Equipment and method for preparing regenerated artificial composite fiberboard

By designing recycled artificial composite fiberboard preparation equipment, using uniform cutting, deep woven and hot pressing treatment, the problems of environmental pollution and low utilization rate of waste furniture boards are solved, and efficient and environmentally friendly recycled artificial board production is achieved, which has improved the Performance and durability.

CN118893682AActive Publication Date: 2024-11-05HUNAN SANGYUAN HOME FURNISHING CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411066436.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-11-05
Estimated Expiration
2044-08-05

AI Technical Summary

Technical Problem

In the prior art, when dealing with waste furniture boards, chemical or heat treatment leads to environmental pollution, and the renovation and reuse utilization rate of solid wood materials is not high, and the size and specifications vary greatly, making it difficult to effectively recycle and utilize it.

Method used

A recycled artificial composite fiberboard preparation equipment is designed, including housing components, conveying components, pore-breathing components, cutting components and wool-beating components. Recycled artificial boards are formed through uniform cutting, deep wool-beating, glue-applying and hot pressing treatment. Three-step wooling method and the upper and lower panels of thermoplastic polyolefin waterproof coils are used to ensure uniform wooling effect, waterproof performance and durability.

Benefits of technology

It realizes the recycling and utilization of used furniture boards with green and environmental protection, improves the performance and durability of recycled artificial boards, reduces production costs, avoids environmental pollution, is highly applicable, and the size of recycled artificial boards is flexible.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118893682A_ABST
    Figure CN118893682A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of multi-layer regenerated artificial boards, in particular to equipment and a method for preparing a regenerated artificial composite fiberboard. The preparation equipment for the regenerated artificial composite fiberboard comprises a shell assembly, a conveying assembly, a hole dredging assembly, a cutting assembly and a roughening assembly. The invention provides a three-time step-by-step roughening method, so that the roughening effect is more uniform and consistent, the subsequent sizing and hot-pressing combination degree is ensured, the performance and durability of a product are improved, meanwhile, the abrasion of tools such as roughening steel wires is reduced, the loss is reduced, the production cost is reduced, the core material preparation process is physical cutting, no waste gas is discharged, and the method is not limited by material specifications, and is suitable for industrial production. The method has the advantages of high material utilization rate, no special requirements on specifications of raw materials and high applicability, and the boards to be spliced are placed in a crossed manner, the upper panel and the lower panel are subjected to hot-press gluing, so that the roughening effect is more uniform and consistent, the subsequent gluing and hot-press combination degree is ensured, and the performance and durability of the product are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of multi-layer recycled artificial boards, and in particular to a preparation device and method for recycled artificial composite fiber boards. Background Art

[0002] With the rapid development of social economy and the acceleration of urbanization, the amount of waste furniture is increasing. Improper handling of waste furniture will cause serious pollution to the environment and waste resources. It has become an urgent need to seek effective ways to recycle waste furniture panels.

[0003] At present, the main methods for treating waste furniture boards are: 1. Making recycled industrial materials through chemical or thermal treatment. For example, decomposing waste artificial boards into recycled cellulose, lignin, etc., which are used to produce wood products such as paper, fiberboard, particleboard, etc.; 2. Releasing heat energy through incineration. This part of heat energy can be used for energy such as hot water and steam in industrial production, and can also be used for heating and power generation; 3. For solid wood materials, renovation and reuse are usually adopted. However, chemical or thermal treatment methods and incineration will cause greater environmental pollution; and nowadays, the renovation and reuse of solid wood materials has a low utilization rate due to the large differences in the size specifications of solid wood materials. Summary of the invention

[0004] Based on this, it is necessary to provide a device and method for preparing a recycled artificial composite fiberboard to solve at least one technical problem in the background technology.

[0005] A regenerated artificial composite fiberboard preparation device comprises a shell component, a conveying component, a hole-draining component, a cutting component and a roughening component, wherein the shell component comprises a first lateral shell, a second lateral shell, a plurality of connecting cross bars, two inclined strip funnels, two collecting buckets and a top shell component, wherein the bottom of the first lateral shell is placed on one side of an installation ground, the bottom of the second lateral shell is placed on the other side of the installation ground, and the first lateral shell and the second lateral shell are arranged oppositely, one end of a plurality of connecting cross bars is respectively installed on the inner side of the first lateral shell along the length direction, the other ends of a plurality of connecting cross bars are respectively installed on the inner side of the second lateral shell along the length direction, the outer ends of the second lateral shell are respectively provided with funnel passing grooves, the two inclined strip funnels ... The inner ends of the buckets are respectively installed at the two ends of the inner side of the first lateral shell, the outer ends of the two inclined strip funnels are respectively passed through the two funnel through grooves and protruded on the outer side of the second lateral shell, the bottoms of the two collecting buckets are placed on the installation ground adjacent to the side of the second lateral shell, and the two collecting buckets are respectively located directly below the outer ends of the two inclined strip funnels, the top surface of the top shell element is respectively installed on the top of the first lateral shell and the second lateral shell, the conveying assembly is installed at both ends of the first lateral shell and the second lateral shell, the interior of the first lateral shell is hollow to form a first hollow cavity, the interior of the second lateral shell is hollow to form a second hollow cavity, the hole dredging assembly, the cutting assembly and the roughening assembly are all installed in the first hollow cavity and the second hollow cavity.

[0006] As a further improvement of the present invention, a conveying installation groove is recessed at one end of the top surface of the first lateral shell, a first conveying rotation hole is recessed at one end of the top of the inner side of the first hollow cavity and the second hollow cavity adjacent to the conveying installation groove, a second conveying rotation hole is recessed at the other end of the top of the inner side of the first hollow cavity and the second hollow cavity, a first vertical slide groove and a second vertical slide groove are recessed along the length direction of the first lateral shell and the second lateral shell adjacent to one end of the conveying installation groove, the first vertical slide groove is adjacent to the conveying installation groove, the other end of the top of the first lateral shell and the second lateral shell is recessed with a third vertical slide groove, the first hollow cavity and the second Three connecting grooves are recessed in the middle part of the inner side of the hollow cavity, and the three connecting grooves are respectively located directly below the first vertical slide groove, the second vertical slide groove and the third vertical slide groove. A correction wheel is provided on the inner top of the first lateral shell and the second lateral shell away from the conveying installation groove. Two cutting holes are recessed in the inner top of the first hollow cavity and the second hollow cavity along the length direction. The first lateral shell and the second lateral shell are respectively recessed in the inner top with a primary weeding hole, a secondary weeding hole and a roughening hole, and the primary weeding hole is located below the third vertical slide groove, the secondary weeding hole is located below the second vertical slide groove, and the roughening hole is located below the first vertical slide groove.

[0007] As a further improvement of the present invention, the top shell element includes three switch shells, and the bottom surfaces of the three switch shells are respectively installed on the top surfaces of the first lateral shell and the second lateral shell along the length direction on both sides, and each switch shell has a hollow bottom to form a preparation cavity, and the outer sides of the two preparation cavities away from the conveying installation groove are recessed with second strip slide grooves, and the two second strip slide grooves are respectively located directly above the third vertical slide groove and the second vertical slide groove, and each second strip slide groove is slidably provided with a nozzle, the inner end of the nozzle is located in the preparation cavity, and the outer end of the nozzle is connected to the external softener conveying equipment.

[0008] As a further improvement of the present invention, the conveying assembly includes a feed roller, a feed motor, an output roller and an output motor. The two ends of the feed roller are respectively rotatably installed in the two second conveying rotary holes, the feed motor is installed in the second hollow cavity away from the conveying mounting groove, and the output shaft of the feed motor is connected to the feed roller, the two ends of the output roller are respectively rotatably installed in the two first conveying rotary holes, the output motor is installed in the conveying mounting groove, and the output shaft of the output motor is connected to one end of the output roller.

[0009] As a further improvement of the present invention, the hole-clearing assembly includes two hole-clearing adjustment elements, two primary rollers and two secondary rollers. The two hole-clearing adjustment elements are symmetrically installed at the two ends of the first hollow cavity and the second hollow cavity, one of the primary rollers is installed in the hole-clearing adjustment element away from the conveying installation groove, and the other first roller is rotatably installed in the two primary hole-clearing holes at both ends, one of the secondary rollers is installed in the other hole-clearing adjustment element, and the other secondary roller is rotatably installed in the secondary hole-clearing holes at both ends.

