Method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether

By using an inorganic base catalyst to carry out the ethoxylation reaction between phenol and bisphenol A at low temperature, the problem of difficulty in removing phenol and low reaction selectivity in the prior art is solved, and high purity phenoxyethanol and bisphenol A are achieved The preparation of polyoxyethylene ether reduces energy consumption and by-products, and improves product performance and production efficiency.

CN118894765AActive Publication Date: 2024-11-05WANHUA CHEM GRP CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410932537.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-11-05
Estimated Expiration
2044-07-12

AI Technical Summary

Technical Problem

In the prior art, phenol is difficult to completely remove during the distillation process, low reaction selectivity, strong alkali or strong acid leads to decomposition under the melting process, high energy consumption of solvent process and environmental pollution. The problem.

Method used

The liquid mixture of phenol and bisphenol A is used to carry out ethoxylation reaction under low temperature conditions. The molar of phenol and bisphenol A is controlled by using inorganic base catalyst and ethylene oxide. The reaction temperature is proportional to ensure that the phenol is completely converted and the high-purity bisphenol A polyoxyethylene ether is produced, reducing the reaction temperature and reducing by-products.

Benefits of technology

Achieve high purity of phenoxyethanol (phenol content is less than 10ppm) and efficient preparation of bisphenol A polyoxyethylene ether, reducing reaction temperature and energy consumption, reducing by-products and color issues, improving product performance and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004940172560000051
    Figure BDA0004940172560000051
Patent Text Reader

Abstract

The invention provides a method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether. According to the method, phenol and bisphenol A are mixed to serve as an initiator, inorganic base serves as a catalyst, and phenoxyethanol and bisphenol A polyoxyethylene ether products are prepared at the same time through the two steps of ethoxylation reaction and rectification. According to the method, phenol can be completely converted, a very small amount of high polymer is generated, meanwhile, monomer bisphenol A is converted into a liquid mixture of bisphenol A polyoxyethylene ether and bisphenol A, the reaction temperature can be reduced, and the ethoxylation reaction continues to be conducted to obtain the bisphenol A polyoxyethylene ether product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of polyether synthesis, and particularly relates to a method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether. Background Art

[0002] Ethylene glycol phenyl ether is one of the representative compounds of phenyl ether. Due to its excellent comprehensive properties, ethylene glycol phenyl ether can be used as a solvent for acrylic resin, nitrocellulose, cellulose acetate, ethyl cellulose, epoxy resin, phenoxy resin, etc. It is an ideal solvent for hydroxybenzoic acid esters. In addition, ethylene glycol phenyl ether is also an ideal preservative and a raw material for the production of pesticides, medicines, cosmetics, and cleaning fluids. Due to its low volatility and high boiling point, it can be used as a solvent for ink pad inks and ballpoint pen inks that require penetration, a fragrance diluent, a paint stripper, and a textile processing carrier liquid. It has a wide range of uses. Daily chemical grade ethylene glycol phenyl ether has extremely high requirements for the phenol content, which is less than 10ppm, so extremely high requirements are placed on the refining and separation of this product.

[0003] Bisphenol A polyoxyethylene ether can give the material a certain rigidity and toughness because of its aromatic ring and polyether chain segment in its molecular structure. By adjusting the ratio of the two, bisphenol A polyoxyethylene ether products with specific properties can be obtained, thereby effectively making up for the defects of the material itself and improving performance. Bisphenol A polyoxyethylene ether can be used in the field of UV light curing, as a polyurethane elastomer, and as a coating adhesive. In addition, as a toughening agent for cathode electrophoretic paint, it can effectively improve the flexibility, corrosion resistance, and mechanical strength of electrophoretic paint. Because bisphenol A has a high melting point (152-158°C), the conventional preparation process is a melting process or a solvent process. The melting process reacts at 160°C. Bisphenol A is easily decomposed under strong alkali or strong acid to form isopropenylphenol, which leads to a decrease in product functionality, a darker color, and affects downstream use; the solvent process wastes a lot of energy in solvent removal and recovery.

