 2 .
[0106] Embodiment 10:
[0107] The same as Example 1, except that the methionine with a loading amount of 4 wt% was replaced by threonine with a loading amount of 3 wt%, and the coating amount of the composite particles on the inner surface of the cigarette paper was 15 g / m 2 .
[0108] Embodiment 11:
[0109] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by glycine with a loading amount of 0.5wt%; the activated carbon is replaced by montmorillonite, and the coating amount of the composite particles on the inner surface of the cigarette paper is 3g / m 2 .
[0110] Embodiment 12:
[0111] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by tyrosine with a loading amount of 10wt%; the activated carbon is replaced by sepiolite, and the coating amount of the composite particles on the inner surface of the cigarette paper is 60g / m 2 .
[0112] Embodiment 13:
[0113] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by tryptophan with a loading amount of 5wt%; the activated carbon is replaced by kaolin, and the coating amount of the composite particles on the inner surface of the cigarette paper is 50g / m 2 .
[0114] Embodiment 14:
[0115] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by serine with a loading amount of 8wt%; the activated carbon is replaced by diatomaceous earth, and the coating amount of the composite particles on the inner surface of the cigarette paper is 10g / m 2 .
[0116] Embodiment 15:
[0117] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by lysine with a loading amount of 5wt%; the activated carbon is replaced by diatomaceous earth, and the coating amount of the composite particles on the inner surface of the cigarette paper is 15g / m 2 .
[0118] Embodiment 16:
[0119] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by the threonine with a loading amount of 1wt%; the activated carbon is replaced by diatomaceous earth, and the coating amount of the composite particles on the inner surface of the cigarette paper is 30g / m 2 .
[0120] Embodiment 17:
[0121] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 1:1); the activated carbon is replaced by diatomaceous earth, and the coating amount of the composite particles on the inner surface of the cigarette paper is 20g / m 2 .
[0122] Embodiment 18:
[0123] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by an amino acid mixture with a loading amount of 3wt% (a mixture of lysine and threonine with a mass ratio of 1:1); the activated carbon is replaced by alumina, and the coating amount of the composite particles on the inner surface of the cigarette paper is 30g / m 2 .
[0124] Embodiment 19:
[0125] The method is basically the same as Example 1, except that: the methionine with a loading amount of 4wt% is replaced by arginine with a loading amount of 2wt%; the activated carbon is replaced by ZSM-5 molecular sieve, and the coating amount of the composite particles on the inner surface of the cigarette paper is 30g / m 2 .
[0126] Comparative Example 1:
[0127] (1) Mixing activated carbon particles with a binder (carboxymethyl cellulose) to obtain a composite. The amount of the binder added is 2 wt % based on the total weight of the activated carbon particles.
[0128] (2) The composite material is uniformly coated on the inner surface of the aerosol matrix section of the cigarette paper; the side coated with the composite material is in contact with the aerosol matrix, and the filter body, the hollow device and the aerosol matrix connected in sequence are wrapped with a tipping paper to obtain a heat-not-burn cigarette. The coating amount of the granular material on the inner surface of the cigarette paper is 20 g / m 2 .
[0129] Comparative Example 2:
[0130] The same as comparative example 1, except that the activated carbon was replaced with diatomaceous earth, and the coating amount of the granular material on the inner surface of the cigarette paper was 30 g / m2 .
[0131] The parameters for preparing the heat-not-burn cigarettes in the above-mentioned Examples 1-19 and Comparative Examples 1-2 are shown in Table 1 below; and the GC-MS method described in the literature (Chen X, Bailey PC, Yang C, et al. Targeted characterization of the chemical composition of JUUL systems aerosol and comparison with 3R4Freference cigarettes and IQOS heat sticks[J]. Separations, 2021, 8(10): 168.) was used to test the glycidol content released by the above-mentioned embodiments, comparative examples and control samples (the control sample is a heat-not-burn cigarette in which composite particles are not coated between the aerosol matrix and the wrapping material), and the results are shown in Table 1.
[0132] The central heating method is adopted, and the heating temperature setting value is 310℃; a linear smoking machine is used to smoke heat-not-burn cigarettes, and the cigarette smoking parameters are: smoking volume is 55mL; smoking time is 2s; smoking interval is 30s; number of puffs is 8 times; preheating time is 18s; the smoking curve is bell-shaped.