[0010] As a further improvement of the present invention, each sparse hole adjustment element includes a first lifting motor, two displacement mounting shells, a lifting synchronous shaft, two vertical mounting slide rails, two vertical sliding tables, two sparse hole mounting turntables, a sparse hole driving motor, two lateral sliding tables, two sliding turntables, a coating roller, a coating driving motor and two synchronous lateral moving motors. The first lifting motor is installed at one end of the bottom of the first hollow cavity, and the two displacement mounting shells are respectively installed in two connecting grooves away from the conveying mounting groove or two connecting grooves adjacent to the cutting turn hole. Each displacement mounting shell is hollow inside to form a rotating mounting cavity, and the displacement mounting shell A lifting synchronous rotating hole is recessed at one end of the side wall, and the lifting synchronous rotating hole is connected to the rotating installation cavity. A worm is rotatably arranged in the rotating installation cavity. Both ends of the lifting synchronous shaft are rotatably installed in the two lifting synchronous rotating holes, and one end of the lifting synchronous shaft is connected to the output shaft of the first lifting motor. Turbines are respectively arranged at both ends of the lifting synchronous shaft, and the two turbines are respectively meshed with the two worms. The inner sides of the two vertical installation slide rails are respectively installed in the first hollow cavity or the second hollow cavity, and the two vertical installation slide rails are respectively located directly above the two displacement installation shells, and the inner sides of the two vertical sliding platforms are respectively slidably installed on the outer sides of the two vertical installation slide rails. , an adjusting thread groove is concavely provided in the middle of the bottom surface of each vertical sliding table, the top ends of the two worm gears are rotatably installed in the two adjusting thread grooves respectively, and the top ends of the two vertical sliding tables are respectively penetrated through two third vertical slide grooves or two second vertical slide grooves and convexly arranged in the preparation cavity, the bottom surfaces of the two sparse hole mounting turntables are respectively mounted on one end of the top surfaces of the two vertical sliding tables, the inner sides of the two sparse hole mounting turntables are respectively rotatably connected with the two ends of the primary roller or the two ends of the secondary roller, the sparse hole driving motor is installed on the outer side of one of the sparse hole mounting turntables, and the output shaft of the sparse hole driving motor is connected with one end of the primary roller or one end of the secondary roller, the two The bottom of each lateral sliding platform is respectively installed in the middle of the top surface of the two vertical sliding platforms, the two sliding turn blocks are respectively slidably installed in the two lateral sliding platforms, the two ends of the coating roller are respectively rotatably installed in the two lateral sliding platforms, the coating drive motor is installed in one of the lateral sliding platforms, and the output shaft of the coating drive motor is connected to one end of the coating roller, one of the lateral sliding platforms is recessed with a nozzle mounting hole on the top, and the inner end of the nozzle is installed in the nozzle mounting hole, the two synchronous lateral moving motors are respectively installed on the top surfaces of the two vertical sliding platforms away from one end of the sparse hole mounting turntable, and the output shafts of the two synchronous lateral moving motors are respectively connected to the two lateral sliding platforms.

[0011] As a further improvement of the present invention, the cutting assembly includes a cutting mounting plate, two cutting shafts, two cutting motors and two blade groups. The two sides of the cutting mounting plate are respectively installed in the middle of the top surface of the first lateral outer shell and the middle of the top surface of the second lateral outer shell. The top surface array of the cutting mounting plate is concavely provided with a plurality of cutting grooves. The two ends of the two cutting shafts are respectively rotatably installed in four cutting rotary holes. The two cutting motors are respectively installed on the top of the second hollow cavity, and the output shafts of the two cutting motors are respectively connected to one end of the two cutting shafts. The two blade groups are respectively installed in the two cutting shafts. Each blade group is composed of a plurality of cutting blades. The plurality of cutting blades are installed in the cutting shaft at intervals along the length direction, and the top of the cutting blade passes through the cutting groove and is located in the preparation cavity.

[0012] As a further improvement of the present invention, the roughening assembly includes a roughening drive element and two roughening rollers. The roughening drive elements are respectively installed at one end of the first hollow cavity and the second hollow cavity adjacent to the conveying mounting groove. One of the roughening rollers is rotatably installed in the roughening drive element, and the other roughening roller is rotatably installed at both ends in the two roughening rotating holes.

[0013] As a further improvement of the present invention, the roughening drive element includes a second lifting motor, two displacement shells, a roughening lifting shaft, two roughening vertical slide rails, two roughening vertical slides, two roughening horizontal slides, two roughening horizontal rotating blocks, a roughening drive motor, a scraper shaft, a scraper motor and a burr scraper. The second lifting motor is installed at one end of the bottom of the first hollow cavity, and the two displacement shells are respectively installed at two connecting grooves adjacent to the conveying installation groove. A rotating cavity is formed in the interior of each displacement installation shell, and a roughening is recessed at one end of the side wall of the displacement installation shell. The lifting and lowering rotary hole, a roughing worm is rotatably arranged in the displacement mounting shell, the two ends of the roughing lifting shaft are respectively rotatably installed in the two roughing lifting and lowering rotary holes, one end of the roughing lifting shaft is connected to the output shaft of the second lifting motor, and roughing turbines are respectively arranged at both ends of the roughing lifting shaft, and the two roughing turbines are respectively meshed and connected with the two roughing worms, the inner sides of the two roughing vertical slide rails are respectively installed in the first hollow cavity or the second hollow cavity, and the two roughing vertical slide rails are respectively located directly above the two displacement shells, and the inner sides of the two roughing vertical slide tables are respectively slidably installed on the two On the outside of the roughening vertical slide rail, a roughening thread groove is concavely provided in the middle of the bottom surface of each roughening vertical slide table, the top ends of the two roughening worms are respectively rotatably installed in the two roughening thread grooves, and the top ends of the two vertical sliding tables are respectively penetrated through the two first vertical slide grooves and convexly arranged in the preparation cavity, the bottom surfaces of the two roughening transverse slide tables are respectively installed on the top surfaces of the two vertical sliding tables, the two roughening transverse rotating blocks are respectively slidably installed in the two roughening transverse slide tables, the roughening drive motor is installed on the outside of one of the roughening transverse rotating blocks, and the two ends of the roughening roller are respectively rotatably installed on the two In the roughening transverse slide, the output shaft of the roughening drive motor is connected to one end of the roughening roller, and a roughening transverse adjustment motor is convexly provided at one end of each roughening transverse rotating block, and the roughening transverse adjustment motor is connected to the top of the two vertical sliding tables, and a scraper mounting rotating hole is recessed at one end of the top of the side wall of each roughening transverse rotating block. The scraper motor is installed on the outer top of one of the roughening transverse slides, and the two ends of the scraper rotating shaft are rotatably installed in the two scraper mounting rotating holes, and the output shaft of the scraper motor is connected to one end of the scraper rotating shaft, and the burr scraper is installed in the scraper rotating shaft.

[0014] A method for preparing a regenerated man-made composite fiberboard is provided, which is applied to the above-mentioned regenerated man-made composite fiberboard preparation device, and the preparation method comprises:

[0015] Step S1: placing the waste furniture boards in a regenerated man-made composite fiberboard preparation device, cutting the waste furniture boards into equal widths, and performing deep roughening on the upper and lower surfaces of the waste furniture boards to form boards to be assembled;

[0016] Step S2: gluing the boards to be assembled and staggeredly laying them to form core materials;

[0017] Step S3: a lower panel is arranged on the bottom surface of the core material, and an upper panel is arranged on the top surface of the core material to form a sheet to be formed;

[0018] Step S4: placing the sheet to be formed in a hot pressing device for hot pressing treatment to form a recycled artificial board.

[0019] The beneficial effects of the present invention are as follows:

[0020] 1. The present invention provides a three-step roughening method: the thorn-like protrusions on the first-level roller arranged in two directions form sparse roughening holes, the thorn-like protrusions on the second-level roller form dense roughening holes, and the roughening wires on the roughening rollers form deeply roughened strip plates, ensuring that the roughening effect is more uniform and consistent, ensuring the degree of subsequent gluing and hot pressing bonding, improving the performance and durability of the product, and at the same time, reducing the wear of tools such as the roughening wire, reducing losses, and reducing production costs. In addition, the upper panel and the lower panel made of thermoplastic polyolefin waterproof coiled material can effectively prevent moisture from penetrating into the interior of the recycled artificial board, improve the waterproof performance of the recycled artificial board, avoid deformation and rot of the board due to moisture, and at the same time improve its wear resistance, which can protect the surface of the recycled artificial board from damage such as scratches and abrasion, and extend the service life of the board.