[0004] CN106478385B provides a method for preparing high-purity propylene glycol phenyl ether or ethylene glycol phenyl ether of trace phenol, propylene oxide or ethylene oxide and excess phenol are catalyzed to synthesize phenyl ether, then distill and recover excess phenol, add inorganic alkali (one or any several of potassium hydroxide, sodium hydroxide or potassium carbonate and zinc powder) to convert remaining phenol into salt after obtaining crude product, and then obtain propylene glycol phenyl ether or ethylene glycol phenyl ether of trace phenol (30~90ppm) by rectification. This process is a post-processing process, and crude phenyl ether synthesized using excess phenol is distilled to recover most of phenol, add alkali to form salt, and rectify to obtain phenyl ether product containing trace phenol. This technological process is cumbersome, requires two-step rectification and alkali addition, does not significantly reduce energy consumption, and has low production efficiency.

[0005] CN101712600A discloses a method for preparing ethylene glycol, propylene glycol and butylene glycol phenyl ethers, wherein phenol is reacted with ethylene oxide, propylene oxide or butylene oxide at 70-140°C and a pressure less than 1MPa using base catalysis to generate crude products of ethylene glycol phenyl ether, propylene glycol phenyl ether or butylene glycol phenyl ether, wherein the molar ratio of phenol to epoxy is 1:0.6-1.2. The prepared crude benzene is distilled under reduced pressure to obtain ethylene glycol phenyl ether, propylene glycol phenyl ether or butylene glycol phenyl ether products. The process is not subjected to distillation and purification treatment, and the purity of the obtained product is more than 99%, the product grade is low, and the conversion rates of different epoxy species are different, the by-product content is high, and there is no practical value.

[0006] US20140142345A1 discloses an alkoxylation process for crude bisphenol A, in which crude bisphenol A containing ketone solvents remaining in the bisphenol A manufacturing process is subjected to an alkoxylation reaction at a temperature lower than the melting point of bisphenol A (30-140°C), thereby reducing side reactions and reducing the product color. This process utilizes crude bisphenol A containing ketone solvents produced in the process of preparing bisphenol A to carry out an alkoxylation reaction, and the presence of the solvent plays a role in lowering the reaction temperature. Its mechanism is not significantly different from that of preparing bisphenol A polyethers by conventional solvent processes, and ultimately, the solvent still needs to be removed by steam stripping or other methods.

[0007] In summary, the current production of phenoxyethanol still faces the problem of difficulty in removing phenol during the distillation process, and the problem of low reaction selectivity cannot be solved from a technological perspective. The mainstream of bisphenol A polyether currently uses the melting process and solvent process. The melting process is prone to decomposition when mixed with strong alkali at high temperature, resulting in the production of monofunctional by-products, which affects the downstream application performance and product color. The solvent process has problems such as high energy consumption for solvent removal and environmental pollution. Summary of the invention

[0008] One of the purposes of the present invention is to provide a method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether, which can completely convert phenol and generate a very small amount of polymer, and at the same time, the monomer bisphenol A is converted into a liquid mixture of bisphenol A polyoxyethylene ether and bisphenol A, and the reaction temperature can be lowered to continue the ethoxylation reaction to obtain the bisphenol A polyoxyethylene ether product.

[0009] In order to achieve the above-mentioned invention object, the present invention adopts the following technical scheme:

[0010] A method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether, wherein the method uses a mixture of phenol and bisphenol A as an initiator, uses an inorganic base as a catalyst, and undergoes two steps of ethoxylation reaction and distillation to simultaneously prepare phenoxyethanol and bisphenol A polyoxyethylene ether products.

[0011] In view of the difficulty in removing trace phenol by distillation of phenoxyethanol and the drawbacks of the melting process and solvent process of bisphenol A polyether, the inventors found in their research that by specifically utilizing the physical properties of phenol and bisphenol A adducts, selecting the ratio and temperature in the liquid region for ethoxylation reaction, and based on the difference in ethoxylation reaction activity between phenol and bisphenol A, phenol can be completely converted and a very small amount of polymer is generated, and at the same time, the monomer bisphenol A is converted into a liquid mixture of bisphenol A polyoxyethylene ether and bisphenol A, the reaction temperature can be lowered to continue the ethoxylation reaction to obtain the bisphenol A polyoxyethylene ether product.