[0133] Table 1
[0134]
[0135] As can be seen from the above table, the heat-not-burn cigarettes prepared by the specific method of the present application have a significantly reduced release of glycidol. In Comparative Examples 1 and 2, the inner wall in contact with the aerosol matrix is coated with a porous granular material, but the porous granular material is not loaded with amino acids. Although the glycidol content released by the heat-not-burn cigarettes finally prepared is lower than that of the control sample, the improvement effect is worse than that of the examples of the present application.
[0136] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0137] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.
Claims
1. An aerosol generating device, characterized in that: It comprises a wrapping material, a composite layer, a filter body, a hollow device and an aerosol matrix; the wrapping material is wrapped around the outside of the aerosol matrix; the composite layer is located between the aerosol matrix and the wrapping material; The components of the composite layer include composite particles, and the composite particles include porous particle materials and amino acids loaded in the porous particle materials.
2. The aerosol generating device according to claim 1, characterized in that: Based on the weight of the composite particles, the loading amount of the amino acid is 0.5wt%~10wt%.
3. The aerosol generating device according to claim 2, characterized in that: Based on the weight of the composite particles, the loading amount of the amino acid is 1 wt% to 5 wt%.
4. The aerosol generating device according to claim 1, characterized in that: The amino acid is selected from at least one of glycine, alanine, valine, leucine, isoleucine, phenylalanine, tryptophan, tyrosine, aspartic acid, asparagine, glutamic acid, lysine, glutamine, serine, threonine, cysteine, proline, histidine, arginine and methionine.
5. The aerosol generating device according to claim 4, characterized in that: The amino acid is selected from lysine and threonine.
6. The aerosol generating device according to claim 5, characterized in that: The weight ratio of the lysine to the threonine is (1-3): (1-3).
7. The aerosol generating device according to any one of claims 1 to 6, characterized in that: The porous particle material is selected from at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon and molecular sieves.
8. The aerosol generating device according to claim 7, characterized in that: The natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
9. The aerosol generating device according to any one of claims 1 to 6 and 8, characterized in that: The particle size of the porous granular material is 0.045 mm to 0.25 mm.
10. The aerosol generating device according to any one of claims 1 to 6 and 8, characterized in that: The coating amount of the composite particles is 3 g / m 2 ~60g / m 2 .
11. The aerosol generating device according to any one of claims 1 to 6 and 8, characterized in that: The components of the composite layer also include a binder intermixed with the composite particles.
12. The aerosol generating device according to claim 11, characterized in that: The binder is selected from at least one of gums, cellulose binders, polysaccharides, organic acids and conjugate alkali salts of organic acids.
13. The aerosol generating device according to claim 11, characterized in that: The amount of the binder added is 0.05wt% to 10wt% based on the mass of the composite particles.
14. A method for preparing an aerosol generating device according to any one of claims 1 to 13, characterized in that: The steps include: Mixing the composite particles and a solvent to prepare a composite slurry; Applying the composite slurry to the side of the packaging material in contact with the aerosol substrate, and drying to form a composite layer; and The wrapping material is used to wrap the aerosol matrix, and the side of the wrapping material coated with the composite layer is in contact with the aerosol matrix and covers the outer surface of the aerosol matrix. The filter body, the hollow device and the aerosol matrix are connected in sequence to obtain the aerosol generating device.
15. The method for preparing an aerosol generating device according to claim 14, characterized in that: Also included is a method for preparing the composite particles, comprising the following steps: The amino acid and the porous particle material are mixed and dried to obtain the composite particles.
16. An aerosol generating system, characterized in that: It comprises the aerosol generating device and heating device as described in any one of claims 1 to 13.
17. The aerosol generating system according to claim 16, characterized in that: The heating device comprises a heating component, a battery component for supplying power to the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component and the control component.
Citation Information
Patent Citations
Complex adsorbent capable of reducing release amount of heavy metals in mainstream smoke of cigarettes, preparation method for complex adsorbent and application of complex adsorbent
CN102499479A
Composite paper and aerosol generating product comprising same
CN116420909A
Smoking Article Filter
US20090288671A1