[0021] 2. The processing of the present invention is green and environmentally friendly. The core material preparation process is physical cutting, no waste gas is emitted, and it is not limited by material specifications. The material utilization rate is high, there are no special requirements for raw material specifications, and it has strong applicability.

[0022] 3. The performance of the recycled artificial board produced by the present invention is better than that of the original waste furniture board. By placing the boards to be assembled crosswise, hot-pressing and gluing the upper and lower panels, and ensuring that the roughening effect is more uniform and consistent, the subsequent gluing and hot-pressing bonding degree is guaranteed, the performance and durability of the product are improved, the physical properties are enhanced, and the size of the recycled artificial board is regular, which can be flexibly adjusted according to production requirements.

[0023] 4. The present invention can achieve roughening treatment of different depths and densities, ensuring the controllability and consistency of the roughening depth, and can avoid the deviation and vibration of the board during roughening, ensuring the stability of the roughening process and the accuracy of cutting. The roughening wire is automatically cleaned during the roughening process to maintain the roughening effect of the roughening wire, extend the service life of the tool, and reduce maintenance work. At the same time, a water mist curtain is sprayed to prevent the splashing of wood chips generated during the cutting process from affecting the roughening effect, and at the same time soften the surface of the board, so that the subsequent roughening process is smoother and the moisture is accurately controlled. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a three-dimensional schematic diagram of an embodiment of the present invention.

[0025] Figure 2 It is a three-dimensional schematic diagram of another embodiment of the present invention.

[0026] Figure 3FIG. 4 is an internal schematic diagram of an embodiment of the present invention.

[0027] Figure 4 FIG. 4 is an internal schematic diagram of another embodiment of the present invention.

[0028] Figure 5 FIG. 4 is an internal schematic diagram of yet another embodiment of the present invention.

[0029] Figure 6 It is a three-dimensional schematic diagram of a porous component and a housing element in one embodiment of the present invention.

[0030] Figure 7 It is a three-dimensional schematic diagram of a conveying component and a roughening component in one embodiment of the present invention.

[0031] Figure 8 It is a schematic diagram of the interior of a conveying component and a roughening component in one embodiment of the present invention.

[0032] Fig. 9 FIG. 4 is a side view of a core material in one embodiment of the present invention.

[0033] Fig.10 It is a side view of a recycled artificial board in one embodiment of the present invention.

[0034] In the figure:

[0035] 10. Shell assembly; 11. First lateral shell; 12. Second lateral shell; 13. Connecting crossbar; 14. Inclined strip funnel; 15. Collecting bucket; 16. Top shell element; 121. Funnel through slot; 111. First hollow cavity; 122. Second hollow cavity; 112. Conveying installation slot; 171. First conveying turn hole; 172. Second conveying turn hole; 173. First vertical slide slot; 174. Second vertical slide slot; 175. Third vertical slide slot; 176. Connecting slot; 177. Initial dredging turn hole hole; 178, secondary dredging hole; 179, roughening dredging hole; 170, deviation correction wheel; 161, switch shell; 162, preparation cavity; 164, second strip slide; 165, nozzle; 30, conveying assembly; 31, feeding roller; 32, output roller; 33, output motor; 40, dredging hole assembly; 42, dredging hole adjustment element; 43, primary roller; 44, secondary roller; 421, first lifting motor; 422, displacement installation shell; 423, vertical installation slide rail; 420, lifting synchronization shaft; 424, vertical 425, sparse hole installation turntable; 426, lateral sliding table; 453, sparse hole drive motor; 427, sliding turn block; 428, coating roller; 429, synchronous lateral movement motor; 454, coating drive motor; 451, lifting synchronous turn hole; 452, worm; 450, nozzle installation hole; 50, cutting assembly; 51, cutting installation plate; 52, cutting shaft; 53, blade assembly; 54, cutting groove; 55, cutting blade; 60, roughening assembly; 61, roughening drive element; 62, roughening roller Cylinder; 611, second lifting motor; 612, displacement shell; 613, roughening lifting shaft; 614, roughening vertical slide rail; 615, roughening vertical slide; 616, roughening horizontal rotating block; 610, roughening horizontal slide; 65, roughening driving motor; 617, scraper rotating shaft; 618, scraper motor; 619, burr scraper; 631, roughening lifting rotary hole; 632, roughening worm; 630, roughening horizontal adjustment motor; 633, scraper mounting rotary hole; 21, upper panel; 22, lower panel; 23, core material. DETAILED DESCRIPTION

[0036] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly understood.

[0037] In the description of the present invention, it should be noted that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc. indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0038] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0039] See also Figures 1 to 8 A regenerated man-made composite fiberboard preparation device comprises a shell assembly 10, a conveying assembly 30, a hole-draining assembly 40, a cutting assembly 50 and a roughening assembly 60, wherein the shell assembly 10 comprises a first lateral shell 11, a second lateral shell 12, a plurality of connecting cross bars 13, two inclined strip funnels 14, two collecting buckets 15 and a top shell element 16, wherein the bottom of the first lateral shell 11 is placed on one side of the installation ground, the bottom of the second lateral shell 12 is placed on the other side of the installation ground, and the first lateral shell 11 and the second lateral shell 12 are arranged opposite to each other, one end of the plurality of connecting cross bars 13 is respectively installed on the inner side of the first lateral shell 11 along the length direction, and the other end of the plurality of connecting cross bars 13 is respectively installed on the inner side of the second lateral shell 12 along the length direction, and the outer ends of the second lateral shell 12 are respectively recessed with funnel passing grooves 121, the two inclined strip funnels 14 are respectively arranged on the inner side of the second lateral shell 12, and the two ends of the outer side of the second lateral shell 12 are respectively recessed with funnel passing grooves 121, and the two inclined strip funnels 14 are respectively arranged on the inner side of the second lateral shell 12. The inner ends are respectively installed at the two ends of the inner side of the first lateral shell 11, the outer ends of the two inclined strip funnels 14 are respectively passed through the two funnel through grooves 121 and protrude on the outer side of the second lateral shell 12, the bottoms of the two collecting barrels 15 are placed on the installation ground adjacent to the side of the second lateral shell 12, and the two collecting barrels 15 are respectively located directly below the outer ends of the two inclined strip funnels 14, the top surface of the top shell element 16 is respectively installed on the top of the first lateral shell 11 and the second lateral shell 12, the conveying assembly 30 is installed at both ends of the first lateral shell 11 and the second lateral shell 12, the first lateral shell 11 is hollow inside to form a first hollow cavity 111, the second lateral shell 12 is hollow inside to form a second hollow cavity 122, the hole dredging assembly 40, the cutting assembly 50 and the roughening assembly 60 are all installed in the first hollow cavity 111 and the second hollow cavity 122.

[0040] A conveying installation groove 112 is recessed at one end of the top surface of the first lateral shell 11, a first conveying rotation hole 171 is recessed at one end of the inner top of the first hollow cavity 111 and the second hollow cavity 122 adjacent to the conveying installation groove 112, a second conveying rotation hole 172 is recessed at the other end of the inner top of the first hollow cavity 111 and the second hollow cavity 122, a first vertical slide groove 173 and a second vertical slide groove 174 are recessed along the length direction at one end of the top of the first lateral shell 11 and the second lateral shell 12 adjacent to the conveying installation groove 112, the first vertical slide groove 173 is disposed adjacent to the conveying installation groove 112, a third vertical slide groove 175 is recessed at the other end of the top of the first lateral shell 11 and the second lateral shell 12, and a third vertical slide groove 175 is recessed at the middle of the inner side of the first hollow cavity 111 and the second hollow cavity 122. Three connecting grooves 176 are recessed, and the three connecting grooves 176 are respectively located directly below the first vertical slide groove 173, the second vertical slide groove 174 and the third vertical slide groove 175; a correction wheel 170 is provided at the inner top of the first lateral shell 11 and the second lateral shell 12 away from the conveying installation groove 112; two cutting rotary holes are recessed along the length direction on the inner top of the first hollow cavity 111 and the second hollow cavity 122; a primary dredging rotary hole 177, a secondary dredging rotary hole 178 and a roughening rotary hole 179 are recessed on the inner top of the first lateral shell 11 and the second lateral shell 12, and the primary dredging rotary hole 177 is located below the third vertical slide groove 175, the secondary dredging rotary hole 178 is located below the second vertical slide groove 174, and the roughening rotary hole 179 is located below the first vertical slide groove 173.