[0012] In one embodiment of the present invention, in the ethoxylation reaction, the molar ratio of phenol to bisphenol A is 1:0.3-0.5.

[0013] In one embodiment of the present invention, the molar ratio of ethylene oxide to phenol is 1.1-1.3:1.

[0014] In one embodiment of the present invention, the catalyst is an inorganic base catalyst, preferably an alkaline hydroxide, more preferably potassium hydroxide and / or sodium hydroxide; preferably, the amount of the catalyst is 0.05%-0.1% of the total mass of phenol and bisphenol A.

[0015] In one embodiment of the present invention, the ethoxylation reaction uses a plug flow reactor to carry out ethoxylation reaction of phenol, bisphenol A and a catalyst with ethylene oxide; preferably, the plug flow reactor comprises a tubular reactor and / or a microchannel reactor.

[0016] In one embodiment of the present invention, the reaction temperature is 100-130° C. and the residence time is 1-3 h.

[0017] In one embodiment of the present invention, in the distillation step, phenoxyethanol is produced from the top of the tower, and a mixture of bisphenol A polyoxyethylene ether and bisphenol A is produced from the bottom of the tower; preferably, the operating temperature of the distillation process is 100-120° C.; and the operating pressure is 1-20 mbarA.

[0018] In one embodiment of the present invention, the reflux ratio of the distillation process is 0.5-5. The reflux ratio is the ratio of the reflux flow rate to the tower top extraction rate, and can be adjusted according to the molar ratio of phenol, bisphenol A and ethylene oxide.

[0019] In one embodiment of the present invention, the molar ratio of phenoxyethanol to bisphenol A polyoxyethylene ether is 1:0.1-0.3.

[0020] In one embodiment of the present invention, after the distillation step, optionally, the bisphenol A polyoxyethylene ether and the bisphenol A mixture are further subjected to ethoxylation reaction to obtain bisphenol A polyoxyethylene ethers with different addition numbers.

[0021] Compared with the prior art, the positive effects of the present invention are:

[0022] (1) The molar ratio of ethylene oxide to phenol and bisphenol A is slightly excessive to ensure the complete conversion of phenol. At the same time, the presence of bisphenol A can inhibit the continued reaction of ethylene glycol phenyl ether to form diethylene glycol phenyl ether. Only one step of distillation is required to separate phenoxyethanol and bisphenol A polyoxyethylene ether to obtain daily chemical grade phenoxyethanol (phenol content <10ppm). The conventional process requires more than two steps of distillation to separate phenoxyethanol, polymer and phenol.

[0023] (2) In the reaction process, phenol can act as a solvent for bisphenol A. After bisphenol A reacts with a small amount of ethylene oxide, it becomes a uniform liquid, which greatly reduces the reaction temperature. The mixture of bisphenol A polyoxyethylene ether and bisphenol A can continue to undergo ethoxylation reaction to obtain the product. The product obtained by this process has few by-products and excellent color (Hazen color <10). DETAILED DESCRIPTION

[0024] The following embodiments further illustrate the technical solutions provided by the present invention, but the present invention is not limited to the listed embodiments, and also includes any other known changes within the scope of the present invention.

[0025] Raw material information

[0026]

[0027] Analyze Project

[0028] Analyze Project instrument model Phenoxyethanol Purity Quantification Gas chromatography Agilent 7080B

[0029] Example 1

[0030] Add 94g phenol, 68.4g bisphenol A and 0.11g potassium hydroxide into a batching tank, replace with nitrogen three times, stir and mix, and heat to 100°C;

[0031] The raw materials and ethylene oxide in the batching tank are simultaneously introduced into the tubular reactor, and the reaction temperature is controlled to be maintained at 100±3°C. The feed flow rate of ethylene oxide is 24.2g / h, and the total amount is 48.4g.