[0041] The top shell element 16 includes three switch shells 161. The bottom surfaces of the three switch shells 161 are respectively installed on the top surfaces of the first lateral shell 11 and the second lateral shell 12 along the length direction. Each switch shell 161 is hollow at the bottom to form a preparation cavity 162. The outer sides of the two preparation cavities 162 away from the conveying installation groove 112 are recessed with second strip slide grooves 164. The two second strip slide grooves 164 are respectively located directly above the third vertical slide groove 175 and the second vertical slide groove 174. Each second strip slide groove 164 is slidably provided with a nozzle 165. The inner end of the nozzle 165 is located in the preparation cavity 162, and the outer end of the nozzle 165 is connected to the external softener conveying equipment.

[0042] The conveying assembly 30 includes a feed roller 31, a feed motor, an output roller 32 and an output motor 33. The two ends of the feed roller 31 are respectively rotatably installed in the two second conveying rotary holes 172, the feed motor is installed in the second hollow cavity 122 away from the conveying mounting groove 112, and the output shaft of the feed motor is connected to the feed roller 31, the two ends of the output roller 32 are respectively rotatably installed in the two first conveying rotary holes 171, the output motor 33 is installed in the conveying mounting groove 112, and the output shaft of the output motor 33 is connected to one end of the output roller 32.

[0043] The hole-clearing assembly 40 includes two hole-clearing adjustment elements 42, two primary rollers 43 and two secondary rollers 44. The two hole-clearing adjustment elements 42 are symmetrically installed at the two ends of the first hollow cavity 111 and the second hollow cavity 122, respectively. One of the primary rollers 43 is installed in the hole-clearing adjustment element 42 away from the conveying installation groove 112, and the two ends of the other primary roller 43 are rotatably installed in the two primary hole-clearing holes 177, one of the secondary rollers 44 is installed in the other hole-clearing adjustment element 42, and the two ends of the other secondary roller 44 are rotatably installed in the secondary hole-clearing holes 178.

[0044] Each sparse hole adjustment element 42 includes a first lifting motor 421, two displacement mounting shells 422, a lifting synchronous shaft 420, two vertical mounting slide rails 423, two vertical sliding tables 424, two sparse hole mounting turntables 425, a sparse hole driving motor 453, two lateral sliding tables 426, two sliding turn blocks 427, a coating roller 428, a coating driving motor 454 and two synchronous lateral movement motors 429. The first lifting motor 421 is installed at one end of the bottom of the first hollow cavity 111, and the two displacement mounting shells 422 are respectively installed in two connecting grooves 176 away from the conveying mounting groove 112 or two connecting grooves 176 adjacent to the cutting rotating hole. Each displacement mounting shell 422 is hollow inside to form a rotating mounting cavity. The displacement mounting shell 422 A lifting synchronous rotating hole 451 is recessed at one end of the side wall, and the lifting synchronous rotating hole 451 is connected to the rotating installation cavity. A worm 452 is rotatably arranged in the rotating installation cavity. Both ends of the lifting synchronous shaft 420 are rotatably installed in the two lifting synchronous rotating holes 451, and one end of the lifting synchronous shaft 420 is connected to the output shaft of the first lifting motor 421. Turbines are respectively arranged at both ends of the lifting synchronous shaft 420, and the two turbines are respectively meshed and connected with the two worms 452. The inner sides of the two vertical installation slide rails 423 are respectively installed in the first hollow cavity 111 or the second hollow cavity 122, and the two vertical installation slide rails 423 are respectively located directly above the two displacement installation shells 422, and the inner sides of the two vertical sliding platforms 424 are respectively slidably installed on the outer sides of the two vertical installation slide rails 423. The middle part of the bottom surface of each vertical sliding table 424 is concavely provided with an adjusting thread groove, the top ends of the two worm gears 452 are respectively rotatably installed in the two adjusting thread grooves, and the top ends of the two vertical sliding tables 424 are respectively penetrated through the two third vertical slide grooves 175 or the two second vertical slide grooves 174 and protrude in the preparation chamber 162, the bottom surfaces of the two sparse hole installation turntables 425 are respectively installed on one end of the top surfaces of the two vertical sliding tables 424, the inner sides of the two sparse hole installation turntables 425 are respectively rotatably connected to the two ends of the primary roller 43 or the two ends of the secondary roller 44, the sparse hole driving motor 453 is installed on the outer side of one of the sparse hole installation turntables 425, and the output shaft of the sparse hole driving motor 453 is connected to one end of the primary roller 43 or one end of the secondary roller 44, and the two horizontal sliding tables 4 26 bottoms are respectively installed in the middle of the top surfaces of the two vertical sliding tables 424, the two sliding turn blocks 427 are respectively slidably installed in the two lateral sliding tables 426, the two ends of the coating roller 428 are respectively rotatably installed in the two lateral sliding tables 426, the coating drive motor 454 is installed in one of the lateral sliding tables 426, and the output shaft of the coating drive motor 454 is connected to one end of the coating roller 428, one of the lateral sliding tables 426 has a nozzle mounting hole 450 recessed on the top, the inner end of the nozzle 165 is installed in the nozzle mounting hole 450, the two synchronous lateral moving motors 429 are respectively installed on the top surfaces of the two vertical sliding tables 424 away from one end of the sparse hole mounting turntable 425, and the output shafts of the two synchronous lateral moving motors 429 are respectively connected to the two lateral sliding tables 426.

[0045] The cutting assembly 50 includes a cutting mounting plate 51, two cutting shafts 52, two cutting motors and two blade groups 53. The two sides of the cutting mounting plate 51 are respectively installed in the middle of the top surface of the first lateral shell 11 and the middle of the top surface of the second lateral shell 12. A plurality of cutting grooves 54 are recessed in an array on the top surface of the cutting mounting plate 51. The two ends of the two cutting shafts 52 are respectively rotatably installed in four cutting rotary holes. The two cutting motors are respectively installed on the top of the second hollow cavity 122, and the output shafts of the two cutting motors are respectively connected to one end of the two cutting shafts 52. The two blade groups 53 are respectively installed in the two cutting shafts 52. Each blade group 53 is composed of a plurality of cutting blades 55. The plurality of cutting blades 55 are installed in the cutting shaft 52 at intervals along the length direction, and the top of the cutting blade 55 passes through the cutting groove 54 and is located in the preparation cavity 162.

[0046] The roughening assembly 60 includes a roughening drive element 61 and two roughening rollers 62. The roughening drive element 61 is respectively installed at one end of the first hollow cavity 111 and the second hollow cavity 122 adjacent to the conveying installation groove 112. One of the roughening rollers 62 is rotatably installed in the roughening drive element 61, and the other roughening roller 62 is rotatably installed at both ends in the two roughening rotating holes 179.

[0047] The roughening drive element 61 includes a second lifting motor 611, two displacement shells 612, a roughening lifting shaft 613, two roughening vertical slide rails 614, two roughening vertical slides 615, two roughening horizontal slides 610, two roughening horizontal rotating blocks 616, a roughening drive motor 65, a scraper shaft 617, a scraper motor 618 and a burr scraper 619. The second lifting motor 611 is installed at one end of the bottom of the first hollow cavity 111, and the two displacement shells 612 are respectively installed at two connecting grooves 176 adjacent to the conveying installation groove 112. Each displacement installation shell 422 is hollow inside to form a rotating cavity, and one end of the side wall of the displacement installation shell 422 is concavely provided with a roughening The lifting and lowering rotating hole 631 and the displacement mounting shell 422 are rotatably provided with a roughening worm 632. The two ends of the roughening lifting shaft 613 are respectively rotatably installed in the two roughening lifting and lowering rotating holes 631. One end of the roughening lifting shaft 613 is connected to the output shaft of the second lifting motor 611. The two ends of the roughening lifting shaft 613 are respectively provided with roughening turbines. The two roughening turbines are respectively meshed and connected with the two roughening worms 632. The inner sides of the two roughening vertical slide rails 614 are respectively installed in the first hollow cavity 111 or the second hollow cavity 122, and the two roughening vertical slide rails 614 are respectively located directly above the two displacement shells 612. The inner sides of the two roughening vertical slide tables 615 are respectively slidably installed on the two The outer side of the roughening vertical slide rail 614, the middle part of the bottom surface of each roughening vertical slide 615 is concavely provided with a roughening thread groove, the top ends of the two roughening worms 632 are respectively rotatably installed in the two roughening thread grooves, and the top ends of the two vertical sliding tables 424 are respectively penetrated through the two first vertical slide grooves 173 and protruded in the preparation cavity 162, the bottom surfaces of the two roughening transverse slides 610 are respectively installed on the top surfaces of the two vertical sliding tables 424, the two roughening transverse rotating blocks 616 are respectively slidably installed in the two roughening transverse slides 610, the roughening drive motor 65 is installed on the outer side of one of the roughening transverse rotating blocks 616, and the two ends of the roughening roller 62 are respectively rotatably installed on the two roughening transverse slides In the platform 610, the output shaft of the roughening drive motor 65 is connected to one end of the roughening roller 62, and a roughening horizontal adjustment motor 630 is convexly provided at one end of each roughening horizontal rotating block 616, and the roughening horizontal adjustment motor 630 is connected to the top of the two vertical sliding tables 424. A scraper mounting rotating hole 633 is recessed at one end of the top of the side wall of each roughening horizontal rotating block 616. The scraper motor 618 is installed on the outer top of one of the roughening horizontal sliding tables 610. The two ends of the scraper shaft 617 are rotatably installed in the two scraper mounting rotating holes 633, and the output shaft of the scraper motor 618 is connected to one end of the scraper shaft 617, and the burr scraper 619 is installed in the scraper shaft 617.

[0048] See also Figures 9 and 10 The present invention also provides a method for preparing a regenerated man-made composite fiberboard, which is applied to the above-mentioned regenerated man-made composite fiberboard preparation device and comprises the following steps:

[0049] Step S1: placing the waste furniture boards in a regenerated man-made composite fiberboard preparation device, cutting the waste furniture boards into equal widths, and performing deep roughening on the upper and lower surfaces of the waste furniture boards to form boards to be assembled;

[0050] Step S2: gluing the panels to be assembled and staggeredly laying them to form a core material 23;

[0051] Step S3: The bottom surface of the core material 23 is provided with a lower panel 22, and the top surface of the core material 23 is provided with an upper panel 21 to form a sheet to be formed;

[0052] Step S4: placing the sheet to be formed in a hot pressing device for hot pressing treatment to form a recycled artificial board.

[0053] For example, in one embodiment: the outer wall of the primary roller 43 and the outer wall of the secondary roller 44 are both provided with a plurality of thorn-like protrusions along the circumferential direction, and the density of the thorn-like protrusions in the outer wall of the secondary roller 44 is greater than the density of the thorn-like protrusions in the outer wall of the primary roller 43. The outer wall of the roughening roller 62 is provided with a plurality of roughening steel wires along the circumferential direction, and the outer wall of the coating roller 428 is formed with a sponge cylinder.

[0054] For example, in one embodiment: when it is necessary to recycle the waste furniture board, the waste furniture board is placed on the feeding roller 31, and then the feeding motor is started to rotate the feeding roller 31 to convey the waste furniture board. At the same time, the deviation correction wheel 170 will center the waste furniture board. Then, the sparse hole driving motor 453 and the coating driving motor 454 in the sparse hole adjusting element 42 away from the conveying installation groove 112 will be started. The sparse hole driving motor 453 will drive the primary roller 43 to rotate. Since the outer wall of the primary roller 43 is convexly provided with a plurality of thorn-like protrusions, and one end of the waste furniture board is arranged between the two primary rollers 43 at this time, the rotation of the primary roller 43 will synchronously punch sparse holes on the upper and lower surfaces of the waste furniture board on both sides, and send it to the cutting assembly 50, and then the two cutting assemblies are connected. The cutting motors will be started synchronously, causing the two cutting shafts 52 to rotate, causing the two blade groups 53 to rotate accordingly, causing the multiple cutting blades 55 to rotate in the opposite direction, so that the waste furniture boards are pushed forward and cut into multiple equal-width narrow strips by the reversely rotating blade groups 53. Subsequently, the perforation drive motor 453 and the coating drive motor 454 in the perforation adjustment element 42 adjacent to the conveying installation slot 112 will be started, causing the two secondary rollers 44 to rotate, thereby performing secondary dense punching on the strip boards, so that dense holes are formed on both sides of the strip boards. Subsequently, the roughening drive motor 65 will be started, causing the roughening roller 62 to rotate, and then the roughening steel wire on the roughening roller 62 is used to deeply roughen the strip boards, forming rough surfaces on the upper and lower surfaces of the strip boards to form boards to be spliced. A three-step roughening method is provided: the thorn-like protrusions on the first-level roller 43 arranged in two directions form sparse roughening holes, the thorn-like protrusions on the second-level roller 44 form dense roughening holes, and the roughening wire on the roughening roller 62 forms a deeply roughened strip plate, ensuring that the roughening effect is more uniform and consistent, ensuring the subsequent gluing and hot pressing bonding degree, improving the performance and durability of the product, and at the same time, reducing the wear of tools such as the roughening wire, reducing losses, and reducing production costs.

[0055] For example, in one embodiment: when it is necessary to adjust the roughening depth of the waste furniture board, the first lifting motor 421 will be started to rotate the lifting synchronous shaft 420, so that the turbine follows the synchronous rotation, and the worm 452 rotates. Since the top ends of the two worms 452 are respectively rotatably installed in the two adjusting thread grooves, the two vertical sliding tables 424 are respectively moved down along the two vertical sliding tables 424, so that the two sparse hole installation turntables 425 follow the movement, and then the first-level roller 43 follows the movement, so that the direct distance between the first-level roller 43 and the waste furniture board is reduced, and the depth of the sparse holes will increase. At the same time, the coating roller 428 will follow the movement, so that the sponge tube of the coating roller 428 is attached to the surface of the waste furniture board to apply pressure to the surface of the waste furniture board to prevent the waste furniture board from vibrating when the depth of the holes is increased, which causes the waste furniture board to shift, and then makes it impossible to perform uniform cutting of equal width. The pore regulating element 42 on the secondary roller 44 performs the above-mentioned action process synchronously to deepen the holes of the waste furniture board.

[0056] Subsequently, the second lifting motor 611 will be started synchronously, causing the two roughening vertical slides 615 to descend along the two roughening vertical slide rails 614, causing the two roughening horizontal rotating blocks 616 to move along, causing the roughening rollers 62 therein to move along, and then deepening the roughening synchronously with the deepening depth of the punching.

[0057] At the same time, when roughening, the scraper motor 618 will start, causing the scraper shaft 617 to rotate, and the burr scraper 619 to rotate accordingly, so that the burr scraper 619 will clean the roughening steel wire to ensure a continuous roughening effect. At the same time, the roughening transverse adjustment motor 630 will start, causing the roughening transverse rotating block 616 to move along the roughening transverse slide 610, and then further adjust the degree of fit between the burr scraper 619 and the roughening steel wire to ensure the cleaning effect of the roughening steel wire.

[0058] For example, in one embodiment: the softener is composed of a mixture of water, an organic solvent and a surfactant. The upper panel 21 and the lower panel 22 are made of thermoplastic polyolefin waterproof coiled material, which can effectively prevent moisture from penetrating into the interior of the recycled artificial board, improve the waterproof performance of the recycled artificial board, avoid deformation and decay of the board due to moisture, and improve its wear resistance, which can protect the surface of the recycled artificial board from scratches, wear and tear, and extend the service life of the board.

[0059] For example, in one embodiment: when the output motor 33 is started, the external softener delivery device will be started and sprayed on the two coating rollers 428 through the two nozzles 165 to form a water mist curtain formed by the softener on both ends of the cutting assembly 50, so as to prevent the sawdust from splashing on the surface of the board or splashing and getting stuck in the roughening wire when the cutting blade 55 cuts the waste furniture board, affecting the contact between the roughening wire and the board surface, reducing the roughening effect, and at the same time, softening the waste furniture board, making the subsequent roughening process easier. At the same time, the synchronous transverse motor 429 can be started, so that the sliding block 427 moves along the transverse sliding platform 426, so that the coating roller 428 moves synchronously, and the water receiving area of ​​the coating roller 428 is adjusted, and the amount of softener applied by the coating roller 428 on the waste furniture board is adjusted, so as to prevent the waste furniture board surface from being over-coated with softener, affecting the friction between the subsequent roughening wire and the surface of the waste furniture board, thereby reducing the roughening efficiency.