[0032] The crude product obtained from the tubular reactor is passed into a distillation tower, and the operating temperature of the distillation tower is controlled to be 120°C, the operating pressure is 5mbaA, and the reflux ratio (the ratio of the reflux flow rate to the tower top output) is 2 for distillation separation, wherein a phenoxyethanol product (phenoxyethanol 99.96%, diethylene glycol phenyl ether 0.04%, phenol 4ppm) is obtained at the top of the tower, and a bisphenol A polyoxyethylene ether and a bisphenol A mixture are obtained at the bottom of the tower. The molar ratio of the obtained product phenoxyethanol to bisphenol A polyoxyethylene ether is 1:0.1.

[0033] Example 2

[0034] Add 94g phenol, 114g bisphenol A and 0.212g sodium hydroxide into the batching tank, replace with nitrogen three times, stir and mix, and heat to 120°C;

[0035] The raw materials and ethylene oxide in the batching tank are simultaneously introduced into the tubular reactor, and the reaction temperature is controlled to be maintained at 120±3°C. The feed flow rate of ethylene oxide is 28.6 g / h, and the total amount is 57.2 g.

[0036] The crude product obtained from the tubular reactor is passed into a distillation tower, and the operating temperature of the distillation tower is controlled to be 100°C, the operating pressure is 5mbaA, and the reflux ratio is 0.5 for distillation separation, wherein a phenoxyethanol product (phenoxyethanol 99.99%, diethylene glycol phenyl ether 0.01%, phenol 7ppm) is obtained at the top of the tower, and a bisphenol A polyoxyethylene ether and bisphenol A mixture are obtained at the bottom of the tower. The molar ratio of the obtained product phenoxyethanol to bisphenol A polyoxyethylene ether is 1:0.3.

[0037] The bottom product was introduced into the reactor, the reaction temperature was controlled to be maintained at 120±3°C, and ethylene oxide was continuously introduced at a flow rate of 30.8 g / h and a total amount of 30.8 g. After the feeding was completed, constant temperature aging was performed until the reaction was complete.

[0038] 1.58 g of magnesium silicate adsorbent was added to the obtained bisphenol A polyether, and the mixture was stirred and refined at 120° C. for 2 h, and the BPE2 (BPA+2 molEO) product was obtained after filtration.

[0039] Example 3

[0040] Add 94g phenol, 114g bisphenol A and 0.26g potassium hydroxide into the batching tank, replace with nitrogen three times, start stirring and mixing, and heat to 130°C;

[0041] The raw materials and ethylene oxide in the batching tank are simultaneously injected into the tubular reactor, and the reaction temperature is controlled to be maintained at 130±3°C. The feed flow rate of ethylene oxide is 24.2g / h, and the total amount is 48.4g.

[0042] The crude product obtained from the tubular reactor is passed into a distillation tower, and the operating temperature of the distillation tower is controlled to be 100°C, the operating pressure is 10mbaA, and the reflux ratio is 5 for distillation separation, wherein a phenoxyethanol product (phenoxyethanol 99.995%, diethylene glycol phenyl ether 0.005%, phenol 2ppm) is obtained at the top of the tower, and a bisphenol A polyoxyethylene ether and bisphenol A mixture are obtained at the bottom of the tower. The molar ratio of the obtained product phenoxyethanol to bisphenol A polyoxyethylene ether is 1:0.2.

[0043] The bottom product was introduced into the reactor, the reaction temperature was controlled to be maintained at 120±3°C, and ethylene oxide was continuously introduced at a flow rate of 48.4 g / h and a total amount of 96.8 g. After the feeding was completed, constant temperature aging was performed until the reaction was complete.

[0044] 1.88 g of magnesium silicate adsorbent was added to the obtained bisphenol A polyether, and the mixture was stirred and refined at 120° C. for 2 h, and the BPE6 (BPA+6 molEO) product was obtained after filtration.

[0045] Comparative Example 1

[0046] Compared with Example 1, the only difference is that bisphenol A is not added to the raw materials.