[0060] Installation process: Place the bottom of the first lateral shell 11 on one side of the installation ground, and place the bottom of the second lateral shell 12 on the other side of the installation ground, and the first lateral shell 11 and the second lateral shell 12 are arranged opposite to each other, one end of a plurality of connecting cross bars 13 is respectively installed on the inner side of the first lateral shell 11 along the length direction, and the other ends of a plurality of connecting cross bars 13 are respectively installed on the inner side of the second lateral shell 12 along the length direction, and the inner ends of the two inclined strip funnels 14 are respectively installed on the two ends of the inner side of the first lateral shell 11, and the outer ends of the two inclined strip funnels 14 are respectively passed through the two funnel through grooves 121 and protrude on the outer side of the second lateral shell 12, and the bottoms of the two collecting barrels 15 are both placed on the side of the installation ground adjacent to the second lateral shell 12, and the two collecting barrels 15 are respectively located directly below the outer ends of the two inclined strip funnels 14, and the bottom surfaces of the three switch shells 161 are respectively installed on the top surfaces of the first lateral shell 11 and the second lateral shell 12 along the length direction. The outer end of the nozzle 165 is connected to the external softener conveying device, and the two ends of the feeding roller 31 are respectively rotatably installed in the two second conveying rotating holes 172, and the feeding motor is installed at the end of the second hollow cavity 122 away from the conveying installation groove 112, and the output shaft of the feeding motor is connected to the feeding roller 31, and the two ends of the output roller 32 are respectively rotatably installed in the two first conveying rotating holes 171, and the output motor 33 is installed in the conveying installation groove 112, and the output shaft of the output motor 33 is connected to one end of the output roller 32, and the two ends of one of the primary rollers 43 are divided into The two ends of the secondary roller 44 are respectively rotatably installed in the two primary dredging holes 177, and the two ends of one of the secondary rollers 44 are respectively rotatably installed in the secondary dredging holes 178. The first lifting motor 421 is installed at one end of the bottom of the first hollow cavity 111. The two displacement installation shells 422 are respectively installed in the two connecting grooves 176 away from the conveying installation groove 112 or the two connecting grooves 176 adjacent to the cutting rotation hole. The two ends of the lifting synchronization shaft 420 are respectively rotatably installed in the two lifting synchronization rotation holes 451, and one end of the lifting synchronization shaft 420 is connected to the output shaft of the first lifting motor 421. The two turbines are respectively meshed with the two worm gears 452. The inner sides of the two vertical installation slide rails 423 are respectively installed in the first hollow cavity 111 or the second hollow cavity 122, and the two The two vertical mounting rails 423 are respectively located directly above the two displacement mounting shells 422, the inner sides of the two vertical sliding tables 424 are respectively slidably mounted on the outer sides of the two vertical mounting rails 423, the top ends of the two worm gears 452 are respectively rotatably mounted in the two adjusting thread grooves, and the top ends of the two vertical sliding tables 424 are respectively penetrated through the two third vertical slide grooves 175 or the two second vertical slide grooves 174 and protruded in the preparation chamber 162, the bottom surfaces of the two sparse hole mounting turntables 425 are respectively mounted on one end of the top surfaces of the two vertical sliding tables 424, the inner sides of the two sparse hole mounting turntables 425 are respectively rotatably connected with the two ends of the first-stage roller 43 or the two ends of the second-stage roller 44, the sparse hole driving motor 453 is installed on the outer side of one of the sparse hole mounting turntables 425,The output shaft of the hole-draining driving motor 453 is connected to one end of the primary roller 43 or one end of the secondary roller 44. The bottoms of the two lateral sliding tables 426 are respectively installed in the middle of the top surfaces of the two vertical sliding tables 424. The two sliding turn blocks 427 are respectively slidably installed in the two lateral sliding tables 426. The two ends of the coating roller 428 are respectively rotatably installed in the two lateral sliding tables 426. The coating driving motor 454 is installed in one of the lateral sliding tables 426, and the output shaft of the coating driving motor 454 is connected to one end of the coating roller 428. The inner end of the nozzle 165 is installed in the nozzle mounting hole 450. The two synchronous lateral moving motors 429 are respectively installed on the top surfaces of the two vertical sliding tables 424 away from one end of the hole-draining mounting turntable 425. The output shafts are respectively connected to the two lateral sliding tables 426, and the two sides of the cutting mounting plate 51 are respectively installed in the middle of the top surface of the first lateral shell 11 and the middle of the top surface of the second lateral shell 12. The two ends of the two cutting shafts 52 are respectively rotatably installed in the four cutting rotation holes. The two cutting motors are respectively installed on the top of the second hollow cavity 122, and the output shafts of the two cutting motors are respectively connected to one end of the two cutting shafts 52. The two blade groups 53 are respectively installed in the two cutting shafts 52. A plurality of cutting blades 55 are installed in the cutting shafts 52 at intervals along the length direction, and the top of the cutting blade 55 is arranged through the cutting groove 54 and is located in the preparation cavity 162. The two ends of one of the roughening rollers 62 are respectively rotatably installed in the two roughening rotation holes 179. The second lifting The motor 611 is installed at one end of the bottom of the first hollow cavity 111, and the two displacement shells 612 are respectively installed in the two connecting grooves 176 adjacent to the conveying installation groove 112. The two ends of the roughening lifting shaft 613 are respectively rotatably installed in the two roughening lifting rotating holes 631. One end of the roughening lifting shaft 613 is connected to the output shaft of the second lifting motor 611. The two roughening turbines are respectively meshed with the two roughening worm gears 632. The inner sides of the two roughening vertical slide rails 614 are respectively installed in the first hollow cavity 111 or the second hollow cavity 122, and the two roughening vertical slide rails 614 are respectively located directly above the two displacement shells 612. The inner sides of the two roughening vertical slide tables 615 are respectively slidably installed on the outer sides of the two roughening vertical slide rails 614. The tops of the two roughening worm gears 632 are respectively rotated. The two vertical slide tables 424 are respectively installed in the two roughening thread grooves, and the tops of the two vertical slide tables 424 are respectively penetrated through the two first vertical slide grooves 173 and protruded in the preparation cavity 162. The bottom surfaces of the two roughening transverse slide tables 610 are respectively installed on the top surfaces of the two vertical slide tables 424. The two roughening transverse rotating blocks 616 are respectively slidably installed in the two roughening transverse slide tables 610. The roughening drive motor 65 is installed on the outside of one of the roughening transverse rotating blocks 616. The two ends of the roughening roller 62 are respectively rotatably installed in the two roughening transverse slide tables 610. The output shaft of the roughening drive motor 65 is connected to one end of the roughening roller 62. The roughening transverse adjustment motor 630 is connected to the tops of the two vertical slide tables 424. The scraper motor 618 is installed on the top of the outside of one of the roughening transverse slide tables 610.The two ends of the scraper shaft 617 are rotatably mounted in the two scraper mounting holes 633, and the output shaft of the scraper motor 618 is connected to one end of the scraper shaft 617, and the burr scraper 619 is installed in the scraper shaft 617.

[0061] The present invention can achieve:

[0062] 1. The present invention provides a three-step roughening method: the thorn-like protrusions on the first-level roller 43 arranged in two directions form sparse roughening holes, the thorn-like protrusions on the second-level roller 44 form dense roughening holes, and the roughening wires on the roughening roller 62 form deeply roughened strip plates, ensuring that the roughening effect is more uniform and consistent, ensuring the degree of subsequent gluing and hot pressing bonding, improving the performance and durability of the product, and at the same time, reducing the wear of tools such as roughening wires, reducing losses, and reducing production costs. In addition, the upper panel 21 and the lower panel 22 made of thermoplastic polyolefin waterproof coiled material can effectively prevent moisture from penetrating into the interior of the recycled artificial board, improve the waterproof performance of the recycled artificial board, avoid deformation and decay of the board due to moisture, and at the same time improve its wear resistance, which can protect the surface of the recycled artificial board from damage such as scratches and abrasion, and extend the service life of the board.

[0063] 2. The processing of the present invention is green and environmentally friendly. The preparation process of the core material 23 is physical cutting, no waste gas is emitted, and it is not limited by material specifications. The material utilization rate is high, there are no special requirements for raw material specifications, and it has strong applicability.

[0064] 3. The performance of the recycled artificial board produced by the present invention is better than that of the original waste furniture board. By placing the boards to be assembled crosswise, hot-pressing and gluing the upper panel 21 and the lower panel 22, and ensuring that the roughening effect is more uniform and consistent, the subsequent gluing and hot-pressing bonding degree is guaranteed, the performance and durability of the product are improved, the physical properties are enhanced, and the size of the recycled artificial board is regular, and the production can be flexibly adjusted according to production requirements.

[0065] 4. The present invention can achieve roughening treatment of different depths and densities, ensuring the controllability and consistency of the roughening depth, and can avoid the deviation and vibration of the board during roughening, ensuring the stability of the roughening process and the accuracy of cutting. The roughening wire is automatically cleaned during the roughening process to maintain the roughening effect of the roughening wire, extend the service life of the tool, and reduce maintenance work. At the same time, a water mist curtain is sprayed to prevent the splashing of wood chips generated during the cutting process from affecting the roughening effect, and at the same time soften the surface of the board, so that the subsequent roughening process is smoother and the moisture is accurately controlled.

[0066] The above-mentioned embodiments only express several embodiments of the present invention, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.

Claims

1. A device for preparing recycled man-made composite fiberboard, characterized in that: The invention comprises a shell component (10), a conveying component (30), a hole-draining component (40), a cutting component (50) and a roughening component (60). The shell component (10) comprises a first lateral shell (11), a second lateral shell (12), a plurality of connecting cross bars (13), two inclined strip-shaped funnels (14), two collecting buckets (15) and a top shell component (16). The bottom of the first lateral shell (11) is placed on one side of the installation ground, and the bottom of the second lateral shell (12) is placed on the other side of the installation ground. The first lateral shell (11) and the second lateral shell (12) are arranged opposite to each other. One end of the plurality of connecting cross bars (13) is respectively installed on the inner side of the first lateral shell (11) along the length direction, and the other end of the plurality of connecting cross bars (13) is respectively installed on the inner side of the second lateral shell (12) along the length direction. The outer ends of the second lateral shell (12) are respectively provided with funnel passing grooves (121). The inner ends of the two inclined strip-shaped funnels (14) are respectively installed on the first lateral shell (11). At the two ends of the inner side of the lateral shell (11), the outer ends of the two inclined strip funnels (14) are respectively passed through the two funnel passing grooves (121) and protrude from the outer side of the second lateral shell (12). The bottoms of the two collecting barrels (15) are both placed on the installation ground adjacent to the side of the second lateral shell (12), and the two collecting barrels (15) are respectively located directly below the outer ends of the two inclined strip funnels (14). The top surface of the top shell element (16) is respectively installed on the first lateral shell (11) and the second lateral shell (12). The conveying assembly (30) is installed at the top of the two lateral shells (12), and is installed at both ends of the first lateral shell (11) and the second lateral shell (12). The first lateral shell (11) is hollow inside to form a first hollow cavity (111), and the second lateral shell (12) is hollow inside to form a second hollow cavity (122). The hole-drilling assembly (40), the cutting assembly (50) and the roughening assembly (60) are all installed in the first hollow cavity (111) and the second hollow cavity (122).

2. The equipment for preparing recycled man-made composite fiberboard according to claim 1, characterized in that: A conveying installation groove (112) is recessed at one end of the top surface of the first lateral shell (11), a first conveying rotation hole (171) is recessed at one end of the top of the inner side of the first hollow cavity (111) and the second hollow cavity (122) adjacent to the conveying installation groove (112), and a second conveying rotation hole (172) is recessed at the other end of the top of the inner side of the first hollow cavity (111) and the second hollow cavity (122). 12) A first vertical slide groove (173) and a second vertical slide groove (174) are respectively recessed along the length direction at one end of the top adjacent to the conveying installation groove (112), the first vertical slide groove (173) is arranged adjacent to the conveying installation groove (112), a third vertical slide groove (175) is recessed at the other end of the top of the first lateral shell (11) and the second lateral shell (12), and the middle part of the inner side of the first hollow cavity (111) and the second hollow cavity (122) is Three connecting grooves (176) are concavely arranged, and the three connecting grooves (176) are respectively located directly below the first vertical slide groove (173), the second vertical slide groove (174) and the third vertical slide groove (175). The first lateral shell (11) and the second lateral shell (12) are provided with a correction wheel (170) at the inner top end away from the conveying installation groove (112). The inner top end of the first hollow cavity (111) and the second hollow cavity (122) are provided with a correction wheel (170) along the length. Two cutting holes are recessed in the vertical direction, and the top of the inner side of the first lateral shell (11) and the second lateral shell (12) are respectively recessed with a primary weeding hole (177), a secondary weeding hole (178) and a roughening hole (179), and the primary weeding hole (177) is located below the third vertical slide groove (175), the secondary weeding hole (178) is located below the second vertical slide groove (174), and the roughening hole (179) is located below the first vertical slide groove (173).

3. The equipment for preparing recycled man-made composite fiberboard according to claim 2, characterized in that: The top housing element (16) comprises three switch housings (161). The bottom surfaces of the three switch housings (161) are respectively mounted on the top surfaces of the first lateral housing (11) and the second lateral housing (12) along the length direction. Each switch housing (161) is hollow at the bottom to form a preparation cavity (162). The outer sides of the two preparation cavities (162) away from the conveying installation groove (112) are recessed with second strip slide grooves (164). The two second strip slide grooves (164) are respectively located directly above the third vertical slide groove (175) and the second vertical slide groove (174). Each second strip slide groove (164) is slidably provided with a nozzle (165). The inner end of the nozzle (165) is located in the preparation cavity (162), and the outer end of the nozzle (165) is connected to an external softener conveying device.

4. The equipment for preparing recycled man-made composite fiberboard according to claim 3, characterized in that: The conveying assembly (30) comprises a feeding roller (31), a feeding motor, an output roller (32) and an output motor (33); two ends of the feeding roller (31) are respectively rotatably mounted in two second conveying rotary holes (172); the feeding motor is mounted at one end of the second hollow cavity (122) away from the conveying mounting groove (112); and the output shaft of the feeding motor is connected to the feeding roller (31); two ends of the output roller (32) are respectively rotatably mounted in the two first conveying rotary holes (171); the output motor (33) is mounted in the conveying mounting groove (112); and the output shaft of the output motor (33) is connected to one end of the output roller (32).

5. The equipment for preparing recycled man-made composite fiberboard according to claim 4, characterized in that: The pore-draining assembly (40) comprises two pore-draining adjustment elements (42), two primary rollers (43) and two secondary rollers (44); the two pore-draining adjustment elements (42) are symmetrically arranged and installed at the two ends of the first hollow cavity (111) and the second hollow cavity (122), respectively; one of the primary rollers (43) is installed in the pore-draining adjustment element (42) away from the conveying installation groove (112); the two ends of the other primary roller (43) are rotatably installed in two primary pore-draining rotating holes (177); one of the secondary rollers (44) is installed in the other pore-draining adjustment element (42); the two ends of the other secondary roller (44) are rotatably installed in the secondary pore-draining rotating holes (178).