[0047] Add 94g phenol and 0.07g potassium hydroxide into the batching tank, replace with nitrogen three times, start stirring and mixing, and heat to 120°C;

[0048] The raw materials and ethylene oxide in the batching tank are simultaneously introduced into the tubular reactor, and the reaction temperature is controlled to be maintained at 100±3°C. The feed flow rate of ethylene oxide is 24.2g / h, and the total amount is 48.4g.

[0049] The crude product obtained from the tubular reactor is introduced into a distillation tower, and the operating temperature of the distillation tower is controlled to be 120° C., the operating pressure is 5 mbaA, and the reflux ratio is 2 for distillation separation, wherein a phenoxyethanol product (phenoxyethanol 99.83%, diethylene glycol phenyl ether 0.09%, phenol 0.8%) is obtained at the top of the tower, and a mixture of phenoxyethanol, diethylene glycol phenyl ether, and triethylene glycol phenyl ether is obtained at the bottom of the tower.

[0050] No bisphenol A was added to the reaction raw materials. After the reaction of phenol and EO in a tubular reactor, the products were separated by a single distillation tower. The residual phenol content in the phenoxyethanol at the top of the tower was 800 ppm, which was much higher than the requirement for use in the daily chemical industry (phenol content <10 ppm). A secondary distillation was required to continue to separate phenol.

[0051] At the same time, because bisphenol A is not added, the reaction selectivity of phenoxyethanol is low, the content of multiple addition products such as diethylene glycol phenyl ether and triethylene glycol phenyl ether increases, and the reaction yield decreases.

[0052] Those skilled in the art will appreciate that, based on the teachings of this specification, some modifications or adjustments may be made to the present invention, and these modifications or adjustments should also be within the scope defined by the claims of the present invention.

Claims

1. A method for co-producing phenoxyethanol and bisphenol A polyoxyethylene ether, It is characterized in that The method uses a mixture of phenol and bisphenol A as an initiator, uses an inorganic base as a catalyst, and undergoes two steps of ethoxylation reaction and rectification to simultaneously prepare phenoxyethanol and bisphenol A polyoxyethylene ether products.

2. The method according to claim 1, It is characterized in that In the ethoxylation reaction, the molar ratio of phenol to bisphenol A is 1:0.3-0.5; And / or, the molar ratio of ethylene oxide to phenol is 1.1-1.3:1; and / or, the catalyst is an inorganic base catalyst, preferably an alkaline hydroxide, more preferably potassium hydroxide and / or sodium hydroxide; Preferably, the amount of the catalyst used is 0.05%-0.1% of the total mass of phenol and bisphenol A.

3. The method according to claim 1 or 2, It is characterized in that The ethoxylation reaction uses a plug flow reactor to carry out an ethoxylation reaction of phenol, bisphenol A and a catalyst with ethylene oxide; Preferably, the plug flow reactor comprises a tubular reactor and / or a microchannel reactor; And / or, the reaction temperature is 100-130° C., and the residence time is 1-3 h.

4. The method according to any one of claims 1 to 3, It is characterized in that In the distillation step, phenoxyethanol is produced from the top of the tower, and a mixture of bisphenol A polyoxyethylene ether and bisphenol A is produced from the bottom of the tower; Preferably, the distillation process has an operating temperature of 100-120°C and an operating pressure of 1-20 mbarA; And / or, the reflux ratio of the distillation process is 0.5-5; And / or, the molar ratio of phenoxyethanol to bisphenol A polyoxyethylene ether is 1:0.1-0.

3.

5. The method according to any one of claims 1 to 4, It is characterized in that After the distillation step, optionally, the bisphenol A polyoxyethylene ether and the bisphenol A mixture are further subjected to ethoxylation reaction to obtain bisphenol A polyoxyethylene ethers with different addition numbers.

Citation Information

Patent Citations

  • Preparation method of trace phenol high-purity propylene glycol phenyl ether or glycol phenyl

    CN106478385A

  • Preparation method of bisphenol A polyether

    CN115838474A

  • Aromatic ethers and process for producing aromatic ethers

    US20040181099A1