6. The equipment for preparing recycled man-made composite fiberboard according to claim 5, characterized in that: Each hole-sparse adjustment element (42) comprises a first lifting motor (421), two displacement mounting shells (422), a lifting synchronous shaft (420), two vertical mounting slide rails (423), two vertical sliding tables (424), two hole-sparse mounting turntables (425), a hole-sparse driving motor (453), two lateral sliding tables (426), two sliding turn blocks (427), a coating roller (428), a coating driving motor (454) and two synchronous lateral moving motors (429). The first lifting motor (421) is mounted at one end of the bottom of the first hollow cavity (111), and the two displacement mounting shells (422) are respectively mounted at two connecting grooves (176) away from the conveying mounting groove (112) or two adjacent cutting turntables. In the connecting grooves (176), each displacement mounting shell (422) is hollow inside to form a rotating mounting cavity, a lifting synchronous rotating hole (451) is recessed at one end of the side wall of the displacement mounting shell (422), the lifting synchronous rotating hole (451) is connected with the rotating mounting cavity, a worm (452) is rotatably arranged in the rotating mounting cavity, the two ends of the lifting synchronous shaft (420) are respectively rotatably installed in the two lifting synchronous rotating holes (451), and one end of the lifting synchronous shaft (420) is connected to the output shaft of the first lifting motor (421), turbines are respectively arranged at the two ends of the lifting synchronous shaft (420), and the two turbines are respectively meshed and connected with the two worms (452), and the inner sides of the two vertical mounting slide rails (423) are respectively installed in the first hollow cavity (111) or in the second hollow cavity (122), and the two vertical mounting slide rails (423) are respectively located directly above the two displacement mounting shells (422), the inner sides of the two vertical sliding platforms (424) are respectively slidably mounted on the outer sides of the two vertical mounting slide rails (423), and the middle part of the bottom surface of each vertical sliding platform (424) is concavely provided with an adjustment thread groove, the top ends of the two worm gears (452) are respectively rotatably mounted in the two adjustment thread grooves, and the top ends of the two vertical sliding platforms (424) are respectively penetrated through the two third vertical slide grooves (175) or the two second vertical slide grooves (174) and protruded in the preparation cavity (162), the bottom surfaces of the two sparse hole mounting turntables (425) are respectively mounted on one end of the top surfaces of the two vertical sliding platforms (424), and the two sparse hole mounting turntables (425) are respectively mounted on one end of the top surfaces of the two vertical sliding platforms (424). The inner side of the mounting turntable (425) is rotatably connected to the two ends of the primary roller (43) or the two ends of the secondary roller (44), the sparse hole driving motor (453) is installed on the outer side of one of the sparse hole mounting turntables (425), and the output shaft of the sparse hole driving motor (453) is connected to one end of the primary roller (43) or one end of the secondary roller (44), the bottoms of the two lateral sliding platforms (426) are respectively installed in the middle of the top surfaces of the two vertical sliding platforms (424), the two sliding rotating blocks (427) are respectively slidably installed in the two lateral sliding platforms (426), the two ends of the coating roller (428) are respectively rotatably installed in the two lateral sliding platforms (426), and the coating driving motor (454) is installed in one of the lateral sliding platforms (426).The output shaft of the coating drive motor (454) is connected to one end of the coating roller (428), a nozzle mounting hole (450) is recessed on the top of one of the transverse sliding platforms (426), and the inner end of the nozzle (165) is mounted in the nozzle mounting hole (450), and two synchronous transverse motors (429) are respectively mounted on the top surfaces of the two vertical sliding platforms (424) away from one end of the hole mounting turntable (425), and the output shafts of the two synchronous transverse motors (429) are respectively connected to the two transverse sliding platforms (426).

7. The equipment for preparing recycled man-made composite fiberboard according to claim 6, characterized in that: The cutting assembly (50) comprises a cutting mounting plate (51), two cutting rotating shafts (52), two cutting motors and two blade groups (53). The two sides of the cutting mounting plate (51) are respectively mounted on the middle of the top surface of the first lateral shell (11) and the middle of the top surface of the second lateral shell (12). The top surface of the cutting mounting plate (51) is arrayed with a plurality of cutting grooves (54). The two ends of the two cutting rotating shafts (52) are respectively rotatably mounted in four cutting rotating holes. The two cutting motors are respectively mounted on the top of the second hollow cavity (122), and the output shafts of the two cutting motors are respectively connected to one end of the two cutting rotating shafts (52). The two blade groups (53) are respectively mounted in the two cutting rotating shafts (52). Each blade group (53) consists of a plurality of cutting blades (55). The plurality of cutting blades (55) are installed in the cutting rotating shaft (52) at intervals along the length direction, and the top of the cutting blade (55) passes through the cutting groove (54) and is located in the preparation cavity (162).

8. The equipment for preparing recycled man-made composite fiberboard according to claim 7, characterized in that: The roughening assembly (60) includes a roughening drive element (61) and two roughening rollers (62). The roughening drive element (61) is respectively installed at one end of the first hollow cavity (111) and the second hollow cavity (122) adjacent to the conveying installation groove (112). One of the roughening rollers (62) is rotatably installed in the roughening drive element (61), and the other roughening roller (62) is rotatably installed at both ends in the two roughening rotating holes (179).

9. The equipment for preparing recycled man-made composite fiberboard according to claim 8, characterized in that: The roughening drive element (61) comprises a second lifting motor (611), two displacement shells (612), a roughening lifting shaft (613), two roughening vertical slide rails (614), two roughening vertical slides (615), two roughening horizontal slides (610), two roughening horizontal rotating blocks (616), a roughening drive motor (65), a scraper rotating shaft (617), a scraper motor (618) and a burr scraper (619). The second lifting motor (611) is installed at one end of the bottom of the first hollow cavity (111). The two displacement shells (612) are respectively installed at two connecting grooves (176) adjacent to the conveying installation groove (112). Each displacement installation shell (422) is hollow inside to form a rotating cavity. The displacement installation shell (422) is hollow inside to form a rotating cavity. 22) A roughening lifting rotating hole (631) is recessed at one end of the side wall, a roughening worm (632) is rotatably arranged in the displacement mounting shell (422), two ends of the roughening lifting shaft (613) are respectively rotatably mounted in the two roughening lifting rotating holes (631), one end of the roughening lifting shaft (613) is connected to the output shaft of the second lifting motor (611), and two ends of the roughening lifting shaft (613) are respectively provided with roughening turbines, the two roughening turbines are respectively meshed and connected with the two roughening worms (632), the inner sides of the two roughening vertical slide rails (614) are respectively installed in the first hollow cavity (111) or the second hollow cavity (122), and the two roughening vertical slide rails (614) are respectively located directly above the two displacement shells (612), and the two roughening vertical slide rails (614) are respectively located directly above the two displacement shells (612). The inner sides of the platforms (615) are respectively slidably mounted on the outer sides of the two roughening vertical slide rails (614), and a roughening thread groove is concavely provided in the middle of the bottom surface of each roughening vertical slide platform (615). The top ends of the two roughening worms (632) are respectively rotatably mounted in the two roughening thread grooves, and the top ends of the two vertical sliding platforms (424) are respectively penetrated through the two first vertical slide grooves (173) and protruded in the preparation chamber (162). The bottom surfaces of the two roughening transverse slide platforms (610) are respectively mounted on the top surfaces of the two vertical sliding platforms (424), and the two roughening transverse rotating blocks (616) are respectively slidably mounted in the two roughening transverse slide platforms (610). The roughening drive motor (65) is installed on the outer side of one of the roughening transverse rotating blocks (616). The ends are rotatably mounted in two roughening transverse slides (610), the output shaft of the roughening drive motor (65) is connected to one end of the roughening roller (62), and a roughening transverse adjustment motor (630) is convexly provided at one end of each roughening transverse rotating block (616), and the roughening transverse adjustment motor (630) is connected to the top of the two vertical slides (424), and a scraper installation rotating hole (633) is concavely provided at one end of the top of the side wall of each roughening transverse rotating block (616), and the scraper motor (618) is installed on the outer top of one of the roughening transverse slides (610), and the two ends of the scraper rotating shaft (617) are rotatably mounted in the two scraper installing rotating holes (633), and the output shaft of the scraper motor (618) is connected to one end of the scraper rotating shaft (617).The burr scraper (619) is installed in the scraper shaft (617).

10. A method for preparing a regenerated man-made composite fiberboard, applied to the regenerated man-made composite fiberboard preparation device as claimed in claim 9, characterized in that: The preparation method comprises: Step S1: placing the waste furniture boards in a regenerated man-made composite fiberboard preparation device, cutting the waste furniture boards into equal widths, and performing deep roughening on the upper and lower surfaces of the waste furniture boards to form boards to be assembled; Step S2: applying glue to the boards to be assembled, and laying them in an interlaced manner to form a core material (23); Step S3: a lower panel (22) is arranged on the bottom surface of the core material (23), and an upper panel (21) is arranged on the top surface of the core material (23) to form a sheet to be formed; Step S4: placing the sheet to be formed in a hot pressing device for hot pressing treatment to form a recycled artificial board.

Citation Information

Patent Citations

  • In-line process for preparing wood plastic composite panel with the appearance and texture similar to natural lumbers and apparatus therefor

    CN101316703A

  • Floor treatment process with fine wire drawing effect

    CN109571148A

  • Impregnation treatment method for formaldehyde-free flexible impregnated veneer

    CN111975910A

  • Preparation method of plate with cross section of wood as surface

    CN115709502A

  • Straw raw material pretreatment combined device, method and application of straw raw material pretreatment combined device

    CN116587383A